Bio-based strain sensor and preparation method thereof

By using a combination of bio-based polyurethane film and graphene fabric in flexible strain sensors, the shortcomings of traditional strain sensors in response time, resistance stability and cyclic stability are solved, and more efficient strain detection performance and environmental protection advantages are achieved. .

CN118961008AActive Publication Date: 2024-11-15UNIV OF SCI & TECH BEIJING
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411034307.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-15
Estimated Expiration
2044-07-30

AI Technical Summary

Technical Problem

Existing flexible strain sensors have shortcomings in response time, reply time, resistance stability and long cycle stability, especially in the case of large strain and fast strain, which is difficult to meet high performance needs.

Method used

Using bio-based polyurethane film as the cover layer of the fabric skeleton, combined with graphene fabric, improve the response time, recovery time and resistance stability of the strain sensor through specific preparation methods, including the use of bio-based polydiol, diisocyanate and diol expansion. The combination of chain agents, the hard segment ratio is optimized, and the nickel mesh skeleton is treated by etching to improve conductivity.

Benefits of technology

It significantly improves the response time, reply time and resistance stability of the strain sensor, improves the detection performance under different operating conditions, solves the resource consumption and environmental protection problems of traditional petroleum-based polyurethane strain sensors, and provides better mechanical properties. and long cycle stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118961008A_ABST
    Figure CN118961008A_ABST
Patent Text Reader

Abstract

The invention belongs to the field of new materials, and discloses a bio-based strain sensor which comprises a bio-based polyurethane film and a graphene fabric attached to the surface of the film. The strain sensor adopts the bio-based polyurethane film as an elastic substrate, and can show more excellent response time, recovery time and resistance stability under different working conditions compared with a strain sensor taking petroleum-based polyurethane or polyurethane-urea as a substrate. Meanwhile, the invention also discloses a preparation method of the strain sensor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of new materials, and more specifically, relates to a strain sensor and a preparation method thereof. Background Art

[0002] Flexible strain sensors are devices used to measure the deformation or strain of an object after a force is applied. They work on a variety of principles, including resistive, capacitive, and piezoelectric. In resistive strain sensors, deformation or strain causes a change in the internal resistance of the sensor, which is reflected in the voltage or current change in the circuit. These sensors are widely used in engineering, science, and medicine to monitor the health of structures, the mechanical properties of materials, and the movement of organisms. In engineering, strain sensors can be used to monitor the deformation of structures such as bridges, buildings, and aircraft wings, while in the medical field, they are often used to monitor human movement, muscle activity, and the movement of prosthetic limbs. In general, strain sensors play an important role in many fields, and their wide application and diverse working principles make them one of the indispensable tools in the fields of engineering, science, and medicine.

[0003] Resistive strain sensors are usually composed of a flexible matrix material and a conductive filler: the flexible matrix material provides structural support and flexibility, and the conductive filler forms a conductive path and produces an electrical response to the external load. Although a lot of efforts have been made to optimize the role of these composite materials by developing various conductive materials (such as graphene, carbon nanotubes, carbon black, metal nanoparticles / nanowires, conductive polymers, ionic fluids and liquid metals) and nanostructures (such as films, fibers, textiles, foams, aerogels, snakes, woven fabrics, islands and hierarchical structures), the role of the flexible polymer matrix has long been overlooked.

[0004] For example, CN112853743A discloses a preparation method and application of a fabric strain sensor that can be used to monitor human physiological information. The flexible strain sensor uses common polyurethane (PU) fibers and polyamide (PA) fibers as matrix materials, and utilizes a cross-stretching dip-coating method to adsorb multi-walled carbon nanotubes and reduced graphene oxide on the fabric surface to form a conductive layer to obtain a conductive fabric, thereby completing the strain sensor preparation.

[0005] Thermoplastic polyurethane is an excellent elastomeric material with good flexibility, wear resistance and chemical resistance. There have been many reports on the preparation of strain sensors / flexible sensors based on thermoplastic polyurethane through appropriate processing modification. At present, most of the research focuses on the improvement of performance and the realization of functional diversification (authorization announcement number: CN112980178B; application publication number: CN 112374490 A, CN 117260814 A, CN 117426901 A), and there are few studies on the elastic matrix of strain sensors. In fact, the choice of substrate material has a very important influence on flexible strain sensors. The substrate material with good stretchability and good flexibility gives the flexible strain sensor a corresponding wide sensing detection range and the ability to bend and bend at will.

