Manufacturing method of semiconductor structure

By depositing and annealing the multi-layer contact layer in the trench of the semiconductor structure, the problems of hollows and surface roughness increase after the size of the semiconductor structure are reduced, the gaps and holes are reduced, and the manufacturing effect of the semiconductor structure is improved.

CN119008516APending Publication Date: 2024-11-22NAN YA TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311047434.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-17
Filing Date
2023-08-18
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the manufacturing process of semiconductor structures, as the structural size decreases, the manufacturing process faces problems of hollows and increased surface roughness, which affects yield and performance.

Method used

By forming trenches between bit lines, seed layer and multi-layer contact layer are deposited, and dopants are diffused during an annealing process, a contact plug with a uniform doping concentration is formed, reducing the number of gaps and holes.

Benefits of technology

The reduction of the gap size and number of holes in the contact plug is achieved, and the yield and performance of the semiconductor structure is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008516A_ABST
    Figure CN119008516A_ABST
Patent Text Reader

Abstract

A method of manufacturing a semiconductor structure includes forming a trench between bit lines, depositing a seed layer in the trench, depositing a first contact layer on the seed layer in the trench, depositing a second contact layer on the first contact layer to fill the trench, wherein the second doping concentration of the second contact layer is lower than the first doping concentration of the first contact layer. An annealing process is performed on the first contact layer and the second contact layer such that the dopant in the first contact layer diffuses into the second contact layer to form a contact plug including the first contact layer and the second contact layer. The second contact layer has a lower second doping concentration when deposited, so that the second contact layer may have a lower surface roughness than the first contact layer, thereby reducing the slot size and void count in the contact plug.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a method for manufacturing a semiconductor structure, and more particularly to a method for manufacturing a contact plug of a semiconductor structure. Background Art

[0002] As semiconductor technology advances, the size of semiconductor structures shrinks, resulting in an increased degree of integration of semiconductor devices. In this case, the critical dimensions of semiconductor structures also decrease, allowing the structure of electronic products to be more compact. However, as the critical dimensions of semiconductor structures decrease, the processing technology for manufacturing semiconductor structures also faces many challenges. For example, smaller semiconductor structures require fewer voids to achieve the expected yield and performance. Summary of the invention

[0003] According to an embodiment of the present disclosure, a method for manufacturing a semiconductor structure is provided, comprising forming a trench between bit lines, depositing a seed layer in the trench, and depositing a first contact layer on the seed layer in the trench. The method further comprises depositing a second contact layer on the first contact layer to fill the trench, wherein the second doping concentration of the second contact layer is lower than the first doping concentration of the first contact layer. The method further comprises performing an annealing process on the first contact layer and the second contact layer so that the dopant in the first contact layer diffuses into the second contact layer to form a contact plug comprising the first contact layer and the second contact layer.

[0004] In some embodiments, a first doping concentration of the first contact layer before the annealing process is performed is higher than a doping concentration of the contact plug after the annealing process is performed.

[0005] In some embodiments, the seed layer is undoped before the annealing process is performed.

[0006] In some embodiments, after performing the annealing process, dopants in the first contact layer diffuse into the seed layer to form a contact plug including the seed layer.

[0007] In some embodiments, the seed layer, the first contact layer, and the second contact layer have uniform doping concentrations after performing an annealing process.

[0008] In some embodiments, a thickness of the first contact layer is greater than a thickness of the seed layer, and a thickness of the second contact layer is greater than a thickness of the first contact layer.

[0009] In some embodiments, a ratio of a thickness of the second contact layer to a thickness of the first contact layer is in a range of 1.3 to 3.1.

[0010] In some embodiments, the seed layer, the first contact layer, and the second contact layer are formed of the same polysilicon material.

[0011] In some embodiments, the manufacturing method further includes depositing a capping layer on the second contact layer after depositing the second contact layer and before performing the annealing process. The third doping concentration of the capping layer is lower than the second doping concentration of the second contact layer.

[0012] In some embodiments, the second contact layer includes a recessed portion at a top surface of the second contact layer, and the capping layer fills the recessed portion.

[0013] In some embodiments, after depositing the capping layer, the capping layer has a flat top surface.

[0014] In some embodiments, the thickness of the capping layer is greater than the thickness of the second contact layer.

[0015] In some embodiments, the manufacturing method further includes performing a planarization process after performing the annealing process to make a top surface of the contact plug flush with a top surface of the bit line.

