Intelligent electric arc control method and device and storage medium
By scanning the weld gaps in real time and adjusting the welding parameters, the problems of insufficient melting depth and burn-through caused by uneven gaps in thick plate welding are solved, and the welding quality is improved.
Patent Information
- Application Number
- CN202411320424.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-11-22
AI Technical Summary
During the welding process of thick plates, due to the large size of the workpiece, it is difficult to ensure that the gap is consistent, resulting in the problem of insufficient melting depth at small gaps during the welding process and burning through at large gaps.
The intelligent arc control method is adopted to ensure the consistency of welding quality by scanning the weld root gap in real time and adjusting welding parameters such as current, voltage and wire feeding speed in real time.
It effectively avoids insufficient melting depth and burn-through problems caused by uneven gaps, and significantly improves welding quality.
Smart Images

Figure CN118989519A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an intelligent arc control method, device and storage medium, belonging to the technical field of welding. Background Art
[0002] In the construction machinery and other industries, there are often welding between thick plates. Generally, the welding between thick plates adopts the method of opening grooves and blunt edges to leave gaps and adopts multi-layer and multi-pass welding. Such welding workpieces are as short as a few meters and as long as tens of meters. The method of opening grooves and blunt edges of workpieces is mostly machined. Although the size of grooves and blunt edges can be guaranteed, it is difficult to achieve consistent gaps during actual assembly due to the large size of workpieces. In this way, during the welding process of the entire weld, the gap is sometimes larger than the specified size and sometimes smaller than the specified size. For some small-sized or small-batch workpieces, the blunt edges are manually polished, so the consistency of the blunt edges is difficult to ensure, and the consistency of the gaps cannot be guaranteed during assembly.
[0003] In actual production, the current method is to set the preset current, voltage and welding speed, use arc sensing or laser sensing, and weld along the root of the groove. This will cause insufficient penetration at the location of small gaps, and burn-through at the location of large gaps. Summary of the invention
[0004] The technical problem to be solved by the present invention is to overcome the defects of the prior art and provide an intelligent arc control method, which can adjust the welding parameters in real time according to the actual gap, so as to avoid problems such as insufficient penetration at the position with small gap and burn-through at the position with large gap.
[0005] In order to solve the above technical problems, the technical solution adopted by the present invention is:
[0006] In a first aspect, the present invention provides an intelligent arc control method, comprising the following steps:
[0007] Scan the gap at the root of the weld in real time to obtain the real-time gap at the root of the weld;
[0008] The real-time gap is compared with the preset standard gap, and the arc standard parameters corresponding to the standard gap are adjusted according to the comparison result to obtain the real-time parameters of the arc;
[0009] The arc real-time parameters are sent to the welding part, so that the welding part performs welding operation according to the arc real-time parameters.
[0010] The standard arc parameters include standard current, standard voltage, standard wire feeding speed and standard welding speed; the real-time arc parameters include real-time current, real-time voltage, real-time wire feeding speed and real-time welding speed.
[0011] In the arc standard parameters, let the standard gap be b0, its corresponding standard current be I0, standard wire feeding speed be W0, standard voltage be U0, and standard welding speed be V0. The relationship between wire feeding speed W0 and standard current I0 is as follows: W0=K1*(I0) 2 +K2*I0+K3, where K1, K2 and K3 are constants; the relationship between the standard wire feeding speed W0 and the standard welding speed V0 is as follows: S0=W0 / V0, where S0 is the cross-sectional area of the standard weld.
[0012] When the real-time gap is larger than the standard gap, the real-time gap is recorded as b1, and the adjusted real-time current I1 is calculated as follows: I1=I0+K4*(b0-b1), and the adjusted real-time voltage U1 is calculated as follows: U1=U0+K5*(b0-b1), K4 and K5 are positive constants, respectively. The relationship between the adjusted real-time wire feeding speed W1 and the real-time current I1 is as follows: W1=K1*(I1) 2 +K2*I1+K3, the relationship between the adjusted real-time wire feeding speed W1 and the real-time welding speed V1 is as follows: S0+(p+h)*(b1-b0)=W1 / V1, where p is the blunt edge length and h is the residual height.
