Manufacturing method of aviation bomb shell
By using seamless pipe blanks of different sizes to machining and spin forming of the shell shell, combined with heat rotor and induction heating technology, the problems of large materials and long time in traditional manufacturing methods are solved, and material savings and cost are achieved Reduced effect.
Patent Information
- Application Number
- CN202411461341.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-18
- Publication Date
- 2024-11-29
AI Technical Summary
The traditional manufacturing method of aircraft shells uses large materials and long machine-added time, resulting in high manufacturing costs.
The raw material is processed by seamless pipe blanks of different sizes. The blanks are formed by machining and rotating the rotating machine to form preformed blanks with thick ends at both ends, thin in the middle or thin at one end, and thermal forming is performed using a heat rotating machine and an induction heating furnace. Welding with the split body to form the shell.
Save materials and machining time, reduce manufacturing costs, and improve economic benefits.
Smart Images

Figure CN119035397A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of bomb shell manufacturing, in particular to a method for manufacturing a bomb shell. Background Art
[0002] An aerial bomb is an air-dropped bomb carried by an airplane. The shell of the aerial bomb is a container for the explosive object. The shell has a corn-shaped appearance, that is, the diameter of the head gradually decreases, the middle is straight, the diameter of the tail is slightly reduced, the thin wall is hollow, and the two ends are thickened because they need to be connected to other parts and have threads. Such a structure brings great difficulties to manufacturing. For a long time, the manufacturing of aerial bomb shells generally adopts integral forging, machining and split forming and welding methods. Large bomb bodies are mostly made by integral forging and machining. Usually, thick-walled tubes are selected at both ends forged and formed, and then machined into the shape of the shell. This forming method is a traditional manufacturing method of the shell, which uses a lot of materials, takes a long machining time, and has a very high manufacturing cost. Therefore, the present invention proposes a manufacturing method for aerial bomb shells to solve the above problems. Summary of the invention
[0003] The purpose of the present invention is to provide a method for manufacturing a bomb shell, so as to solve the problems of the traditional shell manufacturing method proposed in the above background technology, such as large amount of materials, long machining time and very high manufacturing cost.
[0004] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a method for manufacturing an aerial bomb shell, comprising processing of raw blanks and processing of prefabricated blanks; The raw material processing comprises the following steps: S1. Use seamless tubes of different sizes as raw materials; S2, machining the original blank to eliminate dimensional errors; S3, the machined raw blank is pressed into a blank by a strong spinning machine to form a variable cross-section preform with thick ends and thin middle or thick one end and thin remaining material; The preform processing includes preform integral spinning forming processing and preform split spinning forming processing; The preform integral spinning forming process comprises the following steps: S4a, clamping the preform with thick ends and thin middle on the hot spinning machine, heating one end of the preform and supplementing heating through the induction heating furnace and the flame heating device until the preform hot forming temperature is reached; S5a, spinning one end of the preform heated by the hot spinning machine into a desired shape, and then spinning the other end of the preform into the desired shape by the same method as in step S4a; The preform split spinning forming process comprises the following steps: S4b, clamping a preform with one end thick and the remaining material thin on a hot spinning machine, heating the thick end of the preform and supplementing the heat through an induction heating furnace and a flame heating device until the preform hot forming temperature is reached, and spinning the heated end of the preform into a desired shape through the hot spinning machine; S5b, performing two-stage split welding or three-stage split welding on the preform processed in step S4b; Two-stage split welding: take two preforms processed in step S4b and weld them together; Three-stage split welding: take two prefabricated blanks processed by step S4b and one original blank machined by step S2, and then weld the three together to form.
[0005] As a preferred solution of the present invention, in step S2, the process of machining the original blank is: cutting and grinding the end of the original blank to remove burrs and eliminate the dimensional error of the original blank.
[0006] As a preferred solution of the present invention, in step S3, the preform with thick ends and thin middle has the required size of the entire bomb shell.