[0006] Among them, CN112113497B discloses a self-healing resistive strain sensor and its preparation method and application. The preparation method is to first soak a nickel sponge in a graphene oxide dispersion, purge and dry it for multiple cycles to obtain a nickel sponge coated with graphene oxide; use hydrogen bromide and thiourea to etch and reduce the nickel sponge coated with graphene oxide, wash and dry it to obtain a three-dimensional hollow thiol graphene skeleton; place the graphene skeleton in a silver nanowire dispersion and soak and dry it for multiple cycles to obtain a highly conductive silver nanowire-loaded graphene skeleton, connect electrodes, place it in a solution of self-healing functionalized polyurethane, dry it, and obtain a self-healing resistive strain sensor.

[0007] This scheme is based on etched graphene wrapped nickel sponge as the skeleton, covered with polyurethane to obtain a strain sensor; the scheme specification records that its response time / recovery time is 40 / 84ms. However, after further research based on this scheme, we found that there is still room for improvement in terms of response time, recovery time, resistance stability under large strain conditions, long cycle stability, and resistance stability under rapid strain conditions. Summary of the invention

[0008] The main purpose of the present invention is to provide a bio-based strain sensor, which, after using a bio-based polyurethane film to act on a fabric skeleton, can exhibit better response time, recovery time and resistance stability under different working conditions than strain sensors prepared from petroleum-based polyurethane.

[0009] At the same time, the invention also discloses a method for preparing the strain sensor.

[0010] According to a first aspect of the present invention, there is provided a strain sensor comprising a graphene fabric and a bio-based polyurethane film attached to a surface of the fabric.

[0011] The bio-based polyurethane film can exhibit better response time, recovery time and resistance stability under different working conditions than strain sensors made of petroleum-based polyurethane, indicating that the use of bio-based and petroleum-based raw materials is very important for the product in the application scenarios of the present invention.

[0012] During the experiment, we expected that the bio-based polyurethane-urea film should show the same rules as the bio-based polyurethane film. It was found that the bio-based polyurethane-urea film did not show similar excellent performance, indicating that the selection and use of the chain extender is also very important in the application scenario of the present invention.

[0013] In the above-mentioned bio-based strain sensor, the bio-based polyurethane film comprises the following structural units:

[0014] 60-80 parts by weight of bio-based polyglycol;

[0015] 20 to 35 parts by weight of diisocyanate;

[0016] 2 to 10 parts by weight of diol chain extender;

[0017] In the above-mentioned bio-based strain sensor, the hard segment ratio in the bio-based polyurethane film is 20-40wt%, and preferably, the hard segment ratio in the bio-based polyurethane is 23-40wt%.

[0018] In the above-mentioned bio-based strain sensor, the molecular weight of the bio-based polyglycol is 1000-2700, and preferably, the molecular weight of the bio-based polyglycol is 2000-2700.

[0019] In the above-mentioned bio-based strain sensor, the structural unit of the bio-based polyglycol is one or more combinations of propylene glycol, butylene glycol and hexylene glycol.

[0020] In the above strain sensor, the bio-based polyurethane film is attached to the upper and lower surfaces of the graphene fabric; the thickness of the bio-based polyurethane film is 0.05 to 1 mm.

[0021] In the above-mentioned bio-based strain sensor, the skeleton of the fabric is a nickel mesh, and graphene is deposited on the surface of the nickel mesh; the mesh number of the nickel mesh is 100-200 meshes; and the wire diameter of the nickel mesh is 50-100 μm.

[0022] In the above-mentioned bio-based strain sensor, the nickel mesh with graphene is etched to remove the nickel mesh.

[0023] At the same time, the present invention also discloses a method for preparing any of the strain sensors described above, which comprises sticking a fabric on a bio-based polyurethane film and connecting a wire to the fabric.

[0024] In the above-mentioned preparation method, the preparation method of the fabric is: placing a clean nickel mesh in a tubular furnace and undergoing four steps of heating, heat preservation, deposition, and cooling, introducing argon and hydrogen during the heating process, and introducing methane after a period of heat preservation to deposit graphene grown on the nickel mesh skeleton; using FeCl3·HCl solution to etch the nickel mesh with graphene attached to obtain a fabric with graphene on the surface.

