Alpha coil insulation wrapping and sealing method

Through the Alpha coil insulation bandaging sealing method, multi-layer insulation banding and polyimide composite film are used to solve the complexity of the structure of the submerged winding of the submerged oil motor and electromagnetic compatibility, achieving efficient insulation and sealing effects, and improving the motor Stability and compatibility.

CN119010495AActive Publication Date: 2024-11-22HUNAN CRRC SHANGQU ELECTRIC CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411148661.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-22
Estimated Expiration
2044-08-21

AI Technical Summary

Technical Problem

The existing submersible motors adopt a complex structure with a loose winding structure, low space utilization, and may introduce electromagnetic interference in high-voltage and high humidity downhole environments, affecting the electromagnetic compatibility of the motor and supporting equipment.

Method used

Alpha coil insulation bandaging sealing method is adopted, through sintering and multi-layer insulation bandaging technology, the polyimide composite film is used for semi-packing and cladding, filling and bandaging, ensuring the insulating and sealing of the coil, and in high-temperature insulation oil. Perform sealing treatment.

Benefits of technology

The stator insulation process is simplified, the lifting force of the motor is improved, the electromagnetic compatibility is enhanced, the stability and reliability of the coil in high-voltage and high humidity environments, and the ability to withstand AC voltages above 10KV.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119010495A_ABST
    Figure CN119010495A_ABST
Patent Text Reader

Abstract

The invention discloses an alpha coil insulation binding and sealing method. The method comprises the following steps: S1, winding an electromagnetic wire by adopting a polyimide composite film, and then sintering; s2, carrying out half-lapped wrapping and insulation wrapping on all series wires and lead-out wires in the alpha coil by using a composite film, and then binding and fixing the series wires and the lead-out wires; s3, binding all alpha coil cakes by using the composite film for one layer; s4, the starting point of the second layer of insulation wrapping is located at the outer leading-out wire of the alpha coil, and the composite film is adopted to continuously wrap the coil cake and the serial connection wire; s5, putting the alpha coil into an oven for sintering treatment; s6, carrying out third-layer and fourth-layer insulation wrapping on the alpha coil; and S7, the whole alpha coil is put into an oven to be sintered, and the coil is soaked in insulating oil after being wrapped in an insulating mode. According to the invention, the stator insulation process is simplified, and the insulativity and the sealing property of the alpha coil are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of motor coils, and in particular to an alpha coil insulation wrapping and sealing method. Background Art

[0002] Submersible motors for oil production have the characteristics of simple structure, energy saving, environmental protection and online control. They are suitable for oil production in horizontal oil wells, directional inclined wells and low permeability oil wells. Due to the limitation of the wellhead, submersible motors are designed as slender structures to obtain sufficient torque. Therefore, the magnetic flux of the stator winding will directly determine the lifting force of the motor. Most submersible pump motors are loose winding structures. The electromagnetic wire itself has a layer of paint film with insulation performance. The electromagnetic wire is embedded or inserted into the core slot. The stator with windings is then insulated (dipped in paint or potting). This process requires the completion of winding embedding, end shaping, insulation treatment and other processes. The design and manufacturing process of submersible motors with loose winding structures is more complicated, requiring precise calculation and arrangement of each winding component, but in a limited space, the space utilization rate is low; the loose winding structure may introduce additional electromagnetic interference, especially in the high-pressure and high-humidity environment underground, which may affect the electromagnetic compatibility performance of the motor and supporting equipment.

[0003] The patent with the prior art application number CN202210569555.2 discloses a method for automatically and continuously winding multiple alpha coils, including: S1, winding the electromagnetic wire in a wire storage drum; S2, installing the winding mold and the wire storage drum on a rotating mechanism; S3, controlling the rotation of the rotating mechanism to make the electromagnetic wire in the wire storage drum wind the coil cake on the winding mold. Although it can achieve efficient production of coils and ensure the consistency of coil performance, the shortcoming of this patent is that it does not provide effective insulation protection for the formed coils. Summary of the invention

[0004] The main problem solved by the present invention is that the design and manufacturing process of the submersible motor using a loose winding structure in the prior art is more complicated, requiring precise calculation and arrangement of each winding element, and the space utilization rate is low within a limited space. The loose winding structure may introduce additional electromagnetic interference, especially in the high-pressure and high-humidity environment underground, which may affect the electromagnetic compatibility performance of the motor and supporting equipment. An alpha coil insulation wrapping and sealing method is provided.