[0016] According to another embodiment of the present disclosure, a method for manufacturing a semiconductor structure is provided, including forming a trench between bit lines, delivering a first gas source of silane and phosphine to the trench to form a first contact layer, delivering a second gas source of silane and phosphine to the trench to form a second contact layer on the first contact layer, wherein a first ratio of phosphine to silane of the first gas source is higher than a second ratio of phosphine to silane of the second gas source. The method also includes delivering a third gas source of silane and phosphine to the trench to form a capping layer on the second contact layer, and performing an annealing process to form a contact plug from the first contact layer and the second contact layer.

[0017] In some embodiments, the first gas source has a first ratio of phosphine to silane greater than 0.3.

[0018] In some embodiments, the flow rate of the second gas source is higher than the flow rate of the first gas source.

[0019] In some embodiments, the third ratio of phosphine to silane of the third gas source is lower than the second ratio of phosphine to silane of the second gas source.

[0020] In some embodiments, the third ratio of phosphine to silane of the third gas source is less than 0.05.

[0021] In some embodiments, the flow rate of the second gas source is higher than the flow rate of the third gas source.

[0022] In some embodiments, forming the first contact layer, forming the second contact layer, and forming the capping layer are performed in-situ.

[0023] According to the above-mentioned embodiment, the manufacturing method of the semiconductor structure includes annealing a first contact layer with a higher doping concentration and a second contact layer with a lower doping concentration to form a single contact plug. Since the second contact layer formed later has a lower doping concentration, the formed second contact layer can have a low surface roughness, thereby reducing the gap size and the number of voids in the contact plug. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] When read in conjunction with the accompanying drawings, various aspects of the present disclosure can be best understood from the following detailed description. It should be noted that, in accordance with standard methods in the industry, various features are not drawn to scale. In fact, the size of various features may be arbitrarily increased or reduced for clarity of discussion.

[0025] Figure 1 The present invention is a flowchart of a method for manufacturing a semiconductor structure according to some embodiments of the present disclosure.

[0026] FIG. 2A to FIG. 2F and Figure 2H Cross-sectional views are shown of various intermediate stages of fabricating a semiconductor structure according to some embodiments of the present disclosure.

[0027] Figure 2G An enlarged cross-sectional view is shown of an intermediate stage in the fabrication of a semiconductor structure according to some embodiments of the present disclosure.

[0028] Figure 3 The cross-sectional view is shown in an intermediate stage of manufacturing a semiconductor structure according to some embodiments of the present disclosure.

[0029] Figure 4A and Figure 4B Cross-sectional views are shown of various intermediate stages of fabricating a semiconductor structure according to some embodiments of the present disclosure. DETAILED DESCRIPTION

[0030] In order to realize the different features of the mentioned subject matter, the following disclosure provides many different embodiments or examples. Specific examples of components, numerical values, configurations, etc. are described below to simplify the present disclosure. Of course, these are merely examples and are not restrictive. For example, in the following description, forming a first feature on or above a second feature may include an embodiment in which the first feature and the second feature are formed in direct contact, and may also include an embodiment in which an additional feature is formed between the first feature and the second feature so that the first feature and the second feature may not be in direct contact. In addition, the present disclosure may repeat reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself represent the relationship between the various embodiments and / or configurations discussed.

[0031] Furthermore, spatially relative terms, such as "below," "beneath," "lower," "above," "upper," and the like, may be used herein to facilitate describing one element or feature's relationship to another element or feature as illustrated in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein interpreted accordingly.

[0032] The present disclosure provides a method for manufacturing a semiconductor structure, comprising depositing a first contact layer with a higher doping concentration, depositing a second contact layer with a lower doping concentration, and annealing the two contact layers to form a contact plug between bit lines. Since the second contact layer has a lower doping concentration, the second contact layer can have a lower surface roughness than the first contact layer, thereby reducing the seam size and the number of voids in the contact plug.

[0033] According to some embodiments of the present disclosure, Figure 1 A flow chart of a method S100 for manufacturing a semiconductor structure is shown. Figure 1 As shown in , method S100 includes steps S110 to S180. FIG. 2A to FIG. 2H The method S100 is further described in detail. FIG. 2A to FIG. 2F and Figure 2H depicts cross-sectional views of various intermediate stages in the fabrication of the semiconductor structure 10, and Figure 2G An enlarged cross-sectional view is shown of an intermediate stage in the fabrication of the semiconductor structure 10 .

