Preparation method and system for isolated mineral insulated flexible cable

By using automatic detection and parameter adjustment technology in the isolation mineral insulated flexible cable preparation system, the problems of frequent replacement of copper tape reels and poor welding quality are solved, and seamless continuous production and efficient welding are achieved.

CN118983152AActive Publication Date: 2024-11-19WENZHOU WEIERYING NEW MATERIAL CABLE CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202411219949.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-02
Publication Date
2024-11-19
Estimated Expiration
2044-09-02

AI Technical Summary

Technical Problem

During the preparation of isolated mineral insulated flexible cables, copper tape reels need to be replaced frequently, resulting in production shutdowns and poor welding quality.

Method used

The system is adopted that includes copper belt conveying modules, photodetectors, welding modules, welding detection components, storage modules and processing modules to automatically detect the usage status of copper belts, adjust the conveying speed and welding parameters, and ensure seamless and continuous production and welding quality.

Benefits of technology

It realizes continuous production without shutdown, improves the consistency and production efficiency of welding quality, and reduces production costs and material waste.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983152A_ABST
    Figure CN118983152A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of insulated flexible cables, and discloses a preparation method and system for an isolated mineral insulated flexible cable, and the preparation system comprises a copper strip conveying module, a conveying vehicle, and a photoelectric detector. A welding module; welding the detection assembly; a storage module; the processing module is configured to adjust the moving speed of an assembly line bearing the copper strip when the photoelectric detector judges that the copper strip is used up, similarity comparison is carried out according to an unwelded image and each historical pre-welding image, and a historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity serves as an initial welding parameter combination; the processing module is further configured to perform first-stage adjustment and second-stage adjustment; and a control module. By means of automatic detection, intelligent adjustment, continuous production and the like, the production efficiency and the product quality of the isolated mineral insulated flexible cable are remarkably improved, meanwhile, the production cost is reduced, and efficient production of long-distance cables is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of insulated flexible cables, and in particular to a preparation method and system for isolated mineral insulated flexible cables. Background Art

[0002] When producing isolated mineral insulated flexible cables, it is necessary to wrap a copper tape reel on the surface of the copper core to form a copper sheath isolation layer for isolation. However, the length of the copper tape reel is limited. Whenever the cable is produced to the kilometer level, the copper tape reel needs to be replaced. At this time, it is necessary to stop the machine for replacement, and manually weld the connection between the newly replaced copper tape reel and the original copper tape reel. This step not only reduces production efficiency and fails to meet the unlimited length production requirements; in the welding process, due to inappropriate welding parameters, the welding quality of the connection is poor.

[0003] In order to improve product quality, reduce production costs and realize mass automated production, it is particularly important to study a process for continuously preparing isolated mineral insulated flexible cables without stopping the machine. Summary of the invention

[0004] In view of this, the present invention proposes a preparation method and system for an isolated mineral insulated flexible cable, aiming to solve the problem in the current technology that the copper strip reel needs to be constantly replaced and the welding quality at the connection between the new and old copper strip reels is poor.

[0005] On the one hand, the present invention provides a preparation system for an isolated mineral insulated flexible cable, comprising:

[0006] A copper belt conveying module, comprising a conveying vehicle for placing a copper belt reel and a photoelectric detector for detecting the use status of the copper belt;

[0007] A welding module is configured to weld the connection of the copper sheath isolation layer formed by two copper tape reels;

[0008] A welding detection component is configured to collect real-time welding temperature, weld width, object contrast, unwelded images, and welding end images during the welding process;

[0009] A storage module is configured to store grayscaled historical pre-welding images and historical welding end images and corresponding historical welding parameter combinations, and the storage module also stores a standard object contrast of a standard welded part;

[0010] The processing module is configured to adjust the moving speed of the assembly line carrying the copper strip when the photoelectric detector determines that the copper strip is exhausted, compare the similarity between the unwelded image and each of the historical pre-welding images, and use the historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity as the initial welding parameter combination; the initial welding parameter combination includes: an initial welding speed and an initial welding voltage;

[0011] The processing module is further configured to, when welding is started with the initial welding parameter combination, perform a primary adjustment on the real-time welding temperature according to the real-time object contrast during welding; and perform a secondary adjustment according to the difference between the historical welding end image and the welding end image;

[0012] a control module configured to control welding parameters of the welding process according to the instructions of the processing module;

[0013] The photoelectric detector is arranged between the conveying vehicle and the welding module, and the laser beam output end and the receiving end of the photoelectric detector are respectively located on both sides of the copper belt. When the copper belt is exhausted, the receiving end of the photoelectric detector detects the laser signal, and the copper belt conveying module determines that the copper belt usage status is exhausted.

[0014] Furthermore, when the photoelectric detector determines that the copper strip is exhausted, the processing module obtains the distance between the straight line where the laser signal is located and the copper strip on the next transport vehicle, pre-sets the copper strip docking time, and the adjusted assembly line moving speed satisfies the following relationship:

[0015] ;

[0016] Wherein, V is the adjusted moving speed of the assembly line; v is the average moving speed of the transport vehicle; a is the spacing distance, and t is the pre-set copper strip docking time;

[0017] The photoelectric detector starts timing after determining that the copper strip is exhausted. When the copper strip docking time is met, the welding module is set to move along the moving direction of the assembly line and start welding.

