Welding control method and device for arc striking and arc extinguishing and storage medium

By employing a two-stage variable acceleration control method to manage welding parameters and wire feed speed in gas metal arc welding, the problems of arc ignition and wire breakage have been solved, improving welding quality and production efficiency in frequent welding scenarios.

CN119016837APending Publication Date: 2024-11-26PANASONIC WELDING SYST TANGSHAN
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411178077.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

Existing technologies, when the motor speed is high, result in a long arc ignition time for gas metal arc welding, which can easily lead to problems such as arc ignition, prolonged short circuits, and wire breakage, affecting welding quality and production cycle time. This is especially true in frequent welding scenarios such as compressor spot welding, where high product qualification rates are required.

Method used

A two-stage variable acceleration control method is adopted. During the arc initiation and arc termination stages of gas metal arc welding, the welding parameters and wire feed speed are adjusted by two-stage variable acceleration to ensure synchronous updating of current and voltage commands and match the motor speed with the output energy of the welding power supply.

Benefits of technology

It improves the arc initiation and termination performance of the welding power source, avoids problems such as arc ignition and wire breakage, and ensures the consistency of welding quality and the stability of production cycle.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119016837A_ABST
    Figure CN119016837A_ABST
Patent Text Reader

Abstract

The invention discloses an arc striking and arc extinguishing welding control method and device and a storage medium, and the control method comprises the steps that in the arc striking stage of gas metal arc welding, a welding parameter instruction and a wire feeding instruction are accelerated from a slow wire feeding speed to a main welding wire feeding speed in a two-section type variable acceleration mode; in the arc suppression stage of gas metal arc welding, the welding parameter instruction and the wire feeding instruction are decelerated from the main welding wire feeding speed to the burn-back wire feeding speed in a two-section type variable acceleration mode. The arc striking and arc extinguishing performance of the welding power source is improved through the arc striking and arc extinguishing method controlled by the variable acceleration.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of consumable arc welding, and in particular relates to a welding control method, device and storage medium for arc starting and arc ending. Background Art

[0002] With the development of welding technology, gas shielded arc welding is increasingly used in actual welding operations, and the technology is becoming more and more mature. The arc starting and arc ending process of gas shielded arc welding is divided into two parts. One is the process of the motor feeding the welding wire, and the other is that the electric welder continuously updates the parameters to the set current parameters. After the welding gun switch is closed, the motor starts to rotate and accelerate to the slow wire feeding stage, and the welding wire is slowly fed out of the conductive nozzle. When the welding wire contacts the base material to generate current, it begins to rotate at a large acceleration to the main welding wire feeding speed value. After reaching the main welding, the wire feeding instruction no longer changes. When the welding gun switch is released, the motor begins to decelerate to the burn-back wire feeding speed. After the burn-back process is completed, the motor speed is reduced to zero. In this process, the electric welder also synchronously updates the welding parameters to match the actual wire feeding speed, otherwise the arc will burn up, the arc will break, and other phenomena will occur, affecting the welding quality. The conventional gas shielded welding arc starting and arc ending control schematic diagram can be referred to Figure 1 .

[0003] Figure 1 The conventional schematic diagram of arc starting and arc ending control of gas shielded welding is explained as follows: Mot_Acc0 is the acceleration used for motor speed control in the arc starting stage; Parm_Acc0 is the acceleration used for updating welding parameters in the arc starting stage; Mot_Acc2 is the acceleration used for motor speed control in the arc ending stage; Parm_Acc2 is the acceleration used for updating welding parameters in the arc ending stage; SlowSpd is the slow wire feeding speed; MainSpd is the main welding wire feeding speed; BrunSpd is the burn-back wire feeding speed.

[0004] Figure 2 and Figure 3 The changes of various parameters in the arc striking and arc ending stages are further explained. Figure 2 From top to bottom, they are M02-welding machine parameter update acceleration, M01-wire feeding command acceleration, M03-current command and M04-voltage command. After current is detected, M01 accelerates to the predetermined speed according to the predetermined value, and M02 accelerates synchronously. The M03 current command and M04 voltage command are updated according to the real-time value of M02. Figure 3 From top to bottom are M01-wire feeding instruction, M02-parameter update instruction, M03-current instruction and M04-voltage instruction. When the welding gun is released, M01 and M02 are synchronously decelerated to the burn-back wire feeding speed, and the M03 current instruction and M04 voltage instruction are updated according to the value of M02. After the burn-back process is completed, the motor speed drops to zero and the welding machine parameters return to the initial values.