[0005] In view of the above technical problems, the technical solutions of the present invention are as follows:

[0006] An alpha coil insulation wrapping and sealing method comprises the following steps:

[0007] S1, wrapping the electromagnetic wire with the composite film, sintering it, and winding it into an alpha coil after cooling;

[0008] S2. Half-wrap all the series wires and lead wires in the Alpha Coil with the composite film, wherein the half-wrap direction is from the previous coil cake to the corresponding length of the next coil cake, so as to maintain the electrical connection and insulation between the coil cakes, and then tie and fix the Alpha Coil after insulation wrapping;

[0009] S3, wrapping all the Alpha coil cakes with a layer of the composite film, the inner circle of the Alpha coil is wrapped in a half-overlapping manner, and the outer circle of the Alpha coil is wrapped in a overlapping manner;

[0010] S4, the starting point of the second layer of insulation wrapping is located at the external lead wire of the Alpha coil, and the composite film is used to continuously wrap the coil cake and the string wire until the external lead wire at the other end of the coil cake ends; in the process of wrapping the lead wire to the coil cake, the intersection between the lead wire and the coil cake is filled and wrapped; in the process of wrapping the coil cake to the string wire, the intersection between the coil cake and the string wire is filled and wrapped;

[0011] Among them, the two intersection positions are divided into four quadrants according to the separation of the coil cake, the lead wire and the series wire, the left and right sides of the series wire are the first quadrant and the second quadrant respectively, and the left and right sides of the lead wire are the third quadrant and the fourth quadrant respectively; in the process of wrapping the lead wire to the coil cake, a gap is formed between the second and third quadrants, and the composite film is first passed through the third quadrant, and the composite film is inserted into the second quadrant, and then the composite film is passed through the first quadrant, and the composite film is inserted into the second quadrant, and finally the composite film is passed through the fourth quadrant, and the coil cake can be wrapped, wherein the process of passing the composite film from the third quadrant and inserting the composite film into the second quadrant is gap filling.

[0012] S5. After the second layer of insulation wrapping is completed, the entire Alpha coil is placed in a baking furnace for sintering, so that the insulation of the Alpha coil reaches a predetermined standard;

[0013] S6, after the Alpha coil is cooled, the Alpha coil is subjected to a third layer and a fourth layer of insulation wrapping, and the insulation wrapping method of the third layer and the fourth layer is the same as the insulation wrapping method of the second layer;

[0014] S7. After the fourth layer of insulation wrapping is completed, the entire Alpha coil is placed in a baking furnace for sintering until all insulation layers are tightly combined to achieve the best insulation effect; after the Alpha coil is insulated and wrapped, it is immersed in insulating oil, and the insulating oil is heated to a certain temperature to seal the stator as a whole and cool it to room temperature.

[0015] Furthermore, the composite film is a polyimide composite film.

[0016] Furthermore, in step S3, the length of the package is controlled to be between 3 mm and 4 mm.

[0017] Furthermore, in step S4, the composite film is used for wrapping, the inner circle of the coil cake is half-overlapped, and the outer circle is overlapped, and the overlapping length is controlled between 3mm-4mm. At the same time, the lead wire and the series wire are both wrapped in a half-overlapping manner, and the coil cake, the lead wire and the series wire form an insulating whole.

[0018] Furthermore, in step S4, during the wrapping process from the coil cake to the series connection line, after the lead-out line of the coil cake is wrapped, the coil cake is wrapped again, wherein the inner circle of the coil cake is wrapped in a half-overlapping manner, and the outer circle of the coil cake is wrapped in a overlapping manner, and the length of the overlapping is in the range of 3mm-4mm. When the wrapping process reaches the intersection position of the coil cake and the series connection line, filling wrapping is performed.

[0019] Furthermore, during the filling and wrapping, when the next string of wires is located on the left side of the previous string of wires, a gap is formed between the second quadrant and the third quadrant. The composite film is firstly used to wrap the intersection of the coil cake and the string of wires six times in a penetration-insertion manner, and then the composite film is penetrated from the first quadrant.

[0020] Furthermore, the third and fourth penetration-insertion of the composite film are both penetration from the third quadrant and then insertion from the second quadrant, and the third and fourth penetration-insertion of the composite film are gap filling.

