Method for detecting connection matching strength of injection molding part shell of washing machine
Through random sampling and grouping testing of the shell of injection molded parts of the washing machine, multiple indicators of the samples before and after connection are evaluated, the problem of poor evaluation of connection fit strength in the prior art is solved, the evaluation accuracy and product reliability are improved, and the accuracy of evaluation is improved, and the reliability of the product is reduced. Resource waste and production costs.
Patent Information
- Application Number
- CN202411463959.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-21
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-10-21
AI Technical Summary
The prior art fails to effectively evaluate the connection fit strength of the shell of the injection molded parts of the washing machine, resulting in loosening or separation of the connection parts, affecting the reliability of the product, and may require rework or recall, resulting in waste of resources.
Random sampling and grouping testing methods are used, including compressive strength test, ultrasonic test, tensile test, vibration test and stress test, to evaluate sample data before and after connection, analyze compressive strength index, defect degree index, and coordination strength index. Performance fluctuation index and load-bearing capacity index to determine whether the sample quality is qualified.
Through multi-stage evaluation, the accuracy and reliability of quality assessment are improved, the cost of rework and recall is reduced, the product can withstand external forces during use, and the safety guarantee for marketing and user use is provided.
Smart Images

Figure CN118980511A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of quality monitoring and relates to a method for detecting the connection and matching strength of an injection-molded shell of a washing machine. Background Art
[0002] In the manufacturing process of household appliances such as washing machines, the connection strength of the injection molded shell, as a key component to protect the internal mechanical structure and circuit, directly affects the overall performance, durability and user safety of the product. As consumers' requirements for product quality continue to increase, it is particularly important to accurately and efficiently test the connection strength of the injection molded shell of washing machines.
[0003] For example, the Chinese invention with publication number CN110774517A discloses a method for molding a washing machine injection molded part shell, which relates to the field of injection molding technology and comprises the following steps: plasticizing: preheating the pouring system, feeding the injection molding pellets into the barrel through the hopper, raising the barrel temperature to the melting temperature, maintaining the plasticizing pressure, and making the pellets in a molten state; filling: injecting the plasticized melt into the preheated mold through the nozzle of the hot runner, so that the melt fills the entire mold cavity; holding pressure: after the filling stage is completed, entering the holding pressure stage, under the action of the holding pressure, the melt at the gate continues to flow into the mold cavity, replenishing the space generated by the shrinkage of the plastic part, so that the shape of the product plastic part is complete; cooling and shaping: the cooling and shaping time is; demoulding: after the cooling and shaping time is up, opening the mold to eject the plastic part, and obtaining the washing machine injection molded part shell. The product prepared by the present invention has excellent comprehensive performance, and the molding method is simple and easy to implement, which greatly improves the production efficiency and product quality.
[0004] The above-mentioned prior art has the following problems: 1. The prior art does not fully evaluate the injection-molded shell of the washing machine before connection, which may waste a lot of time, manpower and material resources in the subsequent after-sales process. For example, the connection operation of the injection-molded shell of the washing machine with insufficient compressive strength or serious defects may eventually need to be reworked or scrapped, resulting in a huge waste of resources.
[0005] 2. The existing technology may not be able to intuitively reflect the firmness of the connection part of the washing machine injection molded part shell, and it is difficult to determine whether the connection part of the washing machine injection molded part shell can withstand the corresponding external force in actual use. This may cause the connection part to loosen or separate during the use of the product, affecting the reliability of the product. Summary of the invention
[0006] In view of this, in order to solve the problems raised in the above background technology, a method for detecting the connection and fitting strength of the outer shell of an injection-molded part of a washing machine is now proposed.
[0007] The purpose of the present invention can be achieved through the following technical solutions: The present invention provides a method for detecting the connection strength of the injection molded shell of a washing machine, including: S1, sample grouping test: randomly select multiple samples from the produced injection molded shell of the washing machine for testing, and group the multiple samples for compressive strength test, ultrasonic test, tensile test, vibration test and stress test.
