PCBA full-automatic production method
Through fully automated production methods, including multiple automation steps, replacing manual operations, the problem that the semi-automated model of the PCBA manufacturing industry cannot meet the industry needs is solved, efficient and high-quality unmanned intelligent production is achieved, and market competitiveness is enhanced.
Patent Information
- Application Number
- CN202411061284.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-19
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing PCBA manufacturing industry still adopts a semi-automated + manual production process model, which cannot meet the trend of global labor population shrinking, rising labor costs and market bidding pressure, and cannot achieve fully automated unmanned intelligent production.
Adopt fully automated production methods, including PCB loading, printed solder paste, QC inspection, SMT patch, reflow soldering, AOI detection, pin-type component insertion, wave soldering, pressing parts, repair soldering, ICT detection, and functional initial testing , substrate cleaning and three-proof paint coating, etc., to achieve unmanned intelligent production through automated equipment.
Effectively ensure the consistency of product output, improve product efficiency and quality, enhance cost-effectiveness, significantly improve production efficiency and quality, and improve market competitiveness.
Smart Images

Figure CN118984544A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of PCBA production, and in particular to a fully automated PCBA production process. Background Art
[0002] PCB stands for printed circuit board, also known as printed circuit board. It is an important electronic component in electronic products, a support for electronic components, and a carrier for the electrical connection of electronic components. Because it is made using electronic printing technology, it is called a "printed" circuit board. It is abbreviated as PCBA, which can also be understood as a bare board, and a processed PCBA board is a finished electronic board.
[0003] The process of transforming PCB into PCBA requires dozens of processing steps to be completed.
[0005] However, the current PCBA manufacturing industry is still generally following the PSPP semi-automatic + manual production process model of the 3rd Industrial Revolution. Under the general trend of shrinking global labor force, rising labor costs, and lower product market bidding, the PSPP semi-automatic + manual production process model can no longer meet the needs of the industry. Therefore, existing equipment and methods continue to be upgraded and optimized to achieve fully automated unmanned intelligent production. Summary of the invention
[0006] In order to solve the above technical problems, a fully automated PCBA production method with fully automated unmanned intelligent production is proposed.
[0007] To achieve the above object, the technical solution adopted by the present invention is as follows: a fully automated PCBA production method, characterized in that it includes the following steps:
[0008] PCB loading step: place the PCB to be assembled in the predetermined position;
[0009] Printing solder paste steps: print the solder paste evenly on the pad position of the PCB board;
[0010] QC inspection steps: Check the printing effect of the PCB board printed with solder paste (the inspection content includes but is not limited to the uniformity of solder paste, the presence of insufficient solder, solder bridging, pulling tip, displacement, and missing printing);
[0011] SMT patch steps: attach the surface mount components SMD to the PCB with solder paste;
[0012] Reflow soldering step: solder the mounted components on the PCB board through a reflow soldering furnace;
[0013] AOI inspection steps: Use AOI equipment to perform quality inspection on the PCB with good patching;
[0014] Insertion steps: insert the pin-type components into the corresponding positions of the PCB;
[0015] Pre-furnace inspection: Use magnification tools to inspect PCB boards and components for defects;
[0016] Wave soldering steps: solder the plug-in components on the PCB board through a wave soldering furnace;
[0017] Pressing step: Press the components firmly onto the PCB through mechanical pressure or heat pressing;
[0018] Repair welding steps: welding after the pressing is completed, repair welding operations are performed on welding defects or additional components;
[0019] ICT test steps: connect the test probe of the test equipment to the test point on the circuit board to measure the electrical characteristics of the circuit; (the test content mainly includes the detection of circuit open circuit, short circuit, resistance, capacitance, inductance, diode and transistor parameters);
[0020] Functional initial test steps: Use automatic test equipment ATE to test the various functions of the above processed circuit boards;
[0021] Substrate cleaning: clean the substrate to remove debris;
[0022] B / T surface three-proof paint: Apply three-proof paint on the B and T surfaces of the circuit board after cleaning;
[0023] Glue dispensing / IC three-proofing: Use glue dispensing equipment to apply glue to the surface of the corresponding part of the PCB board, and then apply three-proof paint.
[0024] Preferably, the operating conditions of the solder paste printing step are as follows:
[0025] 1) Lead-free solder paste should be stored at 2-10°C for ≤6 months, warmed up for 3-4 hours, stirred for 5-6 minutes, and have a viscosity of 200±20pa.s;
[0026] 2) The tension of the practical steel mesh is ≥32N.cm2;
[0027] 3) Printing machine parameter setting table:
[0028] Printing speed: 50±10mm / s;
[0029] Printing pressure: 23±5N(*0.01N);
[0030] Gap between steel mesh and substrate: -0.5±0.1mm;
[0031] Drop speed: 5.0±0.5mm / s;
[0032] Lowering stroke 3.0mm;
[0033] Demolding method: first use the scraper and then demould;
[0034] Automatic cleaning is performed every 4 prints and manual cleaning is performed every 20 prints.
[0035] Printing environment temperature: 20-26℃;
[0036] The service life of the steel mesh is ≤ 100,000 times.
