Epitaxial equipment cleaning method, epitaxial wafer and computer readable medium
Through the preliminary purge, heating and repeatable cleaning steps of the epitaxial equipment, the accumulation of impurities by-products caused by the downtime of the epitaxial equipment Scrubber is solved, and the effective removal of the surface particles of the epitaxial sheet and the improvement of product quality are achieved.
Patent Information
- Application Number
- CN202411028001.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-07-30
AI Technical Summary
When the Scrubber of the epitaxial equipment goes down, impurity by-products cannot be discharged in time, resulting in particle deposition on the surface of the epitaxial sheet, seriously affecting product quality.
Using an epitaxial device cleaning method, including performing repeatable cleaning steps after initial purge and heating, through purge, hydrogen baking and etching gas treatment, gradually remove contaminants from the reaction chamber, and detect cleaning by testing silicon wafers Indicators to ensure that preset standards are met.
Effectively clean the reaction chamber of the epitaxial equipment, reduce the deposition of particles on the surface of the epitaxial sheet, improve product quality, and ensure that the cleaning indicators meet preset standards.
Smart Images

Figure CN118950633A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor processing technology, and in particular to an epitaxial equipment cleaning method, an epitaxial wafer, and a computer-readable medium. Background Art
[0002] The epitaxial growth process of silicon is an important process in the manufacture of semiconductor chips. It is a method of growing an epitaxial layer with controllable resistivity, thickness, no crystal-origin particles (COP) defects and no oxygen precipitation on a polished wafer as a substrate under certain conditions. It mainly includes vacuum epitaxial deposition, vapor phase epitaxial deposition and liquid phase epitaxial deposition. Among them, vapor phase epitaxial deposition is the most widely used. In a high temperature environment, a single crystal silicon is generated by the reaction of silicon source gas and hydrogen and deposited on the surface of the silicon wafer to obtain an epitaxial layer.
[0003] The epitaxial process requires a large amount of HCl (hydrogen chloride) and SiHCl 3 (Silicon Hydrochloride), B 2 H 6 (dihydride diboride), H 2 (hydrogen) and other special gases, including HCl, SiHCl 3 , B 2 H 6 These gases are all highly toxic and will affect the personal and environmental safety around the plant, so the gases in the epitaxial equipment need to be handled safely to avoid accidents.
[0004] The epitaxial gas scrubber is a device specially designed to treat the epitaxial gas exhaust. Through the exhaust pipe of the epitaxial furnace and the air inlet of the gas scrubber, the epitaxial exhaust gas enters the gas scrubber for reaction and then discharges the pollution-free gas.
[0005] Generally, the reaction exhaust gas of the epitaxial equipment is processed by the scrubber and finally discharged into the air. However, when the scrubber of the epitaxial equipment fails, the impurity byproducts generated by the reaction in the epitaxial furnace chamber cannot be discharged out of the chamber in time, and will return to the reaction chamber from the exhaust pipe of the reaction chamber, causing the chamber environment to deteriorate, resulting in particle deposition on the surface of the epitaxial wafer (EPI Wafer), which seriously affects the product quality. Summary of the invention
[0006] The disclosed embodiment provides a method for cleaning epitaxial equipment, which can reduce epitaxial wafer particle contamination and improve product quality.
[0007] The technical solutions provided by the embodiments of the present disclosure are as follows:
[0008] In a first aspect, an embodiment of the present disclosure provides a method for cleaning an epitaxial device, comprising the following steps:
[0009] The first step is to preliminarily purge the reaction chamber of the epitaxial equipment;
[0010] The second step is to preliminarily heat up the reaction chamber of the epitaxial device;
[0011] The third step is to perform a repeatable cleaning step on the reaction chamber, wherein the repeatable cleaning step comprises:
[0012] The first sub-step is to purge the reaction chamber;
[0013] The second sub-step is to increase the temperature of the reaction chamber;
[0014] The third sub-step is to perform hydrogen baking on the reaction chamber;
[0015] The fourth sub-step is to deliver etching gas into the reaction chamber to etch pollutants on the surface of the reaction chamber and the surfaces of internal components;
[0016] The fifth sub-step is to purge the reaction chamber to discharge the etching products and residual etching gas;
[0017] The sixth sub-step is to cool the reaction chamber;
[0018] Step 4: Cooling down the reaction chamber so that the chamber temperature of the reaction chamber is cooled down to the process temperature during epitaxial growth;
[0019] Step 5: placing a blank test silicon wafer in the reaction chamber to grow a film to obtain a test epitaxial wafer;
[0020] The sixth step is to detect the surface particles of the test epitaxial wafer to determine whether the cleaning index of the reaction chamber meets the preset cleaning index; and if the cleaning index of the reaction chamber does not meet the preset cleaning index, the third step, the fourth step, the fifth step and the sixth step are performed again until the cleaning index meets the preset cleaning index.
