High-turn large-inductance high-temperature superconducting magnet stress segmented detection method based on multi-optical fiber interference system
By using a multi-fiber interferometry system to accurately measure stress changes in high-temperature superconducting magnets, the problems of accuracy and speed in traditional detection methods have been solved, achieving high-precision and high-sensitivity stress monitoring and ensuring magnet stability.
Patent Information
- Application Number
- CN202411281625.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-19
AI Technical Summary
Traditional stress detection methods are not accurate enough, are cumbersome to operate and slow in high-temperature superconducting magnets, and cannot meet the requirements for real-time and accurate stress monitoring, thus affecting the stability and safety of the magnet.
A multi-fiber interferometry system is used to split light into multiple beams through 1×(N+1) and 1×N fiber couplers. The change in optical path difference between the fiber and the reference fiber is measured. Combined with a photodetector and a data processor, the stress of various parts of the high-temperature superconducting magnet can be accurately measured.
It achieves high-precision, high-sensitivity, and strong anti-interference stress detection, which is suitable for stable operation monitoring of high-temperature superconducting magnets and avoids the risk of quenching.
Smart Images

Figure CN118980447A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of superconducting magnet applications and relates to a segmented stress detection method for a high-turns, high-inductance, high-temperature superconducting magnet based on a multi-fiber interference system. Background Art
[0002] High-temperature superconducting magnets, with their excellent electromagnetic properties and low energy consumption, have development potential in cutting-edge technology fields such as power transmission, maglev trains, nuclear magnetic resonance imaging, and controlled nuclear fusion. However, the operating stability of the magnet is affected by its internal strain. Small stress changes can cause fluctuations in the operating state and even lead to quenching, releasing huge heat and posing a serious threat to the equipment. Therefore, it is particularly important to perform real-time and accurate stress detection on high-temperature superconducting magnets.
[0003] Traditional stress detection methods, such as magnetic measurement and mechanical methods, face many limitations. Problems such as poor measurement accuracy in strong magnetic fields and low temperature environments, cumbersome operation procedures and slow detection speed have greatly limited their application in superconducting magnet strain monitoring. This not only affects the detection efficiency, but also may lead to potential risks due to information lag.
[0004] In view of this, it is urgent to develop a stress detection technology with high stability, high precision and high sensitivity. This technology needs to be able to adapt to the unique operating environment of high-temperature superconducting magnets, accurately capture the strain changes of each part, ensure the stable operation of the magnet, avoid the risk of quenching, and provide a solid guarantee for the widespread application of superconducting magnets. Summary of the invention
[0005] The purpose of the present invention is to propose a segmented stress detection method for a high-turn, high-inductance, high-temperature superconducting magnet based on a multi-fiber interference system. The stress of each part of the superconducting magnet can be measured during the operation of the high-temperature superconducting magnet, and the method has high detection accuracy, high sensitivity, and strong anti-interference ability.
[0006] The core idea of the present invention is that in an interference system, there is a quantitative relationship between the refractive index of an optical fiber and the strain it is subjected to. By measuring the interference image before and after the stress change, the change in the optical path difference can be obtained, and then the strain of each section of the magnet can be calculated. The present invention uses a 1×(N+1) type fiber coupler to divide the incident light into N+1 beams, which are respectively sent into N measuring optical fibers and 1 reference optical fiber. The outgoing light of the reference optical fiber is divided into N beams by a 1×N type fiber coupler, and interferes with the outgoing light of the N measuring optical fibers in the N fiber couplers. When the superconducting magnet starts to run or fails, the disturbance of the magnet will cause the stress of the measuring optical fiber to change, thereby causing the refractive index of the optical fiber to change. By measuring the change in the optical path difference formed by each measuring optical fiber and the reference optical fiber, the stress change of each section of the magnet can be accurately obtained.
