Detachable soft rainwater collecting cistern based on water conservancy project and production process thereof
Through the removable rainwater collecting cellar with corrosion-resistant fabrics and epoxy resin coating, the problems of high costs and easy corrosion in water conservancy projects are solved, and the rainwater collecting cellar with lightweight and fast installation and long life is achieved, which is suitable for acid and alkaline environments.
Patent Information
- Application Number
- CN202411079170.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In existing water conservancy projects, the construction of water storage facilities such as water cellars and pools is expensive and covers a large area, making it difficult to achieve detachable and corrosion-resistant rainwater storage cellars, especially in acid-base and salt environments, which affect their service life.
The detachable soft-collecting rainwater cellar made of corrosion-resistant fabrics is connected to the mounting bracket by fastening ropes, combining Velcro wool surfaces and threaded sleeves to achieve rapid assembly, and the fabric is protected by a specially made corrosion-resistant epoxy resin coating. Ensure corrosion resistance in acid and alkali environments.
It realizes a lightweight and fast installation of detachable rainwater collecting cellar, extends its service life, reduces costs, and maintains corrosion resistance in acid-base environments, avoiding the corrosion problems of traditional facilities.
Smart Images

Figure CN118997269A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of rainwater collection pits, and in particular to a detachable soft rainwater collection pit based on a water conservancy project and a production process thereof. Background Art
[0002] Agricultural water resources are unevenly distributed in different regions, years and seasons. Water supply and demand are often inconsistent in time and space. Droughts and floods or alternating droughts and floods greatly affect the high and stable yields of agriculture. Therefore, rainwater accumulation and collection are the main technologies for rainwater harvesting and irrigation in the Loess Plateau. By building water storage facilities such as water cellars, pools and flood ponds, the runoff collected by the collection surface can be intercepted and stored. Through water storage measures, flood flow in the flood season can be reduced, and rainstorm runoff can be prevented from gathering in depressions, increasing river flow in the dry season and the storage of water resources in the region in drought years.
[0003] However, the construction of water storage facilities such as water cellars, pools and ponds is costly and occupies a large area. Therefore, how to solve the above problems with a detachable soft rainwater collection cellar based on water conservancy projects and its production process, and ensure that the soft rainwater collection cellar has high corrosion resistance and will not be damaged by the acid, alkali and salt environment when placed on the ground, and ensure its service life, is also a technical problem that the present invention needs to solve. Summary of the invention
[0004] In order to overcome the above-mentioned technical problems, the purpose of the present invention is to provide a detachable soft rainwater collection cellar based on water conservancy projects and its production process: the water storage bag is connected to the mounting bracket by a fastening rope, and the water receiving bucket is connected to the mounting bracket by the Velcro fur surface and the Velcro thorn surface, and then the bottom end of the water inlet pipe is extended into the water receiving pipe, and then the threaded sleeve is connected to the water receiving pipe threaded connection, and finally the filter screen is placed on the top of the water inlet pipe to complete the assembly of the corrosion-resistant detachable soft rainwater collection cellar. The rainwater collection cellar is arranged to be detachable, and then it can be quickly installed and connected by installing the bracket, the water storage bag and the water receiving bucket, and the mounting bracket can be used repeatedly. Compared with the traditional water cellar, the rainwater collection cellar does not damage the soil, and the water storage bag and the water receiving bucket are both made of corrosion-resistant fabrics, and the corrosion-resistant fabrics have excellent corrosion resistance to solve the technical defects proposed by the background technology.
[0005] The purpose of the present invention can be achieved through the following technical solutions: a detachable soft rainwater collection cellar based on a water conservancy project, comprising a mounting bracket, a water storage bag and a water receiving bucket, wherein a water storage bag is placed in the inner cavity of the mounting bracket, and a drain valve is installed at the bottom of one side of the water storage bag;
[0006] The top corners of the water storage bag are installed with fastening ropes, the water storage bag is connected to the mounting bracket through the fastening ropes, the top of the mounting bracket is installed with a water receiving bucket, the axis of the water receiving bucket is installed with a water inlet pipe, the top axis of the water storage bag is installed with a water receiving pipe, the water receiving pipe and the water inlet pipe are matching components, the water storage bag and the water receiving bucket are both made of corrosion-resistant fabric, and the corrosion-resistant fabric is composed of non-woven fabric and corrosion-resistant coatings on the upper and lower surfaces of the non-woven fabric.
[0007] As a further solution of the present invention: the mounting bracket is composed of a rectangular frame and four legs, the four legs are respectively installed at the four corners of the bottom of the rectangular frame, Velcro fleece surfaces and Velcro thorn surfaces are installed at the four side edges of the bottom of the water receiving bucket, the Velcro fleece surfaces and Velcro thorn surfaces are matching components, and the four sides of the water receiving bucket are respectively connected to the four sides of the rectangular frame through the Velcro fleece surfaces and Velcro thorn surfaces.
[0008] As a further solution of the present invention: a filter screen is embedded in the top of the water inlet pipe, and the filter screen passes through the top axis of the water receiving bucket. The bottom end of the water inlet pipe is located inside the water receiving pipe. A limit ring is installed on the water inlet pipe, and the limit ring is located in the inner cavity of the connecting threaded sleeve. The connecting threaded sleeve is movably sleeved on the water inlet pipe, and the connecting threaded sleeve is threadedly connected to the top end of the water receiving pipe.
