Preparation process of bendable hardened PC (polycarbonate) board

By applying the hardened layer and the flexible cured layer on the PC sheet, the problem of reduced flexibility after hardening is solved, the balance between hardening and flexibility is achieved, and the wear resistance, high temperature and corrosion resistance of the PC sheet is improved.

CN119017746AInactive Publication Date: 2024-11-26FICK OPTICAL TECH(CHANGZHOU) CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411357525.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-27
Publication Date
2024-11-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The flexibility of existing PC boards is greatly reduced after hardening, making it difficult to take into account both hardening and flexibility.

Method used

The PC coil is hardened by coating the hardened layer, and a flexible curing layer is applied to the surface of the hardened layer. The hardened layer includes composite resin, antioxidants, ultraviolet absorbers and lubricants. The flexible curing layer includes prepolymers, Active monomers, photoinitiators and solvents achieve a balance between hardening and flexibility through ultraviolet curing and natural curing.

Benefits of technology

It realizes the flexibility of PC sheet while hardening, and improves its wear resistance, high temperature and corrosion resistance.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a preparation process and a manufacturing mold of a bendable hardened PC (polycarbonate) board, and the preparation process comprises the following steps: step 1, unwinding a PC roll, pulling out the PC roll through a driving device, and laying the PC roll on a conveying belt; secondly, a protective film of the PC roll on the conveying belt is torn off, and the surface of the PC roll is coated with a hardened layer; 3, a hardened layer is attached and cured through an ultraviolet (UV) curing device; step 4, conveying to another conveying line, and coating the surface of the hardened layer with a flexible curing layer again; and step 5, after coating is completed, placing at room temperature for natural curing. The PC coiled material is subjected to hardening treatment in a manner of coating the hardening coating, so that the PC coiled material has certain flexibility while being hardened, and the surface of the hardening layer is coated with the curing layer, so that the PC coiled material is more wear-resistant, high-temperature-resistant and corrosion-resistant.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of PC sheets, and in particular to a preparation process and a manufacturing mold for a bendable and hardened PC sheet. Background Art

[0002] PC board is also called polycarbonate board, polyester board, capron board. It is resistant to weak acid. It is made of polycarbonate as the main component and is made by co-extrusion technology CO-EXTRUSION. It shows that PC board is resistant to neutral oil, not resistant to strong acid, not durable, not resistant to alkali, and needs to be coated with UV.

[0003] However, the flexibility of existing PC sheets will be greatly reduced after the hardening layer is used. Summary of the invention

[0004] In accordance with the above technical problems to be solved, a preparation process of a bendable and hardened PC board is provided.

[0005] To achieve the above-mentioned purpose, the present invention is configured in a preferred embodiment to include the following steps: step 1: unwinding the PC roll, pulling it out through a driving device and laying it on a conveyor belt; step 2: tearing off the protective film of the PC roll on the conveyor belt, and applying a hardening layer to the surface of the PC roll; step 3: attaching and curing the hardening layer through an ultraviolet UV curing device; step 4: sending it to another conveyor line, and applying a flexible curing layer to the surface of the hardening layer again; step 5: placing it at room temperature for natural curing after coating.

[0006] In a preferred embodiment of the present invention, the hardening layer includes a composite resin, an antioxidant, an ultraviolet absorber and a lubricant, which are mixed and extruded through a screw machine, and a modified polycarbonate masterbatch is produced by melting, extruding and granulating, and the polycarbonate masterbatch is injection molded and applied to the surface of the PC roll.

[0007] In a preferred embodiment of the present invention, the mass ratio of the composite resin, the antioxidant, the ultraviolet absorber and the lubricant is 100:0.5-1:0.6-1.2:1-2.

[0008] In a preferred embodiment of the present invention, the antioxidant can be further configured as follows: the antioxidant is a hindered phenol antioxidant, including one of antioxidant-1010, antioxidant-1076, and antioxidant-3114; the ultraviolet absorber is a triazine ultraviolet absorber, including one of UV-1577, UV-627, and UV-1164; and the lubricant is sodium dodecyl sulfate or sodium hexadecyl sulfonate.

[0009] In a preferred embodiment of the present invention, the raw materials of the flexible curing layer include 40 to 50 parts by weight of prepolymer, 0.8 to 1.4 parts of active monomer, 0.5 to 1 part of photoinitiator and 30 to 40 parts of solvent.

[0010] In a preferred embodiment of the present invention, the prepolymer is prepared by heating the hyperbranched polyurethane mixture to 60-70°C, adding hydroxy acrylate, cooling to 30-40°C, adding fluorine-substituted acrylate, and keeping the mixture warm for 1.5-2.5 hours to obtain the prepolymer.

[0011] In a preferred embodiment, the present invention can be further configured to further include modified nanoparticles, and the weight ratio of the modified nanoparticles to the active monomer is 1:(1.5-2.5).

[0012] Beneficial effect: The preparation process of a bendable hardened PC board of the present invention hardens the PC coil by applying a hardening coating, so that it has a certain flexibility while hardening, and a curing layer is also applied on the surface of the hardened layer to make it more wear-resistant, high-temperature-resistant and corrosion-resistant. DETAILED DESCRIPTION

[0013] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the protection scope of the present invention.

