Dustproof oxygen-permeable deoxidizer packing material and production process thereof

By using a three-layer structure of breathable skeleton layer, dustproof film and inner membrane in the dustproof and oxygen-permeable deoxidant packaging material, combined with specific material composition and preparation technology, the problem of insufficient strength and leakage-proof performance of the packaging material is solved. It achieves higher tensile and deformation resistance and powder leakage resistance.

CN118952801AActive Publication Date: 2024-11-15NANJING JIEYUAN PACKING CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411232170.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-15
Estimated Expiration
2044-09-04

AI Technical Summary

Technical Problem

The overall strength of existing dust-proof and oxygen-permeable deoxidant packaging materials is low, easy to tear and deform, and insufficient powder leakage resistance.

Method used

Adopt a three-layer structure of breathable skeleton layer, dustproof film and inner membrane. The breathable skeleton layer consists of ultra-thin non-woven fabric, pulp, modified corn starch, cellulose and iron hydroxide to enhance material performance through a specific preparation process. , combined with the adhesion process of dust-proof film and inner film, improve the tensile resistance and powder leakage resistance of the packaging material.

Benefits of technology

It effectively improves the strength, tensile resistance and deformation resistance of the dust-permeable deoxidant packaging material, significantly improves the powder leakage performance, and avoids tear deformation and dust leakage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118952801A_ABST
    Figure CN118952801A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of deoxidizing agents, particularly relates to a dustproof oxygen-permeable deoxidizing agent packing material and a production process thereof, and provides the following scheme aiming at the problems that an existing packing material is low in strength, easy to tear and deform and poor in powder leakage prevention performance. The dustproof oxygen-permeable deoxidizer packing material comprises a breathable framework layer, a dustproof film adhered to the upper surface of the breathable framework layer and an inner film adhered to the lower surface of the breathable framework layer, the breathable skeleton layer is prepared from the following raw materials in parts by mass: 15 to 25 parts of ultrathin non-woven fabric, 70 to 80 parts of paper pulp liquid, 1 to 5 parts of modified corn starch, 1 to 5 parts of organic glass glue, 0.50 to 1.00 parts of cellulose and 0.10 to 0.50 part of ferric hydroxide, so that an effective dustproof and oxygen-permeable function can be achieved, and the material characteristics of the breathable skeleton layer are utilized, so that the air permeability of the breathable skeleton layer is improved; the strength of the dustproof oxygen-permeable deoxidizer packing material can be enhanced, the tensile capacity is improved, the dustproof oxygen-permeable deoxidizer packing material is prevented from being torn and deformed, and the deformation resistance and the powder leakage prevention performance are greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of deoxidizers, and in particular to a dust-proof and oxygen-permeable deoxidizer packaging material and a production process thereof. Background Art

[0002] The Chinese patent document with application number 201911177719.1 discloses a dustproof oxygen-permeable deoxidizer packaging material and its production process, including a polyethylene co-extruded layer, a dustproof paper layer, and a polyester film layer; a glue layer is provided between the polyethylene co-extruded layer and the dustproof paper layer, and between the dustproof paper layer and the polyester film layer; the glue in each glue layer has a gram weight of 3-5g / m2, and the coverage of the glue on both sides of the dustproof paper layer is 50-60% respectively; the polyethylene co-extruded layer and the polyester film layer are provided with air holes. The dustproof oxygen-permeable deoxidizer packaging material has the advantages of good dustproof effect and air permeability effect.

[0003] However, there are also some problems with the dust-proof and oxygen-permeable deoxidizer packaging material and its production process. For example, although the packaging material has good air permeability, in actual use, the overall strength of the packaging material is low, it is prone to tearing and deformation, and the anti-powder leakage performance is difficult to guarantee. Summary of the invention

[0004] Based on the problems that the background technology has low strength, easy tearing and deformation, and poor anti-powder leakage performance, the present invention proposes a dust-proof and oxygen-permeable deoxidizer packaging material and a production process thereof.

[0005] The present invention provides a dust-proof oxygen-permeable deoxidizer packaging material, which comprises a breathable skeleton layer, a dust-proof film bonded to the upper surface of the breathable skeleton layer, and an inner film bonded to the lower surface of the breathable skeleton layer; The raw material composition and content of the breathable skeleton layer include 15 to 25 parts of ultra-thin non-woven fabric, 70 to 80 parts of pulp slurry, 1 to 5 parts of modified corn starch, 1 to 5 parts of plexiglass glue, 0.50 to 1.00 parts of cellulose and 0.10 to 0.50 parts of iron hydroxide by mass. The dust-proof, oxygen-permeable and deoxidizer packaging material of the present application adopts a three-layer structure of a breathable skeleton layer, a dust-proof film and an inner membrane, which can play an effective dust-proof and oxygen-permeable function. In addition, by utilizing the material properties of the breathable skeleton layer, the strength of the dust-proof, oxygen-permeable and deoxidizer packaging material can be enhanced, the tensile resistance can be improved, the dust-proof, oxygen-permeable and deoxidizer packaging material can be prevented from tearing and deformation, and the deformation resistance and powder leakage prevention performance are greatly improved.

