HBC battery, battery pack and photovoltaic system
By alternately setting the amorphous silicon layer and polysilicon layer on the backlight surface of the silicon substrate of the HBC cell, the density and etch resistance of the polysilicon layer are improved, the problem of insufficient carrier recombination rate and stability is solved, and the solar cell is improved Performance and efficiency.
Patent Information
- Application Number
- CN202411390523.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2024-11-22
AI Technical Summary
The increasing recombination rate of carriers and insufficient stability in existing HBC batteries lead to low photoelectric conversion efficiency and high manufacturing cost.
The backlight surface of the silicon substrate alternately arranges the first and second regions that do not overlap each other, and an amorphous silicon layer is arranged in the first region, and its extinction coefficient is greater than the extinction coefficient of the polysilicon layer in the second region, thereby improving the density of the polysilicon layer. and resistance to electrode slurry etching ability, reducing carrier recombination rate.
The matching performance and field passivation effect between the polysilicon layer and the electrode slurry are improved, the working performance of the solar cell is enhanced, the carrier recombination rate is reduced, and the photoelectric conversion efficiency and stability are improved.
Smart Images

Figure CN119008735A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of photovoltaic technology, and in particular relates to an HBC battery, a battery pack and a photovoltaic system. Background Art
[0002] In the existing HBC (Heterojunction with Back Contact) cells, significant progress has been made compared to BC (Back Contact) cells, but there are still some technical problems that limit its further improvement of photoelectric conversion efficiency and reduction of manufacturing costs.
[0003] HBC batteries rely on heterojunction structures in their design. Although this structure improves the photoelectric conversion efficiency, improper heterojunction processing can easily cause the generated carriers to recombine before reaching the electrode, reducing the current that can be collected, resulting in an increase in the carrier recombination rate. In addition, the lack of material density leads to poor etching resistance, especially in the electrode manufacturing process. The electrode slurry used may damage or penetrate the material layer, affecting the matching between the electrode and the silicon layer, and thus affecting the overall performance and stability of the battery. Summary of the invention
[0004] The present invention provides an HBC battery, aiming to solve the problems of increased recombination rate of carriers and insufficient stability in the existing HBC battery.
[0005] The present invention is achieved in that a HBC battery comprises:
[0006] A silicon substrate, wherein the silicon substrate has a backlight surface and a light-facing surface that are oppositely arranged, a first region and a second region are arranged on the backlight surface of the silicon substrate, the first region and the second region are arranged alternately, and the first region and the second region do not overlap;
[0007] The first region includes an amorphous silicon layer, and the second region includes a polycrystalline silicon layer. The amorphous silicon layer and the polycrystalline silicon layer are of different types, and the extinction coefficient of the amorphous silicon layer is greater than the extinction coefficient of the polycrystalline silicon layer.
[0008] Optionally, a ratio of an extinction coefficient of the amorphous silicon layer to an extinction coefficient of the polycrystalline silicon layer is greater than 1.3 and less than 11.
[0009] Optionally, a difference between an extinction coefficient of the amorphous silicon layer and an extinction coefficient of the polycrystalline silicon layer is greater than 0.01 and less than 0.08.
[0010] Optionally, an isolation region is further included, wherein the isolation region is placed between the first region and the second region.
[0011] Optionally, the thickness of the amorphous silicon layer is greater than 13 nm and less than 17 nm.
[0012] Optionally, the thickness of the polysilicon layer is greater than 280 nm and less than 300 nm.
[0013] Optionally, the refractive index of the amorphous silicon layer is greater than the refractive index of the polycrystalline silicon layer.
[0014] Optionally, a ratio of a refractive index of the amorphous silicon layer to a refractive index of the polycrystalline silicon layer is greater than 1 and less than 1.2.
[0015] Optionally, a difference between a refractive index of the amorphous silicon layer and a refractive index of the polycrystalline silicon layer is greater than 0.01 and less than 0.5.
[0016] Optionally, the amorphous silicon layer is a P-type amorphous silicon layer, and the polycrystalline silicon layer is an N-type polycrystalline silicon layer.
[0017] The present invention also provides a battery pack, comprising the above-mentioned HBC battery.
[0018] The present invention also provides a photovoltaic system, comprising the above-mentioned battery group.