[0021] Exemplarily, in the fourth sub-step, before the etching gas is delivered into the reaction chamber, the height of the susceptor in the reaction chamber is lowered from a first height to a second height, so that the etching gas is delivered into the reaction chamber and can at least etch the upper dome, the lower dome and the back side of the susceptor of the reaction chamber;
[0022] In the fifth step, when the blank test silicon wafer is placed in the reaction chamber to grow a film, the susceptor carrying the blank test silicon wafer is raised from the second height to the first height.
[0023] Exemplarily, in the first step, the reaction chamber is purged with nitrogen for 2 to 4 hours at a nitrogen flow rate of 25 to 30 L / min.
[0024] Exemplarily, in the second step, the chamber temperature of the reaction chamber after the initial heating is 1180° C., and the heating rate is 3° C. / S.
[0025] Exemplarily, in the second sub-step, after the reaction chamber is heated up, the chamber temperature is 1160-1180° C., and the heating rate is 3° C. / S.
[0026] Exemplarily, in the fourth sub-step, while the chamber temperature of the reaction chamber is maintained at 1160-1180° C., the reaction chamber is purged by introducing hydrogen into the reaction chamber, and the hydrogen flow rate is 6 slm.
[0027] Exemplarily, in the fourth step, the reaction chamber is controlled to execute an idle procedure, and the idle time is 30 minutes, so that the reaction chamber is cooled down to the process temperature during epitaxial growth.
[0028] Exemplarily, in the fifth step, the number of the blank test silicon wafers used for growing the film is 15.
[0029] Exemplarily, when the exhaust gas treatment device of the epitaxial equipment is in a shutdown state, the first step, the second step, the third step, the fourth step, the fifth step, and the sixth step are performed to clean the epitaxial equipment.
[0030] In the second aspect, the embodiments of the present disclosure further provide an epitaxial wafer, which is formed by epitaxial growth on a silicon wafer using an epitaxial device, and the epitaxial device is cleaned during the epitaxial growth process using the method described above, and the surface particle detection result of the epitaxial wafer is an LLS@200nm average value of less than 0.4ea.
[0031] In a third aspect, an embodiment of the present disclosure further provides a computer-readable storage medium, wherein the computer-readable storage medium stores at least one instruction, and the at least one instruction is used to be executed by a processor to implement the epitaxial device cleaning method provided by the embodiment of the present disclosure.
[0032] The beneficial effects brought by the embodiments of the present disclosure are as follows:
[0033] In the above scheme, when cleaning the reaction chamber of the epitaxial equipment, the reaction chamber is first preliminarily purged to remove particles on the chamber surface and pipelines, and then the reaction chamber is heated up before a repeatable cleaning step is performed. When performing the repeatable cleaning step, the reaction chamber is first purged and heated up again, and after the chamber is heated up, an etching gas is delivered into the chamber to etch the chamber surface and the surface of the chamber internal components to remove pollutants on the chamber surface and the surface of the chamber internal components, and then the etching products and residual etching gas are discharged out of the reaction chamber by another purge. After performing the above repeatable cleaning step, the reaction chamber is cooled down again, and the surface particle detection result obtained by detecting the blank test silicon wafer after film growth is used to verify whether the current cleaning index of the reaction chamber meets the preset cleaning index. When the cleaning index of the reaction chamber does not meet the preset cleaning index, the above repeatable cleaning step is performed again until the cleaning index meets the preset cleaning index. In this way, the reaction chamber of the epitaxial equipment can be effectively cleaned to discharge the impurity byproducts generated by the epitaxial reaction out of the reaction chamber in time, thereby improving the environment of the reaction chamber, reducing the phenomenon of particle deposition on the surface of the epitaxial wafer, and improving product quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 A schematic diagram showing a structure of a reaction chamber of an epitaxial device;
[0035] Figure 2 A schematic diagram showing a structure of an epitaxial device;
[0036] Figure 3 A flow chart showing a method for cleaning an epitaxial device provided by an embodiment of the present disclosure;
[0037] Figure 4 A flow chart showing repeatable cleaning steps in the epitaxial device cleaning method provided in an embodiment of the present disclosure. DETAILED DESCRIPTION
[0038] In order to make the purpose, technical solution and advantages of the embodiments of the present disclosure clearer, the technical solution of the embodiments of the present disclosure will be clearly and completely described below in conjunction with the drawings of the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the described embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.