[0006] Preferably, the preparation method of the ultra-thin non-woven fabric is as follows: polyvinyl alcohol is melt-purified, and polyvinyl alcohol fibers are made by centrifugal spinning, and then the polyvinyl alcohol fibers are combed into a thin cotton web with uniform thickness by physical opening, and the primary cotton web is rolled vertically and horizontally to make a preliminary rolling shape, and then impregnated with a polyvinyl alcohol aqueous solution adhesive, and rolled for a second time. The drying temperature is 160°C-190°C to obtain a finished ultra-thin non-woven fabric, which can enhance material properties.

[0007] Preferably, the method for preparing the pulp liquid comprises: obtaining plant wood powder, adding methanol to the plant wood powder, dissolving cellulose in the plant wood powder by methanol, and then performing solid-liquid separation to obtain a cellulose dissolution liquid, heating the cellulose dissolution liquid, using heat to evaporate the methanol to obtain a cellulose paste liquid, evaporating the cellulose paste liquid, drying and evaporating the remaining methanol in the cellulose paste liquid, adding water to prepare a fiber pulp, adjusting the water content of the obtained fiber pulp to 50wt%-70wt%, adding excess acetic anhydride to the fiber pulp according to the water content, heating to 50°C-70°C, performing a hydrolysis reaction, adjusting the mass ratio of cellulose, acetic anhydride, and acetic acid to 1:(2-3):(8-12), heating to 80°C-95°C, performing an esterification reaction, and obtaining a pulp liquid, which can increase the performance of the pulp liquid.

[0008] Preferably, the raw material composition and content of the modified corn starch include 95% corn starch, 1% chitosan, 1% metal ions, 2% maltogenic amylase and 1% hexose oxidase by mass, and the metal ions are selected from one of calcium ions, copper ions and magnesium ions, so that the corn starch can be modified.

[0009] Preferably, the preparation method of the modified corn starch comprises: obtaining corn starch, adding 10 times the amount of deionized water to the corn starch, mixing to form a starch emulsion, adding metal ions to the starch emulsion, subjecting the starch emulsion after adding the metal ions to a pulse electric field treatment, wherein the pulse field strength is 10KV / cm to 30KV / cm, the pulse width is 20μs to 40μs, and the pulse treatment time is 10ms. After the pulse electric field treatment, chitosan and maltose amylase are added to perform enzymolysis to deactivate the enzyme activity, and then hexose oxidase is added to perform a lactonization reaction on the oligoglucans in the starch emulsion to deactivate the enzyme activity, and the modified corn starch is obtained after air flow drying, thereby ensuring the modification effect.

[0010] Preferably, the inner film is a CPP film with a thickness of 20um to 25um, which can isolate the deoxidizer.

[0011] Preferably, the dustproof film is made of polyethylene PE film or polyethylene terephthalate PET film, with a thickness of 0.012 mm, a density of 1.4, and a grammage per unit area of ​​35 g / ㎡, so as to be dustproof.

[0012] A production process of a dust-proof and oxygen-permeable deoxidizer packaging material comprises the following steps: S1: adding modified corn starch, cellulose, iron hydroxide and organic glass glue to pulp liquid in sequence, stirring and mixing by a high-speed mixer to prepare pulp; S2: Lay the ultra-thin non-woven fabric flat, and then evenly spray the pulp on the ultra-thin non-woven fabric, so that the pulp submerges and covers the ultra-thin non-woven fabric, removes part of the water, and becomes a wet pulp belt; S3: The roller presses the fibers and ultra-thin non-woven fabric in the pulp tape together, squeezes out the moisture therein, and makes the pulp tape more compact. The roller with a smooth surface is used to iron the paper surface to make it smooth, and the pulp tape is dried at the same time to obtain a paper tape. S4: The dust-proof film is heated and pasted on the front side of the paper tape, the inner film is heated and pasted on the back side of the paper tape, and finally cut to obtain the dust-proof and oxygen-permeable deoxidizer packaging material.

[0013] Preferably, in S1, the stirring speed is controlled at 640 rpm to 720 rpm, the stirring temperature is controlled at 35° C. to 50° C., and the stirring process is performed for 15 minutes to 30 minutes to enhance the stirring effect.

[0014] Preferably, in S4, both the dustproof film and the inner film are coated with carrageenan and then pasted on the paper tape to ensure the bonding effect.

[0015] Beneficial effects of the present invention: The dust-proof, oxygen-permeable, and deoxidizer packaging material of the present application adopts a three-layer structure of a breathable skeleton layer, a dust-proof film, and an inner film, which can play an effective dust-proof and oxygen-permeable function. In addition, by utilizing the material properties of the breathable skeleton layer, the strength of the dust-proof, oxygen-permeable, and deoxidizer packaging material can be enhanced, the tensile strength can be improved, and the dust-proof, oxygen-permeable, and deoxidizer packaging material can be prevented from tearing and deforming, and the deformation resistance and powder leakage prevention performance can be greatly improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 The working flow chart proposed by the present invention. DETAILED DESCRIPTION

[0017] The present invention will be further explained below in conjunction with specific embodiments.

