Method for treating wastewater containing copper nitrate and copper sulfate in high-purity copper industry
By combining flocculant treatment and pH optimization with diffusion dialysis, activated carbon adsorption, and reverse osmosis separation technologies, the problem of high heavy metal sludge content in high-purity copper industrial wastewater has been solved, achieving sludge stabilization and resource utilization, and recovering high-purity copper products.
Patent Information
- Application Number
- CN202411165555.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-08-23
AI Technical Summary
Existing chemical treatment methods for wastewater containing copper nitrate and copper sulfate from the high-purity copper industry result in sludge with high levels of heavy metals, which may lead to secondary pollution.
After treatment with flocculants, heavy metals are removed and utilized as resources through online monitoring and pH optimization, combined with diffusion dialysis, activated carbon adsorption, reverse osmosis separation, sludge stabilization and bioleaching technologies.
It effectively reduced the heavy metal content in sludge, achieved sludge stabilization and resource utilization, avoided secondary pollution, and recovered high-purity copper products.
Smart Images

Figure CN119019034A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of environmental engineering, in particular to a method for treating wastewater containing copper nitrate and copper sulfate in a high-purity copper industry. Background Art
[0002] In the high-purity copper industry, wastewater containing copper nitrate and copper sulfate is a common pollutant. If these wastewaters are discharged directly without treatment, they will cause serious pollution to the water body, affecting the ecological environment and human health. Therefore, it is particularly important to develop effective treatment methods. At present, the treatment methods for this type of wastewater mainly include chemical precipitation, electrolysis, adsorption, ion exchange, etc. Among them, chemical precipitation is widely used because of its mature technology and low cost.
[0003] Although existing treatment methods reduce the burden of environmental pollution, the chemical treatment method adjusts the pH value to make copper ions form copper hydroxide precipitation, and then performs solid-liquid separation to remove the precipitate. This process will produce a large amount of sludge containing heavy metals. If this sludge is not handled properly, it may cause secondary pollution. Summary of the invention
[0004] 1. Technical issues to be resolved In view of the shortcomings of the prior art, the present invention provides a method for treating wastewater containing copper nitrate and copper sulfate in the high-purity copper industry, which has the advantage of low heavy metal sludge content and solves the problem of high heavy metal sludge content in traditional chemical treatment methods.
[0005] (II) Technical solution To achieve the above object, the present invention provides the following technical solution: a method for treating wastewater containing copper nitrate and copper sulfate in high-purity copper industry, comprising the following steps: Step 1, pretreatment: filter the copper nitrate and copper sulfate wastewater respectively, and collect the filtrate into the A and B reaction tanks respectively; Step 2, adding flocculant: adding flocculant to the reaction tank of copper nitrate and copper sulfate; Step 3: Optimize the pH value of the reaction pool: The online monitoring instrument monitors the pH value of the reaction pool during the reaction process and adjusts the pH value in real time; Step 4: breaking the complex: adding hydrogen peroxide into the reaction tank A to break the complex copper and convert it into Cu2+, and the supernatant is used as the effluent; Step 5: Conversion: The copper nitrate and copper sulfate wastewaters from reaction tanks A and B are treated by diffusion dialysis technology respectively; Step 6: Advanced treatment: Use activated carbon adsorption and reverse osmosis separation technology to further remove residual copper ions; Step 7: Sludge stabilization treatment: Stabilization treatment is performed on the sludge produced by deep treatment; Step 8: Sludge washing: The sludge is washed 8 times with circulating water; Step 9: Sludge composting: Based on sludge stabilization, the sludge is converted into organic fertilizer through composting technology; Step 10: Heavy metal recovery: Bioleaching technology uses microorganisms or their metabolites to interact with metals in sludge to leach valuable metals; Step 11: Final treatment: neutralize the treated wastewater and discharge it into the comprehensive wastewater pool; Step 12: Recycling: The recovered copper is prepared into a 98% pure copper product through electrolysis.
[0006] Preferably, the pretreatment in step 1 is as follows: the copper nitrate and copper sulfate wastewaters are filtered separately to obtain copper nitrate filtrate and copper sulfate filtrate, the copper nitrate filtrate is collected into reaction tank A, and the copper sulfate filtrate is collected into reaction tank B.
[0007] Preferably, in step 2, a flocculant is added: 15% polyaluminium chloride is added to reaction tank A, and 20% polyacrylamide is added to reaction tank B.
[0008] Preferably, the pH value of the reaction tank is optimized in step three: when the pH of reaction tank A is <6, 20% sodium hydroxide is added for adjustment; when the pH of reaction tank A is >9, 10% hydrochloric acid is added for adjustment; when the pH of reaction tank B is <6, 10% potassium hydroxide is added for adjustment; when the pH of reaction tank A is >9, 5% sulfuric acid is added for adjustment.
[0009] Preferably, the network breaking conditions in step 4 are: S1.1, control the solution pH between 6-9; S1.2. While using hydrogen peroxide, add 80 mg and 40 mg of polyacrylamide.
