Dispersible oil suspending agent containing cyantraniliprole and thiocyclam and preparation method thereof
By optimizing the composition and preparation process of the dispersible oil suspension, the problem of poor stability of the insecticidal ring was solved, and the stability and high efficiency of the suspension under different environments were achieved, especially the excellent control effect on thrips on scallions.
Patent Information
- Application Number
- CN202411074594.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-11-15
AI Technical Summary
In existing technologies, insecticidal rings have poor stability, causing them to decompose under high temperature, high humidity or light conditions, which affects the control effect. In addition, high-content oil suspensions are prone to poor dispersibility, insufficient anti-caking and viscosity reduction during storage and use, which affects the efficacy.
A dispersible oil suspension with a specific composition, including emulsifiers, alkyl naphthalene sulfonates, bromocyanamide, insecticidal rings, silicone defoamers, viscosity reducers, and ethylene glycol, is formed into a suspension with a particle size of less than 2 to 6 micrometers through high-speed shearing and sand milling processes. Viscosity reducers and ethylene glycol are added to ensure the stability and sprayability of the suspension.
It improves the stability and control effect of the insecticidal ring, especially showing excellent effect on thrips on scallions. The suspension maintains dispersion stability under different environmental conditions, expands the application range, and improves operation efficiency and ease of use.
Smart Images

Figure BDA0004981845930000141 
Figure BDA0004981845930000151
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of pesticide preparations, and in particular to a dispersible oil suspension containing cyantraniliprole and cypermethrin and a preparation method thereof. Background Art
[0002] In agricultural production, pest control has always been a key link in improving crop yield and quality. In order to effectively control pests, various chemical pesticides are widely used. Among them, cyantraniliprole and cypermethrin, as two highly effective insecticides, have been proven to have good control effects on a variety of crop pests. However, the stability of these active ingredients and the stability of the formulations are important challenges to achieve their long-term effectiveness.
[0003] As a biologically active substance, insecticide ring may encounter decomposition problems during storage and use when added at a high dosage, especially under high temperature, high humidity or light conditions. Its decomposition will lead to reduced efficacy and affect the control effect. Therefore, how to improve the stability of insecticide ring and extend its validity period is a key issue that needs to be solved in formulation development.
[0004] Oil suspension is a preparation form in which oily active ingredients are dispersed in an aqueous phase, which can improve the bioavailability and persistence of the active ingredients. However, it is a technical challenge to prepare high-content oil suspensions and maintain their stability. When stored for a long time or used at different temperatures, the suspension may have problems such as poor dispersibility, anti-bottoming and insufficient viscosity reduction, resulting in uneven or reduced drug efficacy.
[0005] In order to overcome the above problems, the present invention provides a dispersible oil suspension containing cyantraniliprole and cypermethrin and a preparation method thereof. By optimizing the selection of oil-based solvents and emulsifiers and adopting a specific process flow, the present invention aims to improve the stability of the cypermethrin and ensure the stability and effectiveness of the oil suspension under long-term storage and different application conditions. In addition, by adding a viscosity reducer and optimizing the dispersion process, the present invention also solves the viscosity reduction and bottoming prevention problems of high-content oil suspensions, thereby improving the overall performance and use effect of the preparation.
[0006] Chinese invention patent application CN116076517A discloses a dispersible oil suspension containing cyantraniliprole and cyclopentane and its preparation and application, including the following components and weight percentages: cyantraniliprole 0.1-20%, cyclopentane 0.1-30%, emulsifier 15-25%, dispersant 0.1-5%, thickener 0.1-3%, viscosity reducer 0.1-3%, stabilizer 0.1-10%, synergist 0.1-50%, and oil phase carrier supplemented to 100%. Compared with the prior art, the dispersible oil suspension containing cyantraniliprole and cyclopentane of the invention is environmentally friendly, has good stability, has high protective effect on vegetable yellow striped flea beetles and good safety, and its preparation method is simple and easy to industrialize and mass produce. In addition, the block polymer carboxylate compound 100# selected by the invention provides a good viscosity reduction idea and choice for the later development of dispersible oil suspension products containing soybean oil and other vegetable oil systems. However, the dispersible oil suspension of the invention has poor control effect on onion thrips, low formulation stability and easy to form a bottom. Summary of the invention
[0007] In view of the deficiencies in the prior art, the technical problem to be solved by the present invention is to provide a dispersible oil suspension containing cyantraniliprole and cypermethrin, which has good control effect on onion thrips, high formulation stability and anti-bottoming, and a preparation method thereof.