[0018] Reference Figure 1 , Embodiment 1 This embodiment provides a dust-proof oxygen-permeable deoxidizer packaging material, which includes a breathable skeleton layer, a dust-proof film bonded to the upper surface of the breathable skeleton layer, and an inner film bonded to the lower surface of the breathable skeleton layer; The raw material composition and content of the breathable skeleton layer include 20 parts of ultra-thin non-woven fabric, 71 parts of pulp slurry, 5 parts of modified corn starch, 3 parts of organic glass glue, 0.80 parts of cellulose and 0.20 parts of ferric hydroxide by weight. The preparation method of the ultra-thin non-woven fabric is as follows: polyvinyl alcohol is melt-purified, and polyvinyl alcohol fiber is made into polyvinyl alcohol fiber by centrifugal spinning method, and then the polyvinyl alcohol fiber is combed into a thin cotton web with uniform thickness by physical opening, and the primary cotton web is rolled vertically and horizontally to make a preliminary rolling, and then impregnated with polyvinyl alcohol aqueous solution adhesive, and the secondary rolling is formed. The drying temperature is 170°C to obtain a finished ultra-thin non-woven fabric. The preparation method of pulp slurry is as follows: plant wood powder is obtained, and plant wood is Methanol is added to the powder, and cellulose in the plant wood powder is dissolved by methanol, and then solid-liquid separation is performed to obtain a cellulose dissolution liquid, the cellulose dissolution liquid is heated, and the methanol is evaporated by heat to obtain a cellulose paste liquid, the cellulose paste liquid is evaporated, and the remaining methanol in the cellulose paste liquid is dried and evaporated, and water is added to prepare a fiber pulp, and the water content of the obtained fiber pulp is adjusted to 60wt%. According to the water content, excess acetic anhydride is added to the fiber pulp, and the fiber pulp is heated to 60°C for hydrolysis reaction, and the mass ratio of cellulose, acetic anhydride and acetic acid is adjusted to 1:2:11, and the fiber pulp is heated to 85°C for esterification reaction to obtain a pulp liquid. The raw material composition and content of the modified corn starch include 95% by mass. Corn starch, 1% chitosan, 1% metal ions, 2% maltose amylase and 1% hexose oxidase, the metal ions are selected as calcium ions, and the preparation method of modified corn starch is as follows: corn starch is obtained, 10 times the amount of deionized water is added to the corn starch, and the mixture is configured into a starch emulsion, metal ions are added to the starch emulsion, and the starch emulsion after the addition of metal ions is subjected to pulse electric field treatment, the pulse field strength is 15KV / cm, the pulse width is 30μs, and the pulse treatment time is 10ms. After the pulse electric field treatment, chitosan and maltose amylase are added to perform enzymolysis to passivate the enzyme activity, and then hexose oxidase is added to perform lactone treatment on the oligoglucans in the starch emulsion. The reaction is carried out to passivate the enzyme activity, and the modified corn starch is obtained after air flow drying. The inner film adopts CPP film with a thickness of 22um, which can isolate the deoxidizer. The dust-proof film adopts polyethylene PE film and polyethylene terephthalate PET film with a thickness of 0.012mm, a density of 1.4, and a unit area weight of 35g / ㎡. The dust-proof and oxygen-permeable deoxidizer packaging material of the present application adopts a three-layer structure of a breathable skeleton layer, a dust-proof film and an inner membrane, which can play an effective dust-proof and oxygen-permeable function, and utilizes the material properties of the breathable skeleton layer to enhance the strength of the dust-proof and oxygen-permeable deoxidizer packaging material, improve the tensile strength, prevent the dust-proof and oxygen-permeable deoxidizer packaging material from tearing and deformation, and greatly improve the deformation resistance and anti-leakage performance.

[0019] A production process of a dust-proof and oxygen-permeable deoxidizer packaging material comprises the following steps: S1: adding modified corn starch, cellulose, iron hydroxide and organic glass glue to the pulp liquid in sequence, stirring and mixing them by a high-speed mixer, controlling the stirring speed at 680 rpm and the stirring temperature at 45° C. for 20 minutes to prepare pulp; S2: Lay the ultra-thin non-woven fabric flat, and then evenly spray the pulp on the ultra-thin non-woven fabric, so that the pulp submerges and covers the ultra-thin non-woven fabric, removes part of the water, and becomes a wet pulp belt; S3: The roller presses the fibers and ultra-thin non-woven fabric in the pulp tape together, squeezes out the moisture therein, and makes the pulp tape more compact. The roller with a smooth surface is used to iron the paper surface to make it smooth, and the pulp tape is dried at the same time to obtain a paper tape. S4: Heat the dust-proof film and stick it on the front side of the paper tape, heat the inner film and stick it on the back side of the paper tape, apply carrageenan on both the dust-proof film and the inner film, and then stick them on the paper tape, and finally cut them to obtain the dust-proof and oxygen-permeable deoxidizer packaging material.

