Semiconductor device and method for manufacturing semiconductor device
By doping carbon on the charge storage layer of the semiconductor device and forming a tunnel layer and a channel layer, the problem of reduced conformity of the charge storage layer is solved, and electrical characteristics, especially threshold voltage distribution and deviation uniformity are improved.
Patent Information
- Application Number
- CN202380029680.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-22
- Filing Date
- 2023-03-21
- Publication Date
- 2024-11-22
AI Technical Summary
In the manufacturing process of semiconductor devices, as the number of stacks increases, the conformity of the charge storage layer decreases, resulting in a decrease in electrical characteristics, including an increase in cell threshold voltage distribution and threshold voltage deviation.
Carbon is doped on the charge storage layer, the conformity of the charge storage layer is improved by heat treatment, and a tunnel layer and a channel layer are formed thereon.
The conformity of the charge storage layer is improved, the electrical characteristics of the semiconductor device are improved, such as reducing the threshold voltage deviation between cells and the threshold voltage deviation in the upper and lower regions, and improving the uniformity of the charge storage layer.
Smart Images

Figure CN119014136A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a semiconductor device and a method for manufacturing the semiconductor device. Background Art
[0002] Semiconductor devices are mainly used as components of devices similar to electronic circuits that utilize the conductive properties of semiconductors. Semiconductors can be divided into memory semiconductors and non-memory semiconductors. Memory semiconductors can be divided into volatile memories such as dynamic random access memory (DRAM) and static random access memory (SRAM) and non-volatile memories such as mask read-only memory (Mask ROM), erasable programmable read-only memory (EPROM), electrically erasable programmable read-only memory (EEPROM) and flash memory.
[0003] Figure 1 The structure of a semiconductor device is shown.
[0004] Reference Figure 1 To manufacture the semiconductor device 1 , first, insulating layers 110 a to 110 e and gate layers 112 a to 112 e may be alternately and repeatedly deposited on the substrate 100 to form a thin film structure TS.
[0005] Then, a trench TR exposing the substrate 100 by penetrating the thin film structure TS may be formed.
[0006] When the trench TR is formed, semiconductor patterns 120, 130, 140, and 150 may be formed inside the trench TR. More specifically, an adhesion layer 120 covering at least a portion of the trench TR and a charge storage layer 130 disposed on the adhesion layer 120 may be formed inside the trench TR. In addition, a tunnel layer 140 may be formed on the charge storage layer 130. After the tunnel layer 140 is formed, the exposed portion of the substrate 100 may be covered by forming a channel layer 150.
[0007] Sure Figure 1 One of the factors affecting the electrical characteristics of the semiconductor device 1 shown is the conformality of the charge storage layer 130. The conformality of the charge storage layer 130 is represented by Figure 1 The conformality of the charge storage layer 130 can be the uniformity of the thickness of the charge storage layer 130 measured in the Z-axis direction. For example, the conformality of the charge storage layer 130 can be the ratio D2 / D1 of the thickness D1 of the charge storage layer 130 measured in the upper region of the semiconductor device 1 (for example, the region around the gate layer 112e) and the thickness D2 of the charge storage layer 130 measured in the lower region (for example, the region around the gate layer 112a). The closer D2 / D1 is to 1, the higher its conformality. The higher its conformality, the more uniform the thickness of the charge storage layer 130.
[0008] However, with the Figure 1As the number of cell stacking of the semiconductor device 1 of the structure shown, that is, the number of insulating layers 110a to 110e and gate layers 112a to 112e included in the thin film structure TS increases, the aspect ratio of the semiconductor device 1 will increase. As the aspect ratio of the semiconductor device 1 increases, the length of the charge storage layer 130 along the Z-axis direction will also become longer, so there is a problem of reduced conformality of the charge storage layer 130 during the manufacturing process of the semiconductor device 1.
[0009] When the conformality of the charge storage layer 130 is reduced, the electrical characteristics of the semiconductor device 1 may be reduced. For example, when the conformality of the charge storage layer 130 is reduced, there is a problem that the threshold voltage (VT) distribution of the cells included in the semiconductor device 1 increases. Also, when the conformality of the charge storage layer 130 is reduced, there is a problem that the deviation between the threshold voltages of the cells included in the semiconductor device 1 or the deviation between the threshold voltages of the cells in the upper region and the threshold voltages of the cells in the lower region of the semiconductor device 1 increases. Summary of the invention
[0010] Technical issues
[0011] The purpose of this specification is to improve the conformality of a charge storage layer during the manufacturing process of a semiconductor device, thereby improving the electrical characteristics of the semiconductor device.
