High-strength outer hexagon bolt and preparation method thereof

By hot-dip galvanizing the outer hexagonal bolts, the chemical composition and combination of plating agents are optimized, the problem of insufficient strength and corrosion resistance in the prior art is solved, and the effect of high strength and good corrosion resistance is achieved.

CN118957449AActive Publication Date: 2024-11-15HANDAN ZHIZENG FASTENER MANUFACTURING CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202411145484.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-15
Estimated Expiration
2044-08-20

AI Technical Summary

Technical Problem

The strength of existing external hexagon bolts is low, which affects their load-bearing capacity and service life, and is insufficient corrosion resistance.

Method used

By hot-dip galvanizing the bolt body, its chemical composition is optimized, including a specific proportion of components and plating agent combinations, a zinc layer is formed to improve tensile strength and corrosion resistance.

Benefits of technology

It significantly improves the tensile strength and corrosion resistance of the outer hexagon bolts, meets the requirements of high strength and corrosion resistance, and complies with relevant standards and specifications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The invention relates to the technical field of fasteners, and provides a high-strength outer hexagon bolt and a preparation method thereof. A high-strength outer hexagon bolt comprises a bolt body and a zinc layer obtained after the bolt body is subjected to hot galvanizing treatment, and the bolt body is composed of, by mass, 0.01%-0.05% of C, 1.5%-2.5% of Mn, 12%-16% of Cr, 0.08%-0.11% of Ti, 5.2%-8.7% of Ni, 0.18%-0.72% of Cu, 1.2%-3.7% of Al, 2.9%-4.3% of Mo, 0.05%-0.12% of B, 1.1%-2.3% of Nb, 0.03%-0.16% of Ta, smaller than or equal to 0.015% of P, smaller than or equal to 0.01% of S and the balance Fe and other inevitable impurities. According to the technical scheme, the problem that an outer hexagon bolt in the related technology is low in strength is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of fasteners, and in particular to a high-strength external hexagonal bolt and a preparation method thereof. Background Art

[0002] Bolts are common threaded connectors and a type of fastener, widely used in various industrial and construction fields. Bolts can be classified into hexagonal head bolts, round head bolts, square head bolts and countersunk head bolts according to the shape of the head, among which hexagonal head bolts are the most common type. According to different structures, hexagonal head bolts are divided into external hexagon and internal hexagon. External hexagon bolts are the most commonly used and can be used in a variety of occasions.

[0003] The strength of hexagonal bolts directly affects their load-bearing capacity and service life, and is an important mechanical performance indicator for examining safety and reliability. Therefore, improving the strength of hexagonal bolts is a research hotspot in this field, and providing a high-strength hexagonal bolt is of great significance to this field. Summary of the invention

[0004] The invention provides a high-strength external hexagonal bolt and a preparation method thereof, which solves the problem of low strength of the external hexagonal bolt in the related art.

[0005] The technical solution of the present invention is as follows: A high-strength external hexagonal bolt comprises a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in percentage by mass: C 0.01%-0.05%, Mn 1.5%-2.5%, Cr 12%-16%, Ti0.08%-0.11%, Ni 5.2%-8.7%, Cu 0.18%-0.72%, Al 1.2%-3.7%, Mo 2.9%-4.3%, B 0.05%-0.12%, Nb 1.1%-2.3%, Ta 0.03%-0.16%, P≤0.015%, S≤0.01%, and the rest is Fe and other inevitable impurities.

[0006] As a further technical solution, in terms of mass percentage, 1≤(Cr+Cu-1.5Mo) / Ni≤1.6.

[0007] The present invention stipulates that, in terms of mass percentage, 1≤(Cr+Cu-1.5Mo) / Ni≤1.6, which further improves the tensile strength of the external hexagonal bolt.

[0008] As a further technical solution, in terms of mass percentage, 0.1≤(B+Ta) / Nb≤0.18.

[0009] The present invention stipulates that, in terms of mass percentage, 0.1≤(B+Ta) / Nb≤0.18, which further improves the tensile strength of the external hexagonal bolt.

[0010] As a further technical solution, the hot-dip galvanizing treatment is specifically as follows: after pickling the bolt body, immersing it in a plating agent, drying it, hot-dip galvanizing it, and cooling it to obtain a high-strength external hexagon bolt; The plating assistant includes an organic plating assistant and an inorganic plating assistant.