[0009] As a further solution of the present invention: a production process of a detachable soft rainwater collection cellar based on a water conservancy project comprises the following steps:
[0010] Step 1: Weigh 30-50 parts of corrosion-resistant epoxy resin, 5-15 parts of curing agent, 8-16 parts of diluent, 20-60 parts of polyacrylate and 1-8 parts of amino silicone oil according to weight, and set aside;
[0011] Step 2: Stir and mix the corrosion-resistant epoxy resin, curing agent, diluent, polyacrylate and amino silicone oil at a stirring rate of 800-1200 r / min for 3-5 hours to obtain a corrosion-resistant coating;
[0012] Step 3: Coat the upper and lower surfaces of the non-woven fabric with a corrosion-resistant coating, and solidify the coating at a temperature of 30-60°C to form a corrosion-resistant coating to obtain a corrosion-resistant fabric;
[0013] Step 4: Cut and sew the corrosion-resistant fabric into shape to obtain a water storage bag and a water receiving bucket;
[0014] Step 5: Sew the Velcro fleece surface and Velcro thorn surface on the four side edges of the water receiving bucket, connect the water inlet pipe to the threaded sleeve and then glue it to the axis of the water receiving bucket, glue the water receiving pipe to the top axis of the water storage bag, sew the fastening rope to the top corner of the water storage bag, and glue the drain valve to the bottom of one side of the water storage bag;
[0015] Step six: install the water receiving bucket on the mounting bracket, place the water storage bag inside the mounting bracket, connect the water inlet pipe and the water receiving pipe to obtain the corrosion-resistant detachable soft rainwater collection cellar.
[0016] As a further solution of the present invention: the curing agent is TAC-900 alicyclic amine curing agent, and the diluent is a mixture of n-butanol and xylene in a mass ratio of 7:3.
[0017] As a further solution of the present invention: the preparation process of the corrosion-resistant epoxy resin is as follows:
[0018] Step 1: Add 1,2,3-trichlorobenzene, sulfolane, potassium fluoride and benzyltriethylammonium chloride into a reaction kettle, introduce nitrogen protection, and keep the temperature and pressure at 170-180°C and 2-3MPa for 2-4h. After the reaction, distill to obtain intermediate 1;
[0019] The reaction principle is as follows:
[0020]
[0021] Step 2: Add intermediate 1 and dichloroethane to a three-necked flask equipped with a stirrer and a constant pressure dropping funnel, stir for 10-30 minutes at a temperature of 0-10°C and a stirring rate of 200-300 r / min, then add sodium bromide aqueous solution and sodium dihydrogen phosphate aqueous solution and continue stirring for 20-30 minutes, then add sodium hypochlorite aqueous solution dropwise while stirring, control the drop rate to 1 drop / s, control the temperature not to exceed 15°C, continue stirring and react for 1-2 hours after the dropwise addition is completed, and after the reaction is completed, let the reaction product stand for stratification, wash the organic phase with distilled water until neutral, and then remove the solvent by rotary evaporation to obtain intermediate 2;
[0022] The reaction principle is as follows:
[0023]
[0024] Step 3: Add sodium ethoxide and toluene to a three-necked flask equipped with a stirrer and a constant pressure dropping funnel, add intermediate 2 dropwise while stirring at a temperature of 20-25°C and a stirring rate of 200-300r / min, and control the dropping rate to be 1 drop / s. After the addition is completed, heat the temperature to 80-85°C and stir at a constant temperature for 5-6h. After the reaction is completed, cool the reaction product to room temperature, add deionized water and continue stirring for 5-10min, then stand and stratify, wash the organic phase with distilled water until neutral, then dry with anhydrous magnesium sulfate, vacuum filter, and distill the filtrate under reduced pressure. Collect the fractions at a temperature of 97-99°C and a pressure of 137.3Pa to obtain intermediate 3;
[0025] The reaction principle is as follows:
[0026]
[0027] Step 4: Add intermediate 3 and glacial acetic acid to a three-necked flask equipped with a stirrer, a reflux condenser and a constant pressure dropping funnel, stir for 10-30 minutes at a temperature of 20-25°C and a stirring rate of 200-300r / min, then add hydrobromic acid dropwise while stirring, and control the dropping rate to 1 drop / s. After the addition is complete, the temperature is raised to reflux, and then the reaction is stirred at a constant temperature for 9-10 hours. After the reaction is completed, the reaction product is added to ice water, and then extracted with toluene, allowed to stand and stratified, the organic phase is washed with distilled water until neutral, and then dried with anhydrous magnesium sulfate, vacuum filtered, and the filtrate is rotary evaporated to remove the solvent, and then distilled under reduced pressure, and the fractions at a temperature of 77-79°C and a pressure of 107.9Pa are collected to obtain intermediate 4;
[0028] The reaction principle is as follows:
[0029]
[0030] Step 5: Add intermediate 4, N,N-dimethylformamide and cesium carbonate to a reactor, add trifluorobromomethane while stirring at a temperature of 0°C and a stirring rate of 300-500r / min, then heat to 50-55°C and continue stirring to react for 8-10h. After the reaction is completed, pour the reaction product into ice water, extract with toluene, stand for stratification, wash the organic phase with distilled water until neutral, dry with anhydrous magnesium sulfate, vacuum filter, rotary evaporate the filtrate to remove the solvent, and then distill under reduced pressure to collect the fraction at a temperature of 89-91°C and a pressure of 500.1Pa to obtain intermediate 5;
[0031] The reaction principle is as follows:
[0032]
[0033] Step 6: Add magnesium powder and tetrahydrofuran to a four-necked flask equipped with a stirrer, an air duct, a reflux condenser and a constant pressure dropping funnel, stir for 10-30 min at a temperature of 40-45 ° C and a stirring rate of 200-300 r / min, then add 1 / 20 of the intermediate 5 dropwise while stirring, control the drop rate to 1 drop / s, continue stirring and reacting for 20-30 min after the addition is complete, then cool to 3-5 ° C, add the remaining intermediate 5 dropwise while stirring, control the drop rate to 1-3 drops / s, heat to 20-25 ° C after the addition is complete, stir and react for 1-2 h at a constant temperature, then add silicon tetrachloride solution dropwise, control the drop rate to 1 drop / s s, control the temperature not to exceed -10°C, after the addition is completed, heat to 20-25°C and stir at a constant temperature for 5-6h, after the reaction is completed, remove unreacted silicon tetrachloride in vacuo at a temperature of 30-40°C to obtain intermediate 6, then add triethylamine dropwise while stirring at a temperature of -40°C and a stirring rate of 200-300r / min, control the drop rate to 1 drop / s, after the addition is completed, add anhydrous methanol dropwise while stirring, control the drop rate to 1 drop / s, control the temperature not to exceed -20°C, after the addition is completed, heat to 20-25°C and stir at a constant temperature for 5-6h, after the reaction is completed, filter the reaction product under nitrogen protection, collect the filter cake, and dry to obtain intermediate 7;
[0034] The reaction principle is as follows:
[0035]
[0036] Step seven: Add EP44, intermediate 7, dibutyltin dilaurate and toluene into a four-necked flask equipped with a stirrer, a reflux condenser and a constant pressure dropping funnel, stir for 8-10 hours at a temperature of 90-100°C and a stirring rate of 300-500r / min. After the reaction is completed, the reaction product is rotary evaporated to remove the solvent, and then placed in a vacuum drying oven, dried at a temperature of 50-55°C for 8-10 hours, and then heated to 80-90°C and dried for 40-50 hours to obtain a corrosion-resistant epoxy resin.