[0018] Further, when the similarity comparison is performed between the unwelded image and each of the historical pre-welding images, and an initial welding parameter combination is determined, it includes:

[0019] The unwelded image is grayed and denoised, and the unwelded image and the historical pre-welding image are selected for feature extraction based on the ORB algorithm, wherein the initial maximum number of feature points in the feature extraction is 500, the scale factor is 1.2, and the number of pyramid layers is 8;

[0020] Perform feature matching on the unwelded image and the feature descriptors obtained by the ORB algorithm of the historical pre-welded image, wherein the feature matching adopts a brute force matching algorithm, measures the similarity between the feature descriptors according to the Hamming distance, pre-sets a distance threshold, and regards the matches below the distance threshold as valid matches;

[0021] The similarity satisfies the following relationship:

[0022] ;

[0023] Wherein, S is the similarity, n is the matching point that satisfies the distance threshold, N1 is the number of feature points of the unwelded image, N2 is the number of feature points of the historical image before welding, and min (A, B) means selecting the smaller value of A and B;

[0024] When obtaining the similarity of each of the historical pre-welding images, the processing module is further configured to: sort all the historical pre-welding images according to the magnitude relationship of each similarity;

[0025] The historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity is selected as the initial welding parameter combination.

[0026] Furthermore, after the welding process is finished, the processing module determines whether to discard the pre-welding image and the welding end image and the corresponding welding parameter combination:

[0027] The welding detection component obtains the real-time object contrast of the welding area, and the processing module pre-sets a contrast threshold and compares it with the real-time object contrast;

[0028] When the real-time object contrast is less than or equal to the contrast threshold, the storage module stores the welding end image as a historical welding end image and stores the corresponding historical welding parameter combination; when the real-time object contrast is greater than the contrast threshold, the storage module does not store the welding end image and the welding parameter combination;

[0029] The contrast threshold is 0.7-1.1 times the contrast of the standard object.

[0030] Further, the real-time welding temperature is adjusted in one level according to the real-time object contrast during the welding process, including:

[0031] The real-time welding temperature during the welding process is obtained, and the real-time welding temperature is adjusted in a first level according to the difference between the standard object contrast and the real-time object contrast to obtain a first-level temperature adjustment value, and the first-level temperature adjustment value satisfies the following relationship:

[0032] ;

[0033] Wherein, T1 is the primary temperature adjustment value, k1 is the contrast difference adjustment coefficient, C0 is the standard object contrast, C1 is the real-time object contrast, k2 is the contrast change acceleration adjustment coefficient, and t is time.

[0034] Furthermore, the processing module is also configured to: When , the processing module reduces the real-time welding temperature by a first-level temperature adjustment value; when When , the processing module increases the real-time welding temperature, and the increase value is the first-level temperature adjustment value.

[0035] Furthermore, before the secondary adjustment, it also includes:

[0036] When the welding process is completed, the final object contrast obtained based on X-ray detection is obtained, and the final object contrast is compared with the standard object contrast to determine whether secondary adjustment is required;

[0037] When the difference between the final object contrast and the standard object contrast is less than or equal to ±5%, it is determined that no secondary adjustment is required;

[0038] When the difference between the final object contrast and the standard object contrast is greater than 5%, it is determined that a secondary adjustment is required.

[0039] Furthermore, when making secondary adjustments, it includes:

[0040] The weld width and the historical weld width are obtained according to the welding end image and the historical welding end image, and the initial welding speed is adjusted according to the relationship between the weld width and the historical weld width to obtain the adjusted welding speed and satisfy the following relationship:

[0041] ;

[0042] Among them, V2 is the adjusted welding speed, V0 is the initial welding speed, W0 is the historical weld width, W2 is the weld width, α=0.1, β=0.05.

[0043] Furthermore, when making secondary adjustments, it also includes:

[0044] According to the difference between the final object contrast and the standard object contrast, the initial welding voltage is adjusted to obtain an adjusted welding voltage that satisfies the following relationship:

[0045] ;

[0046] Among them, U2 is the adjusted welding voltage, U0 is the initial welding voltage, kD is the welding voltage adjustment coefficient, C2 is the final object contrast, and C0 is the standard object contrast.

[0047] On the other hand, the present invention also proposes a method for applying to the above-mentioned system for preparing an isolated mineral insulated flexible cable, the method comprising:

[0048] When the photoelectric detector determines that the copper strip is exhausted, the moving speed of the assembly line carrying the copper strip is adjusted, and the similarity between the unwelded image and each historical pre-welding image is compared, and the historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity is used as the initial welding parameter combination;

[0049] When welding is started with the initial welding parameter combination, the real-time welding temperature is adjusted in the first level according to the real-time object contrast during welding; the second level is adjusted according to the difference between the historical welding end image and the welding end image;

[0050] The photoelectric detector is arranged between the conveyor vehicle and the welding area, and the laser beam output end and the receiving end of the photoelectric detector are respectively located on both sides of the copper belt. When the copper belt is exhausted, the receiving end of the photoelectric detector detects the laser signal and determines that the copper belt is in an exhausted state.

