Bacterium-containing magnetic slurry for dam repair and grouting method

By using a bacterial magnetic grout and injection method, and employing ultrasonic detection and magnetic grout injection into dam cracks, combined with the self-repairing properties of the repairing bacteria, the problem of dam crack expansion was solved, achieving efficient and environmentally friendly dam repair.

CN118993605APending Publication Date: 2024-11-22CHINA THREE GORGES UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411014954.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Improper construction and maintenance of membrane bag concrete dams can easily lead to irregular cracks, resulting in reduced durability and safety. In particular, the cracks can widen under the scouring of seawater, affecting the quality of the project.

Method used

The method employs a bacterial magnetic grout and injection technique. Cracks are measured using an ultrasonic detector. Magnetic grout and restorative porous rock are injected into the cracks, which are then self-healed by restorative bacteria. Moisture is treated using a sealing layer and suction equipment to ensure uniform grout distribution.

Benefits of technology

It improves the strength and durability of the repaired dam, achieving self-repair and efficient, environmentally friendly repair effects, and is suitable for the durable and efficient repair of dams.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118993605A_ABST
    Figure CN118993605A_ABST
Patent Text Reader

Abstract

The present invention provides a bacterium-containing magnetic slurry for dam repair, the bacterium-containing magnetic slurry comprises water, concrete, a water reducing agent, a curing agent, a flocculant, K39 epoxy resin and magnetic powder, the water cement ratio of the concrete is 0.35-0.5, the mass ratio of the concrete and the water is 50-72.5%, the mass ratio of the magnetic powder is 20-50%, and the mass ratio of the water reducing agent, the curing agent, the flocculant, the K39 epoxy resin and the magnetic powder is 20-50%. The mass ratio of the water reducing agent is 1%-4%, the mass ratio of the K39 epoxy resin is 1.5%-5%, and the mass ratio of the flocculating agent is 5%-8%. The method has the advantages of durability, high efficiency, environment friendliness, self-repairing property and the like, and has wide practical significance and application prospects in engineering.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of dam microbial magnetic slurry repair, and in particular to a bacteria-containing magnetic slurry and a grouting method for dam repair. Background Art

[0002] Due to its advantages of convenient and fast construction, strong integrity and good stability, film bag concrete is widely used in engineering construction, especially in dam slope protection, bank protection, deep water bank protection, bottom protection and other protective projects, which greatly improves the overall quality of construction and plays a pivotal role in engineering protection. However, due to problems such as non-standard construction and neglect of concrete maintenance in the later stage, irregular cracks appear in the film bag concrete, which will cause the cracks to expand further and the internal concrete to calcify under the scouring of seawater, affecting the durability and safety of the project.

[0003] Therefore, there is an urgent need for a bacteria-containing magnetic slurry and a grouting method for dam repair to solve the above problems. Summary of the invention

[0004] The purpose of the present invention is to overcome the above-mentioned shortcomings and provide a bacterial-containing magnetic slurry and a grouting method for dam repair to solve the problems raised in the background technology.

[0005] In order to solve the above technical problems, the technical solution adopted by the present invention is: a bacterial magnetic slurry for dam repair, including water, concrete, a water reducer, a curing agent, a flocculant, a K39 epoxy resin and magnetic powder, the water-cement ratio of the concrete is 0.35-0.5, the mass proportion of the concrete + water is 50%-72.5%, the mass proportion of the magnetic powder is 20%-50%, the mass proportion of the water reducer is 1%-4%, the mass proportion of the K39 epoxy resin is 1.5%-5%, and the mass proportion of the flocculant is 5%-8%.

