Flow sensor packaging method
By using the chip-mounting groove and copper clad layer structure in the MEMS flow sensor and combining sealant fixation, the chip surface unevenness and glue connection problems are solved, the accuracy and stability of the fluid flow rate are improved, and the measurement accuracy of the sensor is enhanced. and scope of application.
Patent Information
- Application Number
- CN202411135069.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-11-22
AI Technical Summary
The existing MEMS flow sensor packaging method causes uneven chip surfaces, affecting the accuracy and stability of fluid flow velocity, and the glue connection can easily lead to media fluctuations and thermal isolation cavity overflow, affecting measurement accuracy.
Using a chip-loading groove and copper-clad layer structure, the chip is set on the substrate and fixed by sealant to eliminate the height difference between the chip and the substrate, and prevent the sealant from overflowing through micro grooves and pressure balance holes, ensuring that the chip surface is flat and Stable connection.
It improves the accuracy and stability of the fluid flow rate, avoids the fluctuations in fluid media affecting measurement accuracy, and enhances the reliability and application range of the sensor.
Smart Images

Figure CN118992969A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a flow sensor packaging method, belonging to the technical field of micro-electromechanical sensors. Background Art
[0002] MEMS (Micro Electro Mechanical Systems) flow sensor is a fluid measurement method based on the principle of heat exchange. Due to its unique advantages such as small size, low power consumption, wide range ratio, high sensitivity, and ultra-low starting flow, MEMS flow sensor is widely used in many fields such as industry, medical treatment, semiconductor, and new energy. The packaging method of MEMS flow sensor has an important impact on the performance and reliability of the product. The packaging structure ensures that the medium flowing through the sensor is laminar flow and ensures that the sensor is not damaged in the application of sudden pressure changes.
[0003] The Chinese utility model patent with announcement number CN216038651U discloses a sensor structure and an electronic device, the sensor structure comprising: a silicon substrate; a film structure arranged on one side of the silicon substrate, wherein a cavity is arranged on the side of the silicon substrate away from the film structure; a packaging substrate, the packaging substrate is arranged on the side of the silicon substrate away from the film structure; a connecting layer, arranged between the silicon substrate and the packaging substrate, a first gap is formed in the connecting layer, and the first gap is used to connect the cavity with the environment outside the sensor structure. The sensor structure provided by the embodiment of the application can simplify the process, improve production efficiency and reduce costs, but still has the following shortcomings:
[0004] 1. After the chip is bonded to the substrate, there is a certain height difference between the substrate and the chip surface. When the fluid flows over the chip surface, especially when the flow rate is high, obvious eddy currents are generated on the chip surface, thus affecting the accurate measurement and stability of the fluid flow rate;
[0005] 2. The flow sensor chip is connected to the substrate by glue packaging, which may easily cause the chip surface to tilt. When the fluid medium flows through the chip surface, it is easy to cause medium fluctuations and affect the measurement accuracy. Moreover, due to the small base area of the sensor chip and the use of glue packaging, the glue is easy to overflow into the thermal isolation cavity of the sensor, which will cause the zero-point output of the sensor to be too large.
[0006] Therefore, a flow sensor packaging method is needed to achieve a flat chip surface and improve the accuracy and stability of measuring fluid flow rate. Summary of the invention
[0007] The technical problem to be solved by the present invention is: in order to overcome the deficiencies of the prior art, a flow sensor packaging method is provided to achieve chip surface flatness and improve the accuracy and stability of measuring fluid flow rate.