[0051] Compared with the prior art, the present invention has the following beneficial effects:

[0052] The traditional process requires stopping the machine to replace the copper tape reel when the copper tape reel is exhausted, which not only interrupts the production process but also reduces the overall production efficiency. Through the copper tape conveying module and photoelectric detector in this system, the copper tape usage status can be automatically detected, and the conveying speed can be automatically adjusted when the copper tape is exhausted without stopping, thereby achieving the continuity of production and improving efficiency. Through the welding detection component and processing module in this system, real-time data in the welding process, such as welding temperature, weld width and object contrast, can be automatically collected and analyzed, and welding parameters can be automatically adjusted. This eliminates the need for manual intervention, ensures the consistency and stability of welding quality, and makes large-scale automated production possible. This system automatically selects the best initial welding parameter combination by comparing the similarity between the historical pre-welding image and the unwelded image, and performs primary and secondary adjustments according to real-time data during the welding process. This intelligent adjustment method can effectively deal with the problem of poor welding quality caused by inappropriate welding parameters, ensure that the welding quality of the joint meets the requirements, and thus improve the overall quality of the product. By improving production efficiency and automation, this system reduces downtime and manual intervention, thereby reducing production costs. In addition, the optimized welding quality reduces rework and scrap rates, further reducing material and labor costs. In traditional processes, the length of the copper tape reel is limited, and the machine needs to be stopped and replaced whenever the copper tape is exhausted, which makes it impossible to achieve unlimited length production. Through the copper tape conveying module and photoelectric detector of this system, the copper tape reel can be replaced without stopping production, realizing the continuous production of unlimited length cables and meeting the production needs of long-distance cables. The storage module and processing module of this system support the storage and analysis of historical welding data, and realize intelligent welding parameter adjustment by comparing with real-time data. This data-driven welding method not only improves the accuracy of production, but also provides reliable data support for subsequent process optimization. BRIEF DESCRIPTION OF THE DRAWINGS

[0053] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:

[0054] Figure 1 A simplified diagram of the copper strip welding process of a manufacturing system for an isolated mineral insulated flexible cable according to an embodiment of the present invention;

[0055] Figure 2 The present invention is a functional block diagram of a system for preparing an isolated mineral insulated flexible cable according to an embodiment of the present invention.

[0056] In the figure, 1, copper strip; 21, first transport vehicle; 22, second transport vehicle; 31, photoelectric detector transmitting end; 32, photoelectric detector receiving end; 4, welding module. DETAILED DESCRIPTION

[0057] Exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art. It should be noted that, in the absence of conflict, the embodiments of the present invention and the features described in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0058] Figure 1 This is a simplified diagram of the copper strip welding process of the preparation system according to an embodiment of the present invention, and not all structures of the preparation system are shown in the figure. Figure 1 (A) is the normal working state of the assembly line. At this time, the first transport vehicle 21 transports the copper strip 1 along the moving direction of the assembly line; the second transport vehicle 22 is on standby right behind the first transport vehicle 21, and the laser beam emitted by the photodetector transmitting end 31 is blocked by the copper strip 1 and cannot be captured by the photodetector receiving end 32; the welding module 4 is in standby state; Figure 1 (B) is the working state when the copper strip 1 on the first transport vehicle 21 is exhausted. When the copper strip 1 on the first transport vehicle 21 is exhausted, the copper strip 1 cannot block the laser beam, and the photoelectric detector receiving end 32 can receive the laser signal. The system determines that the use state of the copper strip 1 is the exhaustion state. At this time, the first transport vehicle 21 moves backward, and the second transport vehicle 22 moves forward and replaces the position of the original first transport vehicle 21. In order to facilitate the second transport vehicle to reach the target position as soon as possible and facilitate the welding process, the moving speed of the assembly line decreases. a is the interval distance from the straight line where the laser signal is located to the copper strip on the next transport vehicle; the welding module 4, the copper strip 1, and the assembly line move at the same speed and in the same direction and start the welding process; Figure 1 (C) is a schematic diagram of the copper strip welding process of the preparation system of an embodiment of the present invention.

[0059] See also Figure 2 As shown, an embodiment of the present invention provides a system for preparing an isolated mineral insulated flexible cable, comprising:

[0060] A copper belt conveying module, comprising a conveying vehicle for placing a copper belt reel and a photoelectric detector for detecting the use status of the copper belt;

[0061] A welding module is configured to weld the connection of the copper sheath isolation layer formed by two copper tape reels;

[0062] A welding detection component is configured to collect real-time welding temperature, weld width, object contrast, unwelded images and welded end images during the welding process;

[0063] A storage module is configured to store grayscaled historical pre-welding images and historical welding end images and corresponding historical welding parameter combinations, and the storage module also stores standard object contrast of standard welded parts;

[0064] The processing module is configured to adjust the moving speed of the assembly line carrying the copper strip when the photoelectric detector determines that the copper strip is exhausted, compare the similarity between the unwelded image and each historical pre-welding image, and use the historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity as the initial welding parameter combination; the initial welding parameter combination includes: an initial welding speed and an initial welding voltage;

[0065] The processing module is further configured to make a primary adjustment to the real-time welding temperature according to the real-time object contrast during welding when welding is started with the initial welding parameter combination, and a secondary adjustment according to the difference between the historical welding end image and the welding end image;

[0066] a control module configured to control welding parameters of the welding process according to the instructions of the processing module;

[0067] Among them, the photoelectric detector is arranged between the conveyor vehicle and the welding module, and the laser beam output end and the receiving end of the photoelectric detector are respectively located on both sides of the copper belt. When the copper belt is exhausted, the receiving end of the photoelectric detector detects the laser signal, and the copper belt conveying module determines that the copper belt usage status is exhausted.

