Preparation method and preparation equipment of modified polyphenylene sulfide fiber

The airflow and water mist sprayed through the nozzle to cool down, and the fiber wires were absorbed by the limit frame and sponge block, which solved the problem of fiber wire breakage during the preparation of polyphenylene sulfide fibers, and improved the integrity and winding efficiency of fiber wires. Ensures rapid positioning and finishing of fiber wires.

CN118996643AInactive Publication Date: 2024-11-22SINOMA (SUZHOU) NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411340799.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-25
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the preparation of existing polyphenylene sulfide fibers, fiber wire breaks often occur when cooling by immersing in water, causing the fiber wire to swing under the impact of the water flow, affecting the normal winding of the surrounding fiber wires.

Method used

The airflow and water mist are sprayed out of the nozzle to cool down, and the fiber wire is adsorbed by the limit frame and discharge port to prevent breakage. The water mist is adsorbed through the sponge block for preliminary cooling and dust cleaning to ensure the integrity and cleanliness of the fiber wire. .

Benefits of technology

It effectively avoids breakage of fiber wires during the winding process, improves the integrity and winding efficiency of fiber wires, ensures rapid positioning and finishing of fiber wires, and reduces the impact of dust.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118996643A_ABST
    Figure CN118996643A_ABST
Patent Text Reader

Abstract

The invention relates to the field of polyphenylene sulfide fiber production, in particular to modified polyphenylene sulfide fiber preparation equipment which comprises a mounting frame, a motor, conveying rollers and the like. A plurality of motors are fixedly connected to the mounting frame; a plurality of conveying rollers are rotationally connected to the mounting frame; and an output shaft of each motor is fixedly connected with the corresponding conveying roller. Cooling work is carried out in the mode that the nozzles spray airflow and water mist, the cellosilk keeps moving under the action of external winding equipment, namely, the cooling speed of the cellosilk is low, multiple nozzles are often needed to spray airflow and water mist to gradually lower the temperature of the cellosilk, but in the process, cracks can be avoided, and the service life of the cellosilk is prolonged. And therefore, the fracture risk of the fibers in the winding process is reduced, and the integrity of the fibers is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of polyphenylene sulfide fiber production, and in particular to a preparation method and preparation equipment of modified polyphenylene sulfide fiber. Background Art

[0002] Polyphenylene sulfide fiber is a special fiber with excellent chemical corrosion resistance, high temperature resistance, good flame retardancy, insulation, etc. It is often prepared into fiber filaments, but the existing fiber filaments are divided into two types, one is micron-level fiber: generally used for high-performance composite materials, with a diameter of 5-50 microns, and the other is millimeter-level fiber: used for reinforcing materials or for industrial purposes, with a diameter of 0.5-5 mm. Different diameters and thicknesses can meet different application requirements, such as reinforcing materials, filter materials, high temperature resistant materials, etc. The main characteristics of polyphenylene sulfide fiber are excellent chemical corrosion resistance, high temperature resistance, etc. Temperature resistance, good flame retardancy, insulation, that is, it is often prepared into millimeter-level fibers to enhance the material's chemical corrosion resistance, high temperature resistance, good flame retardancy, insulation, etc. The fiber filaments are mainly made by drawing, but the preparation process is accompanied by high temperature, that is, cooling treatment is required during the winding process. The existing technology often cools down by immersing in water, but in the winding process, breakage problems often occur. The broken fiber filaments will be impacted by the water flow, and the fiber filaments will swing in the water under the impact of the water flow, thereby affecting the normal winding of the remaining fiber filaments around them. Summary of the invention

[0003] In order to overcome the disadvantage that the prior art often cools down by immersing in water, but the fiber filaments often break during the winding process, and the broken fiber filaments are impacted by the water flow. Under the impact of the water flow, the fiber filaments will swing in the water, thereby affecting the normal winding of the remaining fiber filaments around them, the present invention provides a preparation device for modified polyphenylene sulfide fiber.

[0004] The technical implementation scheme of the present invention is: a method for preparing modified polyphenylene sulfide fiber, comprising the following steps: Step 1: Place the modified polyphenylene sulfide resin into an extruder and heat it to a molten state; Step 2: Select a suitable spinning head and ensure that its aperture can meet the required fiber diameter; Step 3: Extruding the molten polyphenylene sulfide through a spinning head to form preliminary fiber filaments; Step 4: Rapidly cool the extruded fiber filaments, usually using air or water cooling to cool the fiber filaments, and observe whether the fiber filaments break during the cooling process. If the fiber filaments break, stop the machine to adjust the equipment and run it again; Step 5: Rolling up the polyphenylene sulfide fiber filaments.