[0037] Preferably, the reflow soldering step satisfies the following conditions:
[0038] 1) Furnace temperature parameter setting benchmark: heating rate 1~4℃ / s, preheating time 60~120s, preheating end 200℃, reflux temperature 245~260℃, reflux time 30~60s, cooling rate 1~5℃ / s;
[0039] 2) Service life of furnace temperature test board: ≦60 times;
[0040] 3) The width of the reflow conveyor belt should match that of the substrate (the margin is about 1mm), and the spacing between substrates should be ≥5cm;
[0041] 4) 0201 component welding strength ≥ 300g;
[0042] 0402 component welding strength ≥500g;
[0043] 0603 component welding strength ≥800g;
[0044] Welding strength of 0805 or above ≥1000g;
[0045] The welding strength of IC components is ≥1000g.
[0046] Preferably, the pressing step operating conditions are as follows:
[0047] 1) Soldering iron temperature: 450-480℃;
[0048] 2) Foot length standard: 1.5~2.2mm;
[0049] 3) Standard: The solder joints are intact without shearing, cracking, burrs, missing shearing, damage to components, and copper foil;
[0050] 3) High-quality standards: relay ≦0.2mm, screw terminal block ≦0.3mm, terminal block, socket ≦0.5mm, electrolytic capacitor ≦0.7mm, bare wire ≦1.0mm, horizontal ≦0.7mm, horizontal 1.5~6.3mm maximum 8.0, vertical 0.4~1.5mm.
[0051] Preferably, the operating conditions of the wave soldering step are as follows:
[0052] 1) Furnace temperature parameter setting benchmark: temperature rise 1~2℃ / s, preheating time 60~120s, preheating temperature 90~130℃, tin temperature 255~275℃, high wave time 1~2s, flat wave time 3~4s, elevation angle 5~7°;
[0053] 2) Actual parameters of furnace temperature: chain speed 0.9m.Min, spray 0.22ms, preheat 85, preheat 95, preheat 105℃, tin temperature 262℃; the height of solder bath liquid level is 5-10mm from the edge of the tin bath;
[0054] 3) The distance between substrates is ≥5cm;
[0055] 4) Air pressure 3.0-4.0Kg; flux stock ≥ 3 / 5; flux specific gravity: 0.8~0.82g / cm;
[0056] 5) Welding quality warning: single board defect points: missing parts ≥1, high parts ≥2, empty welding / continuous welding / false welding ≥3; frequency of occurrence: ≦10 boards.
[0057] Preferably, the pressing step further includes a repair welding step: repair welding is performed on components with welding defects or additional components, and the step should meet the following conditions:
[0058] 1) Welding temperature: 420-450℃, duration ≤ 3S;
[0059] 2) Key soldering points: screw terminal block, toroidal inductor, large capacitor, yellow wire passing through T2 and soldered to hole A;
[0060] 3) Solder point standard: Solder point = 100% pad area, tin tip vertically ≤ 0.6mm; tin tip die direction ≤ pad and ≥ safety distance 0.76mm for weak current / 5.0mm for strong current.
[0061] Preferably, the substrate cleaning step satisfies the following conditions:
[0062] 1) Control point: Clean the main substrate at a 45° tilt;
[0063] 2) Residue limit standards: Points ≤ 5, no charring in the 600m2 area.
[0064] Preferably, the B / T surface three-proofing step meets the following conditions:
[0065] 1) Varnish: diluent = 1:1:
[0066] 2)Both the board surface and the bottom of the board need to be painted;
[0067] 3) Control points: brush twice horizontally and vertically, lay the board with the bottom facing up and air dry for ≥1 minute, and do not touch the surface of the back welded parts, sockets, plugs, terminal blocks, and DIP switches with varnish;
[0068] 4) Brushing standard: Brushing should be uniform and free of bubbles. The bubble limit standard is: 600m㎡ area points ≤ 5.
[0069] Preferably, the dispensing operation in the dispensing / IC three-proofing step meets the following conditions:
[0070] 1) Gluing location: electrolytic capacitors, safety capacitors, cement resistors, wires;
[0071] 2) Control points: no leaks, place the glue-applied surface facing up and air dry for ≥30 minutes, and the surface of the back welded parts, sockets, plugs, terminal blocks, and DIP switches at the bottom of the board should not be stained with glue;
[0072] 3) Glue dispensing limit mark: The length of the junction between the bottom of the device body and the substrate is ≧50%, and the height is ≧25%.
[0073] Preferably, after the dispensing / IC three-proofing steps, the steps of assembling a heat sink, a withstand voltage test, a fan test, aging, a final load test, an appearance inspection and packaging are also included in sequence.
[0074] Beneficial technical effects of the present invention: In the PCBA production process of the present invention, automated equipment is used to replace manual labor in the production line, which can effectively ensure the output consistency of products, improve product performance and quality, enhance the cost performance of products, greatly improve production efficiency and quality, and greatly improve market competitiveness. BRIEF DESCRIPTION OF THE DRAWINGS
[0075] Figure 1 The present invention is a flowchart of the steps of a fully automated PCBA production method. DETAILED DESCRIPTION
[0076] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with embodiments, but the scope of protection claimed in the present invention is not limited to the following specific embodiments.