[0007] As a preferred solution of the present invention, in step S3, the preform with one end thick and the remaining material thin includes three size structures, one with the size required for the head of the bomb shell, the second with the size required for the head and middle of the bomb shell, and the third with the size required for the tail of the bomb shell; The second and third size structures are used for two-section split welding, and the first and third size structures are used for three-section split welding.
[0008] As a preferred embodiment of the present invention, in step S4a and step S4b, the preform hot forming temperature is 1200°C.
[0009] As a preferred embodiment of the present invention, in step S5a, the spinning process of the preform with thick ends and thin middle is as follows: one end of the preform is spun into a conical structure of the bomb shell head, and the other end of the preform is spun into a bowl-shaped structure of the bomb shell tail.
[0010] As a preferred embodiment of the present invention, in step S4b, the spinning process of the preform with one end thick and the remaining material thin is as follows: the thick end of the preform with the first and second size structures is spun into a conical structure of the head of the bomb shell, and the thick end of the preform with the third size structure is spun into a bowl-shaped structure at the tail of the bomb shell.
[0011] As a preferred embodiment of the present invention, in step S5b, the welding process of the two-stage split welding is: welding the unspun end of the preform of the second size structure with the unspun end of the preform of the third size structure to form the bomb shell structure.
[0012] As a preferred embodiment of the present invention, in step S5b, the original blank has the required size for the middle part of the bomb shell, and the welding process of the three-stage split welding is as follows: the unspun end of the preform of the first size structure and the unspun end of the preform of the third size structure are respectively welded to the two ends of the original blank to form the bomb shell structure.
[0013] Compared with the prior art, the present invention has the following beneficial effects: The thickened parts at both ends of the preform of the present invention are reserved by the strong spinning process to ensure that the material used for the deformation and thickening of the head and tail of the preform is sufficient. The shell spinning is completed by a hot spinning machine. First, one end (such as the tail end) is heated and hot-shrinking spinning is performed, and then the other end (such as the front end) is heated and hot-shrinking spinning is performed. Compared with traditional spinning or extrusion methods, this process saves a lot of materials and machining time, reduces manufacturing costs, and has considerable economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 is a flow chart of the present invention; Figure 2 It is a schematic structural diagram of the original blank of the present invention; Figure 3 It is a schematic structural diagram of the preform of the present invention; Figure 4 It is a structural schematic diagram of the preform during the overall spinning process of the present invention when one end is spun; Figure 5 It is a schematic structural diagram of the preform during the overall spinning process of the present invention when both ends are spun; Figure 6 It is a schematic diagram of the structure of the preform during two-stage split spinning forming of the present invention; Figure 7 It is a schematic diagram of the structure of the preform during three-stage split spinning forming of the present invention. DETAILED DESCRIPTION
[0015] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0016] Embodiment 1
[0017] See also Figure 1-Figure 5 , a method for manufacturing an aircraft bomb shell, including raw billet processing and prefabricated billet processing; The raw material processing comprises the following steps: S1. Use seamless tubes of different sizes as raw materials; S2, machining the original blank to eliminate dimensional errors; The process of machining the original blank is as follows: cutting and grinding the end of the original blank to remove burrs and eliminate the dimensional error of the original blank; S3, the machined raw blank is pressed into a blank by a strong spinning machine to form a variable cross-section preform with thick ends and thin middle; The preform integral spinning forming process comprises the following steps: S4a, clamping the preform with thick ends and thin middle on the hot spinning machine, heating one end of the preform and supplementing heating through the induction heating furnace and the flame heating device until the preform hot forming temperature is reached, specifically, the preform hot forming temperature is 1200°C; S5a, spinning one end of the preform heated by the hot spinning machine into a desired shape, and then spinning the other end of the preform into the desired shape by the same method as in step S4a; In step S5a, the spinning process of the preform with thick ends and thin middle is: one end of the preform is spun into a conical structure of the bomb shell head, and the other end of the preform is spun into a bowl-shaped structure of the bomb shell tail.
