Fracture forming and flow experiment combined operation method for tight reservoir refracturing rock core
Through the joint method of repeated fracturing cores of dense reservoirs and flow experiments, the problem of fracture distribution differences caused by the separation of core production and flow experiments in the existing technology is solved, and more accurate simulation of dense reservoirs and capacity maintenance is achieved. , improve the accuracy of the experiment and capacity maintenance effect.
Patent Information
- Application Number
- CN202410930562.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-03-01
- Filing Date
- 2024-07-11
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The production and flow experiment of existing repeated fracturing cores are separated from flow experiments, resulting in large differences in the distribution of fractures from the actual formation, making it difficult to simulate the repeated fracturing process of dense reservoirs. The production capacity of dense rocks such as shale and limestone gradually decreases, and it takes multiple times. Renovation maintains production capacity.
The joint method of joint fracturing cores of dense reservoirs and flow experiments is adopted. Through multiple fracturing and flow experimental cycles, the experimental cores are completed and heat shrink tube wrapping and MTS three The mechanical analysis of axial rocks, the comprehensive use of confining pumps, axial pressure pumps and temperature control systems, simulate formation conditions, and conduct fracturing and flow experiments of the core.
It better simulates the development changes of reservoir fractures, provides experimental cores that are closer to the actual formation, extends the number of simulated fracturing times of the experiment, improves the accuracy of the experiment and the capacity maintenance of repeated fracturing.
Smart Images

Figure CN118997712A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of shale oil and gas and tight oil and gas development, and in particular relates to a joint method of fracture creation and flow experiment of tight reservoir repeated fracturing core. Background Art
[0002] At present, the method for making re-fractured cores is mainly through mold filling, high-temperature firing, and high-pressure pressing: in the prior art, sand, clay, and aluminum phosphate are mixed together in a certain proportion, stirred evenly, and placed in a cylindrical or rectangular mold, and then a zinc sheet with a thickness that simulates the direction, shape, and width of the core crack is placed in the simulated position, and then a fractured core is formed by high-temperature firing and high-pressure pressing. The prior art also uses a similar process of sand mixing, mold filling, high-pressure pressing, heating and curing, cutting or coring. The production of the core is also separate from the flow experiment. The crack distribution obtained by re-fractured cores of this type is quite different from that of actual formation rocks, and it cannot be achieved for dense rocks such as shale, limestone, and dolomite. Therefore, it is urgent to propose a method for combining fracture creation and flow experiment of re-fractured cores in dense reservoirs. Summary of the invention
[0003] In order to solve the above technical problems, the present invention proposes a method for combining fracture creation and flow experiment of repeated fracturing cores in tight reservoirs. After one fracturing, the production capacity of tight reservoirs such as shale, limestone, and dolomite gradually decreases with the extension of production time during the production process, and then multiple repeated fracturing transformations are required to maintain a higher production capacity.
[0004] To achieve the above object, the present invention provides a method for combining fracture creation and flow experiment of repeated fracturing cores in tight reservoirs, comprising:
[0005] S1, obtaining the initial core;
[0006] S2, performing a first core fracturing experiment on the initial core to obtain a core wrapped in a heat shrink tube;
[0007] S3, performing the first fracturing and seaming core flow experiment on the core wrapped by the heat shrink tube;
[0008] S4, performing the first core solidification on the core after the first fracturing and fracture core flow experiment to obtain a cooled and solidified fracturing and fracture core;
[0009] S5, performing a secondary core fracturing and seaming experiment on the cooled and solidified core after fracturing and seaming, to obtain an experimental core solidified after secondary fracturing;
[0010] S6, conducting a secondary fracturing and seam-forming core flow experiment on the experimental core that has been solidified after the secondary fracturing, repeating S4 to S6, and sequentially conducting several core fracturing and seam-forming experiments and core flow experiments until the number of simulated fracturing times designed for the experiment is reached.
[0011] According to a method for combining fracture creation and flow experiment of a tight reservoir repeated fracturing core provided by the present invention, a method for obtaining an initial core includes:
[0012] A small cylindrical core of preset size is drilled from the core column for drilling sampling, and the end surface of the drilled core is polished and smoothed to obtain the initial core.