[0039] Unless otherwise defined, the technical terms or scientific terms used in the present disclosure should be understood by people with ordinary skills in the field to which the present disclosure belongs. The "first", "second" and similar words used in the present disclosure do not indicate any order, quantity or importance, but are only used to distinguish different components. Similarly, similar words such as "one", "one" or "the" do not indicate quantity restrictions, but indicate that there is at least one. Similar words such as "include" or "comprise" mean that the elements or objects appearing before the word cover the elements or objects listed after the word and their equivalents, without excluding other elements or objects. Similar words such as "connect" or "connected" are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.
[0040] like Figure 1 As shown, the epitaxial device may include a reaction chamber, internal components disposed inside the reaction chamber, and a heating assembly disposed outside the reaction chamber, etc. The reaction chamber may include an upper quartz bell jar 110, a lower quartz bell jar 120, an air inlet 130, and an exhaust port 140. The internal components may include a pedestal 210, a pedestal support rod 220, and a wafer support rod 230, etc., wherein the pedestal 210 is used to place the silicon wafer 10. The heating assembly includes an upper lamp group 310 disposed above the pedestal 210 and a lower lamp group 320 disposed below the pedestal 210.
[0041] When epitaxial growth is performed, a silicon wafer is transported into the reaction chamber and placed on the pedestal 210, and the upper lamp group 310 and the lower lamp group 320 heat the silicon wafer. In addition, a raw material gas is supplied to the main surface of the silicon wafer, thereby performing vapor phase growth. After the vapor phase growth, the epitaxial wafer obtained by the vapor phase growth is output to the outside of the reaction chamber. During the growth process, the pedestal support rod 220 plays the role of fixing the pedestal 210 and driving the pedestal 210 to rotate, so that the epitaxial growth can be performed uniformly on the substrate.
[0042] Figure 2 The figure shows the structure of the epitaxial equipment. The transfer blade in the front-end module B transfers the silicon wafer from the loading port A to the load lock unit C, which is evacuated and backfilled with nitrogen. The transfer robot in the transfer unit D transfers the silicon wafer in the load lock unit C to the reaction chamber E through the transfer unit D for epitaxial growth. After the growth is completed, the silicon wafer returns along the original route.
[0043] The gas enters the reaction chamber through the gas mixing system or bubbler, and the following reactions occur:
[0044] SiHCl 3 +H 2 →Si↓+3HCl↑
[0045] In the semiconductor epitaxial process production, many dangerous byproducts are generated during the epitaxy (EPI) process, and these byproducts will spread throughout the process chamber and the back-end pipeline.
[0046] The epitaxial process requires a large amount of HCl (hydrogen chloride) and SiHCl 3 (Silicon Hydrochloride), B 2 H 6 (dihydride diboride), H 2 (hydrogen) and other special gases, including HCl, SiHCl 3 , B 2 H 6 These gases are all highly toxic and will affect the personal and environmental safety around the plant, so the gases in the epitaxial equipment need to be handled safely to avoid accidents.
[0047] Generally, the reaction exhaust gas of the epitaxial equipment is processed by the scrubber and finally discharged into the air. However, when the scrubber of the epitaxial equipment fails, the impurity byproducts generated by the reaction in the epitaxial furnace chamber cannot be discharged out of the chamber in time, and will return to the reaction chamber from the exhaust pipe of the reaction chamber, causing the chamber environment to deteriorate, resulting in particle deposition on the surface of the epitaxial wafer (EPI Wafer), which seriously affects the product quality.
[0048] In order to improve particle contamination on the surface of an epitaxial wafer during epitaxial growth, the embodiments of the present disclosure provide an epitaxial equipment cleaning method, an epitaxial wafer, and a computer-readable medium.