[0021] Furthermore, during the filling and wrapping, when the next string of wires is located on the right side of the previous string of wires, a gap is formed between the first quadrant and the fourth quadrant. The composite film is firstly used to wrap the intersection of the coil cake and the string of wires eight times in a penetration-insertion manner, and then the composite film is penetrated from the first quadrant.

[0022] Furthermore, the fourth and fifth penetration-insertion of the composite film are both penetration from the fourth quadrant and then insertion from the first quadrant, and the fourth and fifth penetration-insertion of the composite film are gap filling.

[0023] Furthermore, in step S6, the insulation wrapping method of the third and fourth layers of the alpha coil is the same as the insulation wrapping method of the second layer.

[0024] Compared with the prior art, the present invention has the following beneficial effects:

[0025] 1. During the wrapping process, the present invention performs special filling and wrapping at the intersection of the lead wire and the coil cake and the intersection of the coil cake and the series wire, thereby ensuring the stability of the coil cake and the reliability of the overall structure; the alpha coil adopts a continuous winding structure of multiple alpha coils, which can avoid problems such as poor contact, dimensional tolerance and poor sealing caused by coil short circuit.

[0026] 2. After the Alpha coil is wrapped with four layers of insulation, it can achieve insulation and sealing effects at the same time. The Alpha coil can be directly assembled with the disc-shaped iron core. The assembled stator with winding does not need to be insulated again, which simplifies the stator insulation process, saves motor space, and maximizes the lifting force of the motor.

[0027] 3. The insulation wrapping and sealing method adopted in the present invention has the advantages of simple structure and convenient wrapping operation, and adopts polyimide composite film for winding and sintering. Each layer of insulation layer is sintered after wrapping, so that the coil can withstand an AC voltage of more than 10KV, and at the same time can achieve higher heat resistance and environmental adaptability. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a schematic diagram of the structure of multiple alpha coils of the present invention;

[0029] Figure 2 A schematic diagram of wrapping the lead wire to the coil cake of an Alpha coil insulation wrapping and sealing method;

[0030] Figure 3 A schematic diagram of a coil cake to string wire wrapping method 1 of an Alpha coil insulation wrapping and sealing method;

[0031] Figure 4 A schematic diagram of a second coil cake to string wire wrapping method of an Alpha coil insulation wrapping and sealing method.

[0032] In the figure, 1 to 17 are the order of inserting and piercing the composite film; 20. first coil cake; 21. lead wire; 22. series connection wire; 23. second coil cake. DETAILED DESCRIPTION

[0033] In order to clearly illustrate the technical features of the application scheme of the present invention, the present invention is described in detail below through specific implementation methods and in conjunction with the accompanying drawings.

[0034] In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application may also be implemented in other ways different from those described herein. Therefore, the scope of protection of the present application is not limited to the specific embodiments disclosed below.

[0035] Example 1

[0036] like Figure 1 As shown, an Alpha coil insulation wrapping and sealing method comprises the following steps:

[0037] S1, wrapping the electromagnetic wire with the composite film, sintering it, and winding it into an alpha coil after cooling;

[0038] S2. Half-wrap all the series wires and lead wires in the Alpha coil with the composite film, and the half-wrap direction is from the previous coil cake to the corresponding length of the next coil cake, so as to maintain the electrical connection and insulation between the coil cakes, and then tie and fix the coil after insulation wrapping;

[0039] S3, wrapping all the Alpha coil cakes with a layer of the composite film, with the inner circle of the Alpha coil being wrapped in a half-folded manner and the outer circle of the Alpha coil being wrapped in a lapped manner;

[0040] S4, the starting point of the second layer of insulation is located at the external lead wire of the Alpha coil, and the composite film is used to continuously wrap the coil cake and the series wire until the external lead wire at the other end of the coil cake ends; in the process of wrapping the lead wire to the coil cake, the intersection between the lead wire and the coil cake is filled and wrapped; in the process of wrapping the coil cake to the series wire, the intersection between the coil cake and the series wire is filled and wrapped;

[0041] Among them, the two intersection positions are divided into four quadrants according to the separation of the coil cake, the lead wire and the series wire, the left and right sides of the series wire are the first quadrant and the second quadrant respectively, and the left and right sides of the lead wire are the third quadrant and the fourth quadrant respectively; in the process of wrapping the lead wire to the coil cake, a gap is formed between the second and third quadrants, and the composite film is first passed through the third quadrant, and the composite film is inserted into the second quadrant, and then the composite film is passed through the first quadrant, and the composite film is inserted into the second quadrant, and finally the composite film is passed through the fourth quadrant, and the coil cake can be wrapped, wherein the process of passing the composite film from the third quadrant and inserting the composite film into the second quadrant is gap filling.