[0012] The purpose of this specification is not limited to the above purpose, and other purposes and advantages of this specification not mentioned are more clearly understood through the embodiments of this specification described below. In addition, the purposes and advantages of this specification can be achieved through the structural elements and their combinations recorded in the scope of the invention.
[0013] Technical Solution
[0014] A method for manufacturing a semiconductor device according to an embodiment of the present invention comprises the following steps: forming a thin film structure on a substrate; forming a groove in the thin film structure; forming an adhesion layer covering at least a portion of the groove; forming a charge storage layer on the adhesion layer; doping carbon in the charge storage layer; forming a tunnel layer on the charge storage layer; and forming a channel layer covering the tunnel layer and the substrate.
[0015] A semiconductor device according to an embodiment of the present invention may include: a substrate; a thin film structure formed on the substrate; an adhesion layer covering at least a portion of a groove formed in the thin film structure; a charge storage layer formed on the adhesion layer; a tunnel layer formed on the charge storage layer; and a channel layer covering the tunnel layer and the substrate, wherein carbon is rubbed into the charge storage layer.
[0016] Effects of the Invention
[0017] In the manufacturing process of the semiconductor device, the embodiment of the present invention can improve the conformality of the charge storage layer. Therefore, the embodiment of the present invention can improve the electrical characteristics of the semiconductor device, for example, the threshold voltage distribution of the cells included in the semiconductor device, the threshold voltage deviation between the cells, and the threshold voltage deviation between the cells in the upper region and the cells in the lower region. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 The structure of a semiconductor device is shown.
[0019] Figures 2 to 4 A manufacturing process of a semiconductor device according to an embodiment of the present invention is shown. DETAILED DESCRIPTION
[0020] With reference to the accompanying drawings, the above-mentioned objects, features and advantages will be described in detail, so that ordinary technicians in the technical field to which this specification belongs can easily implement the embodiments of this specification. In the process of describing this specification, if it is determined that the specific description of the relevant known technology makes the subject of this specification unclear, the detailed description thereof will be omitted. Below, with reference to the accompanying drawings, the preferred embodiments of this specification will be described in detail. In the accompanying drawings, the same reference numerals represent the same or similar structural elements.
[0021] Figures 2 to 4 A manufacturing process of a semiconductor device according to an embodiment of the present invention is shown.
[0022] First, if Figure 2 As shown, insulating layers 210 a to 210 e and gate layers 212 a to 212 e may be alternately and repeatedly deposited on a substrate 200 , thereby forming a thin film structure TS.
[0023] In one embodiment, although the substrate 200 may be a silicon substrate, a germanium substrate, or a silicon germanium substrate, the type of the substrate 200 is not limited thereto.
[0024] In one embodiment, the insulating layers 210a to 210e may be silicon oxide films formed by a thermal oxidation process, or may be silicon oxide films formed by a deposition technique. In one embodiment, each of the insulating layers 210a to 210e may have the same thickness. In another embodiment, some of the insulating layers 210a to 210e may have different thicknesses.
[0025] In one embodiment, the gate layers 212a to 212e may include a silicon nitride film formed by a nitridation process. The gate layers 212a to 212e may be sacrificial films. That is, after the formation of the channel layer 250 described above is completed, the silicon nitride film is removed, and then a metal material such as aluminum (Al), copper (Cu), and tungsten (W) is deposited on the gate layers 212a to 212e.
[0026] In one embodiment, the insulating layers 210 a to 210 e and the gate layers 212 a to 212 e may be formed by thermal chemical vapor deposition (Thermal CVD), plasma enhanced chemical vapor deposition (Plasma enhanced CVD), physical chemical vapor deposition (physical CVD) or atomic layer deposition (Atomic Layer Deposition; ALD) processes.
[0027] Then, a thin film structure TS in which the trench TR is exposed by penetrating the substrate 200 may be formed. When viewed from a planar perspective, the trench TR may be formed two-dimensionally on the upper surface of the thin film structure TS. In one embodiment, the trench TR may be formed by the following steps: forming a first mask pattern (not shown) having a plurality of openings, the openings defining an area on the thin film structure TS where the trench TR is formed; and anisotropically etching the thin film structure TS using the first mask pattern (not shown) as an etching mask. The first mask pattern may be made of a material that is selective to the insulating layers 210a to 210e and the gate layers 212a to 212e. The upper surface of the substrate 200 may be overetched by an etching process, thereby causing the upper portion of the substrate 200 to be recessed.