[0013] According to a method for combining fracture creation and flow experiment of a core of a tight reservoir repeatedly fractured by the present invention, a method for performing a first core fracture creation experiment on the initial core to obtain a core wrapped in a heat shrink tube comprises:
[0014] Step 1: Place the initial core into a heat shrink sleeve, use a hot air gun to blow the heat shrink tube from bottom to top, so that the heat shrink tube and the core are tightly wrapped, and then place it vertically on the pressure chamber base of the MTS tri-axial rock mechanics analyzer and place it in the center of the base;
[0015] Step 2: Install the external displacement sensor and the internal displacement sensor and adjust them to the appropriate position;
[0016] Step 3: Cover the top cover of the pressure chamber, seal the pressure chamber, open the first confining pressure pump and the confining pressure pump valve, fill the pressure chamber with confining pressure oil until the confining pressure reaches the formation pressure, then keep the confining pressure constant, and adjust the temperature control system of the pressure chamber until the temperature rises to the formation temperature and stabilizes for half an hour;
[0017] Step 4: start the axial pressure pump to apply axial pressure to the initial core at a certain loading rate;
[0018] Step 5: Closely observe the core stress-strain curve displayed in the display system. When the core stress-strain curve reaches the experimental requirements, turn off the first confining pressure pump, the axial pressure pump, and the temperature control system to naturally reduce the temperature to room temperature.
[0019] Step 6: Open the first confining pressure pump and the axial pressure pump, withdraw the pumps to release the pressure to the atmosphere, open the top cover of the pressure chamber, take out the core wrapped in the heat shrink tube, and complete the first core fracturing and seam making experiment.
[0020] According to a method for combining fracture creation and flow experiment of a core of a tight reservoir repeatedly fractured by the present invention, a method for conducting a first fracture creation core flow experiment on a core wrapped in a heat shrink tube comprises:
[0021] Place the core wrapped in the heat shrink tube into a rubber sleeve of preset size and into the core holder so that the two ends of the core holder fit tightly with the two end faces of the sealed core. Turn on the second confining pressure pump of the core holder, add confining pressure and adjust the back pressure at the outlet of the core holder according to the needs of the core flow experiment. Open the upper and lower valves of the first intermediate container filled with the experimental fluid and adjust the experimental temperature of the thermostat to carry out the core flow experiment.
[0022] According to a method for combining fracture creation and flow experiment of a repeatedly fractured core in a tight reservoir provided by the present invention, a method for performing a first core solidification on a core after a first fracture creation core flow experiment to obtain a cooled and solidified fractured core includes:
[0023] Step 1: After the core flow experiment is completed, the second confining pressure pump of the core holder and the valve at the outlet of the core holder are adjusted to the formation pressure, the upper and lower valves of the third intermediate container filled with petroleum ether and the displacement pump are opened, the pressure of the displacement pump is adjusted to be slightly higher than the pressure at the outlet of the core holder, and the valve at the inlet of the core holder is opened to allow petroleum ether to flow into the core for cleaning, until the fluid flowing out of the outlet of the core holder is consistent with the color of the fluid at the inlet of the core holder, and the core cleaning is completed; the upper and lower valves of the third intermediate container and the displacement pump are closed;
[0024] Step 2: Open the upper and lower valves of the second intermediate container filled with high-pressure nitrogen and the displacement pump, open the valve at the inlet end of the core holder, inject nitrogen into the core at a pressure higher than the formation pressure to purge the core until no liquid flows out of the outlet end, and close the upper and lower valves of the second intermediate container and the displacement pump;
[0025] Step 3, placing the hot melt resin in a fourth intermediate container and placing it in a constant temperature box, opening the upper and lower valves of the fourth intermediate container and the displacement pump, opening the valve at the inlet end of the core holder, and injecting the hot melt resin into the core at a pressure higher than the formation pressure until the hot melt resin is observed to flow out continuously in the conical bottle at the outlet end, and closing the valve at the inlet end of the core holder and the valve at the outlet end of the core holder when no gas is observed to be generated in the gas meter at the outlet end;
[0026] Step 4: turn off the temperature control system of the thermostatic box, allow the core holder to cool naturally to room temperature, slowly open the partitions at two sections of the core holder, and take out the cooled and solidified core after fracturing.
[0027] According to a method for combining fracture creation and flow experiment of a repeatedly fractured core of a tight reservoir provided by the present invention, a secondary core fracture creation experiment is performed on the cooled and solidified fractured core to obtain a solidified experimental core after secondary fracturing, comprising:
[0028] The cooled and solidified core after fracturing is placed in the pressure chamber of the MTS rock mechanical properties analyzer, and steps 3 to 6 in S2 are repeated to complete the secondary core fracturing experiment.