[0037] The reaction principle is as follows:
[0038]
[0039] As a further scheme of the present invention: the usage ratio of the 1,2,3-trichlorobenzene, cyclopentane, potassium fluoride and benzyltriethylammonium chloride in step 1 is 0.1 mol: 0.2-0.25 mol: 0.3-0.4 mol: 0.15-0.35 g.
[0040] As a further scheme of the present invention: the dosage ratio of the intermediate 1, dichloroethane, sodium bromide aqueous solution, sodium dihydrogen phosphate aqueous solution and sodium hypochlorite aqueous solution in step 2 is 0.1 mol: 50 mL: 40-50 mL: 50-60 mL: 80-100 g, the mass fraction of the sodium bromide aqueous solution is 20-25%, the mass fraction of the sodium dihydrogen phosphate aqueous solution is 20-25%, and the mass fraction of the sodium hypochlorite aqueous solution is 10-15%.
[0041] As a further solution of the present invention: the usage ratio of the sodium ethoxide, toluene, intermediate 2 and deionized water in step three is 0.3 mol: 80-100 mL: 0.2 mol: 80-100 mL.
[0042] As a further solution of the present invention: the usage ratio of the intermediate 3, glacial acetic acid and hydrobromic acid in step 4 is 0.5 mol: 150 mL: 50-60 mL, and the mass fraction of the hydrobromic acid is 40-47%.
[0043] As a further solution of the present invention: the usage ratio of the intermediate 4, N,N-dimethylformamide, cesium carbonate and bromotrifluoromethane in step 5 is 0.1 mol: 150-200 mL: 40-50 g: 0.15-0.2 mol.
[0044] As a further scheme of the present invention: the dosage ratio of the magnesium powder, tetrahydrofuran, intermediate 5, silicon tetrachloride solution, triethylamine and anhydrous methanol in step six is 12-15g:400-450mL:0.5mol:400-450mL:1.5-2.0mol:5mol, and the silicon tetrachloride solution is a solution formed by dissolving carbon tetrachloride in tetrahydrofuran at a ratio of 200g:150-200mL, and the solution is cooled to below -40°C for storage.
[0045] As a further solution of the present invention: the usage ratio of EP44, intermediate 7, dibutyltin dilaurate and toluene in step seven is 50-70g: 20-30g: 1.5-2.0g: 60-70g.
[0046] The beneficial effects of the present invention are as follows:
[0047] The detachable soft rainwater collection cellar based on water conservancy projects of the present invention and its production process, the water storage water bag is connected to the installation bracket by a fastening rope, the water receiving bucket is connected to the installation bracket by a Velcro fur surface and a Velcro thorn surface, then the bottom end of the water inlet pipe is extended into the water receiving pipe, and then the threaded sleeve is connected to the water receiving pipe threaded connection, and finally the filter screen is placed on the top of the water inlet pipe to complete the assembly of the corrosion-resistant detachable soft rainwater collection cellar, the rainwater collection cellar is set to be detachable, and then it can be quickly installed and connected by the installation bracket, the water storage water bag and the water receiving bucket, it is easy to use, the installation bracket can be used repeatedly, and compared with the traditional water cellar, the rainwater collection cellar does not damage the soil, and the water storage water bag and the water receiving bucket are both made of corrosion-resistant fabrics, the corrosion-resistant fabrics have excellent corrosion resistance, therefore, it will not be easily corroded when placed on the ground, the service life is long, and the use cost is reduced;
[0048] In the process of preparing a corrosion-resistant detachable soft rainwater collection cellar, a corrosion-resistant fabric is first prepared, 1,2,3-trichlorobenzene is reacted with potassium fluoride to generate intermediate 1, and the fluorine element is introduced. Then, intermediate 1 is reacted with sodium bromide to introduce the bromine element into intermediate 1 to obtain intermediate 2. Then, intermediate 2 is reacted with sodium ethoxide to generate intermediate 3. Intermediate 3 is reacted with hydrobromic acid to generate intermediate 4. Intermediate 4 is reacted with trifluorobromomethane to generate intermediate 5, and a CF bond is introduced. Then, intermediate 5 is reacted with silicon tetrachloride to generate intermediate 6, and then reacted with anhydrous methanol to generate intermediate 7. Intermediate 7 is EP4. 4 is modified, a large number of Si-O bonds, CF bonds and benzene rings are introduced into EP44 to obtain a corrosion-resistant epoxy resin, and a coating is made of the corrosion-resistant epoxy resin to form a coating on a non-woven fabric to obtain the corrosion-resistant fabric. The molecular chain of the corrosion-resistant epoxy resin contains a large number of Si-O bonds, CF bonds and benzene rings. The benzene rings are highly stable and difficult to be destroyed. The bond energies of the Si-O bonds and CF bonds are large, thereby giving the corrosion-resistant epoxy resin excellent performance in terms of heat resistance, weather resistance and chemical resistance. Therefore, under the synergistic effect of the benzene rings and the Si-O bonds and CF bonds, the corrosion-resistant epoxy resin exhibits good corrosion resistance. BRIEF DESCRIPTION OF THE DRAWINGS
[0049] The present invention will be further described below in conjunction with the accompanying drawings.