[0042] S5. After the second layer of insulation wrapping is completed, the entire Alpha coil is placed in a baking furnace for sintering, so that the insulation of the Alpha coil reaches a predetermined standard;

[0043] S6, after the Alpha coil is cooled, performing a third layer and a fourth layer of insulation wrapping on the Alpha coil;

[0044] S7. After the fourth layer of insulation wrapping is completed, the entire Alpha coil is placed in a baking furnace for sintering until all insulation layers are tightly combined to achieve the best insulation effect. After the Alpha coil is insulated and wrapped, it is immersed in insulating oil. The insulating oil is heated to a certain temperature, the stator is sealed as a whole and cooled to room temperature.

[0045] In this embodiment, the composite film is a polyimide composite film, and all the series wires and lead wires of the Alpha Coil are wrapped with the polyimide composite film. The direction of the half-wrap is from the previous coil cake to the corresponding length of the next coil cake to maintain the electrical connection and insulation between the coils. After the insulation wrapping, the wires are tied and fixed.

[0046] All coil cakes are wrapped with a layer of polyimide composite film. The inner circle of the Alpha coil cake is half-overlapped, and the outer circle is overlapped. The length of the overlap is controlled between 3mm and 4mm, in order to achieve the best insulation and fixation effect for the Alpha coil; the coil is continued to be wrapped with a second layer, and the starting point of the second layer of insulation wrapping is located at the external lead-out line of the Alpha coil, and then the coil cake and the series connection line are continuously wrapped until they extend to the other end of the external lead-out line of the Alpha coil. In this wrapping process, polyimide composite film is used for wrapping, and the inner circle of the coil cake is half-overlapped, and the outer circle is overlapped by 3mm-4mm. At the same time, the lead-out line and the series connection line are both wrapped in a half-overlapping manner, so that the coil cake, the series connection line and the lead-out line form an insulating whole, thereby ensuring the insulation of the Alpha coil.

[0047] In the process of wrapping the lead wire to the coil cake, special attention should be paid to the filling and wrapping of the intersection. Filling and wrapping is performed at the intersection of the lead wire and the coil cake. This step is more important. The purpose is to ensure the stability of the coil cake and the firmness of the overall structure. The specific method of filling and wrapping is as follows: Figure 2 As shown, a gap is formed between the second quadrant and the third quadrant. The film is first penetrated from position 1 of the third quadrant and inserted into position 2 of the second quadrant. Then, the film is penetrated from position 3 of the first quadrant and inserted into position 4 of the second quadrant. Finally, the film is penetrated from position 5 of the fourth quadrant, wherein the process of penetrating the film from position 1 of the third quadrant and inserting the film at position 2 of the second quadrant is gap filling.

[0048] After the lead wire of the coil cake is wrapped, the coil cake is wrapped next. The inner circle of the coil cake is half-wrapped and the outer circle is wrapped with a layer. The length of the wrapping ranges from 3mm to 4mm. When the wrapping process reaches the position where the coil cake and the string line intersect, special filling and wrapping are required, such as Figure 3 As shown, when the next string of wires is located on the left side of the previous string of wires, a gap is formed between the second quadrant and the third quadrant, and the composite film is wrapped six times at the intersection of the coil cake and the string of wires in a penetration-insertion manner. Specifically, the film is first penetrated from position 1 of the third quadrant, and the film is inserted into position 2 of the first quadrant, and then the film is penetrated from position 3 of the fourth quadrant, and then the film is inserted into position 4 of the first quadrant. Figure 3The composite film is marked for penetration and insertion, and the penetration and insertion are repeated, wherein the process of penetrating from position 5 of the third quadrant and inserting into position 6 of the second quadrant and penetrating from position 7 of the third quadrant and inserting into position 8 of the second quadrant is gap filling.