[0029] According to a method for combining fracture creation and flow experiment of a repeated fractured core of a tight reservoir provided by the present invention, a method for conducting a secondary fractured fractured core flow experiment on the experimental core solidified after the secondary fracturing comprises:
[0030] Step 1: Put the solidified experimental core after secondary fracturing into a rubber sleeve and into a core holder, so that the two ends of the core holder are tightly fitted with the two end cover plates of the sealed core, turn on the second confining pressure pump of the core holder, add confining pressure, and adjust the back pressure of the valve at the outlet end of the core holder according to the needs of the core flow experiment, and adjust the temperature of the thermostat to the formation temperature;
[0031] Step 2: Use petroleum ether to displace and clean the hot melt resin until the liquid color at the outlet of the core holder is consistent with that at the inlet of the core holder, and no liquefied hot melt resin flows out, until it is cleaned thoroughly, and then proceed to step 1 in S4;
[0032] Step 3: purge the core with high-pressure nitrogen and perform step 2 in S4;
[0033] Step 4: Open the upper and lower valves of the first intermediate container filled with the experimental fluid, adjust the experimental temperature, and carry out the secondary fracturing and fracture core flow experiment.
[0034] Technical effect of the invention: The invention discloses a method for combining fracture creation and flow experiment of repeated fracturing cores in tight reservoirs, which can better simulate the development and change process of reservoir fractures during repeated fracturing and better provide experimental cores for repeated fracturing core flow experiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] The drawings constituting a part of the present application are used to provide a further understanding of the present application. The illustrative embodiments and descriptions of the present application are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0036] Figure 1 Schematic diagram of a triaxial experiment according to an embodiment of the present invention, wherein 1 is an axial pressure pump; 2 is an external displacement sensor; 3 is a fixing fixture; 4 is an oil injection inlet; 5 is a device side plate; 6 is a pressure chamber partition; 7 is a device bottom plate; 8 is an internal displacement sensor; 9 is a core wrapped in a shrink tube; 10 is a pressure chamber base; 11 is a first confining pressure pump; 12 is a confining pressure pump valve; 13 is a display system; 14 is a pressure chamber top cover; 15 is a pressure chamber; 16 is a temperature control system;
[0037] Figure 2Schematic diagram of the core flow experiment equipment of the embodiment of the present invention, wherein 17 is a thermostatic box; 18 is a core holder; 19 is a rubber sleeve; 20 is a core after fracturing; 21 is a conical bottle; 22 is a gas meter; 23 is a displacement pump; 2401 is a valve at the upper end of the first intermediate container, 2402 is a valve at the lower end of the first intermediate container, 2403 is a valve at the upper end of the second intermediate container, 2404 is a valve at the lower end of the second intermediate container, 2405 is a valve at the upper end of the third intermediate container, 2406 is a valve at the lower end of the third intermediate container, 2407 is a valve at the upper end of the fourth intermediate container, 2408 is a valve at the lower end of the fourth intermediate container, 2501 is a first intermediate container; 2502 is a second intermediate container; 2503 is a third intermediate container; 2504 is a fourth intermediate container; 26 is a second confining pressure pump; 27 is a valve at the inlet end of the core holder; 28 is a valve at the outlet end of the core holder;
[0038] Figure 3 The present invention is a schematic flow chart of a method for combining fracture creation and flow experiment of a tight reservoir repeated fracturing core according to an embodiment of the present invention. DETAILED DESCRIPTION
[0039] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0040] It should be noted that the steps shown in the flowcharts of the accompanying drawings can be executed in a computer system such as a set of computer executable instructions, and that, although a logical order is shown in the flowcharts, in some cases, the steps shown or described can be executed in an order different from that shown here.
[0041] like Figure 3 As shown, this embodiment provides a method for combining fracture creation and flow experiment of repeated fracturing cores in a tight reservoir, comprising the following steps:
[0042] Step 1: Core Drilling and Cutting
[0043] A small cylindrical core with a diameter of 25 mm and a length of 50 to 100 mm is drilled from the core column for drilling sampling. The end face of the drilled core is cut and polished flat with a rock cutter, and the flatness is less than 0.002 mm.