[0008] The technical solution adopted by the present invention to solve the above problem is: a flow sensor packaging method, comprising the following steps:
[0009] Step S1, preparing a substrate;
[0010] Step S1.1, opening a wafer loading slot on the upper surface of the substrate;
[0011] Step S1.2, copper is coated on the bottom of the wafer loading slot to form a copper coating layer, there is a gap between the copper coating layer and the front, back, left and right inner walls of the wafer loading slot, the gap forms a micro groove, and then a pressure balance hole is opened on the upper surface of the copper coating layer, the pressure balance hole extends upward to the lower surface of the substrate;
[0012] Step S2, applying sealant;
[0013] Applying sealant in the micro grooves;
[0014] Step S3, chip loading;
[0015] Step S3.1, place the chip into the chip loading slot, with the lower surface of the chip in contact with the copper cladding layer, the front, back, left, and right sides of the chip are all connected with the sealant, and through size calculation, the upper surface of the chip and the upper surface of the substrate are in the same plane;
[0016] Step S3.2, curing the sealant to fix the chip and the substrate;
[0017] The chip includes a dielectric layer and a substrate which are sequentially distributed from top to bottom. A thermal isolation cavity is arranged on the lower surface of the substrate. The thermal isolation cavity extends to the upper surface of the substrate. The thermal isolation cavity is directly connected to the pressure balance hole. The position of the dielectric layer directly opposite to the thermal isolation cavity is a suspended sensitive film area. Three thermistors are arranged in the suspended sensitive film area.
[0018] Step S4, bonding;
[0019] Using a wire to electrically connect a first pad on the upper surface of the substrate and a second pad on the upper surface of the chip;
[0020] Step S5, coating;
[0021] The first pad, the second pad and the wire are completely covered with the coating adhesive.
[0022] Preferably, the copper cladding layer has a thickness of 48um to 52um, with a specific value of 50um.
[0023] Preferably, the microgroove width is 0.15 mm.
[0024] Preferably, the substrate is made of FR4 or ceramic.
[0025] Preferably, the thickness of the sealant is 68um to 72um, with a specific value of 70um.
[0026] Preferably, the sealant is epoxy glue.
[0027] Preferably, two groups of first silk screen layers are provided on the upper surface of the substrate, and the two groups of first silk screen layers are arranged symmetrically about the film loading slot. Each group of first silk screen layers is provided with two, and the two first silk screen layers in the same group are respectively arranged on the left and right sides of the suspended sensitive film area.
[0028] Preferably, the conductive wire is a gold wire or an aluminum wire.
[0029] Preferably, the lower surface of the chip is consistent in size with the lower surface of the copper cladding layer.
[0030] Preferably, an annular second silk-screen layer is provided on the upper surface of the substrate, and the coating glue is placed in the annular hole of the second silk-screen layer.
[0031] Compared with the prior art, the advantages of the present invention are:
[0032] 1. By placing the chip in the chip loading slot on the substrate, the upper surface of the chip and the upper surface of the substrate are in the same plane, eliminating the height difference between the chip and the substrate, and improving the accuracy and stability of measuring the fluid flow rate;
[0033] 2. The chip and substrate are bonded and sealed with sealant, so that the bottom of the chip does not need to be connected to the substrate with glue, to prevent the glue on the bottom of the chip from being uneven and the thermal expansion and contraction of the glue from causing the upper surface of the chip to tilt, thereby avoiding changes in the fluid medium above the suspended sensitive film area and affecting the measurement accuracy. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 A cross-sectional view of a flow sensor packaging method of the present invention;
[0035] Figure 2 It is a structural schematic diagram of step S1.1;
[0036] Figure 3 It is a structural schematic diagram of the method of step S1.2;
[0037] Figure 4 It is a structural schematic diagram of step S2;
[0038] Figure 5 It is a structural diagram of step S3;
[0039] Figure 6 It is a structural diagram of step S4;
[0040] Figure 7 It is a structural diagram of step S5;
[0041] Figure 8 This is the relationship diagram between the sensor output and the set air flow rate.
