Thermal expansion phase change sample processing method
By cutting and grinding steel plate samples, combined with electric spark wire cutting technology, the problem of strict tolerance requirements for sample size in thermal expansion phase change test is solved, and high-precision and high-efficiency sample batch processing is achieved, suitable for thermal expansion phase Change experiment.
Patent Information
- Application Number
- CN202411314640.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-11-26
AI Technical Summary
The existing sample processing technology is difficult to meet the strict dimensional tolerance requirements of cylindrical samples in thermal expansion phase change tests, resulting in low processing accuracy and low efficiency, which cannot meet the test requirements.
By selecting steel plate samples, cutting and removing the hardened areas of the surrounding areas, milling and grinding, ensuring that the surface roughness and parallelism meet the requirements, and then using an electric spark wire cutting machine to cut out multiple cylindrical samples, which is directly applicable to Thermal expansion phase change test.
It improves sample processing accuracy and efficiency, reduces subsequent inspection and processing steps, and can produce dozens of samples that meet the standards at one time, meets batch processing needs, and reduces milling time and insert losses.
Smart Images

Figure CN119017022A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of sample processing, and in particular to a thermal expansion phase change sample processing method. Background Art
[0002] Phase transformation test is mainly used to determine the cooling phase transformation curve of supercooled austenite of steel. The push rod method in the thermal expansion method of phase transformation test is one of the most commonly used detection methods. The required sample is a cylindrical specimen with 10±0.05mm×Ф4mm or Ф5mm and the surface parallelism of both ends of the sample is ±0.01mm. The sample size tolerance requirements are strict and the sample processing difficulty coefficient is high.
[0003] Conventional sample preparation methods have low sample processing accuracy, which makes it impossible to 100% meet the phase change sample testing requirements. Since conventional sample preparation methods only complete the cutting of a single sample each time, the single sample after cutting needs to be tested in terms of size, parallelism, surface roughness, etc., and the test results meet the sample requirements before the sample can be used for subsequent phase change tests. This method has the disadvantages of being time-consuming and inefficient. Summary of the invention
[0004] In order to solve the above problems, the present application provides a method for processing a thermal expansion phase change sample.
[0005] The present application provides a method for processing a thermal expansion phase change specimen, comprising: selecting a steel plate specimen for specimen preparation, cutting and removing the hardened processing zone on the four sides of the steel plate specimen, milling the two side surfaces in the thickness direction of the steel plate specimen, wherein the roughness Ra of the two side surfaces in the thickness direction of the steel plate specimen is ≤0.8 μm after milling, grinding the two side surfaces in the thickness direction of the steel plate specimen, wherein the thickness of the steel plate specimen is 10±0.05 mm, the parallelism of the two side surfaces in the thickness direction is 0.01 mm, and the roughness Ra is ≤0.4 μm after grinding, and cutting the steel plate specimen into a plurality of cylindrical specimens for use as thermal expansion phase change specimens.
[0006] In some embodiments, in the step of selecting a steel plate sample for sample preparation, the steel plate sample is selected at a position in the steel billet that can represent material characteristics based on national standards, technical protocols, and customer requirements.
[0007] In some embodiments, after selecting the steel plate sample, the steel plate sample is subjected to appearance inspection, the appearance inspection includes edge flatness defect inspection, and the detected edge flatness defects are removed.
[0008] In some embodiments, the edge flatness defects include, but are not limited to, iron oxide nodules or burrs, which are removed by grinding.
[0009] In some embodiments, the steel plate sample is milled to a thickness of 11 mm ± 0.2 mm.
[0010] In some embodiments, when grinding the two side surfaces of the steel plate sample in the thickness direction, rough grinding and fine grinding are performed sequentially, the feed amount of rough grinding does not exceed 0.05 mm / time, and the feed amount of fine grinding is 0.01 mm / time.
[0011] In some embodiments, rough grinding is performed until the machining allowance of the steel plate sample is 0.1 mm, followed by fine grinding.