[0020] Reference Figure 1 , Embodiment 2 This embodiment provides a dust-proof oxygen-permeable deoxidizer packaging material, which includes a breathable skeleton layer, a dust-proof film bonded to the upper surface of the breathable skeleton layer, and an inner film bonded to the lower surface of the breathable skeleton layer; The raw material composition and content of the breathable skeleton layer include 21 parts of ultra-thin non-woven fabric, 72 parts of pulp slurry, 4 parts of modified corn starch, 2 parts of organic glass glue, 0.70 parts of cellulose and 0.30 parts of ferric hydroxide by weight. The preparation method of the ultra-thin non-woven fabric is as follows: polyvinyl alcohol is melt-purified, and polyvinyl alcohol fiber is made into polyvinyl alcohol fiber by centrifugal spinning method, and then the polyvinyl alcohol fiber is combed into a thin cotton web with uniform thickness by physical opening, and the primary cotton web is rolled vertically and horizontally to make a preliminary rolling, and then impregnated with polyvinyl alcohol aqueous solution adhesive, and the secondary rolling is formed. The drying temperature is 170°C to obtain a finished ultra-thin non-woven fabric. The preparation method of pulp slurry is as follows: plant wood powder is obtained, and plant wood is Methanol is added to the powder, and cellulose in the plant wood powder is dissolved by methanol, and then solid-liquid separation is performed to obtain a cellulose dissolution liquid, the cellulose dissolution liquid is heated, and the methanol is evaporated by heat to obtain a cellulose paste liquid, the cellulose paste liquid is evaporated, and the remaining methanol in the cellulose paste liquid is dried and evaporated, and water is added to prepare a fiber pulp, and the water content of the obtained fiber pulp is adjusted to 60wt%. According to the water content, excess acetic anhydride is added to the fiber pulp, and the fiber pulp is heated to 60°C for hydrolysis reaction, and the mass ratio of cellulose, acetic anhydride and acetic acid is adjusted to 1:2:11, and the fiber pulp is heated to 85°C for esterification reaction to obtain a pulp liquid. The raw material composition and content of the modified corn starch include 95% by mass. Corn starch, 1% chitosan, 1% metal ions, 2% maltose amylase and 1% hexose oxidase, the metal ions are selected as calcium ions, and the preparation method of modified corn starch is as follows: corn starch is obtained, 10 times the amount of deionized water is added to the corn starch, and the mixture is configured into a starch emulsion, metal ions are added to the starch emulsion, and the starch emulsion after the addition of metal ions is subjected to pulse electric field treatment, the pulse field strength is 15KV / cm, the pulse width is 30μs, and the pulse treatment time is 10ms. After the pulse electric field treatment, chitosan and maltose amylase are added to perform enzymolysis to passivate the enzyme activity, and then hexose oxidase is added to perform lactone treatment on the oligoglucans in the starch emulsion. The reaction is carried out to passivate the enzyme activity, and the modified corn starch is obtained after air flow drying. The inner film adopts CPP film with a thickness of 22um, which can isolate the deoxidizer. The dust-proof film adopts polyethylene PE film and polyethylene terephthalate PET film with a thickness of 0.012mm, a density of 1.4, and a unit area weight of 35g / ㎡. The dust-proof and oxygen-permeable deoxidizer packaging material of the present application adopts a three-layer structure of a breathable skeleton layer, a dust-proof film and an inner membrane, which can play an effective dust-proof and oxygen-permeable function, and utilizes the material properties of the breathable skeleton layer to enhance the strength of the dust-proof and oxygen-permeable deoxidizer packaging material, improve the tensile strength, prevent the dust-proof and oxygen-permeable deoxidizer packaging material from tearing and deformation, and greatly improve the deformation resistance and anti-leakage performance.

[0021] A production process of a dust-proof and oxygen-permeable deoxidizer packaging material comprises the following steps: S1: adding modified corn starch, cellulose, iron hydroxide and organic glass glue to the pulp liquid in sequence, stirring and mixing them by a high-speed mixer, controlling the stirring speed at 680 rpm and the stirring temperature at 45° C. for 20 minutes to prepare pulp; S2: Lay the ultra-thin non-woven fabric flat, and then evenly spray the pulp on the ultra-thin non-woven fabric, so that the pulp submerges and covers the ultra-thin non-woven fabric, removes part of the water, and becomes a wet pulp belt; S3: The roller presses the fibers and ultra-thin non-woven fabric in the pulp tape together, squeezes out the moisture therein, and makes the pulp tape more compact. The roller with a smooth surface is used to iron the paper surface to make it smooth, and the pulp tape is dried at the same time to obtain a paper tape. S4: Heat the dust-proof film and stick it on the front side of the paper tape, heat the inner film and stick it on the back side of the paper tape, apply carrageenan on both the dust-proof film and the inner film, and then stick them on the paper tape, and finally cut them to obtain the dust-proof and oxygen-permeable deoxidizer packaging material.