[0013] When the real-time gap is smaller than the standard gap, the real-time gap is recorded as b2, and the adjusted real-time current I2 is calculated as follows: I2=I0+K6*(b0-b1), and the adjusted real-time voltage U2 is calculated as follows: U2=U0+K7*(b0-b1), K6 and K7 are positive constants, respectively. The relationship between the adjusted real-time wire feeding speed W2 and the real-time current I2 is as follows: W2=K1*(I2) 2 +K2*I1+K3, the relationship between the adjusted real-time wire feeding speed W2 and the real-time welding speed V2 is as follows: S0+(p+h)*(b2-b0)=W2 / V2, where p is the blunt edge length and h is the excess height.
[0014] The scanning position during the welding process should be in front of the welding position, and the distance between the scanning position and the welding position is fixed.
[0015] The adjusting of the arc standard parameters corresponding to the standard gap according to the comparison result is specifically: when it is determined that the real-time gap changes relative to the standard gap, the arc standard parameters are adjusted in real time, or when it is determined that the real-time gap changes relative to the standard gap to a preset threshold, the arc standard parameters are adjusted in real time.
[0016] The preset threshold is a percentage of the standard gap, specifically, the ratio of the absolute value of the gap change to the standard gap multiplied by 100%.
[0017] In a second aspect, the present invention provides an intelligent arc control device, comprising:
[0018] Real-time gap acquisition adjustment is used to scan the gap at the root of the weld in real time and obtain the real-time gap at the root of the weld;
[0019] The arc real-time parameter adjustment module is used to compare the real-time gap with the preset standard gap, and adjust the arc standard parameters corresponding to the standard gap according to the comparison result to obtain the arc real-time parameters;
[0020] The welding operation module is used to send the arc real-time parameters to the welding part, so that the welding part performs welding operation according to the arc real-time parameters.
[0021] In a third aspect, the present invention provides a computer-readable storage medium having a computer program / instruction stored thereon, which, when executed by a processor, implements the steps of the intelligent arc control method.
[0022] Beneficial effects of the invention: The invention provides an intelligent arc control method, device and storage medium, which performs real-time scanning on the root gap of the weld to obtain the real-time gap of the weld root, and then compares the real-time gap with a preset standard gap. According to the comparison result, the arc standard parameters corresponding to the standard gap are adjusted to obtain the real-time parameters of the arc. During the welding process, the welding current, welding voltage, wire feeding speed and welding speed are adjusted in real time to ensure the consistency of the penetration depth even under the condition of uneven root gap, avoid problems such as insufficient penetration depth at the position with small gap and burn-through at the position with large gap, and greatly improve the welding quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 This is a schematic diagram of the joint form and assembly gap of the thick plate bevel weld;
[0024] Figure 2 Schematic diagram of the penetration depth of the base weld at different root gaps;
[0025] Figure 3 This is a schematic diagram of the working principle of the welding gun and laser generator controlled by the present invention;
[0026] Figure 4 It is a schematic diagram of a new control adjustment method for different root gaps of the present invention. DETAILED DESCRIPTION
[0027] The present invention will be further described below in conjunction with the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solutions of the present invention and are not intended to limit the protection scope of the present invention.
[0028] Example 1
[0029] The present invention discloses an intelligent arc control method, which is mainly used for gas shielded arc welding of carbon steel, stainless steel, aluminum alloy, and other nonferrous metals under gap welding conditions, and is suitable for pulse and short-circuit welding modes, and mainly includes the following steps:
[0030] Scan the gap at the root of the weld in real time to obtain the real-time gap at the root of the weld;
[0031] The real-time gap is compared with the preset standard gap, and the arc standard parameters corresponding to the standard gap are adjusted according to the comparison result to obtain the real-time parameters of the arc;
[0032] The arc real-time parameters are sent to the welding part, so that the welding part performs welding operation according to the arc real-time parameters.