[0007] The technical solution of the present invention is as follows:
[0008] A stress segmented detection method for a high-turn, high-inductance, high-temperature superconducting magnet based on a multi-fiber interference system is characterized in that it comprises a light source, whose output end is connected to N+1 equal-length optical fibers through a first optical fiber coupler, wherein the N optical fibers (measurement optical fibers) are synchronously wound with the superconducting tape, and the output end of each measurement optical fiber is respectively connected to the input end of N second optical fiber couplers. Another optical fiber (reference optical fiber) has the same structure and environment as the measurement optical fiber, and its output end is connected to a third optical fiber coupler, and the output end of the coupler is further connected to N second optical fiber couplers.
[0009] The emitted light of the measuring fiber and the reference fiber meet in the second fiber coupler and interfere with each other. The interference image formed is converted into an electrical signal by a photodetector, and then analyzed by a data processor after amplification and data collection. The optical path difference is calculated by comparing the changes in the number of light and dark fringes in the interference image, and then the strain of each part of the superconducting magnet is accurately obtained based on the determined relationship between the optical path difference and stress.
[0010] To ensure the accuracy of the measurement, the ambient temperature must be kept constant throughout the process, and the measuring optical fiber and the reference optical fiber should be under the same environmental conditions.
[0011] Wherein, the light source is a fiber laser or other light-emitting device.
[0012] The first optical fiber coupler is of 1×(N+1) type, and the splitting ratio is 1:1. The second optical fiber coupler is of 2×1 type. The third optical fiber coupler is of 1×N type, and the splitting ratio is 1:1.
[0013] The superconducting magnet is wound from superconducting tape and is cooled by immersion cooling, gas cooling, conduction cooling or the like.
[0014] The stress segmented detection method of a high-turns, high-inductance, high-temperature superconducting magnet using the multi-fiber interference system comprises the following steps:
[0015] ① After activating the light source, the light beam is finely divided into N+1 parts through the first fiber coupler, of which N parts are respectively directed to N measuring fibers, and the other part enters the reference fiber. Subsequently, the outgoing light of the N measuring fibers is respectively directed to the N second fiber couplers. At the same time, the outgoing light of the reference fiber is evenly divided into N parts through the third fiber coupler and also sent to the N second fiber couplers to achieve precise interference with the outgoing light of the measuring fiber.
[0016] The interfered optical signal is captured by the photodetector and then converted into an electrical signal. This electrical signal is quickly transmitted to the data processor, and the optical path difference between each measuring optical fiber and the reference optical fiber is obtained through precise calculation, providing key data for the precise calculation of subsequent stress changes.
[0017] ②When the superconducting magnet is started and maintained in a long-term superconducting operation state, the strain phenomenon inside the magnet will cause strain differences between the N measurement optical fibers and the reference optical fibers. This difference directly causes the refractive index of the light inside the optical fiber to change, which in turn affects the propagation path of the light in the optical fiber, that is, the optical path. As a result, the interference image observed in the interference system will show a significant change in the number of light and dark fringes. This change intuitively reflects the tiny fluctuations in the stress of each part of the superconducting magnet. The specific principles are as follows:
[0018] In the interference image, if the optical path difference OPD = kλ, the interference image is bright fringes; if the optical path difference OPD = (k+1 / 2)λ, the interference image is dark fringes; where k is a positive integer and λ is the wavelength of light.
[0019] In the interference system, the optical path difference between N measuring optical fibers and the reference optical fiber can be expressed as OPD (1-N) =OPL (1-N) -OPL0=n (1-N) (ε (1-N) )L (1-N) -n0(ε0)L0=△n (1-N) △L (1-N) , where n (1-N) (ε (1-N) ) represents the stress ε of each measuring optical fiber (1-N) The refractive index under the initial stress ε0 is n0(ε0), and L (1-N) Indicates the length of each measured optical fiber, L0 indicates the length of the reference optical fiber, △L (1-N) Indicates the length of the stress change section of each measuring optical fiber.