[0068] It should be noted that, in this embodiment, the transport vehicle at least includes: a first transport vehicle 21 and a second transport vehicle 22 .

[0069] By introducing an automated detection and adjustment module, the continuity and efficiency of the production process are achieved. The system automatically adjusts the line speed without stopping when the copper strip is exhausted, and intelligently selects the best welding parameter combination based on historical welding data. During the welding process, precise adjustments are made by real-time monitoring of welding temperature and object contrast, thereby improving welding quality and reducing human intervention and errors. This not only improves production efficiency and product quality, but also significantly reduces production costs and supports large-scale automated production.

[0070] In some embodiments of the present application, when the photoelectric detector determines that the copper strip is exhausted, the processing module obtains the distance between the straight line where the laser signal is located and the copper strip on the next transport vehicle, and pre-sets the copper strip docking time. The adjusted assembly line moving speed satisfies the following relationship:

[0071] ;

[0072] Among them, V is the adjusted moving speed of the assembly line; v is the average moving speed of the transport vehicle; a is the interval distance, and t is the pre-set copper belt docking time;

[0073] The photoelectric detector starts timing after determining that the copper strip is exhausted. When the copper strip docking time is met, the welding module is set to move along the moving direction of the assembly line and start welding.

[0074] It should be noted that by adjusting the speed of the assembly line, the copper strip docking time is accurately matched, ensuring that the copper strip can be smoothly and seamlessly docked after it is exhausted, avoiding human errors, and improving the continuity and automation level of production. The system automatically adjusts the speed and prepares for welding when the copper strip is exhausted, reducing the downtime caused by copper strip replacement and improving production efficiency. By controlling the welding module to accurately follow the assembly line and start welding when the copper strip docking time arrives, the stability and consistency of the welding process are guaranteed, thereby improving the welding quality and reducing the possibility of welding defects. By setting different copper strip docking times and interval distances, the system can flexibly adjust the speed to adapt to production tasks of different specifications and requirements, improving the applicability and reliability of the system.

[0075] In some embodiments of the present application, when a similarity comparison is performed between the un-welded image and each historical pre-welding image, and an initial welding parameter combination is determined, the method includes:

[0076] The unwelded images were grayed and denoised, and the unwelded images and historical pre-welding images were selected for feature extraction based on the ORB algorithm. The initial maximum number of feature points in feature extraction was 500, the scale factor was 1.2, and the number of pyramid layers was 8.

[0077] The feature descriptors obtained by the ORB algorithm are matched between the unwelded image and the historical pre-welding image. The feature matching adopts the brute force matching algorithm, and the similarity between the feature descriptors is measured according to the Hamming distance. The distance threshold is set in advance, and the matches below the distance threshold are regarded as valid matches.

[0078] The similarity satisfies the following relationship:

[0079] ;

[0080] Among them, S is the similarity, n is the matching point that meets the distance threshold, N1 is the number of feature points of the unwelded image, N2 is the number of feature points of the historical image before welding, and min (A, B) means selecting the smaller value of A and B;

[0081] When obtaining the similarity of each historical pre-welding image, the processing module is further configured to: sort all historical pre-welding images according to the magnitude relationship of each similarity;

[0082] The historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity is selected as the initial welding parameter combination.

[0083] It should be noted that the denoising process in this embodiment adopts Gaussian filtering method.

[0084] It is understandable that by performing feature extraction and feature matching through the ORB algorithm, this method can efficiently and accurately capture the key features in the image, and accurately match the unwelded image with the historical pre-welding image, so as to select the initial parameter combination that best suits the current welding conditions and reduce the error of manually set parameters. The system can automatically adjust the initial welding parameters according to different unwelded images, making the welding process more intelligent, adapting to different production needs, and improving the automation and operation convenience of the production line. Accurate welding parameter selection can not only reduce welding defects, but also improve the stability of welding quality, thereby improving the consistency and reliability of products, reducing the defective rate in production, and further improving production efficiency. Through feature extraction and matching of the ORB algorithm, the system can complete complex image processing tasks with lower computing resource usage, so that the entire system can still work in real time under high-speed production lines.

[0085] In some embodiments of the present application, after the welding process is completed, the processing module determines whether to discard the pre-welding image and the welding end image and the corresponding welding parameter combination:

[0086] The welding detection component obtains the real-time object contrast of the welding area, and the processing module pre-sets the contrast threshold and compares it with the real-time object contrast;

[0087] When the real-time object contrast is less than or equal to the contrast threshold, the storage module stores the welding end image as a historical welding end image and stores the corresponding historical welding parameter combination; when the real-time object contrast is greater than the contrast threshold, the storage module does not store the welding end image and the welding parameter combination;

[0088] The contrast threshold is 0.7-1.1 times the contrast of the standard object.