[0077] The explanations of the English abbreviations mentioned in this embodiment are as follows:
[0078] PSPP (PCBA semi-automatic production process): The process flow for semi-automatic production of electronic circuit boards PCBA.
[0079] PAPP (PCBA automatic production process): The process for fully automated unmanned production of electronic circuit boards PCBA.
[0080] PCBA is the abbreviation of Printed Circuit Board Assembly, which means printed circuit board assembly. Specifically, PCBA is the process of installing electronic components (such as integrated circuits, resistors, capacitors, etc.) on a printed circuit board (PCB) by welding to form a complete circuit system.
[0081] The specific scheme of this embodiment is as follows:
[0082] like Figure 1 As shown, a PCBA fully automated production method includes the following steps:
[0083] PCB loading steps: Place the PCB to be assembled at the predetermined position and use the PCB loading machine to implement: During production, just stack the PCB boards and place them in the rack of the loading machine. The loading machine will actively identify whether the PCB board needs to be delivered based on the real-time status of the current production line. When it obtains the delivery signal, it will automatically pick up the PCB board and deliver it to the conveyor belt, realizing fully automatic loading.
[0084] Printing solder paste step: print the solder paste evenly on the pad position of the PCB board, and use the scraper to print the solder paste evenly on the pad position of the PCB board. In this step, a fully automatic solder paste printer is used: during production, the printer recognizes the real-time status of the equipment throughout the process, and automatically completes the PCB board feeding-identification-dust removal-screen sticking-knife start-printing-film stripping-track return-board output-screen cleaning and other related printing steps, realizing fully automatic solder paste printing.
[0085] Specifically, the detailed operation and conditions for printing solder paste are as follows:
[0086] 1. The storage temperature of lead-free solder paste is 2-10℃, ≤6 months, return to temperature for 3-4 hours, stir for 5-6 minutes, and the viscosity is 200±20pa.s;
[0087] 2. Use the steel mesh corresponding to the machine model, with tension ≧32N.cm2 and no deformation;
[0088] 3. Printing machine parameter setting table:
[0089] Printing speed: 50±10mm / s;
[0090] Printing pressure: 23±5N(*0.01N);
[0091] Gap between steel mesh and substrate: -0.5±0.1mm;
[0092] Drop speed: 5.0±0.5mm / s, drop stroke 3.0mm;
[0093] Demolding method: first use the scraper and then demould;
[0094] Automatic cleaning is performed every 4 prints and manual cleaning is performed every 20 prints.
[0095] Printing environment temperature: 20-26℃, steel mesh service life ≤ 100,000 times;
[0096] QC inspection steps: Check the printing effect of the printed solder paste PCB board, including but not limited to the uniformity of the solder paste, the presence of insufficient solder, solder joints, pull tips, displacement, missing printing and other defects. SPI imaging equipment is used in this step: during production, the equipment takes real-time images of the PCB printing surface, compares it with the standard block, identifies the solder paste shape, and automatically reports abnormal printing points.
[0097] Using the above standard conditions to print solder paste can greatly improve the uniformity of printing standards and improve printing uniformity, quality and efficiency.
[0098] SMT patch steps: Attach the surface mount components SMD to the PCB with solder paste. Automatic patching is performed using fully automatic patch machines and other equipment. The fully automatic patch machine can automatically grab, position and place components according to preset programs, greatly improving production efficiency and accuracy.
[0099] The following conditions must be met:
[0100] 1. The patch program is called correctly;
[0101] 2. The specifications, directions and positions of the SMD components are correct;
[0102] 3. Check whether the mounting angle and offset meet the requirements.
[0103] The use of fully automatic placement machines for device placement has greatly improved the efficiency of placement, and is especially suitable for batch production of micro-sized devices and high-density PCBs. It has significant advantages in placement quality control and efficiency that cannot be achieved by manual labor.
[0104] Reflow soldering step: solder the components already attached to the PCB through the reflow soldering furnace, heat the reflow soldering furnace to melt the solder paste pre-coated on the pad, and then wet the component pins and pads, and finally cool and solidify to form solder joints, which is particularly suitable for surface mount technology (SMT) components, such as chips, resistors, capacitors, etc.
[0105] Specifically, the conditions that reflow soldering should meet are as follows:
[0106] 1. Furnace temperature parameter setting benchmark: heating rate 1~4℃ / s, preheating time 60~120s, preheating end 200℃, reflux temperature 245~260℃, reflux time 30~60s, cooling rate 1~5℃ / s;
[0107] 2. Service life of furnace temperature test board: ≦60 times;
[0108] 3. The width of the reflow conveyor belt should be consistent with the substrate (the margin is about 1mm), and the spacing between substrates should be ≥5cm;
[0109] 4. 0201 component welding strength ≥ 300g;
[0110] 0402 component welding strength ≥500g;
[0111] 0603 component welding strength ≥800g;
[0112] Welding strength of 0805 or above ≥1000g;
[0113] The welding strength of IC components is ≥1000g.
