Temperature adjustment mold, temperature adjustment method, and device for manufacturing resin container
By designing a temperature adjustment mold for hot parison type blow molding, cooling and temperature distribution adjustment are performed by shrinkage of preformed blanks, the problem of insufficient cooling in the prior art is solved and the appearance quality of the container is improved.
Patent Information
- Application Number
- CN202380033315.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-02-16
- Filing Date
- 2023-02-15
- Publication Date
- 2024-11-19
AI Technical Summary
During the blow molding process of hot parison, the cooling and temperature distribution adjustment in the preformed blank is insufficient, resulting in insufficient cooling and poor container appearance.
Design a temperature adjustment mold, including the first mold in contact with the outer peripheral surface of the preform, the second mold is inserted into the neck and is tightly inserted into the inner side, the third mold is integrated into the second mold, and has an opening for introducing compressed air, and is cooled by air At the same time, the cooling and temperature distribution adjustment are used to adjust the preform.
Good cooling and temperature distribution adjustment of the preformed blank are achieved, and residual thinning and spherical crystallization at the bottom of the container caused by insufficient cooling is avoided, ensuring the appearance quality of the container.
Smart Images

Figure CN118984769A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a temperature regulating mold, a temperature regulating method, and a manufacturing device for a resin container. Background Art
[0002] Conventionally, as one of the manufacturing apparatuses of resin containers, a hot parison type blow molding apparatus is known. The hot parison type blow molding apparatus is a structure that utilizes the heat retained during injection molding of a preform to blow-mold a resin container, and is advantageous in that it can manufacture a variety of resin containers with excellent appearance and aesthetics compared to the cold parison type.
[0003] In order to shorten the hot preform molding cycle, for example, it is proposed to shorten the injection molding time of the preform as the speed-limiting stage (the cooling time of the preform in the injection mold), and perform additional cooling of the high-temperature preform in the temperature adjustment process after injection molding. In addition, as a method of additionally cooling the preform, there is also known a method in which the outer peripheral surface of the preform is brought into contact with a cooling mold to exchange heat during the temperature adjustment step, and compressed air is directed into the preform to cool it (see Patent Documents 1 to 3). Prior art literature Patent Literature
[0004] Patent Document 1: Japanese Patent No. 6505344 Patent Document 2: International Publication No. 2020 / 158918 Patent Document 3: Japanese Patent No. 2509042 Summary of the invention Problems to be solved by the invention
[0005] In such additional cooling of the preform, there is a possibility that cooling in the temperature adjustment step and adjustment of the temperature distribution may become insufficient.
[0006] Therefore, the present invention has been made in view of such a problem, and an object of the present invention is to provide a temperature adjustment mold which can utilize the shrinkage of the preform during air cooling in the temperature adjustment step to satisfactorily cool the preform and adjust the temperature distribution. Technical solutions to solve problems
[0007] One embodiment of the present invention is a temperature-regulating mold for regulating the temperature of a resin preform having a bottom shape that is injection molded. The temperature-regulating mold comprises: a first mold that accommodates the preform inside and contacts the outer peripheral surface of the preform; a second mold that is inserted into the preform and is in close contact with the neck of the preform; and a third mold that is inserted into the preform as a whole with the second mold so that the mold surface bears the bottom of the preform. The third mold has an opening for introducing compressed air into the preform. When the third mold is inserted into the preform, the interval from the mold surface of the third mold to the first mold is larger than the thickness of the preform. Effects of the Invention
[0008] According to one aspect of the present invention, it is possible to provide a temperature adjustment mold capable of satisfactorily cooling a preform and adjusting the temperature distribution by utilizing the shrinkage of the preform during air cooling in a temperature adjustment step. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 It is a figure which shows typically the structure of the blow molding apparatus which concerns on this embodiment. Figure 2 It is a diagram showing a configuration example of a temperature adjustment unit. Figure 3 It means from Figure 2 A diagram showing a state where compressed air is introduced into a preform. Figure 4 This is a flow chart showing the steps of the blow molding method. DETAILED DESCRIPTION
[0010] [Implementation Method] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In the embodiments, in order to facilitate the understanding of the description, the structures and elements other than the main parts of the present invention are simplified or omitted for description. In addition, in the drawings, the same symbols are marked for the same elements. It should be noted that the shapes, sizes, etc. of the elements shown in the drawings are schematically represented and do not represent the actual shapes, sizes, etc.
