Method for cold drawing of air conditioner compressor shell

By simplifying the production process of cold-drawn air-conditioning compressor shell, including shearing, stamping, welding and pickling and phosphating treatment of galvanized steel plates, the problems of complex process and low yield in the existing technology are solved, and high strength and High efficiency production.

CN118951599AInactive Publication Date: 2024-11-15WUXI HUALIN REFRIGERATION EQUIP CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410868728.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-01
Publication Date
2024-11-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The shell process of existing cold-drawn air-conditioning compressors is complex and has low yield, making it difficult to ensure high strength and precise wall thickness control at the same time.

Method used

The galvanized steel plate is used to shear, stamp, welding, grinding, cold-drawing mold pipe expansion, cutting, cleaning, shaping, pickling and phosphating treatment steps to simplify the process and improve the yield rate.

Benefits of technology

The production of cold-drawn air-conditioning compressor shells with high strength, simple process and high yield is achieved, reducing production costs and improving production efficiency.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for cold drawing of an air conditioner compressor shell. The method comprises the following steps that firstly, a galvanized steel plate is selected to be sheared; step 2, stamping the sheared galvanized steel sheet into a sheet metal to obtain a coiled shell; thirdly, the coiled shell is welded and closed to obtain a tubular shell, and a weld joint is polished; 4, the tubular shell is subjected to pipe expanding through a cold-drawing die and a stretching machine; 5, the tubular shell obtained after pipe expanding is cut, and grease, rust and the like are cleaned and removed; sixthly, the cut tubular shell is subjected to flat head chamfering and shaping, and a formed tubular shell is obtained; and seventhly, the formed tubular shell is subjected to acid pickling and phosphating treatment. The invention belongs to the technical field of air conditioner compressor shell production, and relates to a method for cold drawing of an air conditioner compressor shell, which ensures the strength, and is simple in process and high in yield.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of air-conditioning compressor shell production, and specifically refers to a method for cold-drawing an air-conditioning compressor shell. Background Art

[0002] The air-conditioning compressor plays the role of compressing and driving the refrigerant in the air-conditioning refrigerant circuit. Its shell is usually set in a cylindrical structure during production and processing, and is made by shearing, stamping, welding and other processes of metal plates. The strength of cold-drawn tubes is generally about 20%-30% higher than that of hot-rolled tubes, and its rigidity and processability are relatively good. Therefore, the air-conditioning compressor shell made by the cold-drawn production process has a longer service life.

[0003] Existing methods for cold-drawing air-conditioning compressor casings, such as a method for cold-drawing an air-conditioning compressor casing disclosed in application number CN201810116478.9, can make the processed casing have higher strength and can accurately control the wall thickness of the casing. However, the process is complicated and the yield is low. Therefore, we propose a method for making the processed casing have higher strength and can accurately control the wall of the casing to solve the above problems. Summary of the invention

[0004] In view of the above situation, in order to overcome the defects of the prior art, the present invention provides a method for cold drawing an air-conditioning compressor housing, which is a method for cold drawing an air-conditioning compressor housing that ensures strength while having a simple process and a high yield.

[0005] The technical solution adopted by the present invention is as follows: The present invention provides a method for cold drawing an air-conditioning compressor housing, comprising the following steps:

[0006] Step 1: Select galvanized steel plate for shearing;

[0007] Step 2: stamping the galvanized steel sheet after shearing to obtain a rolled shell;

[0008] Step 3: welding the rolled shell to obtain a tubular shell, and grinding the weld;

[0009] Step 4: Expand the tubular shell through a cold drawing die and a stretching machine;

[0010] Step 5: Cut the expanded tubular shell and clean it to remove grease, rust, etc.

[0011] Step 6: Chamfer and shape the cut tubular shell to obtain a formed tubular shell;

[0012] Step 7: The formed tubular shell is pickled and phosphated;

[0013] Furthermore, the thickness of the galvanized steel plate in step one is 3-7 mm, and the coverage width of each side of the weld in step three is 2-4 mm.

[0014] Furthermore, the concentration of the pickling solution in step seven is 15%-35%, and the temperature is controlled at 35-60°C, the pickling time in step seven is 10-15min, and the total acidity and free acidity of the pickling solution are greater than 1:15.

[0015] Furthermore, after the fourth step of tube expansion, the wall thickness of the tubular shell is 2-5 mm, and the compressive strength is greater than 4.5 MPa.

[0016] The beneficial effects achieved by the present invention using the above structure are as follows: This scheme provides a method for cold-drawing an air-conditioning compressor casing, which can ensure strength while simplifying the production process, reduce production costs, and have a high yield rate. In particular, the simple process also indirectly improves production efficiency. DETAILED DESCRIPTION

[0017] The technical solutions in the embodiments of the present invention will be clearly and completely described below in combination with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments; based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0018] Embodiment 1: A method for cold drawing an air-conditioning compressor housing, comprising the following steps:

[0019] Step 1: Select galvanized steel plate for shearing;

[0020] Step 2: stamping the galvanized steel sheet after shearing to obtain a rolled shell;

[0021] Step 3: welding the rolled shell to obtain a tubular shell, and grinding the weld;

[0022] Step 4: Expand the tubular shell through a cold drawing die and a stretching machine;

[0023] Step 5: Cut the expanded tubular shell and clean it to remove grease, rust, etc.

