Manufacturing method for combining lens and prefabricated metal solder

By performing metal deposition process and surface protection treatment on the lens and wafer combination, the problem of mismatch between lens and metal solder is solved, the tolerance of high-temperature welding and packaging stability are improved, and the high-density optical module is satisfied. need.

CN118951192APending Publication Date: 2024-11-15XIAMEN YEYING ELECTRONIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411008918.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

In the prior art, there is a mismatch problem between the lens and metal solder, which leads to insufficient temperature resistance and risk of surface damage in a high-temperature eutectic welding environment, and cannot meet the needs of high-density optical module packaging.

Method used

By optimizing the production method of prefabricated metal lenses, including performing metal deposition processes on the lens and wafer combination, forming multi-layer metal and urgency films, and applying protective wax to the lens surface, ensuring precise control of each production step, achieving The perfect combination of lenses and metal solder.

Benefits of technology

It improves the reliability and stability of the packaging, enhances the resistance of lens welding at high temperatures, avoids surface damage and lobe risks, and meets the fast bonding needs of high-density optical modules in high temperature environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118951192A_ABST
    Figure CN118951192A_ABST
Patent Text Reader

Abstract

The invention provides a manufacturing method for combining a lens and a prefabricated metal solder, which comprises the following steps of: providing a combination body of the lens and a wafer, the combination body is provided with a lens front surface and a wafer back surface which are opposite to each other, and the wafer back surface is divided into a metal region and a non-metal region; performing protection processing on the front surface of the lens; forming multiple layers of metal in a metal area on the back surface of the wafer through a metal deposition process; removing the protection treatment on the front surface of the lens, and forming an antireflection film on the front surface of the lens; and an antireflection film is formed in the non-metal area on the front face of the lens and the back face of the wafer, so that the metal solder prefabricating and antireflection film sputtering process is completed on the lens, by optimizing the manufacturing method of the metal solder prefabricating and the lens, accurate control over all the manufacturing steps is ensured, perfect combination of the lens and the metal solder is achieved, and the yield of the lens is improved. Therefore, the reliability and the stability of packaging are improved, and rapid bonding of a high-density optical module in a high-temperature eutectic environment is met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of optical communication packaging, and in particular to a manufacturing method for combining a lens with prefabricated metal solder. Background Art

[0003] At present, lenses are widely used in optical module products, especially in BOX and COB packaging. BOX packaging, also known as hermetic packaging, encapsulates electronic components such as lenses and chips in a sealed metal or ceramic box filled with inert gas (such as nitrogen, helium, etc.) to protect these components from the external environment. COB packaging is to install the chip directly on the PCB, and the lens can optimize the propagation path of light and improve the light efficiency.

[0004] The existing technology mainly uses industrial adhesives such as epoxy resin and acrylic resin to connect the lens to the supporting structure through dispensing and curing processes. This method is widely used because of its simple process, low cost and easy large-scale production. However, the adhesive method has problems such as difficult to control the dispensing amount, insufficient reliability, poor environmental stability, low mechanical strength, long curing time and poor chemical stability, which makes it difficult to meet the packaging needs of high-density optical modules.

[0005] To this end, those skilled in the art have tried to replace the adhesive form with metal solder, but the existing lens preparation process is not compatible with metal applications, resulting in the inability to successfully achieve the replacement for the following reasons:

[0006] On the one hand, most lenses are made of silicon, of which the transmittance of silicon in the infrared band is only 60%, while the transmittance required in the infrared communication band must be greater than 99.7%. The commonly used method is to alternately deposit multiple materials as anti-reflection films, but the temperature resistance of this type of anti-reflection film is only 200°C, which cannot withstand the eutectic welding temperature of metal solder at 320-350°C, thus causing the anti-reflection film to fail.