[0034] It should be noted that unless otherwise stated, FIG. 2A to FIG. 2H When a series of steps are depicted or described as an embodiment, the order in which the steps are described should not be limiting. For example, some steps may be performed in a different order than the embodiment described, some steps may occur simultaneously, some steps may not be required, and / or some steps may be repeated. In addition, additional steps may be performed before, during, or after each of the depicted steps to fully form the semiconductor structure.

[0035] In order to clearly describe the components included in the semiconductor structure 10, FIG. 2A to FIG. 2H Only some of the elements of the semiconductor structure 10 are shown, but a semiconductor structure 10 including additional elements (eg, word lines, contact pads, etc.) is also within the scope of the present disclosure.

[0036] refer to Figure 1 and Figure 2AIn step S110 of method S100, a plurality of bit lines 130 are formed on substrate 100. Specifically, bit lines 130 include a plurality of material layers stacked along the z-axis direction on the top surface of substrate 100. Bit lines 130 are spaced apart from each other in the x-axis direction, and each bit line 130 extends along the y-axis direction on substrate 100.

[0037] In some embodiments, the substrate 100 may be a bulk semiconductor, a semiconductor-on-insulator (SOI) or other semiconductor substrate. The semiconductor material included in the substrate 100 may be Si, Ge, a compound semiconductor, an alloy semiconductor or a combination thereof. The substrate 100 may be undoped or doped with a dopant. The substrate 100 may further include a polysilicon bit line 110 and a polysilicon bit line 120 as a conductive path. For example, Figure 2A As shown in , polysilicon bit line 110 and polysilicon bit line 120 may be disposed under bit line 130 and electrically connected to bit line 130 to transmit current to bit line 130 .

[0038] In some embodiments, the bit line 130 may include a dielectric layer 132 on the top surface of the substrate 100, a first conductive layer 134 on the dielectric layer 132, a second conductive layer 136 on the first conductive layer 134, and an isolation layer 138 on the second conductive layer 136. The dielectric layer 132 and the isolation layer 138 may be formed of silicon oxide, silicon nitride, a high-k dielectric material, a combination thereof, or the like, to separate other layers of the bit line 130 from the substrate 100 and to separate other layers of the bit line 130 from components above the bit line 130.

[0039] The first conductive layer 134 and the second conductive layer 136 may be formed of polysilicon, metal, metal nitride, metal silicide, combinations thereof, or the like, such that the combination of the first conductive layer 134 and the second conductive layer 136 may serve as a gate structure of the bit line 130. In embodiments where at least one of the first conductive layer 134 and the second conductive layer 136 includes a metal or a metal compound, the bit line 130 may be referred to as a metal bit line.

[0040] In some embodiments, the bit line spacer 140 may be formed on the sidewalls of the bit line 130 to protect the bit line 130 in subsequent manufacturing processes. The bit line spacer 140 may conformally cover the sidewalls of the bit line 130. In some examples, the bit line spacer 140 may further extend from the sidewalls of the bit line 130 into the substrate 100. The bit line spacer 140 may be a single or multiple layers of silicon nitride, a low dielectric constant dielectric layer, other suitable dielectric layers, or a combination thereof.

[0041] refer to Figure 1 and Figure 2B In step S120 of method S100, trenches 150 are formed between bit lines 130. Specifically, substrate 100 between adjacent bit lines 130 is etched so that the etched surface of substrate 100 is lower than the bottom surface of bit line 130. Therefore, trench 150 is formed between two adjacent bit lines 130, and trench 150 has a bottom surface lower than the bottom surface of bit line 130.

[0042] In some embodiments, the substrate 100 may be etched along the bit line spacers 140 on the sidewalls of the bit lines 130 so that the trenches 150 expose the bit line spacers 140. In such embodiments, the width of the trenches 150 in the x-axis direction may be approximately equal to the distance between the bit line spacers 140 on two adjacent bit lines 130. In some embodiments, the bottom surface of the trenches 150 may have a thickness of Figure 2B In other embodiments, the bottom surface of the trench 150 may be a straight line or other shape along the x-axis direction to form a contact plug (see FIG. Figure 2H 1 and 10 ).

[0043] refer to Figure 1 and Figure 2C In step S130 of method S100, a seed layer 160 is formed in the trench 150. Specifically, the seed layer 160 is formed in the trench 150 by, for example, chemical vapor deposition (CVD). Figure 2B 140 . The deposited polysilicon material covers the bottom surface and sidewalls of the trench 150 to form a seed layer 160. The seed layer 160 may also cover the top surface of the bit line 130, so that the seed layer 160 continuously covers the surface of the bit line 130, the bit line spacer 140 and the trench 150. After the seed layer 160 is deposited, a portion of the trench 150 remains above the seed layer 160.

