Short-process manufacturing method and system for sinking stringer of carrier rocket
Through the new process of non-stable materials after solid solution quenching, combined with profile stretching and straightening, sawing, down stamping and aging strengthening, the warping and deformation problems caused by quenching heat treatment in traditional stringer processing are solved, and efficient Automated launch vehicle truss manufacturing significantly improves production efficiency and accuracy.
Patent Information
- Application Number
- CN202411505772.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-28
- Publication Date
- 2024-11-26
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In traditional carrier rocket stringer processing, warping and deformation occur frequently after heat treatment, resulting in loss of accuracy and low production efficiency. Relying on manual proofreading leads to cumbersome and time-consuming processes.
Using non-stable material after solid solution quenching, through the new process of quenching heat treatment - profile stretching and straightening - sawing - down stamping forming - aging strengthening, the cumbersomeness of traditional forming processes and parts distortion are eliminated, and automated production is achieved.
The processing process has been greatly reduced and the manual proofreading process has been canceled, achieving a cost reduction of about 30% and an efficiency improvement of more than 4 times, improving the accuracy and production efficiency of parts.
Smart Images

Figure CN119017029A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of metal stringer forming, and in particular to a short-process manufacturing method and system for sunken stringers of a launch vehicle. Background Art
[0002] In the field of aerospace equipment, stringer profiles are an important part of the rocket body. Various types of stringers, beams and other profiles together form the "skeleton" of the rocket body. The length of such structural parts is generally 1m to 5m, and the flatness and straightness requirements must not be greater than 0.5mm. The shape correction accuracy requirements are far higher than other parts. For a long time, the processing and correction methods using manual hammer repairs have resulted in low product production efficiency and hammer marks on the surface, affecting the surface quality. In addition, since stringer parts generally require quenching, a large amount of warping and deformation occurs. After quenching, their straightness and flatness need to be repeatedly corrected. Some stringers with small cross-sections or asymmetric shapes, such as L-shaped and Z-shaped, are more time-consuming and labor-intensive to correct. The correction process alone accounts for more than 80% of the stringer processing hours.
[0003] Through literature search of the prior art, it was found that the stringer material is generally made of high-strength aluminum alloy profiles, such as 7XXX series super-hard aluminum materials, which have high strength and poor plasticity. Most of the stringers are installed to avoid frame rings, and sinking features are set at the ends. These features are difficult to form at room temperature in the aging state. Therefore, traditionally, the sinking processing of the stringers is all in the annealing state (O), when the material strength is low and the plasticity is good. The problem is that after quenching and heat treatment, the annealed stringers will produce a large amount of warping and torsion, which requires repeated manual correction. Patent documents CN1166899552 and CN217451586U only proposed auxiliary shaping solutions from the perspective of improving the efficiency of manual shaping, and did not fundamentally solve the problem that the large warping deformation caused by quenching and heat treatment causes a great loss of part accuracy. How to avoid the influence of quenching and heat treatment deformation on the dimensional accuracy of the blank and get rid of the dependence on manual shaping has become a key issue in improving the manufacturing efficiency of stringer parts. Summary of the invention
[0004] In view of the defects in the prior art, the object of the present invention is to provide a short-process manufacturing method and system for a launch vehicle sunken stringer.
[0005] The short-process manufacturing method of the carrier rocket sunken stringer provided by the present invention comprises: Step S1: performing quenching heat treatment on the stringers to process the stringers into a solid solution non-steady state; Step S2: straightening the beams using a profile stretching device, and transferring the straightened profiles to a sawing device; Step S3: using a sawing device to cut the beams to a fixed length and adjusting the cutting angle; Step S4: using a CNC punching machine to drill connecting holes for connecting the truss with the frame ring and the skin; Step S5: using a sinking stamping forming device to form sinking features of the beams; Step S6: The beams whose ends have been sunken and formed are subjected to aging strengthening treatment in batches; Step S7: Perform surface treatment and packaging protection.
[0006] Preferably, the quenching heat treatment conditions are: solution temperature is 475°C±5°C, holding time is 30min-45min, quenching medium is water, and quenching transfer time does not exceed 10s.
[0007] Preferably, the sinking stamping forming device has the function of upper and lower mold clamping, and the bending process obtains a 4° sinking feature.
[0008] Preferably, the aging treatment system is 120±5°C for 3h, superimposed with 160±5°C for 3h.