[0114] Through the above setting conditions, the efficiency and quality of reflow soldering can be greatly improved. At the same time, the use of a multi-temperature zone nitrogen reflow soldering furnace will significantly improve the soldering quality of mounted components, especially suitable for batch production of micro-components and high-density PCBs.
[0115] Mounting AOI inspection steps: Use AOI equipment to perform quality inspection on the PCBs that have been mounted. AOI inspection can efficiently and accurately detect various defects on the PCB. The AOI equipment automatically scans the PCB to be inspected through a high-definition CCD camera, collects images, compares them with the qualified parameters in the data, and analyzes the differences;
[0116] Specifically, the AOI inspection steps meet the following conditions:
[0117] 1. The AOI program is called correctly;
[0118] 2. The specifications, directions and positions of the SMD components are correct; check that the mounting angle and offset meet the requirements;
[0119] 3. Check the solder joints for tinning, cold soldering, continuous soldering, empty soldering, and poor component tombstone and solder beads;
[0120] 4. Component offset ≤ 1 / 4 of the body; Tin intake ≥ 1 / 4 of pad height and 1 / 2 of pad width; Tin bead Points ≤ 5 (no short circuit risk, no violation of electrical safety distance 0.76mm for weak current / 5.0mm for strong current).
[0121] AOI inspection through the above steps and conditions greatly improves the accuracy and efficiency of inspection.
[0122] After the AOI inspection step there is an X-Rey inspection step.
[0123] X-Rey inspection steps: Use X-Rey equipment to perform quality inspection on the PCB with good patching. X-ray inspection can intuitively, efficiently and accurately detect various hidden soldering defects of BGA devices on PCB. X-Rey equipment inspection is an effective supplement to AOI equipment.
[0124] Specifically, the X-Rey detection step meets the following conditions:
[0125] 1. The X-ray optical distance and magnification are correctly called;
[0126] 2. The internal welding of SMD components meets the requirements;
[0127] 3. Check all kinds of hidden solder joints to see if there is any soldering, false soldering, continuous soldering, empty soldering, or poor tin particles;
[0128] 4. Solve the shortcomings of visual inspection that cannot be seen from the outside.
[0129] The above steps and conditions can greatly improve the coverage and accuracy of X-Rey inspection.
[0130] Automatic plug-in machine steps: insert the pin-type components into the corresponding positions of the PCB. According to the type of device, horizontal plug-in machines, vertical plug-in machines, and special-shaped plug-in machines can be used for configuration and production. The plug-in step mainly involves inserting components that cannot be mounted by SMT (such as DIP packaged components) into the corresponding positions of the PCB;
[0131] Specifically, the automatic plug-in machine steps meet the following conditions:
[0132] 1. The plug-in machine program is called correctly;
[0133] 2. The specifications, directions and positions of the plug-in components are correct;
[0134] 3. Check whether the plug-in angle and folding foot amount meet the requirements.
[0135] The use of fully automatic plug-in machines for device insertion has greatly improved the efficiency of insertion, and is especially suitable for batch production of various types of devices and high-density PCBs. It has significant advantages in insertion quality control and efficiency that cannot be achieved by manual labor.
[0136] Before the plug-in step, conventional operations such as material delivery and device molding are required for components that require plug-in operations.
[0137] Material delivery is the process of delivering the electronic components and materials required for production to the production line or processing area in accordance with the requirements of the BOM (Bill of Materials) and production plan.
[0138] Device molding is a pre-processing step for some electronic components that cannot be installed by direct plug-in. These components may need to be processed and formed first due to size, shape or pin length to meet the requirements of plug-in and welding.
[0139] Full wave soldering steps: solder the components on the PCB board through a wave soldering furnace. The PCB passes through the preheating zone, wave soldering zone and cooling zone in sequence through a conveyor belt to achieve mechanical and electrical connections between the component pins and the PCB pads. It is mainly used for soldering pin-type components; fully automatic wave soldering is achieved through a wave soldering furnace.
[0140] Wave soldering needs to meet the following conditions:
[0141] 1. Furnace temperature parameter setting benchmark: temperature rise 1~2℃ / s, preheating time 60~120s, preheating temperature 90~130℃, tin temperature 250~270℃, high wave time 1~2s, flat wave time 3~4s, elevation angle 5~7°;
[0142] 2. Actual parameters of furnace temperature: chain speed 0.9m.Min, spray 0.22ms, preheat 85, preheat 95, preheat 105℃, tin temperature 262℃;
[0143] 3. The width of the conveyor belt should be consistent with the substrate (the margin is about 0.5mm, so that the substrate will not be stuck or dropped);
[0144] 4. The distance between substrates is ≥5cm;
[0145] 5. Specific gravity of flux: 0.8~0.82g / cm;
[0146] 6. Welding quality warning: Calculate the number of defective points based on a single board: missing parts ≥ 1, high parts ≥ 2, empty welding / continuous welding / false welding ≥ 3;
[0147] Frequency of occurrence: ≤ 10 boards.
[0148] By operating under the above standard conditions, the welding quality and efficiency of wave soldering can be greatly improved. The use of a multi-temperature zone nitrogen wave soldering furnace will significantly improve the welding quality of PCBs, especially for batch production of PCBs that require high solder penetration rates and device-intensive PCBs.
