Local mismatch model of WPE effect and extraction method thereof

By forming device structures with different well sizes on the wafer and measuring the mismatch rate, a local mismatch model was established, which solved the problem of failure to consider the mismatch characteristics of the well size to the device in the prior art, and achieved the WPE effect Accurate characterization and better reflection of device performance.

CN119008441AInactive Publication Date: 2024-11-22SHANGHAI HUALI INTEGRATED CIRCUIT CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411018124.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing SPICE model fails to effectively consider the impact of different well sizes on device mismatch characteristics, especially when the well edge is close to the channel region, the resulting WPE effect is not fully explained.

Method used

By forming device structures with different well sizes on the wafer, measuring and calculating the mismatch rate of each parameter, establishing a local mismatch model related to the well size, and adjusting the model parameters through curve fitting to make them match the measurement data If appropriate, a local mismatch model of WPE effect is formed.

Benefits of technology

Effectively characterizing the impact of different well sizes on device mismatch performance provides a basis for considering the actual characteristics of the device during design, and improves the accuracy and reliability of the design.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008441A_ABST
    Figure CN119008441A_ABST
Patent Text Reader

Abstract

The invention provides a method for extracting a local mismatch model of a WPE effect. The method comprises the following steps: forming device structures with different well sizes in a wafer; values of parameters of adjacent device structures in the same bare chip are measured and obtained, and the parameters comprise linear threshold voltage, saturation threshold voltage, linear current and saturation current; calculating the mismatch rate of each parameter; establishing a local mismatch model related to the well size; and performing curve fitting on the parameters of the local mismatch model until the fitting result is consistent with the mismatch rate of each parameter of the device structure. According to the invention, the problem that the existing model does not consider the influence of different well sizes on the mismatch characteristic of the device is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductor manufacturing, and in particular to a local mismatch model of WPE effect and an extraction method thereof. Background Art

[0002] In the field of chip manufacturing technology, the use of wells can significantly improve the technical performance of complementary metal oxide semiconductors (CMOS). Through the use of high-energy ion implantation and the optimization of heat treatment processes, the heavy doping of the well region can hardly affect the doping morphology of the MOS tube surface, thereby greatly reducing the impact of well doping on the surface device area. More importantly, deep well ion implantation has many advantages, such as providing a low-resistance path for the device and suppressing parasitic bipolar transistors and improving the noise isolation performance of the device. Therefore, well technology has been widely used and promoted in integrated circuit manufacturing. However, when the size of the well is small and the edge of the well is closer to the channel area, some ions in the deep well doping process will be scattered to the surface device area, modulating the threshold voltage and current of the device to a certain extent. This phenomenon is called the well proximity effect (WPE).

[0003] Currently, the SPICE model is able to take into account the impact of channel size (channel width W and channel length L) on device electrical mismatch, but fails to consider the mismatch caused by differences in device layout environments when the channel sizes are exactly the same. Summary of the invention

[0004] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a local mismatch model of WPE effect and an extraction method thereof, so as to solve the problem that the existing model does not consider the influence of different well sizes on the mismatch characteristics of the device.

[0005] To achieve the above object and other related objects, the present invention provides a method for extracting a local mismatch model of a WPE effect, the method comprising:

[0006] Forming device structures with different well sizes in a wafer, wherein the wafer includes a plurality of bare chips, and the device structure is formed with a gate, a drain terminal and a well;

[0007] For a plurality of the bare chips, the values ​​of the parameters of the adjacent device structures in the same bare chip are measured and obtained, wherein the parameters include a linear threshold voltage, a saturation threshold voltage, a linear current and a saturation current, and the linear threshold voltage is the gate voltage when the drain terminal reaches a specific current value when a first voltage is applied to the drain terminal, the saturation threshold voltage is the gate voltage when the drain terminal reaches the specific current value when a second voltage is applied to the drain terminal, the linear current is the drain terminal current when the second voltage is applied to the gate and the first voltage is applied to the drain terminal, and the saturation current is the drain terminal current when the second voltage is applied to both the gate and the drain terminal;

[0008] Calculate the mismatch rate of each parameter;

[0009] Establish a local mismatch model related to well size;

[0010] Performing curve fitting on the parameters of the local mismatch model until the fitting result is consistent with the mismatch rate of each parameter of the device structure;

[0011] Wherein, the channel length and the channel width of each of the device structures are the same, and the first voltage is less than the second voltage.

[0012] Optionally, the wafer includes N bare chips, and two adjacent device structures are selected from the same bare chip, wherein N is a positive integer greater than or equal to 2.