[0044] The polysilicon material of the seed layer 160 may be undoped. Since the seed layer 160 does not include a dopant, the seed layer 160 has a low surface roughness after deposition, and thus the seed layer 160 in the trench 150 may provide a smooth surface for subsequent deposition.

[0045] In some embodiments, the thickness of the seed layer 160 can be thin and conformally cover the surface of the groove 150. For example, the thickness of the seed layer 160 in the groove 150 can be in the range of 1.0 nanometers to 1.5 nanometers. If the thickness of the seed layer 160 is less than 1.0 nanometers, the seed layer 160 may be too thin to provide a smooth surface exposed in the groove 150. If the thickness of the seed layer 160 is greater than 1.5 nanometers, too much time and material may be spent when depositing the seed layer 160 without significantly improving the surface roughness of the seed layer 160.

[0046] refer to Figure 1 and Figure 2D In step S140 of method S100, a first contact layer 170 is formed on the seed layer 160. Specifically, by chemical vapor deposition, for example, Figure 2C The polysilicon material is deposited on the structure shown in FIG. The deposited polysilicon material covers the seed layer 160 to form the first contact layer 170. Since the seed layer 160 provides a smooth surface for depositing the first contact layer 170, the roughness of the first contact layer 170 can be reduced. Figure 2D As shown in FIG. 1 , the first contact layer 170 may continuously cover the seed layer 160 in the trench 150 and the seed layer 160 on the top surface of the bit line 130. After depositing the first contact layer 170, a portion of the trench 150 remains above the first contact layer 170.

[0047] Relative to the seed layer 160, the polysilicon material of the first contact layer 170 is doped with a dopant. For example, the seed layer 160 and the first contact layer 170 may include the same polysilicon, but the first contact layer 170 is doped with an n-type dopant such as phosphorus. More specifically, the first contact layer 170 has a doping concentration that is close to or higher than the expected doping concentration of the contact plug to be formed subsequently. The first contact layer 170 having such a doping concentration can serve as a dopant source for the contact plug to be formed subsequently. When the expected doping concentration of the contact plug is about 1×10 21 cm -3 In some embodiments, the doping concentration of the first contact layer 170 may be 1×10 21 cm -3 Up to 5×10 21 cm -3 in the range.

[0048] In some embodiments, the deposition of the first contact layer 170 and the seed layer 160 may be performed in situ. For example, a gas source of silane may be first delivered into the trench 150 to deposit the seed layer 160. After the seed layer 160 is formed, a mixed gas source of silane and phosphine is delivered into the same chamber to form the first contact layer 170 on the seed layer 160. The ratio of phosphine to silane may be higher than 0.3 to form the first contact layer 170 with a high doping concentration. The concentration of silane in the mixed gas source is higher than the concentration of phosphine, so the main component of the first contact layer 170 is still polysilicon.

[0049] In some embodiments, the thickness of the first contact layer 170 may be greater than the thickness of the seed layer 160. If the thickness of the first contact layer 170 is less than the thickness of the seed layer 160, the first contact layer 170 may be too thin to serve as a dopant source for the contact plug formed subsequently. However, the thickness of the first contact layer 170 is controlled so that a portion of the trench 150 remains after the first contact layer 170 is deposited. Figure 2D As shown in FIG. 1 , the first contact layer 170 can be thin and conformally cover the seed layer 160. In an embodiment where the width of the trench 150 along the x-axis direction is about 45 nanometers, the thickness of the first contact layer 170 in the trench 150 can be in the range of 5.5 nanometers to 9.5 nanometers.

[0050] refer to Figure 1 and Figure 2E In step S150 of method S100, a second contact layer 180 is formed on the first contact layer 170 to fill the trench 150. Specifically, by chemical vapor deposition, for example, Figure 2D The deposited polysilicon material covers the first contact layer 170 to form a second contact layer 180. Figure 2E As shown in FIG. 1 , the second contact layer 180 fills the remaining portion of the trench 150 . The deposited second contact layer 180 covers the first contact layer 170 in the trench 150 and extends onto the first contact layer 170 above the top surface of the bit line 130 .