[0008] S2. Collection of test data before connection: obtaining the compressive strength data of the sample before connection through compressive strength test; obtaining the defect degree data of the sample before connection through ultrasonic test.
[0009] S3. Collection of test data after connection: Connect multiple samples of tensile test, vibration test and stress test with preset connecting parts at the connection position to obtain multiple connected samples, and obtain the matching strength data of the connected samples through tensile test; obtain the performance fluctuation data of the connected samples through vibration test; and obtain the stress test data of the connected samples through stress test.
[0010] S4. Test data analysis: Analyze the compressive strength index of the sample before connection through the compressive strength data of the sample before connection ; Analyze the defect degree index of the sample before connection through the defect degree data of the sample before connection ; Analyze the matching strength index of the connected samples through the matching strength data of the connected samples ; Analyze the performance fluctuation index of the connected samples through the performance fluctuation data of the connected samples ; Analyze the load-bearing capacity index of the connected sample through the stress test data of the connected sample .
[0011] S5. Sample quality warning: Based on the compressive strength index and defect index of the sample before connection, analyze the quality compliance index of the sample before connection ; Based on the matching strength index, performance fluctuation index and load-bearing capacity index of the connected samples, the quality compliance index of the connected samples is analyzed. ; Then analyze the quality compliance index of the sample to determine whether the quality of the injection molded shell of the washing machine is qualified, and then issue an early warning.
[0012] Compared with the prior art, the present invention has the following beneficial effects: (1) The present invention can ensure sufficient quality evaluation of the injection molded shells of washing machines in a production batch through random sampling and group testing, thereby reducing the deviation caused by single sample testing and improving the accuracy and reliability of the evaluation. Group testing helps to discover possible quality problems or defects at an early stage, and promptly discover and repair problems in the production process, thereby avoiding large-scale recalls and rework, thereby saving costs. In addition, by optimizing the process and reducing the defective product rate, production costs can also be reduced in the long run.
[0013] (2) The present invention obtains the compressive strength data of the washing machine injection molded parts shell (including the pressure value when cracks first appear on multiple samples before connection), defect degree data (including the area, depth and number of each defect type of multiple samples before connection), fit strength data (including the tensile force value when the connecting parts of multiple samples after connection fall off and the corresponding deformation length of the connecting parts), performance fluctuation data (including the displacement of the connecting parts of multiple samples after connection and the acceleration at each monitoring time point) and stress test data (including the stress value when deformation first appears at the connection position of multiple samples after connection) through scientific testing methods. The present invention can quickly screen out the washing machine injection molded parts shell with poor performance, reduce the cost of later changes and rework, shorten the time cycle from product research and development to market launch, and the testing process from pre-connection samples to post-connection samples can evaluate the performance and risks of the product, providing a solid guarantee for the market promotion of the product and the safety of user use.
[0014] (3) The present invention can fully understand the basic conditions of the samples before connection by performing data analysis on the compressive strength and defect degree of the samples before connection, so that corresponding measures can be taken in advance, such as screening out samples with insufficient compressive strength or serious defects to avoid wasting time and resources in the subsequent connection process. By analyzing the matching strength, performance fluctuation degree and bearing capacity of the samples after connection, the effect of the connection process can be accurately evaluated. The matching strength index can intuitively reflect the firmness of the connection and ensure that the connected samples can withstand the corresponding external force in actual use. The performance fluctuation degree index can help determine whether the performance of the connected samples is stable, which is crucial for application scenarios that require high precision and high reliability. The bearing capacity index can promptly discover problems that may occur during the connection process and avoid product failure due to cracking.
[0015] (4) The present invention can more accurately judge whether the quality of the injection molded shell of the washing machine is qualified by comprehensively considering the quality compliance index of the samples before and after connection. Compared with a single-stage evaluation, this multi-stage analysis takes more factors into consideration, reduces the possibility of misjudgment, and improves the accuracy of quality judgment. In addition, the early warning function can send a signal at an early stage when quality problems occur, so that the manufacturer can take timely measures to intervene, which helps to avoid further deterioration of quality problems and reduce losses. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0017] Figure 1 It is a schematic diagram for implementing the method steps of the present invention.