[0006] In addition, the present invention also discloses a grouting method of a bacteria-containing magnetic slurry for dam repair, which comprises the following steps: Step 1. Materials and tools preparation: water, concrete, water reducing agent, curing agent, flocculant, anti-dispersant, K39 epoxy resin, magnetic powder, restorative porous rock, grouting pipe, sealing pad, fixing screws, clamps, plugging tape, magnetic components and grouting equipment; Step 2. Measure cracks: Aim the probe of the ultrasonic detector at the object to be measured, start the device and begin measuring; Step 3 Data Analysis: Based on the received signal, the ultrasonic detector will display the pulse waveform on the screen; Step 4. Prepare magnetic slurry: water, concrete, water reducing agent, curing agent, flocculant, anti-dispersant, K39 epoxy resin and magnetic powder are stirred in the required proportion to prepare magnetic slurry; Step 5. Install the magnetic component: install the magnetic component at the pre-designed position in the crack; Step 6. Seal the cracks: Use a sealing pad and fixing screws to seal the cracks, wrap the sealing tape around the suction pipe interface, and reinforce it with a clamp. Wrap the sealing tape around the suction pipe interface, and use a suction device to extract the moisture in the cracks; Step 7. Install the grouting equipment: Assemble the grouting pipe and related accessories according to the design requirements, and then fix the grouting pipe on the reserved grouting hole; Step 8. Grouting: Mix the magnetic slurry and the restorative porous rock together and inject them into the cracks. Turn on the grouting equipment and inject the slurry into the formation through the grouting pipe. Step 9. End grouting: When all the magnetic slurry is injected, turn off the grouting equipment, remove the grouting pipe from the predetermined position, wait for the slurry to solidify, remove the sealing pad layer and other devices, and then clean the equipment for next use; Step 10. Inspection and maintenance: After completing the grouting work, the repair area needs to be inspected to confirm whether the expected effect has been achieved.

[0007] Furthermore, the restorative porous rock in Step 1 includes: porous rock, restorative bacteria and flocs, and flocs are added to the porous rock, and the flocs wrap the magnetic powder and the restorative bacteria.

[0008] Furthermore, in Step 6, a sealing gasket layer is placed at the crack and fixed with fixing screws, and holes are reserved on the sealing gasket layer for grouting and suction.

[0009] Furthermore, during the grouting process of Step 8, it is necessary to control the grouting speed and observe the grouting situation at all times.

[0010] Furthermore, in Step 10, the building structure needs to be maintained and serviced regularly.

[0011] The present invention has the following beneficial effects: 1. The magnetic slurry used in the present invention is a mixture of high-strength concrete, magnetic powder, flocculant, water reducer, K39 epoxy resin, and curing agent. The purpose is to add a variety of materials to improve the strength and durability of cracks after repair; 2. The purpose of adding repair bacteria, magnetic powder and floccules to the repair porous rock developed by the present invention is to make the repair porous rock magnetic and adsorbed by magnetic components, so that the repair bacteria can secrete substances when it is subsequently damaged to repair the cracks; the floccules can better wrap the materials and make it easier for the materials to stay in the holes; 3. The sealing cushion layer selected in the present invention has reserved suction holes and grouting holes. The purpose is that when the cracks are sealed with the sealing cushion layer, a large amount of liquid such as water will remain. It is easier to grout by using a suction machine to drain the water through the reserved holes before grouting. 4. The magnetic slurry and the restorative porous rock used in the present invention are grouted simultaneously, the purpose of which is to make the restorative porous rock more evenly distributed in the cracks, so as to facilitate the subsequent repair of the cracks by bacteria; 5. The present invention has the advantages of durability, high efficiency, environmental protection, self-repair, etc. and has broad practical significance and application prospects in engineering. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 Schematic diagram of grouting state; Figure 2 Schematic diagram of magnetic component attracting magnetic slurry; Figure 3 This is a schematic diagram of restorative porous rock; Figure 4 This is a detailed diagram of the holes in the restorative porous rock; Figure 5 Schematic diagram of the repair of the damaged dock. DETAILED DESCRIPTION