[0009] Preferably, the surface treatment includes: hanging, cleaning, anodizing, sealing, coloring and sealing the stringers to form a dense oxide film on the surface of the stringers.
[0010] The short-process manufacturing system for the carrier rocket sunken stringer provided by the present invention comprises: Module M1: quenching heat treatment is performed on the stringers to process the stringers into a solid solution non-steady state; Module M2: Use the profile stretching device to straighten the beams and transfer the straightened profiles to the sawing device; Module M3: Use a sawing device to cut the stringers to the required length and adjust the cutting angle; Module M4: Use a CNC punching machine to drill stringer connection holes for connection with frame rings and skins; Module M5: uses a sinking stamping forming device to form sinking features of the beams; Module M6: The beams with both ends sunken and formed are subjected to aging strengthening treatment in batches; Module M7: Surface treatment and packaging protection.
[0011] Preferably, the quenching heat treatment conditions are: solution temperature is 475°C±5°C, holding time is 30min-45min, quenching medium is water, and quenching transfer time does not exceed 10s.
[0012] Preferably, the sinking stamping forming device has the function of upper and lower mold clamping, and the bending process obtains a 4° sinking feature.
[0013] Preferably, the aging treatment system is 120±5°C for 3h, superimposed with 160±5°C for 3h.
[0014] Preferably, the surface treatment includes: hanging, cleaning, anodizing, sealing, coloring and sealing the stringers to form a dense oxide film on the surface of the stringers.
[0015] Compared with the prior art, the present invention has the following beneficial effects: The present invention reconstructs the processing flow of launch vehicle stringers, adopts non-steady-state materials after solid solution quenching, and eliminates the problems of cumbersome traditional forming processes, high energy consumption, poor working environment, large part distortion, and huge shaping amount through the new route of "stretching and straightening - sawing - drilling - sag forming - aging strengthening". The original stringer processing flow is greatly reduced, and all manual shaping processes are cancelled. In actual engineering operations, the method of the present invention is used to achieve a cost reduction of about 30% and an efficiency improvement of more than 4 times. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Other features, objects and advantages of the present invention will become more apparent from the detailed description of non-limiting embodiments made with reference to the following drawings: Figure 1 Schematic diagram of a typical part with sunken beams Figure 2 This is a flow chart of the traditional processing scheme for sunken stringers; Figure 3 This is a flow chart of the short process method with sunken beams of the present invention; Figure 4 It is a schematic diagram of the mechanical straightening of profiles in the present invention which replaces the traditional manual straightening. DETAILED DESCRIPTION
[0017] The present invention is described in detail below in conjunction with specific embodiments. The following embodiments will help those skilled in the art to further understand the present invention, but are not intended to limit the present invention in any form. It should be noted that, for those of ordinary skill in the art, several changes and improvements can also be made without departing from the concept of the present invention. These all belong to the protection scope of the present invention.
[0018] Example 1 like Figure 1 As shown, this embodiment selects a typical long straight T-shaped beam: The material is 7A09, the T-section height (facade 1) is 35mm, the web 2 width is 40mm, the total length is 3810mm, with 4° depression and 61.2° bevel angle features at both ends. There are 208 connection holes with a diameter of 2.5mm.
[0019] like Figure 2 The figure shows the flow chart of the traditional processing scheme of sunken beams.
[0020] like Figure 3As shown, the short-process stringer shape coordination solution proposed by the present invention includes the following steps: Step S1: The incoming material is 7A09 extruded profile, and quenching heat treatment is performed, the solution temperature is 475℃±5℃, the holding time is 30min-45min, the quenching medium is water, and the quenching transfer time does not exceed 10s. The solid solution non-steady state profile is obtained. After the solid solution heat treatment, the strength and hardness of the alloy are reduced compared with the aging state, but the plasticity and toughness are improved; Heat treatment strengthens aluminum alloys and heats them to form a supersaturated solid solution. They are taken out of the quenching heating furnace and transferred to the quenching water tank. After cooling in the air for just a dozen seconds or even a few seconds, strengthening phases will precipitate, affecting the strengthening effect. The transfer from the quenching furnace to the quenching medium must be completed within the specified maximum transfer time, which is called the maximum allowable transfer time or quenching delay time. If conditions permit, the shorter the quenching transfer time, the better.