[0012] In some embodiments, when a steel plate sample is cut into a plurality of cylindrical specimens, a wire electric discharge machine is used to perform multiple rows of cutting, and each row sequentially cuts a plurality of cylindrical specimens from the same side toward the other side.
[0013] In some embodiments, the cutting positions of two adjacent cylindrical specimens in each row of the steel plate sample are spaced 1 mm apart.
[0014] In some embodiments, the diameter of the cylindrical specimen is 4 mm or 5 mm.
[0015] The beneficial effects of the present application are as follows: a method for processing a thermal expansion phase change sample is provided. After selecting a steel plate sample for sample preparation, the steel plate sample is sawed or sheared by a shearing machine, and the hardened areas on the four sides of the steel plate sample are sawed or sheared in sequence, which can eliminate the surface hardened area and heat-affected area of the steel plate sample, while ensuring the flatness of the edge of the steel plate sample. The steel plate sample after sawing or shearing retains sufficient processing allowance. The sawing or shearing also reduces the processing time of the steel plate sample in the subsequent milling machine and the loss of the alloy blade of the milling machine, thereby improving the milling work efficiency; after sawing or shearing the hardened areas on the four sides of the steel plate sample, the surfaces on both sides of the thickness direction of the steel plate sample are milled, and the surface roughness Ra is ≤0.8μm when the milling is completed, and then the steel plate sample is cut. The surfaces on both sides of the plate sample in the thickness direction are ground. When grinding is completed, the thickness of the steel plate sample is 10±0.05mm, the parallelism of the surfaces on both sides in the thickness direction is 0.01mm, and the roughness is ≤0.4μm. A plurality of cylindrical specimens are cut from the steel plate sample by an electric spark wire cutting machine. After that, there is no need to detect and process the size, parallelism, surface roughness, etc. of each sample. The prepared cylindrical specimens can be directly used as thermal expansion phase change specimens. The application scheme introduces the processing precautions in detail from the aspects of processing accuracy, parallelism and surface roughness. Dozens of cylindrical specimens can be produced at a time, which is suitable for batch processing of specimens. The produced specimens meet the inspection requirements of subsequent phase change tests, and have the advantages of high processing accuracy, short time consumption and high efficiency as a whole. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for describing the embodiments are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention.
[0017] Figure 1 A flow chart of a thermal expansion phase change sample processing method provided in this application. DETAILED DESCRIPTION
[0018] The phase transformation test is mainly used to determine the cooling phase transformation curve of supercooled austenite of steel. It can systematically reflect the influence of cooling rate on the starting point of phase transformation, the degree of phase transformation and the products obtained by phase transformation. It is an important basis for studying the theory of solid-state phase transformation, effectively controlling the heat treatment cooling process of steel and the microstructure and properties after heat treatment, and has guiding significance for practical applications in product development and process research.
[0019] The push rod method in the thermal expansion method of phase change test is the most commonly used detection method. Its measurement principle is to use a push rod-type fused quartz or high-purity alumina expansion instrument to detect the length change of the solid sample relative to its carrier. Due to the high sensitivity of the push rod method, the required sample is a cylindrical sample of 10±0.05mm×Ф4mm or Ф5mm and the sample surface parallelism is ±0.01mm. The sample size tolerance requirements are strict and the processing difficulty coefficient is high. Conventional sample processing and preparation methods can no longer meet the needs of subsequent experiments.
[0020] In order to ensure the accuracy of the measurement data of the phase change test, it is necessary to ensure that the geometric size parameters, parallelism parameters, and surface roughness parameters of the produced and processed samples are within the allowable range, and a large number of samples need to be provided for multiple tests. To this end, the present application provides a thermal expansion phase change sample processing method for producing thermal expansion phase change samples that meet the requirements of geometric size parameters, parallelism parameters, and surface roughness parameters, and applying the thermal expansion phase change samples to the phase change test of determining the supercooled austenite cooling phase transformation curve of steel.