[0049] like Figure 3 and Figure 4 As shown, the epitaxial device cleaning method provided by the embodiment of the present disclosure includes the following steps:
[0050] The first step S01, preliminarily purging the reaction chamber of the epitaxial device;
[0051] The second step S02, preliminarily heating the reaction chamber of the epitaxial device;
[0052] The third step S03 is to perform a repeatable cleaning step (clean recipe) on the reaction chamber, wherein the repeatable cleaning step comprises:
[0053] The first sub-step S031 is to purge the reaction chamber;
[0054] Second sub-step S032, heating the reaction chamber;
[0055] The third sub-step S033 is to perform hydrogen baking on the reaction chamber;
[0056] Fourth sub-step S034, delivering etching gas into the reaction chamber to etch pollutants on the surface of the reaction chamber and the surfaces of internal components;
[0057] The fifth sub-step S035 is to purge the reaction chamber to discharge the etching products and residual etching gas;
[0058] The sixth sub-step S036 is to cool the reaction chamber;
[0059] The fourth step S04, cooling the reaction chamber to reduce the chamber temperature of the reaction chamber to the process temperature during epitaxial growth;
[0060] The fifth step S05, placing a blank test silicon wafer in the reaction chamber to grow a film to obtain a test epitaxial wafer;
[0061] The sixth step S06 is to detect the surface particles of the test epitaxial wafer to determine whether the cleaning index of the reaction chamber meets the preset cleaning index; and if the cleaning index of the reaction chamber does not meet the preset cleaning index, the third step S03, the fourth step S04, the fifth step S05 and the sixth step S06 are executed again until the cleaning index meets the preset cleaning index.
[0062] In the above scheme, when cleaning the reaction chamber of the epitaxial equipment, first, the reaction chamber is preliminarily purged to remove particles on the surface of the reaction chamber and on the pipeline;
[0063] Then, after the reaction chamber is heated, a repeatable cleaning step is performed. When the repeatable cleaning step is performed, the reaction chamber is purged and heated again, and an etching gas is delivered into the chamber after the chamber is heated to etch the chamber surface and the surface of the chamber internal components to remove pollutants on the chamber surface and the surface of the chamber internal components, and then the etching products and residual etching gas are discharged out of the reaction chamber by purging again with a large flow rate;
[0064] After executing the above-mentioned repeatable cleaning steps, the reaction chamber is cooled again, and the surface particle detection results obtained after the blank test silicon wafer film growth are used to verify whether the current cleaning index of the reaction chamber meets the preset cleaning index, and when the cleaning index of the reaction chamber does not meet the preset cleaning index, the above-mentioned repeatable cleaning steps are executed again until the cleaning index meets the preset cleaning index.
[0065] In this way, the reaction chamber of the epitaxial equipment can be effectively cleaned to discharge the impurity byproducts generated by the epitaxial reaction out of the reaction chamber in time, thereby improving the environment of the reaction chamber, reducing the phenomenon of particle deposition on the surface of the epitaxial wafer, and improving product quality.
[0066] In some exemplary embodiments, the epitaxial equipment cleaning method provided in the embodiments of the present disclosure may be to perform the first step S01, the second step S02, the third step S03, the fourth step S04, the fifth step S05, and the sixth step S06 to clean the epitaxial equipment when the tail gas treatment device of the epitaxial equipment is in a shutdown state. In this way, after the tail gas treatment device is shut down, the reaction chamber of the epitaxial equipment may be cleaned to discharge the impurity byproducts generated by the reaction out of the chamber in time, improve the chamber environment, reduce the particle deposition on the surface of the epitaxial wafer, and improve the product quality.
[0067] It should be noted that the epitaxial equipment cleaning method provided in the embodiments of the present disclosure is not limited to being applied after the tail gas treatment device is shut down, but can also be applied to other scenarios where the reaction chamber of the epitaxial equipment needs to be cleaned.
[0068] In some exemplary embodiments, in the first step S01, the reaction chamber is purged with nitrogen, and the purging time is 2 to 4 hours, and the nitrogen flow rate is 25-30 L / min. For example, nitrogen is used for preliminary purging, the purging time is 3 hours, and the nitrogen flow rate is 25-30 L / min. In this way, the surface particle impurities of the reaction chamber and internal components can be removed by purging with a large flow of nitrogen.