[0149] Plug-in AOI inspection steps: Use AOI equipment to conduct quality inspection on the PCB that has been wave-soldered by the plug-in. AOI inspection can efficiently and accurately detect various defects on the PCB. The AOI equipment automatically scans the PCB to be inspected through a high-definition CCD camera, collects images, compares them with the qualified parameters in the data, and analyzes the differences;
[0150] Specifically, the AOI inspection steps meet the following conditions:
[0151] 1. The AOI program is called correctly;
[0152] 2. The specifications, directions and positions of the plug-in components are correct;
[0153] 3. Check the solder joints for tinning, cold soldering, continuous soldering, empty soldering, and poor component tombstone and solder beads;
[0154] 4. Component offset ≤ 1 / 4 of the body; Tin intake ≥ 1 / 4 of pad height and 1 / 2 of pad width; Tin bead Points ≤ 5 (no short circuit risk, no violation of electrical safety distance 0.76mm for weak current / 5.0mm for strong current).
[0155] AOI inspection through the above steps and conditions greatly improves the accuracy and efficiency of inspection.
[0156] Selective wave soldering steps: repair the bad solder joints on the PCB board through the selective wave soldering furnace. The PCB passes through the preheating zone, selective soldering zone and cooling zone in turn through the conveyor belt to repair the bad solder joints. Selective wave soldering is an effective supplement to the fully automatic wave soldering. Its working area accepts the bad information fed back by the AOI after the furnace;
[0157] Specifically, the requirements for repair welding are as follows:
[0158] 1. The program is called correctly;
[0159] 2. Welding temperature: 420-450℃, duration ≦3S;
[0160] 2. The solder joints are full, without tin cracks, empty solder joints, continuous solder joints, false solder joints, thin tin, solder wrapping, and no damage to the SMD parts;
[0161] 3. Solder point standard: Solder point = 100% pad area (acceptable ≧75% area), tin tip (vertical) ≦0.6mm (vertical), tin tip (mold direction) ≦ pad and ≧safety distance: 0.76mm for weak current / 5.0mm for strong current.
[0162] Repair soldering under the above conditions can greatly improve the uniformity of repair soldering and improve the quality of repair soldering. The use of selective wave soldering can effectively replace manual visual soldering and save labor costs.
[0163] ICT test steps: connect the test probe of the test equipment to the test point on the circuit board to measure the electrical characteristics of the circuit; this step can be tested with the Lude ICT online test equipment. The test content mainly includes the detection of circuit open circuit, short circuit, resistance, capacitance, inductance, diode and transistor parameters; ICT testing can be automated, greatly improving the test efficiency.
[0164] After ITC testing, the product needs to be burned / labeled A.
[0165] Specifically, the steps of product program burning are: select the corresponding burning software to burn the product program, follow the prompts of the burning software and click OK to complete. There are two ways of burning: offline and online.
[0166] Specifically, the burning requirements are as follows:
[0167] 1. The program is called correctly;
[0168] 2. Check the program checksum;
[0169] 3. Record of program burning;
[0170] 4. Re-inspection of product program codes.
[0171] Burn the product program under the above conditions to ensure the accuracy of the burning program.
[0172] Product label engraving steps: Use a marking machine to engrave the model label on the product. This can be done by laser coding, printing, and labeling.
[0173] Specifically, the labeling requirements are as follows:
[0174] 1. The label position, format and content are correct;
[0175] 2. The label font is correct and the handwriting is clear and legible;
[0176] 3. Barcodes and QR codes can be read effectively;
[0177] 4. Product label registration records.
[0178] The above conditions are used to identify product labels and ensure the uniqueness of individual products.
[0179] Functional initial test steps: Use automatic test equipment ATE to test the various functions of the above processed circuit boards; through functional initial test, potential problems on the circuit boards can be discovered and repaired in time to ensure product quality and reliability. The use of automatic test equipment ATE often has high efficiency and accuracy.
[0180] Substrate cleaning: Clean the substrate to remove debris. Dry ice automatic cleaning equipment can be used for cleaning to achieve fully automatic cleaning;
[0181] The requirements for substrate cleaning are as follows:
[0182] 1. There is no tin beads, tin slag, scraps, rosin and other foreign matter left on the board surface and bottom;
[0183] 2. Control points: Tilt the main substrate at 45° for cleaning. When using board cleaning water on seriously stained areas, be careful not to use board cleaning water on sockets, plugs, terminal blocks, and DIP switches.
[0184] 3. Residue limit standards: Points ≤ 5, no charring (600mm² area).
[0185] Meeting the above conditions can greatly improve the cleanliness and efficiency of substrate cleaning. Depending on the product category, equipment such as disc brush scrubbers and automatic dry ice cleaners can be used for cleaning.