[0033] The present invention adjusts the welding current, welding voltage, wire feeding speed and welding speed in real time during the welding process, thereby ensuring the consistency of the penetration depth even under the condition of uneven root gap, avoiding problems such as insufficient penetration depth at a position with a small gap and burn-through at a position with a large gap, and greatly improving the welding quality.
[0034] Example 2
[0035] In thick plate welding, the actual production is often carried out by opening a groove and blunt edge and leaving a gap. The groove angle a, blunt edge p, gap b, plate thickness t are as follows: Figure 1 (a) As shown in the figure. The actual welded workpieces are as short as a few meters or as long as tens of meters. It is difficult to achieve a consistent gap in the actual assembly, resulting in the root gap of the weld of tens of meters being larger in some places and smaller in others. The specific schematic diagram is shown in the figure. Figure 1 (b) shown.
[0036] Thick plate welding usually sets a fixed current, voltage, and welding speed to weld the entire weld. If the root gap can be kept consistent, the weld penetration can meet the requirements, such as Figure 2 (a). If the root gap is larger than the required gap, it is easy to weld through, such as Figure 2 (b). If the root gap is smaller than the required gap, there will be lack of fusion at the root of the weld, such as Figure 2 (c) shown.
[0037] The present invention discloses an intelligent arc control method, comprising the following steps:
[0038] Step 1: Scan the gap at the root of the weld in real time to obtain the real-time gap at the root of the weld. The present invention uses a fixed line laser at the front end of the welding gun to scan the gap b at the root of the weld in real time. The scanning position during welding should be in front of the welding position, and the distance m between the line laser and the arc is known. In this way, the welding current, welding voltage, wire feeding speed and welding speed can be adjusted in real time. The specific working diagram is shown in FIG. Figure 3 shown.
[0039] Step 2, compare the real-time gap with the pre-set standard gap, adjust the arc standard parameters corresponding to the standard gap according to the comparison results, and obtain the arc real-time parameters. In the present invention, the arc standard parameters include standard current, standard voltage, standard wire feeding speed and standard welding speed; the arc real-time parameters include real-time current, real-time voltage, real-time wire feeding speed and real-time welding speed. In the present invention, the arc standard parameters corresponding to the standard gap are adjusted according to the comparison results, specifically: when the real-time gap is judged to change relative to the standard gap, the arc standard parameters are adjusted in real time, or when the real-time gap is judged to change relative to the standard gap to a preset threshold, the arc standard parameters are adjusted in real time. Among them, the preset threshold △a is a percentage of the standard gap, specifically the absolute value of the gap change and the ratio of the standard gap multiplied by one hundred percent, which can be any value between 1% and 30% in actual use.
[0040] The present invention first makes a current and voltage database that can ensure that the weld formation meets the requirements when the gaps are different, and finds the relationship between the current and voltage corresponding to the different gaps through data fitting. There is also a fitting relationship between different currents I and wire feeding speeds W, and the wire feeding speed W can be calculated by the known current I. In the arc standard parameters, let the standard gap be b0, its corresponding standard current be I0, standard wire feeding speed be W0, standard voltage be U0, and standard welding speed be V0, then the relationship between wire feeding speed W0 and standard current I0 is as follows: W0=K1*(I0) 2 +K2*I0+K3, where K1, K2 and K3 are constants.
[0041] In the first case, when the line laser detects that the root gap of the weld has increased to b1, the real-time adjusted current is I1, and the real-time adjusted voltage is U1. The adjusted real-time current I1 is calculated as follows: I1=I0+K4*(b0-b1), K4 is a positive value. In this way, when the root gap increases, the actual welding current decreases, and the corresponding voltage can be selected as the unified voltage corresponding to I1, or the voltage can be automatically matched according to the expert database. The adjusted real-time voltage U1 is calculated as follows: U1=U0+K5*(b0-b1), K5 is a positive value, thereby preventing root burn-through. The relationship between the real-time wire feeding speed W1 and the real-time current I1 is as follows: W1=K1*(I1) 2+K2*I1+K3.
