Ultra-small and ultra-multiple spiral hole laser welding device and welding process

By setting spiral holes on the surface of metal sheets and using inert gas purge technology, the problem of welding joint oxidation during welding is solved, and high-quality ultra-small and multi-spiral hole laser welding is achieved, avoiding yellowing and blackening of the welding joints etc.

CN119016873AActive Publication Date: 2024-11-26KUNSHAN KUNSHUO PRECISION COMPONENTS CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202411424685.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-12
Publication Date
2024-11-26
Estimated Expiration
2044-10-12

AI Technical Summary

Technical Problem

During the welding process of metal sheets, high temperatures cause oxidation of the solder joints, affecting the quality and appearance of the welding. The existing technology is difficult to effectively prevent defects such as yellowing and blackening of the solder joints.

Method used

Using ultra-small and multiple spiral holes laser welding devices and processes, by setting spiral holes on the surface of the metal sheet and purge inert gas to the welding holes at an inclined angle during laser welding, gas circuit boards, gas circuit transfer boards, gas circuits The deflector and the blowing plate blow the gas evenly to form a protective atmosphere to prevent the solder joints from oxidizing.

Benefits of technology

Effectively prevent defects such as yellowing and blackening of the solder joints, laser welding of ultra-small and multiple spiral holes is realized, improving the welding quality and appearance, and avoiding oxidation during the welding process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119016873A_ABST
    Figure CN119016873A_ABST
Patent Text Reader

Abstract

The invention aims at disclosing an ultra-small and ultra-multi-spiral-hole laser welding device and a welding process, and relates to the technical field of metal sheet laser welding, the ultra-small and ultra-multi-spiral-hole laser welding device comprises a laser welding assembly, an upper die assembly and a lower die assembly; the upper die assembly comprises an upper die base and a stripping assembly. The stripping assembly comprises a fixing plate, a gas circuit plate, a gas circuit transfer plate, a gas circuit guide plate, a blowing plate and a shaping pressing plate. At least one first horizontal air inlet hole and at least one second horizontal air inlet hole are symmetrically formed in the two sides of the air path plate; a plurality of inclined holes are formed in the third hollow part; the blowing direction of the inclined hole is aligned with the welding hole; the laser welding device has the technical effects that the inert gas uniformly passes through the gas path plate, the gas path transfer plate, the gas path guide plate and the gas blowing plate, so that the wind speed of each inclined hole is consistent, and laser welding of ultra-small and ultra-multi spiral holes can be realized; and the defects of yellowing, blackening and the like of welding spots are effectively avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of laser welding of metal sheets, in particular to a laser welding device and a welding process for ultra-small and ultra-multiple spiral holes. Background Art

[0002] With the rapid development of 3C electronics and precision machining, two metal sheets need to be firmly welded. However, during welding, the solder joints of the metal sheets will turn yellow, black, and undergo oxidation at high temperatures, affecting the welding quality and appearance.

[0003] In view of this, it is necessary to develop an ultra-small and ultra-multi spiral hole laser welding device and welding process. Summary of the invention

[0004] In order to solve the above technical problems, the purpose of the present invention is to disclose an ultra-small and ultra-multiple spiral hole laser welding device and welding process.

[0005] The first inventive object of the present invention is to develop an ultra-small and ultra-multi-spiral hole laser welding device.

[0006] The second inventive object of the present invention is to develop a laser welding process for ultra-small and ultra-multiple spiral holes.

[0007] To achieve the above first invention objective, the present invention provides an ultra-small ultra-multiple spiral hole laser welding device, comprising a laser welding assembly, an upper mold assembly and a lower mold assembly;

[0008] The metal sheet to be welded is arranged between the upper die assembly and the lower die assembly;

[0009] The upper die assembly comprises an upper die seat and a stripping assembly;

[0010] The lower die assembly comprises a lower die base, a lower pad and a lower die plate;

[0011] The stripping assembly includes a fixing plate, an air path plate, an air path transmission plate, an air path guide plate, an air blowing plate and a shaping pressing plate;

[0012] The upper die base, the fixing plate and the gas circuit plate are respectively provided with hollow parts matching the welding range of the metal sheet;

[0013] At least one first horizontal air inlet hole and at least one second horizontal air inlet hole are symmetrically arranged on both sides of the air path plate, the first horizontal air inlet hole passes through the air path plate and is connected to the hollow portion, and the second horizontal air inlet hole passes through the air path plate and is connected to the hollow portion;

