Ammonia gas supply device applied to NH3-SCR (Selective Catalytic Reduction) catalytic technology and use method thereof
By designing an ammonia supply device in NH3-SCR catalytic technology, using the urea catalytic layer to decompose ammonia and optimizing ammonia supply through the pneumatic three-way valve switching mechanism, the problem of urea crystallization and ammonia response time at low temperature is solved, and the response time of ammonia is improved NOx processing capability of diesel engines under low temperature conditions.
Patent Information
- Application Number
- CN202411149868.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-22
AI Technical Summary
Under low temperature conditions, diesel engines cannot effectively use NH3-SCR technology to process NOx, because urea injection at too low temperatures will crystallize on the catalyst surface, blocking the catalyst, resulting in a decrease in catalyst performance, and cannot provide enough NH3 during the cold start stage to use NOx reaction.
An ammonia supply device was designed, including a urea nozzle, a urea decomposition part, an ammonia storage part and an ammonia nozzle. The urea catalytic layer decomposes urea to generate ammonia, and the pneumatic three-way valve switching mechanism is used to accelerate the cold start stage. Ammonia gas response time, adjust the ammonia gas supply after the engine runs smoothly, ensuring sufficient ammonia gas supply on the catalyst surface.
It realizes independent decomposition of urea under low temperature conditions, avoids urea crystallization, improves the ammonia response speed, solves the problem of ammonia injection delay and overspraying in the cold start stage, and effectively alleviates NOx emissions under low temperature conditions.
Smart Images

Figure CN118997899A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of NH3-SCR catalytic technology, and in particular to an ammonia supply device applied to NH3-SCR catalytic technology and a use method thereof. Background Art
[0002] Diesel engines are widely used in non-passenger vehicles because they operate under lean-burn conditions and have excellent fuel economy. However, because they operate under lean-burn conditions, the fuel is burned efficiently and a large amount of thermal NO is generated. x It uses copper-based molecular sieve catalyst as the reaction medium and adopts NH3-SCR technology route. x The copper-based molecular sieve catalyst has excellent durability, selectivity and low-temperature performance, especially the latter. Under the catalysis of copper-based molecular sieve, NO x The actual reaction temperature with NH3 is low, at 150℃, NO x The conversion efficiency can be close to 70%, and NO x The conversion efficiency can reach more than 90%, as reported in the literature Fabrication of Cu-CHA composites with enhanced NH3-SCR catalytic performances and hydrothermal stabilities. Because urea injected at too low a temperature will crystallize on the catalyst surface, block and poison the catalyst, and reduce the efficiency of the catalyst, in actual applications, urea is injected only when the pre-SCR temperature is ≥180°C, and the exhaust gas temperature is used to decompose it into NH3, which reacts with NO under the action of the catalyst. Therefore, during the cold start stage, the NO generated by the engine x The inability to obtain the reducing agent NH3 to react with NO has become a difficult problem to solve in the entire emission cycle. In summary, ensuring the supply of NH3 under low temperature conditions is the key to improving the NO reduction of diesel engines under low temperature conditions. x One of the keys to processing power. Summary of the invention
[0003] The purpose of the present invention is to overcome and supplement the deficiencies in the prior art, and to provide an ammonia supply device and a method for using the ammonia supply device applied to NH3-SCR catalytic technology. The working mechanism of the entire component is that urea is sprayed from a nozzle, passes through a urea catalytic layer with a heating function, and urea is catalytically decomposed on the surface of the urea catalytic layer. At this time, the pneumatic three-way valve is switched to connect the urea decomposition part with the ammonia storage part, and the decomposed ammonia is adsorbed in the ammonia storage part until the adsorption is saturated; in the cold start stage, in order to speed up the response time, the ammonia storage part is directly heated and the ammonia is released and sprayed into the mixer through the ammonia nozzle to mix with the tail gas, and participate in the SCR reaction on the catalyst surface; after the engine runs smoothly, the urea sprayed through the urea nozzle is decomposed by the heated urea decomposition part, and the three-way valve is connected to the urea decomposition part and the ammonia nozzle, and the ammonia enters the mixer and mixes with the tail gas, and participates in the SCR reaction on the catalyst surface. During the operation, when the temperature of the ammonia storage part drops to room temperature, the three-way valve is switched to connect the urea decomposition part and the ammonia storage part, and the ammonia adsorption amount of the ammonia storage part is replenished in time.