[0018] Embodiment 2
[0019] See also Figure 1-Figure 3 as well as Figure 6 , a method for manufacturing an aircraft bomb shell, including raw billet processing and prefabricated billet processing; The raw material processing comprises the following steps: S1. Use seamless tubes of different sizes as raw materials; S2, machining the original blank to eliminate dimensional errors; The process of machining the original blank is as follows: cutting and grinding the end of the original blank to remove burrs and eliminate the dimensional error of the original blank; S3, the machined raw blank is pressed into a blank by a strong spinning machine to form a variable cross-section preform with a thick end and a thin residual material; In step S3, the preform with thicker end and thinner residual material includes three size structures, one with the size required for the head of the bomb shell, the second with the size required for the head and middle of the bomb shell, and the third with the size required for the tail of the bomb shell; The second and third size structures are used for two-stage split welding, and the first and third size structures are used for three-stage split welding; The preform split spinning forming process comprises the following steps: S4b, clamping a preform with one end thick and the remaining material thin on a hot spinning machine, heating the thick end of the preform and supplementing heating it through an induction heating furnace and a flame heating device until the preform hot forming temperature is reached. Specifically, the hot forming temperature of the preform is 1200° C. The heated end of the preform is spun into a desired shape through the hot spinning machine; In step S4b, the spinning process of the preform with thicker end and thinner residual material is as follows: the thicker end of the preform with the first and second size structures is spun into a conical structure of the bomb shell head, and the thicker end of the preform with the third size structure is spun into a bowl-shaped structure of the bomb shell tail; S5b, performing two-stage split welding on the preform processed in step S4b; Two-stage split welding: take two preforms processed in step S4b and weld them together; The welding process of the two-stage split welding is: welding the unspun end of the preform of the second size structure to the unspun end of the preform of the third size structure to form the bomb shell structure.
[0020] Embodiment 3
[0021] See also Figure 1-Figure 3 as well as Figure 7 , a method for manufacturing an aircraft bomb shell, including raw billet processing and prefabricated billet processing; The raw material processing comprises the following steps: S1. Use seamless tubes of different sizes as raw materials; S2, machining the original blank to eliminate dimensional errors; S3, the machined raw blank is pressed into a blank by a strong spinning machine to form a variable cross-section preform with thick ends and thin middle or thick one end and thin remaining material; In step S3, the preform with thicker end and thinner residual material includes three size structures, one with the size required for the head of the bomb shell, the second with the size required for the head and middle of the bomb shell, and the third with the size required for the tail of the bomb shell; The second and third size structures are used for two-stage split welding, and the first and third size structures are used for three-stage split welding; The preform split spinning forming process comprises the following steps: S4b, clamping a preform with one end thick and the remaining material thin on a hot spinning machine, heating the thick end of the preform and supplementing heating it through an induction heating furnace and a flame heating device until the preform hot forming temperature is reached. Specifically, the hot forming temperature of the preform is 1200° C. The heated end of the preform is spun into a desired shape through the hot spinning machine; In step S4b, the spinning process of the preform with thicker end and thinner residual material is as follows: the thicker end of the preform with the first and second size structures is spun into a conical structure of the bomb shell head, and the thicker end of the preform with the third size structure is spun into a bowl-shaped structure of the bomb shell tail; S5b, performing three-stage split welding on the prefabricated blank processed in step S4b; Three-stage split welding: take two prefabricated blanks processed in step S4b and one original blank machined in step S2, the original blank having the required size for the middle part of the bomb shell, and then weld the three together to form; The welding process of the three-stage split welding is as follows: the unspun end of the preform of the first size structure and the unspun end of the preform of the third size structure are respectively welded to the two ends of the original blank to form the bomb shell structure.