[0008] In order to achieve the above-mentioned object of the invention, the present invention adopts the following technical solutions:
[0009] A dispersible oil suspension containing cyantraniliprole and cypermethrin, comprising the following components in percentage by weight:
[0010] 3-4% emulsifier, 1-3% alkylnaphthalene sulfonate, 4-6% cyantraniliprole, 25-35% cyclohexane, 0.05-0.2% silicone defoamer, 0.5-2% viscosity reducer, 0.3-0.5% ethylene glycol, and the balance is oil-based solvent.
[0011] A method for preparing a dispersible oil suspension containing cyantraniliprole and cypermethrin is as follows:
[0012] Weigh each raw material according to weight percentage, add emulsifier and alkylnaphthalene sulfonate to the oil-based solvent, use a stirrer to mix, add cyantraniliprole and cypermethrin under high-speed shear conditions, mix evenly, add an organosilicon defoamer, continue to stir and mix until a uniform suspension is formed, place the suspension in a sand mill, use zirconium beads as grinding media, and perform fine grinding. After the grinding is completed, add a viscosity reducer and ethylene glycol, stir and mix evenly to obtain a dispersible oil suspension.
[0013] The oil-based solvent is a mixture of epoxidized soybean oil and methyl oleate in a weight ratio of 1:4.
[0014] The emulsifier is a mixture of fatty alcohol polyoxyethylene ether and polyvinyl alcohol in a weight ratio of 3:1.
[0015] The particle size after the fine grinding process is less than 2 to 6 microns.
[0016] The preparation method of the viscosity reducer is as follows, in parts by weight:
[0017] Step 1: dissolving 80 to 100 parts of N,N-dimethylacrylamide, 1 to 3 parts of sodium p-styrene sulfonate and 2 to 4 parts of lauryl acrylate in 400 to 600 parts of a solvent, introducing nitrogen, and stirring at 40 to 60° C. for 20 to 40 minutes to obtain a mixed solution;
[0018] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 is raised to 60-80° C., 0.5-0.8 parts of an initiator is added, and a free radical polymerization reaction is carried out for 5-10 hours to obtain a crude product;
[0019] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried for 5 to 15 hours to obtain a pretreated viscosity reducer;
[0020] Step 4: compounding the pretreatment viscosity reducer prepared in step 3 with 1 to 3 parts of vinyldimethylfluorosilane; during the compounding process, adding 4 to 6 parts of acetaldehyde and 2 to 4 parts of sodium bisulfite, adjusting the pH value, and treating at 50 to 80° C. for 4 to 6 hours to obtain a post-treatment viscosity reducer;
[0021] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, and adjust the temperature of the spray drying equipment to obtain the viscosity reducer.
[0022] The solvent is one of dimethyl sulfoxide, dimethylformamide or N-methylpyrrolidone.
[0023] The initiator is one of benzoyl peroxide and azobisisobutyronitrile.
[0024] The temperature of the spray drying equipment is adjusted so that the inlet temperature is between 200 and 300°C and the outlet temperature is between 80 and 90°C.
[0025] The pH value is adjusted to 4-7 by adding aminosulfonic acid.
[0026] In the preparation method of the dispersible oil suspension containing cyantraniliprole and cyclopentane, an oil-based solvent (a mixture of epoxidized soybean oil and methyl oleate) is used as the basis of the suspension, providing a medium to dissolve and disperse the active ingredients cyantraniliprole and cyclopentane.
[0027] Emulsifier (mixture of fatty alcohol polyoxyethylene ether and polyvinyl alcohol): helps stabilize the oil-water interface, allowing the oil-based solvent to mix with the water phase to form a stable emulsion, thereby improving the dispersibility of the suspending agent.
[0028] As surfactants, alkylnaphthalene sulfonates help reduce the surface tension of the oil-water interface, promote oil-water mixing, and enhance the stability of the suspension.