[0050] Figure 1 It is a structural schematic diagram of a detachable soft rainwater collection cellar based on a water conservancy project in the present invention;
[0051] Figure 2 It is a bottom view of the water receiving bucket in the present invention;
[0052] Figure 3 This is a connection view of the water inlet pipe and the water receiving pipe in the present invention;
[0053] Figure 4 It is a structural schematic diagram of the corrosion-resistant fabric in the present invention.
[0054] In the figure: 101, mounting bracket; 102, water storage bag; 103, drain valve; 104, fastening rope; 105, water receiving bucket; 106, water inlet pipe; 107, filter screen; 108, Velcro fleece surface; 109, Velcro thorn surface; 110, connecting threaded sleeve; 111, limiting ring; 112, water receiving pipe; 113, non-woven fabric; 114, corrosion-resistant coating. DETAILED DESCRIPTION
[0055] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0056] Example 1: Please refer to Figure 1-4 As shown, this embodiment is a detachable soft rainwater cellar based on a water conservancy project, comprising a mounting bracket 101, a water storage bag 102 and a water receiving bucket 105. The water storage bag 102 is placed in the inner cavity of the mounting bracket 101, a drain valve 103 is installed at the bottom of one side of the water storage bag 102, and fastening ropes 104 are installed at the top corners of the water storage bag 102. The water storage bag 102 is connected to the mounting bracket 101 through the fastening ropes 104. A water receiving bucket 105 is installed on the top of the mounting bracket 101, a water inlet pipe 106 is installed at the axis of the water receiving bucket 105, a water receiving pipe 112 is installed at the top axis of the water storage bag 102, the water receiving pipe 112 and the water inlet pipe 106 are matching components, the water storage bag 102 and the water receiving bucket 105 are both made of corrosion-resistant fabrics, and the corrosion-resistant fabrics are composed of non-woven fabrics 113 and corrosion-resistant coatings 114 on the upper and lower surfaces of the non-woven fabrics 113;
[0057] The mounting bracket 101 is composed of a rectangular frame and four legs, and the four legs are respectively mounted at the four corners of the bottom of the rectangular frame. Velcro velcro surfaces 108 and Velcro thorn surfaces 109 are installed at the four side edges of the bottom of the water receiving bucket 105. The Velcro velcro surfaces 108 and Velcro thorn surfaces 109 are matching components. The four sides of the water receiving bucket 105 are respectively connected to the four sides of the rectangular frame through the Velcro velcro surfaces 108 and Velcro thorn surfaces 109;
[0058] A filter screen 107 is embedded in the top of the water inlet pipe 106, and the filter screen 107 passes through the top axis of the water receiving bucket 105. The bottom end of the water inlet pipe 106 is located inside the water receiving pipe 112. A limit ring 111 is installed on the water inlet pipe 106, and the limit ring 111 is located in the inner cavity of the connecting threaded sleeve 110. The connecting threaded sleeve 110 is movably sleeved on the water inlet pipe 106, and the connecting threaded sleeve 110 is threadedly connected to the top end of the water receiving pipe 112.
[0059] Embodiment 2: This embodiment is a method for preparing a corrosion-resistant epoxy resin, comprising the following steps:
[0060] Step 1: add 0.1 mol 1,2,3-trichlorobenzene, 0.2-0.25 mol sulfolane, 0.3-0.4 mol potassium fluoride and 0.15-0.35 g benzyltriethylammonium chloride into a reaction kettle, introduce nitrogen protection, keep the temperature and pressure at 170-180°C and 2-3 MPa for 2-4 hours, and distill after the reaction to obtain intermediate 1;
[0061] Step 2: Add 0.1 mol of intermediate 1 and 50 mL of dichloroethane to a three-necked flask equipped with a stirrer and a constant pressure dropping funnel, stir for 10-30 min at a temperature of 0-10 ° C and a stirring rate of 200-300 r / min, then add 40-50 mL of a 20-25% sodium bromide aqueous solution and 50-60 mL of a 20-25% sodium dihydrogen phosphate aqueous solution and continue stirring for 20-30 min, then add 80-100 g of a 10-15% sodium hypochlorite aqueous solution dropwise while stirring, control the drop rate to 1 drop / s, control the temperature not to exceed 15 ° C, continue stirring the reaction for 1-2 h after the dropwise addition is completed, and after the reaction is completed, let the reaction product stand for stratification, wash the organic phase with distilled water until neutral, and then remove the solvent by rotary evaporation to obtain intermediate 2;
[0062] Step 3: Add 0.3 mol sodium ethoxide and 80-100 mL toluene to a three-necked flask equipped with a stirrer and a constant pressure dropping funnel, add 0.2 mol intermediate 2 dropwise while stirring at a temperature of 20-25 ° C and a stirring rate of 200-300 r / min, and control the dropping rate to 1 drop / s. After the dropwise addition is completed, the temperature is raised to 80-85 ° C and stirred at a constant temperature for 5-6 hours. After the reaction is completed, the reaction product is cooled to room temperature, and then 80-100 mL of deionized water is added and continued to stir for 5-10 minutes, and then allowed to stand for stratification, the organic phase is washed with distilled water until neutral, and then dried with anhydrous magnesium sulfate, vacuum filtered, and the filtrate is distilled under reduced pressure. The fractions under the conditions of a temperature of 97-99 ° C and a pressure of 137.3 Pa are collected to obtain intermediate 3;