[0186] Automatic spraying three-proofing steps: Apply three-proofing paint on the B and T sides of the cleaned circuit board. Depending on the product category, single-sided spraying machines and flip-plate double-sided spraying machines can be used for PCB three-proofing spraying;
[0187] The requirements for B / T surface three protections are as follows:
[0188] 1. The spraying program is called correctly;
[0189] 2. Varnish: diluent = 1:1;
[0190] 3. Control points: Spraying thickness ≧50um, the bottom of the board is placed flat with the streamline air drying time ≧1 minute, the surface of the back welding body, sockets, plugs, terminal blocks, and DIP switches on the bottom of the board are not stained with varnish;
[0191] 4. Brushing standard: Brushing evenly, without missing any spots, without bubbles, and without whitening. Bubble limit standard: Points ≤ 5 (600m2 area).
[0192] The automatic spraying machine can accurately control the spraying amount, effectively avoiding the defects such as missed brushing, paint sticking, uneven paint layer, etc. caused by manual brushing, ensuring the consistency of product operation.
[0193] Automatic dispensing steps: Use the automatic dispensing machine to dispense glue on the corresponding surface of the PCB board, and apply the pre-prepared glue on the surface of the product through the dispensing equipment, especially the parts that need to be sealed, fixed or improved in anti-vibration and waterproofing capabilities, such as connectors, LEDs and other devices on the circuit board. This step can be done by fully automatic dispensing and semi-automatic dispensing.
[0194] In this embodiment, 704 glue and 268 glue can be used for dispensing.
[0195] Among them, the dispensing operation requirements are as follows:
[0196] 1. The dispensing program is called correctly;
[0197] 2. Control points: no leaks, place the glue-applied surface facing up and air dry for ≥30 minutes, and the surface of the back welded parts, sockets, inserts, terminal blocks, and DIP switches at the bottom of the board should not be stained with glue;
[0198] 3. Glue dispensing limit standard: The length of the junction between the bottom of the device body and the substrate is ≧50%, and the height is ≧25%.
[0199] Among them, the requirements for dispensing with 268 glue are as follows:
[0200] 1. Gluing position: main chip;
[0201] 2. Control points: no leaks, lay flat with the glued surface facing up and air dry for ≥30 minutes, buttons, sockets, buzzers, wiring sockets, and digital screens must not be stained with glue;
[0202] 3. Glue dispensing limit standard: chip body and pin glue coverage ≧100%, thickness ≧2mm.
[0203] The automatic dispensing machine can accurately control the dispensing amount, effectively avoiding the related defects such as missing points, insufficient points, excessive points, inconsistent glue amount, different shapes, etc. caused by manual dispensing, ensuring the consistency of product operation.
[0204] IC three-proofing steps: The IC three-proofing steps after dispensing are the same as the previous B / T surface three-proofing operations. IC three-proofing is mainly to improve the working stability and durability of integrated circuits in harsh environments, usually including waterproof, dustproof, shockproof and other treatments. Use self-adhesive film or paper tape to shield and protect the parts that do not need to be coated with three-proof paint to prevent these parts from being accidentally coated, and then do the three-proofing.
[0205] The dispensing / IC three-proofing steps also include the steps of assembling the heat sink, voltage resistance test, fan test, aging, final load test, appearance inspection and packaging.
[0206] Specifically, the requirements for assembling the radiator are as follows:
[0207] 1. First, screw the 7 support columns into the screw holes for about 1 turn, and then tighten them one by one with an electric screwdriver;
[0208] 2. Place two ceramic sheets with holes on the transistor paste positions and align them with the screw holes;
[0209] 3. Control points: (In winter, the support column is soaked in water for 2 hours) No components are missing, the components are intact and not damaged, the ceramic sheet and the screw hole are aligned and not skewed, the support column is locked in place and the bottom is attached to the board, and the floating height is ≦0.1mm;
[0210] Electric screwdriver torque: 3.5~4.0kgf.cm.
[0211] The assembly work can be carried out with an automatic screw locking machine. The equipment can ensure the accuracy and consistency of product operations and effectively control related defects such as omissions, force and torque differences, component damage, stress damage, etc. caused by manual operations.
[0212] The withstand voltage test is carried out by a withstand voltage tester. The requirements for the withstand voltage test are as follows:
[0213] 1. The test operation steps are correct and consistent;
[0214] 2. ACL / ACN, LA / LB, UVW for radiator;
[0215] 3. The test sound prompt is normal, and there is no alarm;
[0216] 4. The test screen displays normal;
[0217] 5. The test voltage parameters are correct: AC1.5KV 5.0mA 5S.
[0218] The pressure test equipment is used for implementation. Through accurate detection by the instrument and equipment, the product meets the relevant safety requirements, and defective products are screened out in time to ensure product quality.
[0219] The fan test is carried out using a special test tool. The fan test requirements are as follows:
[0220] 1. The test operation steps are correct and consistent;
[0221] 2. The test fixture and product indicator lights show normal;
[0222] 3. The test sound prompt is normal;
[0223] 4. The line control screen displays normally;
[0224] 5. The fan starts and runs normally without any lag;
[0225] 6. The fan operation time should not be too long, and the test should be completed within 10 seconds to prevent overheating damage (without radiator installed).
[0226] The semi-finished product testing tooling is used for implementation. With the assistance of the testing tooling, the semi-finished product and its related functional devices are electrically connected and simulated functional testing is carried out to ensure that the product performance is qualified.
