Waterproof eye shadow and preparation method thereof
By using waterproof eyeshadow formulas such as talc powder and water-based wax film-forming polymers, the existing eyeshadow's shortcomings in waterproof performance and durability are solved, and the makeup is not easy to fall off and long-term in humid environments. The lasting effect improves the user experience.
Patent Information
- Application Number
- CN202411510662.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-28
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-10-28
AI Technical Summary
Existing eyeshadow products have shortcomings in waterproofing and durability, especially in wet or sweaty environments, and it is difficult to maintain long-term makeup effects.
It adopts a waterproof eye shadow formula composed of talc powder, light calcium carbonate, barium sulfate, mica powder, silica, kaolin and other filled powders and aqueous wax film-forming polymers, emulsifiers, oils, antioxidants, preservatives, etc. Lightweight, easy to apply, waterproof and anti-smudge-resistant eyeshadows are prepared by specific grinding and stirring steps.
It achieves waterproofness and long-lasting makeup effects that keep the makeup from falling off in a humid environment, improves the anti-smudge effect and user experience of eyeshadows, and ensures the neatness and beauty of eye makeup.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of cosmetics, in particular to a waterproof eye shadow and a preparation method thereof. Background Art
[0002] With the development of society and the improvement of people's living standards, cosmetics have become an indispensable part of modern women's daily life. In particular, eye shadow, as an important cosmetic for modifying and beautifying the eyes, has a growing market demand. However, while the existing eye shadow products on the market meet the aesthetic requirements, there are still some defects and deficiencies, especially in terms of waterproof performance and durability. Summary of the invention
[0003] Based on the deficiencies of the prior art, the present invention provides a waterproof eye shadow and a preparation method thereof.
[0004] To achieve the above objectives, the present invention is implemented through the following technical solutions: A waterproof eye shadow comprises the following components by weight: 50-70 parts of filling powder, 12-16 parts of water-based wax film-forming polymer, 5-15 parts of colorant, 5-15 parts of oil, 2-4 parts of emulsifier, 0.5-2 parts of antioxidant and 0.5-2 parts of preservative.
[0005] The filling powder is composed of 20-30 parts of talc powder, 10-20 parts of light calcium carbonate, 0-5 parts of barium sulfate, 5-15 parts of mica powder, 2-10 parts of silicon dioxide and 2-5 parts of kaolin by weight.
[0006] The talc has a lower density and can provide a light texture, making the eye shadow easy to apply and not thick. The talc can improve the skin feel and provide a soft and silky touch; light calcium carbonate can provide covering power, help the eye shadow color to be fuller, and increase the brightness and whiteness of the eye shadow if necessary; barium sulfate is heavier, which helps the eye shadow to adhere to the eyelid, reduces the flying powder phenomenon, and can provide a covering effect, making the color look fuller; mica powder can reflect light, bring gloss to the eye shadow, and increase the three-dimensional sense and visual appeal of the eye shadow; silicon dioxide can improve the fluidity of the eye shadow, making the eye shadow easier to distribute evenly, and helping to maintain the light texture of the eye shadow; kaolin can absorb excess skin oil, reduce the smudging and removal of eye shadow, help the eye shadow to adhere better to the skin, and improve durability.
[0007] The aqueous wax film-forming polymer is composed of 4-8 parts of beeswax, 0.5-2 parts of citric acid, 0.5-3 parts of polysorbate, 1-5 parts of acrylic acid (ester) / stearyl alcohol polyether-20 methacrylate copolymer and 2-5 parts of water by weight.
[0008] The aqueous wax film-forming polymer can form a protective film on the skin surface, which helps to improve the waterproof and anti-fading properties of eye shadow, can give the eye shadow a natural luster and silky texture, can maintain its color and integrity, and is not easy to remove or fade. In addition, the film formed by the copolymer is flexible and elastic, which helps the eye shadow remain intact when the facial expression changes.
[0009] The colorant is a combination of one or more of red iron oxide, lycopene, beetroot red, sodium copper chlorophyll, purple cabbage, ultramarine, caramel color, titanium dioxide, and pearlescent agent.
[0010] The oil is a combination of one or more of sunflower oil, safflower oil, castor oil, coconut oil, grape seed oil, olive oil and palm oil.
[0011] The emulsifier is composed of 0.5 to 2 parts of polydimethylsiloxane / vinyl polydimethylsiloxane cross-linked polymer, 0.5 to 2 parts of magnesium stearate, and 0.5 to 1 part of sodium polyacrylate, by weight. The combination of these emulsifiers ensures that the formula of the waterproof eye shadow can be evenly mixed to form a stable paste with excellent spreadability, stability and waterproofness.