[0018] Figure 2 It is a schematic diagram of the steps of analyzing the coordination strength index of the connected sample according to the present invention.
[0019] Figure 3 It is a schematic diagram of the steps of analyzing the performance fluctuation index of the connected sample according to the present invention. DETAILED DESCRIPTION
[0020] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0021] See also Figure 1 As shown, the present invention provides a method for detecting the connection strength of the injection molded shell of a washing machine, the method comprising: S1, sample grouping test: randomly selecting multiple samples from the produced injection molded shell of the washing machine for testing, and grouping the multiple samples for compressive strength test, ultrasonic test, tensile test, vibration test and stress test.
[0022] As a preferred embodiment, the specific process of grouping the multiple samples is: extracting multiple samples, and then equally dividing the multiple samples into five groups.
[0023] For example, if fifty samples are taken and divided equally into five groups, the number of samples in each group will be ten.
[0024] The present invention can ensure a full quality assessment of the injection molded housing of the washing machine in the production batch through random sampling and group testing, reduce the deviation caused by single sample testing, improve the accuracy and reliability of the assessment, and the group testing helps to find possible quality problems or defects at an early stage, timely find and repair problems in the production process, avoid large-scale recalls and rework, and thus save costs. In addition, by optimizing the process and reducing the defective product rate, the production cost can also be reduced in the long run.
[0025] S2. Collection of test data before connection: obtaining the compressive strength data of the sample before connection through compressive strength test; obtaining the defect degree data of the sample before connection through ultrasonic test.
[0026] S3. Collection of test data after connection: Connect multiple samples of tensile test, vibration test and stress test with preset connecting parts at the connection position to obtain multiple connected samples, and obtain the matching strength data of the connected samples through tensile test; obtain the performance fluctuation data of the connected samples through vibration test; and obtain the stress test data of the connected samples through stress test.
[0027] The present invention obtains the compressive strength data of the outer shell of the injection molded parts of the washing machine (including the pressure value when cracks first appear on multiple samples before connection), the defect degree data (including the area, depth and number of each defect type of multiple samples before connection), the matching strength data (including the tensile force value when the connecting parts of multiple samples after connection fall off and the deformation length of the corresponding connecting parts), the performance fluctuation data (including the displacement of the connecting parts of multiple samples after connection and the acceleration at each monitoring time point) and the stress test data (including the stress value when deformation first appears at the connection position of multiple samples after connection) through a scientific testing method. The outer shell of the injection molded parts of the washing machine with poor performance can be quickly screened out, the cost of later changes and rework can be reduced, and the time cycle from research and development to market launch of the product can be shortened. In addition, the testing process from the samples before connection to the samples after connection can evaluate the performance and risks of the product, and provide a solid guarantee for the market promotion of the product and the safety of user use.
[0028] S4. Test data analysis: Analyze the compressive strength index of the sample before connection through the compressive strength data of the sample before connection ; Analyze the defect degree index of the sample before connection through the defect degree data of the sample before connection ; Analyze the matching strength index of the connected samples through the matching strength data of the connected samples ; Analyze the performance fluctuation index of the connected samples through the performance fluctuation data of the connected samples ; Analyze the load-bearing capacity index of the connected sample through the stress test data of the connected sample .
[0029] Furthermore, the analysis of the compressive strength index of the sample before connection includes: selecting a target test surface from each surface of the sample before connection, taking it and the surface opposite to it as opposite surfaces, obtaining the opposite surface of the sample before connection, and then obtaining the opposite surfaces of multiple samples before connection.
[0030] Gradually apply pressure to the center positions of opposite surfaces of multiple pre-connected samples in the compressive strength test through a pressure-applying device until cracks first appear on the multiple pre-connected samples in the compressive strength test, observe and record the pressure values when cracks first appear on the multiple pre-connected samples, and screen out the minimum pressure value when cracks first appear on the pre-connected samples.