[0089] It should be noted that, for the acquisition of real-time object contrast in the welding area: at the end of welding, the welding detection component will acquire the real-time object contrast in the welding area. Object contrast is an important indicator to measure the visual difference between the welding area and the surrounding background, and is usually used to evaluate the quality of the weld. Setting and comparison of contrast threshold: The processing module pre-sets a contrast threshold, which is set based on 0.7 to 1.1 times the standard object contrast (i.e., the contrast of an ideal welded part). This range can flexibly adapt to the micro-changes that may occur under different production conditions, ensuring that the evaluation of welding quality is neither too strict nor too loose. After the real-time object contrast is acquired, the processing module compares it with the preset contrast threshold. For the decision of storage and rejection: when the real-time object contrast is less than or equal to the preset contrast threshold, it means that the quality of this welding meets the requirements. At this time, the storage module will store the end-of-welding image of this time as a historical end-of-welding image, and at the same time store the corresponding welding parameter combination. If the real-time object contrast is greater than the preset contrast threshold, it means that the welding quality is not ideal or there are defects. In order to prevent the low-quality welding parameter combination from affecting the future welding process, the system will not save the end-of-welding image and its corresponding welding parameter combination.

[0090] By comparing the real-time contrast with the preset contrast threshold, the system can automatically remove welding images and parameter combinations that do not meet the quality standards. This ensures that the data in the historical welding parameter library are of high quality, thereby improving the consistency of welding quality in future welding processes. The system only retains those welding parameter combinations that have passed the quality assessment, so that the welding parameter library can be continuously optimized, and those parameters that may cause welding defects can be eliminated, thereby improving the overall welding efficiency and quality of the production line. By eliminating parameter combinations of low-quality welding, the system effectively reduces the defective rate caused by inappropriate welding parameters, thereby improving the qualified rate of products and reducing rework and scrap losses in production. The set contrast threshold range (0.7 to 1.1 times the standard object contrast) gives the system a certain degree of flexibility, allowing the system to adapt to different production environments and material differences without being too rigid or too loose in evaluating welding quality. By filtering out welding data that does not meet the requirements, the system reduces the storage of useless data, saves storage space, and improves the efficiency and accuracy of data processing. This also provides a more reliable data basis for subsequent welding parameter selection and optimization.

[0091] In some embodiments of the present application, the real-time welding temperature is adjusted in one level according to the real-time object contrast during the welding process, including:

[0092] The real-time welding temperature during the welding process is obtained, and the real-time welding temperature is adjusted in one level according to the difference between the standard object contrast and the real-time object contrast to obtain a first-level temperature adjustment value, which satisfies the following relationship:

[0093] ;

[0094] Among them, T1 is the first-level temperature adjustment value, k1 is the contrast difference adjustment coefficient, C0 is the standard object contrast, C1 is the real-time object contrast, k2 is the contrast change acceleration adjustment coefficient, and t is time.

[0095] It should be noted that the method for determining k1 is as follows:

[0096] Select a batch of representative welding conditions (porosity of welding area) to cover various situations that may occur during the production process. Set multiple welding temperatures and record the standard object contrast C0 at each temperature and the real-time object contrast C1 after actual welding. Perform welding experiments at the set welding temperature, collect the real-time object contrast C1 of each welding, record the temperature T, standard contrast C0 and real-time object contrast C1 under each experimental condition, and calculate the difference between them. .

[0097] Using the statistical method of linear regression, the contrast difference The relationship between the welding temperature adjustment value T1 is fitted to obtain a function form: k1 is the slope of the fitting equation, whose value is determined by regression analysis and represents the sensitivity of contrast difference to temperature adjustment.

[0098] The method for determining k2 is the same as k1. Replace with That's it.

[0099] It can be understood that by monitoring the difference between the object contrast and the standard contrast in real time and dynamically adjusting the welding temperature according to this difference, the system can quickly respond to and compensate for any quality fluctuations in the welding process. This adjustment mechanism can ensure the stability of the weld quality, thereby reducing the occurrence of welding defects. By introducing the contrast change acceleration adjustment coefficient (k2) and the contrast difference adjustment coefficient (k1), the system not only considers the contrast difference, but also comprehensively considers the speed and trend of the contrast change. This multi-dimensional adjustment method makes the control of the welding temperature more precise and helps to prevent quality problems caused by excessive temperature fluctuations during the welding process. The real-time welding temperature adjustment is based on the real-time data obtained during the welding process, allowing the system to provide instant feedback and make adjustments. This fast feedback mechanism enables the system to better adapt to the dynamic changes in the welding process and maintain the continuous stability of the welding quality. The adjustment mechanism adjusts the temperature in an automated manner, reducing the need for manual monitoring and intervention, and improving the automation and efficiency of the production process. At the same time, it also reduces the problem of inconsistent welding quality caused by manual operation errors. Because the adjustment mechanism takes into account the contrast difference and its changing speed, the system can maintain high consistency of welding quality under various welding conditions (such as different materials or welding speeds), with strong adaptability and robustness. By accurately controlling the welding temperature, the system can effectively reduce the defective rate in the welding process and thus improve the qualified rate of the product. This not only helps to improve production efficiency, but also reduces the cost caused by rework or waste disposal.