[0069] In some exemplary embodiments, in the second step S02, the chamber temperature of the reaction chamber after the initial heating is 1180°C, and the heating rate is 3°C / S.
[0070] In some exemplary embodiments, in the first sub-step, hydrogen (H 2 ) The reaction chamber is purged, specifically, the flow rate of hydrogen can be 6slm.
[0071] In some exemplary embodiments, in the second sub-step S032, after the reaction chamber is heated up, the chamber temperature may be 1160-1180°C, for example, 1180°C, and the heating rate may be 3°C / S.
[0072] In some exemplary embodiments, in the third sub-step S033, baking can be performed using hydrogen at a chamber temperature of 1160-1180° C. Specifically, the flow rate of hydrogen can be 6 slm. At the same time, some etching gas, such as HCL, can also be introduced in this step, and the flow rate of HCL can be 3 slm.
[0073] In some exemplary embodiments, in the fourth sub-step S034, the reaction chamber is etched by introducing HCL into the reaction chamber while the chamber temperature of the reaction chamber is maintained at 1160-1180° C. The etching gas may be, for example, HCL, and the flow rate of HCL may be 6 slm. In addition, in this step, hydrogen may also be introduced at the same time, and the flow rate of hydrogen may be 3 slm.
[0074] In some exemplary embodiments, in the fourth sub-step S034, before the etching gas is delivered into the reaction chamber, the height of the susceptor 210 in the reaction chamber is lowered from a first height to a second height, so that the etching gas is delivered into the reaction chamber and can at least etch the upper dome, the lower dome and the back side of the susceptor 210 of the reaction chamber.
[0075] By adopting the above scheme, the etching gas is delivered to the reaction chamber to etch the quartz bell jar to be cleaned. Specifically, the etching gas can be HCl (hydrogen chloride), and the flow rate of HCl can be 3slm.
[0076] In this embodiment, by lowering the height of the susceptor 210 , the flow path of the etching gas is changed to control the etching gas to not only etch the deposits on the upper dome surface of the reaction chamber to be cleaned, but also etch the deposits on the lower dome and the back side of the susceptor 210 .
[0077] Wherein, the first height and the second height can be silicon wafer exchange positions, and the silicon wafer exchange position refers to the position exchange of silicon wafers in the semiconductor manufacturing process. In a semiconductor factory, silicon wafers need to be exchanged at different positions when passing through different processes. This position exchange can be completed by an automated system or a robot to ensure the accurate transfer and processing of silicon wafers between different processes. In this embodiment, when the silicon wafer is epitaxially grown, the silicon wafer is transported into the reaction chamber and placed on the base 210, and then the base 210 is raised, and the base 210 carries the silicon wafer for epitaxial growth.
[0078] The second height may be the height of the susceptor 210 when the silicon wafer is transported to the reaction chamber via a transport device such as a transport blade and loaded onto the susceptor 210; the first height may be the position of the susceptor 210 when the silicon wafer is epitaxially grown in the reaction chamber.
[0079] In some exemplary embodiments, in the fifth step S05, when the blank test silicon wafer is placed in the reaction chamber for film growth, the susceptor 210 carrying the blank test silicon wafer is raised from the second height to the first height, that is, the height of the susceptor 210 is raised and restored to the height for epitaxial growth. In this way, the height adjustment of the susceptor 210 can be completed by relying on the existing lifting mechanism of the susceptor 210.
[0080] It is understandable that the height adjustment method of the susceptor 210 is not limited thereto, as long as the height of the susceptor 210 can be adjusted to change the flow path of the etching gas to etch the deposits on the lower dome and the back of the susceptor 210 .
[0081] In some exemplary embodiments, in the fifth sub-step S035, the reaction chamber may be purged with hydrogen at a chamber temperature of 1150°C, and the flow rate of hydrogen may be 8 slm. In this way, the etched product may be purged with a large flow of H2 and discharged out of the reaction chamber; the impurities and residual HCL gas after corrosion may be discharged through the exhaust port 140 by introducing H2.
[0082] In some exemplary embodiments, in the sixth sub-step S036, when cooling the reaction chamber, the cooling rate may be 9°C / s, the cooling time may be 30s-35s, and the chamber temperature after cooling may be 850°C.