[0007] On the other hand, silicon lenses used in infrared communication bands have strict control over the surface shape after preparation. During the subsequent semiconductor process of metal solder, the machine needs to grab and adsorb the surface of the silicon lens. Since the prepared silicon lens has a ball height of 20 to 100 μm, it is very easy to be damaged during the grabbing process, and there is a risk of failure to adsorb and cause cracks. It is also not feasible to improve this problem by adjusting the preparation order of the lens and gold tin, because when the metal is prepared first and then the lens, the sheet source will warp because there is already metal on one side, which will cause abnormal lens preparation. Summary of the invention

[0008] The purpose of the present invention is to address the deficiencies in the prior art and provide a method for combining a lens and a prefabricated metal solder. By optimizing the method for manufacturing the prefabricated metal lens, precise control of each manufacturing step is ensured to achieve a perfect combination of the lens and the metal solder, thereby improving the reliability and stability of the package and meeting the requirements for rapid bonding of high-density optical modules in a high-temperature eutectic environment.

[0009] In order to achieve the above object, the present invention provides the following technical solutions:

[0010] A method for combining a lens and a prefabricated metal solder comprises the following steps:

[0011] a. providing a combination of a lens and a wafer, wherein the combination has a front side of the lens and a back side of the wafer facing each other, and the back side of the wafer is divided into a metal area and a non-metal area;

[0012] b. Performing protective treatment on the front side of the lens;

[0013] c. forming a multilayer metal on the metal area on the back side of the wafer by a metal deposition process;

[0014] d. forming an anti-reflection film on the non-metallic area on the back side of the wafer;

[0015] e. removing the protective treatment on the front side of the lens and forming an antireflection film on the front side of the lens;

[0016] The metal deposition process comprises:

[0017] c2. exposing and developing the photoresist coating on the back of the wafer to expose the metal area on the back of the wafer;

[0018] c3, forming a metal layer on the back side of the wafer, wherein the metal layer is located on the surface of the photoresist coating layer and the metal area on the back side of the wafer;

[0019] c4. Remove the metal layer and the photoresist coating in the non-metallic area on the back side of the wafer, and reserve metal in the metal area on the back side of the wafer.

[0020] As a preferred embodiment, the multi-layer metal includes an inner metal layer, and before the step c2, the metal deposition process further includes the following steps:

[0021] The back side of the wafer is cleaned, and a photoresist coating is applied on the back side of the wafer.

[0022] As a preferred embodiment, the inner metal layer includes an adhesion layer and a barrier layer, and the step c3 includes the following steps:

[0023] An adhesion layer and a barrier layer are plated on the surface of the photoresist coating layer and the metal area on the back side of the wafer by sputtering, wherein the adhesion layer is made of metal titanium material and the barrier layer is made of metal platinum material.

[0024] As a preferred embodiment, the multi-layer metal includes an outer metal layer, and before step c2, the metal deposition process further includes the following steps:

[0025] A photoresist coating required for molding the outer metal layer is coated on the side of the inner metal layer away from the assembly.

[0026] As a preferred embodiment, the outer metal layer is made of gold-tin alloy material, and step c3 includes the following steps:

[0027] Gold-tin alloy is plated on the surface of the photoresist coating layer and the surface of the inner metal layer by evaporation.

[0028] As a preferred embodiment, the step c4 comprises the following steps:

[0029] The metal layer and photoresist coating in the non-metal area are removed by a lift-off process.

[0030] As a preferred embodiment, the step a comprises the following steps:

[0031] a1. Providing a wafer, wherein the front side of the wafer has a lens forming area;

[0032] a2, coating photoresist on the front side of the wafer;

[0033] a3, exposing and developing the photoresist on the front side of the wafer to retain the photoresist in the lens forming area;

[0034] a4. By baking, the photoresist in the lens forming area is formed into a lens with a spherical structure to obtain the assembly.

[0035] As a preferred embodiment, the step b comprises the following steps:

[0036] The front side of the lens is protected by coating wax, applying film, or bonding.

[0037] As a preferred embodiment, the step d comprises the following steps:

[0038] d1. Coating a photoresist required for forming an anti-reflection film on the back side of the wafer;

[0039] d2, exposing and developing the photoresist coated on the back side of the wafer to expose the non-metallic area on the back side of the wafer;

[0040] d3, coating an anti-reflection film on the back of the wafer by evaporation, wherein the anti-reflection film is located on the surface of the photoresist and on the non-metallic area on the back of the wafer;

[0041] d4. Remove the photoresist in the metal area on the back side of the wafer to retain the anti-reflection film in the non-metal area on the back side of the wafer.