[0005] In some special industries, the welding performance requirements for arc initiation and arc extinguishing are very high. For example, spot welding of compressors usually completes welding within 1.5 seconds, and arc initiation and arc extinguishing actions are frequently performed, and the product qualification rate requirements are also very strict. In some welding industries, such as three-spot welding or six-spot welding of compressors, frequent arc initiation and extinguishing are required, and the product qualification rate requirements are very high, or some industries require high-frequency spot welding. Therefore, designing a special arc initiation and arc extinguishing control method is a technical problem that needs to be solved urgently.

[0006] With current technology, when the motor speed is high, the arc striking time is long, which makes it easy for the arc to ignite, the welding wire to hit the base material without melting due to long-term short circuit, and the welding wire to break, resulting in secondary arc striking that affects the welding quality and production rhythm. Summary of the invention

[0007] The purpose of the present invention is to overcome the deficiencies in the prior art and to provide a welding control method, device, and storage medium for arc starting and arc ending, so as to improve the arc starting and arc ending performance of a welding power source through an arc starting and arc ending method controlled by variable acceleration.

[0008] To achieve the above object, the present invention is implemented by adopting the following technical solutions:

[0009] In a first aspect, the present invention provides a welding control method for arc starting and arc ending, comprising:

[0010] In the arc initiation stage of MIG / MAG welding, a two-stage variable acceleration method is used to accelerate the welding parameter update speed and wire feeding speed from the slow wire feeding speed to the main welding wire feeding speed.

[0011] In the arc closing stage of metal arc welding, a two-stage variable acceleration method is used to slow down the welding parameter update speed and wire feeding speed from the main welding wire feeding speed to the back-burning wire feeding speed.

[0012] Furthermore, in the arc starting stage of the metal arc welding, the welding parameter update speed and the wire feeding speed are accelerated from the slow wire feeding speed to the main welding wire feeding speed by using a two-stage variable acceleration method, including:

[0013] After the arc ignition stage begins, the welding parameter update speed starts to accelerate from the parameter update first acceleration to the parameter update first maintenance speed, and after maintaining the parameter update first maintenance time, it accelerates to the main welding wire feeding speed with the parameter update second acceleration;

[0014] The wire feeding speed starts from a slow wire feeding speed and is accelerated to a first maintaining speed by updating the speed with a first acceleration. After maintaining the speed update for a first maintaining time, the wire feeding speed is accelerated to a main welding wire feeding speed by updating the second acceleration by the speed.

[0015] Further, at the beginning of the welding parameter update speed, the parameter update first acceleration is accelerated to the parameter update first maintaining speed stage, and the current instruction and the voltage instruction are updated synchronously;

[0016] During the first maintenance time of parameter update, the current command and the voltage command are not updated;

[0017] When the welding parameter update speed is accelerated to the main welding wire feeding speed by the second acceleration of parameter update, the current instruction and the voltage instruction are updated synchronously;

[0018] After the welding parameter update speed reaches the main welding wire feeding speed, the current command and voltage command are not updated.

[0019] Furthermore, the first acceleration for updating the parameters is greater than the first acceleration for updating the rotational speed, and the second acceleration for updating the parameters is greater than the second acceleration for updating the rotational speed.

[0020] Furthermore, in the arc closing stage of the metal arc welding, the welding parameter update speed and the wire feeding speed are decelerated from the main welding wire feeding speed to the burn-back wire feeding speed by adopting a two-stage variable acceleration method, including:

[0021] After the arc closing stage begins, the welding parameter update speed starts to decelerate from the third acceleration of parameter update to the second maintaining speed of parameter update. After maintaining the second maintaining time of parameter update, it is decelerated to the burn-back wire feeding speed with the fourth acceleration of parameter update. The wire feeding speed starts to decelerate from the main welding wire feeding speed with the third acceleration of speed update to the second maintaining speed of speed update. After maintaining the second maintaining time of speed update, it is decelerated to the burn-back wire feeding speed with the fourth acceleration of speed update.