[0022] The specific process of spinning the original blank in the first, second and third embodiments of the present invention through a strong spinning machine to form a preform with a variable cross-section that is thick at both ends and thin in the middle or thick at one end and thin at the rest is as follows: 1. Fix the blank: First, put the original blank on the mold of the strong spinning machine and fix it; 2. Spinning: The spindle of the spinning machine drives the core mold and the blank to rotate, and at the same time, the spinning wheel or the driving rod starts to extrude the tube body blank from the end. Under the combined action of the feeding motion of the spinning wheel and the rotating motion of the blank, the local plastic deformation gradually expands to the entire surface of the blank and adheres closely to the mold to complete the spinning process of the part; Plastic deformation: During the spinning process, the metal flows along the warp direction, which is equivalent to the metal being rolled during the spinning process. In this way, the blank undergoes plastic deformation point by point, and finally forms a tube body that is thick at both ends and thin in the middle, or thick at one end and thin at the rest. Forming characteristics: The high-power spinning process mainly relies on thinning the thickness of the blank to achieve forming, and the outer diameter of the blank remains basically unchanged. This process can easily produce various rotationally symmetrical thin-walled rotating parts and various pipe fittings.
[0023] The specific process of spinning the preform into the desired shape by the hot spinning machine is as follows: 1. Clamp the blank: clamp the preform on the core mold of the hot spinner. The design of the core mold should match the shape of the head and tail of the bomb shell; 2. Heating the blank: Heat the preform to the hot forming temperature so that it has sufficient plastic deformation capacity. The heating temperature should be adjusted according to the type and characteristics of the material; 3. Spinning head: Start the hot spinning machine to make the core mold rotate with the main shaft, and the spinning wheel moves along the core mold to apply pressure to the tube body blank, so that it deforms along the shape of the core mold to form the shape of the bomb shell head; During the spinning process, the pressure and speed of the spinning wheel need to be controlled to ensure the accuracy of the head shape and surface quality; 4. Spinning tail: After completing the spinning of the head, turn the preform over so that the other end faces the spinning machine; Similarly, the hot spinner is started to rotate the core mold along the main shaft, and the spinner moves along the core mold to apply pressure to the tube blank, so that it deforms along the shape of the core mold to form the shape of the tail of the bomb shell; 5. Cooling and inspection: After spinning is completed, allow the tube to cool naturally or undergo appropriate cooling treatment, and check the shape, size and surface quality of the head and tail of the bomb shell to ensure that it meets the design requirements.
[0024] The first part of the present invention heat treats seamless tube blanks of different sizes to make the metal tubes in the best plastic state; The second step partially determines the dimensions of different raw billets, i.e. the length, inner diameter and outer diameter of the raw billets, and then processes the seamless tube billets into raw billets of corresponding dimensions; The third part determines the strong spinning process, designs the strong spinning tooling, the strong spinning process material, designs the spinning wheel structure, designs the strong spinning process parameters, and obtains high-quality parts. After inspection, it is determined as follows: 1. Determine the size and accuracy of the core mold, and process it according to the design size to the accuracy of the drawing; 2. Design the roller and determine the front angle and R value of the roller; 3. Determine the strong spinning process parameters, i.e. spindle speed, feed rate, spinning passes, etc.; 4. Make blanks and correct the spinning process parameters during the blank making process; The fourth part is the transformation of hot spinning equipment, adding a mobile induction heating furnace system to achieve online rapid heating, adding a fire auxiliary heating system to achieve hot forging insulation. And system cooling lubrication, thermal protection, etc.; The fifth part is to design the hot-sealing tooling, fixtures, rotary wheels, etc.; The sixth part designs the process curve of the revolving head, as well as process parameters such as pass number, speed, and pressing amount; The seventh part designs the process curve of the spiral tail, as well as process parameters such as pass number, speed, and reduction; Part 8 Physical inspection, performance, flaw detection, etc. of the bomb shell after forming.
[0025] The comparison of the blanking weight of the bomb shell manufactured by the spinning method adopted by the present invention and the bomb shell manufactured by the traditional forging and extrusion method is shown in the following table:
[0026] It can be seen from the above table that compared with the traditional spinning or extrusion method, the present invention saves a lot of materials and machining time, reduces the manufacturing cost, and has considerable economic benefits.
[0027] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.