[0012] The antioxidant is composed of 0.2-1 part of tocopherol, 0.2-1 part of vitamin E plant and 0.1-0.5 part of steryl isostearate by weight.
[0013] The preservative consists of 0.1-1 part of phenoxyethanol, 0.1-1 part of potassium sorbate and 0.1-1 part of tea tree oil by weight.
[0014] The method for preparing the waterproof eye shadow comprises the following steps: S1: Heat the beeswax and control the temperature at 62-68°C until the beeswax is completely melted into a liquid state, add citric acid, maintain the temperature at which the beeswax melts, stir for 10-18 minutes, and set the stirring speed at 200-400 rpm. Add polysorbate, acrylates / stearyl alcohol polyether-20 methacrylate copolymer and water, control the temperature at 60-65°C, stir for 5-10 minutes, and stir at a speed of 200-300 rpm. After stirring evenly, a water-based wax film-forming polymer is formed. Control the temperature at 60-65°C, add oil and emulsifier, stir for 15-20 minutes, and increase the stirring speed to 800-1100 rpm to form a stable emulsified system. Control the temperature and rotation speed unchanged, add antioxidants and preservatives, and stir for 3-5 minutes to ensure uniform distribution to obtain a water eyeshadow base.
[0015] S2: talcum powder, light calcium carbonate, sulfuric acid, mica powder, silicon dioxide and kaolin are mixed evenly and ground by a grinder. The mixed raw materials are finely ground by a grinder and sieved with a 200-mesh screen to obtain a filling powder.
[0016] S3: preheat the water eyeshadow base obtained in step S1 to 40°C to 50°C, add the filling powder to the preheated water eyeshadow base, stir at a speed of 200 to 400 rpm, stir for 10 to 20 minutes, then set the stirring speed to 100 to 150 rpm, slowly add the colorant, stir for 15 to 20 minutes, increase the stirring speed to 400 to 600 rpm, stir for 30 to 40 minutes, and obtain a uniform paste and waterproof eyeshadow.
[0017] The present invention provides a waterproof eye shadow and a preparation method thereof, which has the following beneficial effects: 1. The waterproof eyeshadow of the present invention has excellent waterproof properties due to its special formula and preparation method. It can keep the makeup from falling off even in a humid or sweaty environment, and is suitable for users who go out for a long time or need a long-lasting makeup effect.
[0018] 2. The present invention adopts a unique combination of emulsifier and oil, so that the eye shadow has a good anti-smudge effect, which can effectively prevent the color from spreading on the skin and ensure the neatness and beauty of the eye makeup.
[0019] 3. The carefully selected filling powder and water-based synthetic film polymer of the present invention make the eye shadow light in texture, easy to apply, not easy to remove or fade, and bring a silky touch, thereby improving the user experience. DETAILED DESCRIPTION
[0020] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Example 1
[0021] A waterproof eye shadow, wherein the components and their corresponding weight parts are shown in the formula table 1, the filling powder component table 2 and the water-based wax film-forming polymer component table 3, and is prepared by the following steps: S1: Place beeswax in a heating container and gradually heat it to 62°C to 68°C, maintaining the temperature until the beeswax is completely melted into a liquid state. After the beeswax melts, add a predetermined amount of citric acid to it, maintain the temperature within the range of 62°C to 68°C, continue stirring for 10 to 18 minutes, and set the stirring speed to 200 to 400 rpm. Then add polysorbate, acrylates / stearyl alcohol polyether-20 methacrylate copolymer and water in sequence, control the temperature between 60°C and 65°C, continue stirring for 5 to 10 minutes, and adjust the stirring speed to 200 to 300 rpm until the mixture is evenly mixed to form a water-based wax film-forming polymer. Lower the temperature of the water-based wax film-forming polymer to 60°C to 65°C, then add oils and emulsifiers, increase the stirring speed to 800 to 1100 rpm, and continue stirring for 15 to 20 minutes to form a stable emulsified system. Keeping the current temperature and speed unchanged, add antioxidants and preservatives, and continue stirring for 3 to 5 minutes to ensure that all ingredients are evenly distributed to obtain the desired water eyeshadow base.
[0022] S2: Mix talcum powder, light calcium carbonate, sulfuric acid, mica powder, silicon dioxide and kaolin evenly, and grind them through a grinder to ensure that the particles are fine and uniform. Grind the ground materials through a grinder, and use a 200-mesh sieve to obtain filling powder.