[0019] The beneficial effect achieved by the present invention is that, since non-overlapping first and second regions are alternately arranged on the backlight surface of the silicon substrate, the extinction coefficient of the amorphous silicon layer arranged in the first region is greater than the extinction coefficient of the polycrystalline silicon layer arranged in the second region, so that the polycrystalline silicon layer has a relatively high density, and thus the polycrystalline silicon layer has a relatively high ability to resist electrode slurry etching, preventing the manufactured electrode from penetrating the polycrystalline silicon layer, improving the matching between the polycrystalline silicon layer and the electrode slurry, and ensuring that the polycrystalline silicon layer has a high field passivation effect, reducing the carrier recombination rate on the backlight side, and improving the working performance of the solar cell. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of the solar cell structure provided by the present invention.
[0021] Description of reference numerals:
[0022] 100, HBC battery; 110, first region; 111, amorphous silicon layer; 120, second region; 121, polycrystalline silicon layer; 130, isolation region; 140, silicon substrate. DETAILED DESCRIPTION
[0023] In order to make the purpose, technical scheme and advantages of the present invention clearer, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. Examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements with the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and should not be construed as limiting the present invention. In addition, it should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0024] In the description of the present invention, it is necessary to understand that the terms "length", "width", "up", "down", "left", "right", "horizontal", "top", "bottom", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0025] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0026] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or mutual communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0027] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0028] The disclosure below provides many different embodiments or examples to realize different structures of the present invention. In order to simplify the disclosure of the present invention, the parts and settings of specific examples are described below. Of course, they are only examples, and the purpose is not to limit the present invention. In addition, the present invention can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplification and clarity, which itself does not indicate the relationship between the various embodiments and / or settings discussed. In addition, the examples of various specific processes and materials provided by the present invention, but those of ordinary skill in the art can be aware of the application of other processes and / or the use of other materials.
[0029] The present invention alternately arranges non-overlapping first and second regions on the backlight surface of a silicon substrate, and the extinction coefficient of an amorphous silicon layer arranged in the first region is greater than the extinction coefficient of a polycrystalline silicon layer arranged in the second region, so that the polycrystalline silicon layer has a relatively high density, and further the polycrystalline silicon layer has a relatively high ability to resist electrode slurry etching, preventing the manufactured electrode from penetrating the polycrystalline silicon layer, improving the matching between the polycrystalline silicon layer and the electrode slurry, and ensuring that the polycrystalline silicon layer has a high field passivation effect, reducing the carrier recombination rate on the backlight side, and improving the working performance of the solar cell.
[0030] Embodiment 1
[0031] like Figure 1 As shown, this embodiment provides a HBC battery 100, including:
[0032] A silicon substrate 140, wherein the silicon substrate 140 has a backlight surface and a light-facing surface that are oppositely disposed, and a first region 110 and a second region 120 are disposed on the backlight surface of the silicon substrate 140, the first region 110 and the second region 120 are alternately disposed, and the first region 110 and the second region 120 do not overlap;
[0033] The first region 110 includes an amorphous silicon layer 111 , and the second region 120 includes a polycrystalline silicon layer 121 . The amorphous silicon layer 111 and the polycrystalline silicon layer 121 are of different types, and the extinction coefficient of the amorphous silicon layer 111 is greater than the extinction coefficient of the polycrystalline silicon layer 121 .
[0034] The HBC cell 100 (Heterojunction with Back Contact solar cell) is a solar cell with a heterojunction structure and a back contact design. It combines the advantages of different materials and improves the photoelectric conversion efficiency. The heterojunction is formed on the back of the cell by different types of silicon materials (usually amorphous silicon and polycrystalline silicon), which can improve the efficiency of the cell.
[0035] The silicon substrate 140 has two main surfaces, a light-facing surface and a backlight surface. The light-facing surface directly faces the sunlight, while the backlight surface is the other side. The two surfaces are arranged opposite to each other.
[0036] Two different regions are arranged on the backlight surface of the silicon substrate 140, namely, a first region 110 and a second region 120. The two regions are arranged alternately and do not overlap each other. The first region 110 and the second region 120 can be arranged adjacent to each other, or other regions can be arranged between the first region 110 and the second region 120.