[0005] The preparation method uses a preparation device for modified polyphenylene sulfide fiber, including a mounting frame, a motor and a conveying roller; a plurality of motors are fixedly connected to the mounting frame; a plurality of conveying rollers are rotatably connected to the mounting frame; the output shaft of each motor is fixedly connected to the corresponding conveying roller; the device also includes a first mounting frame, a second mounting frame, a connecting frame, a limiting frame, an air pipe, an exhaust pipe and a limiting rod; the first mounting frame is fixedly connected to the mounting frame; the second mounting frame is fixedly connected to the mounting frame; the connecting frame is fixedly connected inside the mounting frame; the connecting frame is fixedly connected to the There are several limit frames in the sliding connection, each of which is connected to several sliding blocks, each of which is provided with a through hole for conveying fiber filaments, each of which is provided with several nozzles, and each of which is provided with several exhaust ports on the through hole; each of which is connected to an air supply pipe, which is connected to the first installation frame; each of which is connected to an exhaust pipe, which is connected to the second installation frame; each of which is connected to each sliding block of each limit frame is connected with several limit rods; and all of the limit rods are fixedly connected to the connecting frame.

[0006] More preferably, a sealing block made of rubber material is provided at the connection position between the first installation frame and the air supply pipe, and a sealing block made of rubber material is provided at the connection position between the second installation frame and the exhaust pipe.

[0007] More preferably, the surface of the conveying roller is provided with a solid lubricant coating mainly composed of polytetrafluoroethylene.

[0008] More preferably, the through holes formed on the limiting frame are two circular through holes, one larger than the other and the other smaller than the other, in the shape of a gourd.

[0009] More preferably, a sensor is provided on the through hole opened on the limiting frame.

[0010] More preferably, the end of the limiting rod is made of rubber material.

[0011] More preferably, an isolation component is also included, which includes a first connecting plate, a first sponge block, a second sponge block and a second connecting plate; a plurality of first connecting plates are connected to the top cover; each first connecting plate is connected to a first sponge block; all the first sponge blocks are connected to a connecting frame; a plurality of second connecting plates are connected to the bottom plate; each second connecting plate is connected to a second sponge block; all the second sponge blocks are connected to the connecting frame; and each second sponge block is in contact with the corresponding second connecting plate.

[0012] More preferably, the first connecting plate and the first sponge block are arranged in a quick-release structure, and the second sponge block and the second connecting plate are also arranged in a quick-release structure.

[0013] More preferably, the first sponge block and the second sponge block are both provided with a concave structure that is larger on the outside and smaller on the inside, and the combination forms a concave truncated cone shape.