[0021] Step S2: Use the profile stretching device to straighten the beams. The beams will also be deformed by external forces during transportation, storage and hoisting. In this step, the deformation is stretched to eliminate it. The stretching deformation is set to 0.5%-5%. Generally, the total length of the incoming profile is 6m, and the stretching amount is controlled at 60mm. The straightened profile is transferred to the sawing device. Step S3: Use a sawing device to cut the beams to a fixed length. In this embodiment, the beams are cut according to the design drawing requirements, and the cutting size is 3810 mm.
[0022] The sawing device can adjust the cutting angle. In this embodiment, the cutting angle is set to 61.2° with respect to the web plane.
[0023] Step S4: Use a CNC punching machine to drill truss connection holes for connection with the frame ring and the skin. There are 208 holes in total, with a diameter of 2.5 mm; Optionally, this process can be adjusted to the assembly stage, and the connection holes can be made later; Step S5: using a sinking stamping forming device to form sinking features of the beams; The sinking stamping forming device is a stamping device with upper and lower mold clamping functions and a 4° sinking feature obtained by bending.
[0024] Step S6: Aging treatment: The beams that have been sunken at both ends are subjected to aging treatment in batches, with the aging treatment system being 120±5℃ for 3h and superimposed at 160±5℃ for 3h.
[0025] Step S7: Surface treatment and packaging for protection. After the stringers are hung, cleaned, anodized, sealed, colored and sealed, a dense oxide film is formed on the surface of the stringers, which are then dried and packaged for protection.
[0026] The process of forming a dense oxide film is as follows: aluminum and its alloys are placed in the corresponding electrolyte (such as sulfuric acid, chromic acid, oxalic acid, etc.) as anodes, and electrolyzed under specific conditions and external current. The aluminum or its alloy at the anode undergoes an oxidation reaction, and a thin layer of aluminum oxide is formed on the surface, with a thickness of 5 to 20 microns, and the hard anodized film can reach 60 to 200 microns.
[0027] like Figure 4 As shown, a schematic diagram of profile stretching and straightening that replaces traditional manual straightening. The profile stretching device comprises a first stretching arm 3-1 and a second stretching arm 3-2. The first clamp 4-1 on the first stretching arm 3-1 and the second clamp 4-2 on the second stretching arm 3-2 can stably clamp the two ends of the profile and apply a stretching force. The lines of action of the stretching forces of the two stretching arms are coaxial. The mechanical straightening deformation is 0.3%-3%.
[0028] Example 2 The present invention also provides a short-process manufacturing system for a launch vehicle sunken stringer. The short-process manufacturing system for a launch vehicle sunken stringer can be realized by executing the process steps of the short-process manufacturing method for the launch vehicle sunken stringer. That is, technical personnel in this field can understand the short-process manufacturing method for the launch vehicle sunken stringer as a preferred implementation mode of the short-process manufacturing system for the launch vehicle sunken stringer.
[0029] The short-process manufacturing system for the sunken stringers of a carrier rocket provided by the present invention comprises: module M1: performing quenching heat treatment on the stringers to process the stringers into a solid solution non-steady state; module M2: adopting a profile stretching device to straighten the stringers, and transferring the straightened profiles to a sawing device; module M3: adopting a sawing device to cut the stringers to a fixed length, and adjusting the incision angle; module M4: adopting a CNC punching machine to drill stringer connection holes for connection with a frame ring and a skin; module M5: adopting a sunken stamping forming device to form the sinking features of the stringers; module M6: performing aging strengthening treatment in batches on the stringers whose two ends have been sunken; and module M7: performing surface treatment and packaging protection.
[0030] The quenching heat treatment conditions are: solution temperature is 475°C±5°C, holding time is 30min-45min, quenching medium is water, and quenching transfer time does not exceed 10s.
[0031] The sinking stamping forming device has the function of upper and lower mold clamping, and the bending process obtains a 4° sinking feature.
[0032] The aging treatment system is 120±5℃ for 3h, superimposed with 160±5℃ for 3h.
[0033] The surface treatment includes: hanging, cleaning, anodizing, sealing, coloring and sealing the beams to form a dense oxide film on the surface of the beams.