[0029] Cyantraniliprole is an effective insecticide that is toxic to specific pests and is used to control and reduce pest populations.
[0030] Cyclopentanil is another insecticide that works synergistically with cyantraniliprole to enhance the control effect on pests.
[0031] Silicone defoamers reduce the generation of bubbles during the mixing process to prevent foam from affecting the quality and use effect of the suspension.
[0032] Zirconium beads (as grinding media of sand mill) are used in the physical grinding process to ensure the fine particle size of active ingredients in the suspension and improve the dispersion and uniformity of the suspension.
[0033] Viscosity reducers are used to reduce the viscosity of suspension concentrates, making them easier to spray and use, and to enhance the control effect on onion thrips.
[0034] Ethylene glycol acts as a wetting agent and stabilizer, helping to maintain the fluidity and stability of the suspension.
[0035] Vinyldimethylfluorosilane is used in the compounding process of viscosity reducers and may be used to enhance the temperature resistance and salt resistance of suspension concentrates.
[0036] Acetaldehyde is used in the compounding process of viscosity reducers, possibly for cross-linking reactions to enhance the structural stability of the viscosity reducers.
[0037] Sodium bisulfite, as a reducing agent, may be used to adjust the chemical reaction environment of the viscosity reducer and affect its final performance.
[0038] Aminosulfonic acid is used to adjust the pH value to ensure that the viscosity reducer is stable under appropriate acid and alkaline conditions. It also affects the overall stability of the suspension concentrate and the activity of the active ingredient.
[0039] These substances work together to ensure the high efficiency and stability of the dispersible oil suspension, enabling it to be effectively used in the control of agricultural pests.
[0040] Compared with the prior art, the present invention has the following beneficial effects:
[0041] 1) The dispersible oil suspension of the present invention combines two effective ingredients, cyantraniliprole and cypermethrin, and can provide a wider range of control effects on different pests, thereby enhancing the control ability of pests.
[0042] 2) The dispersible oil suspension of the present invention uses a specific emulsifier and an oil-based solvent mixture, and through high-speed shearing and sand milling processes, ensures uniform dispersion of the active ingredients, thereby improving the dispersibility and stability of the suspension.
[0043] 3) The viscosity reducer added to the dispersible oil suspension of the present invention helps to reduce the viscosity of the suspension, making the product easier to spray and use, improving the working efficiency and convenience of use, and having an excellent control effect on onion thrips.
[0044] 4) The dispersible oil suspension of the present invention can maintain dispersion stability and effectiveness under different environmental conditions, thereby expanding its application in different crops and regions. DETAILED DESCRIPTION
[0045] Main sources of substances:
[0046] Epoxidized soybean oil: Shandong Yousuo Chemical Technology Co., Ltd., product number: 4506211.
[0047] Fatty alcohol polyoxyethylene ether: Jiangsu Wei Tu Chemical Co., Ltd., product number: AEO3.
[0048] Polyvinyl alcohol: Langfang Feitai New Material Technology Co., Ltd., item number: 2488-1.
[0049] Alkylnaphthalene sulfonate: Wuhan Lanabai Pharmaceutical Chemical Co., Ltd., model: Petro 22NL IQU ID.
[0050] Cyantraniliprole: Guangzhou Weida Pharmaceutical Co., Ltd., product number: 001.
[0051] Insecticidal ring: Anhui Changrong Biotechnology Co., Ltd., CAS: 31895-21-3.
[0052] Silicone defoamer: Nanjing Leipu Chemical Co., Ltd., item number: 105.
[0053] Example 1
[0054] A method for preparing a dispersible oil suspension containing cyantraniliprole and cypermethrin is as follows:
[0055] 3.5 g of emulsifier and 2 g of alkylnaphthalene sulfonate are added to 58 g of oil-based solvent, wherein the oil-based solvent is a mixture of epoxy soybean oil and methyl oleate in a weight ratio of 1:4, and the emulsifier is a mixture of fatty alcohol polyoxyethylene ether and polyvinyl alcohol in a weight ratio of 3:1. The mixture is mixed using a stirrer, and 5 g of cyantraniliprole and 30 g of insecticide ring are added under high-speed shear conditions, and the mixture is mixed evenly. 0.1 g of silicone defoamer is added, and the mixture is stirred and mixed continuously until a uniform suspension is formed. The suspension is placed in a sand mill, and zirconium beads are used as grinding media for fine grinding until the particle size is less than 4 microns. After the grinding is completed, 1 g of viscosity reducer and 0.4 g of ethylene glycol are added, and the mixture is stirred and mixed evenly to obtain a dispersible oil suspension.