[0020] At the beginning, the length and stress of the N measurement fibers and the reference fiber are equal, L (1-N) =L0,ε (1-N) =ε0, so OPD (1-N) = 0. When the superconducting magnet is in operation or fails, the strain of the superconducting magnet causes a certain length of N measuring optical fibers to be △L (1-N) The stress ε (1-N) The change in refractive index n (1-N) Change, at this time the optical path difference OPD (1-N) This causes changes in the light and dark fringes in the interference image. By recording the number of changes in the light and dark fringes to obtain the k value, the corresponding optical path differences OPD1, OPD2, ... OPD can be obtained. N .
[0021] ③ The data processor performs data processing, assuming that each optical fiber is initially in a zero stress state, ε0 = 0, and uses the following formula to obtain the stress ε1, ε2, ...ε of each segment of the magnet after the change N :
[0022]
[0023] Where: L is the length of the initial measurement fiber, n(ε0) is the refractive index of the measurement fiber under the initial stress ε0, C ε Indicates the strain coefficient of the measured optical fiber. The above data can be obtained through calibration measurement or from the manufacturer.
[0024] The beneficial effects of the present invention are:
[0025] The present invention proposes a new technology for segmented stress detection of high-temperature superconducting magnets using a multi-fiber interference system. This technology combines N measuring optical fibers with one reference optical fiber to achieve accurate measurement of strains in various parts of the superconducting magnet during operation. This method uses the relationship between the refractive index of the optical fiber and the stress to reflect the stress changes of the magnet by measuring the optical path difference. Compared with traditional stress detection methods, this technology has significant advantages such as simple operation, high detection accuracy, high sensitivity, and strong anti-interference ability. It is particularly suitable for application in the stable operation monitoring of high-temperature superconducting magnets. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Attached Figure 1 Schematic diagram of the superconducting magnet structure prepared by winding three measuring optical fibers together with superconducting tapes;
[0027] Description of reference numerals: 101 - measuring optical fiber; 102 - superconducting tape;
[0028] Attached Figure 2 is a schematic diagram of the reference optical fiber structure;
[0029] Description of reference numerals: 201 - reference optical fiber;
[0030] Attached Figure 3 This is a system connection block diagram of a temperature segmented detection method for a high-turn, high-inductance, high-temperature superconducting magnet based on a multi-fiber interference system;
[0031] Description of reference numerals: 301-light source; 302-first optical fiber coupler; 303-measurement optical fiber; 304-second optical fiber coupler; 305-reference optical fiber; 306-third optical fiber coupler; 307-photodetector; 308-amplifier; 309-data acquisition card; 310-data processor; 311-high temperature superconducting magnet; DETAILED DESCRIPTION
[0032] The following will be combined with the accompanying drawings in the examples of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. It is obvious that the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0033] The present invention provides a segmented stress detection method for a high-turn, high-inductance, high-temperature superconducting magnet based on a multi-fiber interference system. The present invention is further described below by taking a four-fiber interference system as an example in combination with embodiments and drawings.
[0034] 1. As attached Figure 1 , three measuring optical fibers and superconducting tapes are wound in sections to prepare a superconducting magnet 1, and the specific process is as follows:
[0035] Three measuring optical fibers are respectively wound on the segmented superconducting tape, and the composite structure is wound into a solenoid shape, wherein the three measuring optical fibers are of equal length and completely the same shape, and then the measuring optical fibers are fixed to the middle of the superconducting tape using a low-temperature adhesive, and the attached Figure 1 The solenoid-shaped high-temperature superconducting magnet 1 is shown.
[0036] 2. As attached Figure 2 , prepare reference fiber 2: wind the reference fiber into the same spiral structure as the measurement fiber, and obtain the following Figure 2 Reference fiber 2 is shown.