[0004] The technical solution adopted by the present invention is: An ammonia supply device applied to NH3-SCR catalytic technology, comprising: a urea nozzle, a urea decomposition part, an ammonia storage part, an ammonia nozzle, and a mixer, wherein the urea nozzle is arranged at one end of the urea decomposition part, and the urea nozzle extends into the urea decomposition part to spray urea into the urea decomposition part, and the other end of the urea decomposition part is respectively connected to the ammonia storage part and the ammonia nozzle, and the ammonia storage part is also connected to the ammonia nozzle, and an SCR catalyst is arranged at the end of the mixer, and ammonia is mixed with tail gas and participates in the SCR reaction on the surface of the SCR catalyst.
[0005] Preferably, the ammonia supply device applied to NH3-SCR catalytic technology, wherein: a pneumatic three-way valve is arranged between the urea decomposition part and the ammonia storage part, the urea decomposition part is connected to the ammonia nozzle through the pneumatic three-way valve and the first pipeline in sequence, and the ammonia storage part is connected to the ammonia nozzle through the second pipeline.
[0006] Preferably, the ammonia supply device applied to NH3-SCR catalytic technology, wherein: the urea decomposition part includes a first honeycomb metal carrier, an anti-corrosion layer, and a urea catalyst layer arranged in sequence from bottom to top, and the material of the urea catalyst layer is selected from two or more composite oxides of aluminum oxide, zirconium oxide, titanium oxide, and iron oxide; the material of the anti-corrosion layer is selected from one of aluminum oxide, aluminum nitride, and silicon carbide.
[0007] Preferably, in the ammonia supply device applied to NH3-SCR catalytic technology, the loading amount of the urea catalytic layer is 80g / L-200g / L, and the loading amount of the anti-corrosion layer is 2g / L-10g / L.
[0008] Preferably, the ammonia supply device applied to NH3-SCR catalytic technology, wherein: the ammonia storage part includes a second honeycomb metal carrier, a heat conductive layer and an ammonia storage coating arranged in sequence from bottom to top, and the material of the heat conductive layer is selected from one of alumina, aluminum nitride, and silicon carbide; the material of the ammonia storage coating is selected from one or more material combinations of molecular sieves, Al2O3, SiO2, B2O3, Nb2O5, Al2O3-SiO2, Al2O3 / B2O3, kaolin, bentonite, and montmorillonite.
[0009] Preferably, in the ammonia supply device applied to NH3-SCR catalytic technology, the loading capacity of the ammonia storage coating is 100g / L-300g / L, and the loading capacity of the heat conductive layer is 2g / L-10g / L.
[0010] Preferably, in the ammonia supply device applied to NH3-SCR catalytic technology, the ammonia storage coating has the function of storing ammonia, and the ammonia storage capacity is 1mmol / g-10mmol / g coating.
[0011] Preferably, in the ammonia supply device applied to NH3-SCR catalytic technology, the number of NH3-TPD peaks of the ammonia storage coating is 1-3, wherein the adsorption amount of the first adsorption peak accounts for 30-100% of the total adsorption amount.
[0012] The present invention also provides a method for using an ammonia supply device applied to NH3-SCR catalytic technology, which comprises the following steps: Step S1. Urea is sprayed from the urea nozzle and passes through the urea decomposition unit with a heating function. The urea is catalytically decomposed on the surface of the urea catalyst layer. Then, the pneumatic three-way valve is switched to connect the urea decomposition unit with the ammonia storage unit. The ammonia decomposed in the urea decomposition unit is adsorbed in the ammonia storage unit until the adsorption is saturated. Step S2. During the cold start phase, the ammonia storage unit is heated and released to be injected into the mixer through the ammonia nozzle and mixed with the exhaust gas, and participates in the SCR reaction on the catalyst surface. After the engine runs smoothly, the urea injected through the urea nozzle is decomposed by the heated urea decomposition unit. At this time, the pneumatic three-way valve connects the urea decomposition unit and the ammonia nozzle, and the ammonia enters the mixer to mix with the exhaust gas and participates in the SCR reaction on the SCR catalyst surface.