[0021] It should be noted that the samples in this embodiment are all thermal expansion phase change samples.
[0022] In this application, a steel plate sample for sample preparation is first selected. Except for special provisions, according to national standards, technical agreements and customer needs, a position that can represent the material characteristics is selected in the steel billet, and the steel plate sample is taken out from the steel billet by flame cutting to complete the steel plate sample selection process. The selection method can be flame cutting to cut the steel plate sample from the steel billet.
[0023] In order to ensure the accuracy and effectiveness of the test data, the client selects the number of steel plate samples that need to be processed and prepared based on the standards and actual conditions, so as to prepare a sufficient number of thermal expansion phase change specimens that meet the parameter requirements.
[0024] After preparing a steel plate sample that can represent the material characteristics, the steel plate sample is inspected for appearance. When inspecting the appearance of the steel plate sample, the edge flatness of the steel plate sample is mainly checked to determine whether the current steel plate sample meets the sample processing requirements.
[0025] In the method of cutting a steel plate sample from a steel billet by flame cutting, the steel plate sample will have defects on the periphery of the steel plate sample caused by flame cutting of the steel billet, which can be called edge flatness defects, and will cause work hardening areas on the periphery of the steel plate sample. When there are defects on the periphery of the steel plate sample caused by flame cutting of the steel billet, the edge flatness defects include but are not limited to iron oxide nodules and burrs, pretreatment is required to remove the edge flatness defects on the periphery of the steel plate sample, and the pretreatment method can be grinding, and the iron oxide nodules or burrs are removed by grinding.
[0026] When the steel plate sample passes the appearance inspection, the specific steel plate sample processing process begins. According to GB / T2975 "Steel and Steel Product Mechanical Properties Test Sampling Location and Sample Preparation Requirements", the surface work hardening and heat affected zone of the steel plate sample should be removed during the processing of the steel plate sample; after the processing is completed and the sample is prepared, the size and shape of the sample should be within the tolerance range specified in the test standard and meet the corresponding test method requirements. The tolerance range specified in the test standard and the corresponding test method requirements include the above-mentioned requirements for the geometric size parameters, parallelism parameters, and surface roughness parameters of the sample.
[0027] During the sample processing, the hardened areas on the four sides of the steel plate sample are cut and removed in combination with the actual laboratory conditions and the processing equipment capabilities. Specifically, the hardened areas on the four sides of the steel plate sample can be cut and removed by a sawing machine or a shearing machine. When a sawing machine is used, the hardened areas on the four sides of the steel plate sample are sawed in sequence by the sawing machine. When a shearing plate is used, the hardened areas on the four sides of the steel plate sample are sheared in sequence by the shearing machine. Through the above-mentioned steps of cutting and removing the hardened areas on the four sides of the steel plate sample, the surface hardened area and the heat affected zone of the steel plate sample can be eliminated, while ensuring the flatness of the edge of the steel plate sample.
[0028] It should be noted that the steel plate sample retains sufficient processing allowance after cutting and removing the hardened zone on the four sides of the steel plate sample. By cutting and removing the hardened zone on the four sides of the steel plate sample, the processing time of the steel plate sample in the subsequent milling machine is reduced, the loss of the milling machine alloy blade is reduced, and it is beneficial to improve the milling work efficiency.
[0029] After sawing or shearing the hardened area around the periphery of the steel plate sample, the upper and lower surfaces of the steel plate sample are milled. The upper and lower surfaces of the steel plate sample are the two side surfaces in the thickness direction of the steel plate sample. When milling the upper and lower surfaces of the steel plate sample, according to factors such as the material to be processed, the type of tool and the cutting conditions, select the appropriate milling machine feed speed, feed depth and feed amount, which is conducive to reducing the loss of the milling machine alloy blade and the depth of the milling cutter marks on the sample surface. When the upper and lower surfaces of the steel plate sample are milled, the roughness of the upper and lower surfaces of the steel plate sample is Ra≤0.8μm.