[0227] The product is aged by using a withstand voltage tester. The requirements for the aging operation are as follows:
[0228] 1. The aging operation steps are correct and consistent;
[0229] 2. The wiring of the substrate is correct: aging dial 111100, short-circuit 4-5 of CN31 and 3-4 of CN601;
[0230] 3. The fan starts and runs normally without any jamming or malfunction;
[0231] 4. The LED indication of the substrate is normal;
[0232] 5. Aging conditions: AC220V 50℃ 4 hours;
[0233] 6. Check once at the beginning, middle (2 hours) and end of aging.
[0234] According to the characteristics of the products, the corresponding aging equipment is matched, and the products are aged in a specific environment to test the functional reliability of the products, eliminate the hidden faults and ensure the product quality.
[0235] Use special test equipment to carry out the final load test. The requirements for the final load test are as follows:
[0236] 1. The test operation steps are correct and consistent;
[0237] 2. The test fixture and product indicator lights show normal;
[0238] 3. The test sound prompt is normal;
[0239] 4. The display of the wired control screen is normal and the model code is consistent;
[0240] 5. The press is running normally (up-frequency 82, dial code 111110, press 36K);
[0241] 6. Test electrical parameters correctly.
[0242] The finished product testing tooling is used for implementation. With the assistance of the testing tooling, the semi-finished product is electrically connected to its related functional components, and simulated functional testing is performed to ensure that the product performance is qualified and can meet the needs of users.
[0243] The product is packaged using a packaging machine. The packaging requirements are as follows:
[0244] 1. Load the products into the corresponding card slots; 4 units per box;
[0245] 2. Control points: The packing quantity is correct, not too few or mixed; the packing arrangement is consistent; the outer box label is consistent with the product model, serial number and quantity; the label is attached flatly, without wrinkles or corners; the tape sealing is firm and compact, without wrinkles or looseness.
[0246] Using automatic packaging machines to package and seal products can effectively reduce the workload of manual operations, ensure the consistency and accuracy of operations, improve production efficiency, and save labor costs.
[0247] After the PCBA is packaged, it will undergo OQC inspection and can be shipped and sold after being put into storage.
[0248] In the PCBA production process of the present invention, automated equipment is used to replace manual labor in the production line, which can effectively ensure the output consistency of products, improve product performance and quality, enhance the cost performance of products, greatly improve production efficiency and quality, and greatly improve market competitiveness.
[0249] According to the disclosure and teaching of the above description, those skilled in the art to which the present invention belongs may also make changes and modifications to the above embodiments. Therefore, the present invention is not limited to the specific embodiments disclosed and described above, and some modifications and changes to the invention should also fall within the scope of protection of the claims of the present invention. In addition, although some specific terms are used in this specification, these terms are only for the convenience of description and do not constitute any limitation to the invention.
Claims
1. A fully automated PCBA production method, characterized in that: The following steps are involved: PCB loading step: place the PCB to be assembled in the predetermined position; Printing solder paste steps: print the solder paste evenly on the pad position of the PCB board; QC inspection steps: Check the printing effect of the PCB board printed with solder paste; SMT patch steps: attach the surface mount components SMD to the PCB with solder paste; Reflow soldering step: solder the SMD components already attached to the PCB board through a reflow soldering furnace; AOI inspection steps: Use AOI equipment to perform quality inspection on the PCB with good patching; Insertion steps: insert the pin-type components into the corresponding positions of the PCB; Pre-furnace inspection: Use magnification tools to inspect PCB boards and components for defects; Wave soldering steps: solder the plug-in components on the PCB board through a wave soldering furnace; Pressing step: Press the components firmly onto the PCB through mechanical pressure or heat pressing; Repair welding steps: welding after the pressing is completed, repair welding operations are performed on welding defects or additional components; ICT test steps: connect the test probes of the test equipment to the test points on the circuit board to measure the electrical characteristics of the circuit; Functional initial test steps: Use automatic test equipment ATE to test the various functions of the above processed circuit boards; Substrate cleaning: clean the substrate to remove debris; B / T surface three-proof paint: Apply three-proof paint on the B and T surfaces of the circuit board after cleaning; Glue dispensing / IC three-proofing: Use glue dispensing equipment to apply glue to the surface of the corresponding part of the PCB board, and then apply three-proof paint.
2. A fully automated PCBA production method as claimed in claim 1, characterized in that: The operating conditions of the printing solder paste step are as follows: 1) Lead-free solder paste should be stored at 2-10°C for ≤6 months, warmed up for 3-4 hours, stirred for 5-6 minutes, and have a viscosity of 200±20pa.s; 2) The tension of the practical steel mesh is ≥32N.cm2; 3) Printing machine parameter setting table: Printing speed: 50±10mm / s; Printing pressure: 23±5N(*0.01N); Gap between steel mesh and substrate: -0.5±0.1mm; Drop speed: 5.0±0.5mm / s; Lowering stroke 3.0mm; Demolding method: first use the scraper and then demould; Automatic cleaning is performed every 4 prints and manual cleaning is performed every 20 prints. Printing environment temperature: 20-26℃; The service life of the steel mesh is ≤ 100,000 times.