[0063] Step 4: Add 0.5 mol of intermediate 3 and 150 mL of glacial acetic acid to a three-necked flask equipped with a stirrer, a reflux condenser and a constant pressure dropping funnel, stir for 10-30 min at a temperature of 20-25 ° C and a stirring rate of 200-300 r / min, then add 50-60 mL of hydrobromic acid with a mass fraction of 40-47% dropwise while stirring, and control the dropping rate to 1 drop / s. After the addition is completed, the temperature is raised to reflux, and then the reaction is stirred at a constant temperature for 9-10 hours. After the reaction is completed, the reaction product is added to ice water, and then extracted with toluene, allowed to stand and stratified, the organic phase is washed with distilled water until neutral, and then dried with anhydrous magnesium sulfate, vacuum filtered, and the filtrate is rotary evaporated to remove the solvent, and then distilled under reduced pressure, and the fractions at a temperature of 77-79 ° C and a pressure of 107.9 Pa are collected to obtain intermediate 4;
[0064] Step 5: Add 0.1 mol of intermediate 4, 150-200 mL of N, N-dimethylformamide and 40-50 g of cesium carbonate to a reactor, and introduce 0.15-0.2 mol of bromotrifluoromethane while stirring at a temperature of 0°C and a stirring rate of 300-500 r / min, then heat to 50-55°C and continue stirring to react for 8-10 hours. After the reaction is completed, pour the reaction product into ice water, extract with toluene, stand and stratify, wash the organic phase with distilled water until neutral, dry with anhydrous magnesium sulfate, vacuum filter, rotary evaporate the filtrate to remove the solvent, and then distill under reduced pressure to collect the fraction at a temperature of 89-91°C and a pressure of 500.1 Pa to obtain intermediate 5;
[0065] Step 6: Add 12-15g magnesium powder and 400-450mL tetrahydrofuran to a four-necked flask equipped with a stirrer, an air guide tube, a reflux condenser and a constant pressure dropping funnel, stir for 10-30min at a temperature of 40-45°C and a stirring rate of 200-300r / min, then add 0.025mol of intermediate 5 dropwise while stirring, control the drop rate to 1 drop / s, continue stirring and reacting for 20-30min after the addition is complete, then cool to 3-5°C, add 0.475mol of intermediate 5 dropwise while stirring, control the drop rate to 1-3 drops / s, heat to 20-25°C after the addition is complete, and stir and react for 1-2h at a constant temperature, then add carbon tetrachloride dropwise according to 200g:150-200mL dissolved in tetrahydrofuran to form -40°C The following silicon tetrachloride solution 400-450mL, control the drop rate to 1 drop / s, control the temperature not to exceed -10°C, after the dropwise addition is completed, heat to 20-25°C and stir at a constant temperature for 5-6h, after the reaction is completed, remove the unreacted silicon tetrachloride in vacuo at a temperature of 30-40°C to obtain intermediate 6, then add 1.5-2.0mol triethylamine dropwise while stirring at a temperature of -40°C and a stirring rate of 200-300r / min, control the drop rate to 1 drop / s, after the dropwise addition is completed, add 5mol anhydrous methanol dropwise while stirring, control the drop rate to 1 drop / s, control the temperature not to exceed -20°C, after the dropwise addition is completed, heat to 20-25°C and stir at a constant temperature for 5-6h, after the reaction is completed, filter the reaction product under nitrogen protection, collect the filter cake, and dry it to obtain intermediate 7;
[0066] Step seven: Add 50-70g EP44, 20-30g intermediate 7, 1.5-2.0g dibutyltin dilaurate and 60-70g toluene into a four-necked flask equipped with a stirrer, a reflux condenser and a constant pressure dropping funnel, stir for 8-10h at a temperature of 90-100°C and a stirring rate of 300-500r / min. After the reaction is completed, the reaction product is rotary evaporated to remove the solvent, and then placed in a vacuum drying oven, dried at a temperature of 50-55°C for 8-10h, and then heated to 80-90°C and dried for 40-50h to obtain a corrosion-resistant epoxy resin.
[0067] Embodiment 3: This embodiment is a method for preparing a corrosion-resistant epoxy resin, comprising the following steps:
[0068] Step 1: add 0.1 mol 1,2,3-trichlorobenzene, 0.2-0.25 mol sulfolane, 0.3-0.4 mol potassium fluoride and 0.15-0.35 g benzyltriethylammonium chloride into a reaction kettle, introduce nitrogen protection, keep the temperature and pressure at 170-180°C and 2-3 MPa for 2-4 hours, and distill after the reaction to obtain intermediate 1;
[0069] Step 2: Add 0.1 mol of intermediate 1 and 50 mL of dichloroethane to a three-necked flask equipped with a stirrer and a constant pressure dropping funnel, stir for 10-30 min at a temperature of 0-10 ° C and a stirring rate of 200-300 r / min, then add 40-50 mL of a 20-25% sodium bromide aqueous solution and 50-60 mL of a 20-25% sodium dihydrogen phosphate aqueous solution and continue stirring for 20-30 min, then add 80-100 g of a 10-15% sodium hypochlorite aqueous solution dropwise while stirring, control the drop rate to 1 drop / s, control the temperature not to exceed 15 ° C, continue stirring the reaction for 1-2 h after the dropwise addition is completed, and after the reaction is completed, let the reaction product stand for stratification, wash the organic phase with distilled water until neutral, and then remove the solvent by rotary evaporation to obtain intermediate 2;
[0070] Step 3: Add 0.3 mol sodium ethoxide and 80-100 mL toluene to a three-necked flask equipped with a stirrer and a constant pressure dropping funnel, add 0.2 mol intermediate 2 dropwise while stirring at a temperature of 20-25 ° C and a stirring rate of 200-300 r / min, and control the dropping rate to 1 drop / s. After the dropwise addition is completed, the temperature is raised to 80-85 ° C and stirred at a constant temperature for 5-6 hours. After the reaction is completed, the reaction product is cooled to room temperature, and then 80-100 mL of deionized water is added and continued to stir for 5-10 minutes, and then allowed to stand for stratification, the organic phase is washed with distilled water until neutral, and then dried with anhydrous magnesium sulfate, vacuum filtered, and the filtrate is distilled under reduced pressure. The fractions under the conditions of a temperature of 97-99 ° C and a pressure of 137.3 Pa are collected to obtain intermediate 3;