[0023] S3: Preheat the water eyeshadow base obtained in step S1 to 40°C to 50°C, add the filling powder obtained in step S2 to the preheated water eyeshadow base, stir at a speed of 200 to 400 rpm, stir for 10 to 20 minutes, and ensure that the filling powder and the water eyeshadow base are fully mixed. Then set the stirring speed to 100 to 150 rpm, slowly add the colorant, stir for 15 to 20 minutes, increase the stirring speed to 400 to 600 rpm, stir for 30 to 40 minutes, and obtain a uniform paste and waterproof eyeshadow.
[0024] The waterproof eye shadow prepared in Example 2-10 has the same preparation method and operating conditions as Example 1. The difference from Example 1 is that the components and their corresponding weight parts are shown in the formula table 1, the filler powder component table 2, the water-based wax film-forming polymer component table 3 and the emulsifier component table 4: Table 1 Components Example 1 Example 2 Example 3 Example 4 Example 5 Example 6 Example 7 Example 8 Example 9 Example 10 Filling powder 65 servings 70 servings 60 servings 55 servings 50 servings 58 servings 62 servings 69 copies 65 servings 52 servings Water-based wax film-forming polymer 14 servings 16 servings 15 servings 16 servings 12 servings 14 servings 16 servings 12 servings 13 servings 15 servings Colorants 12 servings 15 servings 10 servings 8 servings 5 servings 6 servings 13 servings 7 servings 14 servings 11 servings grease 12 servings 15 servings 10 servings 8 servings 5 servings 6 servings 13 servings 7 servings 7 servings 11 servings Emulsifier 2.5 servings 4 servings 2.7 servings 4 servings 2 servings 3.1 serving 3.5 servings 2.8 servings 3.9 servings 3.2 servings Antioxidants 0.75 serving 2 servings 1 serving 1.5 servings 0.5 serving 1.25 servings 1.75 servings 0.9 parts 2 servings 1.1 serving preservative 0.75 serving 2 servings 1 serving 1.5 servings 0.5 serving 1.25 servings 1.75 servings 0.9 parts 2 servings 1.1 serving Table 2 Example talcum powder Light calcium carbonate Barium sulfate Mica powder Silicon dioxide Kaolin 1 25 servings 20 servings 1 serving 15 servings 2 servings 2 servings 2 30 servings 15 servings 3 servings 12 servings 6 servings 4 servings 3 28 servings 10 servings 5 servings 10 servings 5 servings 2 servings 4 22 servings 12 servings 2 servings 11 servings 5 servings 3 servings 5 20 servings 13 servings 2 servings 10 servings 3 servings 2 servings 6 26 servings 15 servings 3 servings 5 servings 8 servings 4 servings 7 24 servings 18 servings 4 servings 11 servings 2 servings 3 servings 8 30 servings 10 servings 5 servings 9 servings 10 servings 5 servings 9 28 servings 10 servings 3 servings 13 servings 7 servings 4 servings 10 25 servings 13 servings 2 servings 6 servings 4 servings 2 servings Table 3 Example beeswax Citric acid Polysorbate Acrylates / Steareth-20 Methacrylate Copolymer water 1 4 servings 1.4 servings 1.7 servings 2.9 servings 4 servings 2 6 servings 2 servings 2 servings 3.5 servings 2.5 servings 3 7 servings 0.5 serving 3 servings 1.5 servings 3 servings 4 8 servings 0.5 serving 1.5 servings 2 servings 4 servings 5 4 servings 0.5 serving 1 serving 5 servings 1.5 servings 6 5 servings 0.6 parts 2 servings 4.4 servings 2 servings 7 7 servings 0.5 serving 3 servings 1 serving 4.5 servings 8 4 servings 0.8 parts 1 serving 2.7 servings 3.5 servings 9 4.5 servings 1 serving 1 serving 3.5 servings 3 servings 10 6.5 servings 2 servings 1 serving 3.5 servings 2 servings Table 4 Example Dimethicone / Vinyl Dimethicone Crosspolymer Magnesium Stearate Sodium polyacrylate 1 0.5 serving 1 serving 1 serving 2 1.8 servings 1.5 servings 0.7 parts 3 1.5 servings 0.5 serving 0.7 parts 4 2 servings 1 serving 1 serving 5 1 serving 0.5 serving 0.5 serving 6 1.2 servings 1.1 serving 0.8 parts 7 1.8 servings 1.2 servings 0.5 serving 8 1.4 servings 0.9 parts 0.5 serving 9 1.4 servings 1.5 servings 1 serving 10 1 serving 1.3 servings 0.9 parts Comparative Example 1 The main difference between Comparative Example 1 and Example 1 is that barium sulfate is not used in step S2 of Comparative Example 1. In addition, Comparative Example 1 is consistent with Example 1 in other aspects, including but not limited to raw material ratio, preparation method, operating conditions, etc., and all follow the specific steps and parameters described in Example 1.
