Preparation method of programmed delayed tackifying oil displacement system
By preparing a programmed delayed viscosity-enhancing oil displacement system, an amphiphilic polymer shell of Janus flakes is formed using water-in-oil emulsion. This solves the problems of viscosity loss and short migration distance in high water-cut oilfields, and achieves effective profile control and oil displacement.
Patent Information
- Application Number
- CN202411108570.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-13
- Publication Date
- 2024-11-22
AI Technical Summary
Existing polymer flooding technology has several drawbacks in high water-cut oilfields, including high initial viscosity leading to high injection pressure, short migration distance, poor viscosity resistance to temperature and salt, and severe shear degradation. Furthermore, conventional flooding polymers have long dissolution and maturation times, which increases investment costs.
A programmed delayed viscosity-enhancing oil displacement system is adopted. By adding specific monomers and initiators to the oil and water phases, a water-in-oil emulsion is formed. The emulsion polymerizes to form an amphiphilic polymer shell with Janus plates, releasing the inner phase polymer for profile control and oil displacement.
It achieves effective profile control and oil displacement under reservoir conditions, expands the swept volume, has a temporary plugging breakthrough function, and has a thin shell and high coverage, which prolongs the viscosity retention time.
Smart Images

Figure CN118995176A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of oil and gas field enhanced recovery and oilfield chemistry, and specifically relates to a method for preparing a programmed delayed viscosity enhancement oil displacement system, and more specifically relates to a method for preparing a programmed delayed viscosity enhancement oil displacement system for deep profile control and targeted oil displacement. Background Art
[0002] At present, my country's main energy source is still oil, but crude oil production has approached the safety red line, and improving crude oil recovery is urgent. At present, my country's main oil fields have generally entered the high water content period. Chemical flooding to improve oil recovery has been proven to be an effective and reliable technology, and polymer flooding is one of the important directions. One of the main principles of polymer flooding technology is to adjust the mobility ratio of oil to water by increasing the viscosity of the displacement fluid, thereby expanding the swept volume. The main polymers currently used are polyacrylamide and its derivatives, which are low-priced and highly designable. However, in field applications, they are often accompanied by problems such as high injection pressure and short migration distance caused by high initial viscosity, poor temperature and salt resistance of viscosity, and high viscosity loss rate caused by shear degradation during injection and migration. At the same time, conventional oil-displacing polymers have a long dissolution and maturation time, requiring corresponding ground configuration processes, which increases investment. The above problems limit the further development of polymer flooding.
[0003] Chinese patent CN202010247265.7 discloses a method for preparing a nano-network structure delayed viscosity polymer emulsion and its application. By synthesizing a polymerizable emulsifier, a core-shell structure delayed viscosity polymer with a polyurethane shell and an acrylamide polymer inner phase is prepared, which can release the inner phase polymer at a certain temperature and pH drop to play the role of delayed viscosity. However, the core polymer has no surface activity and temperature-resistant and salt-resistant groups, and the shell only provides protection and is not further utilized.
[0004] Chinese patent CN202211031821.2 discloses a targeted viscosity-enhancing polymer for oil displacement and its preparation method, which further enhances the high temperature resistance and calcium and magnesium resistance of the inner shell polymer, and the prepared polymer has good delayed viscosity-enhancing ability. However, the shell structure is also not utilized, and the surface activity of the released polymer is also weak. Summary of the invention
[0005] In order to solve the above problems, the present invention proposes a method for preparing a programmed delayed viscosity-increasing oil displacement system. The oil displacement system is a heterogeneous dispersion with a programmed oil displacement function. In the early stage, it has a function similar to that of cross-linked polymer microspheres, which can delay expansion when exposed to water and play a role in temporary plugging, breakthrough and profile adjustment. Under reservoir conditions, the shell polymer will degrade to form a Janus sheet and release the internal amphiphilic polymer oil displacement system, which will expand the displacement fluid and play an oil displacement function.
[0006] The preparation method of the programmed delayed viscosity increase oil displacement system provided by the present invention comprises the following steps: (1) The oil-soluble monomer, the degradable oil-soluble cross-linking agent, the oil-soluble oxidizing initiator and 0# white oil are uniformly mixed to prepare the oil phase, and the water-soluble monomer, the surface active functional monomer, the water-soluble cross-linking agent, the water-soluble reducing initiator and deionized water are mixed to prepare the water phase; (2) The aqueous phase, oil phase and emulsifier in step (1) are mixed, ultrasonically treated to obtain a water-in-oil emulsion, and subjected to an inverse emulsion polymerization reaction to form a polymer protective layer with heterogeneous hydrophilic and hydrophobic properties on both sides at the interface, thereby obtaining a programmed delayed viscosity enhancement flooding system.