[0013] Preferably, the method of use, wherein: in step S2, during operation, when the temperature of the ammonia storage part drops to room temperature, the pneumatic three-way valve is switched to connect the urea decomposition part and the ammonia storage part, so as to replenish the ammonia adsorption capacity of the ammonia storage part in time.
[0014] Advantages of the present invention: The ammonia supply device and the use method thereof applied to the NH3-SCR catalytic technology of the present invention can realize independent decomposition of urea, is not affected by the engine exhaust temperature, and can effectively solve the problem of urea decomposition and crystallization at low temperature; at the same time, by providing an ammonia storage part, it can effectively solve the response time problem of urea conversion to ammonia, solve the ammonia injection in the cold start stage, and solve the ammonia injection delay and overspray during the application process, and effectively alleviate the NOx in low temperature conditions. x Emission problem. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the structure of an ammonia supply device applied to NH3-SCR catalytic technology of the present invention.
[0016] Figure 2 It is a structural schematic diagram of the urea decomposition unit of the present invention.
[0017] Figure 3 It is a schematic structural diagram of the ammonia storage unit of the present invention.
[0018] Figure 4 The graph is a graph showing the change in ammonia storage capacity of the ammonia storage coating with temperature in Examples 1 and 2 of the present invention. DETAILED DESCRIPTION
[0019] The present invention will be further described below in conjunction with specific drawings and embodiments.
[0020] Example 1
[0021] like Figure 1-3 , an ammonia supply device applied to NH3-SCR catalytic technology, wherein: it includes a urea nozzle 1, a urea decomposition part 2, an ammonia storage part 3, an ammonia nozzle 5, and a mixer 6. The urea nozzle 1 is arranged at one end of the urea decomposition part 2, and the urea nozzle 1 extends into the urea decomposition part 2 to spray urea into the urea decomposition part 2. The other end of the urea decomposition part 2 is respectively connected to the ammonia storage part 3 and the ammonia nozzle 5, and the ammonia storage part 3 is also connected to the ammonia nozzle 5. The ammonia nozzle 5 extends into the mixer 6 to spray ammonia into the mixer 6. An SCR catalyst 7 is arranged at the end of the mixer 6. The ammonia is mixed with the exhaust gas and participates in the SCR reaction on the surface of the SCR catalyst 7.
[0022] A pneumatic three-way valve 4 is arranged between the urea decomposition part 2 and the ammonia storage part 3. The urea decomposition part 2 is connected to the ammonia nozzle 5 through the pneumatic three-way valve 4 and the first pipeline 8 in sequence, and the ammonia storage part 3 is connected to the ammonia nozzle 5 through the second pipeline 9; the urea decomposition part 2 includes a first honeycomb metal carrier 2-3, an anti-corrosion layer 2-2 and a urea catalytic layer 2-1 arranged in sequence from bottom to top; the ammonia storage part 3 includes a second honeycomb metal carrier 3-3, a heat conductive layer 3-2 and an ammonia storage coating 3-1 arranged in sequence from bottom to top; the first honeycomb metal carrier 2-3 and the second honeycomb metal carrier 3-3 are selected from a metal honeycomb carrier whose main material is FeCrAl, the mesh density is 300 mesh, and the outer dimensions are 190.5mm×190.5mm×101.6mm. The honeycomb carrier can heat the carrier to a maximum of 500°C under a 60V external power supply through the metal honeycomb carrier's own heating wire, thereby providing a heat source for urea decomposition or ammonia desorption in the ammonia storage part.
[0023] The material of the urea catalyst layer 2-1 is a composite oxide composed of titanium oxide and iron oxide in a mass ratio of 1:1; the material of the anti-corrosion layer 2-2 is silicon carbide.