[0013] The present invention will be further described below in conjunction with the accompanying drawings and embodiments: See also Figures 1 to 5A bacterial magnetic slurry for dam repair includes water, concrete, a water reducer, a curing agent, a flocculant, a K39 epoxy resin and magnetic powder. The water-cement ratio of the concrete is 0.35-0.5, the mass proportion of the concrete + water is 50%-72.5%, the mass proportion of the magnetic powder is 20%-50%, the mass proportion of the water reducer is 1%-4%, the mass proportion of the K39 epoxy resin is 1.5%-5%, and the mass proportion of the flocculant is 5%-8%. In the present invention, the water reducer is selected from polycarboxylic acid water reducer, the curing agent is selected from epoxy resin curing agent, the flocculant is selected from polyacrylamide flocculant, and the anti-dispersion agent is selected from underwater anti-dispersion grouting material; K39 epoxy resin enhances the bonding and sealing properties of cement, and the epoxy resin curing agent is used to improve the strength and durability of cement; the repair bacteria such as Bacillus pasteurianus and Bacillus candidum selected in the present invention have the following capabilities: 1. Self-repair: When cracks appear in concrete, water will penetrate from the cracks; at this time, the bacterial spores germinate and begin to devour calcium lactate, consume oxygen, and soluble lactic acid Calcium is converted into insoluble limestone, which begins to harden and automatically fills the cracks without any external force. ② Durability: Naturally present in extremely alkaline lakes near volcanoes, these tenacious bacteria can produce limestone. This characteristic makes the cracks filled with this magnetic slurry more durable. ③ High efficiency: Bacillus pasteurianus uses urea and calcium source solution as substrates for mineralization. It contains a urease that can decompose urea into NH3 and CO2. NH3 is highly soluble in water and generates OH, which promotes the conversion of CO2 to CO32-. At the same time, the bacterial surface carries a negative charge, which continuously combines with cations (Ca2+) in the solution, and uses itself as a nucleation site to react with CO32- to form calcium carbonate crystals. The precipitation generation amount in this process is large and the rate is high. ④ Environmental protection: Microbial remediation is an environmentally friendly remediation method that does not require additional chemicals or energy input.

[0014] In addition, the present invention also discloses a grouting method of a bacteria-containing magnetic slurry for dam repair, which comprises the following steps: Step 1. Materials and tools preparation: water, concrete, water reducing agent, curing agent, flocculant, anti-dispersant, K39 epoxy resin, magnetic powder, restorative porous rock, grouting pipe 1, sealing pad 2, fixing screws 3, clamps 4, plugging tape 5, magnetic components 6 and grouting equipment 7; Step 2. Measure cracks: Aim the probe of the ultrasonic detector at the object to be measured, start the device and begin measuring; Step 3. Data analysis: Based on the received signal, the ultrasonic detector will display the pulse waveform on the screen; Step 4. Prepare magnetic slurry: water, concrete, water reducing agent, curing agent, flocculant, anti-dispersant, K39 epoxy resin and magnetic powder are stirred in the required proportion to prepare magnetic slurry; Step 5. Install the magnetic component 6: Install the magnetic component 6 at a pre-designed position in the crack; Step 6. Seal the cracks: seal the cracks with a sealing pad 2 and fixing screws 3, wrap the leak-proof tape 5 around the suction pipe interface, and reinforce the leak-proof tape 5 around the suction pipe interface with a clamp 4, and use a suction device to extract the moisture in the cracks; Step 7. Install grouting equipment 7: Assemble the grouting pipe 1 and related accessories according to the design requirements, and then fix the grouting pipe 1 on the reserved grouting hole; Step 8. Grouting: Mix the magnetic slurry and the restorative porous rock together and inject them into the cracks. Turn on the grouting equipment 7 to allow the slurry to be injected into the formation through the grouting pipe 1. Step 9. End grouting: When all the magnetic slurry is injected, turn off the grouting equipment 7, remove the grouting pipe 1 from the predetermined position, wait for the slurry to solidify, remove the sealing pad layer 2 and other devices, and then clean the equipment for next use; Step 10. Inspection and maintenance: After completing the grouting work, the repair area needs to be inspected to confirm whether the expected effect has been achieved.

[0015] Furthermore, the restorative porous rock in Step 1 includes: porous rock, restorative bacteria and flocs, and flocs are added to the porous rock, and the flocs wrap the magnetic powder and the restorative bacteria.

[0016] Furthermore, in Step 6, a sealing gasket layer 2 is placed at the crack and fixed with fixing screws 3, and holes are reserved on the sealing gasket layer 2 for grouting and suction.