[0007] In step (1) of the above method, the oil-soluble monomer includes, but is not limited to, one or more of styrene, divinylbenzene, and methyl acrylate; The degradable oil-soluble crosslinking agent includes but is not limited to one or more of ethylene glycol dimethacrylate, 1,4-butanediol dimethacrylate, and hexanediol dimethacrylate; The oil-soluble oxidation initiator includes, but is not limited to, one or more of cumene hydroperoxide, dibenzoyl peroxide, and dicumyl peroxide.
[0008] The water-soluble monomer includes, but is not limited to, one or more of acrylamide, 2-acrylamide-2-methylpropane sulfonic acid, sodium acrylate, partially alcoholyzed polyvinyl alcohol, and acrylic acid; preferably, the mass proportion of acrylamide in the water-soluble monomer is greater than 70%; The surface active functional monomer is one or two of vinyl pyrrolidone and vinyl polyoxyethylene ether; The water-soluble cross-linking agent is N,N-methylenebisacrylamide; The water-soluble reducing initiator includes but is not limited to one or more of ascorbic acid, sodium sulfite, and sodium bisulfite; In the oil phase, the mass ratios of the oil-soluble monomer, the degradable oil-soluble crosslinking agent, the oil-soluble oxidation initiator and the 0# white oil may be (20-40): (15-25): (0.015-0.15): (35-65) in sequence; In the aqueous phase, the mass ratios of the water-soluble monomer, the surface active functional monomer, the water-soluble cross-linking agent, the water-soluble reducing initiator and the deionized water may be (56-70): (5-20): (2-5): (0.015-0.15): 160, respectively; In step (2) of the above method, the emulsifier is a mixture of Tween 80 and Span 60, and the HLB value is 6-7.
[0009] The mass ratio of oil phase, emulsifier and water phase is (30-45): (6-12): (45-65), specifically 4:1:8, 4:1.2:8 or 6:1.2:6; The ultrasonic treatment may be performed at 400 W, 40 KHz, and 4-10° C. for 10-30 min; The conditions of the inverse emulsion polymerization reaction are: heating to 30-60° C. and reacting for 2-5 hours under nitrogen protection.
[0010] The particle size of the obtained programmed delayed viscosity enhancement flooding system is 80 nm-5 µm.
[0011] The programmed delayed viscosity enhancement oil displacement system prepared by the above method also belongs to the protection scope of the present invention.
[0012] The application of the above-mentioned programmed delayed viscosity increase flooding system in the development and recovery of oil and gas fields also falls within the protection scope of the present invention.
[0013] In the application, the programmed delayed viscosity increase oil recovery system has a function similar to that of cross-linked polymer microspheres in the early stage, which can delay expansion when in contact with water, and play the role of temporary plugging, breakthrough and profile adjustment; under reservoir conditions, the shell polymer will degrade to form Janus sheets, and release the internal amphiphilic polymer oil recovery system, thereby expanding the displacement fluid and playing the oil recovery function.
[0014] Compared with the prior art, the present invention has the following beneficial effects: 1. The particle size of the prepared oil displacement system is 80 nm-5 µm, which meets the requirements of most stratum migration. The introduction of hydrophobic monomers in the shell layer can delay expansion and is conducive to deep profile control. Compared with other delayed viscosity enhancement systems, it also has similar microsphere temporary plugging-breakthrough-profile control functions before releasing the internal phase viscosity enhancement system.
[0015] 2. The use of oil-soluble oxidation initiators and water-soluble reduction initiators is conducive to the in-situ formation of a polymer shell at the interface. The inside and outside of the shell have different hydrophilic and hydrophobic properties. After fragmentation, an amphiphilic oil displacement system similar to Janus particles is formed, further utilizing the shell material.
[0016] 3. Compared with other cases where the initiator is added to the oil phase or water phase alone, the shell thickness is thinner, which ensures a high coverage rate of the internal phase polymer solution and is conducive to better exerting the delayed viscosity increasing properties. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic diagram of the process of the present invention.
[0018] Figure 2 This is the particle size distribution diagram of the product obtained in Example 1 of the present invention.
[0019] Figure 3 This is the particle size distribution diagram of the product obtained in Example 2 of the present invention.
[0020] Figure 4 This is the particle size distribution diagram of the product obtained in Example 3 of the present invention. DETAILED DESCRIPTION
[0021] The present invention is further described in detail below in conjunction with specific embodiments, and the examples provided are only for illustrating the present invention, rather than for limiting the scope of the present invention. The examples provided below can be used as a guide for further improvements by those of ordinary skill in the art, and do not constitute a limitation of the present invention in any way.