[0011] (Description of Blow Molding Device) Figure 1 1 is a diagram schematically showing the structure of the blow molding device 20 of the present embodiment. The blow molding device 20 of the present embodiment is a device that uses a hot preform method (also called a one-stage method) to blow-mold a container by effectively utilizing the retained heat (internal heat) during injection molding without cooling the preform to room temperature.
[0012] The blow molding device 20 includes an injection molding unit 21, a temperature regulating unit 22, a blow molding unit 23, a take-out unit 24, and a conveying mechanism 26. The injection molding unit 21, the temperature regulating unit 22, the blow molding unit 23, and the take-out unit 24 are arranged at positions each rotated by a given angle (e.g., 90 degrees) around the conveying mechanism 26.
[0013] The conveying mechanism 26 has a vertical Figure 1 The transfer plate 28 ( Figure 1 On the transfer plate 28, one or more neck molds 27 (not shown) for holding the neck 11 of the preform 10 or the container are arranged at given angles. Figure 1 The conveying mechanism 26 sequentially conveys the preform 10 (or container) whose neck is held by the neck mold 27 to the injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24 by moving the transfer plate 28 by 90 degrees each time. It should be noted that the conveying mechanism 26 also includes a mold opening mechanism for the neck mold 27, etc.
[0014] (Injection molding section 21) The injection molding unit 21 includes an injection cavity mold and an injection core mold (not shown) for manufacturing the following Figure 2 The preform 10 shown in FIG. 1 is connected to the injection molding section 21 , and an injection device 25 for supplying a molten resin material as a raw material of the preform 10 is connected to the injection molding section 21 .
[0015] In the injection molding section 21, the above-mentioned injection cavity mold, injection core mold, and neck mold 27 of the conveying mechanism 26 are closed to form a mold space in the shape of a preform. Then, the preform 10 is manufactured by the injection molding section 21 by flowing a molten resin material from the injection device 25 into the mold space in the shape of the preform.
[0016] Here, if Figure 2 As shown, the overall shape of the preform 10 is a bottomed bowl shaped protruding downward. On the upper side of the preform 10, a cylindrical neck 11 opening upward is formed, and the bottom 12 faces the lower side of the preform 10. In addition, the neck 11 and the bottom 12 are connected by a trunk 13. It should be noted that the preform 10, for example, makes the ratio of the diameter of the neck 11 to the total length of the preform 10 to be greater than 0.5 and less than 4.0 (preferably greater than 1.0 and less than 3.0, more preferably greater than 1.1 and less than 1.5), and the shape of the trunk 13 can be roughly conical. In addition, the diameter of the neck 11 of the preform 10 can be greater than 40 mm and less than 150 mm (preferably greater than 60 mm and less than 130 mm, more preferably greater than 80 mm and less than 110 mm), and the length of the trunk 13 can be shorter than the neck 11. It should be noted that the above-described shape of the preform 10 is merely an example, and for example, the preform 10 may be in the shape of a bottomed cylinder extending in the longitudinal direction.
[0017] The material of the container and the preform 10 is a thermoplastic synthetic resin, which can be appropriately selected according to the use of the container. Specific types of materials include, for example, PET (polyethylene terephthalate), PEN (polyethylene naphthalate), PCTA (polycyclohexanedimethylene terephthalate), Tritan ((registered trademark): copolyester manufactured by Eastman Chemical Co., Ltd.), PP (polypropylene), PE (polyethylene), PC (polycarbonate), PES (polyether sulfone), PPSU (polyphenyl sulfone), PS (polystyrene), COP / COC (cyclic olefin polymer), PMMA (polymethyl methacrylate: propylene), PLA (polylactic acid), etc.
[0018] It should be noted that when the injection molding section 21 is opened, the neck mold 27 of the conveying mechanism 26 is not opened but is maintained to hold and convey the preform 10. The number of preforms 10 simultaneously molded in the injection molding section 21 (that is, the number of containers that can be simultaneously molded by the blow molding device 20) can be appropriately set.