[0022] Further, when the welding parameter update speed starts to decelerate from the parameter update third acceleration to the parameter update second maintaining speed stage, the current command and the voltage command are updated synchronously;

[0023] During the second holding time of parameter update, the current command and the voltage command are not updated;

[0024] When the welding parameter update speed is decelerated from the fourth acceleration of parameter update to the stage of wire feeding speed of burn-back, the current instruction and the voltage instruction are updated synchronously;

[0025] After the wire feeding speed is decelerated to the burn-back wire feeding speed by the fourth acceleration with the rotation speed update, the current command and the voltage command are not updated.

[0026] Further, the third acceleration for updating the parameters is smaller than the third acceleration for updating the rotational speed, and the fourth acceleration for updating the parameters is larger than the fourth acceleration for updating the rotational speed.

[0027] Further, the synchronous updating of the current instruction and the voltage instruction includes:

[0028] According to the current welding parameter update speed, the current value and voltage value corresponding to the current welding parameter update speed are obtained from the data table of the set welding power source.

[0029] In a second aspect, a welding control device for arc starting and arc ending includes:

[0030] The arc starting control module is used for accelerating the welding parameter update speed and wire feeding speed from the slow wire feeding speed to the main welding wire feeding speed in the arc starting stage of the metal arc welding.

[0031] The arc closure control module is used to decelerate the welding parameter update speed and wire feeding speed from the main welding wire feeding speed to the back-burning wire feeding speed in a two-stage variable acceleration manner during the arc closure stage of metal arc gas shielded welding.

[0032] In a third aspect, the present invention provides a computer storage medium having a computer program stored thereon, wherein the computer program, when executed by a processor, implements the steps of the method described in the first aspect.

[0033] Compared with the prior art, the present invention has the following beneficial effects:

[0034] The present invention is mainly aimed at welding scenarios with frequent arcing, such as spot welding process, and improves the arcing and arcing performance of the welding power source through the arcing and arcing methods controlled by variable acceleration.

[0035] Good arc striking performance is reflected in the absence of arc breaking, wire breakage, long-term short circuit, arc ignition, etc. In this stage, the current motor speed and the energy output of the welding power supply must be reasonably matched to ensure good repeatable arc striking, thereby ensuring the consistency of the weld.

[0036] The quality of arc extinguishing affects the next arc striking. After the welding gun switch is released, the arc extinguishing stage begins. The motor speed decreases, and the welding power supply's reasonable output current and voltage match the current speed to ensure a reasonable change in arc length. The arc does not suddenly shorten so that the welding wire does not melt, or the arc length becomes longer and damages the conductive nozzle, or the remaining welding wire becomes shorter after welding, which prolongs the next arc striking time and affects the welding rhythm. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 The figure shows the conventional arc starting and arc ending control schematic diagram of metal arc welding;

[0038] Figure 2 The figure shows the change of various parameters in the arc starting stage of conventional metal arc gas shielded welding;

[0039] Figure 3 The figure shows the change of various parameters in the arc closing stage of conventional metal arc gas shielded welding;

[0040] Figure 4 Shown is a schematic diagram of arc starting and arc ending welding control provided by an embodiment of the present invention;

[0041] Figure 5 Shown is a schematic diagram of arc striking control provided by an embodiment of the present invention;

[0042] Figure 6 The figure shows a schematic diagram of arc closure control provided by an embodiment of the present invention;

[0043] Figure 7 The figure is a schematic diagram of the arc ignition stage control process provided by an embodiment of the present invention;

[0044] Figure 8 The figure is a schematic diagram of the control flow of the arc closing stage provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0045] The technical concept of the present invention is as follows: in the arc starting stage of MIG / MAG welding, the welding parameter instructions and wire feeding instructions use a two-stage variable acceleration method to accelerate from a slow wire feeding speed to a main welding wire feeding speed; in the arc ending stage of MIG / MAG welding, the welding parameter instructions and wire feeding instructions use a two-stage variable acceleration method to decelerate from the main welding wire feeding speed to a burn-back wire feeding speed. The arc starting and arc ending methods controlled by variable acceleration can improve the arc starting and arc ending performance of the welding power source.

[0046] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present application and its application or use.

