Graphene antibacterial plastic
By blending modified graphene oxide with polypropylene resin and combining antioxidants and lubricants, the problem of insufficient antibacterial properties of existing plastic materials is solved, and efficient antibacterial, flame retardant and mechanical properties are achieved, ensuring graphene The chemical stability and long-term properties of antibacterial plastics.
Patent Information
- Application Number
- CN202411307190.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-19
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing plastic materials lack antibacterial properties and are prone to breed harmful bacteria under specific conditions, affecting the hygiene of food, medicine and daily necessities. Moreover, graphene agglomeration in organic polymer materials leads to a decline in performance and cannot fully exert its antibacterial properties.
Modified graphene oxide is blended with polypropylene resin, and the dispersion and antibacterial properties of graphene are improved through amidation and quaternization reactions, and antioxidants and lubricants are added to form excellent antioxidant, antibacterial and flame retardant. Performance graphene antibacterial plastic.
It significantly enhances the flame retardant, antibacterial and mechanical strength of the plastic, improves chemical stability and oxidation resistance, avoids graphene agglomeration, and ensures the long-term stability and efficient performance of the material.
Smart Images

Figure FKCTYI5ACZLDI47VUJBWMEEWKE2TUUHQBCMQXQP0 
Figure IBB2PYJLH76FWM86SABSCXRNGXHYIAOZL5ZVJS98 
Figure YBPDJGXXHXTE5HORCBC3GRBVABPTRBOZIF71XMGB
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of antibacterial plastics, and specifically relates to a graphene antibacterial plastic. Background Art
[0002] With the continuous improvement of living standards, people's health awareness is gradually increasing, and their requirements for their living environment are getting higher and higher. Especially in the fields of food, medicine and agricultural product packaging and daily necessities such as pens, mobile phones, computers, toothbrushes, furniture, etc., the hygiene requirements for the materials used are getting higher and higher. In public places such as stations, squares, parks, etc., the flow of people is very large, and public facilities are frequently used, which is easy to produce germs and spread easily, affecting public health. At present, plastic products are increasingly widely used in these fields due to their unique properties.
[0003] Common plastic materials include polyethylene, polypropylene, polyvinyl chloride, etc., but these plastics themselves do not have antibacterial properties. When used as packaging materials for food, medicine, etc., under the specific temperature and humidity conditions for storing food and medicine, the plastic surface is prone to breed bacteria and other microorganisms that are harmful to human health. The growth and reproduction of microorganisms will contaminate the stored food or medicine, causing it to deteriorate, mold, or even rot. Daily necessities in life such as toothbrushes and tableware are also very likely to produce pathogens during use, which directly affect human health.
[0004] Graphene is a two-dimensional honeycomb planar structure composed of tightly stacked single-layer carbon atoms. Its thickness is only 0.34nm, making it the thinnest material known in the world. This special structural feature makes graphene the basic unit for building other dimensional carbon materials. Graphene has excellent mechanical, electrical, thermal and barrier properties. In addition to these properties, researchers have found in recent years that graphene also has good biocompatibility and antibacterial properties. However, directly adding graphene to organic polymer materials will cause graphene to agglomerate, which will not only result in the performance of graphene not being fully utilized, but also reduce the performance of the material. Therefore, it is urgent to solve the above problems to meet the higher requirements in the field of antibacterial plastic technology. Summary of the invention
[0005] The purpose of the present invention is to overcome the defects of the prior art and provide a graphene antibacterial plastic.
[0006] The purpose of the present invention can be achieved through the following technical solutions: A graphene antibacterial plastic is prepared by the following steps: The polypropylene resin was dried in an oven for 12 hours, added into a mixing barrel with modified graphene oxide, an antioxidant and a lubricant, mixed, poured into a twin-screw extruder, melt-blended and extruded to obtain graphene antibacterial plastic.
[0007] Furthermore, the raw materials are calculated in parts by weight as follows: 80-100 parts of polypropylene resin, 10-20 parts of modified graphene oxide, 3-9 parts of antioxidant, and 2-6 parts of lubricant.
[0008] Furthermore, the antioxidant is obtained by compounding phosphite and hindered phenol antioxidant in a mass ratio of 1:2.
[0009] Furthermore, the lubricant is one of stearic acid, zinc stearate, calcium stearate, aluminum stearate, magnesium stearate and stearic acid amide.
[0010] Polypropylene is used as the matrix, which gives the plastic a certain mechanical strength and chemical stability; the antioxidants are phosphites and hindered phenol antioxidants, among which phosphites can act as a type of auxiliary antioxidant and can synergize with hindered phenol antioxidants to greatly enhance the antioxidant properties of plastics.