[0049] After completing the second layer of insulation wrapping, after sintering and cooling, continue with the third and fourth layers of insulation wrapping. The insulation wrapping method of the third and fourth layers is the same as that of the first layer, in order to further consolidate and enhance the insulation effect of the coil; when the fourth layer of insulation wrapping is completed, the entire coil is placed in a baking furnace for sintering until all insulation layers are tightly combined to achieve the best insulation effect; after the Alpha coil is insulated, it needs to be immersed in insulating oil, and the insulating oil is heated to a certain temperature. The stator is sealed as a whole and cooled to room temperature. Therefore, the stator coil is in a vacuum environment. In order to ensure that the insulation performance of the Alpha coil does not decrease, the insulation sealing must be ensured during the Alpha coil insulation wrapping process to prevent motor creepage and breakdown.

[0050] Example 2

[0051] like Figure 1 As shown, an Alpha coil insulation wrapping and sealing method includes step S4, the starting point of the second layer of insulation is located at the external lead wire of the Alpha coil, the composite film is used to continuously wrap the coil cake and the string wire until the external lead wire at the other end of the coil cake ends, in the process of wrapping the lead wire to the coil cake, the intersection between the lead wire and the coil cake is filled and wrapped; in the process of wrapping the coil cake to the string wire, the intersection between the coil cake and the string wire is filled and wrapped. Figure 4 As shown, in this embodiment, when the wrapping process reaches the position where the coil cake and the string line intersect, special filling and wrapping are required, such as Figure 4 When the next string line is located on the right side of the previous string line, a gap is formed between the first quadrant and the fourth quadrant. The composite film is wrapped six times at the intersection of the coil cake and the string line in a penetration-insertion manner. Specifically, the film is first penetrated from position 1 of the third quadrant, inserted into position 2 of the first quadrant, and then penetrated from position 3 of the fourth quadrant, and then inserted into position 4 of the second quadrant. Figure 4 The composite film is marked to pass through and insert in sequence, and the passing through and inserting process is repeated, wherein the composite film passes through from the fourth quadrant 7 position to the first quadrant 8 position, and passes through from the fourth quadrant 9 position to the first quadrant 10 position for gap filling. The coil is wrapped in this way to ensure the insulation of the coil.

[0052] Example 3

[0053] like Figure 1As shown, an Alpha coil insulation wrapping and sealing method, in this embodiment, during the first layer of insulation wrapping, all coil cakes are wrapped with a layer of polyimide composite film, the inner circle is half-overlapped, and the outer circle is overlapped, and the overlap length is 3mm. At the same time, during the wrapping process from the second layer of coil cake to the series line, after the lead wire of the coil cake is wrapped, the coil cake is then wrapped. For the inner circle of the coil cake, a half-overlapping method is used, and the outer circle is also overlapped, and the overlap length is 3mm, the same as the first layer. By analogy, the outer circles of the third and fourth layers of coil cakes also use an overlap method with a length of 3mm, which improves the accuracy and consistency of the coil wrapping and maintains the stability of the coil.

[0054] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.

Claims

1. An Alpha coil insulation wrapping and sealing method, It is characterized in that The steps include: S1, wrapping the electromagnetic wire with the composite film and then sintering it, and then winding it into an alpha coil after cooling; S2. Half-wrap all the series wires and lead wires in the Alpha Coil with the composite film, wherein the half-wrap direction is from the previous coil cake to the corresponding length of the next coil cake, so as to maintain the electrical connection and insulation between the coil cakes, and then tie and fix the Alpha Coil after insulation wrapping; S3, wrapping all the Alpha coil cakes with a layer of the composite film, the inner circle of the Alpha coil is wrapped in a half-overlapping manner, and the outer circle of the Alpha coil is wrapped in a overlapping manner; S4, the starting point of the second layer of insulation wrapping is located at the external lead wire of the Alpha coil, and then the composite film is used to continuously wrap the coil cake and the string wire until the external lead wire at the other end of the coil cake ends; in the process of wrapping the lead wire to the coil cake, the intersection between the lead wire and the coil cake is filled and wrapped; in the process of wrapping the coil cake to the string wire, the intersection between the coil cake and the string wire is filled and wrapped; Among them, at the two intersection positions, four quadrants are divided according to the separation of the coil cake, the lead wire and the series wire, the left and right sides of the series wire are the first quadrant and the second quadrant respectively, and the left and right sides of the lead wire are the third quadrant and the fourth quadrant respectively; in the process of wrapping the lead wire to the coil cake, a gap is formed between the second and third quadrants, and the composite film is first penetrated from the third quadrant, and the composite film is inserted from the second quadrant, and then the composite film is penetrated from the first quadrant, and the composite film is inserted from the second quadrant, and finally the composite film is penetrated from the fourth quadrant, and the coil cake can be wrapped, wherein the process of penetrating the composite film from the third quadrant and inserting the composite film into the second quadrant is gap filling; S5. After the second layer of insulation wrapping is completed, the entire Alpha coil is placed in a baking furnace for sintering, so that the insulation of the Alpha coil reaches a predetermined standard; S6, after the Alpha coil is cooled, performing a third layer and a fourth layer of insulation wrapping on the Alpha coil; S7. After the fourth layer of insulation wrapping is completed, the entire Alpha coil is placed in a baking furnace for sintering until the insulation layers are tightly combined. After the Alpha coil is insulated and wrapped, it is immersed in insulating oil. The insulating oil is heated to a certain temperature, the stator is sealed as a whole and cooled to room temperature.