[0047] Example 1

[0048] This embodiment provides a welding control method for arc starting and arc ending, such as Figure 4 As shown, the following steps are included:

[0049] In the arc initiation stage of MIG / MAG welding, a two-stage variable acceleration method is used to accelerate the welding parameter update speed and wire feeding speed from the slow wire feeding speed to the main welding wire feeding speed.

[0050] In the arc closing stage of metal arc welding, a two-stage variable acceleration method is used to slow down the welding parameter update speed and wire feeding speed from the main welding wire feeding speed to the back-burning wire feeding speed.

[0051] In the arc initiation stage of the metal arc welding, a two-stage variable acceleration method is used to accelerate the welding parameter update speed and the wire feeding speed from the slow wire feeding speed to the main welding wire feeding speed, including:

[0052] After the arc ignition stage begins, the welding parameter update speed starts to accelerate from the parameter update first acceleration to the parameter update first maintenance speed, and after maintaining the parameter update first maintenance time, it accelerates to the main welding wire feeding speed with the parameter update second acceleration;

[0053] The wire feeding speed starts from a slow wire feeding speed and is accelerated to a first maintaining speed by updating the speed with a first acceleration. After maintaining the speed update for a first maintaining time, the wire feeding speed is accelerated to a main welding wire feeding speed by updating the second acceleration by the speed.

[0054] At the beginning of the welding parameter update speed, the welding process accelerates from the parameter update first acceleration stage to the parameter update first maintenance speed stage, and synchronously updates the current command and the voltage command;

[0055] During the first maintenance time of parameter update, the current command and the voltage command are not updated;

[0056] When the welding parameter update speed is accelerated to the main welding wire feeding speed by the second acceleration of parameter update, the current instruction and the voltage instruction are updated synchronously;

[0057] After the welding parameter update speed reaches the main welding wire feeding speed, the current command and voltage command are not updated.

[0058] The first acceleration for updating the parameters is greater than the first acceleration for updating the rotational speed, and the second acceleration for updating the parameters is greater than the second acceleration for updating the rotational speed.

[0059] In the arc closing stage of the metal arc welding, the welding parameter updating speed and the wire feeding speed are decelerated from the main welding wire feeding speed to the burn-back wire feeding speed by adopting a two-stage variable acceleration method, including:

[0060] After the arc closing stage begins, the welding parameter update speed starts to decelerate from the third acceleration of parameter update to the second maintaining speed of parameter update. After maintaining the second maintaining time of parameter update, it is decelerated to the burn-back wire feeding speed with the fourth acceleration of parameter update. The wire feeding speed starts to decelerate from the main welding wire feeding speed with the third acceleration of speed update to the second maintaining speed of speed update. After maintaining the second maintaining time of speed update, it is decelerated to the burn-back wire feeding speed with the fourth acceleration of speed update.

[0061] At the welding parameter update speed, the third acceleration of parameter update is decelerated to the second maintenance speed stage of parameter update, and the current instruction and the voltage instruction are updated synchronously;

[0062] During the second holding time of parameter update, the current command and the voltage command are not updated;

[0063] When the welding parameter update speed is decelerated from the fourth acceleration of parameter update to the stage of wire feeding speed of burn-back, the current instruction and the voltage instruction are updated synchronously;

[0064] After the wire feeding speed is decelerated to the burn-back wire feeding speed by the fourth acceleration with the rotation speed update, the current command and the voltage command are not updated.

[0065] The third acceleration for updating the parameters is smaller than the third acceleration for updating the rotation speed, and the fourth acceleration for updating the parameters is larger than the fourth acceleration for updating the rotation speed.

[0066] The synchronous updating of the current instruction and the voltage instruction comprises:

[0067] According to the current welding parameter update speed, the current value and voltage value corresponding to the current welding parameter update speed are obtained from the data table of the set welding power source.

[0068] The following is an example to illustrate the arc starting and arc ending welding control method of this embodiment.

[0069] Arc welding control process reference Figure 5 and Figure 7 , including the following steps:

[0070] After the welding gun switch is closed, the motor starts to accelerate to slow wire feeding. When the welding wire contacts the base material and generates current, it enters the arc striking stage.