[0031] The contact area between the pressure device and the sample before connection is extracted from the database, and the minimum pressure value when the sample before connection first cracks is divided by the contact area between the pressure device and the sample before connection to obtain the compressive strength value of the sample, which is recorded as .
[0032] Extract the standard compressive strength values of the injection molded housing of the washing machine from the database.
[0033] Analyze the compressive strength index of the sample before connection , ,in Indicates the standard compressive strength value of the injection molded shell of the washing machine.
[0034] Furthermore, the analysis of the defect degree index of the pre-connection sample includes: scanning multiple pre-connection samples in the ultrasonic test with an ultrasonic tester, obtaining ultrasonic signal images of the multiple pre-connection samples in the ultrasonic test, and extracting the area, depth and number of each defect type of the multiple pre-connection samples.
[0035] Substitute the areas of each defect type of multiple samples before connection into the average calculation formula to obtain the areas of each defect type of the samples before connection, recorded as ,in Indicates The number corresponding to the defect type, .
[0036] According to the analysis method of the area of each defect type of the sample before connection, the depth and number of each defect type of the sample before connection are obtained in the same way, which are recorded as and .
[0037] Analyze the defect index of the sample before joining , ,in , and Respectively represent the first The allowable area, allowable depth and allowable number of each defect type, , and The weight factors corresponding to the area deviation value, depth deviation value and number deviation value of the defect type of the injection molded shell of the washing machine are represented respectively, and .
[0038] As a preferred embodiment, the , and They can be set to 0.5, 03 and 0.2 respectively. The area usually reflects the size of the space occupied by the defect in the sample and is an important indicator for evaluating the severity of the defect. The depth is also a key parameter, which is related to the degree of influence of the defect on the internal structure of the sample. Deeper defects may be more likely to cause the sample to break or degrade. However, in some cases, the impact of depth may not be as intuitive or significant as area, so a slightly lower weight factor can be given. Although the number is important, it may not directly reflect the severity of the defect as the area and depth of a single defect. Multiple small defects may not have as great an impact on the sample as one large defect. Therefore, in the comprehensive evaluation, a relatively low weight factor can be given to the number.
[0039] The various defect types include: air marks and bubbles, etc.
[0040] The gas lines are caused by defects on the mold surface or too fast injection speed, resulting in incomplete discharge of gas in the plastic.
[0041] The bubbles are small cavities formed when the gas inside the plastic is not completely discharged.
[0042] The specific process of obtaining the area of the air streak is as follows: in the ultrasonic signal image, the air streak appears as a continuous or dispersed low-grayscale area. The air streak area is separated from the background by the area selection tool in the image processing software, the number of pixels in the air streak area is calculated, and it is converted into the actual area according to the actual resolution of the image, thereby obtaining the area of the air streak.
[0043] The specific process of obtaining the depth of the air streak is: utilizing the attenuation characteristics of ultrasound to estimate the depth of the air streak by comparing the difference in signal intensity between the air streak area and the surrounding normal area. Generally, the decrease in signal intensity is proportional to the depth.
[0044] Number of air streaks: In the ultrasonic signal image, all identified air streak areas are counted through the automatic counting function of the image processing software to obtain the number of air streaks.
[0045] Area of bubbles: Bubbles usually appear as low-grayscale circular or elliptical areas in ultrasonic signal images. The bubble area is defined by the circular or elliptical fitting algorithm in the image processing software, and the number of pixels in the fitting area is calculated and then converted into the actual area to obtain the area of the bubble.
[0046] Depth of bubbles: The depth of bubbles is calculated by emitting ultrasonic waves and measuring the time difference from emission to reflection from the bubble interface (i.e., echo time), and then extracting the sound velocity of the washing machine injection molded part shell from the database.
[0047] Number of bubbles: All bubble areas identified in the image are automatically counted by image processing software to obtain the number of bubbles.
[0048] See also Figure 2 As shown, further, the analysis of the matching strength index of the connected samples includes: A1, fixing a plurality of connected samples, and performing a tensile test on the connecting parts of the fixed samples.