[0025] More specifically, the argon flow rate is 200 sccm, the hydrogen flow rate is 100 sccm, and the methane flow rate is 27 sccm.

[0026] The heating rate is 17°C / min, the temperature is raised to 1000°C, the temperature is kept for 10 minutes, the deposition time is 20 minutes, and then air-cooled to room temperature. The FeCl3·HCl solution used for etching contains 3-4g of FeCl3, 4-5ml of 12mol / L hydrochloric acid, and 40-50ml of deionized water.

[0027] One of the above technical solutions of the present invention has at least one of the following advantages or beneficial effects:

[0028] The present invention uses bio-based polyurethane film as a matrix to prepare a strain sensor, solving the resource consumption and environmental problems caused by the current use of non-bio-based polyurethane. At the same time, compared with the commercially available BASF 60A polyurethane, the bio-based polyurethane film still has important mechanical properties such as excellent rebound performance. The prepared bio-based polyurethane film strain sensor has more stable strain sensing performance, better long-cycle stability, better rapid responsiveness, etc. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 The uniaxial sensing performance test results of bio-based polyurethane strain sensor 2 and petroleum-based polyurethane strain sensor 7;

[0030] Figure 2 The response performance test results of the bio-based polyurethane strain sensor 1 are shown;

[0031] Figure 3 The response performance test results of the bio-based polyurethane strain sensor 2;

[0032] Figure 4 The response performance test results of the petroleum-based polyurethane strain sensor 7 are shown;

[0033] Figure 5 The strain resistance stability test results of bio-based polyurethane strain sensor 2 and petroleum-based polyurethane strain sensor 7 are shown;

[0034] Figure 6 The long cycle resistance stability test results of the bio-based polyurethane strain sensor 1;

[0035] Figure 7 The long cycle resistance stability test results of bio-based polyurethane strain sensor 2;

[0036] Figure 8 The long cycle resistance stability test results of the bio-based polyurethane-urea strain sensor 5;

[0037] Fig. 9 The long cycle resistance stability test results of petroleum-based polyurethane strain sensor 7;

[0038] Fig.10 The resistance stability test results of the bio-based polyurethane strain sensor 1 at different strain rates;

[0039] Fig.11 The resistance stability test results of bio-based polyurethane strain sensor 2 at different strain rates;

[0040] Fig.12 The resistance stability test results of petroleum-based polyurethane strain sensor 7 at different strain rates;

[0041] Fig.13 The resistance stability test results of the bio-based polyurethane strain sensor 1 under different strain stretching;

[0042] Fig.14 The resistance stability test results of the bio-based polyurethane strain sensor 2 under different strain stretching;

[0043] Fig.15 The resistance stability test results of the bio-based polyurethane-urea strain sensor 5 under different strain stretching;

[0044] Fig.16 These are the resistance stability test results of petroleum-based polyurethane strain sensor 7 under different strain stretching conditions. DETAILED DESCRIPTION

[0045] The embodiments of the present invention are described in detail below. The embodiments are exemplary and are only used to explain the present invention, but are not to be construed as limiting the present invention.

[0046] Part I Preparation of Bio-based Polyurethane

[0047] Example 1

[0048] Step 1: Place the bio-based polydiester with a molecular weight of 2000 and the BDO chain extender in a vacuum oven and dry at 90°C for 1 hour to remove water.

[0049] Step 2: A one-step method is used to synthesize bio-based polyurethane, with the ratio of soft segment bio-based polydiester being 60wt%, the ratio of hard segment diisocyanate and chain extender being 40wt%, 60 parts by weight of bio-based polydiol, 31 parts by weight of diisocyanate, 9 parts by weight of chain extender, and the reaction is carried out at 55°C for 4h.

[0050] Step 3: Drying the bio-based polyurethane generated by the reaction.

[0051] Bio-based polyurethane 1 was obtained.

[0052] Example 2

[0053] Step 1: Place the bio-based polydiester with a molecular weight of 2000 and the PDO chain extender in a vacuum oven and dry at 90°C for 1 hour to remove water.