[0042] in:
[0043] Substrate 1, chip 2, chip loading slot 3, pressure balance hole 4, first pad 5, second pad 6, wire 7, copper clad layer 8, sealant 9, coating glue 10, first silk screen layer 11, second silk screen layer 12, micro groove 13;
[0044] Dielectric layer 201 , substrate 202 , thermal isolation cavity 203 , suspended sensitive film region 204 , thermistor 205 . DETAILED DESCRIPTION
[0045] like Figure 1-8 As shown, a flow sensor packaging structure in this embodiment includes a substrate 1 and a chip 2, the upper surface of the substrate 1 is concave to form a chip loading slot 3, the chip 2 is arranged in the chip loading slot 3, the upper surface of the substrate 1 is provided with a first pad 5, the upper surface of the chip 2 is provided with a second pad 6, the first pad 5 and the second pad 6 are electrically connected through a wire 7, the wire 7 is a gold wire or an aluminum wire, and the upper surface of the chip 2 and the upper surface of the substrate 1 are in the same plane;
[0046] The substrate 1 is made of FR4 or ceramic. FR4 is a common composite material and is widely used in the electronic and electrical industry. FR4 is a thermosetting plastic composite material composed of glass fiber and epoxy resin, and has excellent insulation, mechanical strength and heat resistance.
[0047] The first pad 5, the second pad 6 and the wire 7 are coated by a coating adhesive 10;
[0048] A copper coating 8 is provided at the bottom of the chip loading slot 3, and the lower surface of the chip 2 is bonded to the copper coating 8. The thickness of the copper coating 8 is 48um to 52um, and the specific value is 50um. The front, back, left, and right sides of the chip 2 are respectively connected to the front, back, left, and right side walls of the chip loading slot 3 through a sealant 9.
[0049] A pressure balance hole 4 is provided on the upper surface of the copper cladding layer 8, and the pressure balance hole 4 extends upward to the lower surface of the substrate 1;
[0050] The length, width and height of the chip loading slot 3 are respectively 0.15mm, 0.15mm and 0.1mm larger than those of the chip 2;
[0051] The chip 2 includes a dielectric layer 201 and a substrate 202 which are sequentially arranged from top to bottom. A thermal isolation cavity 203 is arranged on the lower surface of the substrate 202. The thermal isolation cavity 203 extends to the upper surface of the substrate 202. The thermal isolation cavity 203 is directly connected to the pressure balance hole 4. The position of the dielectric layer 201 directly opposite the thermal isolation cavity 203 is a suspended sensitive film area 204. Three thermistors 205 are arranged in the suspended sensitive film area 204. Here, the pressure balance hole 4 is used to protect the suspended sensitive film area 204 to prevent the suspended sensitive film area 204 from being damaged due to a sudden pressure change.
[0052] A gap is provided between the suspended sensitive film area 204 and the coating adhesive 10;
[0053] Two groups of first silk-screen layers 11 are arranged on the upper surface of the substrate 1, and the two groups of first silk-screen layers 11 are arranged symmetrically with respect to the chip loading slot 3. Each group of first silk-screen layers 11 is provided with two, and the two first silk-screen layers 11 in the same group are arranged on the left and right sides of the suspended sensitive film area 204, respectively. The first silk-screen layers 11 facilitate quick alignment of the suspended sensitive film area 204 with the pressure balance hole 4 when the chip 2 is loaded;
[0054] The upper surface of the substrate 1 is provided with an annular second silk-screen layer 12, and the coating glue 10 is placed in the annular hole of the second silk-screen layer 12. The coating range of the coating glue 10 is determined by the second silk-screen layer 12 to prevent the coating glue 10 from being too large or too small in area and affecting the product yield;
[0055] The thickness of the sealant 9 is 68um to 72um, and the specific value is 70um;
[0056] The sealant 9 is epoxy glue, which has a small thermal expansion coefficient and helps to stabilize the size of the sensor package;
[0057] A flow sensor packaging method comprises the following steps:
[0058] Step S1, preparing a substrate 1;
[0059] Step S1.1, opening a wafer loading slot 3 on the upper surface of the substrate 1;
[0060] Step S1.2, copper is coated on the bottom of the film loading slot 3 to form a copper coating 8, the thickness of the copper coating 8 is 48um-52um, and the specific value is 50um. There is a gap between the copper coating 8 and the front, back, left and right inner walls of the film loading slot 3, and the gap forms a micro groove 13, and the width of the micro groove 13 is 0.15mm. Then, a pressure balance hole 4 is opened on the upper surface of the copper coating 8, and the pressure balance hole 4 extends upward to the lower surface of the substrate 1;
[0061] The substrate 1 is made of FR4 or ceramic. FR4 is a common composite material and is widely used in the electronic and electrical industry. FR4 is a thermosetting plastic composite material composed of glass fiber and epoxy resin, and has excellent insulation, mechanical strength and heat resistance.