[0071] Step 4: Add 0.5 mol of intermediate 3 and 150 mL of glacial acetic acid to a three-necked flask equipped with a stirrer, a reflux condenser and a constant pressure dropping funnel, stir for 10-30 min at a temperature of 20-25 ° C and a stirring rate of 200-300 r / min, then add 50-60 mL of hydrobromic acid with a mass fraction of 40-47% dropwise while stirring, and control the dropping rate to 1 drop / s. After the addition is completed, the temperature is raised to reflux, and then the reaction is stirred at a constant temperature for 9-10 hours. After the reaction is completed, the reaction product is added to ice water, and then extracted with toluene, allowed to stand and stratified, the organic phase is washed with distilled water until neutral, and then dried with anhydrous magnesium sulfate, vacuum filtered, and the filtrate is rotary evaporated to remove the solvent, and then distilled under reduced pressure, and the fractions at a temperature of 77-79 ° C and a pressure of 107.9 Pa are collected to obtain intermediate 4;
[0072] Step 5: Add 0.1 mol of intermediate 4, 150-200 mL of N, N-dimethylformamide and 40-50 g of cesium carbonate to a reactor, and introduce 0.15-0.2 mol of bromotrifluoromethane while stirring at a temperature of 0°C and a stirring rate of 300-500 r / min, then heat to 50-55°C and continue stirring to react for 8-10 hours. After the reaction is completed, pour the reaction product into ice water, extract with toluene, stand and stratify, wash the organic phase with distilled water until neutral, dry with anhydrous magnesium sulfate, vacuum filter, rotary evaporate the filtrate to remove the solvent, and then distill under reduced pressure to collect the fraction at a temperature of 89-91°C and a pressure of 500.1 Pa to obtain intermediate 5;
[0073] Step 6: Add 12-15g magnesium powder and 400-450mL tetrahydrofuran to a four-necked flask equipped with a stirrer, an air guide tube, a reflux condenser and a constant pressure dropping funnel, stir for 10-30min at a temperature of 40-45°C and a stirring rate of 200-300r / min, then add 0.025mol of intermediate 5 dropwise while stirring, control the drop rate to 1 drop / s, continue stirring and reacting for 20-30min after the addition is complete, then cool to 3-5°C, add 0.475mol of intermediate 5 dropwise while stirring, control the drop rate to 1-3 drops / s, heat to 20-25°C after the addition is complete, and stir and react for 1-2h at a constant temperature, then add carbon tetrachloride dropwise according to 200g:150-200mL dissolved in tetrahydrofuran to form -40°C The following silicon tetrachloride solution 400-450mL, control the drop rate to 1 drop / s, control the temperature not to exceed -10°C, after the dropwise addition is completed, heat to 20-25°C and stir at a constant temperature for 5-6h, after the reaction is completed, remove the unreacted silicon tetrachloride in vacuo at a temperature of 30-40°C to obtain intermediate 6, then add 1.5-2.0mol triethylamine dropwise while stirring at a temperature of -40°C and a stirring rate of 200-300r / min, control the drop rate to 1 drop / s, after the dropwise addition is completed, add 5mol anhydrous methanol dropwise while stirring, control the drop rate to 1 drop / s, control the temperature not to exceed -20°C, after the dropwise addition is completed, heat to 20-25°C and stir at a constant temperature for 5-6h, after the reaction is completed, filter the reaction product under nitrogen protection, collect the filter cake, and dry it to obtain intermediate 7;
[0074] Step seven: Add 50-70g EP44, 20-30g intermediate 7, 1.5-2.0g dibutyltin dilaurate and 60-70g toluene into a four-necked flask equipped with a stirrer, a reflux condenser and a constant pressure dropping funnel, stir for 8-10h at a temperature of 90-100°C and a stirring rate of 300-500r / min. After the reaction is completed, the reaction product is rotary evaporated to remove the solvent, and then placed in a vacuum drying oven, dried at a temperature of 50-55°C for 8-10h, and then heated to 80-90°C and dried for 40-50h to obtain a corrosion-resistant epoxy resin.
[0075] Example 4: Please refer to Figure 1-4 As shown, this embodiment is a production process of a detachable soft rainwater collection cellar based on a water conservancy project, comprising the following steps:
[0076] Step 1: Weigh 30 parts of the corrosion-resistant epoxy resin, 5 parts of the curing agent, 8 parts of the diluent, 20 parts of the polyacrylate and 1 part of the amino silicone oil from Example 2 according to weight parts, and set aside;
[0077] Step 2: Stir and mix the corrosion-resistant epoxy resin, curing agent, diluent, polyacrylate and amino silicone oil at a stirring rate of 800 r / min for 3 hours to obtain a corrosion-resistant coating;
[0078] Step 3: coating the upper and lower surfaces of the non-woven fabric 113 with a corrosion-resistant coating, and curing the coating at a temperature of 30° C. to form a corrosion-resistant coating 114 to obtain a corrosion-resistant fabric;
[0079] Step 4: Cut and sew the corrosion-resistant fabric into shape to obtain a water storage bag 102 and a water receiving bucket 105;
[0080] Step 5: Sew the Velcro fleece surface 108 and the Velcro thorn surface 109 on the four side edges of the water receiving bucket 105, sleeve the water inlet pipe 106 with the threaded sleeve 110 and then bond it to the axis of the water receiving bucket 105, bond the water receiving pipe 112 to the top axis of the water storage bag 102, sew the fastening rope 104 to the top corner of the water storage bag 102, and bond the drain valve 103 to the bottom of one side of the water storage bag 102;
[0081] Step 6: Install the water receiving bucket 105 on the mounting bracket 101, place the water storage bag 102 inside the mounting bracket 101, connect the water inlet pipe 106 and the water receiving pipe 112, and obtain the corrosion-resistant detachable soft rainwater collection cellar.