[0054] Step 2: A one-step method is used to synthesize bio-based polyurethane, with the ratio of soft segment bio-based polydiester being 70wt%, the ratio of hard segment diisocyanate and chain extender being 30wt%, 70 parts by weight of bio-based polydiol, 25 parts by weight of diisocyanate, 5 parts by weight of chain extender, and the reaction is carried out at 55°C for 4h.

[0055] Step 3: Drying the bio-based polyurethane generated by the reaction.

[0056] Bio-based polyurethane 2 was obtained.

[0057] Example 3

[0058] Step 1: Place the bio-based polydiester with a molecular weight of 2700 and the HDO chain extender in a vacuum oven and dry at 90°C for 1 hour to remove water.

[0059] Step 2: A one-step method is used to synthesize bio-based polyurethane, with the ratio of soft segment bio-based polydiester being 77wt%, the ratio of hard segment diisocyanate and chain extender being 23wt%, 80 parts by weight of bio-based polydiol, 20 parts by weight of diisocyanate, 4 parts by weight of chain extender, and the reaction is carried out at 55°C for 4h.

[0060] Step 3: Drying the bio-based polyurethane generated by the reaction.

[0061] Bio-based polyurethane 3 was obtained.

[0062] Example 4

[0063] Step 1: Place the bio-based polydiester with a molecular weight of 2000 and ADH adipic acid dihydrazide in a vacuum oven and dry at 90°C for 1 hour to remove water.

[0064] Step 2: Bio-based polyurethane-urea is synthesized by a two-step method, with the ratio of soft segment bio-based polydiester being 80wt%, the ratio of hard segment diisocyanate and chain extender being 23wt%, 80 parts by weight of bio-based polydiol, 13 parts by weight of diisocyanate, and 7 parts by weight of chain extender. In the first step, bio-based polydiester and diisocyanate are added, and the reaction is carried out at 55°C for 4h. In the second step, adipic acid dihydrazide dissolved in a solvent is added to the product of the first step, and the reaction is carried out at 40°C for 10h.

[0065] Step 3: Drying the bio-based polyurethane-urea generated by the reaction.

[0066] Bio-based polyurethane-urea 4 was obtained.

[0067] Part II Fabric Preparation

[0068] Example 5

[0069] Step 1: A 100-mesh nickel mesh was ultrasonically cleaned and dried with acetone, ethanol, and deionized water, respectively, and then used for later use, wherein the diameter of the nickel wire was 50 μm.

[0070] Step 2: Place the clean nickel mesh in a tube furnace, pass a mixed protective gas (argon with a flow rate of 200 sccm and hydrogen with a flow rate of 100 sccm), and then start heating at 17°C / min, heating to 1000°C and then keep warm for 10 minutes;

[0071] Step 3: introduce methane gas (flow rate 27 sccm, methane concentration 8%) for 20 minutes of deposition, and after the reaction is completed, air cool to room temperature to obtain a graphene nickel mesh.

[0072] Step 4: Cut the graphene nickel mesh prepared in step 3 into sample strips with a size of 6 mm × 15 mm.

[0073] Step 5: Etch the nickel mesh at 60° C. for 2 h using FeCl3·HCl solution. The FeCl3·HCl solution used for etching contains 3-4 g of FeCl3, 4-5 ml of 12 mol / L hydrochloric acid, and 40-50 ml of deionized water.

[0074] Step 6: Soak the graphene fabric in deionized water at 60° C. for 10 min, wash it several times, and dry it at 60° C. for later use to obtain fabric 1.

[0075] Example 6

[0076] Step 1: A 200-mesh nickel mesh was ultrasonically cleaned and dried with acetone, ethanol, and deionized water, respectively, and then used for later use, wherein the diameter of the nickel wire was 100 μm.

[0077] Step 2: Place the clean nickel mesh in a tube furnace, pass a mixed protective gas (argon with a flow rate of 200 sccm and hydrogen with a flow rate of 100 sccm), and then start heating at 17°C / min, heating to 1000°C and then keep warm for 10 minutes;

[0078] Step 3: introduce methane gas (flow rate 27 sccm, methane concentration 8%) for 20 minutes of deposition, and after the reaction is completed, air cool to room temperature to obtain a graphene nickel mesh.

[0079] Step 4: Cut the graphene nickel mesh prepared in step 3 into sample strips with a size of 6 mm × 15 mm.