[0010] Preferably, the conversion process in step 5 is: S2.1, pretreatment step: using diffusion dialysis equipment to filter copper nitrate and copper sulfate waste liquid; S2.2, Operation process: Use sulfur dioxide as the reducing agent of copper nitrate and copper sulfate filtrate to reduce copper sulfate to copper, control the pH value of copper nitrate and copper sulfate filtrate in reaction tanks A and B between 6-9, set the ambient temperature to 20-30℃, let stand for 2 hours, and the inlet water acidity is 5g / L; S2.3, Re-separation: Copper and sulfuric acid are separated by installing diffusion dialysis equipment at the outlet.
[0011] Preferably, in step six, the deep treatment is as follows: activated carbon with a ratio multiple of 3 is put into reaction tank A to adsorb residual copper ions, and then reverse osmosis separation technology is used to further remove the copper ions adsorbed by the activated carbon. In reaction tank B, the copper sulfate wastewater is passed through a reactor equipped with ion exchange resin at a flow rate of 10 meters per second.
[0012] Preferably, in the step 7, the sludge stabilization treatment is as follows: when the pH of the A and B reaction tanks is greater than 9, the sludge produced by the deep treatment is treated by a stabilization method, and a combination of calcium oxide and magnesium salt in a ratio of 5:1 is used, and the mixture is uniformly mixed with the sludge and then put into the A and B reaction tanks: Calcium oxide reacts with water: CaO+H2O→Ca(OH)2+heatCaO+H2O→Ca(OH)2+heat Calcium hydroxide reacts with carbon dioxide: Ca(OH)2+CO2→CaCO3+H2O+heatCa(OH)2+CO2→CaCO3+H2O+heat.
[0013] Preferably, in the biological leaching technology process in step ten: when the water temperature of reaction tanks A and B is maintained between 30-35°C and the pH value is between 6-9, a combination of Thiobacillus ferrooxidans, Thiobacillus thiooxidans and Aspergillus niger in a ratio of 3:1:2 is put into the reaction tank to interact with the copper ions in the sludge, and 50% oxygen is introduced into the bottom of reaction tanks A and B, and the stirring paddle is turned on for stirring for 2-4 hours.
[0014] Preferably, the step eleven is the final treatment: adding 20% sodium hydroxide, 10% hydrochloric acid, 10% potassium hydroxide or 5% sulfuric acid to the treated wastewater to neutralize the wastewater discharged from the A and B reaction tanks. When the pH value of the neutralization treatment is between 7 and 8, it is discharged into a comprehensive sewage pool or a municipal sewage network.
[0015] Compared with the prior art, the present invention provides a method for treating wastewater containing copper nitrate and copper sulfate in high-purity copper industry, which has the following beneficial effects: 1. The present invention optimizes the pH value of the reaction tank. When the pH of reaction tank A is less than 6, 20% sodium hydroxide is added for adjustment; when the pH of reaction tank A is greater than 9, 10% hydrochloric acid is added for adjustment; when the pH of reaction tank B is less than 6, 10% potassium hydroxide is added for adjustment; when the pH of reaction tank B is greater than 9, 5% sulfuric acid is added for adjustment. The above adjustment process can be assisted by the automatic feeding equipment of the reaction tank to ensure that the pH value in the reaction tank is in the optimal state, thereby assisting the subsequent sludge treatment.
[0016] 2. The present invention combines calcium oxide and magnesium salt in a ratio of 5:1, uniformly mixes the mixture with sludge, and puts the mixture into reaction tanks A and B for treatment with chemical reagents. The sludge can be effectively stabilized, and the purposes of solidification and sterilization can be achieved. The storage and transportation conditions can also be improved to avoid secondary pollution. The stabilized sludge meets the requirements of recycling, such as being used for cement clinker, building materials, garden soil and soil conditioner, thus realizing the resource utilization of sludge. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a process flow chart of the present invention; DETAILED DESCRIPTION
[0018] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0019] See also Figure 1 A method for treating wastewater containing copper nitrate and copper sulfate in high-purity copper industry comprises the following steps: Step 1, pretreatment: filter the copper nitrate and copper sulfate wastewater respectively, and collect the filtrate into the A and B reaction tanks respectively; Step 2: Add flocculant: Add flocculant to the reaction tank of copper nitrate and copper sulfate to enhance the precipitation effect of copper ions and form larger particles of precipitate, thereby improving the efficiency of solid-liquid separation; Step 3: Optimize the pH value of the reaction tank: The online monitoring instrument monitors the pH value of the reaction tank during the reaction process and adjusts the pH value in real time to ensure that the copper ions are precipitated to the greatest extent in the form of copper hydroxide, which can not only improve the precipitation efficiency, but also reduce the problem of redissolution of precipitates caused by inappropriate pH value; Step 4: breaking the complex: adding hydrogen peroxide into the reaction tank A to break the complex copper and convert it into Cu2+, and the supernatant is used as the effluent; Step 5: Conversion: The copper nitrate and copper sulfate wastewaters from reaction tanks A and B are treated by diffusion dialysis technology respectively; Step 6: Advanced treatment: Use activated carbon adsorption and reverse osmosis separation technology to further remove residual copper ions; Step 7: Sludge stabilization treatment: The sludge produced by deep treatment is treated by stabilization method to convert the heavy metals in the sludge into a stable form, reducing its solubility and toxicity; Step 8: Sludge washing: The sludge is washed 8 times with circulating water to remove impurities and toxic substances, so as to facilitate subsequent treatment and utilization, and effectively reduce the content of heavy metals in the sludge; Step 9: Sludge composting: Based on sludge stabilization, the sludge is converted into organic fertilizer through composting technology. This method not only solves the sludge treatment problem, but also provides resources for agriculture; Step 10: Heavy metal recovery: Bioleaching technology uses microorganisms or their metabolites to interact with metals in sludge to leach valuable metals; Step 11: Final treatment: neutralize the treated wastewater and then discharge it into the comprehensive wastewater pool; Step 12: Recycling: The recovered copper is electrolyzed to produce a 98% pure copper product, and the nitric acid is converted into nitrogen fertilizer containing amide nitrogen and nitrate nitrogen, while other finished products in the wastewater are processed at the same time.