[0014] The air path transmission plate includes a step portion and a bottom plate, a third horizontal air inlet hole flush with and connected to the first horizontal air inlet hole and a fourth horizontal air inlet hole flush with and connected to the second horizontal air inlet hole are respectively arranged on both sides of the step portion, and the fixing plate blocks the top surface of the step portion;

[0015] A first vertical air inlet hole communicating with the third horizontal air inlet hole is further provided on the step portion, a second vertical air inlet hole communicating with the fourth horizontal air inlet hole is further provided on the step portion, and a first hollow portion matching the outer contour of the metal sheet is provided on the bottom plate;

[0016] The air path guide plate is provided with a second hollow portion matching the outer contour of the metal sheet, an air path guide groove is provided along the outer side of the contour of the second hollow portion, the air path guide groove is connected with the first vertical air inlet hole and the second vertical air inlet hole, and a plurality of vertical through holes are provided along the bottom surface of the air path guide groove;

[0017] The blowing plate is provided with a third hollow portion matching the outer contour of the metal sheet, and a plurality of oblique holes are provided along the third hollow portion, and the oblique holes correspond to the vertical through holes one by one;

[0018] The shaping press plate comprises a plurality of welding holes corresponding to the spiral holes of the metal sheet one by one, and the blowing direction of the inclined holes is aligned with the welding holes;

[0019] Inert gas is introduced into the first horizontal air inlet hole and the second horizontal air inlet hole simultaneously.

[0020] Preferably, the number of the metal sheets is three pairs, and each of the metal sheets is provided with 32 spiral holes.

[0021] Preferably, the first horizontal air inlet hole is provided with four first branch air paths, and the second horizontal air inlet hole is provided with four second branch air paths.

[0022] Preferably, the gas circuit board is further provided with a fifth horizontal air inlet hole and a sixth horizontal air inlet hole penetrating the gas circuit board;

[0023] The step portion is provided with a plurality of seventh horizontal air inlet holes flush with and connected to the fifth horizontal air inlet holes, and a plurality of eighth horizontal air inlet holes flush with and connected to the sixth horizontal air inlet holes;

[0024] A third vertical air inlet hole communicating with the seventh horizontal air inlet hole is further provided on the step portion, and a fourth vertical air inlet hole communicating with the eighth horizontal air inlet hole is further provided on the step portion.

[0025] Preferably, the angle between the inclined hole and the horizontal plane is 45°.

[0026] Preferably, the blowing wind speed of the inclined holes is 3m / s-8m / s.

[0027] Preferably, nitrogen, argon or helium is blown through the inclined holes.

[0028] Preferably, a first upper convex curved surface and a second upper convex curved surface are provided below the shaping press plate;

[0029] The lower template is provided with a third upper convex arc surface corresponding to the first upper convex arc surface, and the lower template is provided with a fourth upper convex arc surface corresponding to the second upper convex arc surface.

[0030] Preferably, the shaping pressing plate comprises a thin end and a thick end, the thickness of the thin end is 1 mm-1.3 mm, and the thickness of the thick end is 1.9 mm-2.5 mm.

[0031] Based on the same inventive principle, in order to achieve the above-mentioned first inventive object, the present invention provides an ultra-small ultra-multiple spiral hole laser welding process, comprising the following steps:

[0032] Placing the metal sheets to be welded at predetermined positions and determining the positions of several spiral welding points;

[0033] A laser welding path of a laser welding assembly is preset, wherein two closest spiral welding points in the welding path are spaced apart by at least one spiral welding point;

[0034] Compressing the metal sheets to be welded by the upper die assembly and the lower die assembly;

[0035] During laser welding, an inert gas is blown toward each spiral welding point at an angle of 30°-60°, and the wind speed of the inert gas is 3m / s-8m / s.

[0036] Compared with the prior art, the technical effects of the present invention are as follows:

[0037] (1) The surface of the metal sheet of the present invention is pre-arranged with a plurality of spiral holes, the depth of the spiral holes being approximately half the thickness of the metal sheet. The spiral holes are welded respectively by laser in a vertical posture along a preset path. The laser penetrates the spiral holes and heat-melts the metal layer below to realize the welding of the upper and lower layers of the metal sheets. During the welding process, an inert gas is purged toward each welding hole at an inclined angle toward the spiral hole to provide a protective atmosphere, thereby effectively preventing defects such as yellowing and blackening of the weld points.