[0014] The beneficial effects of the present invention are as follows: 1. The present invention performs cooling work by spraying airflow and water mist through the nozzle, and the fiber filaments keep moving under the action of the external winding device, that is, the cooling speed of the fiber filaments is slow, and it is often necessary to spray airflow and water mist from multiple nozzles to gradually reduce the temperature of the fiber filaments, but in this process, the generation of cracks can be avoided, thereby reducing the risk of fiber filaments breaking during the winding process, thereby ensuring the integrity of the fiber filaments, the discharge port adsorbs the lower surface of the fiber filaments, fixes the fiber filaments on the limit frame, and avoids the external winding device driving the fiber filaments to continue to move, resulting in the continuous swing of the broken end of the fiber filaments that loses the restriction, affecting the normal winding work of the surrounding fiber filaments, in this device, the broken head of the fiber filament is adsorbed by the discharge port, that is, in the subsequent process of arranging the fiber filaments, the staff can quickly find the broken head of the fiber filament, thereby improving the winding efficiency; 2. In the present invention, water mist will move toward the openings on both sides of the mounting frame. The water mist will contact the first sponge block and the second sponge block when it moves toward both sides. The water mist will be absorbed by the first sponge block and the second sponge block, so that the first sponge block and the second sponge block, that is, the first sponge block and the second sponge block close to the extruder, will initially cool down the fiber filaments just extruded, so that the fiber filaments will be cooled quickly, and at the same time, the dust attached to the fiber filaments will be cleaned, and the dust attached to the fiber filaments will be cleaned again by approaching the winding machine, so that the fiber filaments remain in a clean state and the dust will not affect the winding of the fiber filaments. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a structural schematic diagram of the preparation equipment of the modified polyphenylene sulfide fiber of the present invention; Figure 2 It is a schematic diagram of the combined structure of the motor, conveying roller and connecting frame of the preparation equipment of the modified polyphenylene sulfide fiber of the present invention; Figure 3 It is a schematic diagram of the combined structure of the connecting frame, the limiting frame and the air transmission pipe of the preparation equipment of the modified polyphenylene sulfide fiber of the present invention; Figure 4 for Figure 3 A magnified image of area A; Figure 5 It is a schematic structural diagram of a limit frame of a preparation device for modified polyphenylene sulfide fiber of the present invention; Figure 6 This is a schematic diagram of the combined structure of the first connecting plate and the first sponge block of the isolation assembly of the preparation equipment of the modified polyphenylene sulfide fiber of the present invention; Figure 7 This is a schematic diagram of the combined structure of the second sponge block and the second connecting plate of the equipment for preparing modified polyphenylene sulfide fiber of the present invention; Figure 8 It is a schematic diagram of the combined structure of the first sponge block and the second sponge block of the equipment for preparing modified polyphenylene sulfide fiber of the present invention.

[0016] The markings of the components in the accompanying drawings are as follows: 001-fiber filament, 1-mounting frame, 2-first mounting frame, 3-second mounting frame, 4-motor, 5-conveying roller, 6-connecting frame, 7-limiting frame, 7001-nozzle, 7002-discharge port, 8-air supply pipe, 9-exhaust pipe, 10-limiting rod, 101-first connecting plate, 102-first sponge block, 103-second sponge block, 104-second connecting plate. DETAILED DESCRIPTION

[0017] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0018] Example 1 A method for preparing modified polyphenylene sulfide fiber comprises the following steps: Step 1: Place the modified polyphenylene sulfide resin into an extruder and heat it to a molten state; Step 2: Select a suitable spinning head and ensure that its aperture can meet the required fiber diameter; Step 3: Extruding the molten polyphenylene sulfide through a spinning head to form preliminary fiber filaments 001; Step 4: Rapidly cool the extruded fiber filament 001, usually using air or water cooling to cool the fiber filament 001, and observe whether the fiber filament 001 breaks during the cooling process. After the fiber filament 001 breaks, stop the machine to adjust the equipment and run it again; Step 5: Roll up the polyphenylene sulfide fiber 001.

[0019] The preparation method includes a preparation device for a modified polyphenylene sulfide fiber, such as Figure 1-Figure 5 As shown, it includes a mounting frame 1, a motor 4 and a conveying roller 5; the mounting frame 1 is bolted with two symmetrically arranged motors 4; the mounting frame 1 is rotatably connected with two symmetrically arranged conveying rollers 5; the output shaft of each motor 4 is fixedly connected to the corresponding conveying roller 5; It also includes a first mounting frame 2, a second mounting frame 3, a connecting frame 6, a limiting frame 7, an air pipe 8, an exhaust pipe 9 and a limiting rod 10; the first mounting frame 2 is fixedly connected to the mounting frame 1; the second mounting frame 3 is fixedly connected to the mounting frame 1; the connecting frame 6 is fixedly connected inside the mounting frame 1; sixty-six limiting frames 7 in a rectangular array are slidably connected to the connecting frame 6, each limiting frame 7 is connected to four sliding blocks distributed in a rectangular shape, each limiting frame 7 is provided with a through hole, each limiting frame 7 has three annular equidistantly distributed nozzles 7001 on the through hole, and each limiting frame 7 has three annular equidistantly distributed exhaust ports 7002 on the through hole; each limiting frame 7 is connected to an air pipe 8, and the air pipe 8 is connected to the first mounting frame 2; each limiting frame 7 is connected to an exhaust pipe 9, and the exhaust pipe 9 is connected to the second mounting frame 3; two limiting rods 10 are inserted into each sliding block of each limiting frame 7; all limiting rods 10 are fixedly connected to the connecting frame 6.