[0051] More specifically, the deposition of the second contact layer 180 in the trench 150 starts from the surface of the first contact layer 170. As the deposition continues, the material of the second contact layer 180 on the sidewalls of the trench 150 becomes thicker and thicker toward the center of the trench 150. Figure 2E When the second contact layer 180 contacts the interface 180a in the trench 150, the second contact layer 180 fills the trench 150. It should be noted that the interface 180a is illustrated for the purpose of describing the deposition of the second contact layer 180 in detail, and in reality, the interface 180a may not be observed in the second contact layer 180.

[0052] In some embodiments, the second contact layer 180 may be conformal to the first contact layer 170, so that a portion of the second contact layer 180 conforms to the corner of the bit line 130 to form a recessed portion 180b. The recessed portion 180b appears on the top surface of the second contact layer 180, and the bottom of the recessed portion 180b is aligned with the interface 180a along the z-axis direction.

[0053] Similar to the first contact layer 170, the second contact layer 180 is also doped with a dopant. Both the first contact layer 170 and the second contact layer 180 are doped, but the doping concentration of the second contact layer 180 is lower than the doping concentration of the first contact layer 170. The second contact layer 180 has a lower doping concentration, so that the second contact layer 180 filling the trench 150 can have a low surface roughness. Therefore, the gap formed at the interface 180a has a smaller size. In other words, depositing the second contact layer 180 with a low doping concentration can reduce the number of voids in the second contact layer 180. When the doping concentration of the first contact layer 170 is 1×10 21 cm -3 Up to 5×10 21 cm -3 In some embodiments of the range of 4×10 20 cm -3 Up to 5×10 20 cm -3 in the range.

[0054] As described above, the deposited seed layer 160 has no dopant, the deposited first contact layer 170 has a high doping concentration, and the deposited second contact layer 180 has a lower doping concentration than the first contact layer 170. After forming the second contact layer 180, the seed layer 160, the first contact layer 170, and the second contact layer 180 fill the trench 150. Therefore, when measured along the x-axis direction, the doping concentration rises from the interface 180a to the first contact layer 170, and drops from the first contact layer 170 to the seed layer 160.

[0055] In some embodiments, the first contact layer 170 and the second contact layer 180 may be formed of the same polysilicon and include the same dopant. Therefore, the deposition of the second contact layer 180 and the deposition of the first contact layer 170 may be performed in situ. For example, a mixed gas source of silane and phosphine may be first delivered to the trench 150 to deposit the first contact layer 170. After the first contact layer 170 is formed, the ratio of phosphine to silane in the mixed gas source in the same chamber may be lowered, and the second contact layer 180 may be formed on the first contact layer 170. In embodiments where the ratio of phosphine to silane in forming the first contact layer 170 is greater than 0.3, the ratio of phosphine to silane in forming the second contact layer 180 may be between 0.05 and 0.3. Therefore, the doping concentration of the second contact layer 180 is lower than the doping concentration of the first contact layer 170.

[0056] In addition, the gas source flow rate for forming the second contact layer 180 may be higher than the gas source flow rate for forming the first contact layer 170. The high flow rate for forming the second contact layer 180 may completely deposit the second contact layer 180 from the bottom of the trench 150, thereby reducing the risk of forming voids at the bottom of the second contact layer 180.

[0057] In some embodiments, the thickness of the second contact layer 180 may be greater than the thickness of the first contact layer 170. Figure 2E , the thickness of the second contact layer 180 is defined herein as the distance D1 between the surface of the first contact layer 170 and the interface 180a in the x-axis direction, and the thickness of the first contact layer 170 is defined as the distance D2 between the seed layer 160 and the second contact layer 180 in the x-axis direction. The thickness ratio of the second contact layer 180 to the first contact layer 170 may be in the range of 1.3 to 3.1. If the ratio is less than 1.3, the size of the gap or the number of voids in the second contact layer 180 may increase. If the ratio is greater than 3.1, it may be difficult for the first contact layer 170 to provide sufficient dopants for the contact plugs formed subsequently. In the thickness of the first contact layer 170 (i.e., Figure 2E In an embodiment where the distance D2 in the trench 150 is about 5.5 nanometers to about 9.5 nanometers, the thickness of the second contact layer 180 in the trench 150 (ie, Figure 2E The distance D1) in the embodiment may be in the range of 13 nm to 17 nm.