[0025] Comparative Example 2 The main difference between Comparative Example 2 and Example 1 is that mica powder is not used in step S2 of Comparative Example 2. In addition, Comparative Example 2 is consistent with Example 1 in other aspects, including but not limited to raw material ratio, preparation method, operating conditions, etc., and all follow the specific steps and parameters described in Example 1.
[0026] Comparative Example 3 The main difference between Comparative Example 3 and Example 1 is that silicon dioxide is not used in step S2 of Comparative Example 3. In addition, Comparative Example 3 is consistent with Example 1 in other aspects, including but not limited to raw material ratio, preparation method, operating conditions, etc., and all follow the specific steps and parameters described in Example 1.
[0027] Comparative Example 4 The main difference between Comparative Example 4 and Example 1 is that kaolin is not used in step S2 of Comparative Example 4. In addition, Comparative Example 4 is consistent with Example 1 in other aspects, including but not limited to raw material ratio, preparation method, operating conditions, etc., and all follow the specific steps and parameters described in Example 1.
[0028] Comparative Example 5 The main difference between Comparative Example 5 and Example 1 is that no emulsifier is used in step S1 of Comparative Example 5. In addition, Comparative Example 5 is consistent with Example 1 in other aspects, including but not limited to raw material ratio, preparation method, operating conditions, etc., and all follow the specific steps and parameters described in Example 1.
[0029] Comparative Example 6 The main difference between Comparative Example 6 and Example 1 is that no emulsifier is used in step S1 of Comparative Example 6, and polyvinyl alcohol is used instead of acrylic acid (ester) / stearyl alcohol polyether-20 methacrylate copolymer. Apart from this, Comparative Example 6 is consistent with Example 1 in other aspects, including but not limited to the raw material ratio, preparation method, operating conditions, etc., all following the specific steps and parameters described in Example 1.
[0030] Comparative Example 7 The main difference between Comparative Example 7 and Example 1 is that in step S1 of Comparative Example 7, beeswax is placed in a heating container, gradually heated to 62°C to 68°C, and the temperature is maintained until the beeswax is completely melted into a liquid state, citric acid, polysorbate, acrylic acid (ester) / stearyl alcohol polyether-20 methacrylate copolymer is not added, water is added, the temperature is controlled between 60°C and 65°C, stirring is continued for 5 to 10 minutes, the stirring speed is 200 to 300 rpm, and then oil and emulsifier are added, the stirring speed is increased to 800 to 1100 rpm, and stirring is continued for 15 to 20 minutes to form a stable emulsified system. In addition, Comparative Example 7 is consistent with Example 1 in other aspects, including but not limited to the raw material ratio, preparation method, operating conditions, etc., all of which follow the specific steps and parameters described in Example 1.
[0031] Product experience evaluation test: A total of 50 volunteers aged 18-30 were selected to test the waterproof eye shadows prepared in Examples 1-10 and Comparative Examples 1-7, and the waterproof durability, anti-smudge effect, smoothness, lightness and makeup effect were scored. The scores were all 1-10 points. The higher the score, the better the experience. The scores were recorded and the average value was recorded in Table 5: Table 5 Group Waterproof durability Anti-smudge effect Smooth feeling Lightness Makeup effect Example 1 9.3 9.6 9.4 9.3 9.4 Example 2 9.4 9.5 9.2 9.4 9.6 Example 3 9.5 9.4 9.1 9.4 9.0 Example 4 9.7 8.9 9.3 9.4 8.8 Example 5 9.8 9.4 9.2 9.1 8.9 Example 6 9.4 9.5 8.9 9.1 9.1 Example 7 9.7 9.3 9.2 9.0 9.5 Example 8 9.1 9.2 8.8 9.2 9.1 Example 9 9.0 9.4 8.9 9.3 9.5 Example 10 9.4 9.6 9.1 9.4 9.0 Comparative Example 1 9.4 8.0 9.3 9.4 8.1 Comparative Example 2 9.3 9.5 9.4 9.2 8.3 Comparative Example 3 9.0 8.7 9.1 8.2 7.6 Comparative Example 4 8.9 8.2 9.2 7.3 9.0 Comparative Example 5 6.8 8.4 7.6 6.9 7.7 Comparative Example 6 7.1 8.5 9.5 9.2 8.7 Comparative Example 7 6.7 8.1 7.9 8.8 7.3 Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A waterproof eye shadow, characterized in that: The composition includes the following components by weight: 50-70 parts of filling powder, 12-16 parts of water-based wax film-forming polymer, 5-15 parts of colorant, 5-15 parts of oil, 2-4 parts of emulsifier, 0.5-2 parts of antioxidant and 0.5-2 parts of preservative.