[0044] Step 2: First core fracturing experiment Figure 1 Shown
[0045] (1) Place the core in a heat shrink tube and use a hot air gun to blow the heat shrink tube from bottom to top so that the heat shrink tube and the core are tightly wrapped. Then place it vertically on the pressure chamber base 10 of the MTS tri-axial rock mechanics analyzer and place it in the center of the base.
[0046] (2) Install the external displacement sensor 2 and the internal displacement sensor 8 and adjust them to the appropriate positions.
[0047] (3) Cover the pressure chamber top cover 14, seal the pressure chamber 15, open the first confining pressure pump 11 and the confining pressure pump valve 12, and fill the pressure chamber 15 with confining pressure oil until the confining pressure reaches the formation pressure. Then, keep the confining pressure constant and adjust the temperature control system 16 of the pressure chamber until the temperature reaches the formation temperature and stabilizes for half an hour.
[0048] (4) Start the axial pressure pump 1 to apply axial pressure to the core at a certain loading rate.
[0049] (5) Closely observe the stress-strain curve of the core displayed in the display system 13. When the stress-strain curve of the core reaches the experimental requirements, turn off the first confining pressure pump 11, the axial pressure pump 1, and the temperature control system 16 to allow the temperature to naturally drop to room temperature.
[0050] (6) The first confining pressure pump 11 and the axial pressure pump 1 are turned on, the pumps are withdrawn to release the pressure to the atmosphere, the pressure chamber top cover 14 is opened, and the core 9 wrapped in the heat shrink tube is taken out. The first core fracturing and seam-making experiment is completed.
[0051] Step 3: First fracturing core flow experiment
[0052] like Figure 2 As shown, the core 9 wrapped in the heat shrink tube is carefully placed in a rubber sleeve 19 with an inner diameter of 25 mm, and then placed in the core holder 18, so that the two ends of the core holder are tightly fitted with the two end faces of the sealed core, the second confining pressure pump 26 of the core holder is turned on to add confining pressure, and at the same time, the back pressure at the outlet of the core holder 18 is adjusted according to the needs of the core flow experiment, the upper and lower end valves 2401 and 2402 of the first intermediate container 2501 filled with experimental fluid (fluids such as crude oil, natural gas or formation water) are opened, the experimental temperature of the thermostat 17 is adjusted, and the core flow experiment is carried out.
[0053] Step 4: First Core Curing
[0054] (1) After the core flow experiment is completed, the confining pressure pump 26 of the core holder and the valve 28 at the core holder outlet are adjusted to the formation pressure, the upper and lower valves 2405 and 2406 of the third intermediate container 2503 filled with petroleum ether and the displacement pump 23 are opened, the pressure of the displacement pump 23 is adjusted to be slightly higher than the pressure at the core holder outlet, and the valve 27 at the core holder inlet is opened to allow petroleum ether to flow into the core for cleaning. When the color of the fluid flowing out of the core holder outlet is consistent with that of the fluid at the core holder inlet, the core cleaning is completed; then the upper and lower valves 2405 and 2406 of the third intermediate container 2503 and the displacement pump 23 are closed.
[0055] (2) Open the upper and lower valves 2403 and 2404 and the displacement pump 23 of the second intermediate container 2502 filled with high-pressure nitrogen, open the valve 27 at the inlet end of the core holder, and inject nitrogen into the core at a pressure slightly higher than the formation pressure to purge the core until no liquid flows out of the outlet end of the core holder. Then, close the upper and lower valves 2403 and 2404 and the displacement pump 23 of the second intermediate container 2502.
[0056] (3) Injecting hot-melt resin into the core: The hot-melt resin is placed in a fourth intermediate container 2504, and placed in a constant temperature box 17. The upper and lower valves 2407 and 2408 and the displacement pump 23 of the fourth intermediate container 2504 containing the hot-melt resin are opened. The valve 27 at the inlet end of the core holder is opened. The hot-melt resin is injected into the core at a pressure slightly higher than the formation pressure until the hot-melt resin is observed to continuously flow out of the conical bottle 21 at the outlet end of the core holder. When no gas is observed to be generated in the gas meter 22 at the outlet end of the core holder, the valve 27 at the inlet end of the core holder and the valve 28 at the outlet end of the core holder are closed.
[0057] (4) Cooling and solidifying the core: Turn off the temperature control system of the thermostat to allow the core holder 18 to cool naturally to room temperature, slowly open the partitions at the two sections of the core holder, and take out the cooled and solidified core 20 after fracturing.