[0020] A sealing block made of rubber material is provided at the connection position between the first installation frame 2 and the air supply pipe 8, and a sealing block made of rubber material is provided at the connection position between the second installation frame 3 and the exhaust pipe 9, so as to enhance the sealing effect and prevent water mist leakage.

[0021] The surface of the conveying roller 5 is provided with a solid lubricant coating mainly composed of polytetrafluoroethylene to reduce friction.

[0022] The through holes formed on the limiting frame 7 are two circular through holes, one larger than the other and the other smaller than the other, in the shape of a gourd. The smaller through hole at the bottom is used to cooperate with the discharge port 7002 to absorb the fiber filament 001 .

[0023] A sensor is provided on the through hole formed on the limit frame 7 to determine whether the fiber filament 001 is broken by means of pressure detection.

[0024] The end of the limiting rod 10 is made of rubber material, which ensures that the limiting frame 7 is limited and has the property of rapid release.

[0025] First, the staff installed the preparation equipment of modified polyphenylene sulfide fiber on the wire drawing machine, and then used the external gas injection equipment to connect with the gas pipeline 8, and used the external suction equipment to connect with the exhaust pipe 9. The first installation frame 2 and the second installation frame 3 then used tools to place the fiber filament 001 extruded by the extruder on the conveying roller 5, and then passed through the corresponding limit frame 7, and placed on the conveying roller 5 at the other end, and then fixed it on the external winding roller for winding, and then controlled the motor 4 to drive the conveying roller 5 to rotate and convey the fiber filament 001, and the external The winding roller also starts to work synchronously to realize the winding of the fiber filament 001, and at the same time controls the operation of the external gas injection equipment to inject the atomized water mist into the gas pipe 8, and then sprays out the airflow and water mist at a uniform speed through the nozzle 7001. The sprayed airflow and water mist are used to reduce the temperature of the fiber filament 001. During this process, the first installation frame 2 cooperates with the limit frame 7, the exhaust pipe 9 and the exhaust port 7002 to perform suction work, that is, the airflow sprayed from the nozzle 7001 and the water mist of the first installation frame 2 will be sucked into the exhaust port 7002, and then through the limit frame 7 and the exhaust pipe 9 The air pipe 9 is transferred to the waste barrel built into the exhaust device, and at the same time, the dust in the wire drawing process is cleaned, and the harmful gases generated in the production process are absorbed and cleaned synchronously to ensure the working environment. It should be noted that the cooling work is carried out by directly immersing in water. The fiber filament 001 is quickly converted from a high-temperature environment to a low-temperature environment. Although it can shorten the production cycle and improve the production efficiency of the fiber filament 001, this method will cause cracks in the fiber filament 001 during the cooling process. After the cracks appear, the fiber filament 001 is more likely to break due to the tension of winding. However, the cooling work is carried out by spraying airflow and water mist through the nozzle 7001, and the fiber filament 001 keeps moving under the action of the external winding device, that is, the cooling speed of the fiber filament 001 is slow, and it is often necessary to spray airflow and water mist from multiple nozzles 7001 to gradually reduce the temperature of the fiber filament 001. However, in this process, the generation of cracks can be avoided, thereby reducing the risk of breakage of the fiber filament 001 during the winding process, thereby ensuring the integrity of the fiber filament 001. Furthermore, during the transportation of the fiber filament 001, it is easy to break. When the fiber filament 001 breaks, it is necessary to stop the machine in time for corresponding repair treatment. If the fiber filament 001 is not stopped in time, the wire drawing machine will continue to transport the fiber filament 001, but the position where the fiber filament 001 is broken will lose the traction of the winding wheel, that is, the fiber filament 001 will not only not be transported, but will also pile up and entangle on the remaining fiber filaments 001 on both sides, affecting the transportation of the remaining fiber filaments 001, and the fiber filament 001 at one end of the winding roller will swing under the drive of the winding roller. This causes the fiber filament 001 to contact with the other fiber filaments 001 on both sides, thereby affecting the reeling of the other fiber filaments 001 on both sides. When the fiber filament 001 breaks, the airflow ejected from the nozzle 7001 will drive the fiber filament 001 to move downward close to the inner ring surface of the limit frame 7, and at the same time cooperate with the discharge port 7002 to adsorb the lower surface of the fiber filament 001, so that the fiber filament 001 is fixed on the limit frame 7, to prevent the external reeling device from driving the fiber filament 001 to continue to move, causing the broken end of the fiber filament 001 to lose its restriction and continue to swing, affecting the normal reeling of the surrounding fiber filaments 001. The other end of the broken fiber 001 is adsorbed by the discharge port 7002, that is, the fiber 001 is squeezed by the suction of the discharge port 7002, and the sensor set on the through hole of the limit frame 7 is triggered by the sensor to remind the staff to check the problem of the broken fiber 001. In this process, if the extruder does not stop working in time, the fiber 001 is still transported. Although the fiber 001 will pile up together, the fiber 001 will not be driven to swing by the airflow and water mist sprayed from the nozzle 7001. However, in the prior art, in order to maintain the cooling efficiency during the water cooling process, it is usually necessary to continue The water flow is conveyed to avoid the water temperature from rising, but the broken fiber filaments 001 will be driven by the water flow, causing the fiber filaments 001 to constantly swing in the water, which will not only affect the rest of the surrounding fiber filaments 001, but also in the process of stopping the machine to sort the fiber filaments 001, when too many fiber filaments 001 are accumulated, it is difficult to find the broken head of the fiber filament 001 in the water, thereby affecting the work efficiency. However, in this equipment, the broken head of the fiber filament 001 is adsorbed by the discharge port 7002, that is, in the subsequent process of sorting the fiber filaments 001, the staff can quickly find the broken head of the fiber filament 001, thereby improving the winding efficiency.