[0083] In some exemplary embodiments, in the fourth step S04, the reaction chamber is controlled to execute an idle program, which means that the epitaxial equipment is in an idle state, that is, the equipment is not performing any task or work; wherein the idle time is 30 minutes, so that the reaction chamber can be cooled down to the process temperature during epitaxial growth.
[0084] In some exemplary embodiments, in the fifth step S05, the number of the blank test silicon wafers used for growing the film is 15 pcs. However, the number of the blank test silicon wafers is not limited thereto.
[0085] In addition, in the above-mentioned fifth step S05, specifically, if the LLS@200nm average value of the particle inspection result of the blank test silicon wafer is less than 0.4ea, it means that the chamber cleaning index meets the standard and the equipment can resume normal production; if the LLS@200nm average value is greater than or equal to 0.4ea, the reaction chamber is cleaned again by executing a repeatable cleaning step (clean recipe).
[0086] LLS@200nm means: LLS refers to "Light Line Scatter", which means light scattering. In the particle results of the test silicon wafer, the mean value of LLS@200nm is less than 0.4ea, which means that within the size range of 200 nanometers, the average value of light scattering is less than 0.4 units. In other words, the average value of light scattering is less than 0.4 units, which is the preset cleaning index (quality control standard) used to evaluate the particle level on the surface of the silicon wafer. It is understandable that the preset cleaning index is not limited to this.
[0087] The epitaxial equipment cleaning method provided in the embodiment of the present disclosure can improve the product quality by improving the cleaning process. In the size range of 200nm, the average value of light scattering is reduced from 0.48 particles before the improvement to 0.16 particles.
[0088] Based on the above, in the second aspect of the present disclosure, an epitaxial wafer is further provided. The epitaxial wafer is formed by epitaxial growth on a silicon wafer using an epitaxial device, and the epitaxial device is cleaned during the epitaxial growth process using the method provided in an embodiment of the present disclosure. The surface particle detection result of the epitaxial wafer is that the LLS@200nm average is less than 0.4ea.
[0089] In addition, in a third aspect, an embodiment of the present disclosure further provides a computer-readable medium, wherein the computer-readable storage medium stores at least one instruction, and the at least one instruction is used to be executed by a processor to implement the epitaxial device cleaning method provided by an embodiment of the present disclosure.
[0090] An embodiment of the present application further provides a computer-readable storage medium storing at least one instruction, wherein the at least one instruction is used to be executed by a processor to implement the epitaxial device cleaning method described in the above embodiments.
[0091] An embodiment of the present application also provides a computer program product, which includes computer instructions, which are stored in a computer-readable storage medium; a processor of a computing device reads the computer instructions from the computer-readable storage medium, and the processor executes the computer instructions, so that the computing device executes to implement the epitaxial device cleaning method described in the above-mentioned embodiments.
[0092] Those skilled in the art should be aware that in one or more of the above examples, the functions described in the embodiments of the present application can be implemented with hardware, software, firmware, or any combination thereof. When implemented using software, these functions can be stored in a computer-readable medium or transmitted as one or more instructions or codes on a computer-readable medium. Computer-readable media include computer storage media and communication media, wherein the communication media include any media that facilitates the transmission of a computer program from one place to another. The storage medium can be any available medium that a general or special-purpose computer can access.
[0093] There are a few points to note:
[0094] (1) The drawings of the embodiments of the present disclosure only relate to the structures related to the embodiments of the present disclosure, and other structures may refer to the general design.
[0095] (2) For the sake of clarity, in the drawings used to describe the embodiments of the present disclosure, the thickness of layers or regions is exaggerated or reduced, that is, these drawings are not drawn according to the actual scale. It is understood that when an element such as a layer, film, region or substrate is referred to as being "on" or "under" another element, the element may be "directly" "on" or "under" the other element or there may be intermediate elements.
[0096] (3) In the absence of conflict, the embodiments of the present disclosure and the features therein may be combined with each other to obtain new embodiments.
[0097] The above are only specific implementations of the present disclosure, but the protection scope of the present disclosure is not limited thereto, and the protection scope of the present disclosure shall be based on the protection scope of the claims.