[0042] As a preferred embodiment, the antireflection film is made of high temperature resistant material.

[0043] Compared with the prior art, this technical solution has the following advantages:

[0044] Traditional anti-reflection film materials will fail at 200°C and cannot meet the 320-350°C eutectic soldering temperature required by gold-tin solder. Through improved material selection and coating process, the stability of the anti-reflection film at 350°C is achieved, which greatly improves the tolerance of the lens during high-temperature soldering and ensures the optical performance after soldering;

[0045] The wax coating and bonding protection method is adopted to effectively solve the damage and cracking risks caused by the spherical height of the lens surface in the existing technology. By coating the protective wax on the lens surface and maintaining the integrity of the surface in the subsequent process, the high-quality surface shape is maintained.

[0046] The present invention is further described below with reference to the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0047] Figure 1 A flow chart of a method for combining a lens and a prefabricated metal solder according to the present invention;

[0048] Figure 2 A flow chart of the metal deposition process of the present invention;

[0049] Figure 3 It is a schematic diagram of the structure of the prefabricated metal for the lens of the present invention.

[0050] In the figure: 100 assembly, 100a front side of lens, 100b back side of wafer, 100b1 metal area, 100b2 non-metal area, 110 lens, 120 wafer, 200 metal, 300 anti-reflection film. DETAILED DESCRIPTION

[0051] The following description is used to disclose the present invention so that those skilled in the art can implement the present invention. The preferred embodiments described below are only examples, and those skilled in the art can think of other obvious variations. The basic principles of the present invention defined in the following description can be applied to other embodiments, variations, improvements, equivalents, and other technical solutions that do not deviate from the spirit and scope of the present invention.

[0052] like Figure 1 and Figure 3 As shown, the method for manufacturing the lens and the prefabricated metal solder comprises the following steps:

[0053] a. Provide a combination 100 of a lens 110 and a wafer 120, wherein the combination 100 has a lens front side 100a and a wafer back side 100b opposite to each other, wherein the wafer back side 100b is divided into a metal region 100b1 and a non-metal region 100b2.

[0054] refer to Figure 3 , the lens 110 and the wafer 120 are arranged from top to bottom, the front side 110a of the lens corresponds to the spherical surface of the lens, and the back side 100b of the wafer is a horizontal plane, on which the multilayer metal 200 is formed. The lens 110 is an optical element made of a transparent material (such as glass, crystal, etc.), which performs optical effects such as converging or diverging light, and the wafer 120 refers to a silicon wafer used for manufacturing silicon semiconductor integrated circuits, and its original material is silicon.

[0055] The step a comprises the following steps:

[0056] a1. providing a wafer 120, wherein the front side of the wafer 120 has a lens forming area;

[0057] a2. Coating photoresist on the front side of the wafer 120;

[0058] a3, exposing and developing the photoresist on the front side of the wafer 120 to retain the photoresist in the lens forming area;

[0059] a4. By baking, the photoresist in the lens forming area forms a lens 110 with a spherical structure, so as to obtain the assembly 100.

[0060] In step a1, it is necessary to clean and remove impurities, contaminants and oxides on the surface of the wafer 120 to ensure a clean surface of the wafer 120 and ensure the optical performance during the lens manufacturing process. Taking the oxide removal as an example, chemical cleaning or plasma cleaning methods can be used to remove the surface oxides.

[0061] In the step a2, a layer of photoresist with a thickness of 15 to 45 microns is coated on the front side of the wafer 120 .

[0062] In step a3, a photoresist is exposed and developed to form a photolithographic pattern. The exposure principle of the photoresist is to control the intensity, wavelength and exposure time of light so that the light can pass through the transparent area on the mask and enter the photoresist. While absorbing light energy, the photosensitizer of the photoresist undergoes a physical or chemical reaction, resulting in the breakage of the organic chain or structural change, that is, the photoresist in the non-lens forming area on the front of the wafer 120 is dissolved, while the photoresist in the lens forming area on the front of the wafer 120 is retained for the forming of the lens 110. After exposure, development is required. Development is performed by treating the photoresist with a chemical solution to make a difference between the photoresist exposed to light and the photoresist not exposed to light. A developer is usually used to achieve this process. The developer can dissolve or remove the area where the chemical reaction occurs in the photoresist, thereby forming the desired photolithographic pattern.