[0024] Step 6: Chamfer and shape the cut tubular shell to obtain a formed tubular shell;

[0025] Step 7: The formed tubular shell is pickled and phosphated;

[0026] The thickness of the galvanized steel plate in step one is 4 mm, and the coverage width of each side of the weld in step three is 2 mm.

[0027] The pickling solution concentration in step seven is 15%, and the temperature is controlled at 40° C. The pickling time in step seven is 10 minutes, and the total acidity and free acidity of the pickling solution are greater than 1:15.

[0028] After the fourth step of tube expansion, the wall thickness of the tubular shell is 2 mm, and the compressive strength is greater than 4.5 MPa.

[0029] Embodiment 2: A method for cold drawing an air-conditioning compressor housing, comprising the following steps:

[0030] Step 1: Select galvanized steel plate for shearing;

[0031] Step 2: stamping the galvanized steel sheet after shearing to obtain a rolled shell;

[0032] Step 3: welding the rolled shell to obtain a tubular shell, and grinding the weld;

[0033] Step 4: Expand the tubular shell through a cold drawing die and a stretching machine;

[0034] Step 5: Cut the expanded tubular shell and clean it to remove grease, rust, etc.

[0035] Step 6: Chamfer and shape the cut tubular shell to obtain a formed tubular shell;

[0036] Step 7: The formed tubular shell is pickled and phosphated;

[0037] The thickness of the galvanized steel plate in step one is 5 mm, and the coverage width of each side of the weld in step three is 3 mm.

[0038] The pickling solution concentration in step seven is 25%, and the temperature is controlled at 50° C. The pickling time in step seven is 12 minutes, and the total acidity and free acidity of the pickling solution are greater than 1:15.

[0039] After the fourth step of tube expansion, the wall thickness of the tubular shell is 3 mm, and the compressive strength is greater than 4.5 MPa.

[0040] Embodiment 3: A method for cold drawing an air-conditioning compressor housing, comprising the following steps:

[0041] Step 1: Select galvanized steel plate for shearing;

[0042] Step 2: stamping the galvanized steel sheet after shearing to obtain a rolled shell;

[0043] Step 3: welding the rolled shell to obtain a tubular shell, and grinding the weld;

[0044] Step 4: Expand the tubular shell through a cold drawing die and a stretching machine;

[0045] Step 5: Cut the expanded tubular shell and clean it to remove grease, rust, etc.

[0046] Step 6: Chamfer and shape the cut tubular shell to obtain a formed tubular shell;

[0047] Step 7: The formed tubular shell is pickled and phosphated;

[0048] The thickness of the galvanized steel plate in step one is 7 mm, and the coverage width of each side of the weld in step three is 4 mm.

[0049] The pickling solution concentration in step seven is 35%, and the temperature is controlled at 60° C. The pickling time in step seven is 15 minutes, and the total acidity and free acidity of the pickling solution are greater than 1:15.

[0050] After the fourth step of tube expansion, the wall thickness of the tubular shell is 5 mm, and the compressive strength is greater than 4.5 MPa.

[0051] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0052] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

[0053] The present invention and its embodiments are described above, and such description is not restrictive. What is shown in the description is only one of the embodiments of the present invention, and the actual structure is not limited thereto. In short, if ordinary technicians in the field are inspired by it, without departing from the purpose of the invention, they can design a structure and embodiment similar to the technical solution without creativity, which should belong to the protection scope of the present invention.

Claims

1. A method for cold drawing an air-conditioning compressor housing, characterized in that: The following steps are involved: Step 1: Select galvanized steel plate for shearing; Step 2: stamping the galvanized steel sheet after shearing to obtain a rolled shell; Step 3: welding the rolled shell to obtain a tubular shell, and grinding the weld; Step 4: Expand the tubular shell through a cold drawing die and a stretching machine; Step 5: Cut the expanded tubular shell and clean it to remove grease, rust, etc. Step 6: Chamfer and shape the cut tubular shell to obtain a formed tubular shell; Step seven: The formed tubular shell is pickled and phosphated.

2. The method for cold drawing an air-conditioning compressor housing according to claim 2, characterized in that: The thickness of the galvanized steel plate in step one is 3-7 mm, and the coverage width of each side of the weld in step three is 2-4 mm.

3. The method for cold drawing an air-conditioning compressor housing according to claim 3, characterized in that: The pickling solution concentration in step seven is 15%-35%, and the temperature is controlled at 35-60°C. The pickling time in step seven is 10-15 minutes, and the total acidity and free acidity of the pickling solution are greater than 1:

15.

4. The method for cold drawing an air-conditioning compressor housing according to claim 4, characterized in that: After the fourth step of tube expansion, the wall thickness of the tubular shell is 2-5 mm, and the compressive strength is greater than 4.5 MPa.

Citation Information

Patent Citations

  • Method for cold drawing of compressor shell of air conditioner

    CN108339863A