[0037] 3. As attached Figure 3 , is a connection block diagram of the multi-fiber interference system of the present invention, which is constructed as follows: the output end of the light source (301) is connected to the input end of the first fiber coupler (302), and the four output ends of the first fiber coupler (302) are respectively connected to the input ends of four optical fibers, three of which are measurement optical fibers (303), which are wound in sections together with the superconducting tape and are respectively connected to three second fiber couplers (304) at the output ends. Another optical fiber is used as a reference optical fiber (305), and its output end is connected to the input end of the third fiber coupler (306), and then the output end of the third fiber coupler (306) is respectively connected to the additional input ends of the three second fiber couplers (304), and the output ends of the three second fiber couplers (304) are connected to a photodetector (307) for converting optical signals into electrical signals. The converted electrical signals are enhanced by an amplifier (308) and then sent to a data processor (310) for analysis and processing via a data acquisition card (309).
[0038] Three of the four optical fibers of equal length are used as measurement fibers and are wound in sections along with the superconducting tape to form a superconducting magnet 311. The three measurement optical fibers evenly divide the superconducting magnet and have the same bending shape. The other optical fiber is also wound in the same shape as a reference optical fiber and is in the same environment as the superconducting magnet.
[0039] The light source 301 is a fiber laser or other light emitting device.
[0040] The first fiber coupler 302 is of 1×4 type, and the splitting ratio is 1:1. The second fiber coupler 304 is of 2×1 type. The third fiber coupler 306 is of 1×3 type, and the splitting ratio is 1:1.
[0041] The following are the relevant devices and parameters in the embodiment
[0042] The light source 301 is a self-made 632.8nm band helium-neon laser with an output light intensity of 35mW and a line width of 1MHz. Other fiber lasers or other light-emitting devices may also be used.
[0043] The first fiber coupler 302 is a 1×4 single-mode fiber coupler with a splitting ratio of 1:1. The second fiber coupler 304 is a 2×1 single-mode fiber coupler. The third fiber coupler 306 is a 1×3 single-mode fiber coupler with a splitting ratio of 1:1.
[0044] The photodetector 307 is a high-speed detector that converts optical signals into electrical signals. The bandwidth of the photodetector used in the example of the present invention is 25 GHz, which can realize high-speed optical pulse signal detection. Other types of high-speed photodetectors can also be used.
[0045] Amplifier 308 is a device that amplifies an electrical signal. Other types of amplifying elements may also be used.
[0046] The data acquisition card 309 is a device for triggering data acquisition. The data acquisition card sampling rate used in the present invention is 3GS / s. Other types of high-speed acquisition cards can also be used.
[0047] The data processor 310 is mainly used to process and display in real time the data collected by the data acquisition card 309. The system processing software written in the example of the present invention is based on the data acquisition card.
[0048] The multi-fiber interference system is used to perform segmented stress detection on a high-turns, high-inductance, high-temperature superconducting magnet, including the following steps:
[0049] ① After activating the light source, the light beam is finely divided into N+1 parts through the first fiber coupler, of which N parts are respectively directed to N measuring fibers, and the other part enters the reference fiber. Subsequently, the outgoing light of the N measuring fibers is respectively directed to the N second fiber couplers. At the same time, the outgoing light of the reference fiber is evenly divided into N parts through the third fiber coupler and also sent to the N second fiber couplers to achieve precise interference with the outgoing light of the measuring fiber.
[0050] The interfered optical signal is captured by the photodetector and then converted into an electrical signal. This electrical signal is quickly transmitted to the data processor, and the optical path difference between each measuring optical fiber and the reference optical fiber is obtained through precise calculation, providing key data for the precise calculation of subsequent stress changes.
[0051] ②When the superconducting magnet is started and maintained in a long-term superconducting operation state, the strain phenomenon inside the magnet will cause strain differences between the N measurement optical fibers and the reference optical fibers. This difference directly causes the refractive index of the light inside the optical fiber to change, which in turn affects the propagation path of the light in the optical fiber, that is, the optical path. As a result, the interference image observed in the interference system will show a significant change in the number of light and dark fringes. This change intuitively reflects the tiny fluctuations in the stress of each part of the superconducting magnet. The specific principles are as follows:
[0052] In the interference image, if the optical path difference OPD = kλ, the interference image is bright fringes; if the optical path difference OPD = (k+1 / 2)λ, the interference image is dark fringes; where k is a positive integer and λ is the wavelength of light.