[0038] (2) The inert gas passes through the gas path plate, gas path transfer plate, gas path guide plate, and air blowing plate in a uniform manner, so that the wind speed of each inclined hole is consistent, which can realize laser welding of ultra-small and ultra-multiple spiral holes and effectively avoid defects such as yellowing and blackening of the welds. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0040] Figure 1 Schematic diagram of three pairs of metal sheets to be welded according to the present invention.

[0041] Figure 2 It is a schematic diagram of the three-dimensional structure of the ultra-small and ultra-multi spiral hole laser welding device of the present invention.

[0042] Figure 3 It is a cross-sectional schematic diagram of the ultra-small and ultra-multi spiral hole laser welding device of the present invention.

[0043] Figure 4 The present invention Figure 3 Schematic diagram of the enlarged structure when A is not welded.

[0044] Figure 5 The present invention Figure 3 Schematic diagram of the enlarged structure at A in the welding state.

[0045] Figure 6 It is a schematic diagram of the three-dimensional structure of the stripping assembly of the present invention.

[0046] Figure 7 It is a schematic diagram of the three-dimensional structure of the gas circuit board of the present invention.

[0047] Figure 8 It is a schematic diagram of the three-dimensional structure of the gas circuit board of the present invention.

[0048] Fig. 9 It is a schematic diagram of the three-dimensional structure of the gas path transmission plate of the present invention.

[0049] Fig.10 It is a schematic diagram of the three-dimensional structure of the gas path transmission plate of the present invention.

[0050] Fig.11 It is a schematic diagram of the three-dimensional structure of the gas path guide plate of the present invention.

[0051] Fig.12 It is a schematic diagram of the three-dimensional structure of the gas path guide plate of the present invention.

[0052] Fig.13 It is a schematic diagram of the three-dimensional structure of the blowing plate of the present invention.

[0053] Fig.14 It is a schematic diagram of the three-dimensional structure of the blowing plate of the present invention.

[0054] Fig.15It is a schematic diagram of the three-dimensional structure of the shaping pressing plate of the present invention.

[0055] Fig.16 It is a top view schematic diagram of the shaping pressing plate of the present invention.

[0056] Fig.17 It is a schematic diagram of the cooperation principle of the shaping pressing plate and the lower template of the present invention.

[0057] Fig.18 This is a process flow chart of the ultra-small and ultra-multiple spiral hole laser welding of the present invention.

[0058] Among them, 1. laser welding assembly; 2. upper mold assembly; 21. upper mold seat; 22. stripping assembly; 221. fixing plate; 222. air path plate; 2221. first horizontal air inlet; 2222. second horizontal air inlet; 2223. first branch air path; 2224. second branch air path; 2225. fifth horizontal air inlet; 2226. sixth horizontal air inlet; 223. air path transfer plate; 2231. step portion; 2232. bottom plate; 2233. third horizontal air inlet; 2234. fourth horizontal air inlet; 2235. first hollow portion; 2236. seventh horizontal air inlet; 223 7. Eighth horizontal air inlet hole; 224. Air path guide plate; 2241. Second hollow portion; 2242. Air path guide groove; 2243. Vertical through hole; 225. Blowing plate; 2251. Third hollow portion; 2252. Oblique hole; 226. Shaping pressing plate; 2261. First upper convex arc surface; 2262. Second upper convex arc surface; 2263. Thin end; 2264. Thick end; 2265. Welding hole; 3. Lower die assembly; 31. Lower die seat; 32. Lower pad; 33. Lower die plate; 331. Third upper convex arc surface; 332. Fourth upper convex arc surface; 4. Hollow portion; 5. Metal sheet; 51. Spiral hole. DETAILED DESCRIPTION

[0059] The present invention is described in detail below in conjunction with the various embodiments shown in the accompanying drawings, but it should be noted that these embodiments are not limitations of the present invention, and any equivalent transformations or substitutions in functions, methods, or structures made by ordinary technicians in the field based on these embodiments are all within the scope of protection of the present invention.

[0060] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0061] Example 1

[0062] Ginseng Figure 1 and Fig.17 As shown, this embodiment discloses a specific implementation of an ultra-small and ultra-multi-spiral hole laser welding device.