[0026] Example 2 On the basis of the above-mentioned embodiment 1, Figure 6-Figure 8As shown, an isolation component is also included, which includes a first connecting plate 101, a first sponge block 102, a second sponge block 103 and a second connecting plate 104; twelve symmetrically arranged first connecting plates 101 are connected to the top cover; each first connecting plate 101 is connected to a first sponge block 102; all the first sponge blocks 102 are connected to the connecting frame 6; twelve symmetrically arranged second connecting plates 104 are connected to the bottom plate; each second connecting plate 104 is connected to a second sponge block 103; all the second sponge blocks 103 are connected to the connecting frame 6; each second sponge block 103 is in contact with the corresponding second connecting plate 104.

[0027] The first connecting plate 101 and the first sponge block 102 are arranged in a quick-release structure, and the second sponge block 103 and the second connecting plate 104 are also arranged in a quick-release structure, so as to facilitate replacement of the first sponge block 102 and the second sponge block 103 .

[0028] The first sponge block 102 and the second sponge block 103 are both provided with a concave structure that is larger on the outside and smaller on the inside, and the combination forms a concave truncated cone shape, which is used to scrape away impurities on the fiber filaments 001.

[0029] In the process of spraying air flow and water mist through the nozzle 7001, since in the space composed of the mounting frame 1, the first mounting frame 2, the second mounting frame 3, the top cover and the bottom plate, only the two sides of the mounting frame 1 are used to convey the fiber filaments 001 and are connected to the outside world, in this process, the water mist will move toward the openings on both sides of the mounting frame 1, and the water mist will contact the first sponge block 102 and the second sponge block 103 when it moves to both sides. The water mist will be adsorbed by the first sponge block 102 and the second sponge block 103, so that the first sponge block 102 and the second sponge block 103, that is, the first sponge block 102 and the second sponge block 103 close to the extruder, perform preliminary cooling of the fiber filaments 001 just extruded, so that the fiber filaments 001 are cooled quickly, and at the same time, the dust attached to the fiber filaments 001 is cleaned, and the dust attached to the fiber filaments 001 is cleaned again by approaching the winding, so that the fiber filaments 001 are kept in a clean state to prevent dust from affecting the winding of the fiber filaments 001.

[0030] Although the present disclosure has been shown and described with reference to specific exemplary embodiments of the present disclosure, it should be understood by those skilled in the art that various changes in form and details may be made to the present disclosure without departing from the spirit and scope of the present disclosure as defined by the appended claims and their equivalents. Therefore, the scope of the present disclosure should not be limited to the above-mentioned embodiments, but should be determined not only by the appended claims, but also by the equivalents of the appended claims.