[0080] Step 5: Etch the nickel mesh at 60° C. for 2 h using FeCl3·HCl solution. The FeCl3·HCl solution used for etching contains 3-4 g of FeCl3, 4-5 ml of 12 mol / L hydrochloric acid, and 40-50 ml of deionized water.

[0081] Step 6: Soak the graphene fabric in deionized water at 60°C for 10 minutes, wash it several times, and dry it at 60°C for later use to obtain fabric 2.

[0082] Part III Preparation of strain sensors

[0083] Strain sensor 1

[0084] Step 1: Dissolve the bio-based polyurethane in DMF at a mass ratio of TPU (bio-based polyurethane 1 of Example 1):DMF=1:5 to prepare a bio-based polyurethane solution for use.

[0085] Step 2: Pour the bio-based polyurethane solution into a polytetrafluoroethylene mold with a length of 60 mm, a width of 40 mm, and a depth of 2 mm, and dry it at 60°C for 4 hours.

[0086] Step 3: Use a small amount of DBSA solution to stick fabric 1 to the TPU film. After it is naturally air-dried, use conductive silver glue to stick copper wires about 3 cm long on both ends of fabric 1. The silver glue is naturally air-dried.

[0087] Step 4: Fill the mold again with the bio-based polyurethane solution and dry it at 60°C for 4 hours. Take out the film and cut it into the bio-based polyurethane strain sensor 1.

[0088] Strain Sensor 2

[0089] Step 1: Dissolve the bio-based polyurethane in DMF at a mass ratio of TPU (bio-based polyurethane 2 of Example 2):DMF=1:5 to prepare a bio-based polyurethane solution for use.

[0090] Step 2: Pour the bio-based polyurethane solution into a polytetrafluoroethylene mold with a length of 60 mm, a width of 40 mm, and a depth of 2 mm, and dry it at 60°C for 4 hours.

[0091] Step 3: Use a small amount of DBSA solution to stick fabric 2 to the TPU film. After it is naturally air-dried, use conductive silver glue to stick copper wires about 3 cm long on both ends of fabric 2. The silver glue is naturally air-dried.

[0092] Step 4: Fill the mold again with the bio-based polyurethane solution and dry it at 60°C for 4 hours. Take out the film and cut it into the bio-based polyurethane strain sensor 2.

[0093] Strain Sensor 3

[0094] Step 1: Dissolve the bio-based polyurethane in DMF at a mass ratio of TPU (bio-based polyurethane 3 of Example 3):DMF=1:5 to prepare a bio-based polyurethane solution for use.

[0095] Step 2: Pour the bio-based polyurethane solution into a polytetrafluoroethylene mold with a length of 60 mm, a width of 40 mm, and a depth of 2 mm, and dry it at 60°C for 4 hours.

[0096] Step 3: Use a small amount of DBSA solution to stick fabric 2 to the TPU film. After it is naturally air-dried, use conductive silver glue to stick copper wires about 3 cm long on both ends of fabric 2. The silver glue is naturally air-dried.

[0097] Step 4: Fill the mold again with the bio-based polyurethane solution and dry it at 60°C for 4 hours. Take out the film and cut it into the bio-based polyurethane strain sensor 3.

[0098] Strain Sensor 4

[0099] Step 1: Dissolve the bio-based polyurethane-urea in DMF at a mass ratio of TPU (bio-based polyurethane-urea 4 of Example 4):DMF=1:5 to prepare a bio-based polyurethane-urea solution for use.

[0100] Step 2: Pour the bio-based polyurethane-urea solution into a polytetrafluoroethylene mold with a length of 60 mm, a width of 40 mm, and a depth of 2 mm, and dry it at 60°C for 4 hours.

[0101] Step 3: Use a small amount of DBSA solution to stick fabric 1 to the TPU film. After it is naturally air-dried, use conductive silver glue to stick copper wires about 3 cm long on both ends of fabric 1. The silver glue is naturally air-dried.

[0102] Step 4: Fill the mold again with the bio-based polyurethane-urea solution and dry it at 60°C for 4 hours. Take out the film and cut it into the bio-based polyurethane-urea strain sensor 4

[0103] Strain sensor 5

[0104] Step 1: Dissolve the bio-based polyurethane-urea in DMF at a mass ratio of TPU (bio-based polyurethane-urea 4 of Example 4):DMF=1:5 to prepare a bio-based polyurethane-urea solution for use.