[0011] Furthermore, the modified graphene oxide is prepared by the following steps: S1. Add 3,5-diaminopyridine, diethylphosphoacetic acid, dicyclohexylcarbodiimide (DCC, dehydrating agent) and pyridine to a three-necked flask equipped with a stirring device, stir and mix well, place in a 55°C water bath, and heat in a water bath for 6 hours. After the reaction is completed, filter, remove the solvent by vacuum distillation, and then purify by column chromatography (the eluent is a mixed solvent of benzene / ethyl acetate, and the volume ratio of the two is 2:3), and remove the eluent by rotary evaporation to obtain an intermediate; the ratio of 3,5-diaminopyridine, diethylphosphoacetic acid, dicyclohexylcarbodiimide and pyridine is 12.4g:19.6g:20.6g:100mL; Under the action of dicyclohexylcarbodiimide, 3,5-diaminopyridine and diethylphosphoacetic acid undergo amidation reaction. By controlling the molar ratio of the two to be close to 1:1 and a slight excess of 3,5-diaminopyridine, only one amino group on 3,5-diaminopyridine participates in the reaction to obtain an intermediate. The specific reaction process is as follows: S2. After mixing the intermediate with N,N-dimethylformamide (DMF) in a three-necked flask equipped with a stirring device, add dicyclohexylcarbodiimide and stir evenly; then slowly add graphene oxide dispersion (DMF as a dispersion medium, concentration of 10 mg / mL), stir magnetically while adding, ultrasonically treat for 40 minutes to make it dispersed evenly, react at 60°C for 12 hours, stir continuously during the reaction, and after the reaction is completed, vacuum distillation, ethyl acetate washing, and freeze-drying to obtain pre-modified graphene oxide; the ratio of the intermediate, N,N-dimethylformamide, dicyclohexylcarbodiimide, and graphene oxide dispersion is 6.5g:100mL:5.5g:100mL; Under the action of dicyclohexylcarbodiimide, the amino group of the intermediate undergoes an amidation reaction with the carboxyl group on the surface of graphene oxide, and the amino group on the intermediate 1 is grafted onto the graphene oxide to obtain pre-modified graphene oxide. The specific reaction process is as follows: S3. Add pre-modified graphene oxide and N,N-dimethylformamide to a three-necked flask equipped with a stirring device and disperse them evenly by ultrasonication, then slowly drop ethyl bromide. After the dropwise addition is completed, control the reaction temperature to 70°C, keep the reaction for 8 hours, stir continuously during the reaction, and after the reaction is completed, perform vacuum distillation, wash with ethanol, cool and dry to obtain modified graphene oxide; the ratio of pre-modified graphene oxide, N,N-dimethylformamide, and ethyl bromide is 1g:100mL:25mL; The pre-modified graphene oxide undergoes a quaternization reaction with ethyl bromide to obtain modified graphene oxide; the structure of the modified graphene oxide is shown below: The graphene material used is graphene oxide, which has better biocompatibility and dispersibility and more excellent comprehensive performance; graphene oxide has certain antibacterial and flame retardant properties, and by grafting an organic molecular chain on the graphene oxide, that is, forming an organic layer on its surface, the surface hydrophobicity of the graphene oxide is improved, thereby improving the interface compatibility between the graphene oxide and the polypropylene matrix, so that the antibacterial and flame retardant properties of the graphene oxide are fully exerted, and the mechanical strength of the matrix can be enhanced; in addition, the modified graphene oxide also contains pyridinium quaternary ammonium salt, amide group and P element, wherein the pyridinium quaternary ammonium salt is a new type of quaternary ammonium salt, its positive charge is more concentrated, and the bactericidal ability is stronger, avoiding the problem of bacterial resistance caused by the long-term use of quaternary ammonium salt antibacterial agents in large quantities, and can synergize with graphene oxide to greatly enhance the antibacterial property of the matrix; in addition, the amide group is a hydrophobic group, which can further enhance the surface hydrophobicity of the graphene oxide and improve the compatibility with the matrix; finally, the introduced P element can synergize with the N element and the graphene oxide to significantly enhance the flame retardant property of the matrix; It should be noted that the graphene oxide grafted onto the organic molecular chain can effectively protect the organic molecular chain, improve its resistance to migration and permeation, and ensure the long-term stability of the performance of the modified graphene oxide.