[0082] Example 5: Please refer to Figure 1-4 As shown, this embodiment is a production process of a detachable soft rainwater collection cellar based on a water conservancy project, comprising the following steps:
[0083] Step 1: Weigh 50 parts of the corrosion-resistant epoxy resin, 15 parts of the curing agent, 16 parts of the diluent, 60 parts of the polyacrylate and 8 parts of the amino silicone oil from Example 3 according to weight parts, and set aside;
[0084] Step 2: stirring and mixing the corrosion-resistant epoxy resin, curing agent, diluent, polyacrylate and amino silicone oil at a stirring rate of 1200 r / min for 5 hours to obtain a corrosion-resistant coating;
[0085] Step 3: coating the upper and lower surfaces of the non-woven fabric 113 with a corrosion-resistant coating, and curing the coating at a temperature of 60° C. to form a corrosion-resistant coating 114 to obtain a corrosion-resistant fabric;
[0086] Step 4: Cut and sew the corrosion-resistant fabric into shape to obtain a water storage bag 102 and a water receiving bucket 105;
[0087] Step 5: Sew the Velcro fleece surface 108 and the Velcro thorn surface 109 on the four side edges of the water receiving bucket 105, sleeve the water inlet pipe 106 with the threaded sleeve 110 and then bond it to the axis of the water receiving bucket 105, bond the water receiving pipe 112 to the top axis of the water storage bag 102, sew the fastening rope 104 to the top corner of the water storage bag 102, and bond the drain valve 103 to the bottom of one side of the water storage bag 102;
[0088] Step 6: Install the water receiving bucket 105 on the mounting bracket 101, place the water storage bag 102 inside the mounting bracket 101, connect the water inlet pipe 106 and the water receiving pipe 112, and obtain the corrosion-resistant detachable soft rainwater collection cellar.
[0089] The corrosion resistance of the corrosion-resistant fabrics in Examples 4-5 was tested. The corrosion rate test was as follows: the corrosion rate of the corrosion-resistant fabric with an area of 20 cm × 20 cm was calculated by soaking it in the following environment for 48 hours = corrosion area / total area. The test results are as follows:
[0090] sample Water Environment pH = 3 sulfuric acid environment pH = 10 sodium hydroxide environment Example 4 0.02% 0.65% 0.51% Example 5 0.01% 0.48% 0.42%
[0091] Referring to the above data, it can be seen that the corrosion-resistant fabric has good water, acid and alkali resistance. Therefore, the prepared corrosion-resistant detachable soft rainwater collection cellar is not easily corroded, avoiding leakage or even damage due to corrosion, thereby extending its service life.
[0092] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example" and the like means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in a suitable manner in any one or more embodiments or examples. The above contents are merely examples and explanations of the present invention. As long as the technicians in this technical field make various modifications or supplements to the specific embodiments described or replace them in a similar manner, they shall all fall within the scope of protection of the present invention as long as they do not deviate from the invention or exceed the scope defined by the claims.
Claims
1. A detachable soft rainwater collection cellar based on a water conservancy project, comprising a mounting bracket (101), a water storage bag (102) and a water receiving bucket (105), wherein the water storage bag (102) is placed in the inner cavity of the mounting bracket (101), and a drain valve (103) is installed at the bottom of one side of the water storage bag (102). Features: A fastening rope (104) is installed at the top corner of the water storage bag (102), and the water storage bag (102) is connected to the mounting bracket (101) through the fastening rope (104). A water receiving bucket (105) is installed at the top of the mounting bracket (101), and a water inlet pipe (106) is installed at the axis of the water receiving bucket (105). A water receiving pipe (112) is installed at the axis of the top of the water storage bag (102), and the water receiving pipe (112) and the water inlet pipe (106) are matching components. The water storage bag (102) and the water receiving bucket (105) are both made of corrosion-resistant fabrics, and the corrosion-resistant fabrics are composed of non-woven fabrics (113) and corrosion-resistant coatings (114) on the upper and lower surfaces of the non-woven fabrics (113).
2. The detachable soft rainwater collection cellar based on water conservancy project according to claim 1, It is characterized in that The mounting bracket (101) is composed of a rectangular frame and four legs, the four legs are respectively mounted at the four corners of the bottom of the rectangular frame, the edges of the four sides of the bottom of the water receiving bucket (105) are all mounted with Velcro fleece surfaces (108) and Velcro thorn surfaces (109), the Velcro fleece surfaces (108) and Velcro thorn surfaces (109) are matching components, and the four sides of the water receiving bucket (105) are respectively connected to the four sides of the rectangular frame through the Velcro fleece surfaces (108) and Velcro thorn surfaces (109).
3. The detachable soft rainwater collection cellar based on water conservancy project according to claim 2, It is characterized in that A filter screen (107) is embedded in the top of the water inlet pipe (106), and the filter screen (107) passes through the top axis of the water receiving bucket (105). The bottom end of the water inlet pipe (106) is located inside the water receiving pipe (112). A limit ring (111) is installed on the water inlet pipe (106), and the limit ring (111) is located in the inner cavity of the connecting threaded sleeve (110). The connecting threaded sleeve (110) is movably sleeved on the water inlet pipe (106), and the connecting threaded sleeve (110) is threadedly connected to the top of the water receiving pipe (112).
4. The production process of the detachable soft rainwater collection cellar based on the water conservancy project as claimed in claim 3, It is characterized in that The following steps are involved: Step 1: Weigh 30-50 parts of corrosion-resistant epoxy resin, 5-15 parts of curing agent, 8-16 parts of diluent, 20-60 parts of polyacrylate and 1-8 parts of amino silicone oil according to weight, and set aside; Step 2: Stir and mix the corrosion-resistant epoxy resin, curing agent, diluent, polyacrylate and amino silicone oil at a stirring rate of 800-1200 r / min for 3-5 hours to obtain a corrosion-resistant coating; Step 3: coating the upper and lower surfaces of the non-woven fabric (113) with a corrosion-resistant coating, and curing the coating at a temperature of 30-60° C. to form a corrosion-resistant coating (114), thereby obtaining a corrosion-resistant fabric; Step 4: cutting and sewing the corrosion-resistant fabric into shape to obtain a water storage bag (102) and a water receiving bucket (105); Step 5: Sew the Velcro fleece surface (108) and Velcro thorn surface (109) on the four side edges of the water receiving bucket (105), sleeve the water inlet pipe (106) on the threaded sleeve (110) and then bond it to the axis of the water receiving bucket (105), bond the water receiving pipe (112) to the top axis of the water storage bag (102), sew the fastening rope (104) to the top corner of the water storage bag (102), and bond the drain valve (103) to the bottom of one side of the water storage bag (102); Step 6: Install the water receiving bucket (105) on the mounting bracket (101), place the water storage bag (102) inside the mounting bracket (101), connect the water inlet pipe (106) and the water receiving pipe (112), and obtain the corrosion-resistant detachable soft rainwater collection cellar.