[0053] In the interference system, the optical path difference between N measuring optical fibers and the reference optical fiber can be expressed as OPD (1-N) =OPL (1-N) -OPL0=n (1-N) (ε (1-N) )L (1-N) -n0(ε0)L0=△n (1-N) △L (1-N) , where n (1-N) (ε (1-N) ) represents the stress ε of each measuring optical fiber (1-N) The refractive index under the initial stress ε0 is n0(ε0), and L (1-N) Indicates the length of each measured optical fiber, L0 indicates the length of the reference optical fiber, △L (1-N) Indicates the length of the stress change section of each measuring optical fiber.
[0054] At the beginning, the length and stress of the N measurement fibers and the reference fiber are equal, L (1-N) =L0,ε (1-N) =ε0, so OPD (1-N)= 0. When the superconducting magnet is in operation or fails, the strain of the superconducting magnet causes a certain length of N measuring optical fibers to be △L (1-N) The stress ε (1-N) The change in refractive index n (1-N) Change, at this time the optical path difference OPD (1-N) This causes changes in the light and dark fringes in the interference image. By recording the number of changes in the light and dark fringes to obtain the k value, the corresponding optical path differences OPD1, OPD2, ... OPD can be obtained. N .
[0055] ③ The data processor performs data processing, assuming that each optical fiber is initially in a zero stress state, ε0 = 0, and uses the following formula to obtain the stress ε1, ε2, ...ε of each segment of the magnet after the change N :
[0056]
[0057] Where: L is the length of the initial measurement fiber, n(ε0) is the refractive index of the measurement fiber under the initial stress ε0, C ε Indicates the strain coefficient of the measured optical fiber. The above data can be obtained through calibration measurement or from the manufacturer.
[0058] The above description is only an example of the implementation of the solenoid-shaped superconducting magnet of the present invention, and is not intended to limit the protection scope of the present invention. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed by the present invention. For example, the light source can be natural single-shot light, lasers of other wavelengths, infrared lasers, etc.; other shapes of high-temperature superconducting magnets such as D-type, racetrack type, etc., and the superconducting materials can be wires, strips or composite conductors, etc., all of which are covered within the protection scope of the present invention.
Claims
1. A stress segmentation detection method for a high-turn, high-inductance, high-temperature superconducting magnet based on a multi-fiber interference system, characterized in that it comprises a light source, whose output end is connected to N+1 equal-length optical fibers through a first optical fiber coupler, wherein the N optical fibers (measurement optical fibers) are synchronously wound with the superconducting tape, and the output end of each measurement optical fiber is respectively connected to the input end of N second optical fiber couplers. Another optical fiber (reference optical fiber) has the same structure and environment as the measurement optical fiber, and its output end is connected to a third optical fiber coupler, and the output end of the coupler is further connected to N second optical fiber couplers. The outgoing light of the measuring fiber and the reference fiber meet in the second fiber coupler and interfere with each other. The interference image formed is converted into an electrical signal by a photodetector, and then analyzed by a data processor after amplification and data collection. By comparing the changes in the number of light and dark fringes in the interference image, the optical path difference is calculated, and then the strain of each part of the superconducting magnet is accurately obtained based on the determined relationship between the optical path difference and stress. To ensure the accuracy of the measurement, the ambient temperature must be kept constant throughout the process, and the measuring fiber and the reference fiber should be placed in the same environmental conditions.
2. The method according to claim 1, characterized in that The light source is a fiber laser or other light emitting device.
3. The method according to claim 1, characterized in that The first optical fiber coupler is of 1×(N+1) type, and the splitting ratio is 1:
1. The second optical fiber coupler is of 2×1 type. The third optical fiber coupler is of 1×N type, and the splitting ratio is 1:
1.
4. The method according to claim 1, characterized in that: The superconducting magnet is wound by superconducting tape and is cooled by immersion cooling, gas cooling, conduction cooling or the like.