[0022] The experimental methods in the following examples, unless otherwise specified, are all conventional methods, and are performed according to the techniques or conditions described in the literature in the field or according to the product instructions. The materials, reagents, etc. used in the following examples, unless otherwise specified, can all be obtained from commercial channels.
[0023] Example 1 80 g of acrylamide, sodium acrylate, vinyl pyrrolidone, N,N-methylenebisacrylamide and ascorbic acid mixture (mass ratio 70:12:15:2.98:0.02) were dissolved in 160 g of deionized water to obtain an aqueous phase. 20 g of styrene, 15 g of ethylene glycol dimethacrylate, and 0.015 g of cumene hydroperoxide were dissolved in 65 g of 0# white oil to obtain an oil phase.
[0024] 80 g of water phase, 40 g of oil phase and 10 g of emulsifier (Span 60: Tween 80 = 8:2 (HLB value is 6.4)) were mixed and ultrasonically emulsified at 400 W, 40 KHz and 10°C for 20 min to obtain an oil-in-water emulsion. Nitrogen was passed through an ice bath for 10 min to deoxygenate, and then the temperature was raised to 45°C for 5 h to obtain the target system. In this embodiment, the average particle size of the system was 1 µm.
[0025] Example 2 80 g of acrylamide, vinyl acetate, vinyl pyrrolidone, N,N-methylenebisacrylamide and ascorbic acid mixture (mass ratio 70:12:15:2.98:0.02) were dissolved in 160 g of deionized water to obtain an aqueous phase. 25 g of styrene, 15 g of ethylene glycol dimethacrylate, and 0.015 g of cumene hydroperoxide were dissolved in 60 g of 0# white oil to obtain an oil phase.
[0026] 80 g of water phase, 40 g of oil phase and 12 g of emulsifier (Span 60: Tween 80 = 8:2 (HLB value is 6.4)) were mixed and ultrasonically emulsified at 400 W, 40 KHz and 10°C for 20 min to obtain an oil-in-water emulsion. Nitrogen was passed through an ice bath for 10 min to deoxygenate, and then the temperature was raised to 50°C for 5 h to obtain the target system. In this embodiment, the average particle size of the system was 0.3 µm. Example 3 80 g of acrylamide, vinyl acetate, vinyl pyrrolidone, N,N-methylenebisacrylamide and ascorbic acid mixture (mass ratio 70:12:15:2.98:0.02) were dissolved in 160 g of deionized water to obtain an aqueous phase. 20 g of styrene, 20 g of ethylene glycol dimethacrylate, and 0.015 g of cumene hydroperoxide were dissolved in 60 g of 0# white oil to obtain an oil phase.
[0027] 60 g of water phase, 60 g of oil phase and 12 g of emulsifier (Span 60: Tween 80 = 8:2 (HLB value is 6.4)) were mixed and ultrasonically emulsified at 400 W, 40 KHz and 10°C for 20 min to obtain an oil-in-water emulsion. Nitrogen was passed through an ice bath for 10 min to deoxygenate, and then the temperature was raised to 50°C for 5 h to obtain the target system. In this embodiment, the average particle size of the system was 0.8 µm. Example 4 In order to illustrate the beneficial effects of the present invention, the expansion of the oil displacement system prepared in Examples 1 to 3 is compared with that of the commercial cross-linked polyacrylamide microspheres (the commercial cross-linked polyacrylamide microspheres described in Test Example 1 of Chinese Patent 201910622576.4 (the microspheres are cross-linked polyacrylamide microspheres prepared by inverse emulsion polymerization using N,N'-methylenebisacrylamide as a cross-linking agent and acrylamide as a functional monomer, and the average particle size of the microspheres is 294 nm)). The specific implementation steps are as follows: 500 mg / L suspension of the embodiment and commercial microspheres was prepared, and the change in microsphere size and the expansion time at different times were monitored by a laser particle size analyzer at 25°C. The performance of the embodiment and commercial microspheres was evaluated by the expansion multiple (ratio of particle size before and after expansion) and the time when the particle size did not change, as shown in Table 1. The results in Table 1 show that the prepared oil displacement system has better slow swelling performance than commercial microspheres.
[0028] Table 1 Evaluation of the slow expansion performance of the example system
[0029] Example 5 In order to illustrate the beneficial effects of the present invention, the oil displacement system and delayed viscosity enhancement performance prepared in Examples 1 to 3 were evaluated, and the specific implementation steps were as follows: A 2500 mg / L suspension of the system was prepared. After the initial viscosity was tested, the suspension was aged at 120°C under deoxygenation conditions. The viscosity changes of the systems of each embodiment were measured at different days. The test conditions were ULA rotor, 75°C, and a shear rate of 7.34 s -1 The results are shown in Table 2. It can be seen that each embodiment has a good delayed viscosity increase effect, which is beneficial to deep profile control. After 20 days of testing, the interfacial tension between the solution and the white oil was 10 0 The magnitude of mN / m indicates that the released amphiphilic polymer has a certain oil displacement function.