[0056] The preparation method of the viscosity reducing agent is as follows:
[0057] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of lauryl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0058] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of benzoyl peroxide was added, and a free radical polymerization reaction was carried out for 8 hours to obtain a crude product;
[0059] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0060] Step 4: compounding the pre-treatment viscosity reducer prepared in step 3 with 2 g of vinyldimethylfluorosilane; during the compounding process, adding 5 g of acetaldehyde and 3 g of sodium bisulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70° C. for 5 hours to obtain a post-treatment viscosity reducer;
[0061] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0062] Example 2
[0063] The preparation method of a dispersible oil suspension containing cyantraniliprole and cypermethrin is basically the same as that in Example 1, except that the preparation method of the viscosity reducer is different.
[0064] The preparation method of the viscosity reducing agent is as follows:
[0065] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of hexadecyl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0066] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of benzoyl peroxide was added, and a free radical polymerization reaction was carried out for 8 hours to obtain a crude product;
[0067] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0068] Step 4: compounding the pre-treatment viscosity reducer prepared in step 3 with 2 g of vinyldimethylfluorosilane; during the compounding process, adding 5 g of acetaldehyde and 3 g of sodium bisulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70° C. for 5 hours to obtain a post-treatment viscosity reducer;
[0069] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0070] Example 3
[0071] The preparation method of a dispersible oil suspension containing cyantraniliprole and cypermethrin is basically the same as that in Example 1, except that the preparation method of the viscosity reducer is different.
[0072] The preparation method of the viscosity reducing agent is as follows:
[0073] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of octadecyl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0074] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of benzoyl peroxide was added, and a free radical polymerization reaction was carried out for 8 hours to obtain a crude product;
[0075] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0076] Step 4: compounding the pre-treatment viscosity reducer prepared in step 3 with 2 g of vinyldimethylfluorosilane; during the compounding process, adding 5 g of acetaldehyde and 3 g of sodium bisulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70° C. for 5 hours to obtain a post-treatment viscosity reducer;
[0077] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0078] Example 4
[0079] The preparation method of a dispersible oil suspension containing cyantraniliprole and cypermethrin is basically the same as that in Example 1, except that the preparation method of the viscosity reducer is different.
[0080] The preparation method of the viscosity reducing agent is as follows:
[0081] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of lauryl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0082] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of benzoyl peroxide was added, and a free radical polymerization reaction was carried out for 8 hours to obtain a crude product;
[0083] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0084] Step 4: compounding the pre-treatment viscosity reducer prepared in step 3 with 2g of triethylfluorosilane; during the compounding process, adding 5g of acetaldehyde and 3g of sodium bisulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70°C for 5 hours to obtain a post-treatment viscosity reducer;
[0085] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0086] Example 5
[0087] The preparation method of a dispersible oil suspension containing cyantraniliprole and cypermethrin is basically the same as that in Example 1, except that the preparation method of the viscosity reducer is different.
[0088] The preparation method of the viscosity reducing agent is as follows:
[0089] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of lauryl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0090] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of benzoyl peroxide was added, and a free radical polymerization reaction was carried out for 8 hours to obtain a crude product;
[0091] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0092] Step 4: compounding the pre-treatment viscosity reducer prepared in step 3 with 2 g of 3-aminopropyldimethylfluorosilane; during the compounding process, adding 5 g of acetaldehyde and 3 g of sodium bisulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70° C. for 5 hours to obtain a post-treatment viscosity reducer;
[0093] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0094] Example 6
[0095] The preparation method of a dispersible oil suspension containing cyantraniliprole and cypermethrin is basically the same as that in Example 1, except that the preparation method of the viscosity reducer is different.