[0100] In some embodiments of the present application, the processing module is further configured to: When , the processing module reduces the real-time welding temperature to the first-level temperature adjustment value; when When the temperature is 0, the processing module increases the real-time welding temperature, and the increase value is the first-level temperature adjustment value.

[0101] It should be noted that the welding temperature should be adjusted in time according to the change of real-time contrast to avoid welding defects caused by too high or too low temperature, such as too wide welds, loose welding or material damage. It can automatically adapt to copper strips of different materials and thicknesses, reduce strict requirements for production conditions, and improve the flexibility of the production line. Reduce manual intervention, achieve precise welding through automatic control systems, lower the technical threshold of operators, and improve production efficiency. Through real-time adjustment of temperature, the problem of unstable welding quality caused by environmental changes or equipment fluctuations during welding can be reduced, ensuring production continuity and product consistency.

[0102] In some embodiments of the present application, before the secondary adjustment, the method further includes:

[0103] When the welding process is completed, the final object contrast obtained based on X-ray detection is obtained, and the final object contrast is compared with the standard object contrast to determine whether secondary adjustment is required;

[0104] When the difference between the final object contrast and the standard object contrast is less than or equal to ±5%, it is determined that no secondary adjustment is required;

[0105] When the difference between the final object contrast and the standard object contrast is greater than 5%, it is determined that a secondary adjustment is required.

[0106] It should be noted that after the welding process, the final object contrast is obtained using an X-ray inspection system. This contrast value reflects the actual quality of the welded joint and the internal structure of the weld. The final object contrast obtained is compared with the preset standard object contrast. The purpose of this step is to determine whether the set quality standards are met during the welding process. No secondary adjustment is required: If the difference between the final object contrast and the standard object contrast is within ±5%, the welding quality is considered to meet the standard and no secondary adjustment is required. If the difference between the final object contrast and the standard object contrast exceeds 5%, a secondary adjustment is required. This means that some parameters in the welding process may not have achieved the expected results and need to be adjusted to optimize the welding quality.

[0107] By checking the contrast of the final object after welding, it is ensured that the welded joint meets the standard. If there is a significant deviation, the secondary adjustment can correct the problem in the welding process in a targeted manner and improve the stability and reliability of the welding quality. The secondary adjustment is carried out according to the detection results of the final contrast, so that the welding process can be continuously optimized. This adjustment mechanism helps to identify and correct the deviation of welding parameters, thereby achieving more accurate welding process control. Through timely secondary adjustment, scrap caused by welding quality problems can be reduced. This reduces production costs and reduces economic losses caused by rework or scrapping of unqualified products. The system automatically determines whether secondary adjustment is required based on the contrast difference, reducing the need for manual intervention and improving the automation level of the production line. This not only improves production efficiency, but also reduces the technical requirements for operators. Secondary adjustment ensures that the contrast of the final welded product meets the standard requirements and ensures that the product can achieve the required performance and quality in actual application. This is of great significance to meet customer needs and market competitiveness. This secondary adjustment method based on contrast difference enables the system to adapt to welding requirements under different production conditions and enhances the system's adaptability and flexibility to production changes.

[0108] In some embodiments of the present application, the secondary adjustment includes:

[0109] The weld width and the historical weld width are obtained according to the welding end image and the historical welding end image, and the initial welding speed is adjusted according to the relationship between the weld width and the historical weld width to obtain the adjusted welding speed and satisfy the following relationship:

[0110] ;

[0111] Among them, V2 is the adjusted welding speed, V0 is the initial welding speed, W0 is the historical weld width, W2 is the weld width, α=0.1, β=0.05.

[0112] It should be noted that by adjusting the welding voltage to compensate for the difference between the final object contrast and the standard contrast, the welding quality can be ensured to be closer to the standard requirements. Adjusting the welding voltage allows the welding process to better adapt to the actual welding conditions, thereby improving the quality and consistency of the welded joint. This adjustment mechanism helps to respond to possible quality deviations in the welding process in real time, making the welding process more stable. By adjusting the voltage based on the contrast difference, welding defects caused by inappropriate voltage, such as uneven welds or insufficient strength, are reduced. Accurate welding voltage adjustment can reduce welding defects and reduce the probability of subsequent repairs or reprocessing. This can save time and cost and improve production efficiency. By adjusting the voltage based on the contrast difference, the system can adapt to different welding conditions and material changes. This adaptability is very important for dealing with various changes in production and improves the flexibility of the production line. By adjusting the welding voltage to deal with contrast differences during the production process, the welding quality of each batch of products can be more consistent, reducing quality fluctuations and improving the overall consistency of the final product. This adjustment mechanism reduces the need for manual intervention, improves the automation level of the production line through an automated adjustment process, reduces the technical requirements for operators, and improves production efficiency.

[0113] In some embodiments of the present application, when performing the secondary adjustment, it also includes:

[0114] According to the difference between the final object contrast and the standard object contrast, the initial welding voltage is adjusted to obtain an adjusted welding voltage that satisfies the following relationship:

[0115] ;

[0116] Among them, U2 is the adjusted welding voltage, U0 is the initial welding voltage, kD is the welding voltage adjustment coefficient, C2 is the final object contrast, and C0 is the standard object contrast.