[0063] The present embodiment provides an ultra-small ultra-multiple spiral hole laser welding device, comprising a laser welding assembly 1, an upper mold assembly 2 and a lower mold assembly 3. The laser welding assembly 1 welds each spiral hole one by one according to a preset path; the metal sheet to be welded is arranged between the upper mold assembly 2 and the lower mold assembly 3, and the metal sheet to be welded 5 comprises a bottom sheet and an upper sheet, and a plurality of spiral holes 51 are arranged on the upper sheet, and the depth of each spiral hole 51 is half of the thickness of the upper sheet, the thickness of the upper sheet is 0.1 mm, and the thickness of the lower sheet is 0.2 mm. During laser welding, each spiral hole 51 is melted. The upper die assembly 2 includes an upper die seat 21 and a stripping assembly 22; the lower die assembly 3 includes a lower die seat 31, a lower pad 32 and a lower die plate 33; the stripping assembly 22 includes a fixing plate 221, an air path plate 222, an air path transmission plate 223, an air path guide plate 224, an air blowing plate 225 and a shaping pressing plate 226; the upper die seat 21 and the air path plate 222 are respectively provided with a hollow portion 4 matching the welding range of the metal sheet, and the welding range is shown in FIG. Figure 1The dotted frame shown in the figure; at least one first horizontal air inlet hole 2221 and at least one second horizontal air inlet hole 2222 are symmetrically arranged on both sides of the air path plate 222, and inert gas is simultaneously introduced into the first horizontal air inlet hole 2221 and the second horizontal air inlet hole 2222, the first horizontal air inlet hole 2221 passes through the air path plate 222 and is connected to the hollow portion 4, the second horizontal air inlet hole 2222 passes through the air path plate 222 and is connected to the hollow portion 4, the first horizontal air inlet hole 2221 and the second horizontal air inlet hole 2222 are blocked by the fixing plate 221; the air path transmission plate 223 includes a step portion 2231 and a bottom plate 2232, the step portion 22 A third horizontal air inlet hole 2233 flush with and connected to the first horizontal air inlet hole 2221 and a fourth horizontal air inlet hole 2234 flush with and connected to the second horizontal air inlet hole 2222 are respectively provided on both sides of the step portion 2231, and the fixing plate 221 blocks the top surface of the step portion 2231, and the fixing plate 221 also blocks the third horizontal air inlet hole 2233 and the fourth horizontal air inlet hole 2234 to prevent air leakage; a first vertical air inlet hole connected to the third horizontal air inlet hole 2233 is also provided on the step portion 2231, so that the inert gas changes from a horizontal direction to a vertical direction, and a second vertical air inlet hole connected to the fourth horizontal air inlet hole 2234 is also provided on the step portion 2233. The inert gas is changed from a horizontal direction to a vertical direction by an air inlet hole, and a first hollow portion 2235 matching the outer contour of the metal sheet is provided on the bottom plate 2232; the air path guide plate 224 is provided with a second hollow portion 2241 matching the outer contour of the metal sheet, and an air path guide groove 2242 is provided along the outer side of the contour of the second hollow portion 2241, and the air path guide groove 2242 is connected with the first vertical air inlet hole and the second vertical air inlet hole, and a plurality of vertical through holes 2243 are provided along the bottom surface of the air path guide groove 2242, and the inert gas enters the air path guide groove 2242 after passing through the first vertical air inlet hole and the second vertical air inlet hole, and flows along the air path guide groove 2242 diffuses to the periphery of the contour of each metal sheet, so that the inert gas is evenly distributed; the blowing plate 225 is provided with a third hollow portion 2251 matching the outer contour of the metal sheet, and a plurality of inclined holes 2252 are provided along the third hollow portion 2251, and the inclined holes 2252 correspond to the vertical through holes 2243 one by one. The evenly diffused inert gas blows the inert gas to each spiral point through the plurality of inclined holes 2252, so as to provide a protective gas atmosphere for laser welding, such as nitrogen, argon or helium; the shaping pressing plate 226 includes a plurality of welding holes 2265 corresponding to the spiral holes of the metal sheet one by one, and the blowing direction of the inclined holes 2252 is aligned with the welding holes 2265;In this embodiment, the inert gas enters the third horizontal air inlet 2233 and the fourth horizontal air inlet 2234 through the first horizontal air inlet 2221 and the second horizontal air inlet 2222, respectively, and then enters the air path guide groove 2242 through the first vertical air inlet and the second vertical air inlet, and surrounds the contour of the metal sheet to be welded in a wrapping manner, and then blows to the inclined hole 2252 through the vertical through hole 2243, and finally blows to each spiral hole through the welding hole 2265. The wind speed of each inclined hole 2252 is consistent, which can realize laser welding of ultra-small and ultra-multiple spiral holes, and effectively avoid defects such as yellowing and blackening of the welding points. ;