[0013] Optionally, the method for calculating the mismatch rate of the linear threshold voltage includes:

[0014] Subtracting two linear threshold voltages in the same die to obtain a first difference, and obtaining N first differences;

[0015] The standard deviation of the N first differences is calculated to obtain the mismatch rate of the linear threshold voltage.

[0016] Optionally, the method for calculating the mismatch rate of the saturation threshold voltage includes:

[0017] Subtracting two saturation threshold voltages in the same die to obtain a second difference, and obtaining N second difference values;

[0018] The standard deviation of the N second differences is calculated to obtain the mismatch rate of the saturation threshold voltage.

[0019] Optionally, the method for calculating the mismatch rate of the linear current includes:

[0020] Subtracting two linear currents in the same die and dividing the result by an average of the two linear currents to obtain a first ratio, and obtaining N first ratios;

[0021] The standard deviation of the N first ratios is calculated to obtain the mismatch rate of the linear current.

[0022] Optionally, the method for calculating the mismatch rate of the saturation current includes:

[0023] Subtracting two saturation currents in the same die and dividing the result by an average of the two saturation currents to obtain a second ratio, and obtaining N second ratios;

[0024] A standard deviation is calculated for the N second ratios to obtain a mismatch rate of the saturation current.

[0025] Optionally, the specific current value is 1E-8*W / L amperes, wherein W represents a channel width of the device structure, and L represents a channel length of the device structure.

[0026] Optionally, the functional relationship of the local mismatch model is as follows:

[0027]

[0028] Among them, γ, α, A, B, b, C, c are coefficients, W and L represent the channel width and channel length of the device structure respectively, SC is the distance from the channel edge to the well edge, and pwr() is a power function.

[0029] Optionally, a value range of the first voltage includes 0.04V to 0.06V.

[0030] Optionally, a value range of the second voltage includes 4V to 6V.

[0031] Optionally, before calculating the mismatch rate of each parameter, the method further includes a step of screening and removing unreasonable values ​​of each parameter obtained.

[0032] Optionally, the method further comprises the step of verifying the established local failure model.

[0033] Accordingly, the present invention also provides a local mismatch model of the WPE effect, the formula of the model includes:

[0034]

[0035] Among them, γ, α, A, B, b, C, c are coefficients, W and L represent the channel width and channel length of the device structure respectively, SC is the distance from the channel edge to the well edge, and pwr() is a power function.

[0036] As described above, the local mismatch model of the WPE effect of the present invention and the extraction method thereof, in order to characterize the influence of different well sizes on the mismatch performance of its device, firstly design a layout related thereto, and the designed layout includes a device structure with different well sizes, then obtain a wafer according to the designed layout, and measure the electrical performance of the wafer, analyze, screen and calculate the measurement data, and calculate the mismatch rate of each parameter, and then adjust the coefficient of the local mismatch model formula of the WPE effect so that the mismatch model fits well with the mismatch rate obtained by measurement and calculation, so that the local mismatch model of the WPE effect with different well sizes can be obtained, and the designer can understand the mismatch of the device under different well sizes by simulating the model, so as to take this factor into consideration when starting the design, so that the final design result can better reflect the actual device characteristics. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 Shown is a flow chart of the local mismatch model extraction method of the WPE effect of the present invention.

[0038] Figure 2 Shown is a schematic diagram of the well size SC of the present invention. DETAILED DESCRIPTION

[0039] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0040] See also Figure 1 to Figure 2 It should be noted that the illustrations provided in this embodiment are only schematic illustrations of the basic concept of the present invention. Although the illustrations only show components related to the present invention and are not drawn according to the number, shape and size of components in actual implementation, the form, quantity and proportion of each component in actual implementation may be changed arbitrarily, and the component layout may also be more complicated.

[0041] like Figure 1 As shown, this embodiment provides a method for extracting a local mismatch model of a WPE effect, the method comprising:

[0042] A device structure with different well sizes is formed in a wafer, wherein the wafer includes a plurality of bare chips, and the device structure is formed with a gate, a drain terminal and a well;

[0043] For the plurality of bare chips, the values ​​of the parameters of the adjacent device structures in the same bare chip are measured and obtained, wherein the parameters include a linear threshold voltage Vtlin, a saturation threshold voltage Vtsat, a linear current Idlin, and a saturation current Idsat, and the linear threshold voltage Vtlin is the gate voltage when the drain terminal reaches a specific current value when a first voltage is applied to the drain terminal, the saturation threshold voltage Vtsat is the gate voltage when the drain terminal reaches the specific current value when a second voltage is applied to the drain terminal, the linear current Idlin is the drain terminal current when the second voltage is applied to the gate and the first voltage is applied to the drain terminal, and the saturation current Idsat is the drain terminal current when the second voltage is applied to both the gate and the drain terminal;

[0044] Calculate the mismatch rate of each parameter;

[0045] Establish a local mismatch model related to well size;

[0046] Performing curve fitting on the parameters of the local mismatch model until the fitting result is consistent with the mismatch rate of each parameter of the device structure;

[0047] Wherein, the channel length and the channel width of each of the device structures are the same, and the first voltage is less than the second voltage.