[0096] The preparation method of the viscosity reducing agent is as follows:
[0097] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of lauryl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0098] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of benzoyl peroxide was added, and a free radical polymerization reaction was carried out for 8 hours to obtain a crude product;
[0099] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0100] Step 4: compounding the pre-treatment viscosity reducer prepared in step 3 with 2 g of vinyldimethylfluorosilane; during the compounding process, adding 5 g of acetaldehyde and 3 g of sodium sulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70° C. for 5 hours to obtain a post-treatment viscosity reducer;
[0101] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0102] Comparative Example 1
[0103] The preparation method of a dispersible oil suspension containing cyantraniliprole and cypermethrin is basically the same as that in Example 1, except that the preparation method of the viscosity reducer is different.
[0104] The preparation method of the viscosity reducing agent is as follows:
[0105] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of lauryl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0106] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of azobisisobutyronitrile was added, and free radical polymerization was carried out for 8 hours to obtain a crude product;
[0107] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0108] Step 4: compounding the pre-treatment viscosity reducer prepared in step 3 with 2 g of vinyldimethylfluorosilane; during the compounding process, adding 5 g of acetaldehyde and 3 g of sodium bisulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70° C. for 5 hours to obtain a post-treatment viscosity reducer;
[0109] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0110] Comparative Example 2
[0111] The preparation method of a dispersible oil suspension containing cyantraniliprole and cypermethrin is basically the same as that in Example 1, except that the preparation method of the viscosity reducer is different.
[0112] The preparation method of the viscosity reducing agent is as follows:
[0113] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of lauryl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0114] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of benzoyl peroxide was added, and a free radical polymerization reaction was carried out for 8 hours to obtain a crude product;
[0115] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0116] Step 4: compounding the pre-treatment viscosity reducer prepared in step 3 with 2g of trifluoropropyltriethoxysilane; during the compounding process, adding 5g of acetaldehyde and 3g of sodium bisulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70°C for 5 hours to obtain a post-treatment viscosity reducer;
[0117] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0118] Comparative Example 3
[0119] The preparation method of a dispersible oil suspension containing cyantraniliprole and cypermethrin is basically the same as that in Example 1, except that the preparation method of the viscosity reducer is different.
[0120] The preparation method of the viscosity reducing agent is as follows:
[0121] Step 1: dissolving 90 g of N,N-dimethylacrylamide, 2 g of sodium p-styrenesulfonate and 3 g of lauryl acrylate in 500 g of dimethyl sulfoxide, introducing nitrogen, and stirring at 50° C. for 30 minutes to obtain a mixed solution;
[0122] Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 was raised to 70° C., 0.6 g of benzoyl peroxide was added, and a free radical polymerization reaction was carried out for 8 hours to obtain a crude product;
[0123] Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried in a vacuum drying oven for 10 hours to obtain a pretreated viscosity reducer;
[0124] Step 4: compounding the pretreatment viscosity reducer prepared in step 3 with 2 g of vinyldimethylfluorosilane; during the compounding process, adding 5 g of formaldehyde and 3 g of sodium bisulfite, and then adding aminosulfonic acid to adjust the pH value to 6, and treating at 70° C. for 5 hours to obtain a post-treatment viscosity reducer;
[0125] Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, adjust the temperature of the spray drying equipment to ensure that the inlet temperature is 240° C. and the outlet temperature is 85° C., to obtain the viscosity reducer.
[0126] Comparative Example 4
[0127] A method for preparing a dispersible oil suspension containing cyantraniliprole and cypermethrin is as follows:
[0128] 3.5 g of emulsifier and 2 g of alkylnaphthalene sulfonate are added to 58 g of oil-based solvent, wherein the oil-based solvent is a mixture of epoxy soybean oil and methyl oleate in a weight ratio of 1:4, and the emulsifier is a mixture of fatty alcohol polyoxyethylene ether and polyvinyl alcohol in a weight ratio of 3:1. The mixture is mixed using a stirrer, and 5 g of cyantraniliprole and 30 g of insecticide ring are added under high-speed shear conditions, and the mixture is mixed evenly. 0.1 g of silicone defoamer is added, and the mixture is stirred and mixed continuously until a uniform suspension is formed. The suspension is placed in a sand mill, and zirconium beads are used as grinding media for fine grinding until the particle size is less than 4 microns. After the grinding is completed, 0.4 g of ethylene glycol is added, and the mixture is stirred and mixed evenly to obtain a dispersible oil suspension.