[0014] A preparation process of a bendable hardened PC board comprises the following steps: step 1: unwinding a PC roll, pulling it out through a driving device and laying it on a conveyor belt; step 2: tearing off the protective film of the PC roll on the conveyor belt, and applying a hardening layer to the surface of the PC roll; step 3: attaching and curing the hardening layer through an ultraviolet UV curing device; step 4: sending it to another conveyor line, and applying a flexible curing layer to the surface of the hardening layer again; step 5: placing it at room temperature for natural curing after coating.

[0015] In step 2, the hardening layer includes a composite resin, an antioxidant, an ultraviolet absorber and a lubricant, which are mixed and extruded through a screw machine, and a modified polycarbonate masterbatch is produced by melting, extruding and granulating, and the polycarbonate masterbatch is injection molded and applied to the surface of the PC roll.

[0016] The mass ratio of the composite resin, antioxidant, ultraviolet absorber and lubricant is 100:0.5-1:0.6-1.2:1-2.

[0017] The antioxidant is a hindered phenol antioxidant, including one of antioxidant-1010, antioxidant-1076, and antioxidant-3114; the ultraviolet absorber is a triazine ultraviolet absorber, including one of UV-1577, UV-627, and UV-1164; and the lubricant is sodium dodecyl sulfate or sodium hexadecyl sulfonate.

[0018] The raw materials of the flexible curing layer include 40 to 50 parts by weight of prepolymer, 0.8 to 1.4 parts by weight of active monomer, 0.5 to 1 part by weight of photoinitiator and 30 to 40 parts by weight of solvent.

[0019] The prepolymer is prepared by heating a hyperbranched polyurethane mixed liquid to 60-70°C, adding hydroxy acrylate dropwise, cooling to 30-40°C, adding fluorine-substituted acrylate, and keeping the temperature for 1.5-2.5 hours to obtain the prepolymer.

[0020] The invention also comprises modified nanoparticles, wherein the weight ratio of the modified nanoparticles to the active monomer is 1:(1.5-2.5).

[0021] It should be noted that, in this document, relational terms such as first and second, etc. are merely used to distinguish one entity from another entity, but do not necessarily require or imply the existence of any such actual relationship or order between these entities.

[0022] The above examples are merely illustrative of the present invention and do not constitute a limitation on the protection scope of the present invention. All designs that are the same or similar to the present invention belong to the protection scope of the present invention.

Claims

1. A process for preparing a bendable and hardened PC board, characterized in that: The following steps are included: Step 1: Unwind the PC roll, pull it out through the driving device and lay it on the conveyor belt; Step 2: Tear off the protective film of the PC roll on the conveyor belt and apply a hardening layer to the surface of the PC roll; Step 3: Use ultraviolet UV curing device to adhere and cure the hardened layer; Step 4: Send it to another conveyor line and apply a flexible curing layer to the surface of the hardened layer again; Step 5: After coating, place it at room temperature to cure naturally.

2. A process for preparing a bendable hardened PC board according to claim 1, characterized in that: In step 2, the hardening layer includes a composite resin, an antioxidant, an ultraviolet absorber and a lubricant, which are mixed and extruded through a screw machine, and a modified polycarbonate masterbatch is produced by melting, extruding and granulating, and the polycarbonate masterbatch is injection molded and applied to the surface of the PC roll.

3. The process for preparing a bendable hardened PC board according to claim 2, characterized in that: The mass ratio of the composite resin, antioxidant, ultraviolet absorber and lubricant is 100:0.5-1:0.6-1.2:1-2.

4. The process for preparing a bendable hardened PC board according to claim 3, characterized in that: The antioxidant is a hindered phenol antioxidant, including one of antioxidant-1010, antioxidant-1076, and antioxidant-3114; the ultraviolet absorber is a triazine ultraviolet absorber, including one of UV-1577, UV-627, and UV-1164; and the lubricant is sodium dodecyl sulfate or sodium hexadecyl sulfonate.

5. The process for preparing a bendable hardened PC board according to claim 1, characterized in that: The raw materials of the flexible curing layer include 40 to 50 parts by weight of prepolymer, 0.8 to 1.4 parts by weight of active monomer, 0.5 to 1 part by weight of photoinitiator and 30 to 40 parts by weight of solvent.

6. The process for preparing a bendable hardened PC board according to claim 5, characterized in that: The prepolymer is prepared by heating a hyperbranched polyurethane mixed liquid to 60-70°C, adding hydroxy acrylate dropwise, cooling to 30-40°C, adding fluorine-substituted acrylate, and keeping the temperature for 1.5-2.5 hours to obtain the prepolymer.

7. The process for preparing a bendable and hardened PC board according to claim 6, characterized in that: It also includes modified nanoparticles, wherein the weight ratio of the modified nanoparticles to the active monomer is 1:(1.5-2.5).

Citation Information

Patent Citations

  • Process and apparatus for surface-hardening treatment of PC board coil

    CN104827688A

  • Hardening coating liquid for flexible cover plates

    CN110734698A

  • PC board surface hardness strengthening process

    CN111892733A

  • Preparation process of hardened PC panel

    CN117777696A

  • Surface hardness-modifying plate and its manufacture

    JP1996183144A