2. A waterproof eye shadow according to claim 1, characterized in that: The filling powder is composed of 20-30 parts of talc powder, 10-20 parts of light calcium carbonate, 0-5 parts of barium sulfate, 5-15 parts of mica powder, 2-10 parts of silicon dioxide and 2-5 parts of kaolin by weight.
3. The waterproof eye shadow according to claim 1, characterized in that: The aqueous wax film-forming polymer is composed of 4 to 8 parts of beeswax, 0.5 to 2 parts of citric acid, 0.5 to 3 parts of polysorbate, 1 to 5 parts of acrylic acid (ester) / stearyl alcohol polyether-20 methacrylate copolymer and 2 to 5 parts of water in parts by weight.
4. The waterproof eye shadow according to claim 1, characterized in that: The colorant is a combination of one or more of red iron oxide, lycopene, beetroot red, sodium copper chlorophyll, purple cabbage, ultramarine, caramel color, titanium dioxide, and pearlescent agent.
5. The waterproof eye shadow according to claim 1, characterized in that: The oil is a combination of one or more of sunflower oil, safflower oil, castor oil, coconut oil, grape seed oil, olive oil and palm oil.
6. The waterproof eye shadow according to claim 1, characterized in that: The emulsifier is composed of 0.5 to 2 parts of polydimethylsiloxane / vinyl polydimethylsiloxane cross-linked polymer, 0.5 to 2 parts of magnesium stearate and 0.5 to 1 part of sodium polyacrylate by weight.
7. The waterproof eye shadow according to claim 1, characterized in that: The antioxidant is composed of 0.2-1 part of tocopherol, 0.2-1 part of vitamin E plant and 0.1-0.5 part of steryl isostearate by weight.
8. The waterproof eye shadow according to claim 1, characterized in that: The preservative consists of 0.1-1 part of phenoxyethanol, 0.1-1 part of potassium sorbate and 0.1-1 part of tea tree oil by weight.
9. Preparation of the waterproof eyeshadow according to any one of claims 1 to 8, characterized in that: The preparation method comprises: S1: heating beeswax, controlling the temperature at 62-68°C, until the beeswax completely becomes liquid, adding citric acid, maintaining the temperature at which the beeswax melts, stirring for 10-18 minutes, stirring at a speed of 200-400 rpm, adding polysorbate, acrylates / stearyl alcohol polyether-20 methacrylate copolymer and water, controlling the temperature at 60-65°C, stirring for 5-10 minutes, stirring at a speed of 200-300 rpm, stirring evenly to form a water-based wax film-forming polymer, controlling the temperature at 60-65°C, adding oil and emulsifier, stirring for 15-20 minutes, increasing the stirring speed to 800-1100 rpm, forming a stable emulsified system, controlling the temperature and speed to remain unchanged, adding antioxidants and preservatives, stirring for 3-5 minutes, and obtaining a water eyeshadow base; S2: talcum powder, light calcium carbonate, sulfuric acid, mica powder, silicon dioxide and kaolin are mixed evenly and ground by a grinder. After grinding, a 200-mesh sieve is used to obtain a filling powder; S3: Preheat the water eyeshadow base to 40°C-50°C, add the filling powder to the preheated water eyeshadow base, stir at a speed of 200-400rpm, stir for 10-20min, then set the stirring speed to 100-150rpm, slowly add the colorant, stir for 15-20min, increase the stirring speed to 400-600rpm, stir for 30-40min, and obtain a uniform paste and waterproof eyeshadow.
Citation Information
Patent Citations
Sunscreen lotion and preparation method thereof
CN107362096A
Eye shadow suitable for sensitive skin
CN110169938A
Water-soluble colored modeling hair wax with matte texture and preparation method of hair wax
CN110664634A
Waterproof eye shadow powder with metallic light perception and preparation method thereof
CN110801408A
Water-in-silicon-oil elastic highlight eye shadow and preparation method thereof
CN112006941A