[0017] Furthermore, during the grouting process of Step 8, it is necessary to control the grouting speed and observe the grouting situation at all times.

[0018] Furthermore, in Step 10, the building structure needs to be maintained and serviced regularly.

[0019] The above embodiments are only preferred technical solutions of the present invention and should not be regarded as limiting the present invention. The protection scope of the present invention shall be the technical solutions recorded in the claims, including equivalent replacement solutions of the technical features in the technical solutions recorded in the claims. That is, equivalent replacement improvements within this scope are also within the protection scope of the present invention.

Claims

1. A bacteria-containing magnetic slurry for dam repair, characterized in that: It includes water, concrete, water reducing agent, curing agent, flocculant, K39 epoxy resin and magnetic powder. The water-cement ratio of the concrete is 0.35-0.5, the mass proportion of the concrete + water is 50%-72.5%, the mass proportion of the magnetic powder is 20%-50%, the mass proportion of the water reducing agent is 1%-4%, the mass proportion of the K39 epoxy resin is 1.5%-5%, and the mass proportion of the flocculant is 5%-8%.

2. The grouting method of a bacterial magnetic slurry for dam repair according to claim 1, characterized in that: It includes the following steps: Step 1. Preparation of materials and tools: water, concrete, water reducing agent, curing agent, flocculant, anti-dispersant, K39 epoxy resin, magnetic powder, restorative porous rock, grouting pipe (1), sealing cushion (2), fixing screws (3), clamp (4), plugging tape (5), magnetic component (6) and grouting equipment (7); Step 2. Measure cracks: Aim the probe of the ultrasonic detector at the object to be measured, start the device and begin measuring; Step 3. Data analysis: Based on the received signal, the ultrasonic detector will display the pulse waveform on the screen; Step 4. Prepare magnetic slurry: water, concrete, water reducing agent, curing agent, flocculant, anti-dispersant, K39 epoxy resin and magnetic powder are stirred in the required proportion to prepare magnetic slurry; Step 5. Install the magnetic component (6): install the magnetic component (6) at a pre-designed position in the crack; Step 6. Seal the cracks: Use a sealing pad (2) and fixing screws (3) to seal the cracks, wrap the sealing tape (5) around the suction pipe interface, and reinforce the sealing tape (5) around the suction pipe interface with a clamp (4), and use a suction device to extract the moisture in the cracks; Step 7. Install the grouting equipment (7): Assemble the grouting pipe (1) and related accessories according to the design requirements, and then fix the grouting pipe (1) on the reserved grouting hole; Step 8. Grouting: Mix the magnetic slurry and the restorative porous rock together and inject them into the cracks. Turn on the grouting equipment (7) and allow the slurry to be injected into the formation through the grouting pipe (1); Step 9. End of grouting: When all the magnetic slurry is injected, the grouting equipment (7) is turned off, and the grouting pipe (1) is removed from the predetermined position, and the sealing pad layer (2) and other devices are removed after the slurry solidifies, and then the equipment is cleaned for next use; Step 10. Inspection and maintenance: After completing the grouting work, the repair area needs to be inspected to confirm whether the expected effect has been achieved.

3. The grouting method of a bacterial magnetic slurry for dam repair according to claim 2, characterized in that: The restorative porous rock in Step 1 comprises: porous rock, restorative bacteria and floccules. Floccules are added to the porous rock, and the floccules wrap the magnetic powder and the restorative bacteria.

4. The grouting method of the bacterial magnetic slurry for dam repair according to claim 2 is characterized in that: In step 6, a sealing cushion layer (2) is placed at the crack and fixed with fixing screws (3), and holes are reserved on the sealing cushion layer (2) for grouting and suction.

5. The grouting method of the bacterial magnetic slurry for dam repair according to claim 2, characterized in that: During the grouting process of Step 8, it is necessary to control the grouting speed and observe the grouting situation at all times.

6. The grouting method of the bacterial magnetic slurry for dam repair according to claim 2, characterized in that: In Step 10, the building structure needs to be maintained and serviced regularly.