[0063] In step a4, the photoresist is baked to remove moisture, thereby shrinking the photoresist to form a spherical lens 110. The baking temperature is 90 to 150° C., and the baking time is 5 to 30 minutes. After the photoresist shrinks into the lens 110, the pattern is transferred to the front side of the wafer 120 by etching, and the assembly 100 is finally formed.

[0064] Among them, an etcher can be used for etching. During the etching process, an etchant (such as a chemical solution, gas or plasma) removes the portion of the surface not covered by the photoresist, while the photoresist plays a protective role to prevent the surface below from being etched. In this way, a pattern corresponding to the photoresist pattern is formed on the front side of the wafer 120.

[0065] It should be noted that between steps a1 and a2, step a also includes using laser to mark left and right alignment points on the back side 100b of the wafer, so as to accurately position and align the wafer, which is crucial when the wafer requires multiple processing and handling steps, thereby improving processing accuracy.

[0066] b. Performing protective treatment on the front side of the lens.

[0067] The step b includes the following steps: coating a layer of wax on the front surface 110a of the lens to protect the front surface 110a of the lens, effectively solving the risk of damage and fragmentation caused by the spherical height of the lens surface in the prior art. By coating the protective wax on the front surface 110a of the lens and maintaining the integrity of the surface in subsequent processes, a high-quality surface shape is maintained.

[0068] Alternatively, the front side 110a of the lens is protected by film lamination, bonding, etc. The bonding may be laser bonding, where the surface of the material is heated to a melting point by a laser beam, and then the two materials are pressed together to protect the front side 110a of the lens.

[0069] c. Forming a multi-layer metal 200 on the metal region of the back side 100 b of the wafer by a metal deposition process.

[0070] The multi-layer metal 200 is a metal solder. Figure 2 , the metal deposition process comprises:

[0071] c2, exposing and developing the photoresist coating on the back side 100b of the wafer to expose the metal area 100b1 on the back side 100b of the wafer;

[0072] c3, forming a metal layer on the back side 100b of the wafer, wherein the metal layer is located on the surface of the photoresist coating layer and the metal area 100b1 on the back side 100b of the wafer;

[0073] c4. Remove the metal layer and the photoresist coating in the non-metallic area 100b1 on the back side 100b of the wafer, and reserve metal in the metal area 100b1 on the back side 100b of the wafer.

[0074] The multi-layer metal 200 includes an inner metal layer. Before the step c2, the metal deposition process further includes the following steps:

[0075] The back side 100b of the wafer is cleaned and a photoresist coating is applied to the back side 100b of the wafer. The thickness of the photoresist coating on the back side 100b of the wafer is 2 to 5 microns.

[0076] In the step c2, the metal region 100b1 of the wafer back side 100b is exposed to the outside, so as to form an inner metal layer on the metal region 100b1.

[0077] It should be noted that the laser mark on the back side 100b of the wafer needs to be exposed for alignment to ensure accurate positioning and improve processing accuracy.

[0078] The inner metal layer includes an adhesion layer and a barrier layer, and the step c3 includes the following steps:

[0079] Adhesion layer and barrier layer are plated on the surface of the photoresist coating layer and the metal area on the back of the wafer by sputtering, wherein the adhesion layer is made of metal titanium material (Ti, wavelength is ), the barrier layer is made of metal platinum material (Pt40, wavelength ).

[0080] The step c4 comprises the following steps:

[0081] The metal layer and the photoresist coating of the non-metal region 100b2 are removed by a lift-off process.

[0082] The lift-off process refers to immersing the wafer in a solvent, which dissolves the photoresist and strips off the metal covering it, so that only the inner metal layer deposited directly on the metal area 100b1 is left.

[0083] The multi-layer metal 200 further includes an outer metal layer, and before step c2, the metal deposition process further includes the following steps:

[0084] A photoresist coating required for molding the outer metal layer is coated on the side of the inner metal layer away from the assembly, and the thickness of the photoresist coating required for molding the outer metal layer is 6 to 30 microns.