[0022] Reference Figure 1 , Embodiment 3 This embodiment provides a dust-proof oxygen-permeable deoxidizer packaging material, which includes a breathable skeleton layer, a dust-proof film bonded to the upper surface of the breathable skeleton layer, and an inner film bonded to the lower surface of the breathable skeleton layer; The raw material composition and content of the breathable skeleton layer include 20 parts of ultra-thin non-woven fabric, 74 parts of pulp slurry, 3 parts of modified corn starch, 2 parts of organic glass glue, 0.70 parts of cellulose and 0.30 parts of ferric hydroxide by weight. The preparation method of the ultra-thin non-woven fabric is as follows: polyvinyl alcohol is melt-purified, and polyvinyl alcohol fiber is made into polyvinyl alcohol fiber by centrifugal spinning method, and then the polyvinyl alcohol fiber is combed into a thin cotton web with uniform thickness by physical opening, and the primary cotton web is rolled vertically and horizontally to make a preliminary rolling, and then impregnated with polyvinyl alcohol aqueous solution adhesive, and the secondary rolling is formed. The drying temperature is 170°C to obtain a finished ultra-thin non-woven fabric. The preparation method of pulp slurry is as follows: plant wood powder is obtained, and plant wood is Methanol is added to the powder, and cellulose in the plant wood powder is dissolved by methanol, and then solid-liquid separation is performed to obtain a cellulose dissolution liquid, the cellulose dissolution liquid is heated, and the methanol is evaporated by heat to obtain a cellulose paste liquid, the cellulose paste liquid is evaporated, and the remaining methanol in the cellulose paste liquid is dried and evaporated, and water is added to prepare a fiber pulp, and the water content of the obtained fiber pulp is adjusted to 60wt%. According to the water content, excess acetic anhydride is added to the fiber pulp, and the fiber pulp is heated to 60°C for hydrolysis reaction, and the mass ratio of cellulose, acetic anhydride and acetic acid is adjusted to 1:2:11, and the fiber pulp is heated to 85°C for esterification reaction to obtain a pulp liquid. The raw material composition and content of the modified corn starch include 95% by mass. Corn starch, 1% chitosan, 1% metal ions, 2% maltose amylase and 1% hexose oxidase, the metal ions are selected as calcium ions, and the preparation method of modified corn starch is as follows: corn starch is obtained, 10 times the amount of deionized water is added to the corn starch, and the mixture is configured into a starch emulsion, metal ions are added to the starch emulsion, and the starch emulsion after the addition of metal ions is subjected to pulse electric field treatment, the pulse field strength is 15KV / cm, the pulse width is 30μs, and the pulse treatment time is 10ms. After the pulse electric field treatment, chitosan and maltose amylase are added to perform enzymolysis to passivate the enzyme activity, and then hexose oxidase is added to perform lactone treatment on the oligoglucans in the starch emulsion. The reaction is carried out to passivate the enzyme activity, and the modified corn starch is obtained after air flow drying. The inner film adopts CPP film with a thickness of 22um, which can isolate the deoxidizer. The dust-proof film adopts polyethylene PE film and polyethylene terephthalate PET film with a thickness of 0.012mm, a density of 1.4, and a unit area weight of 35g / ㎡. The dust-proof and oxygen-permeable deoxidizer packaging material of the present application adopts a three-layer structure of a breathable skeleton layer, a dust-proof film and an inner membrane, which can play an effective dust-proof and oxygen-permeable function, and utilizes the material properties of the breathable skeleton layer to enhance the strength of the dust-proof and oxygen-permeable deoxidizer packaging material, improve the tensile strength, prevent the dust-proof and oxygen-permeable deoxidizer packaging material from tearing and deformation, and greatly improve the deformation resistance and anti-leakage performance.

[0023] A production process of a dust-proof and oxygen-permeable deoxidizer packaging material comprises the following steps: S1: adding modified corn starch, cellulose, iron hydroxide and organic glass glue to the pulp liquid in sequence, stirring and mixing them by a high-speed mixer, controlling the stirring speed at 680 rpm and the stirring temperature at 45° C. for 20 minutes to prepare pulp; S2: Lay the ultra-thin non-woven fabric flat, and then evenly spray the pulp on the ultra-thin non-woven fabric, so that the pulp submerges and covers the ultra-thin non-woven fabric, removes part of the water, and becomes a wet pulp belt; S3: The roller presses the fibers and ultra-thin non-woven fabric in the pulp tape together, squeezes out the moisture therein, and makes the pulp tape more compact. The roller with a smooth surface is used to iron the paper surface to make it smooth, and the pulp tape is dried at the same time to obtain a paper tape. S4: Heat the dust-proof film and stick it on the front side of the paper tape, heat the inner film and stick it on the back side of the paper tape, apply carrageenan on both the dust-proof film and the inner film, and then stick them on the paper tape, and finally cut them to obtain the dust-proof and oxygen-permeable deoxidizer packaging material.