3. A fully automated PCBA production method as claimed in claim 1, characterized in that: The reflow soldering step satisfies the following conditions: 1) Furnace temperature parameter setting benchmark: heating rate 1~4℃ / s, preheating time 60~120s, preheating end 200℃, reflux temperature 245~260℃, reflux time 30~60s, cooling rate 1~5℃ / s; 2) Service life of furnace temperature test board: ≦60 times; 3) The width of the reflow conveyor belt should match that of the substrate (the margin is about 1mm), and the spacing between substrates should be ≥5cm; 4) 0201 component welding strength ≥ 300g; 0402 component welding strength ≥500g; 0603 component welding strength ≥800g; Welding strength of 0805 or above ≥1000g; The welding strength of IC components is ≥1000g.
4. A fully automated PCBA production method as claimed in claim 1, characterized in that: The operating conditions of the pressing step are as follows: 1) Soldering iron temperature: 450-480℃; 2) Foot length standard: 1.5~2.2mm; 3) Standard: The solder joints are intact without shearing, cracking, burrs, missing shearing, damage to components, and copper foil; 3) High-quality standards: relay ≦0.2mm, screw terminal block ≦0.3mm, terminal block, socket ≦0.5mm, electrolytic capacitor ≦0.7mm, bare wire ≦1.0mm, horizontal ≦0.7mm, horizontal 1.5~6.3mm maximum 8.0, vertical 0.4~1.5mm.
5. A fully automated PCBA production method as claimed in claim 1, characterized in that: The operating conditions of the wave soldering step are as follows: 1) Furnace temperature parameter setting benchmark: temperature rise 1~2℃ / s, preheating time 60~120s, preheating temperature 90~130℃, tin temperature 255~275℃, high wave time 1~2s, flat wave time 3~4s, elevation angle 5~7°; 2) Actual parameters of furnace temperature: chain speed 0.9m.Min, spray 0.22ms, preheat 85, preheat 95, preheat 105℃, tin temperature 262℃; the height of solder bath liquid level is 5-10mm from the edge of the tin bath; 3) The distance between substrates is ≥5cm; 4) Air pressure 3.0-4.0Kg; flux stock ≥ 3 / 5; flux specific gravity: 0.8~0.82g / cm; 5) Welding quality warning: single board defect points: dropped parts ≥1, high parts ≥2, empty welding / continuous welding / false welding ≥3; frequency of occurrence: ≦10 boards.
6. A fully automated PCBA production method as claimed in claim 1, characterized in that: After the pressing step, a repair welding step is also included: repair welding is performed on components with welding defects or additional components. This step should meet the following conditions: 1) Welding temperature: 420-450℃, duration ≤ 3S; 2) Key soldering points: screw terminal block, toroidal inductor, large capacitor, yellow wire passing through T2 and soldered to hole A; 3) Solder point standard: Solder point = 100% pad area, tin tip vertically ≤ 0.6mm; tin tip die direction ≤ pad and ≥ safety distance 0.76mm for weak current / 5.0mm for strong current.
7. A fully automated PCBA production method as claimed in claim 1, characterized in that: The substrate cleaning step satisfies the following conditions: 1) Control point: Clean the main substrate at a 45° tilt; 2) Residue limit standards: , points ≤ 5, no charring within the 600m2 area.
8. A fully automated PCBA production method as claimed in claim 1, characterized in that: The B / T surface three-proof steps meet the following conditions: 1) Varnish: diluent = 1:1: 2)Both the board surface and the bottom of the board need to be painted; 3) Control points: brush twice horizontally and vertically, lay the board with the bottom facing up and air dry for ≥1 minute, and do not touch the surface of the back welded parts, sockets, plugs, terminal blocks, and DIP switches with varnish; 4) Brushing standard: Brushing should be uniform and free of bubbles. The bubble limit standard is: 、600m㎡ area points ≤5.
9. A fully automated PCBA production method as claimed in claim 1, characterized in that: The dispensing operation in the dispensing / IC three-proofing step meets the following conditions: 1) Gluing location: electrolytic capacitors, safety capacitors, cement resistors, wires; 2) Control points: no leaks, place the glue-applied surface facing up and air dry for ≥30 minutes, and the surface of the back welded parts, sockets, plugs, terminal blocks, and DIP switches at the bottom of the board should not be stained with glue; 3) Glue dispensing limit mark: The length of the junction between the bottom of the device body and the substrate is ≧50%, and the height is ≧25%.
10. A fully automated PCBA production method as claimed in claim 9, characterized in that: The dispensing / IC three-proofing steps also include the steps of assembling the heat sink, voltage resistance test, fan test, aging, final load test, appearance inspection and packaging.
Citation Information
Patent Citations
SMT processing system and SMT processing technology
CN107231762A
Intelligent SMT production error-proof tracing method and process
CN108811365A
PC power supply automatic production line
CN113732723A
SMT (Surface Mount Technology) production process for printed circuit board
CN115988865A
High-process welding process combining reflow soldering and wave soldering