[0129] Test Example 1
[0130] Field trials for controlling onion thrips
[0131] In order to evaluate the control effect of different pesticides on onion thrips, a field trial was conducted at an onion planting base in Huanggang, Hubei. The following is the detailed method of the trial:
[0132] Crops and test subjects: Test crops: Welsh onion, the variety is Dawutong. Test subjects: Onion thrips.
[0133] Test conditions: Location: Soil fertility is at a medium level in the green onion planting area. Field management: Maintain consistency to ensure the accuracy of the test results.
[0134] Experimental design: Treatment setting: There are 10 different pesticide treatments, and each treatment is repeated four times. Experimental layout: Random arrangement is adopted, and the area of each experimental plot is 50 square meters. Clear water is used as the blank control area.
[0135] Test time and application: Application time: June 20, 2023, when the onion thrips are active. Application tools: Use an electric sprayer equipped with a fan-shaped mist nozzle, and the working pressure is controlled between 0.12-0.3Mpa. The dosage is 40g.ai / hm.
[0136] Environmental conditions: The weather on the day of application was sunny to cloudy, with temperatures ranging from 24°C to 32°C.
[0137] Data collection and evaluation: Pest base survey: Before applying the pesticide, a five-point sampling method was used. Six green onion tubes with good growth conditions were selected at each sampling point, and the number of thrips was recorded and marked. Prevention effect evaluation: After applying the pesticide, the marked green onion tubes were rechecked at 3 and 7 days, the number of thrips was counted, and the insect population reduction rate and control effect were calculated accordingly. Observation records: 3 and 7 days after applying the pesticide, the growth status of the green onions was checked, and whether there was any pesticide damage.
[0138] Efficacy evaluation method:
[0139] Pest reduction rate (%) = (number of insects before application - number of insects after application) / number of insects before application × 100 Control effect (%) = (pest reduction rate in treatment area - insect reduction rate in blank control area) / (100 - insect reduction rate in blank control area) × 100
[0140] The control effect on onion thrips is shown in Table 1.
[0141] Table 1 Field test results
[0142]
[0143]
[0144] Test Example 2
[0145] Dispersion stability
[0146] According to the specifications of MT180 and C IPAC Handbook H (P310, 1998), we conducted dispersibility tests on the dispersible oil suspensions prepared in the examples and comparative examples. The test process includes diluting the samples with C IPAC standard water A and D at 30±2°C and observing the initial dispersion after dilution. Then, the diluted samples are placed at room temperature for 48 hours and their dispersibility is evaluated again. The evaluation criteria are mainly based on whether there is precipitation, floating oil and emulsion in the sample. The specific rating criteria are as follows:
[0147] Level 1: There is absolutely no floating oil, precipitation or emulsion in the sample.
[0148] Level 2: There is only slight emulsion in the sample, without floating oil and precipitation.
[0149] Level 3: Slight emulsions and precipitation are present in the sample, but no floating oil is present.
[0150] Level 4: The amount of creaming and precipitation in the sample increases, but there is still no floating oil.
[0151] Level 5: The emulsion and precipitation in the sample increase significantly, and there is slight floating oil.
[0152] Level 6: There is an increase in floating oil in the sample.
[0153] Level 7: The amount of floating oil in the sample increases significantly.
[0154] The results are shown in Table 2.
[0155] Table 2 Dispersion stability test results
[0156] Experimental protocol Initial dispersion Dispersibility after 2 days Example 1 Level 1 Level 1 Example 2 Level 1 Level 2 Example 3 Level 1 Level 2 Example 4 Level 2 Level 3 Example 5 Level 2 Level 3 Example 6 Level 1 Level 2 Comparative Example 1 Level 1 Level 2 Comparative Example 2 Level 2 Level 4 Comparative Example 3 Level 1 Level 2 Comparative Example 4 Level 3 Level 5
[0157] From the test data in Tables 1 and 2, it can be seen that the dispersible oil suspension concentrate obtained in Example 1 of the present invention has good onion thrips control effect and dispersion stability.