[0071] The parameter query instruction starts from the slow wire feeding speed SlowSpd and accelerates to ParmSpd1 with the acceleration of ParmAcc0. This process continuously updates the current instruction and the voltage instruction. When the ParmSpd1 speed is reached, the ParmT0 time is maintained. At this stage, the current instruction and the voltage instruction are no longer updated. After the ParmT0 time is reached, the acceleration of ParmAcc1 is started to accelerate to the main welding wire feeding speed MainSpd. This stage is the second acceleration stage. The current instruction and the voltage instruction are also continuously updated. When MainSpd is reached, the parameters are no longer updated.

[0072] The wire feeding instruction starts from slow wire feeding SlowSpd and accelerates to MotSpd1 with acceleration MotAcc0, then maintains MotT0 time, and climbs to the main welding wire feeding speed MainSpd with MotAcc1 acceleration. After that, the parameters are no longer updated and changes, and enter the stable main welding stage. During the whole process, ParmAcc0 must be greater than MotAcc0, and ParmAcc1 must be greater than MotAcc1 to ensure that the current and voltage parameters have been updated before the motor speed is reached.

[0073] It should be noted that current and voltage represent the output energy of the welding power supply. In the arc initiation stage, the current command and voltage command are constantly updated to reasonably match the current motor speed. The maintenance stage mainly calculates the parameters of the next stage, such as the acceleration of the motor speed, the acceleration of the current command and the voltage command. If the parameters continue to be updated at this stage, the initial value will change.

[0074] Arc welding control process reference Figure 6 and Figure 8 , including the following steps:

[0075] After the welding gun switch is released, the main welding enters the arc extinguishing stage.

[0076] The parameter query instruction starts to decelerate from ParmAcc2 to ParmSpd2. In this stage, the current instruction and voltage instruction are updated synchronously in real time. After the speed reaches ParmSpd2, it is maintained for a period of ParmT1 and then decelerated again to the burn-in speed BrunSpd with ParmAcc3. In this stage, the current instruction and voltage instruction are also updated in real time. At this time, after waiting for the motor speed to drop to BurnSpd to perform the burn-in process, all parameters are restored to their initial values.

[0077] The wire feeding instruction starts from the main welding speed and decelerates to MotSpd2 with acceleration MotAcc2, then maintains MotT1 time, and starts to decelerate to the burn-back speed BurnSpd with acceleration MotAcc3. At this time, the current and voltage parameters have been updated, and the burn-back melting ball processing begins. After the processing is completed, the motor speed is reduced to zero, and the parameter instructions are restored to the initial value, and the entire welding process ends. ParmAcc2 should be less than MotACC2 to prevent the arc from shortening rapidly in a short period of time, and ParmAcc3 should be greater than MotAcc3 to ensure that the parameter instructions have been updated before the speed reaches the burn-back speed.

[0078] It should be noted that in the arc closure stage, ParmT1 is less than MotT1, in order to quickly drop to the burn-back speed, i.e., BurnSpd, in the second stage of arc closure. ParmSpd2 is greater than MotSpd2, in order to make the output energy of the welding power source slightly greater than the current rotation speed, so that the arc length does not suddenly shorten and cause poor welding. In the second stage of arc closure, ParmAcc3 is slightly greater than MotAcc3, reducing the energy output of the welding power source, and when reaching BurnSpd, the tip of the welding wire can form a molten ball of about 1.2 times the diameter of the welding wire.

[0079] The update process mainly consists of two parts, one is the actual speed of the motor, and the other is the energy output by the welding power supply, namely the welding current and voltage.

[0080] Before actual welding, you first need to set the welding current and welding voltage. The relationship between the set current, wire feeding speed and voltage is stored in the data table of the welding power supply. By setting the current, you can query the corresponding wire feeding speed and voltage value. Similarly, you can query the welding current and voltage by the wire feeding speed. For example, if the current is set to 200A, query the data table to obtain the wire feeding speed of 10m / min and the set voltage of 26V. As mentioned above, assuming that the wire feeding speed is set to 10m / min, the query data can obtain the set current of 200A and the set voltage of 26V.

[0081] After starting welding, the wire feeding speed increases from 0 to a slow wire feeding speed of 1 / min. After entering the arc striking stage, the wire feeding speed increases from a slow wire feeding speed of 1m / min to 10m / min. The current increases from 0 to 200A, and the voltage increases from 0 to 26V.

[0082] Update process description:

[0083] M01: Motor speed value. Based on the above conditions, slow wire feeding 1m / min, final speed 10m / min, acceleration ACC, the value of each linear increase can be calculated.