[0034] In the description of the present application, it should be understood that the terms "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0035] Those skilled in the art know that, in addition to implementing the system, device and its various modules provided by the present invention in a purely computer-readable program code, it is entirely possible to implement the same program in the form of logic gates, switches, application-specific integrated circuits, programmable logic controllers and embedded microcontrollers by logically programming the method steps. Therefore, the system, device and its various modules provided by the present invention can be considered as a hardware component, and the modules included therein for implementing various programs can also be considered as structures within the hardware component; the modules for implementing various functions can also be considered as both software programs for implementing the method and structures within the hardware component.
[0036] The above describes the specific embodiments of the present invention. It should be understood that the present invention is not limited to the above specific embodiments, and those skilled in the art can make various changes or modifications within the scope of the claims, which does not affect the essence of the present invention. In the absence of conflict, the embodiments of the present application and the features in the embodiments can be combined with each other arbitrarily.
Claims
1. A short-process manufacturing method for a launch vehicle sunken stringer, characterized in that: include: Step S1: performing quenching heat treatment on the stringers to process the stringers into a solid solution non-steady state; Step S2: straightening the beams using a profile stretching device, and transferring the straightened profiles to a sawing device; Step S3: using a sawing device to cut the beams to a fixed length and adjusting the cutting angle; Step S4: using a CNC punching machine to drill connecting holes for connecting the truss with the frame ring and the skin; Step S5: using a sinking stamping forming device to form sinking features of the beams; Step S6: The beams whose ends have been sunken and formed are subjected to aging strengthening treatment in batches; Step S7: performing surface treatment and packaging protection.
2. The short-process manufacturing method for a launch vehicle sunken stringer according to claim 1, characterized in that: The quenching heat treatment conditions are: solution temperature is 475°C±5°C, holding time is 30min-45min, quenching medium is water, and quenching transfer time does not exceed 10s.
3. The short-process manufacturing method for a launch vehicle sunken stringer according to claim 1, characterized in that: The sinking stamping forming device has the function of upper and lower mold clamping, and the bending process obtains a 4° sinking feature.
4. The short-process manufacturing method for a launch vehicle sunken stringer according to claim 1, characterized in that: The aging treatment system is 120±5℃ for 3h, superimposed with 160±5℃ for 3h.
5. The short-process manufacturing method for a launch vehicle sunken stringer according to claim 1, characterized in that: The surface treatment includes: hanging, cleaning, anodizing, sealing, coloring and sealing the beams to form a dense oxide film on the surface of the beams.
6. A short-process manufacturing system for launch vehicle sunken stringers, characterized in that: include: Module M1: quenching heat treatment is performed on the stringers to process the stringers into a solid solution non-steady state; Module M2: Use the profile stretching device to straighten the beams and transfer the straightened profiles to the sawing device; Module M3: Use a sawing device to cut the stringers to the required length and adjust the cutting angle; Module M4: Use a CNC punching machine to drill stringer connection holes for connection with frame rings and skins; Module M5: uses a sinking stamping forming device to form sinking features of the beams; Module M6: The beams with both ends sunken and formed are subjected to aging strengthening treatment in batches; Module M7: Surface treatment and packaging protection.
7. The launch vehicle sunken stringer short process manufacturing system according to claim 6, characterized in that: The quenching heat treatment conditions are: solution temperature is 475°C±5°C, holding time is 30min-45min, quenching medium is water, and quenching transfer time does not exceed 10s.
8. The launch vehicle sunken stringer short process manufacturing system according to claim 6, characterized in that: The sinking stamping forming device has the function of upper and lower mold clamping, and the bending process obtains a 4° sinking feature.
9. The launch vehicle sunken stringer short process manufacturing system according to claim 6, characterized in that: The aging treatment system is 120±5℃ for 3h, superimposed with 160±5℃ for 3h.
10. The launch vehicle sunken stringer short process manufacturing system according to claim 6, characterized in that: The surface treatment includes: hanging, cleaning, anodizing, sealing, coloring and sealing the beams to form a dense oxide film on the surface of the beams.
Citation Information
Patent Citations
Aluminum alloy pipe and manufacture method thereof
CN102337435A
Method for analyzing finite elements of skin-stringer structures of carrier rockets
CN103678786A
Mechanical rolling straightening device for T section and straightening method
CN107335695A
2-series aluminum alloy profile for civil aircraft wing lower stringer and manufacturing method of 2-series aluminum alloy profile
CN111424199A
7-series aluminum alloy profile for upper stringer of civil aircraft wing and manufacturing method thereof
CN111676399A