Claims
1. A method for manufacturing a bomb shell, characterized in that: Including raw material processing and prefabricated billet processing; The raw material processing comprises the following steps: S1. Use seamless tubes of different sizes as raw materials; S2, machining the original blank to eliminate dimensional errors; S3, the machined raw blank is pressed into a blank by a strong spinning machine to form a variable cross-section preform with thick ends and thin middle or thick one end and thin remaining material; The preform processing includes preform integral spinning forming processing and preform split spinning forming processing; The preform integral spinning forming process comprises the following steps: S4a, clamping the preform with thick ends and thin middle on the hot spinning machine, heating one end of the preform and supplementing heating through the induction heating furnace and the flame heating device until the preform hot forming temperature is reached; S5a, spinning one end of the preform heated by the hot spinning machine into a desired shape, and then spinning the other end of the preform into the desired shape by the same method as in step S4a; The preform split spinning forming process comprises the following steps: S4b, clamping a preform with one end thick and the remaining material thin on a hot spinning machine, heating the thick end of the preform and supplementing the heat through an induction heating furnace and a flame heating device until the preform hot forming temperature is reached, and spinning the heated end of the preform into a desired shape through the hot spinning machine; S5b, performing two-stage split welding or three-stage split welding on the preform processed in step S4b; Two-stage split welding: take two preforms processed in step S4b and weld them together; Three-stage split welding: take two prefabricated blanks processed by step S4b and one original blank machined by step S2, and then weld the three together to form.
2. The method for manufacturing a bomb shell according to claim 1, characterized in that: In step S2, the process of machining the raw material is: cutting and grinding the end of the raw material to remove burrs and eliminate the dimensional error of the raw material.
3. The method for manufacturing a bomb shell according to claim 1 or 2, characterized in that: In step S3, the preform with thick ends and thin middle has the required size of the bomb shell as a whole.
4. The method for manufacturing a bomb shell according to claim 3, characterized in that: In step S3, the preform with thicker end and thinner residual material includes three size structures, one with the size required for the head of the bomb shell, the second with the size required for the head and middle of the bomb shell, and the third with the size required for the tail of the bomb shell; The second and third size structures are used for two-section split welding, and the first and third size structures are used for three-section split welding.
5. The method for manufacturing a bomb shell according to claim 4, characterized in that: In step S4a and step S4b, the preform hot forming temperature is 1200°C.
6. The method for manufacturing a bomb shell according to claim 5, characterized in that: In step S5a, the spinning process of the preform with thick ends and thin middle is: one end of the preform is spun into a conical structure of the bomb shell head, and the other end of the preform is spun into a bowl-shaped structure of the bomb shell tail.
7. The method for manufacturing a bomb shell according to claim 4 or 6, characterized in that: In step S4b, the spinning process of the preform with one end thick and the remaining material thin is: the thick end of the preform with the first and second size structures is spun into a conical structure of the head of the bomb shell, and the thick end of the preform with the third size structure is spun into a bowl-shaped structure at the tail of the bomb shell.
8. The method for manufacturing a bomb shell according to claim 7, characterized in that: In step S5b, the welding process of the two-stage split welding is: welding the unspun end of the preform of the second size structure to the unspun end of the preform of the third size structure to form the bomb shell structure.
9. The method for manufacturing a bomb shell according to claim 8, characterized in that: In step S5b, the original blank has the required size for the middle part of the bomb shell, and the welding process of the three-stage split welding is: the unspun end of the preform of the first size structure and the unspun end of the preform of the third size structure are respectively welded to the two ends of the original blank to form the bomb shell structure.
Citation Information
Patent Citations
Method for manufacturing aluminum liner of vehicular composite cylinder
CN101885137A
Method for manufacturing thin-walled steel liner and use of thin-walled steel liner
CN106917953A
Integral spinning forming method for curved generatrix thin-walled shell with annular reinforcing ribs
CN109351835A
Forming method of thin-wall stainless steel gas cylinder
CN109604938A
Integral spinning forming method and device for hollow thin-wall pull rod and product
CN118237490A
Cited By
Method of manufacture of a projectile shell
EP4821615A1
Method of manufacture of a projectile shell
EP4821616A1
Method of manufacture of a projectile shell
WO2026215613A1
Method of manufacture of a projectile shell
WO2026215614A1