[0058] refer to Figure 1 and Figure 2F In step S160 of method S100, a capping layer 190 is formed on the second contact layer 180. Specifically, by chemical vapor deposition, for example, Figure 2EThe polysilicon material is deposited on the structure shown in FIG. The deposited polysilicon material covers the second contact layer 180 to form a capping layer 190. After the capping layer 190 is deposited, the capping layer 190 has a flat top surface suitable for a subsequent planarization process.

[0059] In the embodiment where the second contact layer 180 has a recessed portion 180 b, the capping layer 190 fills the recessed portion 180 b and provides a flat top surface. The capping layer 190 may be doped to have a lower doping concentration than the first contact layer 170 and the second contact layer 180. Since the capping layer 190 has a low doping concentration, the capping layer 190 may fill the recessed portion 180 b with a low surface roughness, thereby reducing the risk of voids being formed between the second contact layer 180 and the capping layer 190. When the doping concentration of the second contact layer 180 is between 4×10 20 cm -3 Up to 5×10 20 cm -3 In some embodiments of the range of 1×10 20 cm -3 Up to 2×10 20 cm -3 in the range.

[0060] In some embodiments, the second contact layer 180 and the capping layer 190 may include the same polysilicon and dopant. Therefore, depositing the capping layer 190 and depositing the second contact layer 180 may be performed in situ. For example, a mixed gas source of silane and phosphine may be first delivered to the trench 150 to deposit the second contact layer 180. After forming the second contact layer 180, the ratio of phosphine to silane in the mixed gas source may be lowered in the same chamber to form the capping layer 190 on the second contact layer 180. In embodiments where the ratio of phosphine to silane for forming the second contact layer 180 is between 0.05 and 0.3, the ratio of phosphine to silane for forming the capping layer 190 may be less than 0.05. Therefore, the doping concentration of the capping layer 190 is lower than the doping concentration of the second contact layer 180.

[0061] In addition, the gas source flow rate for forming the capping layer 190 may be lower than the gas source flow rate for forming the second contact layer 180. The recessed portion 180b filled by the capping layer 190 is smaller than the trench 150 filled by the second contact layer 180, so the capping layer 190 formed by a lower flow rate can still reduce the risk of forming a void at the bottom of the capping layer 190.

[0062] In some embodiments, the thickness of the capping layer 190 may be greater than the thickness of the second contact layer 180 to provide a flat top surface. For example, the thickness of the capping layer 190 may be close to or equal to the width of the trench 150 in the x-axis direction.

[0063] refer to Figure 1 and Figure 2G In step S170 of method S100, an annealing process is performed on the first contact layer 170 and the second contact layer 180 to form the contact plug 200. During the annealing process, the dopant in the first contact layer 170 diffuses into the adjacent second contact layer 180, thereby increasing the doping concentration of the second contact layer 180. Since the first contact layer 170 before annealing has a high doping concentration, the contact plug 200 formed by the first contact layer 170 and the second contact layer 180 has a high doping concentration after the annealing process.

[0064] To clearly describe the diffusion of dopants, Figure 2G Draw Figure 2F An enlarged cross-sectional view of region A in FIG. Figure 2G As shown in FIG. 1 , the first contact layer 170 with a higher doping concentration serves as a dopant source for the second contact layer 180. When the first contact layer 170 and the second contact layer 180 are heated by the annealing process, the dopant in the first contact layer 170 diffuses toward the second contact layer 180 along the arrow in the x-axis direction.

[0065] It should be noted that the dopant in the first contact layer 170 may also diffuse toward the seed layer 160 along the drawn arrow in the x-axis direction. Since the thickness of the second contact layer 180 is greater than the thickness of the seed layer 160, the dopant may diffuse mainly toward the second contact layer 180. In some other embodiments, the dopant in the first contact layer 170 may diffuse into the cover layer 190 along the z-axis direction. The contact area between the first contact layer 170 and the second contact layer 180 is greater than the contact area between the first contact layer 170 and the cover layer 190, so the dopant may diffuse mainly toward the second contact layer 180 along the x-axis direction.

[0066] After the annealing process, the seed layer 160, the first contact layer 170 and the second contact layer 180 may have similar doping concentrations. In a preferred embodiment, the seed layer 160, the first contact layer 170 and the second contact layer 180 may have uniform doping concentrations. When the seed layer 160, the first contact layer 170 and the second contact layer 180 are formed of the same polysilicon material, there may be no obvious interface between any two layers after the annealing process. Therefore, the seed layer 160, the first contact layer 170 and the second contact layer 180 may be regarded as a contact plug 200. Since the doping concentration of the first contact layer 170 is close to or higher than the expected doping concentration of the contact plug 200, the contact plug 200 formed by the seed layer 160, the first contact layer 170 and the second contact layer 180 can reach the expected doping concentration after the annealing process.