[0030] The steel plate sample after milling should retain sufficient machining allowance for subsequent grinding operations on the upper and lower surfaces of the steel plate sample to ensure the subsequent surface grinding effect. In some embodiments, the inventors studied the milling results of the upper and lower surfaces of the steel plate sample in the present application in actual production, and limited the steel plate sample to be milled to a thickness of 11mm±0.2mm in the milling steps of the upper and lower surfaces of the steel plate sample, which not only ensures the machining allowance for subsequent grinding and the subsequent surface grinding effect, but also ensures that the grinding amount is at a relatively small amount, which is conducive to reducing the grinding processing time.
[0031] Since the minimum processing accuracy of the milling machine is 0.1mm, it cannot meet the accuracy requirements of the phase change specimen height of 10±0.05mm and the surface parallelism of ±0.01mm. After milling the upper and lower surfaces of the steel plate sample, the steel plate sample is placed on a surface grinder and the upper and lower surfaces of the steel plate sample are ground. The upper and lower surfaces of the steel plate sample are first rough ground and then fine ground.
[0032] In order to avoid the phenomenon of surface gelatinization caused by excessive feed, the feed of rough grinding shall not exceed 0.05mm / time. After the machining allowance is 0.1mm, fine grinding shall be carried out, and the feed of fine grinding shall be 0.01mm / time. Fine grinding shall be carried out until the thickness of the steel plate sample is 10±0.05mm, the parallelism of the upper and lower surfaces of the steel plate sample is 0.01mm, and the roughness of the upper and lower surfaces of the steel plate sample is Ra≤0.4μm.
[0033] After the upper and lower surfaces of the steel plate sample are ground by a surface grinder, they can meet the sample height requirements for the phase change test. Since the phase change sample size required for the test is a cylindrical sample of Ф4mm or Ф5mm, an electric spark wire cutting machine is required to cut the sample into a cylindrical sample of Ф4mm or Ф5mm. In the present application, an electric spark wire cutting machine is used to cut a steel plate sample into multiple cylindrical samples used as thermal expansion phase change samples. A steel plate sample can be cut into dozens of cylindrical samples. After that, there is no need to test and process each sample in terms of size, parallelism, surface roughness, etc. The manufactured cylindrical sample can be directly used as a thermal expansion phase change sample.
[0034] In summary, this application scheme introduces in detail the processing precautions from the aspects of processing accuracy, parallelism and surface roughness. It can produce dozens of cylindrical specimens at a time, which is suitable for batch processing of specimens. The produced specimens meet the requirements of subsequent phase change test inspections. Overall, it has the advantages of high processing accuracy, short time consumption and high efficiency.
[0035] Thermal expansion phase change specimens are used to conduct phase change tests, providing accurate and effective data support for new product development and process adjustments.
[0036] When using an electric spark wire cutting machine to cut a steel plate sample, the inventor studied the cutting method, designed and compiled a "single-line" program, cut multiple rows of steel plate samples, and each row is from the same side to the other side, and multiple cylindrical specimens are cut out from each row in sequence. In some embodiments, when the electric spark wire cutting machine cuts the steel plate sample, the cutting positions of two adjacent cylindrical specimens in each row are separated by 1 mm. After cutting the previous cylindrical specimen, the position of the previous cylindrical specimen in the steel plate sample is translated by 1 mm to cut out the cylindrical specimen. After the cutting of the cylindrical specimens in the previous row is completed, the cutting step of the next row of cylindrical specimens is performed.
[0037] Specifically, the steel plate sample is clamped to the sample table of the wire EDM machine, and starting from one side of the steel plate sample, which refers to the length side or the width side, multiple cylindrical samples are cut in sequence along the transverse direction from one side to the other side, with a spacing of 1mm between two adjacent cylindrical samples; after a row of cylindrical samples is cut, the electrode wire returns to the original path and returns to the above-mentioned side from the other side, and then the next row of cylindrical samples is cut. The number of rows to be cut and the number of samples to be cut in each row are selected according to the stroke of the wire EDM machine and the required number of phase change samples.