[0085] In the step c2, after exposure and development, the inner metal layer of the metal area 100b1 on the back side 100b of the wafer is exposed.

[0086] It should be noted that after applying the photoresist coating required for molding the outer metal layer, the marks left on the inner metal layer need to be exposed for positioning to ensure accurate positioning and improve processing accuracy.

[0087] The outer metal layer is made of gold-tin alloy material, and step c3 includes the following steps:

[0088] Gold-tin alloy is plated on the surface of the photoresist coating layer and the surface of the inner metal layer by evaporation.

[0089] The thickness of the outer metal layer is 2 to 10 microns.

[0090] d. forming an anti-reflection film 300 on the non-metallic region 100b2 on the back side of the wafer 100b.

[0091] The forming method of the antireflection film 300 may refer to the metal deposition process. Specifically, the step d includes the following steps:

[0092] d1, coating the photoresist required for forming the anti-reflection film on the back side 100b of the wafer;

[0093] d2, exposing and developing the photoresist coated on the back side 100b of the wafer to expose the non-metallic area 100b2 of the back side 100b of the wafer;

[0094] d3, coating the anti-reflection film 300 on the back side 100b of the wafer by evaporation, wherein the anti-reflection film 300 is located on the surface of the photoresist and on the non-metallic area on the back side 100b of the wafer;

[0095] d4. Remove the photoresist in the metal area on the back side 100b of the wafer to retain the anti-reflection film in the non-metal area 100b2 on the back side 100b of the wafer.

[0096] In the step d1, the thickness of the photoresist required for forming the anti-reflection film is 10-15 microns, which can protect the metal in the metal area 100b1.

[0097] In step d2, the marks left on the outer metal layer are exposed to ensure accurate positioning and improve processing accuracy.

[0098] In the step d3, the vapor deposition is performed according to the design based on the actually required wavelength band.

[0099] In the step d4, the photoresist and the metal thereon may be removed by a lift-off process.

[0100] By designing and optimizing the coating process, adjusting the materials used for coating and designing the deposition thickness and number of layers of different materials, it is ensured that there will be no blistering, falling off, etc. at a high temperature of 350°C while meeting the transmittance; the ball height is filled to the full on the surface of the formed lens, and the remaining silicon wafers are bonded to the surface for protection, so that the gold-tin is prepared on the back.

[0101] The anti-reflection film 300 can be made of high-temperature resistant materials such as Mg2F, SiO2, and Si3N4. The heat resistance of the anti-reflection film 300 can ensure that there is no blistering or peeling at 350°C. Through improved material selection and coating process, the stability of the anti-reflection film at a high temperature of 350°C is achieved, which greatly improves the tolerance of the silicon lens during high-temperature welding and ensures the optical performance after welding.

[0102] e. Release the protection treatment on the front side of the lens, and form an anti-reflection film 300 on the front side of the lens to complete the formation of the prefabricated metal solder and the anti-reflection film on the lens 110 .

[0103] Since a layer of wax is applied to the front surface 110a of the lens in step b, step e includes the following steps: cleaning the wax applied to the front surface 110a of the lens so as to form an antireflection film 300 on the front surface 110a of the lens later, referring to Figure 3 .

[0104] The antireflection film 300 formed on the front area of ​​the lens can also be formed by evaporation.

[0105] In summary, the method for making the lens prefabricated metal solves the key problems in the prior art and significantly improves the application performance of the lens in the infrared communication band by innovatively designing the anti-reflection film of the lens and its surface protection. Specifically, through innovative process flow and material selection, the problem of mismatch between the existing silicon lens preparation process and the application of gold-tin solder is solved, the high-temperature stability of the silicon lens in the infrared communication band is significantly improved, and the surface of the silicon lens is effectively protected during the preparation process to avoid damage and cracking risks. These technical effects show that the present invention has obvious advantages and broad application prospects in the application of high-temperature eutectic welding of silicon lenses.