[0067] refer to Figure 1 and Figure 2H In step S180 of method S100, a planarization process is performed to form the semiconductor structure 10. Specifically, a planarization process such as chemical mechanical polishing (CMP) is performed to make the top surface of the contact plug 200 flush with the top surface of the bit line 130. After the planarization process, the semiconductor structure 10 including the bit line 130 and the contact plug 200 is formed. The risk of generating gaps or voids in the contact plug 200 formed by the method S100 is low, thereby improving the yield and performance of the semiconductor structure 10.

[0068] In some embodiments, Figure 2H As shown in Figure 2F In some other embodiments, the capping layer 190 may not be completely removed from the semiconductor structure. For example, Figure 3 According to some embodiments of the present disclosure, a cross-sectional view of an intermediate stage of manufacturing a semiconductor structure 20 is depicted. The process of forming the semiconductor structure 20 is similar to forming Figure 2H The process of forming the semiconductor structure 10 is similar to that of the semiconductor structure 10 , but the process of forming the semiconductor structure 20 includes an additional step of removing a portion of the deposited layer.

[0069] Specifically, when forming the semiconductor structure 20, a portion of the seed layer 160 on the top surface of the bit line 130 is removed before forming the first contact layer 170. Similarly, a portion of the first contact layer 170 on the top surface of the bit line 130 is removed before depositing the second contact layer 180. After the second contact layer 180 fills the trench, the recessed portion 180b of the second contact layer 180 is lower than the top surface of the bit line 130. The capping layer 190 then fills the recessed portion 180b, so that the capping layer 190 in the recessed portion 180b is lower than the top surface of the bit line 130. Therefore, after the planarization process, the capping layer 190 in the recessed portion 180b can be retained in the semiconductor structure 20. In such an embodiment, the seed layer 160, the first contact layer 170, the second contact layer 180, and the retained capping layer 190 can be regarded as a contact plug 200.

[0070] The contact plug 200 with a smaller gap size and a smaller number of voids may bring advantages to further processing of the semiconductor structure 10. For example, Figure 4A and Figure 4B A semiconductor structure 10 is shown in FIG. Figure 2H A cross-section of the intermediate stage. Figure 4A and Figure 4B, the top surface of the contact plug 200 is first recessed to a position lower than the top surface of the bit line 130. Next, a silicide layer 210 is formed on the top surface of the contact plug 200. In some embodiments, forming the silicide layer 210 may include depositing a metal layer on the top surface of the contact plug 200, and performing an annealing process on the metal layer. During the annealing process, the metal layer reacts with the contact plug 200 to form the silicide layer 210.

[0071] Since the contact plug 200 has a smaller gap size and a smaller number of voids, the possibility of forming voids in the silicide layer 210 can be significantly reduced, thereby reducing the risk of cracking the silicide layer 210. As a result, the silicide layer 210 can protect the contact plug 200 from being affected by the material above the silicide layer 210, such as the metal in the contact pad of the contact plug 200. In other words, improving the structural integrity of the contact plug 200 in this way can further process the semiconductor structure 10 with a higher yield.

[0072] According to the above-mentioned embodiment of the present disclosure, the manufacturing method of the semiconductor structure includes depositing a first contact layer and a second contact layer, and annealing the two contact layers to diffuse dopants between the contact layers. The first contact layer with a higher doping concentration is used as a dopant source for the contact plug. The second contact layer with a lower doping concentration has a lower surface roughness than the first contact layer after formation, thereby reducing the gap size and the number of voids in the contact plug, thereby improving the yield and performance of the semiconductor structure including the contact plug.

[0073] The features of some embodiments are summarized above so that those skilled in the art can better understand the viewpoints of the present disclosure. Those skilled in the art should understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to achieve the same purpose and / or achieve the same advantages as the embodiments described herein. Those skilled in the art should also understand that such equivalent constructions do not depart from the spirit and scope of the present disclosure, and various changes, substitutions and modifications can be made without departing from the spirit and scope of the present disclosure.