[0105] Step 2: Pour the bio-based polyurethane-urea solution into a polytetrafluoroethylene mold with a length of 60 mm, a width of 40 mm, and a depth of 2 mm, and dry it at 60°C for 4 hours.

[0106] Step 3: Use a small amount of DBSA solution to stick fabric 2 to the TPU film. After it is naturally air-dried, use conductive silver glue to stick copper wires about 3 cm long on both ends of fabric 2. The silver glue is naturally air-dried.

[0107] Step 4: Fill the mold again with the bio-based polyurethane-urea solution and dry it at 60°C for 4 hours. Take out the film and cut it into the bio-based polyurethane-urea strain sensor 5

[0108] Strain Sensor 6

[0109] Step 1: dissolving petroleum-based polyurethane in DMF at a mass ratio of TPU (BASF-60A):DMF=1:5 to prepare a petroleum-based polyurethane solution for use.

[0110] Step 2: Pour the petroleum-based polyurethane solution into a polytetrafluoroethylene mold with a length of 60 mm, a width of 40 mm, and a depth of 2 mm, and dry it at 60°C for 4 hours.

[0111] Step 3: Use a small amount of DBSA solution to stick fabric 1 to the TPU film. After it is naturally air-dried, use conductive silver glue to stick copper wires about 3 cm long on both ends of fabric 1. The silver glue is naturally air-dried.

[0112] Step 4: Fill the mold again with petroleum-based polyurethane solution and dry at 60°C for 4 hours. Take out the film and cut it into petroleum-based polyurethane strain sensor 6.

[0113] Strain Sensor 7

[0114] Step 1: dissolving petroleum-based polyurethane in DMF at a mass ratio of TPU (BASF-60A):DMF=1:5 to prepare a petroleum-based polyurethane solution for use.

[0115] Step 2: Pour the petroleum-based polyurethane solution into a polytetrafluoroethylene mold with a length of 60 mm, a width of 40 mm, and a depth of 2 mm, and dry it at 60°C for 4 hours.

[0116] Step 3: Use a small amount of DBSA solution to stick fabric 2 to the TPU film. After it is naturally air-dried, use conductive silver glue to stick copper wires about 3 cm long on both ends of fabric 2. The silver glue is naturally air-dried.

[0117] Step 4: Fill the mold again with petroleum-based polyurethane solution and dry at 60°C for 4 hours. Take out the film and cut out the petroleum-based polyurethane strain sensor 7.

[0118] Performance Testing

[0119] Uniaxial sensing performance test: The uniaxial sensing performance of the bio-based polyurethane strain sensor was tested by a tensile machine and a resistance recorder, with a tensile speed of 12 mm / min and a tensile strain of 50%;

[0120] Response performance test: The responsiveness of the bio-based polyurethane strain sensor was tested by a tensile machine and a resistance recorder, with a tensile speed of 50 mm / min, a tensile strain of 2%, and a dwell time of 2 s;

[0121] Strain resistance stability test: The stability of the bio-based polyurethane strain sensor under a certain strain is tested by a tensile machine and a resistance recorder. The tensile speed is 12mm / min and the tensile strain is 20%;

[0122] Long-cycle resistance stability test: The long-cycle stability of the bio-based polyurethane strain sensor was tested by a tensile machine and a resistance recorder, with a tensile speed of 12 mm / min, a tensile strain of 20%, and a cycle number of 100 times;

[0123] Resistance stability test at different strain rates: The adaptability of the bio-based polyurethane strain sensor to different strain rates was tested by a tensile machine and a resistance recorder. The tensile speeds were 12 mm / min, 24 mm / min, and 48 mm / min, respectively. The tensile strain was 20%, and each tensile speed was cycled 5 times.

[0124] Resistance stability test under different strain stretching: The stability of the bio-based polyurethane strain sensor under different strain stretching was tested by a tensile test machine and a resistance recorder. The stretching speed was 12 mm / min, and the stretching strains were 5%, 10%, 15%, 20%, and 25% respectively. Each stretching speed was cycled 10 times.