[0058] Step 5: Secondary core fracturing and cracking experiment
[0059] The cooled and solidified core 20 after fracturing is placed in the pressure chamber of the MTS rock mechanical properties analyzer, and the second steps (3) to (6) are repeated to complete the secondary core fracturing experiment.
[0060] Step 6: Secondary fracturing and fracture core flow experiment
[0061] (1) The solidified experimental core after secondary fracturing is placed in a rubber sleeve 19 and then in a core holder 18, so that the two ends of the core holder 18 are tightly fitted with the two end cover plates of the sealed core. The second confining pressure pump 26 of the core holder 18 is turned on to increase the confining pressure. At the same time, the back pressure of the valve 28 at the outlet of the core holder is adjusted according to the needs of the core flow experiment, and the temperature of the thermostat 17 is adjusted to the formation temperature.
[0062] (2) Use petroleum ether to displace and clean the hot melt resin until the liquid color at the core holder outlet is consistent with that at the core holder inlet, and no liquefied hot melt resin flows out, ensuring that it is clean. Then proceed with step 4 (1).
[0063] (3) Purge the core with high-pressure nitrogen, and then proceed with step 4 (2).
[0064] (4) Open the upper and lower valves 2401 and 2402 of the first intermediate container 2501 filled with experimental fluid (fluid such as crude oil, natural gas or formation water), adjust the experimental temperature, and carry out the secondary fracturing and fracture core flow experiment.
[0065] Repeat steps 4 to 6, and carry out core fracturing and core flow experiments three, four, and so on, until the number of simulated fracturing times designed by the experiment is reached.
[0066] The above are only preferred specific implementations of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.
Claims
1. A method for combining fracture creation and flow experiment of repeated fracturing cores in tight reservoirs, characterized in that: include: S1, obtaining the initial core; S2, performing a first core fracturing experiment on the initial core to obtain a core wrapped in a heat shrink tube; S3, performing the first fracturing and seaming core flow experiment on the core wrapped by the heat shrink tube; S4, performing the first core solidification on the core after the first fracturing and fracture core flow experiment to obtain a cooled and solidified fracturing and fracture core; S5, performing a secondary core fracturing and seaming experiment on the cooled and solidified core after fracturing and seaming, to obtain an experimental core solidified after secondary fracturing; S6, conducting a secondary fracturing and seam-forming core flow experiment on the experimental core that has been solidified after the secondary fracturing, repeating S4 to S6, and sequentially conducting several core fracturing and seam-forming experiments and core flow experiments until the number of simulated fracturing times designed for the experiment is reached.
2. The method according to claim 1, characterized in that Methods for obtaining initial cores include: A small cylindrical core of preset size is drilled from the core column for drilling sampling, and the end surface of the drilled core is polished and smoothed to obtain the initial core.
3. The method according to claim 1, characterized in that The method of performing the first core fracturing experiment on the initial core to obtain the core wrapped in a heat shrink tube includes: Step 1: Place the initial core into a heat shrink sleeve, use a hot air gun to blow the heat shrink tube from bottom to top, so that the heat shrink tube and the core are tightly wrapped, and then place it vertically on the pressure chamber base (10) of the MTS tri-axial rock mechanics analyzer and place it in the center of the base; Step 2: Install the external displacement sensor (2) and the internal displacement sensor (8), and adjust them to appropriate positions; Step 3: Cover the pressure chamber top cover (14), seal the pressure chamber (15), open the first confining pressure pump (11) and the confining pressure pump valve (12), fill the pressure chamber (15) with confining pressure oil until the confining pressure reaches the formation pressure, then keep the confining pressure constant, and adjust the temperature control system (16) of the pressure chamber until the temperature reaches the formation temperature and stabilizes for half an hour; Step 4: starting the axial pressure pump (1) to apply axial pressure to the initial core at a certain loading rate; Step 5: closely observe the core stress-strain curve displayed in the display system (13); when the core stress-strain curve reaches the experimental requirements, turn off the first confining pressure pump (11), the axial pressure pump (1), and the temperature control system (16), and allow the temperature to naturally drop to room temperature; Step 6: Open the first confining pressure pump (11) and the axial pressure pump (1), withdraw the pump to release the pressure to the atmosphere, open the pressure chamber top cover (14), take out the core (9) wrapped in the heat shrink tube, and complete the first core fracturing and seam making experiment.