[0062] Step S2, applying sealant 9;
[0063] A sealant 9 is applied in the micro groove 13, and the thickness of the sealant 9 is 68um to 72um, and the specific value is 70um;
[0064] The sealant 9 is epoxy glue, which has a small thermal expansion coefficient and helps to stabilize the size of the sensor package;
[0065] Step S3, chip 2 is loaded;
[0066] Step S3.1, placing the chip 2 into the chip loading slot 3, with the lower surface of the chip 2 in contact with the copper cladding layer 8, and the four sides of the chip 2, front, back, left, and right, are all connected to the sealant 9, wherein the lower surface of the chip 2 is consistent in size with the lower surface of the copper cladding layer 8, and through size calculation, the upper surface of the chip 2 is in the same plane as the upper surface of the substrate 1;
[0067] Step S3.2, curing the sealant 9 to fix the chip 2 and the substrate 1;
[0068] Here, the chip 2 includes a dielectric layer 201 and a substrate 202 which are sequentially arranged from top to bottom. A thermal isolation cavity 203 is arranged on the lower surface of the substrate 202. The thermal isolation cavity 203 extends to the upper surface of the substrate 202. The thermal isolation cavity 203 is directly connected to the pressure balance hole 4. The position of the dielectric layer 201 directly facing the thermal isolation cavity 203 is a suspended sensitive film area 204. Three thermistors 205 are arranged in the suspended sensitive film area 204.
[0069] By providing the micro grooves 13, it is possible to facilitate the coating of the sealant 9 and prevent the sealant 9 from overflowing to the thermal isolation cavity 203;
[0070] The upper surface of the substrate 1 is provided with two groups of first silk-screen layers 11, which are arranged symmetrically front and back about the chip loading slot 3, and each group of first silk-screen layers 11 is provided with two. The two first silk-screen layers 11 in the same group are respectively arranged on the left and right sides of the suspended sensitive film area 204, so that the suspended sensitive film area 204 can be quickly aligned with the pressure balance hole 4 when the chip 2 is loaded through the first silk-screen layers 11;
[0071] Step S4, bonding;
[0072] Use a wire 7 to electrically connect a first pad 5 on the upper surface of the substrate 1 and a second pad 6 on the upper surface of the chip 2;
[0073] The wire 7 is a gold wire or an aluminum wire;
[0074] Step S5, coating;
[0075] The first pad 5, the second pad 6 and the wire 7 are completely covered with the coating glue 10, and a gap is provided between the suspended sensitive film area 204 and the coating glue 10;
[0076] The upper surface of the substrate 1 is provided with an annular second silk-screen layer 12, and the coating glue 10 is placed in the annular hole of the second silk-screen layer 12. The coating range of the coating glue 10 is determined by the second silk-screen layer 12 to prevent the coating glue 10 from being too large or too small in area and affecting the product yield;
[0077] In summary, the chip 2 and the substrate 1 are bonded and sealed by the sealant 9, so that the bottom of the chip 2 does not need to be connected to the substrate 1 by glue, which prevents the glue on the bottom of the chip 2 from being uneven and the thermal expansion and contraction of the glue from causing the upper surface of the chip 2 to tilt, thereby avoiding the change of the fluid medium on the suspended sensitive film area 204 and affecting the measurement accuracy. Secondly, by arranging the chip 2 in the chip loading slot 3 on the substrate 1, the upper surface of the chip 2 and the upper surface of the substrate 1 are in the same plane, eliminating the height difference between the chip 2 and the substrate 1, and improving the accuracy and stability of measuring the fluid flow rate;
[0078] In addition, according to the curve of sensor output and set air flow rate, it can be concluded that this packaging structure can make the surface of chip 2 flush with the surface of substrate 1. When the fluid passes through the surface of chip 2 from the surface of substrate 1, the fluid disturbance will not be introduced due to the uneven surface and affect the measurement accuracy. It can also increase the range ratio of the sensor to more than 300:1, expanding the application scenarios of the product.