[0019] (Temperature adjustment unit 22) The temperature regulating section 22 equalizes the temperature of the preform 10 produced in the injection molding section 21 and removes the temperature deviation, and adjusts the temperature of the preform 10 to a temperature suitable for blow molding (e.g., about 90°C to 105°C) and a temperature distribution suitable for the shape of the container to be formed. In addition, the temperature regulating section 22 also has the function of cooling the preform 10 (specifically, the main body 13 and the bottom 12) in a high-temperature state after injection molding.
[0020] Figure 2 , Figure 3 2 is a diagram showing a structural example of the temperature adjustment unit 22. As an example of a mold for temperature adjustment, Figure 2 , Figure 3 The temperature regulating section 22 shown includes a cavity mold (temperature regulating pot) 31 capable of accommodating the preform 10 (specifically, the trunk portion 13 and the bottom portion 12 ), and a temperature regulating core mold 32 .
[0021] The cavity mold 31 is an example of a first mold, and is a mold having a temperature control space of substantially the same shape as the preform 10 manufactured by the injection molding unit 21. The mold surface of the cavity mold 31 is in the shape of a bottomed bowl convex downward, and contacts the outer peripheral surface of the preform 10 (specifically, the main body 13 and the bottom 12). Figure 2 , Figure 3A flow path (not shown) through which a temperature adjustment medium (refrigerant) flows is formed inside the cavity mold 31 shown in the figure. Therefore, the temperature of the cavity mold 31 is maintained at a predetermined temperature by the temperature adjustment medium. The temperature of the temperature regulating medium of the cavity mold 31 is not particularly limited, and can be appropriately selected within a range of, for example, 5°C to 80°C, preferably 30°C to 60°C.
[0022] The temperature regulating core mold 32 has a fitting core 41 and an air introduction member 42, and is inserted inside the neck mold 27 and the preform 10. The temperature regulating core mold 32 can be in airtight contact with the neck 11 of the preform 10 when inserted into the neck mold 27.
[0023] The fitting core 41 and the air introduction member 42 are both hollow cylindrical bodies, and the air introduction member 42 is concentrically arranged inside the fitting core 41 . The interlocking core 41 is an example of a second mold, and when the temperature regulating core mold 32 is inserted into the neck mold 27, it is in close contact with the inner periphery or the upper end surface of the neck 11, and has the function of maintaining airtightness with the preform 10. In addition, between the interlocking core 41 and the air introduction member 42, a flow path for exhausting air from the preform 10 is formed along the axial direction.
[0024] The air introduction member 42 is fixed to the fitting core 41 and has a flow path for supplying compressed air (air, gaseous refrigerant) to the preform 10. An internal thread 42a is formed on the inner periphery of the end of the air introduction member 42, and a terminal core 44 is detachably mounted. The end of the air introduction member 42 is an example of a base.
[0025] The end core 44 is an example of a third mold, and is a mold component mounted on the end side of the air introduction member 42. The end core 44 has a curved surface 45 on the end side, and the curved surface 45 is a mold surface of a shape corresponding to the inner peripheral shape of the preform 10. The curved surface 45 of the end core 44 faces the bottom 12 of the preform 10 and receives the inner peripheral bottom surface of the preform 10 that is contracted. In addition, an opening 46 is formed in the end core 44, and the opening 46 penetrates the member in the axial direction from the center of the curved surface 45, and communicates with the flow path of the air introduction member 42. Here, the end core 44 is preferably formed of a material with high thermal conductivity, such as aluminum or aluminum alloy. In addition, the surface of the curved portion 45 may be roughened to make it difficult for the preform 10 to adhere. The surface roughness (arithmetic mean roughness Ra) of the curved portion 45 is set, for example, in the range of 0.6 μm to 1.0 μm.
[0026] In addition, an external thread 44a is formed on the upper end side of the terminal core 44. The terminal core 44 is attached to the air introduction member 42 by threading the external thread 44a of the terminal core 44 with the internal thread 42a of the air introduction member 42. Thus, the terminal core 44 moves integrally with the fitting core 41 and the air introduction member 42.
[0027] In addition, a spacer 47 for positioning the axial position of the curved surface portion 45 is arranged between the air introduction member 42 and the terminal core 44. For example, the spacer 47 is an annular pad through which the external thread 44a of the terminal core 44 can be inserted, and the axial position of the curved surface portion 45 can be adjusted by adjusting the number of spacers 47 sandwiched between the air introduction member 42 and the terminal core 44. It should be noted that the shape of the spacer 47 is not limited to the above-mentioned shape, and multiple spacers 47 with different thicknesses can be replaced. Alternatively, the spacer 47 may also be a columnar structure, a washer, etc. arranged at intervals in the circumferential direction.