[0024] The material of the ammonia storage coating 3-1 is FeBeta molecular sieve, and the material of the heat conductive layer 3-2 is aluminum nitride; The ammonia storage coating 3-1 has the function of storing ammonia, and the ammonia storage capacity is 2 mmol / g coating; the number of NH3-TPD peaks of the ammonia storage coating 3-1 is 2, among which the adsorption amount of the first adsorption peak accounts for 87.5% of the total adsorption amount.
[0025] The loading amount of the urea catalytic layer 2-1 is 150 g / L, and the loading amount of the anti-corrosion layer 2-2 is 2 g / L; the loading amount of the ammonia storage coating 3-1 is 250 g / L, and the loading amount of the thermal conductive layer 3-2 is 2 g / L.
[0026] The method for using the ammonia supply device applied to the NH3-SCR catalytic technology of Example 1 comprises the following steps: Step S1. Urea is sprayed from the urea nozzle 1 and passes through the urea decomposition unit 2 with a heating function. The urea is catalytically decomposed on the surface of the urea catalyst layer 2-1. Then, the pneumatic three-way valve 4 is switched to connect the urea decomposition unit 2 with the ammonia storage unit 3. The ammonia decomposed in the urea decomposition unit 2 is adsorbed in the ammonia storage unit 3 until the adsorption is saturated. Step S2. During the cold start phase, the ammonia storage unit 3 is heated and the released ammonia is sprayed into the mixer 6 through the ammonia nozzle 5 and mixed with the exhaust gas, and participates in the SCR reaction on the catalyst surface. After the engine runs smoothly, the urea sprayed through the urea nozzle 1 is decomposed by the heated urea decomposition unit 2. At this time, the pneumatic three-way valve 4 connects the urea decomposition unit 2 and the ammonia nozzle 5, and the ammonia enters the mixer 6 and mixes with the exhaust gas, and participates in the SCR reaction on the surface of the SCR catalyst 7; during the operation, when the temperature of the ammonia storage unit 3 drops to room temperature, the pneumatic three-way valve 4 is switched to connect the urea decomposition unit 2 and the ammonia storage unit 3, and the ammonia adsorption amount of the ammonia storage unit 3 is replenished in time.
[0027] Example 2
[0028] like Figure 1-3 , an ammonia supply device applied to NH3-SCR catalytic technology, wherein: it includes a urea nozzle 1, a urea decomposition part 2, an ammonia storage part 3, an ammonia nozzle 5, and a mixer 6. The urea nozzle 1 is arranged at one end of the urea decomposition part 2, and the urea nozzle 1 extends into the urea decomposition part 2 to spray urea into the urea decomposition part 2. The other end of the urea decomposition part 2 is respectively connected to the ammonia storage part 3 and the ammonia nozzle 5, and the ammonia storage part 3 is also connected to the ammonia nozzle 5. The ammonia nozzle 5 extends into the mixer 6 to spray ammonia into the mixer 6. An SCR catalyst 7 is arranged at the end of the mixer 6. The ammonia is mixed with the exhaust gas and participates in the SCR reaction on the surface of the SCR catalyst 7.
[0029] A pneumatic three-way valve 4 is arranged between the urea decomposition part 2 and the ammonia storage part 3 . The urea decomposition part 2 is connected to the ammonia nozzle 5 through the pneumatic three-way valve 4 and the first pipeline 8 in sequence. The ammonia storage part 3 is connected to the ammonia nozzle 5 through the second pipeline 9 .
[0030] The urea decomposition unit 2 includes a first honeycomb metal carrier 2-3, an anti-corrosion layer 2-2 and a urea catalyst layer 2-1 which are arranged in sequence from bottom to top, that is, the anti-corrosion layer material alumina is coated on the first honeycomb metal carrier 2-3 at a loading amount of 2g / L, and then a composite oxide with a titanium-zirconium mass ratio of 1:1 is coated on the anti-corrosion layer 2-2 at a loading amount of 100g / L.