[0079] This flow sensor has a simple packaging process, low cost, easy implementation, a wider dynamic measurement range, and increased product added value;
[0080] In addition to the above embodiments, the present invention also includes other implementation modes. Any technical solutions formed by equivalent transformation or equivalent replacement should fall within the protection scope of the claims of the present invention.
Claims
1. A flow sensor packaging method, Features: The steps include: Step S1, preparing a substrate (1); Step S1.1, opening a wafer loading slot (3) on the upper surface of the substrate (1); Step S1.2, copper is coated on the bottom of the wafer loading slot (3) to form a copper coating layer (8), a gap exists between the copper coating layer (8) and the front, back, left and right inner walls of the wafer loading slot (3), the gap forms a micro groove (13), and then a pressure balance hole (4) is opened on the upper surface of the copper coating layer (8), and the pressure balance hole (4) extends upward to the lower surface of the substrate (1); Step S2, applying sealant (9); Applying a sealant (9) in the micro groove (13); Step S3, chip (2) is loaded; Step S3.1, placing the chip (2) into the chip loading slot (3), with the lower surface of the chip (2) being in contact with the copper cladding layer (8), and the front, back, left, and right sides of the chip (2) being connected to the sealant (9), and by dimensional calculation, the upper surface of the chip (2) and the upper surface of the substrate (1) being in the same plane; Step S3.2, curing the sealant (9) to fix the chip (2) and the substrate (1); The chip (2) comprises a dielectric layer (201) and a substrate (202) which are sequentially arranged from top to bottom; a thermal isolation cavity (203) is arranged on the lower surface of the substrate (202); the thermal isolation cavity (203) extends to the upper surface of the substrate (202); the thermal isolation cavity (203) is directly connected to the pressure balance hole (4); the position of the dielectric layer (201) directly opposite the thermal isolation cavity (203) is a suspended sensitive film area (204); and three thermistors (205) are arranged in the suspended sensitive film area (204); Step S4, bonding; Using a wire (7) to electrically connect a first pad (5) on the upper surface of the substrate (1) and a second pad (6) on the upper surface of the chip (2); Step S5, coating; The first solder pad (5), the second solder pad (6) and the wire (7) are completely covered with a covering glue (10).
2. A flow sensor packaging method according to claim 1, Features: The copper cladding layer (8) has a thickness of 48um to 52um, with a specific value of 50um.
3. A flow sensor packaging method according to claim 1, Features: The width of the micro groove (13) is 0.15 mm.
4. A flow sensor packaging method according to claim 1, Features: The substrate (1) is made of FR4 or ceramic.
5. A flow sensor packaging method according to claim 1, Features: The thickness of the sealant (9) is 68um to 72um, with a specific value of 70um.
6. A flow sensor packaging method according to claim 1, Features: The sealant (9) is epoxy glue.
7. A flow sensor packaging method according to claim 1, Features: Two groups of first silk-screen layers (11) are arranged on the upper surface of the substrate (1), the two groups of first silk-screen layers (11) are arranged symmetrically in front and back with respect to the film loading slot (3), each group of first silk-screen layers (11) is provided with two, and the two first silk-screen layers (11) in the same group are respectively arranged on the left and right sides of the suspended sensitive film area (204).
8. A flow sensor packaging method according to claim 1, Features: The conductive wire (7) is a gold wire or an aluminum wire.
9. A flow sensor packaging method according to claim 1, Features: The lower surface of the chip (2) is consistent in size with the lower surface of the copper cladding layer (8).
10. A flow sensor packaging method according to claim 1, Features: The upper surface of the substrate (1) is provided with an annular second silk-screen layer (12), and the coating glue (10) is placed in the annular hole of the second silk-screen layer (12).