[0158] In Examples 1, 2 and 3, the preparation method of the viscosity reducer involves a free radical polymerization reaction, which is a chain growth polymerization mechanism. During the polymerization process, the carbon chain length of the acrylate compound affects the molecular weight, molecular weight distribution and final physical and chemical properties of the polymer. Specifically, dodecyl acrylate has a shorter carbon chain length than hexadecyl acrylate and octadecyl acrylate. Shorter carbon chains may produce lower molecular weight polymers, which may affect the solubility and dispersibility of the polymer. Lower molecular weight polymers are more easily dispersed in oil-based solvents, thereby improving the dispersion stability of oil suspensions. Shorter carbon chains may cause polymers to have lower viscosity, which helps to improve the fluidity and spray performance of oil suspensions, making them easier to distribute evenly in practical applications. Shorter carbon chains may change the surface activity of the polymer, affecting its adsorption and dispersion ability at the oil-water interface. This may have a positive effect on the stability and control effect of the suspension. Different acrylate compounds may have different interactions with active ingredients such as cyantraniliprole and cypermethrin, affecting their release rate and biological activity. Dodecyl acrylate may interact more favorably with these active ingredients, thereby improving the control effect.
[0159] In embodiment 1, 4, 5 and comparative example 2, the preparation method of viscosity reducer is basically the same, but the silane coupling agent used is different. The main function of these silane coupling agents is as surfactant, they can improve the compatibility of polymer and pesticide molecule, enhance the adhesion and dispersibility of polymer. In these embodiments and comparative examples, vinyl dimethyl fluorosilane, triethyl fluorosilane, 3-aminopropyl dimethyl fluorosilane and trifluoropropyl triethoxysilane are all fluorinated silane coupling agents, but their chemical structure and functional group are different, which may affect their performance in viscosity reducer. The vinyl group in vinyl dimethyl fluorosilane has higher reactivity, can effectively compound with the active group in the polymer chain, thereby improving the stability and dispersibility of polymer. Fluorinated silane coupling agent usually has good interfacial compatibility, can improve the compatibility of polymer with other substances. Vinyl dimethyl fluorosilane may more effectively reduce the interfacial tension between polymer and oil-based solvent in the preparation process of oil suspension, and improve dispersion stability. The molecular structure of vinyldimethylfluorosilane may be more stable than other silane coupling agents, which helps to improve the weather resistance and long-term stability of the final product. Vinyldimethylfluorosilane may show better adaptability under the polymerization reaction conditions in Example 1, which helps to improve the efficiency of the reaction and the quality of the product.
[0160] The main difference between Example 1 and Example 6 in the preparation process of the viscosity reducer is that the types of sulfites used are different. Sodium bisulfite has stronger reducing properties than sodium sulfite. In the preparation process of the viscosity reducer, sodium bisulfite may play a certain antioxidant effect, which helps to protect the polymer chain from oxidative damage, thereby improving the stability and durability of the oil suspension. This antioxidant property may help to maintain the activity of the effective ingredients cyantraniliprole and cypermethrin in the oil suspension, thereby improving the control effect. The use of sodium bisulfite may also improve the onion thrips control effect and dispersion stability of the dispersible oil suspension containing cyantraniliprole and cypermethrin through various mechanisms. These mechanisms include its reducing and antioxidant properties, the regulating effect on pH value, the interaction with the silane coupling agent, and the protective effect on the stability and activity of the effective ingredients.
[0161] In Example 1 and Comparative Example 1, the free radical initiators used in the preparation process of the viscosity reducer are different. Benzoyl peroxide is used in Example 1, while azobisisobutyronitrile is used in Comparative Example 1. Benzoyl peroxide and azobisisobutyronitrile are both commonly used free radical initiators, but their initiation efficiency and reaction rate may be different. Benzoyl peroxide can decompose and generate free radicals at a relatively low temperature, while azobisisobutyronitrile usually requires a higher temperature to effectively decompose. In Example 1, the use of benzoyl peroxide may effectively initiate polymerization at a relatively low reaction temperature, thereby better controlling the molecular weight and molecular weight distribution of the polymer, which may be beneficial for improving the dispersion stability and control effect of the oil suspension.