[0031] The ammonia storage part 3 includes a second honeycomb metal carrier 3-3, a thermal conductive layer 3-2 and an ammonia storage coating 3-1 which are arranged in sequence from bottom to top, that is, the thermal conductive layer material silicon carbide is coated on the second honeycomb metal carrier 3-3 at a loading amount of 2g / L, and then the ammonia storage material which is a combination of FeBeta molecular sieve and Al2O3-SiO2 in a weight ratio of 3:1 is coated on the thermal conductive layer 3-2 at a loading amount of 200g / L.
[0032] The first honeycomb metal carrier 2-3 and the second honeycomb metal carrier 3-3 are made of FeCrAl as the main material, with a mesh density of 300 mesh and an outer size of 190.5mm×190.5mm×101.6mm. The honeycomb carrier can heat the carrier to a maximum of 500°C under a 60V external power supply through the metal honeycomb carrier's own heating wire, thereby providing a heat source for urea decomposition or ammonia desorption in the ammonia storage part.
[0033] The method for using the ammonia supply device applied to the NH3-SCR catalytic technology of Example 2 comprises the following steps: Step S1. Urea is sprayed from the urea nozzle 1 and passes through the urea decomposition unit 2 with a heating function. The urea is catalytically decomposed on the surface of the urea catalyst layer 2-1. Then, the pneumatic three-way valve 4 is switched to connect the urea decomposition unit 2 with the ammonia storage unit 3. The ammonia decomposed in the urea decomposition unit 2 is adsorbed in the ammonia storage unit 3 until the adsorption is saturated. Step S2. During the cold start phase, the ammonia storage unit 3 is heated and the released ammonia is sprayed into the mixer 6 through the ammonia nozzle 5 and mixed with the exhaust gas, and participates in the SCR reaction on the catalyst surface. After the engine runs smoothly, the urea sprayed through the urea nozzle 1 is decomposed by the heated urea decomposition unit 2. At this time, the pneumatic three-way valve 4 connects the urea decomposition unit 2 and the ammonia nozzle 5, and the ammonia enters the mixer 6 and mixes with the exhaust gas, and participates in the SCR reaction on the surface of the SCR catalyst 7; during the operation, when the temperature of the ammonia storage unit 3 drops to room temperature, the pneumatic three-way valve 4 is switched to connect the urea decomposition unit 2 and the ammonia storage unit 3, and the ammonia adsorption amount of the ammonia storage unit 3 is replenished in time.
[0034] Figure 4 The ammonia adsorption diagrams of the ammonia storage coatings of Examples 1 and 2 show that Example 1 has two ammonia storage peaks, which are located at 217°C and 410°C respectively, and the peak area at 217°C accounts for 87.5% of the total peak area, that is, the ammonia adsorption amount of the first peak accounts for 87.5% of the total adsorption amount; while Example 2 has a single adsorption peak, the peak position is located at 208°C, and the ammonia adsorption amount of the first peak is 100%.
[0035] In summary, by setting up an ammonia storage unit, the response time problem of urea conversion to ammonia can be effectively solved, the ammonia injection in the cold start phase, and the ammonia injection delay and overspray during the application process can be solved, and the NO x Emission problem.
[0036] Finally, it should be noted that the above specific implementation methods are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to examples, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.
Claims
1. An ammonia supply device applied to NH3-SCR catalytic technology, characterized by: The invention comprises a urea nozzle (1), a urea decomposition part (2), an ammonia storage part (3), an ammonia nozzle (5), and a mixer (6). The urea nozzle (1) is arranged at one end of the urea decomposition part (2). The urea nozzle (1) extends into the urea decomposition part (2) to spray urea into the urea decomposition part (2). The other end of the urea decomposition part (2) is respectively connected to the ammonia storage part (3) and the ammonia nozzle (5). The ammonia storage part (3) is connected to the ammonia nozzle (5). The ammonia nozzle (5) extends into the mixer (6) to spray ammonia into the mixer (6). An SCR catalyst (7) is arranged at the end of the mixer (6). The ammonia is mixed with the exhaust gas and participates in the SCR reaction under the action of the SCR catalyst (7).