[0125] The above test was carried out using bio-based polyurethane strain sensor 1, bio-based polyurethane strain sensor 2, bio-based polyurethane-urea strain sensor 5, and petroleum-based polyurethane strain sensor 7 as test objects;

[0126] Figure 1The uniaxial tensile sensing performance comparison curve of bio-based polyurethane strain sensor 2 and petroleum-based polyurethane strain sensor 7 is shown in the figure. Under the same strain, the resistance change sensitivity of petroleum-based polyurethane strain sensor 7 is better than that of bio-based polyurethane strain sensor 2. The resistance change sensitivity is close in the strain range of 0%-20%; under 30% strain, the resistance change sensitivity of bio-based polyurethane strain sensor 2 is 6.5, and the resistance change sensitivity of petroleum-based polyurethane strain sensor 7 is 22.1; under 40% strain, the resistance change sensitivity of bio-based polyurethane strain sensor 2 is 10.6, and the resistance change sensitivity of petroleum-based polyurethane strain sensor 7 is 58.0; under 50% strain, the resistance change sensitivity of bio-based polyurethane strain sensor 2 is 18.2, and the resistance change sensitivity of petroleum-based polyurethane strain sensor 7 is 211.1.

[0127] Figure 2 , 3 4 are the response and response time test curves of bio-based polyurethane strain sensor 1, bio-based polyurethane strain sensor 2, and petroleum-based polyurethane strain sensor 7. The tensile strain is 2%, the holding time is 2s, and the tensile and recovery rates are both 50mm / min. The response time of bio-based polyurethane strain sensor 1 is 98ms, and the recovery time is 106ms; the response time of bio-based polyurethane strain sensor 2 is 87ms, and the recovery time is 89ms; the response time of petroleum-based polyurethane strain sensor 7 is 94ms, and the recovery time is 216ms. The rapid response performance of the bio-based polyurethane strain sensor under small strain conditions is significantly better than that of the petroleum-based polyurethane strain sensor 7.

[0128] Figure 5 The resistance change rate curves of bio-based polyurethane strain sensor 2 and petroleum-based polyurethane strain sensor 7 under 20% strain are shown in Figure 2. Bio-based polyurethane strain sensor 2 reaches stability at about 25 minutes under 20% strain, and the resistance change rate decays by 10.2%; petroleum-based polyurethane strain sensor 7 still does not reach stability at 225 minutes under 20% strain, and the resistance change rate decays by as much as 53.8%. It can be seen that the sensing signal of the bio-based polyurethane strain sensor is more stable, and has obvious advantages in signal accuracy.

[0129] Figure 6 , 7Figures 8 and 9 are the 100-cycle sensing curves of 20% strain of bio-based polyurethane strain sensor 1, bio-based polyurethane strain sensor 2, bio-based polyurethane-urea strain sensor 5, and petroleum-based polyurethane strain sensor 7. The resistance change sensitivity of bio-based polyurethane strain sensor 1 is about 13.75, the resistance change sensitivity of bio-based polyurethane strain sensor 2 is about 11, the resistance change sensitivity of bio-based polyurethane-urea strain sensor 5 is about 3, and the resistance change sensitivity of petroleum-based polyurethane strain sensor 7 is about 22.5. The resistance change rate of bio-based polyurethane strain sensor 1 and bio-based polyurethane strain sensor 2 remains basically unchanged during the cycle; the resistance change rate of bio-based polyurethane-urea strain sensor 5 and petroleum-based polyurethane strain sensor 7 shows an increasing trend. It can be concluded that bio-based polyurethane strain sensors have obvious advantages in long-cycle stability.

[0130] Fig.10 , 11 1 and 2 are the variable speed sensing test curves of 20% strain of bio-based polyurethane strain sensor 1, bio-based polyurethane strain sensor 2, and petroleum-based polyurethane strain sensor 7, and the stretching speeds are 12mm / min, 24mm / min, and 48mm / min. The resistance change rate of the bio-based polyurethane strain sensor at different speeds remains basically unchanged; the resistance change rate of the petroleum-based polyurethane strain sensor 7 shows an increasing trend, and the faster the strain speed of the strain sensor, the more unstable its sensing signal, and the greater the peak resistance and the resistance offset at the end of a single cycle. It can be concluded that the bio-based polyurethane strain sensor has obvious advantages in adaptability to different strain speeds.