[0117] It should be noted that by adjusting the welding voltage to compensate for the difference between the final object contrast and the standard contrast, the welding quality can be ensured to be closer to the standard requirements. Adjusting the welding voltage allows the welding process to better adapt to the actual welding conditions, thereby improving the quality and consistency of the welded joint. This adjustment mechanism helps to respond to possible quality deviations in the welding process in real time, making the welding process more stable. By adjusting the voltage based on the contrast difference, welding defects caused by inappropriate voltage, such as uneven welds or insufficient strength, are reduced. Accurate welding voltage adjustment can reduce welding defects and reduce the probability of subsequent repairs or reprocessing. This can save time and cost and improve production efficiency. By adjusting the voltage based on the contrast difference, the system can adapt to different welding conditions and material changes. This adaptability is very important for dealing with various changes in production and improves the flexibility of the production line. By adjusting the welding voltage to deal with contrast differences during the production process, the welding quality of each batch of products can be more consistent, reducing quality fluctuations and improving the overall consistency of the final product. This adjustment mechanism reduces the need for manual intervention, improves the automation level of the production line through an automated adjustment process, reduces the technical requirements for operators, and improves production efficiency.

[0118] See also Figure 2 As shown, an embodiment of the present invention also provides a method for preparing an isolated mineral insulated flexible cable, comprising:

[0119] When the photoelectric detector determines that the copper strip is exhausted, the moving speed of the assembly line carrying the copper strip is adjusted, and the similarity between the unwelded image and each historical pre-welding image is compared, and the historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity is used as the initial welding parameter combination;

[0120] When welding is started with the initial welding parameter combination, the real-time welding temperature is adjusted in the first level according to the real-time object contrast during welding; the second level is adjusted according to the difference between the historical welding end image and the welding end image;

[0121] The photoelectric detector is arranged between the conveyor vehicle and the welding area, and the laser beam output end and the receiving end of the photoelectric detector are respectively located on both sides of the copper belt. When the copper belt is exhausted, the receiving end of the photoelectric detector detects the laser signal and determines that the copper belt is in an exhausted state.

[0122] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in the relevant field should understand that the specific implementation methods of the present invention can still be modified or replaced by equivalents. Any modification or equivalent replacement that does not depart from the spirit and scope of the present invention should be covered within the scope of protection of the claims of the present invention.

Claims

1. A preparation system for an isolated mineral insulated flexible cable, characterized in that: include: A copper belt conveying module, comprising a conveying vehicle for placing a copper belt reel and a photoelectric detector for detecting the use status of the copper belt; A welding module is configured to weld the connection of the copper sheath isolation layer formed by two copper tape reels; A welding detection component is configured to collect real-time welding temperature, weld width, object contrast, unwelded images and welded end images during the welding process; A storage module is configured to store grayscaled historical pre-welding images and historical welding end images and corresponding historical welding parameter combinations, and the storage module also stores a standard object contrast of a standard welded part; The processing module is configured to adjust the moving speed of the assembly line carrying the copper strip when the photoelectric detector determines that the copper strip is exhausted, compare the similarity between the unwelded image and each of the historical pre-welding images, and use the historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity as the initial welding parameter combination; the initial welding parameter combination includes: an initial welding speed and an initial welding voltage; The processing module is further configured to, when welding is started with the initial welding parameter combination, perform a primary adjustment on the real-time welding temperature according to the real-time object contrast during welding; and perform a secondary adjustment according to the difference between the historical welding end image and the welding end image; a control module configured to control welding parameters of the welding process according to the instructions of the processing module; The photoelectric detector is arranged between the conveying vehicle and the welding module, and the laser beam output end and the receiving end of the photoelectric detector are respectively located on both sides of the copper belt. When the copper belt is exhausted, the receiving end of the photoelectric detector detects the laser signal, and the copper belt conveying module determines that the copper belt usage status is exhausted.

2. The preparation system for isolated mineral insulated flexible cables according to claim 1, characterized in that: When the photoelectric detector determines that the copper strip is exhausted, the processing module obtains the distance between the straight line where the laser signal is located and the copper strip on the next transport vehicle, and pre-sets the copper strip docking time. The adjusted assembly line moving speed satisfies the following relationship: ; Wherein, V is the adjusted moving speed of the assembly line; v is the average moving speed of the transport vehicle; a is the spacing distance, and t is the pre-set copper strip docking time; The photoelectric detector starts timing after determining that the copper strip is exhausted. When the copper strip docking time is met, the welding module is set to move along the moving direction of the assembly line and start welding.