[0064] In this embodiment, see Figures 1 to 17, the number of the metal sheets 5 to be welded is three pairs, each of which is provided with 32 spiral holes. It is necessary to laser weld 32*6=192 spiral holes 51 one by one. To ensure the consistency of laser welding, it is necessary to ensure the following two aspects at the same time: first, the uniformity of blowing of the inclined holes 2252, and second, to prevent the metal sheet 5 from deforming due to local high temperature during the laser welding process. To this end, in order to ensure the uniformity of blowing of the inclined holes 2252, the first horizontal air inlet hole 2221 is provided with four first branch air paths 2223, and the four first branch air paths 2223 are connected to the four third horizontal air inlet holes 2233 in a uniform manner, and each third horizontal air inlet hole 2233 is connected to a first vertical air inlet hole, and the air intake is uniform; the second horizontal air inlet hole 2222 is provided with four second branch air paths 2224, and the four second branch air paths 2224 are connected to the four fourth horizontal air inlet holes 2234 in a uniform manner, and each fourth horizontal air inlet hole 2234 is connected to a first vertical air inlet hole, and the air intake is uniform; in addition The air path plate 222 is further provided with a fifth horizontal air inlet hole 2225 and a sixth horizontal air inlet hole 2226 penetrating the air path plate 222. The step portion 2231 is provided with a plurality of seventh horizontal air inlet holes 2236 flush with and connected to the fifth horizontal air inlet hole 2225, and a plurality of eighth horizontal air inlet holes 2237 flush with and connected to the sixth horizontal air inlet hole 2226. Two seventh horizontal air inlet holes 2236 are evenly provided and are perpendicular to the fifth horizontal air inlet hole 2225. Two eighth horizontal air inlet holes 2237 are evenly provided and are perpendicular to the sixth horizontal air inlet hole 2226. The step portion 2231 is provided with a third vertical air inlet hole connected to the seventh horizontal air inlet hole 2236, and the step portion 2231 is provided with a fourth vertical air inlet hole connected to the eighth horizontal air inlet hole 2237; the first horizontal air inlet hole 2221, the second horizontal air inlet hole 2222, the fifth horizontal air inlet hole 2225 and the sixth horizontal air inlet hole 2226 respectively allow the inert gas to flow to the four frames of the step portion 2231, so that the inert gas is uniform when entering, and enters the gas path guide groove 2242 through the multiple vertical air inlet holes and surrounds the contour of the metal sheet to be welded in a wrapping manner. The inert gas is blown through the vertical through hole 2243 to the inclined hole 2252, the angle between the inclined hole 2252 and the horizontal plane is 45°, nitrogen, argon or helium is blown through the inclined hole 2252, the blowing wind speed of the inclined hole 2252 is 3m / s-8m / s, and finally blown to each spiral hole through the welding hole 2265. The wind speed of each inclined hole 2252 is consistent, which can realize laser welding of ultra-small and ultra-multiple spiral holes, and effectively avoid defects such as yellowing and blackening of welds. The blowing wind speed of the inert gas from the inclined hole 2252 can reach the protective atmosphere and prevent the weld from oxidizing. If the blowing wind speed is too large, the molten weld may be blown out of shape, affecting the welding quality.