[0028] Then, an adhesion layer 220 may be formed to cover at least a portion of the trench TR and expose the substrate 100. The adhesion layer 220 may include a high dielectric layer (eg, a metal oxide such as aluminum hydroxide or hafnium oxide) having a higher dielectric constant than the tunnel dielectric layer.
[0029] Then, a charge storage layer 230 may be formed on the adhesion layer 220. The charge storage layer 230 may include a dielectric material having a well capable of storing charges, for example, nitride such as silicon nitride (SiN) and / or metal oxide.
[0030] Then, if Figure 3 As shown, carbon may be doped in the charge storage layer 230. In one embodiment, the carbon compound 300 may be supplied to a chamber in which a semiconductor device 2 is prepared, and the semiconductor device 2 is formed with the charge storage layer 230. In one embodiment, the carbon compound 300 supplied to the chamber may include CH4, C2H4, C2H6, C3H7, C3H8, iC4H 10 、nC4H 10 、nC5H 12、C6H6、C6H 12 、C7H8、C8H 18 , C 10 H 22 and C 12 H 26 At least one of .
[0031] In one embodiment, the atmosphere may be provided into the chamber in which the semiconductor device 2 is prepared. The atmosphere provided into the chamber may be one of H2, D2 and N2.
[0032] When the carbon compound 300 is supplied into the chamber, the pressure in the chamber is set to a preset process pressure, and a heat treatment may be performed on the semiconductor device 2. In one embodiment, the process pressure may be determined within a range of 1 atmosphere to 100 atmospheres. Also, when the heat treatment is performed, the temperature in the chamber, that is, the process temperature may be determined within a range of 400° C. to 600° C.
[0033] When the charge storage layer 230 is doped with carbon through the above-described process, the semiconductor device 2 can be transferred from the chamber to the outside. Figure 3 The carbon compound 300 is shown.
[0034] In the state where the carbon compound 300 is removed, as Figure 4 As shown, a tunnel layer 240 may be formed on the charge storage layer 230. The tunnel layer 240 may include oxide and / or oxidized nitride, etc.
[0035] Then, a channel layer 250 may be formed between the tunnel layers 240. The channel layer 250 may cover the substrate 200 exposed at the lower portion of the trench TR. In one embodiment, the channel layer 250 may include an oxide such as polysilicon.
[0036] exist Figure 4 FIG. 2 shows a semiconductor device 2 of an embodiment produced by the above-described process. Figure 4 In the illustrated embodiment, the semiconductor device 2 includes cells CL1 to CL5 stacked in five layers. However, the number of stacked cells of the semiconductor device 2 may vary according to the embodiment.
[0037] Each of the cells CL1 to CL5 included in the semiconductor device 2 has a stacked structure including gate layers 212a to 212e and semiconductor patterns 220, 230, 240, 250. For example, Figure 4As shown, the first cell CL1 includes a gate layer 212a, an adhesion layer 220, a charge storage layer 230, a tunnel layer 240 and a channel layer 250 stacked in sequence. The second cell CL2 to the fifth cell CL5 may also have the same stacked structure as the first cell CL1. The charge storage layer 230 may contain carbon through the carbon doping process as described above.
[0038] As described above, according to an embodiment of the present invention, after forming the charge storage layer 230, a carbon doping process is performed on the charge storage layer 230. When carbon is doped in the charge storage layer 230, the conformality of the charge storage layer 230 can be improved and the electrical characteristics of the semiconductor device 2 can be improved.
[0039] First, the distribution of the threshold voltage of each cell included in the semiconductor device 2 can be improved. Table 1 shows the results of measuring the threshold voltage of each cell of the semiconductor device 2 manufactured by changing the process pressure when the carbon doping process is performed on the charge storage layer 230 according to the above-mentioned embodiment. In Table 1, "non-doping" is the threshold voltage data of the cell included in the semiconductor device in which the carbon doping process is not performed on the charge storage layer 230.
[0040] Table 1
[0041]
[0042] As shown in Table 1, the results of measuring the threshold voltage of each cell included in the semiconductor device in which the charge storage layer 230 does not contain carbon have a minimum value of 1, a maximum value of 2.3, and a distribution of 1.3. In contrast, according to the above embodiment, the distribution of the threshold voltage of each cell included in the semiconductor device in which the charge storage layer 230 is subjected to a carbon doping process is less than 1.3. Therefore, compared with the semiconductor device in which the charge storage layer 230 does not contain carbon, the semiconductor device in which the charge storage layer 230 contains carbon has a higher cell uniformity.