3. The preparation system for isolated mineral insulated flexible cables according to claim 1, characterized in that: When the similarity comparison is performed between the unwelded image and each of the historical pre-welding images, and an initial welding parameter combination is determined, the method includes: The unwelded image is grayed and denoised, and the unwelded image and the historical pre-welding image are selected for feature extraction based on the ORB algorithm, wherein the initial maximum number of feature points in the feature extraction is 500, the scale factor is 1.2, and the number of pyramid layers is 8; Perform feature matching on the unwelded image and the feature descriptors obtained by the ORB algorithm of the historical pre-welded image, wherein the feature matching adopts a brute force matching algorithm, measures the similarity between the feature descriptors according to the Hamming distance, pre-sets a distance threshold, and regards the matches below the distance threshold as valid matches; The similarity satisfies the following relationship: ; Among them, S is the similarity, n is the matching point that meets the distance threshold, N1 is the number of feature points of the unwelded image, N2 is the number of feature points of the historical image before welding, min ( , ) indicates selection and The smaller value in ; When obtaining the similarity of each of the historical pre-welding images, the processing module is further configured to: sort all the historical pre-welding images according to the magnitude relationship of each similarity; The historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity is selected as the initial welding parameter combination.

4. The preparation system for isolated mineral insulated flexible cables according to claim 3, characterized in that: The processing module determines whether to discard the pre-welding image and the welding end image and the corresponding welding parameter combination after the welding process is completed: The welding detection component obtains the real-time object contrast of the welding area, and the processing module pre-sets a contrast threshold and compares it with the real-time object contrast; When the real-time object contrast is less than or equal to the contrast threshold, the storage module stores the welding end image as a historical welding end image and stores the corresponding historical welding parameter combination; when the real-time object contrast is greater than the contrast threshold, the storage module does not store the welding end image and the welding parameter combination; The contrast threshold is 0.7-1.1 times the contrast of the standard object.

5. The preparation system for isolated mineral insulated flexible cables according to claim 4, characterized in that: One-level adjustment of real-time welding temperature based on real-time object contrast during welding, including: The real-time welding temperature during the welding process is obtained, and the real-time welding temperature is adjusted in a first level according to the difference between the standard object contrast and the real-time object contrast to obtain a first-level temperature adjustment value, and the first-level temperature adjustment value satisfies the following relationship: ; Wherein, T1 is the primary temperature adjustment value, k1 is the contrast difference adjustment coefficient, C0 is the standard object contrast, C1 is the real-time object contrast, k2 is the contrast change acceleration adjustment coefficient, and t is time.

6. The preparation system for isolated mineral insulated flexible cables according to claim 5, characterized in that: The processing module is also configured to: When , the processing module reduces the real-time welding temperature by a first-level temperature adjustment value; when When , the processing module increases the real-time welding temperature, and the increase value is the first-level temperature adjustment value.

7. The preparation system for isolated mineral insulated flexible cables according to claim 6, characterized in that: Before the secondary adjustment, it also includes: When the welding process is completed, the final object contrast obtained based on X-ray detection is obtained, and the final object contrast is compared with the standard object contrast to determine whether secondary adjustment is required; When the difference between the final object contrast and the standard object contrast is less than or equal to ±5%, it is determined that no secondary adjustment is required; When the difference between the final object contrast and the standard object contrast is greater than 5%, it is determined that a secondary adjustment is required.

8. The preparation system for isolated mineral insulated flexible cables according to claim 7, characterized in that: When making secondary adjustments, it includes: The weld width and the historical weld width are obtained according to the welding end image and the historical welding end image, and the initial welding speed is adjusted according to the relationship between the weld width and the historical weld width to obtain the adjusted welding speed and satisfy the following relationship: ; Among them, V2 is the adjusted welding speed, V0 is the initial welding speed, W0 is the historical weld width, W2 is the weld width, α=0.1, β=0.

05.

9. The preparation system for isolated mineral insulated flexible cables according to claim 8, characterized in that: When making secondary adjustments, it also includes: According to the difference between the final object contrast and the standard object contrast, the initial welding voltage is adjusted to obtain an adjusted welding voltage that satisfies the following relationship: ; Among them, U2 is the adjusted welding voltage, U0 is the initial welding voltage, k D is the welding voltage adjustment coefficient, C2 is the final object contrast, and C0 is the standard object contrast.

10. A method for preparing an isolated mineral insulated flexible cable, applied to the preparation system for an isolated mineral insulated flexible cable according to any one of claims 1 to 9, characterized in that: include: When the photoelectric detector determines that the copper strip is exhausted, the moving speed of the assembly line carrying the copper strip is adjusted, and the similarity between the unwelded image and each historical pre-welding image is compared, and the historical welding parameter combination corresponding to the historical pre-welding image with the highest similarity is used as the initial welding parameter combination; When welding is started with the initial welding parameter combination, the real-time welding temperature is adjusted in the first level according to the real-time object contrast during welding; the second level is adjusted according to the difference between the historical welding end image and the welding end image; The photoelectric detector is arranged between the conveyor vehicle and the welding area, and the laser beam output end and the receiving end of the photoelectric detector are respectively located on both sides of the copper belt. When the copper belt is exhausted, the receiving end of the photoelectric detector detects the laser signal and determines that the copper belt is in an exhausted state.

Citation Information

Patent Citations

  • Method for operating a stringer and stringer

    CN102640302A

  • Welding joint morphology monitoring method, system and device and readable storage medium

    CN111157539A

  • Vehicle-mounted image splicing method, system and device

    CN112308987A

  • Automatic welding machine based on machine vision and control method thereof

    CN112935473A

  • CCD alignment pulse thermocompression welding system

    CN113441809A