[0030] Table 2 Viscosity of the system at different times
[0031] The present invention has been described in detail above. For those skilled in the art, without departing from the purpose and scope of the present invention, and without the need to carry out unnecessary experimental conditions, the present invention can be implemented in a wide range under equivalent parameters, concentrations and conditions. Although the present invention provides specific embodiments, it should be understood that the present invention can be further improved. In a word, according to the principles of the present invention, the application is intended to include any changes, uses or improvements to the present invention, including departure from the disclosed scope in the application, and changes made with conventional techniques known in the art.
Claims
1. A method for preparing a programmed delayed viscosity increase flooding system, comprising the following steps: (1) The oil-soluble monomer, the degradable oil-soluble cross-linking agent, the oil-soluble oxidizing initiator and 0# white oil are uniformly mixed to prepare the oil phase, and the water-soluble monomer, the surface active functional monomer, the water-soluble cross-linking agent, the water-soluble reducing initiator and deionized water are mixed to prepare the water phase; (2) The aqueous phase, oil phase and emulsifier in step (1) are mixed, ultrasonically treated to obtain a water-in-oil emulsion, and subjected to an inverse emulsion polymerization reaction to form a polymer protective layer with heterogeneous hydrophilic and hydrophobic properties on both sides at the interface, thereby obtaining a programmed delayed viscosity enhancement flooding system.
2. The method according to claim 1, characterized in that In step (1) of the method, the oil-soluble monomer is selected from: one or more of styrene, divinylbenzene, and methyl acrylate; The degradable oil-soluble crosslinking agent is selected from: one or more of ethylene glycol dimethacrylate, 1,4-butanediol dimethacrylate, and hexanediol dimethacrylate; The oil-soluble oxidation initiator is selected from one or more of cumene hydroperoxide, dibenzoyl peroxide, and dicumyl peroxide; In the oil phase, the mass ratios of the oil-soluble monomer, the degradable oil-soluble cross-linking agent, the oil-soluble oxidation initiator and the 0# white oil can be (20-40): (15-25): (0.015-0.15): (35-65) respectively.
3. The method according to claim 1 or 2, characterized in that: The water-soluble monomer is selected from one or more of acrylamide, 2-acrylamide-2-methylpropane sulfonic acid, sodium acrylate, partially alcoholyzed polyvinyl alcohol, and acrylic acid; The surface active functional monomer is selected from one or two of vinyl pyrrolidone and vinyl polyoxyethylene ether; The water-soluble cross-linking agent is N,N-methylenebisacrylamide; The water-soluble reducing initiator is selected from one or more of ascorbic acid, sodium sulfite, and sodium bisulfite; In the aqueous phase, the mass ratios of the water-soluble monomer, the surfactant functional monomer, the water-soluble cross-linking agent, the water-soluble reducing initiator and the deionized water may be (56-70): (5-20): (2-5): (0.015-0.15): 160, respectively.
4. The method according to claim 1 or 2, characterized in that: In step (2), the emulsifier is a mixture of Tween 80 and Span 60, and the HLB value is 6-7.
5. The method according to claim 1 or 2, characterized in that: The mass ratios of oil phase, emulsifier and water phase are (30~45):(6~12):(45~65) respectively.
6. The method according to claim 1 or 2, characterized in that: The ultrasonic treatment is carried out under the conditions of 400 W, 40 KHz, 4-10° C. for 10-30 min.
7. The method according to claim 1 or 2, characterized in that: The conditions of the inverse emulsion polymerization reaction are: heating to 30-60° C. and reacting for 2-5 hours under nitrogen protection.
8. A programmed delayed viscosity increasing oil displacement system prepared by the method according to any one of claims 1 to 7.
9. The programmed delayed viscosity increase flooding system according to claim 8, characterized in that: The particle size of the programmed delayed viscosity enhancement flooding system is 80 nm-5 µm.
10. Application of the programmed delayed viscosity increase flooding system according to claim 8 or 9 in oil and gas field development and recovery; In the application, the programmed delayed viscosity increase oil recovery system has a function similar to that of cross-linked polymer microspheres in the early stage, which can delay expansion when in contact with water, and play the role of temporary plugging, breakthrough and profile adjustment; under reservoir conditions, the shell polymer will degrade to form Janus sheets, and release the internal amphiphilic polymer oil recovery system, thereby expanding the displacement fluid and playing the oil recovery function.