[0038] The cutting method of the electric spark wire cutting machine tool using the "single-line" program of the present application avoids the problem of material falling off the remaining plate surface of the steel plate sample during the cutting process.
[0039] The cutting method of the electric spark wire cutting machine with the above-mentioned "single-line" program has changed the original single cutting method of the sample. This scheme can quickly cut multiple samples at one time, which is suitable for batch processing of samples, and the cut samples can be traced back to the original position.
[0040] Although the preferred embodiments of the present invention have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.
[0041] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A method for processing a thermal expansion phase change sample, characterized in that: include: Select the steel plate sample for specimen preparation; After selecting the steel plate sample, cutting and removing the work hardening area around the periphery of the steel plate sample; After cutting and removing the hardened areas on the four sides of the steel plate sample, the surfaces on both sides of the steel plate sample in the thickness direction are milled, and the roughness Ra of the surfaces on both sides of the steel plate sample in the thickness direction is ≤0.8 μm after milling. After milling the two side surfaces of the steel plate sample in the thickness direction, grinding the two side surfaces of the steel plate sample in the thickness direction, when grinding is completed, the thickness of the steel plate sample is 10±0.05mm, the parallelism of the two side surfaces in the thickness direction is 0.01mm, and the roughness Ra≤0.4μm; After grinding the surfaces on both sides of the steel plate sample in the thickness direction, the steel plate sample is cut into a plurality of cylindrical samples used as thermal expansion phase change samples.
2. The thermal expansion phase change sample processing method according to claim 1, characterized in that: In the step of selecting a steel plate sample for sample preparation, the steel plate sample is selected at a position in the steel billet that can represent material characteristics according to national standards, technical protocols and customer requirements.
3. The thermal expansion phase change sample processing method according to claim 2, characterized in that: After the steel plate sample is selected, the steel plate sample is subjected to appearance inspection, wherein the appearance inspection includes edge flatness defect inspection, and the detected edge flatness defects are removed.
4. The thermal expansion phase change sample processing method according to claim 3, characterized in that: The edge flatness defects include but are not limited to iron oxide nodules or burrs, which are removed by grinding.
5. The thermal expansion phase change sample processing method according to claim 1, characterized in that: The steel plate sample is milled to a thickness of 11 mm ± 0.2 mm.
6. The thermal expansion phase change sample processing method according to claim 1, characterized in that: When grinding the two side surfaces in the thickness direction of the steel plate sample, rough grinding and fine grinding are performed in sequence, the feed amount of the rough grinding does not exceed 0.05 mm / time, and the feed amount of the fine grinding is 0.01 mm / time.
7. The thermal expansion phase change sample processing method according to claim 6, characterized in that: The rough grinding is performed until the machining allowance of the steel plate sample is 0.1 mm, and then the fine grinding is performed.
8. The thermal expansion phase change sample processing method according to claim 1, characterized in that: When the steel plate sample is cut into a plurality of the cylindrical specimens, a wire-cut electric discharge machine is used to perform multiple-row cutting, and each row sequentially cuts a plurality of the cylindrical specimens from the same side toward the other side.
9. The thermal expansion phase change sample processing method according to claim 8, characterized in that: The cutting positions of two adjacent cylindrical specimens in each row of the steel plate sample are spaced 1 mm apart.
10. The thermal expansion phase change sample processing method according to claim 1, characterized in that: The diameter of the cylindrical test piece is 4 mm or 5 mm.
Citation Information
Patent Citations
Method for processing standard impact test sample with Charpy V-notch
CN101592569A
Flame cutting method for high-carbon-equivalent thick steel plate steel plate
CN104107971A
Preparation method of compound steel board base material tensile specimen
CN108871903A
Sample preparation method for static phase change test
CN111024465A
Frame components machining method, involves machining hardened guide rails by purifying milling using front milling tools and / or peripheral milling tools with geometrically determined cuts, after preprocessing of frame components
DE102010045075A1
Cited By