[0028] In addition, when the temperature-controlled core mold 32 is inserted into the preform 10 (specifically, the concave space formed by the inner surface of the trunk 13 and the bottom 12), the interval L from the curved surface 45 to the mold surface of the cavity mold 31 is greater than the thickness th of the bottom 12 of the preform 10 (L>th). Figure 3 As shown, in a state where the temperature regulating core mold 32 is inserted into the preform 10 , a gap through which compressed air flows can be ensured between the curved surface portion 45 and the bottom portion 12 of the preform 10 .
[0029] (Blow molding section 23) return Figure 1 The blow molding section 23 performs stretch blow molding on the preform 10 whose temperature has been adjusted by the temperature adjustment section 22 to produce a container. The blow molding section 23 includes a blow cavity mold, a bottom mold, a stretching rod, and an air introduction member (blow core mold, all not shown) as a pair of split molds corresponding to the shape of the container. The blow molding section 23 performs blow molding while stretching the preform 10. The main body 13 and the bottom 12 of the preform 10 extending in the biaxial direction (the longitudinal direction and the transverse direction) reduce the heat retention due to the thinning of the wall, and then the thinned main body 13 and the bottom 12 are cooled due to the contact with the blow cavity mold and solidified in the shape of the container. As a result, the preform 10 is shaped into the shape of the blow cavity mold and a container can be manufactured.
[0030] (Taking out section 24) The take-out section 24 is configured to release the neck portion of the container manufactured by the blow-molding section 23 from the neck mold 27 and take the container out of the blow-molding device 20 .
[0031] (Description of Blow Molding Method) Next, a blow molding method using the blow molding device of the present embodiment will be described. Figure 4 This is a flow chart showing the steps of the blow molding method.
[0032] (Step S101: Injection Molding Process) First, in the injection molding section 21 , a molten resin is injected from the injection device 25 into a preform-shaped mold space formed by an injection cavity mold, an injection core mold, and a neck mold 27 of a conveying mechanism 26 , thereby manufacturing the preform 10 . Then, after the injection (filling and holding pressure) of the resin material is completed, or after a minimum cooling time set after the injection is completed, the injection mold of the injection molding portion 21 is opened.
[0033] From the viewpoint of manufacturing the container in a fast molding cycle, in step S101, it is preferred that the mold be opened without providing cooling time for the preform 10 in the injection mold after the injection (filling and holding pressure) of the resin material is completed.
[0034] On the other hand, when the preform 10 is cooled to the minimum extent in the injection mold, the time (cooling time) for cooling the resin material after the injection of the resin material is completed in the injection molding part 21 is preferably 1 / 2 or less of the time (injection time) for injecting the resin material. In addition, the above cooling time can be set shorter than the time for injecting the resin material according to the weight of the resin material, etc. For example, the cooling time is more preferably 2 / 5 or less, more preferably 1 / 4 or less, and particularly preferably 1 / 5 or less of the injection time of the resin material.
[0035] In this embodiment, since the preform 10 has no cooling time in the injection mold (or the cooling time is very short), the skin layer (surface layer where the resin material is cooled and solidified) of the preform is formed thinner and the core layer (internal layer where the resin material is not cooled sufficiently and is softened or molten) is formed thicker than when the preform is fully cooled in the injection mold. That is, in this embodiment, a preform 10 is formed with a large thermal gradient between the skin layer and the core layer and a high thermal retention at high temperature.
[0036] When the injection mold is opened in step S101, the preform 10 is demolded from the injection cavity mold and the injection core mold at a high temperature that can maintain the outer shape. After that, the transfer plate 28 of the conveying mechanism 26 is moved in a manner of rotating a given angle, and the preform 10 maintained at a high temperature in the neck mold 27 is conveyed to the temperature adjustment unit 22.
[0037] (Step S102: Temperature Adjustment Process) Next, in the temperature adjustment section 22 , cooling and temperature adjustment are performed to bring the temperature of the preform 10 close to a temperature suitable for final blow molding (blow molding temperature). In the temperature regulating section 22, the temperature of the preform 10 is lowered to the blow molding temperature, and then the temperature of the preform 10 is maintained at the blow molding temperature until the blow molding is performed. By rapidly cooling the high-temperature preform in the temperature regulating section 22, whitening (white turbidity) caused by spherulite crystallization that may occur when the preform is slowly cooled is suppressed. The preform is formed of a crystalline resin material (such as PET).