[0131] Fig.13 , 14 , 15, and 16 are different strain cycle test curves of bio-based polyurethane strain sensor 1, bio-based polyurethane strain sensor 2, bio-based polyurethane-urea strain sensor 5, and petroleum-based polyurethane strain sensor 7. The resistance change rate of bio-based polyurethane strain sensor under different strains is basically stable; the resistance at the end of a single stretch in the petroleum-based polyurethane strain sensor 7 shows an increasing trend, and the resistance change rate is correspondingly unstable. The greater the strain of the strain sensor, the more unstable its sensing signal is, and the greater the resistance offset at the end of a single cycle. The strain sensing performance of bio-based polyurethane-urea strain sensor 5 is comparable to that of petroleum-based polyurethane strain sensor 7. It can be concluded that bio-based polyurethane strain sensors have obvious advantages in stability under different strain stretches.

[0132] Generally speaking, the use of bio-based materials and petroleum-based materials only has advantages in terms of environmental protection and renewable performance raw materials, and generally there is no obvious performance difference between petroleum-based and bio-based materials.

[0133] The experiments of the present invention have confirmed that the use of bio-based raw materials in strain sensors not only has significant advantages in cost and environmental protection, but also has obvious advantages in strain sensing performance, long-cycle stability, rapid responsiveness, etc.

Claims

1. A bio-based strain sensor, characterized in that: It includes a bio-based polyurethane film and a graphene fabric attached to the surface of the film.

2. The bio-based strain sensor according to claim 1, characterized in that: The bio-based polyurethane film comprises the following structural units: 60-80 parts by weight of bio-based polyglycol; 20 to 35 parts by weight of diisocyanate; 2 to 10 parts by weight of diol chain extender.

3. The bio-based strain sensor according to claim 2, characterized in that: The hard segment ratio in the bio-based polyurethane is 20 to 40 wt %. Preferably, the hard segment ratio in the bio-based polyurethane is 23 to 40 wt %.

4. The bio-based strain sensor according to claim 2, characterized in that: The molecular weight of the bio-based polyglycol is 1000-2700, preferably, the molecular weight of the bio-based polyglycol is 2000-2700.

5. The bio-based strain sensor according to claim 2, characterized in that: The structural unit of the bio-based polyglycol is one or more combinations of propylene glycol, butylene glycol and hexylene glycol.

6. The bio-based strain sensor according to claim 1, characterized in that: The bio-based polyurethane film is attached to the upper and lower surfaces of the fabric; the thickness of the bio-based polyurethane film is 0.05-1 mm.

7. The bio-based strain sensor according to claim 1, characterized in that: The skeleton of the grown graphene is a nickel mesh; the mesh number of the nickel mesh is 100 to 200 meshes; and the wire diameter of the nickel mesh is 50 to 100 μm.

8. The bio-based strain sensor according to claim 7, characterized in that: The nickel mesh with graphene is etched to remove the nickel mesh.

9. The method for preparing a bio-based strain sensor according to any one of claims 1 to 8, characterized in that: Stick the graphene fabric to the bio-based polyurethane film, connect the wires to the fabric, and then attach another layer of bio-based polyurethane film.

10. The preparation method according to claim 9, characterized in that: The preparation method of the fabric comprises the following steps: placing a clean nickel mesh in a tubular furnace and undergoing four steps of heating, heat preservation, deposition and cooling, introducing argon and hydrogen during the heating process, introducing methane after heat preservation for a period of time, and depositing graphene grown on the nickel mesh skeleton; and etching the nickel mesh with graphene attached by using a FeCl3·HCl solution to obtain a fabric with graphene on the surface.

Citation Information

Patent Citations

  • Flexible strain transducer based on carbon nanofiber yarn woven fabric and preparation method thereof

    CN108680095A

  • Antistatic thermoplastic polyurethane and preparation method thereof

    CN111040111A

  • AgNWs / rGO / TPU flexible strain sensor and preparation method thereof

    CN114034239A

  • Preparation method and application of zwitterionic polyurethane and zwitterionic polyurethane-based ionic gel

    CN116693801A

  • Polyurethane material, polyurethane film, biosensor and preparation method of biosensor

    CN117069908A