[0074]

Explanation of symbols

[0075] 10,20:Semiconductor structure

[0076] 100:Substrate

[0077] 110,120: Polysilicon bit lines

[0078] 130: Bit line

[0079] 132: Dielectric layer

[0080] 134: first conductive layer

[0081] 136: second conductive layer

[0082] 138: Isolation layer

[0083] 140: Bit line spacer

[0084] 150: Groove

[0085] 160: Seed layer

[0086] 170: first contact layer

[0087] 180: second contact layer

[0088] 180a: Interface

[0089] 180b: recessed part

[0090] 190: Covering layer

[0091] 200: Contact plug

[0092] 210: Silicide layer

[0093] A: Area

[0094] D1,D2: distance

[0095] S100: Method

[0096] S110,S120,S130,S140,S150,S160,S170,S180: Steps

[0097] x,y,z: axes.

Claims

1. A method for manufacturing a semiconductor structure, characterized in that: include: forming trenches between the plurality of bit lines; depositing a seed layer in the trench; depositing a first contact layer on the seed layer in the trench; depositing a second contact layer on the first contact layer to fill the trench, wherein a second doping concentration of the second contact layer is lower than a first doping concentration of the first contact layer; as well as An annealing process is performed on the first contact layer and the second contact layer so that dopants in the first contact layer diffuse into the second contact layer to form a contact plug including the first contact layer and the second contact layer.

2. The manufacturing method according to claim 1, characterized in that: The first doping concentration of the first contact layer before the annealing process is performed is higher than the doping concentration of the contact plug after the annealing process is performed.

3. The manufacturing method according to claim 1, characterized in that: The seed layer is undoped before performing the annealing process.

4. The manufacturing method according to claim 3, characterized in that: After performing the annealing process, the dopant in the first contact layer diffuses into the seed layer to form the contact plug including the seed layer.

5. The manufacturing method according to claim 1, characterized in that: After performing the annealing process, the seed layer, the first contact layer, and the second contact layer have uniform doping concentrations.

6. The manufacturing method according to claim 1, characterized in that: The thickness of the first contact layer is greater than the thickness of the seed layer, and the thickness of the second contact layer is greater than the thickness of the first contact layer.

7. The manufacturing method according to claim 1, characterized in that: A ratio of a thickness of the second contact layer to a thickness of the first contact layer is in a range of 1.3 to 3.

1.

8. The manufacturing method according to claim 1, characterized in that: The seed layer, the first contact layer, and the second contact layer are formed of the same polysilicon material.

9. The manufacturing method according to claim 1, characterized in that: Further including: After depositing the second contact layer and before performing the annealing process, a capping layer is deposited on the second contact layer, wherein a third doping concentration of the capping layer is lower than the second doping concentration of the second contact layer.

10. The manufacturing method according to claim 9, characterized in that: The second contact layer includes a recessed portion at a top surface of the second contact layer, and wherein the capping layer fills the recessed portion.

11. The manufacturing method according to claim 9, characterized in that: After depositing the capping layer, the capping layer has a flat top surface.

12. The manufacturing method according to claim 9, characterized in that: The thickness of the capping layer is greater than the thickness of the second contact layer.

13. The manufacturing method according to claim 1, characterized in that: Further including: A planarization process is performed after the annealing process is performed to make the top surface of the contact plug flush with the top surfaces of the plurality of bit lines.

14. A method for manufacturing a semiconductor structure, characterized in that: include: forming trenches between the plurality of bit lines; delivering a first source gas of silane and phosphine to the trench to form a first contact layer; delivering a second gas source of silane and phosphine to the trench to form a second contact layer on the first contact layer, wherein a first ratio of phosphine to silane of the first gas source is higher than a second ratio of phosphine to silane of the second gas source; delivering a third gas source of silane and phosphine to the trench to form a capping layer on the second contact layer; as well as An annealing process is performed to form a contact plug from the first contact layer and the second contact layer.

15. The manufacturing method according to claim 14, characterized in that: The first ratio of phosphine to silane in the first gas source is greater than 0.

3.

16. The manufacturing method according to claim 14, characterized in that: The flow rate of the second gas source is higher than the flow rate of the first gas source.

17. The manufacturing method according to claim 14, characterized in that: The third ratio of phosphine to silane of the third gas source is lower than the second ratio of phosphine to silane of the second gas source.

18. The manufacturing method according to claim 14, characterized in that: The third gas source has a third ratio of phosphine to silane less than 0.

05.

19. The manufacturing method according to claim 14, characterized in that: The flow rate of the second gas source is higher than the flow rate of the third gas source.

20. The manufacturing method according to claim 14, characterized in that: Forming the first contact layer, forming the second contact layer, and forming the capping layer are performed in-situ.