[0024] Reference Figure 1 , Embodiment 4 This embodiment provides a dust-proof oxygen-permeable deoxidizer packaging material, which includes a breathable skeleton layer, a dust-proof film bonded to the upper surface of the breathable skeleton layer, and an inner film bonded to the lower surface of the breathable skeleton layer; The raw material composition and content of the breathable skeleton layer include 22 parts of ultra-thin non-woven fabric, 70 parts of pulp slurry, 5 parts of modified corn starch, 2 parts of organic glass glue, 0.60 parts of cellulose and 0.40 parts of ferric hydroxide by weight. The preparation method of the ultra-thin non-woven fabric is as follows: polyvinyl alcohol is melt-purified, and polyvinyl alcohol fiber is made into polyvinyl alcohol fiber by centrifugal spinning method, and then the polyvinyl alcohol fiber is combed into a thin cotton web with uniform thickness by physical opening, and the primary cotton web is rolled vertically and horizontally to make a preliminary rolling, and then impregnated with polyvinyl alcohol aqueous solution adhesive, and the secondary rolling is formed. The drying temperature is 170°C to obtain a finished ultra-thin non-woven fabric. The preparation method of pulp slurry is as follows: plant wood powder is obtained, and plant wood is Methanol is added to the powder, and cellulose in the plant wood powder is dissolved by methanol, and then solid-liquid separation is performed to obtain a cellulose dissolution liquid, the cellulose dissolution liquid is heated, and the methanol is evaporated by heat to obtain a cellulose paste liquid, the cellulose paste liquid is evaporated, and the remaining methanol in the cellulose paste liquid is dried and evaporated, and water is added to prepare a fiber pulp, and the water content of the obtained fiber pulp is adjusted to 60wt%. According to the water content, excess acetic anhydride is added to the fiber pulp, and the fiber pulp is heated to 60°C for hydrolysis reaction, and the mass ratio of cellulose, acetic anhydride and acetic acid is adjusted to 1:2:11, and the fiber pulp is heated to 85°C for esterification reaction to obtain a pulp liquid. The raw material composition and content of the modified corn starch include 95% by mass. Corn starch, 1% chitosan, 1% metal ions, 2% maltose amylase and 1% hexose oxidase, the metal ions are selected as calcium ions, and the preparation method of modified corn starch is as follows: corn starch is obtained, 10 times the amount of deionized water is added to the corn starch, and the mixture is configured into a starch emulsion, metal ions are added to the starch emulsion, and the starch emulsion after the addition of metal ions is subjected to pulse electric field treatment, the pulse field strength is 15KV / cm, the pulse width is 30μs, and the pulse treatment time is 10ms. After the pulse electric field treatment, chitosan and maltose amylase are added to perform enzymolysis to passivate the enzyme activity, and then hexose oxidase is added to perform lactone treatment on the oligoglucans in the starch emulsion. The reaction is carried out to passivate the enzyme activity, and the modified corn starch is obtained after air flow drying. The inner film adopts CPP film with a thickness of 22um, which can isolate the deoxidizer. The dust-proof film adopts polyethylene PE film and polyethylene terephthalate PET film with a thickness of 0.012mm, a density of 1.4, and a unit area weight of 35g / ㎡. The dust-proof and oxygen-permeable deoxidizer packaging material of the present application adopts a three-layer structure of a breathable skeleton layer, a dust-proof film and an inner membrane, which can play an effective dust-proof and oxygen-permeable function, and utilizes the material properties of the breathable skeleton layer to enhance the strength of the dust-proof and oxygen-permeable deoxidizer packaging material, improve the tensile strength, prevent the dust-proof and oxygen-permeable deoxidizer packaging material from tearing and deformation, and greatly improve the deformation resistance and anti-leakage performance.

[0025] A production process of a dust-proof and oxygen-permeable deoxidizer packaging material comprises the following steps: S1: adding modified corn starch, cellulose, iron hydroxide and organic glass glue to the pulp liquid in sequence, stirring and mixing them by a high-speed mixer, controlling the stirring speed at 680 rpm and the stirring temperature at 45° C. for 20 minutes to prepare pulp; S2: Lay the ultra-thin non-woven fabric flat, and then evenly spray the pulp on the ultra-thin non-woven fabric, so that the pulp submerges and covers the ultra-thin non-woven fabric, removes part of the water, and becomes a wet pulp belt; S3: The roller presses the fibers and ultra-thin non-woven fabric in the pulp tape together, squeezes out the moisture therein, and makes the pulp tape more compact. The roller with a smooth surface is used to iron the paper surface to make it smooth, and the pulp tape is dried at the same time to obtain a paper tape. S4: Heat the dust-proof film and stick it on the front side of the paper tape, heat the inner film and stick it on the back side of the paper tape, apply carrageenan on both the dust-proof film and the inner film, and then stick them on the paper tape, and finally cut them to obtain the dust-proof and oxygen-permeable deoxidizer packaging material.