[0038] In the temperature regulating section 22, first, the preform 10 is accommodated in the cavity mold 31. Next, the temperature regulating core mold 32 is inserted into the neck 11 of the preform 10 accommodated in the cavity mold 31. At this time, the neck 11 of the preform 10 and the fitting core 41 are in close contact with each other to maintain an airtight state. In addition, the end core 44 of the temperature regulating core mold 32 is inserted into the preform 10, and the curved surface 45 of the end core 44 faces the bottom 12 of the preform 10.
[0039] Here, since the preform 10 transported to the temperature adjustment section 22 is at a high temperature, the preform 10 is also cooled and shrunk and deformed in a short time before the cooling blow molding described later (for example, the time taken to transport from the injection molding section to the temperature adjustment section immediately after demolding). Specifically, the preform 10 is deformed in such a way that the bottom 12 bulges inwards due to the contraction of the main body 13 and the bottom 12. Figure 2 As shown, the preform 10 is in contact with the curved surface portion 45 of the terminal core 44 , and the bottom portion 12 of the preform 10 is in close contact with (contacting) the curved surface portion 45 .
[0040] By bringing the bottom 12 of the preform 10 into close contact with the curved surface portion 45, heat exchange is performed between the bottom 12 of the preform 10 and the end core 44, and the bottom 12 of the preform 10 is effectively cooled before the cooling blow molding is performed. In addition, by bringing the bottom 12 of the preform 10 into close contact with the curved surface portion 45, the bottom 12 of the preform 10 can be maintained in a shape similar to the curved surface portion 45. Thus, irregular shrinkage of the preform 10 can be suppressed before the cooling blow molding.
[0041] After that, the preform 10 is subjected to cooling blow molding. In the cooling blow molding of the present embodiment, Figure 3 As shown, compressed air is introduced into the preform 10 from the opening 46 via the flow path of the air introduction member 42 and the end core 44 , and the compressed air is discharged from the flow path between the fitting core 41 and the air introduction member 42 .
[0042] During the cooling blow molding, if compressed air is introduced from the opening 46 of the end core 44, the bottom 12 of the preform 10 is Figure 2 The state is pushed by the compressed air and separated from the curved surface 45 of the terminal core 44. Figure 3 As shown, the outer peripheral surface of the preform 10 (specifically, the trunk 13 and the bottom 12) is pressed against the mold surface of the cavity mold 31. As a result, a gap is formed between the inner peripheral surface of the preform 10 and the curved surface 45 of the terminal core 44 for compressed air to flow.
[0043] Therefore, when the preform 10 is cooled during blow molding, a flow of compressed air is generated in the preform 10 from the bottom 12 side toward the neck 11 side, and the preform 10 is cooled from the inside due to contact with the compressed air.
[0044] In addition, during the cooling blow molding, the preform 10 is subjected to the pressure of the compressed air from the inside and is in continuous contact with the cavity mold 31 maintained at a given temperature, and heat exchange is also performed between the preform 10 and the cavity mold 31 (that is, the preform 10 is cooled and the temperature is adjusted). As a result, the temperature of the preform 10 is adjusted from the outside so as not to be lower than the temperature suitable for blow molding, and the temperature deviation generated during injection molding is also reduced. It should be noted that the shape of the preform 10 during the cooling blow molding is maintained by the cavity mold 31 and does not change significantly.
[0045] After the temperature adjustment step, the transfer plate 28 of the transport mechanism 26 moves so as to rotate by a predetermined angle, and the temperature-adjusted preform 10 held by the neck mold 27 is transported to the blow molding section 23 .
[0046] (Step S103: Blow Molding Process) Next, in the blow molding section 23, blow molding of the container is performed. First, the blow cavity mold is closed to accommodate the preform 10 in the mold space, and the air introduction member (blow core) is lowered to make the air introduction member contact the neck 11 of the preform 10. Then, the stretching rod (longitudinal axis stretching member) is lowered to press the bottom 12 of the preform 10 from the inner surface, and longitudinal axis stretching is performed as required, and the preform 10 is transversely stretched by supplying blowing air from the air introduction member. As a result, the preform 10 expands to be closely attached to the mold space of the blow cavity mold and is shaped, and blow-molded into a container. It should be noted that before the blow cavity mold is closed, the bottom mold is on standby at a lower position that does not contact the bottom of the preform 10, and quickly rises to the forming position before or after the mold is closed.