[0011] The invention provides that the plating aid includes an organic plating aid and an inorganic plating aid, thereby improving the corrosion resistance of the external hexagonal bolt.

[0012] As a further technical solution, the molar ratio of the organic plating aid to the inorganic plating aid is 0.03:0.61.

[0013] As a further technical solution, the organic plating aid is an amine, and the inorganic plating aid is a salt.

[0014] As a further technical solution, the amine is ethylenediamine, and the salts include ammonium chloride, zinc chloride, sodium fluoroaluminate and borax.

[0015] In the present invention, the amine is limited to ethylenediamine, and the salts include ammonium chloride, zinc chloride, sodium fluoroaluminate and borax, which further improves the corrosion resistance of the external hexagonal bolt.

[0016] As a further technical solution, the molar ratio of ammonium chloride, zinc chloride, sodium fluoroaluminate and borax is 0.1:2:3:1.

[0017] The present invention limits the molar ratio of ammonium chloride, zinc chloride, sodium fluoroaluminate and borax to 0.1:2:3:1, thereby further improving the corrosion resistance of the external hexagonal bolt.

[0018] The invention also provides a method for preparing a high-strength external hexagonal bolt, comprising the following steps: hot-dip galvanizing the bolt body to obtain the high-strength external hexagonal bolt.

[0019] As a further technical solution, preheating is also included before the hot-dip galvanizing treatment, and the preheating temperature is 160~210℃.

[0020] The working principle and beneficial effects of the present invention are: The present invention provides a high-strength external hexagonal bolt, comprising a bolt body and a zinc layer obtained by hot-dip galvanizing the bolt body. The chemical composition of the bolt body is optimized so that alloy elements cooperate with each other, thereby improving the tensile strength of the external hexagonal bolt and solving the problem of low strength of the external hexagonal bolt in the related art. DETAILED DESCRIPTION

[0021] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] Example 1 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 12%, Ti 0.095%, Ni 6.5%, Cu0.18%, Al 2.2%, Mo 4.3%, B 0.05%, Nb 2.2%, Ta 0.06%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0023] Example 2 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.01%, Mn 1.5%, Cr 12%, Ti 0.08%, Ni 5.2%, Cu 0.18%, Al 1.2%, Mo 2.9%, B 0.05%, Nb 1.1%, Ta 0.03%, P 0.015%, S 0.005%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 160°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 61μm.

[0024] Example 3 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.05%, Mn 2.5%, Cr 16%, Ti 0.11%, Ni 8.7%, Cu 0.72%, Al 3.7%, Mo 4.3%, B 0.12%, Nb 2.3%, Ta 0.16%, P 0.011%, S 0.01%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 210°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 62μm.