[0048] Specifically, the value range of the first voltage includes 0.04V to 0.06V. In this embodiment, the value of the first voltage is 0.05V.

[0049] Specifically, the value range of the second voltage includes 4V to 6V. In this embodiment, the value of the second voltage is 5V.

[0050] Specifically, the wafer includes N bare chips, and two adjacent device structures are selected from the same bare chip, wherein N is a positive integer greater than or equal to 2.

[0051] More specifically, the method for calculating the mismatch rate of the linear threshold voltage includes:

[0052] Subtracting two linear threshold voltages in the same die to obtain a first difference, and obtaining N first differences;

[0053] The standard deviation of the N first differences is calculated to obtain the mismatch rate of the linear threshold voltage.

[0054] More specifically, the method for calculating the mismatch rate of the saturation threshold voltage includes:

[0055] Subtracting two saturation threshold voltages in the same die to obtain a second difference, and obtaining N second difference values;

[0056] The standard deviation of the N second differences is calculated to obtain the mismatch rate of the saturation threshold voltage.

[0057] More specifically, the method for calculating the mismatch rate of the linear current includes:

[0058] Subtracting two linear currents in the same die and dividing the result by an average of the two linear currents to obtain a first ratio, and obtaining N first ratios;

[0059] The standard deviation of the N first ratios is calculated to obtain the mismatch rate of the linear current.

[0060] More specifically, the method for calculating the mismatch rate of the saturation current includes:

[0061] Subtracting two saturation currents in the same die and dividing the result by an average of the two saturation currents to obtain a second ratio, and obtaining N second ratios;

[0062] A standard deviation is calculated for the N second ratios to obtain a mismatch rate of the saturation current.

[0063] Specifically, the specific current value is 1E-8*W / L amperes, wherein W represents the channel width of the device structure, and L represents the channel length of the device structure.

[0064] Specifically, the functional relationship of the local mismatch model is as follows:

[0065]

[0066] Among them, γ, α, A, B, b, C, c are coefficients, W and L represent the channel width and channel length of the device structure respectively, SC is the distance from the channel edge to the well edge, and pwr() is a power function.

[0067] In this embodiment, Figure 2 A schematic diagram of the well size SC is shown.

[0068] Specifically, before calculating the mismatch rate of each parameter, the method further includes the step of screening and removing the acquired unreasonable values ​​of each parameter.

[0069] In this embodiment, when unreasonable values ​​of various parameters are screened and removed, values ​​belonging to the 3σ normal distribution are reasonable values.

[0070] Specifically, the method further includes a step of verifying the established local failure model.

[0071] Accordingly, this embodiment further provides a local mismatch model of the WPE effect, and the formula of the model includes:

[0072]

[0073] Among them, γ, α, A, B, b, C, c are coefficients, W and L are the channel width and channel length of the device structure respectively, SC is the distance from the channel edge to the well edge, and pwr() is a power function.

[0074] In summary, the local mismatch model of the WPE effect of the present invention and the extraction method thereof, in order to characterize the influence of different well sizes on the mismatch performance of its device, firstly, a layout related thereto is designed, and the designed layout includes a device structure with different well sizes, and then a wafer is obtained according to the designed layout, and the electrical performance of the wafer is measured, and the measurement data is analyzed, screened and calculated, and the mismatch rate of each parameter is calculated, and then the coefficient of the local mismatch model formula of the WPE effect is adjusted so that the mismatch model fits the mismatch rate obtained by the measurement calculation well, so that the local mismatch model of the WPE effect of different well sizes can be obtained, and the designer can understand the mismatch of the device under different well sizes by simulating the model, so as to take this factor into consideration when starting the design, so that the final design result can better reflect the actual device characteristics. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.