[0065] Since each metal sheet 5 has 32 spiral holes 51 on its surface, during the laser welding process, each spiral hole of the metal sheet 5 will be melted through by the laser, resulting in local high temperature. If the metal sheet 5 is laser welded in a horizontal state, the metal sheet will have a certain degree of warping after the welding is completed. To solve this defect, a first upper convex arc surface 2261 and a second upper convex arc surface 2262 are arranged below the shaping pressing plate 226; the lower template 33 is provided with a third upper convex arc surface 331 corresponding to the first upper convex arc surface 2261, and the lower template 33 is provided with a third upper convex arc surface 332 corresponding to the second upper convex arc surface 2262. The fourth upper convex arc surface 332, when the shaping pressing plate 226 and the lower mold plate 33 are molded together, the three pairs of metal sheets 5 are clamped between the shaping pressing plate 226 and the lower mold plate 33, and the three metal sheets 5 on one side are clamped between the first upper convex arc surface 2261 and the third upper convex arc surface 331, and the three metal sheets 5 on the other side are clamped between the second upper convex arc surface 2262 and the fourth upper convex arc surface 332, so that the three pairs of metal sheets 5 are laser welded at a very small arc. After welding, each metal sheet 5 is still restored to a flat state; during laser welding, in order to timely extract the smoke generated by welding, see Fig.15 The shaping pressing plates 226 are arranged in pairs and are relatively thin as a whole. Each shaping pressing plate 226 presses three metal sheets 5 on one side. The shaping pressing plate 226 includes a thin end 2263 and a thick end 2264. The thickness of the thin end 2263 is 1mm-1.3mm, and the thickness of the thick end 2264 is 1.9mm-2.5mm. The two ends of the first upper convex arc surface 2261 and the second upper convex arc surface 2262 are the thin end 2263 and the thick end 2264 respectively, and the overall curvature is small; the welding hole 2265 is preferably a waist-shaped hole and the size of the welding hole 2265 is larger than the spiral hole 51. The larger and waist-shaped welding hole 2265 can discharge the smoke generated by laser welding in time, and can also dissipate the local heat generated by laser welding. The purged inert gas also helps to quickly dissipate heat.

[0066] Example 2

[0067] This embodiment discloses a specific implementation method of a laser welding process for ultra-small and ultra-multiple spiral holes.

[0068] Ultra-small and ultra-multiple spiral hole laser welding process, see Fig.18 , including the following steps:

[0069] Step S1: placing the metal sheet to be welded at a predetermined position, and determining the positions of a plurality of spiral welding points; specifically, each spiral welding point corresponds to a spiral hole 51 .

[0070] Step S2: Preset the laser welding path of the laser welding component, and the two closest spiral welding points in the welding path are separated by at least one spiral welding point; specifically, the laser of the laser welding component is vertically and one by one aligned with each spiral hole 51 for welding. To prevent local overheating, when welding the spiral holes 51, two adjacent spiral holes 51 cannot be adjacent in the welding path, and need to be separated by at least one spiral welding point, otherwise the welding quality will be affected due to local overheating.

[0071] Step S3: Press the metal sheet to be welded by the upper mold assembly and the lower mold assembly; specifically, laser welding is performed in a clamped state, and the laser welding assembly aligns the spiral hole 51 one by one through the hollow portion 4, the first hollow portion 2235, the second hollow portion 2241, the third hollow portion 2251 and the welding hole 2265.

[0072] Step S4: During laser welding, an inert gas is blown at an angle of 30°-60° toward each spiral welding point, and the wind speed of the inert gas is 3m / s-8m / s. Specifically, the wind speed of each inclined hole 2252 is consistent, which can achieve laser welding of ultra-small and ultra-multiple spiral holes, and effectively avoid defects such as yellowing and blackening of the welds; the blowing wind speed of the inert gas from the inclined hole 2252 can reach a protective atmosphere and prevent the welds from oxidizing. If the blowing wind speed is too high, the molten welds may be blown out of shape, affecting the welding quality.

[0073] The ultra-small and ultra-multiple spiral hole laser welding process disclosed in Example 2 adopts the ultra-small and ultra-multiple spiral hole laser welding device described in Example 1. Please refer to Example 1 and will not repeat it here.