[0025] Example 4 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer obtained by hot-dip galvanizing the bolt body, wherein the bolt body is composed of the following components in percentage by mass: C 0.03%, Mn 2.0%, Cr 12.6%, Ti 0.095%, Ni 6.5%, Cu 0.2%, Al 2.2%, Mo 4.2%, B 0.05%, Nb 2.2%, Ta 0.06%, P 0.013%, S 0.007%, and the remainder is Fe and other unavoidable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0026] Example 5 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.05%, Nb 2.2%, Ta 0.06%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0027] Example 6 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer obtained by hot-dip galvanizing the bolt body, wherein the bolt body is composed of the following components in percentage by mass: C 0.03%, Mn 2.0%, Cr 14.35%, Ti 0.095%, Ni 6.5%, Cu 0.4%, Al 2.2%, Mo 2.9%, B 0.05%, Nb 2.2%, Ta 0.06%, P 0.013%, S 0.007%, and the remainder is Fe and other unavoidable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0028] Example 7 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer obtained by hot-dip galvanizing the bolt body, wherein the bolt body is composed of the following components in percentage by mass: C 0.03%, Mn 2.0%, Cr 15.7%, Ti 0.095%, Ni 6.5%, Cu 0.69%, Al 2.2%, Mo 3.1%, B 0.05%, Nb 2.2%, Ta 0.06%, P 0.013%, S 0.007%, and the remainder is Fe and other unavoidable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0029] Example 8 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.07%, Nb 1.8%, Ta 0.11%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0030] Example 9 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.11%, Nb 1.5%, Ta 0.16%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0031] Example 10 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.12%, Nb 1.4%, Ta 0.16%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride and 0.4 mol sodium fluoroaluminate to an aqueous solution of ammonium chloride having a concentration of 0.04 mol / L, stirring evenly, to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0032] Embodiment 11 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.07%, Nb 1.8%, Ta 0.11%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.64 mol / L ammonium acetate aqueous solution and stirring evenly to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0033] Example 12 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.07%, Nb 1.8%, Ta 0.11%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride, 0.4 mol sodium fluoroaluminate, and 0.03 mol ammonium acetate to an aqueous solution of ammonium chloride having a concentration of 0.01 mol / L, and stirring uniformly to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0034] Example 13 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.07%, Nb 1.8%, Ta 0.11%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride, 0.4 mol sodium fluoroaluminate, and 0.03 mol ethylenediamine to an aqueous solution of ammonium chloride having a concentration of 0.01 mol / L, and stirring uniformly to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0035] Embodiment 14 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.07%, Nb 1.8%, Ta 0.11%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride, 0.4 mol borax, and 0.03 mol ethylenediamine to an aqueous solution of ammonium chloride having a concentration of 0.01 mol / L, and stirring uniformly to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0036] Embodiment 15 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.07%, Nb 1.8%, Ta 0.11%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride, 0.35 mol sodium fluoroaluminate, 0.05 mol borax, and 0.03 mol ethylenediamine to an aqueous solution of ammonium chloride having a concentration of 0.01 mol / L, and stirring uniformly to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0037] Example 16 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.07%, Nb 1.8%, Ta 0.11%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride, 0.3 mol sodium fluoroaluminate, 0.1 mol borax, and 0.03 mol ethylenediamine to an aqueous solution of ammonium chloride having a concentration of 0.01 mol / L, and stirring uniformly to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0038] Embodiment 17 S1. A high-strength hexagonal bolt, comprising a bolt body and a zinc layer after the bolt body is hot-dip galvanized, wherein the bolt body is composed of the following components in mass percentage: C 0.03%, Mn 2.0%, Cr 14%, Ti 0.095%, Ni 6.5%, Cu 0.31%, Al 2.2%, Mo 3.6%, B 0.07%, Nb 1.8%, Ta 0.11%, P 0.013%, S 0.007%, and the rest is Fe and other inevitable impurities; S2, a method for preparing a plating aid: adding 0.2 mol zinc chloride, 0.2 mol sodium fluoroaluminate, 0.2 mol borax, and 0.03 mol ethylenediamine to an aqueous solution of ammonium chloride having a concentration of 0.01 mol / L, and stirring uniformly to obtain a plating aid; S3. The hot-dip galvanizing treatment of the bolt body is specifically as follows: after pickling the bolt body, immerse it in a plating agent at 25°C for 15 minutes, dry it, preheat it to 190°C, melt the zinc metal into zinc liquid, heat it to 550°C, put the preheated bolt body into the zinc liquid for 30 seconds, take it out, remove the residual zinc and zinc nodules on the surface, cool it, and obtain a high-strength external hexagon bolt with a zinc layer thickness of 59μm.

[0039] The hexagonal bolts obtained in Examples 1 to 10 were tested for tensile strength according to the method in GB / T 228.1-2021 "Tensile test of metallic materials - Part 1: Room temperature test method", and the test rate was 0.005s -1 , the test results are recorded in Table 1.

[0040] Table 1 Tensile strength of hexagonal bolts

[0041] It can be seen from Table 1 that the tensile strength of the hexagonal bolt provided by the present invention is above 942 MPa, has high strength, and meets the standard requirements of DL / T 284-2021 "Hot-dip galvanized bolts and nuts for transmission line towers and power fittings" with a standard value of ≥800 MPa.

[0042] The tensile strength of the hexagonal bolts obtained in Examples 4 to 6 is higher than that in Example 1 and Example 7, indicating that, in terms of mass percentage, 1≤(Cr+Cu-1.5Mo) / Ni≤1.6 can further improve the strength of the hexagonal bolts.

[0043] The tensile strength of the hexagonal bolts obtained in Examples 8-9 is higher than that in Example 5 and Example 10, indicating that, in terms of mass percentage, 0.1≤(B+Ta) / Nb≤0.18 can further improve the strength of the hexagonal bolts.

[0044] The hexagonal bolts obtained in Examples 8 and 11 to 17 were subjected to a corrosion resistance test with reference to the neutral salt spray test method in GB / T 10125-2021 "Artificial atmosphere corrosion test salt spray test", and the time when corrosion began to occur was recorded. The test temperature was 35°C, the concentration of the sodium chloride solution was 50 g / L, and the pH value of the solution was 7. The results are recorded in Table 2.