[0043] Also, as shown in Table 1, when the charge storage layer 230 is subjected to a carbon doping process, as the pressure in the chamber, ie, the process pressure, increases, the distribution of the threshold voltages of the cells included in the semiconductor device decreases and the uniformity increases.
[0044] Furthermore, as shown in the above-mentioned embodiment, when the carbon doping process is performed on the charge storage layer 230, the conformality of the charge storage layer 230 is higher than when the carbon doping process is not performed on the charge storage layer 230. That is, when the carbon doping process is performed on the charge storage layer 230, the thickness of the charge storage layer 230 measured in the Z-axis direction becomes uniform. Therefore, the deviation between the threshold voltages of the cells included in the semiconductor device 2 including carbon in the charge storage layer 230 can be reduced, thereby improving the cell uniformity.
[0045] Furthermore, since the conformality of the charge storage layer 230 is improved by performing a carbon doping process on the charge storage layer 230, the deviation between the threshold voltage of the cell configured in the upper region of the semiconductor device 2 (for example, the 5th cell CL5 or the 4th cell CL4) and the threshold voltage of the cell configured in the lower region of the semiconductor device 2 (for example, the first cell CL1 or the second cell CL2) can be reduced, thereby improving the cell uniformity.
[0046] As described above, this specification is described with reference to the illustrated drawings, but this specification is not limited to the embodiments and drawings disclosed in this specification, and a person skilled in the art of the present invention can make various modifications. Moreover, in the process of describing the embodiments of this specification, although the effects based on the structure of this specification are not explicitly recorded, it should be recognized that the effects can be predicted by the structure.
Claims
1. A method for manufacturing a semiconductor device, characterized in that: The steps include: forming a thin film structure on a substrate; forming a groove in the thin film structure; forming a barrier layer covering at least a portion of the trench; forming a charge storage layer on the blocking layer; doping carbon into the charge storage layer; forming a tunnel layer on the charge storage layer; as well as A channel layer is formed covering the tunnel layer and the substrate.
2. The method for manufacturing a semiconductor device according to claim 1, wherein: The step of doping carbon in the charge storage layer comprises the following steps: When forming the charge storage layer, supplying a carbon compound into a chamber in which the semiconductor device is prepared; and The semiconductor device is subjected to heat treatment in a state where the pressure in the chamber is set to a predetermined process pressure.
3. The method for manufacturing a semiconductor device according to claim 2, wherein: The above-mentioned preset process pressure is determined within the range of 1 atmosphere to 100 atmospheres.
4. The method for manufacturing a semiconductor device according to claim 2, wherein: An ambient gas is provided into the chamber, and the ambient gas is one of H2, D2 and N2.
5. The method for manufacturing a semiconductor device according to claim 2, wherein: The process temperature of the heat treatment in the chamber is determined to be in the range of 400° C. to 600° C.
6. The method for manufacturing a semiconductor device according to claim 2, wherein: The above carbon compounds include CH4, C2H4, C2H6, C3H7, C3H8, iC4H 10 、nC4H 10 、nC5H 12 、C6H6、C6H 12 、C7H8、C8H 18 , C 10 H 22 and C 12 H 26 At least one of .
7. A semiconductor device, characterized in that: include: substrate; A thin film structure is formed on the substrate; a barrier layer covering at least a portion of the groove formed in the thin film structure; A charge storage layer formed on the blocking layer; a tunnel layer formed on the charge storage layer; and a channel layer covering the tunnel layer and the substrate, The charge storage layer is doped with carbon.
8. The semiconductor device according to claim 7, characterized in that When the charge storage layer is formed, a carbon compound is supplied into a chamber in which the semiconductor device is prepared, and a heat treatment is performed on the semiconductor device in a state where the pressure in the chamber is set to a preset process pressure.
9. The semiconductor device according to claim 8, characterized in that The above-mentioned preset process pressure is determined within the range of 1 atmosphere to 100 atmospheres.
10. The semiconductor device according to claim 8, characterized in that An ambient gas is provided into the chamber, and the ambient gas is one of H2, D2 and N2.
11. The semiconductor device according to claim 8, characterized in that The process temperature of the heat treatment in the chamber is determined to be in the range of 400° C. to 600° C.
12. The semiconductor device according to claim 8, characterized in that The above carbon compounds include CH4, C2H4, C2H6, C3H7, C3H8, iC4H 10 、nC4H 10 、nC5H 12 、C6H6、C6H 12 、C7H8、C8H 18 , C 10 H 22 and C 12 H 26 At least one of .