[0047] (Step S104: Container Removal Process) When the blow molding is completed, the blow cavity mold and the bottom mold are opened. Thus, the container can be moved from the blow molding section 23. Next, the transfer plate 28 of the conveying mechanism 26 is moved so as to rotate by a predetermined angle, and the container is conveyed to the take-out section 24. In the take-out section 24, the neck of the container is released from the neck mold 27, and the container is taken out of the blow molding device 20.
[0048] The above-mentioned series of processes of the blow molding method are completed. After that, the above-mentioned processes S101 to S104 are repeated by rotating the transfer plate 28 of the conveying mechanism 26 by a given angle. When the blow molding device 20 is operated, the manufacture of four sets of measuring containers is performed in parallel, and the four sets of measuring containers have a time difference of one process each.
[0049] It should be noted that in the structure of the blow molding device 20, the transfer plate 28 stops for the same length of time in the injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24. Similarly, the conveying time of the transfer plate 28 between the sections is also the same length.
[0050] Hereinafter, the effects of this embodiment will be described. In the temperature adjustment section 22 of the present embodiment, a high-temperature preform 10 that does not have a cooling time in the injection mold (or the cooling time is very short) is accommodated in the cavity mold 31, and cooling blow molding is performed by blowing compressed air into the preform 10 from the temperature regulating core mold 32, thereby cooling and adjusting the temperature of the preform 10.
[0051] Before the cooling blow molding, the bottom 12 of the shrunk preform 10 is in close contact with the curved surface 45 of the end core 44, and the bottom 12 of the preform 10 is cooled by the end core 44. Thus, before the cooling blow molding, the bottom 12 of the preform 10 can be cooled more than other parts. For example, when forming a cup container or a wide-mouth container, if the temperature is adjusted so that the preform as a whole does not reach below the blow molding temperature, the bottom of the preform is prone to insufficient cooling. If the bottom of the preform is insufficiently cooled, the following undesirable conditions (poor appearance) may occur: thin-walled residues at the bottom of the container, transfer marks of the stretch rod, etc. In addition, when the preform is formed from a crystalline resin material such as PET, it is also easy to produce an undesirable condition of spherulite crystallization (whitening) caused by insufficient cooling at the bottom of the container. In contrast, in the present embodiment, the bottom 12 of the preform 10 is locally cooled by the temperature adjustment unit 22, so that the above-mentioned undesirable conditions can be avoided.
[0052] In addition, according to the present embodiment, the bottom 12 of the shrunk preform 10 is brought into close contact with the curved surface 45 of the terminal core 44, thereby suppressing the irregular shrinkage of the preform 10 before the cooling blow molding, and further, the bottom 12 is locally cooled. Therefore, insufficient cooling of the preform 10 before the cooling blow molding and deviation in the adjustment of the temperature distribution are unlikely to occur.
[0053] Furthermore, during the cooling blow molding, the preform 10 in close contact with the terminal core 44 is pushed against the cavity mold 31 by the compressed air. Furthermore, the inner circumference of the preform 10 is cooled by the compressed air, and the outer circumference of the preform 10 is cooled and the temperature is adjusted by contact with the cavity mold 31. By the cooling blow molding, the preform 10 is pushed against the cavity mold 31, thereby restoring the shrunk preform 10 to the shape and position before the shrinkage, and the cooling of the preform 10 and the adjustment of the temperature distribution can be well performed. In particular, if the preform 10 with a relatively shallow bottom, i.e., a bottomed bowl-shaped preform shrinks both before and after cooling blow molding, it is easy to separate from the cavity mold 31, and temperature adjustment is relatively difficult. The temperature adjustment unit 22 of this embodiment can well adjust the cooling and temperature distribution of the preform 10 with a bottomed bowl-shaped preform 10 as described above, even when the preform shrinks (especially when the preform shrinks to a large extent).