[0106] The embodiments described above are only used to illustrate the technical ideas and features of the present invention, and their purpose is to enable technicians in this field to understand the contents of the present invention and implement them accordingly. The patent scope of the present invention cannot be limited only by this embodiment, that is, any equivalent changes or modifications made according to the spirit disclosed by the present invention still fall within the patent scope of the present invention.

Claims

1. A method for combining a lens and a prefabricated metal solder, characterized in that: The following steps are involved: a. providing a combination of a lens and a wafer, wherein the combination has a front side of the lens and a back side of the wafer facing each other, and the back side of the wafer is divided into a metal area and a non-metal area; b. Performing protective treatment on the front side of the lens; c. forming a multilayer metal on the metal area on the back side of the wafer by a metal deposition process; d. forming an anti-reflection film on the non-metallic area on the back side of the wafer, e. removing the protective treatment on the front side of the lens and forming an antireflection film on the front side of the lens; The metal deposition process comprises: c2. exposing and developing the photoresist coating on the back of the wafer to expose the metal area on the back of the wafer; c3, forming a metal layer on the back side of the wafer, wherein the metal layer is located on the surface of the photoresist coating layer and the metal area on the back side of the wafer; c4. Remove the metal layer and the photoresist coating in the non-metallic area on the back side of the wafer, and reserve metal in the metal area on the back side of the wafer.

2. The method for manufacturing a lens and a prefabricated metal solder combination as claimed in claim 1, characterized in that: The multi-layer metal includes an inner metal layer. Before step c2, the metal deposition process further includes the following steps: The back side of the wafer is cleaned, and a photoresist coating is applied on the back side of the wafer.

3. The method for manufacturing a lens and a prefabricated metal solder combination as claimed in claim 2, characterized in that: The inner metal layer includes an adhesion layer and a barrier layer, and the step c3 includes the following steps: An adhesion layer and a barrier layer are plated on the surface of the photoresist coating layer and the metal area on the back side of the wafer by sputtering, wherein the adhesion layer is made of metal titanium material and the barrier layer is made of metal platinum material.

4. The method for manufacturing a lens and a prefabricated metal solder combination as claimed in claim 2, characterized in that: The multi-layer metal includes an outer metal layer. Before step c2, the metal deposition process further includes the following steps: A photoresist coating required for molding the outer metal layer is coated on the side of the inner metal layer away from the assembly.

5. The method for manufacturing a lens and a prefabricated metal solder combination as claimed in claim 4, characterized in that: The outer metal layer is made of gold-tin alloy material, and step c3 includes the following steps: Gold-tin alloy is plated on the surface of the photoresist coating layer and the surface of the inner metal layer by evaporation.

6. The method for manufacturing a lens and a prefabricated metal solder combination as claimed in claim 1, characterized in that: The step c4 comprises the following steps: The metal layer and photoresist coating in the non-metal area are removed by a lift-off process.

7. The method for manufacturing a lens and a prefabricated metal solder combination as claimed in claim 1, characterized in that: The step a comprises the following steps: a1. Providing a wafer, wherein the front side of the wafer has a lens forming area; a2, coating photoresist on the front side of the wafer; a3, exposing and developing the photoresist on the front side of the wafer to retain the photoresist in the lens forming area; a4. By baking, the photoresist in the lens forming area is formed into a lens with a spherical structure to obtain the assembly.

8. The method for manufacturing a lens and a prefabricated metal according to claim 1, characterized in that: The step b comprises the following steps: The front side of the lens is protected by coating wax, applying film, or bonding.

9. The method for manufacturing a lens and a prefabricated metal solder combination as claimed in claim 1, characterized in that: The step d comprises the following steps: d1, coating the photoresist required for forming the anti-reflection film on the back side of the wafer; d2, exposing and developing the photoresist coated on the back side of the wafer to expose the non-metallic area on the back side of the wafer; d3, coating an anti-reflection film on the back of the wafer by evaporation, wherein the anti-reflection film is located on the surface of the photoresist and on the non-metallic area on the back of the wafer; d4. Remove the photoresist in the metal area on the back side of the wafer to retain the anti-reflection film in the non-metal area on the back side of the wafer.

10. The method for manufacturing a lens and a prefabricated metal solder combination as claimed in claim 1, characterized in that: The antireflection film is made of high temperature resistant material.