[0162] Example 1 and Comparative Example 3 used different aldehyde compounds in the preparation process of the viscosity reducer. Acetaldehyde was used in Example 1, while formaldehyde was used in Comparative Example 3. Acetaldehyde has a methyl group and an active aldehyde group, while formaldehyde only contains one aldehyde group. Due to the presence of a methyl group, the intermolecular forces (such as van der Waals forces) of acetaldehyde may be stronger than those of formaldehyde. This stronger intermolecular force may help to improve the solubility of the viscosity reducer in the oil-based solvent, thereby improving the dispersibility of the oil suspension. Formaldehyde is a known environmental pollutant that has certain negative effects on human health and the ecological environment. In contrast, although acetaldehyde also has certain toxicity, its environmental impact may be relatively small.
[0163] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for preparing a dispersible oil suspension containing cyantraniliprole and cypermethrin, characterized in that: The steps include: Weigh each raw material according to weight percentage, add an emulsifier and an alkylnaphthalene sulfonate to an oil-based solvent, mix with a stirrer, add cyantraniliprole and cypermethrin under high-speed shearing conditions, mix evenly, add an organosilicon defoamer, continue to stir and mix until a uniform suspension is formed, place the suspension in a sand mill, use zirconium beads as a grinding medium, perform fine grinding, add a viscosity reducer and ethylene glycol after grinding, stir and mix evenly, and obtain a dispersible oil suspension; The weight percentage composition of the raw materials is 3-4% of emulsifier, 1-3% of alkylnaphthalene sulfonate, 4-6% of cyantraniliprole, 25-35% of cyclohexane, 0.05-0.2% of organosilicon defoamer, 0.5-2% of viscosity reducer, 0.3-0.5% of ethylene glycol, and the balance is oil-based solvent.
2. The method according to claim 1, characterized in that The oil-based solvent is a mixture of epoxidized soybean oil and methyl oleate in a weight ratio of 1:
4.
3. The method according to claim 1, characterized in that The emulsifier is a mixture of fatty alcohol polyoxyethylene ether and polyvinyl alcohol in a weight ratio of 3:
1.
4. The method according to claim 1, characterized in that The particle size after the fine grinding process is less than 2 to 6 microns.
5. The method according to claim 1, characterized in that The preparation method of the viscosity reducer is as follows, in parts by weight: Step 1: dissolving 80 to 100 parts of N,N-dimethylacrylamide, 1 to 3 parts of sodium p-styrene sulfonate and 2 to 4 parts of lauryl acrylate in 400 to 600 parts of a solvent, introducing nitrogen, and stirring at 40 to 60° C. for 20 to 40 minutes to obtain a mixed solution; Step 2: Under a nitrogen atmosphere, the temperature of the mixed solution prepared in step 1 is raised to 60-80° C., 0.5-0.8 parts of an initiator is added, and a free radical polymerization reaction is carried out for 5-10 hours to obtain a crude product; Step 3: The crude product prepared in step 2 is precipitated and washed with acetone to remove unreacted monomers and impurities; the washed product is dried for 5 to 15 hours to obtain a pretreated viscosity reducer; Step 4: compounding the pretreatment viscosity reducer prepared in step 3 with 1 to 3 parts of vinyldimethylfluorosilane; during the compounding process, adding 4 to 6 parts of acetaldehyde and 2 to 4 parts of sodium bisulfite, adjusting the pH value, and treating at 50 to 80° C. for 4 to 6 hours to obtain a post-treatment viscosity reducer; Step 5: spray-dry the post-treatment viscosity reducer prepared in step 4, and adjust the temperature of the spray drying equipment to obtain the viscosity reducer.
6. The method according to claim 5, characterized in that The solvent is one of dimethyl sulfoxide, dimethylformamide or N-methylpyrrolidone.
7. The method according to claim 5, characterized in that The initiator is one of benzoyl peroxide and azobisisobutyronitrile.
8. The method according to claim 5, characterized in that The temperature of the spray drying equipment is adjusted so that the inlet temperature is between 200 and 300°C and the outlet temperature is between 80 and 90°C.
9. The method according to claim 5, characterized in that The pH value is adjusted to 4-7 by adding aminosulfonic acid.
10. A dispersible oil suspension containing cyantraniliprole and cypermethrin, characterized in that: Prepared by the method according to any one of claims 1 to 9.