[0026] Reference Figure 1 Embodiment 5 This embodiment provides a dust-proof oxygen-permeable deoxidizer packaging material, which includes a breathable skeleton layer, a dust-proof film bonded to the upper surface of the breathable skeleton layer, and an inner film bonded to the lower surface of the breathable skeleton layer; The raw material composition and content of the breathable skeleton layer include 15 parts of ultra-thin non-woven fabric, 80 parts of pulp slurry, 3 parts of modified corn starch, 1 part of organic glass glue, 0.80 parts of cellulose and 0.20 parts of ferric hydroxide by weight. The preparation method of the ultra-thin non-woven fabric is as follows: polyvinyl alcohol is melt-purified, and polyvinyl alcohol fiber is made into polyvinyl alcohol fiber by centrifugal spinning method, and then the polyvinyl alcohol fiber is combed into a thin cotton web with uniform thickness by physical opening, and the primary cotton web is rolled vertically and horizontally to make a preliminary rolling, and then impregnated with polyvinyl alcohol aqueous solution adhesive, and the secondary rolling is formed. The drying temperature is 170°C to obtain a finished ultra-thin non-woven fabric. The preparation method of pulp slurry is as follows: plant wood powder is obtained, and plant wood is Methanol is added to the powder, and cellulose in the plant wood powder is dissolved by methanol, and then solid-liquid separation is performed to obtain a cellulose dissolution liquid, the cellulose dissolution liquid is heated, and the methanol is evaporated by heat to obtain a cellulose paste liquid, the cellulose paste liquid is evaporated, and the remaining methanol in the cellulose paste liquid is dried and evaporated, and water is added to prepare a fiber pulp, and the water content of the obtained fiber pulp is adjusted to 60wt%. According to the water content, excess acetic anhydride is added to the fiber pulp, and the fiber pulp is heated to 60°C for hydrolysis reaction, and the mass ratio of cellulose, acetic anhydride and acetic acid is adjusted to 1:2:11, and the fiber pulp is heated to 85°C for esterification reaction to obtain a pulp liquid. The raw material composition and content of the modified corn starch include 95% by mass. Corn starch, 1% chitosan, 1% metal ions, 2% maltose amylase and 1% hexose oxidase, the metal ions are selected as calcium ions, and the preparation method of modified corn starch is as follows: corn starch is obtained, 10 times the amount of deionized water is added to the corn starch, and the mixture is configured into a starch emulsion, metal ions are added to the starch emulsion, and the starch emulsion after the addition of metal ions is subjected to pulse electric field treatment, the pulse field strength is 15KV / cm, the pulse width is 30μs, and the pulse treatment time is 10ms. After the pulse electric field treatment, chitosan and maltose amylase are added to perform enzymolysis to passivate the enzyme activity, and then hexose oxidase is added to perform lactone treatment on the oligoglucans in the starch emulsion. The reaction is carried out to passivate the enzyme activity, and the modified corn starch is obtained after air flow drying. The inner film adopts CPP film with a thickness of 22um, which can isolate the deoxidizer. The dust-proof film adopts polyethylene PE film and polyethylene terephthalate PET film with a thickness of 0.012mm, a density of 1.4, and a unit area weight of 35g / ㎡. The dust-proof and oxygen-permeable deoxidizer packaging material of the present application adopts a three-layer structure of a breathable skeleton layer, a dust-proof film and an inner membrane, which can play an effective dust-proof and oxygen-permeable function, and utilizes the material properties of the breathable skeleton layer to enhance the strength of the dust-proof and oxygen-permeable deoxidizer packaging material, improve the tensile strength, prevent the dust-proof and oxygen-permeable deoxidizer packaging material from tearing and deformation, and greatly improve the deformation resistance and anti-leakage performance.

[0027] A production process of a dust-proof and oxygen-permeable deoxidizer packaging material comprises the following steps: S1: adding modified corn starch, cellulose, iron hydroxide and organic glass glue to the pulp liquid in sequence, stirring and mixing them by a high-speed mixer, controlling the stirring speed at 680 rpm and the stirring temperature at 45° C. for 20 minutes to prepare pulp; S2: Lay the ultra-thin non-woven fabric flat, and then evenly spray the pulp on the ultra-thin non-woven fabric, so that the pulp submerges and covers the ultra-thin non-woven fabric, removes part of the water, and becomes a wet pulp belt; S3: The roller presses the fibers and ultra-thin non-woven fabric in the pulp tape together, squeezes out the moisture therein, and makes the pulp tape more compact. The roller with a smooth surface is used to iron the paper surface to make it smooth, and the pulp tape is dried at the same time to obtain a paper tape. S4: Heat the dust-proof film and stick it on the front side of the paper tape, heat the inner film and stick it on the back side of the paper tape, apply carrageenan on both the dust-proof film and the inner film, and then stick them on the paper tape, and finally cut them to obtain the dust-proof and oxygen-permeable deoxidizer packaging material.

[0028] Comparing the conventional deoxidizer packaging material with the deoxidizer packaging material prepared in Examples 1 to 5, the deoxidizer packaging materials prepared in Examples 1 to 5 are as follows: Comparative Example Embodiment 1 Embodiment 2 Embodiment 3 Embodiment 4 Embodiment 5 Tensile strength % 23 14.8 14.7 14.9 15.1 15.5 Deformation resistance % 7.7 7.8 7.8 7.7 7.9 Powder leakage prevention Failure qualified qualified qualified qualified qualified Test method: Test according to Q / HMR01-2019 "Other multi-layer composite food packaging films (bags)".

[0029] The test method for anti-leakage powder performance is as follows: take a package of samples, cut open the sealed edge and pour out the raw materials. Place the packaging material flat on the table and lay two layers of facial tissue under it. Use colored liquid red ink and use a burette to drop 0.1 ml of red ink onto the surface of the packaging material, which is about half of the air permeability area of ​​the unit piece. After standing for 5 minutes, check whether the facial tissue under the product absorbs the colored liquid red ink. If there is no absorption of red ink, it means the product is qualified.

[0030] It can be seen from the above table that the tensile strength, deformation resistance and powder leakage resistance of the deoxidizer packaging material prepared by the present invention are significantly improved, and the second embodiment is the best embodiment.

[0031] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A dust-proof and oxygen-permeable deoxidizer packaging material, It is characterized in that The dustproof and oxygen-permeable deoxidizer packaging material comprises a breathable skeleton layer, a dustproof film bonded to the upper surface of the breathable skeleton layer, and an inner film bonded to the lower surface of the breathable skeleton layer; The raw material composition and content of the breathable skeleton layer include, by mass, 15 to 25 parts of ultra-thin non-woven fabric, 70 to 80 parts of pulp slurry, 1 to 5 parts of modified corn starch, 1 to 5 parts of organic glass glue, 0.50 to 1.00 parts of cellulose and 0.10 to 0.50 parts of iron hydroxide.