5. The production process of the detachable soft rainwater collection cellar based on water conservancy project according to claim 4, It is characterized in that The curing agent is TAC-900 alicyclic amine curing agent, and the diluent is a mixture of n-butanol and xylene in a mass ratio of 7:
3.
6. The production process of the detachable soft rainwater collection cellar based on water conservancy project according to claim 4, It is characterized in that The preparation process of the corrosion-resistant epoxy resin is as follows: Step 1: Add 1,2,3-trichlorobenzene, sulfolane, potassium fluoride and benzyltriethylammonium chloride into a reaction kettle, introduce nitrogen to protect the reaction under heat and pressure, and perform rectification after the reaction to obtain intermediate 1; Step 2: Add intermediate 1 and dichloroethane into a three-necked flask and stir, then add sodium bromide aqueous solution and sodium dihydrogen phosphate aqueous solution and continue stirring, then add sodium hypochlorite aqueous solution dropwise while stirring, continue stirring to react after the addition is complete, and after the reaction is completed, let the reaction product stand for stratification, wash the organic phase until it is neutral, and then rotary evaporate to obtain intermediate 2; Step 3: Sodium ethoxide and toluene are added to a three-necked flask, and the intermediate 2 is added dropwise while stirring. After the addition is completed, the temperature is raised and the stirring is constant. After the reaction is completed, the reaction product is cooled to room temperature, and then deionized water is added and continued to be stirred. Then, the reaction product is allowed to stand for stratification, and the organic phase is washed with water until it is neutral, and then dried and vacuum filtered. The filtrate is distilled under reduced pressure, and the fractions are collected to obtain the intermediate 3; Step 4: Add intermediate 3 and glacial acetic acid into a three-necked flask and stir, then add hydrobromic acid dropwise while stirring, raise the temperature to reflux after the addition is complete, then stir and react at a constant temperature, add the reaction product into ice water after the reaction is complete, then extract, stand and separate, wash the organic phase until it is neutral, then dry, vacuum filter, rotary evaporate the filtrate, then distill under reduced pressure, collect the fractions, and obtain intermediate 4; Step 5: Add intermediate 4, N,N-dimethylformamide and cesium carbonate to a reactor, add bromotrifluoromethane while stirring, then heat up and continue stirring to react, pour the reaction product into ice water after the reaction is completed, then extract, stand and separate, wash the organic phase until neutral, then dry, vacuum filter, rotary evaporate the filtrate, then distill under reduced pressure, collect the fractions, and obtain intermediate 5; Step 6: Add magnesium powder and tetrahydrofuran to a four-necked flask and stir, then add part of the intermediate 5 dropwise while stirring, continue to stir and react after the addition is complete, then cool down and add the remaining intermediate 5 dropwise while stirring, raise the temperature and stir and react at a constant temperature after the addition is complete, then add silicon tetrachloride solution dropwise, raise the temperature and stir and react at a constant temperature after the addition is complete, remove unreacted silicon tetrachloride in vacuo after the reaction is completed to obtain intermediate 6, then add triethylamine dropwise while stirring, add anhydrous methanol dropwise while stirring after the addition is complete, raise the temperature and stir and react at a constant temperature after the addition is complete, filter the reaction product after the reaction is completed, collect the filter cake, and dry it to obtain intermediate 7; Step 7: Add EP44, intermediate 7, dibutyltin dilaurate and toluene into a four-necked flask and stir. After the reaction is completed, the reaction product is rotary evaporated and then dried to obtain a corrosion-resistant epoxy resin.
7. The production process of the detachable soft rainwater collection cellar based on water conservancy project according to claim 6, It is characterized in that The dosage ratio of the 1,2,3-trichlorobenzene, cyclopentane, potassium fluoride and benzyltriethylammonium chloride in step 1 is 0.1 mol: 0.2-0.25 mol: 0.3-0.4 mol: 0.15-0.35 g; the dosage ratio of the intermediate 1, dichloroethane, sodium bromide aqueous solution, sodium dihydrogen phosphate aqueous solution and sodium hypochlorite aqueous solution in step 2 is 0.1 mol: 50 mL: 40-50 mL: 50-60 mL: 80-100 g, the mass fraction of the sodium bromide aqueous solution is 20-25%, the mass fraction of the sodium dihydrogen phosphate aqueous solution is 20-25%, and the mass fraction of the sodium hypochlorite aqueous solution is 10-15%.
8. The production process of the detachable soft rainwater collection cellar based on water conservancy project according to claim 6, It is characterized in that The dosage ratio of the sodium ethoxide, toluene, intermediate 2 and deionized water in step 3 is 0.3 mol: 80-100 mL: 0.2 mol: 80-100 mL; the dosage ratio of the intermediate 3, glacial acetic acid and hydrobromic acid in step 4 is 0.5 mol: 150 mL: 50-60 mL, and the mass fraction of the hydrobromic acid is 40-47%; the dosage ratio of the intermediate 4, N, N-dimethylformamide, cesium carbonate and trifluorobromomethane in step 5 is 0.1 mol: 150-200 mL: 40-50 g: 0.15-0.2 mol.
9. The production process of the detachable soft rainwater collection cellar based on water conservancy project according to claim 6, It is characterized in that The amount ratio of the magnesium powder, tetrahydrofuran, intermediate 5, silicon tetrachloride solution, triethylamine and anhydrous methanol in step six is 12-15g: 400-450mL: 0.5mol: 400-450mL: 1.5-2.0mol: 5mol, and the silicon tetrachloride solution is a solution formed by dissolving carbon tetrachloride in tetrahydrofuran at a ratio of 200g: 150-200mL, and the solution is cooled to below -40°C for storage; the amount ratio of the EP44, intermediate 7, dibutyltin dilaurate and toluene in step seven is 50-70g: 20-30g: 1.5-2.0g: 60-70g.