[0084] When entering the arc striking stage, start the timer in the electric welder. Every 10ms, the initial speed, i.e. the slow wire feeding speed, increases linearly to the final value, i.e. the main welding wire feeding speed. The increasing pattern is similar to 1, 1.2, 1.4, 1.6, 1, 8, 2.0 to 10m / min, with an interval of 10ms.

[0085] M02: Parameter query, that is, set the wire feeding speed value corresponding to the current and voltage update. If M01 is equal to M02, follow the similar increasing rule of 1, 1.2, 1.4, 1.6, 1, 8, 2.0 to 10m / min, with an interval of 10ms. At this time, query the current value and voltage value at the current wire feeding speed, that is, the energy output by the current welding power supply. Generally speaking, in the early stage of arc initiation, the welding wire has not been preheated by the arc, so more energy is required, that is, when the actual wire feeding speed is 2.0m / min, it may match the current and voltage values ​​corresponding to the wire feeding speed of 2.5m / min. M02 can also be called the wire feeding speed of calculating current and voltage matching, not the actual speed of the motor. M02 has a larger acceleration value than M01 (actual speed of the motor), and the queried current and voltage are higher. It uses higher energy to match the lower wire feeding speed value. The purpose is to quickly and smoothly start the arc and achieve better welding results. If the current and voltage corresponding to the current wire feeding speed are used, wire top and welding short circuit may occur.

[0086] M01 is the actual motor speed. The increment is calculated in advance based on the initial and final speeds and acceleration, and then increments every 10ms until the final speed value is reached. M02 is calculated in the same way as M01, but the acceleration is different, so the increment is different, and the increment is larger. M02 is also updated every 10ms, which is consistent with M01. According to the current speed value of M02, the data table is queried to obtain the current current and voltage command values ​​of the welding power supply. When M02 reaches the final speed first, it maintains this speed and does not change, and the current and voltage commands no longer change.

[0087] The arc-ending stage is similar to the arc-starting stage, except that the wire feeding speed decreases and the update cycle is also 10ms. At this time, since the welding wire is already in a hot state during welding, M01 and M02 can be decreased with the same acceleration, or M02 can be slightly slower than M01. During the decreasing process, the welding voltage and current command values ​​are queried every 10ms through the current value of M02. When the motor speed M01 reaches the burn-back wire feeding speed, the welding outputs the burn-back pulse, the speed command M01 drops directly to 0, and M02 also returns to the initial value 0.

[0088] In the maintenance stage, M01 maintains the current speed value, and M02 also maintains the current value. Since M02 does not change, the welding current and voltage instructions no longer change.

[0089] Example 2

[0090] This embodiment provides a welding control device for arc starting and arc ending, comprising:

[0091] The arc starting control module is used for accelerating the welding parameter update speed and wire feeding speed from the slow wire feeding speed to the main welding wire feeding speed in the arc starting stage of the metal arc welding.

[0092] The arc closure control module is used to decelerate the welding parameter update speed and wire feeding speed from the main welding wire feeding speed to the back-burning wire feeding speed in a two-stage variable acceleration manner during the arc closure stage of metal arc gas shielded welding.

[0093] Example 3

[0094] This embodiment provides a computer storage medium on which a computer program is stored. When the computer program is executed by a processor, the steps of the method described in Embodiment 1 are implemented.

[0095] Those skilled in the art will appreciate that the embodiments of the present application may be provided as methods, systems, or computer program products. Therefore, the present application may adopt the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present application may adopt the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.

[0096] The present application is described with reference to the flowcharts and / or block diagrams of the methods, devices (systems), and computer program products according to the embodiments of the present application. It should be understood that each process and / or box in the flowchart and / or block diagram, as well as the combination of the processes and / or boxes in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.

[0097] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.

[0098] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process in the computer or other programmable device. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.

[0099] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A welding control method for arc starting and arc ending, characterized in that: include: In the arc initiation stage of MIG / MAG welding, a two-stage variable acceleration method is used to accelerate the welding parameter update speed and wire feeding speed from the slow wire feeding speed to the main welding wire feeding speed. In the arc closing stage of metal arc welding, a two-stage variable acceleration method is used to slow down the welding parameter update speed and wire feeding speed from the main welding wire feeding speed to the back-burning wire feeding speed.