2. A dust-proof oxygen-permeable deoxidizer packaging material according to claim 1, It is characterized in that The preparation method of the ultra-thin non-woven fabric comprises the following steps: melting and purifying polyvinyl alcohol, preparing polyvinyl alcohol fibers through a centrifugal spinning method, and then combing the polyvinyl alcohol fibers into a thin cotton web with uniform thickness through physical opening, rolling the primary cotton web vertically and horizontally to form a preliminary shape through a first rolling, then impregnating the web with a polyvinyl alcohol aqueous solution adhesive, and performing a second rolling to form the web, and drying the web at a temperature of 160° C. to obtain a finished ultra-thin non-woven fabric.

3. A dust-proof and oxygen-permeable deoxidizer packaging material according to claim 1, It is characterized in that The method for preparing paper pulp comprises the following steps: obtaining plant wood powder, adding methanol to the plant wood powder, dissolving cellulose in the plant wood powder by using methanol, performing solid-liquid separation to obtain cellulose dissolution liquid, heating the cellulose dissolution liquid, evaporating methanol by using heat to obtain cellulose paste liquid, evaporating the cellulose paste liquid, drying and evaporating the remaining methanol in the cellulose paste liquid, adding water to prepare fiber pulp, adjusting the water content of the obtained fiber pulp to 50wt%-70wt%, adding excess acetic anhydride to the fiber pulp according to the water content, heating to 50℃-70℃, performing hydrolysis reaction, adjusting the mass ratio of cellulose, acetic anhydride and acetic acid to 1:(2-3):(8-12), heating to 80℃-95℃, performing esterification reaction, and obtaining paper pulp.

4. A dust-proof and oxygen-permeable deoxidizer packaging material according to claim 1, It is characterized in that The raw material composition and content of the modified corn starch include 95% corn starch, 1% chitosan, 1% metal ions, 2% maltogenic amylase and 1% hexose oxidase by mass, and the metal ion is selected from one of calcium ion, copper ion and magnesium ion.

5. A dust-proof and oxygen-permeable deoxidizer packaging material according to claim 4, It is characterized in that The preparation method of the modified corn starch comprises the following steps: obtaining corn starch, adding 10 times the amount of deionized water to the corn starch, mixing and configuring into a starch emulsion, adding metal ions to the starch emulsion, subjecting the starch emulsion after the metal ions are added to a pulse electric field treatment, wherein the pulse field strength is 10KV / cm-30KV / cm, the pulse width is 20μs-40μs, and the pulse treatment time is 10ms; after the pulse electric field treatment, adding chitosan and maltose amylase to perform enzymolysis to inactivate the enzyme activity, then adding hexose oxidase to perform a lactonization reaction on oligoglucans in the starch emulsion to inactivate the enzyme activity, and obtaining the modified corn starch after air flow drying.

6. A dust-proof and oxygen-permeable deoxidizer packaging material according to claim 1, It is characterized in that The inner film is a CPP film with a thickness of 20um to 25um.

7. A dust-proof and oxygen-permeable deoxidizer packaging material according to claim 1, It is characterized in that The dust-proof film is made of polyethylene PE film and polyethylene terephthalate PET film, with a thickness of 0.012 mm, a density of 1.4, and a unit area weight of 35 g / ㎡.

8. A production process for preparing a dust-proof, oxygen-permeable deoxidizer packaging material as claimed in claim 1, It is characterized in that The following steps are involved: S1: adding modified corn starch, cellulose, iron hydroxide and organic glass glue to pulp liquid in sequence, stirring and mixing by a high-speed mixer to prepare pulp; S2: Lay the ultra-thin non-woven fabric flat, and then evenly spray the pulp on the ultra-thin non-woven fabric, so that the pulp submerges and covers the ultra-thin non-woven fabric, removes part of the water, and becomes a wet pulp belt; S3: The roller presses the fibers and ultra-thin non-woven fabric in the pulp tape together, squeezes out the moisture therein, and makes the pulp tape more compact. The roller with a smooth surface is used to iron the paper surface to make it smooth, and the pulp tape is dried at the same time to obtain a paper tape. S4: The dust-proof film is heated and pasted on the front side of the paper tape, the inner film is heated and pasted on the back side of the paper tape, and finally cut to obtain the dust-proof and oxygen-permeable deoxidizer packaging material.

9. The production process of a dust-proof and oxygen-permeable deoxidizer packaging material according to claim 8, It is characterized in that In S1, the stirring speed is controlled at 640 rpm to 720 rpm, the stirring temperature is controlled at 35° C. to 50° C., and the stirring process is performed for 15 minutes to 30 minutes.

10. The production process of a dust-proof and oxygen-permeable deoxidizer packaging material according to claim 8, It is characterized in that In S4, the dustproof film and the inner film are both coated with carrageenan and then attached to the paper tape.

Citation Information

Patent Citations

  • Process for manufacturing paper bag

    CN105690932A

  • Modifying manufacturing method of corn starch

    CN110092843A

  • Preparation method of deoxidizing agent packaging material

    CN110524904A

  • Preparation method of paper pulp

    CN114645479A

  • Preparation method of enzyme modified corn starch replacing hydroxypropyl starch

    CN116769853A