[0012] Beneficial effects of the present invention: 1. The plastic produced by the present invention uses polypropylene as a matrix, which gives the plastic a certain mechanical strength and chemical stability; 2. The added antioxidants are phosphite and hindered phenol antioxidants, which can play a synergistic role and greatly enhance the antioxidant properties of plastics; 3. By modifying graphene oxide, the compatibility with the matrix is better than that of ordinary graphene oxide, the agglomeration phenomenon is significantly reduced, and the flame retardancy, antibacterial properties and mechanical strength of the plastic can be significantly enhanced. The performance is stable and not easy to fall off; Therefore, the plastic produced by the present invention has good chemical stability, high mechanical strength, excellent antioxidant performance, and stable and efficient flame retardancy and antibacterial properties, and has important application value in the field of antibacterial plastic technology. DETAILED DESCRIPTION
[0013] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0014] Example 1 Preparation of modified graphene oxide: S1. Add 12.4 g 3,5-diaminopyridine, 19.6 g diethylphosphoacetic acid, 20.6 g dicyclohexylcarbodiimide and 100 mL pyridine to a three-necked flask equipped with a stirring device, stir and mix evenly, place in a 55° C. water bath, and heat in a water bath for 6 h. After the reaction is completed, filter, remove the solvent by vacuum distillation, and then purify by column chromatography (the eluent is a mixed solvent of benzene / ethyl acetate, the volume ratio of the two is 2:3), and remove the eluent by rotary evaporation to obtain an intermediate; S2. After mixing 6.5 g of the intermediate with 100 mL of N,N-dimethylformamide in a three-necked flask equipped with a stirring device, 5.5 g of dicyclohexylcarbodiimide was added and stirred evenly; then 100 mL of graphene oxide dispersion (DMF as a dispersion medium with a concentration of 10 mg / mL) was slowly added, while magnetic stirring was applied, ultrasonic treatment was performed for 40 min to make it evenly dispersed, and the mixture was reacted at 60° C. for 12 h, with continuous stirring during the reaction. After the reaction was completed, vacuum distillation, washing with ethyl acetate, and freeze-drying were performed to obtain pre-modified graphene oxide; S3. Add 1 g of pre-modified graphene oxide and 100 mL of N,N-dimethylformamide to a three-necked flask equipped with a stirring device, and ultrasonically disperse them evenly. Then slowly drop 25 mL of ethyl bromide. After the addition is complete, control the reaction temperature to 70°C and keep the reaction for 8 hours. Stir continuously during the reaction. After the reaction is completed, distill under reduced pressure, wash with ethanol, and cool and dry to obtain modified graphene oxide.
[0015] Example 2 Preparation of modified graphene oxide: S1. Add 24.8 g 3,5-diaminopyridine, 39.2 g diethylphosphoacetic acid, 41.2 g dicyclohexylcarbodiimide and 200 mL pyridine to a three-necked flask equipped with a stirring device, stir and mix well, place in a 55° C. water bath, and heat in a water bath for 6 h. After the reaction is completed, filter, remove the solvent by vacuum distillation, and then purify by column chromatography (the eluent is a mixed solvent of benzene / ethyl acetate, the volume ratio of the two is 2:3), and remove the eluent by rotary evaporation to obtain an intermediate; S2. After mixing 13 g of the intermediate with 200 mL of N,N-dimethylformamide in a three-necked flask equipped with a stirring device, 11 g of dicyclohexylcarbodiimide was added and stirred evenly; then 200 mL of graphene oxide dispersion (DMF as a dispersion medium with a concentration of 10 mg / mL) was slowly added, while magnetic stirring was applied, ultrasonic treatment was performed for 40 min to make it evenly dispersed, and the mixture was reacted at 60° C. for 12 h, with continuous stirring during the reaction. After the reaction was completed, vacuum distillation, washing with ethyl acetate, and freeze-drying were performed to obtain pre-modified graphene oxide; S3. Add 2 g of pre-modified graphene oxide and 200 mL of N,N-dimethylformamide into a three-necked flask equipped with a stirring device, and disperse them evenly by ultrasonication. Then slowly drop 50 mL of ethyl bromide. After the addition is complete, control the reaction temperature to 70°C and keep the reaction for 8 hours. Stir continuously during the reaction. After the reaction is completed, perform vacuum distillation, wash with ethanol, and cool and dry to obtain modified graphene oxide.
[0016] Example 3 After drying 80 g of polypropylene resin in an oven for 12 h, 10 g of the modified graphene oxide prepared in Example 1, 3 g of antioxidant (compounded with 1 g of antioxidant 168 and 2 g of antioxidant 1010) and 2 g of zinc stearate were added to a mixing barrel and mixed, then poured into a twin-screw extruder, melt-blended and extruded to obtain a graphene antibacterial plastic.
[0017] Example 4 After drying 90 g of polypropylene resin in an oven for 12 h, 15 g of modified graphene oxide prepared in Example 2, 6 g of antioxidant (compounded with 2 g of antioxidant 168 and 4 g of antioxidant 1010) and 4 g of calcium stearate were added to a mixing barrel and mixed, then poured into a twin-screw extruder, melt-blended and extruded to obtain graphene antibacterial plastic.
[0018] Example 5 After drying 100 g of polypropylene resin in an oven for 12 h, 20 g of the modified graphene oxide prepared in Example 2, 9 g of antioxidant (3 g of antioxidant 168 and 6 g of antioxidant 1010) and 6 g of calcium stearate were added to a mixing barrel and mixed, then poured into a twin-screw extruder, melt-blended and extruded to obtain graphene antibacterial plastic.