2. The arc starting and arc ending welding control method according to claim 1, characterized in that: In the arc initiation stage of the metal arc welding, a two-stage variable acceleration method is used to accelerate the welding parameter update speed and the wire feeding speed from the slow wire feeding speed to the main welding wire feeding speed, including: After the arc ignition stage begins, the welding parameter update speed starts to accelerate from the parameter update first acceleration to the parameter update first maintenance speed, and after maintaining the parameter update first maintenance time, it accelerates to the main welding wire feeding speed with the parameter update second acceleration; The wire feeding speed starts from a slow wire feeding speed and is accelerated to a first maintaining speed by updating the speed with a first acceleration. After maintaining the speed update for a first maintaining time, the wire feeding speed is accelerated to a main welding wire feeding speed by updating the second acceleration by the speed.

3. The arc starting and arc ending welding control method according to claim 2, characterized in that: At the beginning of the welding parameter update speed, the welding process accelerates from the parameter update first acceleration stage to the parameter update first maintenance speed stage, and synchronously updates the current command and the voltage command; During the first maintenance time of parameter update, the current command and the voltage command are not updated; When the welding parameter update speed is accelerated to the main welding wire feeding speed by the second acceleration of parameter update, the current instruction and the voltage instruction are updated synchronously; After the welding parameter update speed reaches the main welding wire feeding speed, the current command and voltage command are not updated.

4. The arc starting and arc ending welding control method according to claim 2, characterized in that: The first acceleration for updating the parameters is greater than the first acceleration for updating the rotational speed, and the second acceleration for updating the parameters is greater than the second acceleration for updating the rotational speed.

5. The arc starting and arc ending welding control method according to claim 1, characterized in that: In the arc closing stage of the metal arc welding, the welding parameter updating speed and the wire feeding speed are decelerated from the main welding wire feeding speed to the burn-back wire feeding speed by adopting a two-stage variable acceleration method, including: After the arc closing stage begins, the welding parameter update speed starts to decelerate from the third acceleration of parameter update to the second maintaining speed of parameter update. After maintaining the second maintaining time of parameter update, it is decelerated to the burn-back wire feeding speed with the fourth acceleration of parameter update. The wire feeding speed starts to decelerate from the main welding wire feeding speed with the third acceleration of speed update to the second maintaining speed of speed update. After maintaining the second maintaining time of speed update, it is decelerated to the burn-back wire feeding speed with the fourth acceleration of speed update.

6. The arc starting and arc ending welding control method according to claim 5, characterized in that: At the welding parameter update speed, the third acceleration of parameter update is decelerated to the second maintenance speed stage of parameter update, and the current instruction and the voltage instruction are updated synchronously; During the second holding time of parameter update, the current command and the voltage command are not updated; When the welding parameter update speed is decelerated from the fourth acceleration of parameter update to the stage of wire feeding speed of burn-back, the current instruction and the voltage instruction are updated synchronously; After the wire feeding speed is decelerated to the burn-back wire feeding speed by the fourth acceleration with the rotation speed update, the current command and the voltage command are not updated.

7. The arc starting and arc ending welding control method according to claim 5, characterized in that: The third acceleration for updating the parameters is smaller than the third acceleration for updating the rotation speed, and the fourth acceleration for updating the parameters is larger than the fourth acceleration for updating the rotation speed.

8. The arc starting and arc ending welding control method according to claim 3 or 6, characterized in that: The synchronous updating of the current instruction and the voltage instruction comprises: According to the current welding parameter update speed, the current value and voltage value corresponding to the current welding parameter update speed are obtained from the data table of the set welding power source.

9. A welding control device for arc starting and arc ending, characterized in that: include: The arc starting control module is used for accelerating the welding parameter update speed and wire feeding speed from the slow wire feeding speed to the main welding wire feeding speed in the arc starting stage of the metal arc welding. The arc closure control module is used to decelerate the welding parameter update speed and wire feeding speed from the main welding wire feeding speed to the back-burning wire feeding speed in a two-stage variable acceleration manner during the arc closure stage of metal arc gas shielded welding.

10. A computer storage medium having a computer program stored thereon, characterized in that: When the computer program is executed by a processor, the steps of the method according to any one of claims 1 to 8 are implemented.