2. An Alpha coil insulation wrapping and sealing method according to claim 1, It is characterized in that The composite film is a polyimide composite film.

3. The Alpha coil insulation wrapping and sealing method according to claim 1, It is characterized in that In step S3, the length of the package is controlled to be between 3 mm and 4 mm.

4. The alpha coil insulation wrapping and sealing method according to claim 1, It is characterized in that In step S4, the composite film is used for wrapping, the inner circle of the coil cake is half-overlapped, and the outer circle is overlapped, and the overlapping length is controlled between 3mm and 4mm. At the same time, the lead wire and the series wire are both wrapped in a half-overlapping manner, and the coil cake, the lead wire and the series wire form an insulating whole.

5. The Alpha coil insulation wrapping and sealing method according to claim 4, It is characterized in that In the step S4, during the wrapping process from the coil cake to the series connection line, after the lead-out line of the coil cake is wrapped, the coil cake is wrapped again, wherein the inner circle of the coil cake is wrapped in a half-overlapping manner, and the outer circle of the coil cake is wrapped in a overlapping manner, and the overlapping length ranges from 3mm to 4mm. When the wrapping process reaches the intersection position of the coil cake and the series connection line, filling and wrapping are performed.

6. The Alpha coil insulation wrapping and sealing method according to claim 5, It is characterized in that During the filling and wrapping, when the next string of wires is located on the left side of the previous string of wires, a gap is formed between the second quadrant and the third quadrant. First, the composite film is wrapped six times at the intersection of the coil cake and the string of wires in a penetration-insertion manner, and then the composite film is penetrated from the first quadrant.

7. An Alpha coil insulation wrapping and sealing method according to claim 6, It is characterized in that The third and fourth penetration-insertion of the composite film are both penetration from the third quadrant and then insertion from the second quadrant, and the third and fourth penetration-insertion of the composite film are gap filling.

8. The Alpha coil insulation wrapping and sealing method according to claim 5, It is characterized in that During the filling and wrapping, when the next string of wires is located on the right side of the previous string of wires, a gap is formed between the first quadrant and the fourth quadrant. The composite film is firstly used to wrap the intersection of the coil cake and the string of wires eight times in a penetration-insertion manner, and then the composite film is penetrated from the first quadrant.

9. An Alpha coil insulation wrapping and sealing method according to claim 8, It is characterized in that The fourth and fifth penetration-insertion of the composite film are both penetration from the fourth quadrant and then insertion from the first quadrant, and the fourth and fifth penetration-insertion of the composite film are gap filling.

10. An Alpha coil insulation wrapping and sealing method according to claim 1, It is characterized in that In step S6, the insulation wrapping method of the third and fourth layers of the alpha coil is the same as the insulation wrapping method of the second layer.

Citation Information

Patent Citations

  • Epoxy corona-resistant polyimide film glass powder mica tape and preparation method for manufacturing rotor bar of wind driven generator from same

    CN101917080A

  • Method for producing corona discharge-preventing structure, corona discharge-preventing structure, and rotating electrical machine

    CN109075644A

  • Motor forming coil and forming method and forming system thereof

    CN113131691A

  • High-temperature-resistant stator winding structure and production process

    CN116581916A

  • Insulating tape end finishing mechanism

    JP1993276717A