2. The ammonia supply device applied to NH3-SCR catalytic technology according to claim 1 is characterized in that: A pneumatic three-way valve (4) is arranged between the urea decomposition section (2) and the ammonia storage section (3); the urea decomposition section (2) is connected to the ammonia nozzle (5) via the pneumatic three-way valve (4) and the first pipeline (8) in sequence; and the ammonia storage section (3) is connected to the ammonia nozzle (5) via the second pipeline (9).
3. The ammonia supply device applied to NH3-SCR catalytic technology according to claim 1 is characterized in that: The urea decomposition part (2) comprises a first honeycomb metal carrier (2-3), an anti-corrosion layer (2-2), and a urea catalyst layer (2-1) which are arranged in sequence from bottom to top. The material of the urea catalyst layer (2-1) is selected from two or more composite oxides of aluminum oxide, zirconium oxide, titanium oxide, and iron oxide; the material of the anti-corrosion layer (2-2) is selected from one of aluminum oxide, aluminum nitride, and silicon carbide.
4. The ammonia supply device applied to NH3-SCR catalytic technology according to claim 3 is characterized in that: The loading amount of the urea catalyst layer (2-1) is 80 g / L-200 g / L, and the loading amount of the anti-corrosion layer (2-2) is 2 g / L-10 g / L.
5. The ammonia supply device applied to NH3-SCR catalytic technology according to claim 1 is characterized in that: The ammonia storage part (3) comprises a second honeycomb metal carrier (3-3), a heat conductive layer (3-2) and an ammonia storage coating (3-1) which are arranged in sequence from bottom to top, wherein the material of the heat conductive layer (3-2) is selected from one of aluminum oxide, aluminum nitride and silicon carbide; the material of the ammonia storage coating (3-1) is selected from one of a molecular sieve, Al2O3, SiO2, B2O3, Nb2O5, Al2O3-SiO2, Al2O3 / B2O3, kaolin, bentonite and montmorillonite.
6. The ammonia supply device applied to NH3-SCR catalytic technology according to claim 5 is characterized in that: The loading amount of the ammonia storage coating (3-1) is 100g / L-300g / L, and the loading amount of the heat conductive layer (3-2) is 2g / L-10g / L.
7. The ammonia supply device applied to NH3-SCR catalytic technology according to claim 5 is characterized in that: The ammonia storage coating (3-1) has the function of storing ammonia, and the storage amount of ammonia is 1mmol / g-10mmol / g coating.
8. The ammonia supply device applied to NH3-SCR catalytic technology according to claim 5 is characterized in that: The number of NH3-TPD peaks of the ammonia storage coating (3-1) is 1-3, wherein the adsorption amount of the first adsorption peak accounts for 30-100% of the total adsorption amount.
9. The method for using the ammonia supply device applied to NH3-SCR catalytic technology according to any one of claims 1 to 8, characterized in that: The following steps are involved: Step S1. Urea is sprayed from a urea nozzle (1) and passes through a urea decomposition unit (2) having a heating function. The urea is catalytically decomposed on the surface of a urea catalytic layer (2-1). Subsequently, a pneumatic three-way valve (4) is switched to connect the urea decomposition unit (2) with the ammonia storage unit (3). The ammonia decomposed in the urea decomposition unit (2) is adsorbed in the ammonia storage unit (3) until adsorption is saturated. Step S2. During the cold start phase, the ammonia storage unit (3) is heated and released to be injected into the mixer (6) through the ammonia nozzle (5) and mixed with the exhaust gas to participate in the SCR reaction on the catalyst surface. After the engine runs smoothly, the urea injected through the urea nozzle (1) is decomposed by the heated urea decomposition unit (2). At this time, the pneumatic three-way valve (4) connects the urea decomposition unit (2) and the ammonia nozzle (5), and the ammonia enters the mixer (6) to mix with the exhaust gas and participate in the SCR reaction on the surface of the SCR catalyst (7).
10. The method of use according to claim 9, characterized in that: In step S2, during the operation, when the temperature of the ammonia storage part (3) drops to room temperature, the pneumatic three-way valve (4) is switched to connect the urea decomposition part (2) and the ammonia storage part (3), so as to replenish the ammonia adsorption amount of the ammonia storage part (3) in time.