[0019] Comparative Example 1 Ordinary graphene oxide of the same mass was used to replace the modified graphene oxide in Example 5, and the remaining steps were the same as in Example 5 to obtain a plastic.
[0020] Comparative Example 2 Use commercially available polypropylene antimicrobial plastic.
[0021] Examples 3-5 and comparative examples 1-2 were made into corresponding shapes according to different test standards and subjected to the following performance tests: The tensile strength was determined using the national standard GB / T 1040-2006 "Determination of tensile properties of plastics"; The oxidation induction time was determined using the national standard GB / T 19466.6-2009 "Plastic Differential Scanning Calorimetry"; The national standard GB / T 2406-2008 "Test method for combustion performance of plastics" is used to determine the limiting oxygen index of the sample; QB / T 2591-2003A "Test Methods and Antibacterial Effects of Antibacterial Plastics" was used to determine the antibacterial rates of Staphylococcus aureus and Escherichia coli before and after the samples were placed at room temperature for 180 days. The measured results are shown in the following table: It can be seen from the above table that the mechanical strength, flame retardancy and antibacterial properties of the plastics prepared in the embodiments of the present invention are higher than those of the control examples, and the plastics have excellent antioxidant properties and long-term stable properties, and have important application value in the field of antibacterial plastic technology.
[0022] In the description of the specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.
[0023] The above contents are merely examples and explanations of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the invention or exceed the scope defined by the claims, they shall all fall within the protection scope of the present invention.
Claims
1. A graphene antibacterial plastic, characterized in that: The invention comprises the following raw materials in parts by weight: 80-100 parts of polypropylene resin, 10-20 parts of modified graphene oxide, 3-9 parts of antioxidant, and 2-6 parts of lubricant; Wherein, the modified graphene oxide is prepared by the following steps: S1. Stir and mix 3,5-diaminopyridine, diethylphosphoacetic acid, dicyclohexylcarbodiimide and pyridine, place in a water bath at 55°C, heat in the water bath for 6 hours, and after the reaction is completed, filter, distill under reduced pressure, purify by column chromatography, and rotary evaporate to obtain an intermediate; S2. After mixing the intermediate with N,N-dimethylformamide, add dicyclohexylcarbodiimide and stir evenly; then slowly add the graphene oxide dispersion, stir while adding, and perform ultrasonic treatment to make it disperse evenly, react at 60° C. for 12 h, stir continuously during the reaction, and after the reaction is completed, perform vacuum distillation, wash, and freeze-dry to obtain pre-modified graphene oxide; S3. After the pre-modified graphene oxide and N,N-dimethylformamide are uniformly dispersed by ultrasonic mixing, ethyl bromide is added dropwise. After the addition is completed, the mixture is reacted at 70°C for 8 hours with continuous stirring during the reaction. After the reaction is completed, the mixture is distilled under reduced pressure, washed, cooled and dried to obtain modified graphene oxide.
2. The graphene antibacterial plastic according to claim 1, characterized in that: In step S1, the ratio of 3,5-diaminopyridine, diethylphosphoacetic acid, dicyclohexylcarbodiimide and pyridine is 12.4 g: 19.6 g: 20.6 g: 100 mL.
3. The graphene antibacterial plastic according to claim 1, characterized in that: In step S2, the ratio of the amount of the intermediate, N,N-dimethylformamide, dicyclohexylcarbodiimide, and graphene oxide dispersion is 6.5 g:100 mL:5.5 g:100 mL.
4. The graphene antibacterial plastic according to claim 1, characterized in that: In step S3, the ratio of the amount of pre-modified graphene oxide, N,N-dimethylformamide, and ethyl bromide is 1 g:100 mL:25 mL.
5. The graphene antibacterial plastic according to claim 1, characterized in that: The antioxidant is prepared by mixing phosphite and hindered phenol antioxidant in a mass ratio of 1:
2.
6. The graphene antibacterial plastic according to claim 1, characterized in that: The lubricant is one of stearic acid, zinc stearate, calcium stearate, aluminum stearate, magnesium stearate and stearic acid amide.
Citation Information
Patent Citations
Graphene compounded anti-impact PP (Polypropylene) plastic and preparation method thereof
CN106279979A
Antibacterial master batch and application thereof
CN111909454A
Conductive yarn based on graphene composite material
CN116949631A
Epoxy resin slurry based on modified graphene oxide as well as preparation method and application of epoxy resin slurry
CN117143435A
Flame-retardant modified graphene oxide and preparation method thereof
CN117887290A
Cited By
Polyester material based on modified graphene oxide and preparation method thereof
CN120040921A
Graphene-containing far-infrared warm-keeping polyurethane transfer film and preparation method thereof
CN120904801A