4. The method according to claim 1, characterized in that The method for conducting the first fracturing and seaming core flow experiment on the core wrapped by the heat shrink tube comprises: The core (9) wrapped in the heat shrink tube is placed in a rubber sleeve (19) of a preset size and then placed in a core holder (18) so that the two ends of the core holder are tightly fitted with the two end faces of the sealed core. The second confining pressure pump (26) of the core holder is turned on to increase the confining pressure and adjust the back pressure at the outlet of the core holder according to the needs of the core flow experiment. The upper and lower valves (2401) and (2402) of the first intermediate container (2501) filled with the experimental fluid are opened, and the experimental temperature of the thermostatic box (17) is adjusted to carry out the core flow experiment.
5. The method according to claim 1, characterized in that The method of performing the first core solidification on the core after the first fracturing and fracture core flow test to obtain the cooled and solidified fracturing and fracture core includes: Step 1: After the core flow experiment is completed, the second confining pressure pump (26) of the core holder and the valve (28) at the core holder outlet are adjusted to the formation pressure, the upper and lower valves (2405) and (2406) of the third intermediate container (2503) filled with petroleum ether and the displacement pump (23) are opened, the pressure of the displacement pump (23) is adjusted to be slightly higher than the pressure at the core holder outlet, the valve (27) at the core holder inlet is opened, and the petroleum ether is allowed to flow into the core for cleaning, until the fluid flowing out of the core holder outlet is consistent in color with the fluid at the core holder outlet, and the core cleaning is completed; the upper and lower valves (2405) and (2406) of the third intermediate container (2503) and the displacement pump (23) are closed; Step 2: Open the upper and lower valves (2403) and (2404) of the second intermediate container (2502) filled with high-pressure nitrogen and the displacement pump (23), open the valve (27) at the inlet end of the core holder, inject nitrogen into the core at a pressure higher than the formation pressure to purge the core until no liquid flows out of the outlet end, and close the upper and lower valves (2403) and (2404) of the second intermediate container (2502) and the displacement pump (23); Step 3: Place the hot melt resin in a fourth intermediate container (2504), and place it in a thermostatic box (17), open the upper and lower valves (2407) and (2408) of the fourth intermediate container (2504) and the displacement pump (23), open the valve (27) at the inlet end of the core holder, and inject the hot melt resin into the core at a pressure higher than the formation pressure until the hot melt resin is observed to flow out continuously in the conical bottle (21) at the outlet end, and close the valve (27) at the inlet end of the core holder and the valve (28) at the outlet end of the core holder when no gas is observed to be generated in the gas meter (22) at the outlet end; Step 4: turn off the temperature control system of the thermostatic box to allow the core holder (18) to cool naturally to room temperature, slowly open the partitions at two sections of the core holder (18), and take out the cooled and solidified fractured core (20).
6. The method according to claim 1, characterized in that The method of performing a secondary core fracturing and fracture-forming experiment on the cooled and solidified core after fracturing and fracture-forming to obtain a test core solidified after secondary fracturing includes: The cooled and solidified fractured core (20) is placed in the pressure chamber of the MTS rock mechanical property analyzer, and steps 3 to 6 in S2 are repeated to complete the secondary core fracture experiment.
7. The method according to claim 1, characterized in that The method for conducting a secondary fracturing core flow experiment on the experimental core solidified after the secondary fracturing comprises: Step 1: Place the solidified experimental core after secondary fracturing into a rubber sleeve (19) and into a core holder (18), so that both ends of the core holder (18) are tightly fitted with two end cover plates sealing the core, open the second confining pressure pump (26) of the core holder (18), add confining pressure and adjust the back pressure of the valve (28) at the outlet end of the core holder according to the needs of the core flow experiment, and adjust the temperature of the thermostat (17) to the formation temperature; Step 2: Use petroleum ether to displace and clean the hot melt resin until the liquid color at the outlet of the core holder is consistent with that at the inlet of the core holder, and no liquefied hot melt resin flows out, until it is cleaned thoroughly, and then proceed to step 1 in S4; Step 3: purge the core with high-pressure nitrogen and perform step 2 in S4; Step 4: Open the upper and lower valves (2401) and (2402) of the first intermediate container (2501) filled with the experimental fluid, adjust the experimental temperature, and carry out the secondary fracturing and fracture core flow experiment.