Claims

1. A method for preparing modified polyphenylene sulfide fiber, characterized in that: The following steps are involved: Step 1: Place the modified polyphenylene sulfide resin into an extruder and heat it to a molten state; Step 2: Select a suitable spinning head and ensure that its aperture can meet the required fiber diameter; Step 3: Extruding the molten polyphenylene sulfide through a spinning head to form preliminary fiber filaments (001); Step 4: Rapidly cool the extruded fiber filament (001), usually using air or water cooling to cool the fiber filament (001), and observe whether the fiber filament (001) breaks during the cooling process. After the fiber filament (001) breaks, stop the machine to adjust the equipment, and then run it again; Step 5: Rolling up the polyphenylene sulfide fiber (001).

2. A method for preparing a modified polyphenylene sulfide fiber according to claim 1, wherein the preparation method comprises a device for preparing a modified polyphenylene sulfide fiber, characterized in that: The invention comprises a mounting frame (1), a motor (4) and a conveying roller (5); the mounting frame (1) is fixedly connected to a plurality of motors (4); the mounting frame (1) is rotatably connected to a plurality of conveying rollers (5); the output shaft of each motor (4) is fixedly connected to the corresponding conveying roller (5); and the invention also comprises a first mounting frame (2), a second mounting frame (3), a connecting frame (6), a limiting frame (7), an air supply pipe (8), an exhaust pipe (9) and a limiting rod (10); the mounting frame (1) is fixedly connected to the first mounting frame (2); the mounting frame (1) is fixedly connected to the second mounting frame (3); the mounting frame (1) is fixedly connected to the connecting frame (6); the connecting frame (6) is slidably connected to a plurality of limiting frames ( 7), each limit frame (7) is connected to a plurality of sliders, each limit frame (7) is provided with a through hole for conveying fiber filaments (001), each limit frame (7) is provided with a plurality of nozzles (7001) on the through hole, and each limit frame (7) is provided with a plurality of exhaust ports (7002) on the through hole; each limit frame (7) is connected to an air supply pipe (8), and the air supply pipe (8) is connected to the first installation frame (2); each limit frame (7) is connected to an exhaust pipe (9), and the exhaust pipe (9) is connected to the second installation frame (3); each slider of each limit frame (7) is plugged with a plurality of limit rods (10); and all the limit rods (10) are fixedly connected to the connecting frame (6).

3. The preparation device of modified polyphenylene sulfide fiber according to claim 2, characterized in that: A sealing block made of rubber material is provided at a connection position between the first installation frame (2) and the gas delivery pipe (8), and a sealing block made of rubber material is provided at a connection position between the second installation frame (3) and the exhaust pipe (9).

4. The preparation device for modified polyphenylene sulfide fiber according to claim 2, characterized in that: The surface of the conveying roller (5) is provided with a solid lubricant coating mainly composed of polytetrafluoroethylene.

5. The preparation device of modified polyphenylene sulfide fiber according to claim 2, characterized in that: The through holes formed on the limiting frame (7) are two circular through holes, one larger than the other, and the other smaller than the other, in the shape of a gourd.

6. The preparation device of modified polyphenylene sulfide fiber according to claim 2, characterized in that: A sensor is provided on the through hole opened on the limit frame (7).

7. A preparation device for modified polyphenylene sulfide fiber according to any one of claims 2 to 5, characterized in that: The end of the limiting rod (10) is made of rubber material.

8. The preparation device for modified polyphenylene sulfide fiber according to claim 7, characterized in that: The device also includes an isolation component, which includes a first connection plate (101), a first sponge block (102), a second sponge block (103) and a second connection plate (104); a plurality of first connection plates (101) are connected to the top cover; each first connection plate (101) is connected to a first sponge block (102); all the first sponge blocks (102) are connected to a connection frame (6); a plurality of second connection plates (104) are connected to the bottom plate; each second connection plate (104) is connected to a second sponge block (103); all the second sponge blocks (103) are connected to the connection frame (6); and each second sponge block (103) is in contact with a corresponding second connection plate (104).

9. The preparation device for modified polyphenylene sulfide fiber according to claim 8, characterized in that: The first connecting plate (101) and the first sponge block (102) are arranged in a quick-release structure, and the second sponge block (103) and the second connecting plate (104) are also arranged in a quick-release structure.

10. The preparation device of modified polyphenylene sulfide fiber according to claim 8, characterized in that: The first sponge block (102) and the second sponge block (103) are both provided with an inner concave structure that is larger on the outside and smaller on the inside, and the combination forms an inner concave truncated cone shape.