Claims

1. Ultra-small and ultra-multi spiral hole laser welding device, characterized in that: It includes a laser welding assembly, an upper mold assembly and a lower mold assembly; The metal sheet to be welded is arranged between the upper die assembly and the lower die assembly; The upper die assembly comprises an upper die seat and a stripping assembly; The lower die assembly comprises a lower die base, a lower pad and a lower die plate; The stripping assembly includes a fixing plate, an air path plate, an air path transmission plate, an air path guide plate, an air blowing plate and a shaping pressing plate; The upper die base, the fixing plate and the gas circuit plate are respectively provided with hollow parts matching the welding range of the metal sheet; At least one first horizontal air inlet hole and at least one second horizontal air inlet hole are symmetrically arranged on both sides of the air path plate, the first horizontal air inlet hole passes through the air path plate and is connected to the hollow portion, and the second horizontal air inlet hole passes through the air path plate and is connected to the hollow portion; The air path transmission plate includes a step portion and a bottom plate, a third horizontal air inlet hole flush with and connected to the first horizontal air inlet hole and a fourth horizontal air inlet hole flush with and connected to the second horizontal air inlet hole are respectively arranged on both sides of the step portion, and the fixing plate blocks the top surface of the step portion; A first vertical air inlet hole communicating with the third horizontal air inlet hole is further provided on the step portion, a second vertical air inlet hole communicating with the fourth horizontal air inlet hole is further provided on the step portion, and a first hollow portion matching the outer contour of the metal sheet is provided on the bottom plate; The air path guide plate is provided with a second hollow portion matching the outer contour of the metal sheet, an air path guide groove is provided along the outer side of the contour of the second hollow portion, the air path guide groove is connected with the first vertical air inlet hole and the second vertical air inlet hole, and a plurality of vertical through holes are provided along the bottom surface of the air path guide groove; The blowing plate is provided with a third hollow portion matching the outer contour of the metal sheet, and a plurality of oblique holes are provided along the third hollow portion, and the oblique holes correspond to the vertical through holes one by one; The shaping press plate comprises a plurality of welding holes corresponding to the spiral holes of the metal sheet one by one, and the blowing direction of the inclined holes is aligned with the welding holes; Inert gas is introduced into the first horizontal air inlet hole and the second horizontal air inlet hole simultaneously.

2. The ultra-small ultra-multiple spiral hole laser welding device according to claim 1, characterized in that: The number of the metal sheets is three pairs, and each of the metal sheets is provided with 32 spiral holes.

3. The ultra-small ultra-multiple spiral hole laser welding device according to claim 1, characterized in that: The first horizontal air inlet hole is provided with four first branch air paths, and the second horizontal air inlet hole is provided with four second branch air paths.

4. The ultra-small ultra-multiple spiral hole laser welding device according to claim 1, characterized in that: The gas circuit board is further provided with a fifth horizontal air inlet hole and a sixth horizontal air inlet hole penetrating the gas circuit board; The step portion is provided with a plurality of seventh horizontal air inlet holes flush with and connected to the fifth horizontal air inlet holes, and a plurality of eighth horizontal air inlet holes flush with and connected to the sixth horizontal air inlet holes; A third vertical air inlet hole communicating with the seventh horizontal air inlet hole is further provided on the step portion, and a fourth vertical air inlet hole communicating with the eighth horizontal air inlet hole is further provided on the step portion.

5. The ultra-small ultra-multiple spiral hole laser welding device according to claim 1, characterized in that: The angle between the inclined hole and the horizontal plane is 45°.

6. The ultra-small ultra-multiple spiral hole laser welding device according to claim 1, characterized in that: The blowing wind speed of the inclined hole is 3m / s-8m / s.

7. The ultra-small ultra-multiple spiral hole laser welding device according to claim 6, characterized in that: The inclined holes are blown with nitrogen, argon or helium.

8. The ultra-small ultra-multiple spiral hole laser welding device according to any one of claims 1 to 7, characterized in that: A first upper convex curved surface and a second upper convex curved surface are provided below the shaping press plate; The lower template is provided with a third upper convex arc surface corresponding to the first upper convex arc surface, and the lower template is provided with a fourth upper convex arc surface corresponding to the second upper convex arc surface.

9. The ultra-small ultra-multiple spiral hole laser welding device according to claim 8, characterized in that: The shaping pressing plate comprises a thin end and a thick end, the thickness of the thin end is 1 mm-1.3 mm, and the thickness of the thick end is 1.9 mm-2.5 mm.

10. Ultra-small and ultra-multiple spiral hole laser welding process, characterized in that: The following steps are involved: Placing the metal sheets to be welded at predetermined positions and determining the positions of several spiral welding points; A laser welding path of a laser welding assembly is preset, wherein two closest spiral welding points in the welding path are spaced apart by at least one spiral welding point; Compressing the metal sheets to be welded by the upper die assembly and the lower die assembly; During laser welding, an inert gas is blown toward each spiral welding point at an angle of 30°-60°, and the wind speed of the inert gas is 3m / s-8m / s.

Citation Information

Patent Citations

  • Laser welding device

    CN112247347A

  • Aluminum plastic film shell punching device and working process thereof

    CN117483521A

  • Battery package busbar laser mirror welding stage that shakes

    CN205927555U

  • Double-station blanking die for automobile wheel cover stamping part