[0049] A2. Gradually apply tension to multiple connected samples in the tension test by using a tension tester until the connecting parts of the multiple connected samples in the tension test fall off, observe and record the tension values and the corresponding deformation lengths of the connecting parts when the connecting parts of the multiple connected samples fall off, and select the minimum tension value and the maximum deformation length when the connecting parts of the connected samples fall off, and use them as the tension value and deformation length when the connecting parts of the connected samples fall off, respectively. and .
[0050] A3. Analyze the matching strength index of the connected samples .
[0051] The analysis of the combined strength index of the sample after connection The specific process is: ,in and They respectively represent the allowable tensile force value and allowable deformation length of the connection part of the injection molded shell of the washing machine. and They represent the weight factors corresponding to the tensile deviation value and deformation length deviation value of the injection molded shell of the washing machine, respectively, and .
[0052] As a preferred embodiment, the and They can be set to 0.7 and 0.3 respectively. The tensile deviation value is directly related to the stability and durability of the injection molded part shell when subjected to external force. If the tensile deviation value is too large, the shell may become loose or fall off during long-term use, seriously affecting the overall performance and safety of the product. The deformation length deviation value reflects the degree of deformation of the injection molded part shell when subjected to force. Although the deformation length is also an important indicator for evaluating the performance of the shell, its direct impact may be slightly smaller than the tensile deviation value. A large deformation length deviation value may cause the shell shape to change, affecting the appearance and sealing, but it usually does not directly cause the shell to fall off or fail. Therefore, the weight corresponding to the tensile deviation value of the injection molded part shell of the washing machine is greater than the weight factor corresponding to the deformation length deviation value.
[0053] See also Figure 3 As shown, further, the analysis of the performance fluctuation index of the connected samples includes: B1, performing vibration tests on multiple connected samples according to preset vibration frequency, amplitude and duration, and collecting the displacement of the connecting parts of the multiple connected samples and the acceleration at each monitoring time point.
[0054] B2. The maximum displacement of the connector of the connected sample is selected from the displacements of the multiple connected samples, and is taken as the displacement of the connector of the connected sample, denoted as .
[0055] B3. Substitute the acceleration of the connecting parts of the multiple connected samples at each monitoring time point into the average calculation formula to obtain the average acceleration of the connecting parts of the connected samples, and substitute it into the root mean square formula to obtain the root mean square acceleration of the connecting parts of the connected samples, which is recorded as .
[0056] B4. Analyze the performance fluctuation index of the connected samples .
[0057] The performance fluctuation index of the sample after the analysis connection The specific process is: ,in and They represent the allowable displacement and the allowable acceleration root mean square of the connector of the injection molded housing of the washing machine, respectively. and They represent the weight factors corresponding to the displacement deviation value and the root mean square acceleration deviation value of the connector of the injection molded housing of the washing machine, respectively, and .
[0058] As a preferred embodiment, the and They can be set to 0.6 and 0.4 respectively. Displacement is an important parameter to measure the position change of the sample when it is subjected to force or vibration. It directly reflects the rigidity and stability of the sample. The root mean square acceleration is an indicator to measure the vibration intensity of the sample. It reflects the stability of the sample in a dynamic environment. Therefore, the weight factor corresponding to the displacement of the sample after connection is greater than the weight factor corresponding to the root mean square acceleration.
[0059] The specific process of collecting the displacement of the connecting parts of multiple connected samples and the acceleration at each monitoring time point is: collecting the displacement of the connecting parts of multiple connected samples through a displacement sensor; collecting the acceleration of the connecting parts of multiple connected samples at each monitoring time point through an acceleration sensor.
[0060] Further, the analysis of the bearing capacity index of the connected sample includes: gradually applying pressure values to the connecting parts of the multiple connected samples under stress test by a pressure tester, obtaining stress values at the connection positions of the multiple connected samples by a strain gauge, observing and recording the stress values when the connection positions of the multiple connected samples are deformed for the first time, and screening out the minimum stress value when the connection positions of the connected samples are deformed for the first time, and using it as the stress value of the connection position of the connected sample, recorded as .