[0075] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for extracting the local mismatch model of the WPE effect, It is characterized in that The method comprises: Forming device structures with different well sizes in a wafer, wherein the wafer includes a plurality of bare chips, and the device structure is formed with a gate, a drain terminal and a well; For a plurality of the bare chips, the values ​​of the parameters of the adjacent device structures in the same bare chip are measured and obtained, wherein the parameters include a linear threshold voltage, a saturation threshold voltage, a linear current and a saturation current, and the linear threshold voltage is the gate voltage when the drain terminal reaches a specific current value when a first voltage is applied to the drain terminal, the saturation threshold voltage is the gate voltage when the drain terminal reaches the specific current value when a second voltage is applied to the drain terminal, the linear current is the drain terminal current when the second voltage is applied to the gate and the first voltage is applied to the drain terminal, and the saturation current is the drain terminal current when the second voltage is applied to both the gate and the drain terminal; Calculate the mismatch rate of each parameter; Establish a local mismatch model related to well size; Performing curve fitting on the parameters of the local mismatch model until the fitting result is consistent with the mismatch rate of each parameter of the device structure; Wherein, the channel length and the channel width of each of the device structures are the same, and the first voltage is less than the second voltage.

2. The method for extracting the local mismatch model of the WPE effect according to claim 1, It is characterized in that The wafer includes N dies, and two adjacent device structures are selected from the same die, wherein N is a positive integer greater than or equal to 2.

3. The method for extracting the local mismatch model of the WPE effect according to claim 2, It is characterized in that The method for calculating the mismatch rate of the linear threshold voltage includes: Subtracting two linear threshold voltages in the same die to obtain a first difference, and obtaining N first differences; The standard deviation of the N first differences is calculated to obtain the mismatch rate of the linear threshold voltage.

4. The method for extracting the local mismatch model of the WPE effect according to claim 2, It is characterized in that The method for calculating the mismatch rate of the saturation threshold voltage includes: Subtracting two saturation threshold voltages in the same die to obtain a second difference, and obtaining N second difference values; The standard deviation of the N second differences is calculated to obtain the mismatch rate of the saturation threshold voltage.

5. The method for extracting the local mismatch model of the WPE effect according to claim 2, It is characterized in that The method for calculating the mismatch rate of the linear current includes: Subtracting two linear currents in the same die and dividing the result by an average of the two linear currents to obtain a first ratio, and obtaining N first ratios; The standard deviation of the N first ratios is calculated to obtain the mismatch rate of the linear current.

6. The method for extracting the local mismatch model of the WPE effect according to claim 2, It is characterized in that The method for calculating the mismatch rate of the saturation current includes: Subtracting two saturation currents in the same die and dividing the result by an average of the two saturation currents to obtain a second ratio, and obtaining N second ratios; A standard deviation is calculated for the N second ratios to obtain a mismatch rate of the saturation current.

7. The method for extracting the local mismatch model of the WPE effect according to claim 1, It is characterized in that The specific current value is 1E-8*W / L amperes, wherein W represents the channel width of the device structure, and L represents the channel length of the device structure.

8. The method for extracting the local mismatch model of the WPE effect according to claim 1, It is characterized in that The functional relationship of the local mismatch model is as follows: Among them, γ, α, A, B, b, C, c are coefficients, W and L represent the channel width and channel length of the device structure respectively, SC is the distance from the channel edge to the well edge, and pwr() is a power function.

9. The method for extracting the local mismatch model of the WPE effect according to claim 1, It is characterized in that The value range of the first voltage includes 0.04V to 0.06V.

10. The method for extracting the local mismatch model of the WPE effect according to claim 1 or 3, It is characterized in that The second voltage has a value range of 4V to 6V.

11. The method for extracting the local mismatch model of the WPE effect according to claim 1, It is characterized in that Before calculating the mismatch rate of each parameter, the method further includes the step of screening and removing the unreasonable values ​​of each parameter obtained.

12. The method for extracting the local mismatch model of the WPE effect according to claim 1, It is characterized in that The method further comprises the step of verifying the established local failure model.

13. A local mismatch model of WPE effect, It is characterized in that The formula for the model includes: Among them, γ, α, A, B, b, C, c are coefficients, W and L represent the channel width and channel length of the device structure respectively, SC is the distance from the channel edge to the well edge, and pwr() is a power function.

Citation Information

Patent Citations

  • Flicker noise model of semiconductor device, and extraction method for flicker noise model

    CN108763830A

  • General WPE (Well edge-Proximity Effect) optimizing model and extracting method thereof

    CN108875200A

  • Modeling method and device for mismatch model of semiconductor device

    CN114880987A

  • Substrate current model based on well proximity effect and extraction method thereof

    CN116562198A