[0037] The first region 110 includes an amorphous silicon layer 111, and the atomic arrangement of the amorphous silicon layer 111 is disordered and has no long-range order. The second region 120 includes a polycrystalline silicon layer 121, and the polycrystalline silicon is composed of a plurality of small silicon crystals. These grains gather together to form a larger structure, but there are grain boundaries between the grains. The amorphous silicon layer 111 and the polycrystalline silicon layer 121 are of different types, that is, when the amorphous silicon layer 111 is P-type, the polycrystalline silicon layer 121 is N-type, and when the amorphous silicon layer 111 is N-type, the polycrystalline silicon layer 121 is P-type, and the N-type and P-type form a PN junction.
[0038] The higher the extinction coefficient, the stronger the light absorption capacity is, while the lower the extinction coefficient, the weaker the light absorption capacity is. If the extinction coefficient of the amorphous silicon layer 111 is greater than the extinction coefficient of the polysilicon layer 121, the light absorption capacity of the amorphous silicon layer 111 is greater than that of the polysilicon layer 121.
[0039] At the same time, the smaller the extinction coefficient, the denser and more uniform the material structure. The dense polysilicon layer 121 has fewer defects and voids inside, which leads to enhanced physical stability and mechanical strength. On the one hand, the polysilicon layer 121 has high density, a more stable and uniform structure, and can better resist the etching of the electrode slurry during the manufacturing process. This can ensure that the polysilicon layer 121 maintains its integrity during the electrode printing and sintering process, reducing the loss of electrical performance caused by etching. On the other hand, the high density of the polysilicon layer 121 can effectively passivate the surface, reduce the trap states on the surface and in the body, and thus reduce the recombination rate of electrons and holes on the backlight side.
[0040] In this embodiment, non-overlapping first regions 110 and second regions 120 are alternately arranged on the backlight surface of the silicon substrate 140, and the extinction coefficient of the amorphous silicon layer 111 arranged in the first region 110 is greater than the extinction coefficient of the polycrystalline silicon layer 121 arranged in the second region 120, so that the polycrystalline silicon layer 121 has a relatively high density, and thus the polycrystalline silicon layer 121 has a relatively high ability to resist electrode slurry etching, preventing the manufactured electrode from penetrating the polycrystalline silicon layer 121, improving the matching between the polycrystalline silicon layer 121 and the electrode slurry, and ensuring that the polycrystalline silicon layer 121 has a high field passivation effect, reducing the carrier recombination rate on the backlight side, and improving the working performance of the solar cell.
[0041] Embodiment 2
[0042] Based on the first embodiment, the ratio of the extinction coefficient of the amorphous silicon layer 111 to the extinction coefficient of the polycrystalline silicon layer 121 is greater than 1.3 and less than 11.
[0043] By selecting an amorphous silicon layer 111 and a polycrystalline silicon layer 121 with an extinction coefficient ratio between 1.3 and 11, efficient light absorption and optimized light management are achieved in the first region 110 and the second region 120. This is crucial for enhancing light capture and the generation of electron-hole pairs. The appropriate extinction coefficient ratio ensures good matching between the polycrystalline silicon layer 121 and the electrode slurry, reduces electrical contact impedance, enhances electrode adhesion, and makes the polycrystalline silicon layer 121 have a higher resistance to electrode slurry etching, ensuring the stability of the layer structure during printing and sintering. And by precisely controlling the extinction coefficient ratio of the amorphous silicon layer 111 and the polycrystalline silicon layer 121, the surface is effectively passivated, the defects caused by the disordered structure are reduced, and the carrier recombination rate is reduced. Enhancing the field passivation effect helps to improve the open circuit voltage and fill factor of the battery, and ultimately improve the photoelectric conversion efficiency.
[0044] The extinction coefficient is selected reasonably, so that the amorphous silicon layer 111 and the polycrystalline silicon layer 121 achieve the best balance between light absorption and conductivity, thereby improving the photoelectric conversion efficiency of the solar cell, extending the service life of the battery, and improving the output power and use stability.
[0045] Embodiment 3
[0046] Based on the first embodiment, the difference between the extinction coefficient of the amorphous silicon layer 111 and the extinction coefficient of the polysilicon layer 121 is greater than 0.01 and less than 0.08.
[0047] Specifically, amorphous silicon has a higher extinction coefficient and absorbs high-energy photons more effectively. Although polycrystalline silicon has a lower extinction coefficient, it can absorb photons more evenly within this smaller difference range, thereby improving the light absorption efficiency of the entire cell. Since the difference is between 0.01 and 0.08, the reflection and scattering effect of photons at the interface of the two materials is lower, and with the appropriate anti-reflection layer design, light loss can be further reduced and light capture can be optimized.