[0061] The allowable stress value of the injection molded shell of the washing machine is extracted from the database and recorded as , analyze the load-bearing capacity index of the connected samples , .
[0062] By performing data analysis on the compressive strength and defect degree of the samples before connection, the present invention can fully understand the basic conditions of the samples before connection, so that corresponding measures can be taken in advance, such as screening out samples with insufficient compressive strength or serious defects to avoid wasting time and resources in the subsequent connection process. By analyzing the matching strength, performance fluctuation degree and bearing capacity of the samples after connection, the effect of the connection process can be accurately evaluated. The matching strength index can intuitively reflect the firmness of the connection and ensure that the connected samples can withstand the corresponding external force in actual use. The performance fluctuation degree index can help determine whether the performance of the connected samples is stable, which is crucial for application scenarios requiring high precision and high reliability. The bearing capacity index can promptly discover problems that may occur in the connection process to avoid product failure due to cracking.
[0063] S4. Sample quality warning: Based on the compressive strength index and defect index of the sample before connection, analyze the quality compliance index of the sample before connection ; Based on the matching strength index, performance fluctuation index and load-bearing capacity index of the connected samples, the quality compliance index of the connected samples is analyzed. ; Then analyze the quality compliance index of the sample to determine whether the quality of the injection molded shell of the washing machine is qualified, and then issue an early warning.
[0064] Furthermore, the specific formula for analyzing the quality compliance index of the sample before connection is: ,in and They represent the weight factors corresponding to the compressive strength index and defect degree index of the sample before connection, .
[0065] As a preferred embodiment, the and They can be set to 0.7 and 0.3 respectively. The compressive strength index reflects the ability of the sample to resist damage when subjected to external force. This is a key indicator for evaluating the structural strength and stability of the sample. The defect degree index measures the number, type and severity of defects in the sample. Defects may reduce the compressive strength and durability of the sample. Therefore, the weight factor corresponding to the compressive strength index of the sample before connection is greater than the weight factor corresponding to the defect degree index.
[0066] Furthermore, the specific formula for analyzing the quality compliance index of the sample after connection is: ,in , and They represent the weight factors corresponding to the matching strength index, performance fluctuation index and bearing capacity index of the connected samples respectively. .
[0067] As a preferred embodiment, the , and They can be set to 0.5, 0.25 and 0.25 respectively. The fit strength is the key indicator of the stability of the sample after connection. A high-strength fit means that the sample is less likely to be damaged when subjected to force. The degree of performance fluctuation reflects the stability of the sample's performance under different conditions. Smaller fluctuations mean that the sample performance is more reliable. The bearing capacity is an indicator for evaluating whether the sample is prone to cracks or fractures under force or environmental changes. Cracking will significantly reduce the strength and durability of the sample. Therefore, the weight factor corresponding to the fit strength index of the sample after connection is greater than the weight factors corresponding to the performance fluctuation index and the bearing capacity index.
[0068] Furthermore, the specific formula of the quality compliance index of the analyzed sample is: ,in and They represent the weight factors corresponding to the quality compliance index of the sample before connection and the quality compliance index of the sample after connection, and .
[0069] As a preferred embodiment, the and They can be set to 0.4 and 0.6 respectively. The quality compliance index of the sample before connection reflects the quality control level of raw materials, initial design and manufacturing process, which is the basis for ensuring the performance of the sample after connection. However, the quality compliance index of the sample after connection directly reflects the key performance indicators such as the effect of the connection process, the fitting strength of the connector, performance stability and crack resistance. Therefore, the weight factor corresponding to the quality compliance index of the sample after connection is greater than the weight factor corresponding to the quality compliance index of the sample before connection.
[0070] Furthermore, the determination of whether the quality of the injection-molded shell of the washing machine is qualified includes: comparing the quality compliance index of the sample with a preset quality compliance index threshold; if the quality compliance index of the sample is less than the preset quality compliance index threshold, the quality of the injection-molded shell of the washing machine is unqualified, and an early warning is issued.