[0045] Table 2 Corrosion resistance of hexagonal bolts

[0046] It can be seen from Table 2 that the hexagonal bolt provided by the present invention has good corrosion resistance.

[0047] The time when the hexagonal bolts obtained in Examples 12 to 17 began to corrode was higher than that in Example 8 and Example 11, indicating that the organic plating aid and the inorganic plating aid are used in combination, and the two can synergistically greatly improve the corrosion resistance of the hexagonal bolts.

[0048] The time at which the hexagonal bolts obtained in Examples 15 to 17 begin to corrode is higher than that in Examples 12 to 14, indicating that the amine is ethylenediamine, and the salts include ammonium chloride, zinc chloride, sodium fluoroaluminate and borax, which can further improve the corrosion resistance of the hexagonal bolts.

[0049] The time at which the hexagonal bolts obtained in Example 16 begin to corrode is higher than that in Example 15 and Example 17, indicating that the molar ratio of ammonium chloride, zinc chloride, sodium fluoroaluminate and borax is 0.1:2:3:1, which can further improve the corrosion resistance of the hexagonal bolts.

[0050] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A high-strength hexagonal bolt, characterized in that: The invention comprises a bolt body and a zinc layer obtained by hot-dip galvanizing the bolt body, wherein the bolt body is composed of the following components in percentage by mass: C 0.01%-0.05%, Mn 1.5%-2.5%, Cr 12%-16%, Ti 0.08%-0.11%, Ni 5.2%-8.7%, Cu 0.18%-0.72%, Al 1.2%-3.7%, Mo 2.9%-4.3%, B0.05%-0.12%, Nb 1.1%-2.3%, Ta 0.03%-0.16%, P≤0.015%, S≤0.01%, and the rest is Fe and other inevitable impurities.

2. A high-strength hexagonal bolt according to claim 1, characterized in that: In terms of mass percentage, 1≤(Cr+Cu-1.5Mo) / Ni≤1.

6.

3. A high-strength hexagonal bolt according to claim 2, characterized in that: In terms of mass percentage, 0.1≤(B+Ta) / Nb≤0.

18.

4. The high-strength hexagonal bolt according to claim 1, characterized in that: The hot-dip galvanizing treatment specifically comprises: pickling the bolt body, immersing it in a plating agent, drying it, hot-dip galvanizing it, and cooling it to obtain a high-strength external hexagon bolt; The plating assistant includes an organic plating assistant and an inorganic plating assistant.

5. A high-strength hexagonal bolt according to claim 4, characterized in that: The molar ratio of the organic plating aid to the inorganic plating aid is 0.03:0.

61.

6. A high-strength hexagonal bolt according to claim 5, characterized in that: The organic plating assistant is an amine, and the inorganic plating assistant is a salt.

7. A high-strength hexagonal bolt according to claim 6, characterized in that: The amine is ethylenediamine, and the salts include ammonium chloride, zinc chloride, sodium fluoroaluminate and borax.

8. The high-strength hexagonal bolt according to claim 7, characterized in that: The molar ratio of the ammonium chloride, zinc chloride, sodium fluoroaluminate and borax is 0.1:2:3:

1.

9. A method for preparing a high-strength external hexagonal bolt according to any one of claims 1 to 8, characterized in that: The following steps are involved: The bolt body is hot-dip galvanized to obtain a high-strength external hexagon bolt.

10. The method for preparing a high-strength external hexagonal bolt according to claim 9, characterized in that: Before the hot-dip galvanizing treatment, preheating is also included, and the preheating temperature is 160~210℃.

Citation Information

Patent Citations

  • Electrolytic plating assisting method for hot dip galvanizing of steel wire and electrolytic plating assistant

    CN101948990A

  • Bolt surface zinc plating layer production method

    CN103233193A

  • Process for plating zinc on surface of bolt

    CN109594031A

  • Hexagon nut with high wear resistance and corrosion resistance and preparation process thereof

    CN116497278A

  • Si-CONTAINING HIGH STRENGTH GALVANIZED STEEL SHEET HAVING EXCELLENT CORROSION RESISTANCE AND DUCTILITY, AND PRODUCTION METHOD THEREFOR

    JP2003105493A