[0048] Embodiment 4
[0049] On the basis of the first embodiment, an isolation region 130 is further included. The isolation region 130 is disposed between the first region 110 and the second region 120 .
[0050] The isolation region 130 can effectively separate the first region 110 from the second region 120 to prevent the mixing and recombination of charge carriers. In this way, charges can be more effectively separated and transmitted in their respective regions. The isolation region 130 reduces the chance of photogenerated carriers migrating across regions and reduces the probability of carrier recombination, thereby improving the photoelectric conversion efficiency of the solar cell.
[0051] The isolation region 130 also helps to reduce interface defects between the amorphous silicon layer 111 and the polycrystalline silicon layer 121. These defects are usually the main source of carrier recombination, so the provision of the isolation region 130 can improve the passivation effect of the interface, thereby improving the battery performance. The presence of the isolation region 130 makes the interface between the amorphous silicon layer 111 and the polycrystalline silicon layer 121 more stable, reducing the defect expansion caused by repeated stress and thermal cycling at the interface.
[0052] Embodiment 5
[0053] Based on the first embodiment, the thickness of the amorphous silicon layer 111 is greater than 13 nm and less than 17 nm.
[0054] The thickness of the amorphous silicon layer 111 is in the range of 13nm to 17nm, which is conducive to more efficient charge separation. An amorphous silicon layer 111 that is too thick may increase the recombination rate of the charge, while a layer that is too thin may not be sufficient to effectively separate the photogenerated carriers. A reasonable thickness of the amorphous silicon layer 111 can provide a better charge transfer path, reduce energy loss during charge transfer, and thus improve the photoelectric conversion efficiency of the battery.
[0055] Embodiment 6
[0056] Based on the first embodiment, the thickness of the polysilicon layer 121 is greater than 280 nm and less than 300 nm.
[0057] The thickness of the polysilicon layer 121 is in the range of 280nm to 300nm, which helps to efficiently separate the photogenerated charges. This thickness range not only avoids the recombination of charges inside the material, but also provides sufficient volume to support efficient charge transfer. The polysilicon layer 121 with a thickness within this range can reduce resistance and increase carrier transfer speed, thereby improving the fill factor and overall efficiency of the battery.
[0058] Embodiment 7
[0059] Based on the first embodiment, the refractive index of the amorphous silicon layer 111 is greater than the refractive index of the polysilicon layer 121 .
[0060] Since the refractive index of the amorphous silicon layer 111 is greater than that of the polycrystalline silicon layer 121, when light enters the amorphous silicon layer 111, the propagation path of the light will be refracted, so that most of the light can continue to be transmitted to the polycrystalline silicon layer 121, thereby reducing the parasitic absorption in the amorphous silicon layer 111. At the same time, the higher refractive index enables the amorphous silicon layer 111 to have a higher light penetration ability, which means that more light can penetrate the amorphous silicon layer 111 and reach the polycrystalline silicon layer 121 with higher absorption ability, thereby improving the overall light absorption efficiency.
[0061] Embodiment 8
[0062] Based on the seventh embodiment, the ratio of the refractive index of the amorphous silicon layer 111 to the refractive index of the polysilicon layer 121 is greater than 1 and less than 1.2.
[0063] By precisely controlling the refractive index ratio of the amorphous silicon layer 111 and the polycrystalline silicon layer 121 between 1 and 1.2, the propagation path of light can be precisely regulated to ensure effective transmission and absorption of light and maximize optical utilization. This ratio range helps to achieve microscopic optical matching between layers, reduce light reflection losses at the interface, and thus improve the light absorption efficiency of the cell.
[0064] Embodiment 9
[0065] Based on the first embodiment, the difference between the refractive index of the amorphous silicon layer 111 and the refractive index of the polysilicon layer 121 is greater than 0.01 and less than 0.5.
[0066] The refractive index difference between the amorphous silicon layer 111 and the polycrystalline silicon layer 121 is limited to between 0.01 and 0.5, so that the light reflection between the two layers of materials is minimized, thereby improving the light absorption efficiency. This refractive index difference range helps to achieve multiple reflections and effective transmission of light inside the cell, thereby increasing optical utilization.