[0054] In the temperature regulating section 22 of the present embodiment, the end core 44 of the temperature regulating core mold 32 is detachable, and the axial position of the curved surface portion 45 can be adjusted by interposing a spacer 47. Thus, the degree of cooling of the preform 10 caused by contact with the end core 44 and the flow of compressed air between the preform 10 and the end core 44 can be adjusted, so that the cooling of the preform 10 and the adjustment of the temperature distribution can be performed more appropriately.
[0055] The present invention is not limited to the above-described embodiments, and various improvements and design changes may be made without departing from the gist of the present invention.
[0056] In the above embodiment, as an example of a blow molding device, a 4-station device structure of a hot parison type is described. However, the blow molding device of the present invention is not limited to the above embodiment, and can also be applied to other blow molding devices other than the 4-station type as long as it has an injection molding part, a temperature adjustment part, and a blow molding part.
[0057] In the above embodiment, the area of the curved surface 45 of the end core 44 may be reduced so that the end core 44 can be brought into precise contact with a limited portion of the bottom of the preform 10. In addition, a mechanism for maintaining the temperature of the end core 44 may be provided in the temperature regulating core mold 32.
[0058] In the above embodiment, an example is described in which the opening 46 is formed at the lower end of the terminal core 44. However, the position of the opening 46 of the terminal core 44 is not limited to the above embodiment, and for example, the opening 46 may be formed on an inclined surface of the terminal core 44.
[0059] The embodiments disclosed this time are illustrative in all aspects and should not be considered restrictive. The scope of the present invention is indicated by the claims rather than the above description, and is intended to include all modifications within the meaning and scope equivalent to the claims. Explanation of symbols
[0060] 10…preform, 11…neck, 12…bottom, 20…blow molding device, 21…injection molding section, 22…temperature regulating section, 23…blow molding section, 31…cavity mold, 32…temperature regulating core mold, 41…fitting core, 42…air introduction member, 44…end core, 45…curved portion, 46…opening, 47…spacer.
Claims
1. A temperature regulating mold for regulating the temperature of a resin preform having a bottom shape produced by injection molding, comprising: A first mold, which accommodates the preform inside and contacts the outer peripheral surface of the preform; A second mold is inserted into the preform and fits closely to the neck of the preform; and A third mold is inserted into the preform integrally with the second mold, and the mold surface receives the bottom of the preform. The third mold has an opening for introducing compressed air into the preform. When the third die is inserted into the preform, a distance from the die surface of the third die to the first die is larger than a thickness of the preform.
2. The temperature regulating mold according to claim 1, wherein: The third mold uses the mold surface to bear the bottom of the preform that shrinks before the compressed air is introduced. The first die receives the outer peripheral surface of the preform pressed by the compressed air introduced from the opening.
3. The temperature regulating mold according to claim 2, wherein: The compressed air introduced from the opening flows between the third die and the inner peripheral surface of the preform pressed by the first die.
4. The temperature regulating mold according to any one of claims 1 to 3, wherein The temperature adjustment mold further includes an adjustment unit that adjusts a distance between the third mold and the first mold.
5. The temperature regulating mold according to claim 4, wherein: The third mold is detachably mounted on a base fixed to the second mold. The adjustment portion is a spacer that adjusts an installation position of the third mold relative to the base.
6. A temperature control method, comprising: controlling the temperature of a resin preform having a bottom shape which is injection molded by using a temperature control mold; The temperature adjustment mold comprises: A first mold, which accommodates the preform inside and contacts the outer peripheral surface of the preform; A second mold, which is inserted into the preform and closely fits the neck of the preform; as well as A third mold is inserted into the preform integrally with the second mold, and the mold surface receives the bottom of the preform. The third mold has an opening for introducing compressed air into the preform. The temperature adjustment method comprises the following steps: In a first step, the preform is housed in the first mold, and the second mold and the third mold are inserted into the preform; The second step is to use the mold surface of the third mold to bear the shrinkage of the bottom of the preform before the compressed air is introduced; as well as In a third step, the compressed air is introduced from the opening of the third die to press the outer peripheral surface of the preform against the first die with the compressed air, and the preform is cooled with the compressed air.
7. A manufacturing device for a resin container, comprising: An injection molding section that injection molds a preform made of a resin; a temperature regulating section comprising a temperature regulating mold according to any one of claims 1 to 5, and performing temperature regulation of the preform produced by the injection molding section; and The blow molding section blows the temperature-controlled preform to produce a resin container.