[0042] According to the requirements for the first layer of weld reinforcement h, it can be calculated that when the groove angle is a, the blunt edge is p, and the root gap is b0, the cross-sectional area of the first weld is S0. The calculation method of S0 is as follows: S0=b0*(p+h)+(h 2 *tanα) / 2. Figure 4 As shown in (a), the welding speed V0 can be calculated by the following equation: S0=W0 / V0. When the line laser detects that the gap at the root of the weld has increased to b1, the current adjusted in real time is I1, and the corresponding wire feeding speed is W1, as shown in Figure 4 As shown in (b), the welding speed V1 at this time can be calculated by the following equation: S0+(p+h)*(b1-b0)=W1 / V1. In the above formula, all other values except V1 are known, so V1=W1 / {S0+(p+h)*(b1-b0)}.
[0043] In the second case, when the real-time gap is smaller than the real-time gap, the real-time gap is recorded as b2, and the adjusted real-time current I2 is calculated as follows: I2=I0+K6*(b0-b1), K6 is a positive value, so when the root gap becomes smaller, the actual welding current becomes larger, and the corresponding voltage can be selected as the unified voltage corresponding to I2, or the voltage can be automatically matched according to the expert database. The adjusted real-time voltage U2 is calculated as follows: U2=U0+K7*(b0-b1), K7 is a positive value, thereby preventing the root from not being fully melted. The relationship between the real-time wire feeding speed W2 and the real-time current I2 is as follows: W2=K1*(I2) 2 +K2*I1+K3.
[0044] According to the requirements for the first layer of weld reinforcement h, it can be calculated that when the groove angle is a, the blunt edge is p, and the root gap is b0, the cross-sectional area of the first weld is S0. The calculation method of S0 is as follows: S0=b0*(p+h)+(h 2 *tanα) / 2. When the line laser detects that the gap at the root of the weld has become smaller to b2, the current adjusted in real time is I2, and the corresponding wire feeding speed is W2, such as Figure 4 As shown in (c), the welding speed V2 at this time can be calculated by the following equation: S0+(p+h)*(b2-b0)=W2 / V2. In the above formula, all other values except V2 are known, so V2=W2 / {S0+(p+h)*(b2-b0)}.
[0045] Step three, perform welding operations according to real-time arc parameters.
[0046] Example 3
[0047] This embodiment discloses an intelligent arc control device, including:
[0048] Real-time gap acquisition adjustment is used to scan the gap at the root of the weld in real time and obtain the real-time gap at the root of the weld;
[0049] The arc real-time parameter adjustment module is used to compare the real-time gap with the preset standard gap, and adjust the arc standard parameters corresponding to the standard gap according to the comparison result to obtain the arc real-time parameters;
[0050] The welding operation module is used to send the arc real-time parameters to the welding part, so that the welding part performs welding operation according to the arc real-time parameters.
[0051] Example 4
[0052] This embodiment introduces a computer-readable storage medium on which a computer program is stored. When the program is executed by a processor, the steps of the method described in Embodiment 1 or 2 are executed.
[0053] It will be appreciated by those skilled in the art that embodiments of the present invention may be provided as methods, systems, or computer program products. Therefore, the present invention may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Furthermore, the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program code.
[0054] The present invention is described with reference to flowcharts and / or block diagrams of methods, devices (systems), and computer program products according to embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to produce a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0055] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1A function specified in one or more boxes.
[0056] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.
[0057] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. An intelligent arc control method, characterized in that: The following steps are involved: Scan the gap at the root of the weld in real time to obtain the real-time gap at the root of the weld; The real-time gap is compared with the preset standard gap, and the arc standard parameters corresponding to the standard gap are adjusted according to the comparison result to obtain the real-time parameters of the arc; The arc real-time parameters are sent to the welding part, so that the welding part performs welding operation according to the arc real-time parameters.