[0067] Embodiment 10
[0068] On the basis of the first embodiment, the amorphous silicon layer 111 is a P-type amorphous silicon layer 111 , and the polycrystalline silicon layer 121 is an N-type polycrystalline silicon layer 121 .
[0069] Amorphous silicon has a high defect state density, and these defects will capture electrons, resulting in low electron mobility. However, holes move relatively more smoothly in amorphous silicon, so amorphous silicon is more suitable as a P-type material. Amorphous silicon as a P-type material can also effectively passivate the interface with the polycrystalline silicon or crystalline silicon substrate 140, reduce the carrier recombination caused by interface defect states, and thus improve the interface quality. Moreover, amorphous silicon has good long-term stability as a P-type layer, mature technology, and relatively easy control of process parameters, which meets the requirements of large-scale industrial production.
[0070] N-type polysilicon has a large number of free electrons and high electron mobility, which can effectively improve the conductivity of the device and reduce resistance loss. The crystalline structure of polysilicon is better than that of amorphous silicon and has a lower defect state density, which makes polysilicon an N-type material that can better conduct electrons.
[0071] Setting the amorphous silicon layer 111 to P type and the polycrystalline silicon layer 121 to N type fully utilizes the advantages of their respective materials, optimizes the transmission and separation efficiency of carriers, and improves the photoelectric conversion efficiency.
[0072] Embodiment 10
[0073] This embodiment provides a battery pack, including the HBC battery 100 of the above embodiment.
[0074] The beneficial effects of the battery pack of this embodiment are equivalent to the beneficial effects of the above-mentioned HBC battery 100, and will not be described in detail here.
[0075] Embodiment 11
[0076] This embodiment provides a photovoltaic system, including the battery pack of the above embodiment.
[0077] The beneficial effects of the photovoltaic system of this embodiment are equivalent to the beneficial effects of the above-mentioned battery pack, which will not be described in detail here.
[0078] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A HBC battery, characterized in that: include: A silicon substrate, wherein the silicon substrate has a backlight surface and a light-facing surface that are oppositely arranged, a first region and a second region are arranged on the backlight surface of the silicon substrate, the first region and the second region are arranged alternately, and the first region and the second region do not overlap; The first region includes an amorphous silicon layer, and the second region includes a polycrystalline silicon layer. The amorphous silicon layer and the polycrystalline silicon layer are of different types, and the extinction coefficient of the amorphous silicon layer is greater than the extinction coefficient of the polycrystalline silicon layer.
2. A HBC battery as claimed in claim 1, characterized in that: The ratio of the extinction coefficient of the amorphous silicon layer to the extinction coefficient of the polycrystalline silicon layer is greater than 1.3 and less than 11.
3. A HBC battery as claimed in claim 1, characterized in that: The difference between the extinction coefficient of the amorphous silicon layer and the extinction coefficient of the polycrystalline silicon layer is greater than 0.01 and less than 0.
08.
4. A HBC battery as claimed in claim 1, characterized in that: Also included is an isolation region disposed between the first region and the second region.
5. The HBC battery according to claim 1, characterized in that: The thickness of the amorphous silicon layer is greater than 13 nm and less than 17 nm.
6. A HBC battery as claimed in claim 1, characterized in that: The thickness of the polysilicon layer is greater than 280 nm and less than 300 nm.
7. A HBC battery as claimed in claim 1, characterized in that: The refractive index of the amorphous silicon layer is greater than the refractive index of the polysilicon layer.
8. A HBC battery as claimed in claim 7, characterized in that: The ratio of the refractive index of the amorphous silicon layer to the refractive index of the polysilicon layer is greater than 1 and less than 1.
2.
9. A HBC battery as claimed in claim 7, characterized in that: The difference between the refractive index of the amorphous silicon layer and the refractive index of the polysilicon layer is greater than 0.01 and less than 0.
5.
10. The HBC battery according to claim 1, characterized in that: The amorphous silicon layer is a P-type amorphous silicon layer, and the polycrystalline silicon layer is an N-type polycrystalline silicon layer.
11. A battery pack, characterized in that: A HBC battery comprising any one of claims 1 to 10.
12. A photovoltaic system, characterized in that: A battery pack comprising the battery pack of claim 11.
Citation Information
Cited By
HBC cell, battery assembly, and photovoltaic system
WO2026118387A1