Claims
1. A method for cleaning epitaxial equipment, characterized in that: The steps include: The first step is to preliminarily purge the reaction chamber of the epitaxial equipment; The second step is to preliminarily heat up the reaction chamber of the epitaxial device; The third step is to perform a repeatable cleaning step on the reaction chamber, wherein the repeatable cleaning step comprises: The first sub-step is to purge the reaction chamber; The second sub-step is to increase the temperature of the reaction chamber; The third sub-step is to perform hydrogen baking on the reaction chamber; The fourth sub-step is to deliver etching gas into the reaction chamber to etch pollutants on the surface of the reaction chamber and the surfaces of internal components; The fifth sub-step is to purge the reaction chamber to discharge the etching products and residual etching gas; The sixth sub-step is to cool the reaction chamber; Step 4: Cooling down the reaction chamber so that the chamber temperature of the reaction chamber is cooled down to the process temperature during epitaxial growth; Step 5: placing a blank test silicon wafer in the reaction chamber to grow a film to obtain a test epitaxial wafer; The sixth step is to detect the surface particles of the test epitaxial wafer to determine whether the cleaning index of the reaction chamber meets the preset cleaning index; and if the cleaning index of the reaction chamber does not meet the preset cleaning index, the third step, the fourth step, the fifth step and the sixth step are performed again until the cleaning index meets the preset cleaning index.
2. The epitaxial equipment cleaning method according to claim 1, characterized in that: In the fourth sub-step, before the etching gas is delivered into the reaction chamber, the height of the susceptor in the reaction chamber is lowered from a first height to a second height, so that the etching gas is delivered into the reaction chamber and can at least etch the upper dome, the lower dome and the back side of the susceptor of the reaction chamber; In the fifth step, when the blank test silicon wafer is placed in the reaction chamber to grow a film, the susceptor carrying the blank test silicon wafer is raised from the second height to the first height.
3. The epitaxial equipment cleaning method according to claim 1, characterized in that: In the first step, the reaction chamber is purged with nitrogen for 2 to 4 hours at a nitrogen flow rate of 25 to 30 L / min.
4. The epitaxial equipment cleaning method according to claim 1, characterized in that: In the second step, the chamber temperature of the reaction chamber after the initial heating is 1180° C., and the heating rate is 3° C. / S.
5. The epitaxial equipment cleaning method according to claim 1, characterized in that: In the second sub-step, after the reaction chamber is heated up, the chamber temperature is 1160-1180° C., and the heating rate is 3° C. / S.
6. The epitaxial equipment cleaning method according to claim 1, characterized in that: In the third sub-step, the reaction chamber is baked by introducing hydrogen into the reaction chamber while the chamber temperature of the reaction chamber is maintained at 1160-1180° C., and the hydrogen flow rate is 6 slm.
7. The epitaxial equipment cleaning method according to claim 1, characterized in that: In the fourth step, the reaction chamber is controlled to perform an idle procedure with an idle time of 30 minutes so as to cool the reaction chamber to a process temperature for epitaxial growth.
8. The epitaxial equipment cleaning method according to claim 1, characterized in that: In the fifth step, the number of the blank test silicon wafers used for film growth is 15.
9. The epitaxial equipment cleaning method according to claim 1, characterized in that: When the tail gas treatment device of the epitaxial equipment is in a shutdown state, the first step, the second step, the third step, the fourth step, the fifth step, and the sixth step are performed to clean the epitaxial equipment.
10. An epitaxial wafer, characterized in that: The epitaxial wafer is formed by epitaxial growth on a silicon wafer using an epitaxial device, and during the epitaxial growth process, the epitaxial device is cleaned using the method described in any one of claims 1 to 9, and the surface particle detection result of the epitaxial wafer is that the LLS@200nm average is less than 0.4ea.
11. A computer readable medium, characterized in that The computer-readable storage medium stores at least one instruction, and the at least one instruction is used to be executed by a processor to implement the epitaxial equipment cleaning method according to any one of claims 1 to 9.
Citation Information
Patent Citations
Epitaxial growth method for silicon wafer
CN115928205A
Epitaxial growth equipment and temperature control method thereof
CN117265653A
Method for recovering epitaxial reaction furnace
CN117604633A
Method for manufacturing regenerated semiconductor wafer
JP2010283184A
Method and apparatus for manufacturing epitaxial wafer
KR1020180104870A
Cited By
Automatic cleaning device for reaction chamber of epitaxial furnace
CN120362158A