2. The intelligent arc control method according to claim 1, characterized in that: The standard arc parameters include standard current, standard voltage, standard wire feeding speed and standard welding speed; the real-time arc parameters include real-time current, real-time voltage, real-time wire feeding speed and real-time welding speed.
3. The intelligent arc control method according to claim 2, characterized in that: In the arc standard parameters, let the standard gap be b0, its corresponding standard current be I0, standard wire feeding speed be W0, standard voltage be U0, and standard welding speed be V0. The relationship between wire feeding speed W0 and standard current I0 is as follows: W0=K1*(I0) 2 +K2*I0+K3, where K1, K2 and K3 are constants; the relationship between the standard wire feeding speed W0 and the standard welding speed V0 is as follows: S0=W0 / V0, where S0 is the cross-sectional area of the standard weld.
4. The intelligent arc control method according to claim 3, characterized in that: When the real-time gap is larger than the standard gap, the real-time gap is recorded as b1, and the adjusted real-time current I1 is calculated as follows: I1=I0+K4*(b0-b1), and the adjusted real-time voltage U1 is calculated as follows: U1=U0+K5*(b0-b1), K4 and K5 are positive constants, respectively. The relationship between the adjusted real-time wire feeding speed W1 and the real-time current I1 is as follows: W1=K1*(I1) 2 +K2*I1+K3, the relationship between the adjusted real-time wire feeding speed W1 and the real-time welding speed V1 is as follows: S0+(p+h)*(b1-b0)=W1 / V1, where p is the blunt edge length and h is the residual height.
5. The intelligent arc control method according to claim 3, characterized in that: When the real-time gap is smaller than the standard gap, the real-time gap is recorded as b2, and the adjusted real-time current I2 is calculated as follows: I2=I0+K6*(b0-b1), and the adjusted real-time voltage U2 is calculated as follows: U2=U0+K7*(b0-b1), K6 and K7 are positive constants, respectively. The relationship between the adjusted real-time wire feeding speed W2 and the real-time current I2 is as follows: W2=K1*(I2) 2 +K2*I1+K3, the relationship between the adjusted real-time wire feeding speed W2 and the real-time welding speed V2 is as follows: S0+(p+h)*(b2-b0)=W2 / V2, where p is the blunt edge length and h is the excess height.
6. The intelligent arc control method according to claim 1, characterized in that: The scanning position during the welding process should be in front of the welding position, and the distance between the scanning position and the welding position is fixed.
7. The intelligent arc control method according to claim 1, characterized in that: The adjusting of the arc standard parameters corresponding to the standard gap according to the comparison result is specifically: when it is determined that the real-time gap changes relative to the standard gap, the arc standard parameters are adjusted in real time, or when it is determined that the real-time gap changes relative to the standard gap to a preset threshold, the arc standard parameters are adjusted in real time.
8. The intelligent arc control method according to claim 7, characterized in that: The preset threshold is a percentage of the standard gap, specifically, the ratio of the absolute value of the gap change to the standard gap multiplied by 100%.
9. An intelligent arc control device, characterized in that: include; Real-time gap acquisition adjustment is used to scan the gap at the root of the weld in real time and obtain the real-time gap at the root of the weld; The arc real-time parameter adjustment module is used to compare the real-time gap with the preset standard gap, and adjust the arc standard parameters corresponding to the standard gap according to the comparison result to obtain the arc real-time parameters; The welding operation module is used to send the arc real-time parameters to the welding part, so that the welding part performs welding operation according to the arc real-time parameters.
10. A computer-readable storage medium having a computer program / instruction stored thereon, characterized in that: When the computer program / instruction is executed by a processor, the steps of the intelligent arc control method described in any one of claims 1-8 are implemented.
Citation Information
Cited By
Welding control method, system, program product, medium and apparatus
CN120901488A