[0071] The present invention can more accurately judge whether the quality of the injection molded shell of the washing machine is qualified by comprehensively measuring the quality compliance index of the samples before and after connection. Compared with a single-stage evaluation, this multi-stage analysis takes more factors into consideration, reduces the possibility of misjudgment, and improves the accuracy of quality judgment. In addition, the early warning function can send a signal at an early stage when quality problems occur, so that the production enterprise can take timely measures to intervene, which helps to avoid further deterioration of quality problems and reduce losses.
[0072] The above contents are merely examples and explanations of the concept of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the concept of the invention or exceed the scope defined by the present invention, they shall all fall within the protection scope of the present invention.
Claims
1. A method for testing the connection strength of a washing machine injection molded part housing, characterized in that: The method includes: S1. Sample grouping test: Randomly select multiple samples from the produced washing machine injection molded parts shell for testing, and group the multiple samples for compressive strength test, ultrasonic test, tensile test, vibration test and stress test; S2. Test data collection before connection: obtain the compressive strength data of the sample before connection through compressive strength test; obtain the defect degree data of the sample before connection through ultrasonic test; S3. Post-connection test data collection: multiple samples of the tensile test, vibration test and stress test are connected to the preset connecting parts at the connection position to obtain multiple connected samples, and the matching strength data of the connected samples are obtained through the tensile test; the performance fluctuation data of the connected samples are obtained through the vibration test; and the stress test data of the connected samples are obtained through the stress test; S4. Test data analysis: Analyze the compressive strength index of the sample before connection through the compressive strength data of the sample before connection ; Analyze the defect degree index of the sample before connection through the defect degree data of the sample before connection ; Analyze the matching strength index of the connected samples through the matching strength data of the connected samples ; Analyze the performance fluctuation index of the connected samples through the performance fluctuation data of the connected samples ; Analyze the load-bearing capacity index of the connected sample through the stress test data of the connected sample ; S5. Sample quality warning: Based on the compressive strength index and defect index of the sample before connection, analyze the quality compliance index of the sample before connection ; Based on the matching strength index, performance fluctuation index and load-bearing capacity index of the connected samples, the quality compliance index of the connected samples is analyzed. ; Then analyze the quality compliance index of the sample to determine whether the quality of the injection molded shell of the washing machine is qualified, and then issue an early warning.
2. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The compressive strength index of the sample before analysis of connection includes: A target test surface is selected from each surface of the sample before connection, and the target test surface and the surface opposite to the target test surface are used as opposite surfaces to obtain the opposite surface of the sample before connection, and further obtain the opposite surfaces of multiple samples before connection; gradually applying pressure to the center positions of the opposite surfaces of the plurality of pre-connected samples in the compressive strength test by means of a pressure-applying device until cracks first appear on the plurality of pre-connected samples in the compressive strength test, observing and recording the pressure values when cracks first appear on the plurality of pre-connected samples, and screening out the minimum pressure value when cracks first appear on the pre-connected samples; The contact area between the pressure device and the sample before connection is extracted from the database, and the minimum pressure value when the sample before connection first cracks is divided by the contact area between the pressure device and the sample before connection to obtain the compressive strength value of the sample, which is recorded as ; Extract the standard compressive strength value of the injection-molded housing of the washing machine from the database; Analyze the compressive strength index of the sample before connection , ,in Indicates the standard compressive strength value of the injection molded shell of the washing machine.
3. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The defect degree index of the sample before analysis and connection includes: Scanning multiple samples before connection in ultrasonic testing with an ultrasonic tester to obtain ultrasonic signal images of the multiple samples before connection in ultrasonic testing, and extracting the area, depth and quantity of each defect type of the multiple samples before connection; Substitute the areas of each defect type of multiple samples before connection into the average calculation formula to obtain the areas of each defect type of the samples before connection, recorded as ,in Indicates The number corresponding to the defect type, ; According to the analysis method of the area of each defect type of the sample before connection, the depth and number of each defect type of the sample before connection are obtained in the same way, which are recorded as and ; Analyze the defect index of the sample before joining , ,in , and Respectively represent the first The allowable area, allowable depth and allowable number of each defect type, , and The weight factors corresponding to the area deviation value, depth deviation value and number deviation value of the defect type of the injection molded shell of the washing machine are represented respectively, and .
4. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The analysis of the matching strength index of the connected sample includes: A1. Fix multiple connected samples and perform tensile test on the connecting parts of the fixed samples; A2. Gradually apply tension to multiple connected samples in the tension test by using a tension tester until the connecting parts of the multiple connected samples in the tension test fall off, observe and record the tension values and the corresponding deformation lengths of the connecting parts when the connecting parts of the multiple connected samples fall off, and select the minimum tension value and the maximum deformation length when the connecting parts of the connected samples fall off, and use them as the tension value and deformation length when the connecting parts of the connected samples fall off, respectively. and ; A3. Analyze the matching strength index of the connected samples , ,in and They respectively represent the allowable tensile force value and allowable deformation length of the connection part of the injection molded shell of the washing machine. and They represent the weight factors corresponding to the tensile deviation value and deformation length deviation value of the injection molded shell of the washing machine, respectively, and .
5. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The performance fluctuation index of the sample after the analysis connection includes: B1. Perform vibration tests on multiple connected samples according to preset vibration frequency, amplitude and duration, and collect the displacement of the connecting parts of the multiple connected samples and the acceleration at each monitoring time point; B2. The maximum displacement of the connector of the connected sample is selected from the displacements of the multiple connected samples, and is taken as the displacement of the connector of the connected sample, denoted as ; B3. Substitute the acceleration of the connecting parts of the multiple connected samples at each monitoring time point into the average calculation formula to obtain the average acceleration of the connecting parts of the connected samples, and substitute it into the root mean square formula to obtain the root mean square acceleration of the connecting parts of the connected samples, which is recorded as ; B4. Analyze the performance fluctuation index of the connected samples , ,in and They represent the allowable displacement and the allowable acceleration root mean square of the connector of the injection molded housing of the washing machine, respectively. and They represent the weight factors corresponding to the displacement deviation value and the root mean square acceleration deviation value of the connector of the injection molded housing of the washing machine, respectively, and .
6. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The load-bearing capacity index of the sample after analysis of connection includes: The pressure tester is used to gradually apply pressure values to the connectors of the multiple connected samples of the stress test, and the stress values of the connection positions of the multiple connected samples are obtained by the strain gauge. The stress values of the connection positions of the multiple connected samples when deformation occurs for the first time are observed and recorded, and the minimum stress value when deformation occurs for the first time at the connection positions of the connected samples is selected and used as the stress value of the connection position of the connected samples, recorded as ; The allowable stress value of the injection molded shell of the washing machine is extracted from the database and recorded as , analyze the load-bearing capacity index of the connected samples , .
7. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The specific formula for the quality compliance index of the sample before the analysis connection is: ,in and They represent the weight factors corresponding to the compressive strength index and defect degree index of the sample before connection, .
8. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The specific formula for the quality compliance index of the sample after analysis is: ,in , and They represent the weight factors corresponding to the matching strength index, performance fluctuation index and bearing capacity index of the connected samples respectively. .
9. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The specific formula of the quality compliance index of the analyzed sample is: ,in and They represent the weight factors corresponding to the quality compliance index of the sample before connection and the quality compliance index of the sample after connection, and .
10. A method for detecting the connection strength of a washing machine injection molded part housing according to claim 1, characterized in that: The method of judging whether the quality of the injection molded shell of the washing machine is qualified comprises: The quality compliance index of the sample is compared with the preset quality compliance index threshold. If the quality compliance index of the sample is less than the preset quality compliance index threshold, the quality of the injection molded shell of the washing machine is unqualified, and an early warning is issued.
Citation Information
Patent Citations
Method for cleaning and detecting quality of injection molded part
CN116475149A
High-precision finished product detection equipment for household appliance injection molding parts
CN117268727A
Compression resistance detection device and detection process for polymer injection molded part
CN117705557A
Diode aging resistance test method
CN118566687A
Device for detecting impact resistance of injection molded part
CN216350095U