[0020] Pretreatment in step 1: Filter the copper nitrate and copper sulfate wastewaters separately to obtain copper nitrate filtrate and copper sulfate filtrate, collect the copper nitrate filtrate into reaction tank A, and collect the copper sulfate filtrate into reaction tank B.
[0021] In step 2, flocculants are added: 15% polyaluminium chloride (PAC) is added to reaction tank A, and 20% polyacrylamide (PAM) is added to reaction tank B.
[0022] In step three, optimize the pH value of the reaction tank: when the pH of reaction tank A is <6, add 20% sodium hydroxide for adjustment; when the pH of reaction tank A is >9, add 10% hydrochloric acid for adjustment; when the pH of reaction tank B is <6, add 10% potassium hydroxide for adjustment; when the pH of reaction tank A is >9, add 5% sulfuric acid for adjustment.
[0023] The advantages are: by optimizing the pH value of the reaction tank, when the pH of reaction tank A is less than 6, add 20% sodium hydroxide for adjustment; when the pH of reaction tank A is greater than 9, add 10% hydrochloric acid for adjustment; when the pH of reaction tank B is less than 6, add 10% potassium hydroxide for adjustment; when the pH of reaction tank B is greater than 9, add 5% sulfuric acid for adjustment. The above adjustment process can be assisted by the automatic feeding equipment of the reaction tank to ensure that the pH value in the reaction tank is in the optimal state, thereby assisting the subsequent sludge treatment.
[0024] The network breaking conditions in step 4 are: S1.1, control the solution pH between 6-9; S1.2. While using hydrogen peroxide, add 80 mg and 40 mg of polyacrylamide.
[0025] The conversion process in step 5 is: S2.1, pretreatment step: use diffusion dialysis equipment to filter copper nitrate and copper sulfate waste liquid. This step can effectively remove suspended matter or precipitation in the waste liquid and protect the normal operation of subsequent equipment; S2.2, Operation process: Use sulfur dioxide as the reducing agent of copper nitrate and copper sulfate filtrate to reduce copper sulfate to copper, control the pH value of copper nitrate and copper sulfate filtrate in reaction tanks A and B between 6-9, set the ambient temperature to 20-30℃, let stand for 2 hours, and the inlet water acidity is 5g / L; S2.3, Re-separation: Copper and sulfuric acid are separated by installing diffusion dialysis equipment at the outlet.
[0026] In step six, deep treatment is performed by putting activated carbon with a ratio of 3 into reaction tank A to adsorb the residual copper ions, and then using reverse osmosis separation technology to further remove the copper ions adsorbed by the activated carbon. In reaction tank B, the copper sulfate wastewater is passed through a reactor equipped with ion exchange resin at a flow rate of 10 meters per second.
[0027] In step 7, sludge stabilization treatment: When the pH of the A and B reaction tanks is greater than 9, the sludge produced by the deep treatment is treated by stabilization method. Calcium oxide and magnesium salt are combined in a ratio of 5:1, and mixed evenly with the sludge and put into the A and B reaction tanks. When calcium oxide is used, calcium oxide reacts chemically with the water in the sludge to generate calcium hydroxide and release heat, which helps to evaporate part of the water and increase the solid content. The chemical reaction formula is: Calcium oxide reacts with water: CaO+H2O→Ca(OH)2+heatCaO+H2O→Ca(OH)2+heat Calcium hydroxide reacts with carbon dioxide: Ca(OH)2+CO2→CaCO3+H2O+heatCa(OH)2+CO2→CaCO3+H2O+heat In the chemical formula, the above chemical reaction formula helps to reduce the volume of sludge, and the heat generated also helps to evaporate part of the water, thereby increasing the solid content of the treated sludge. At the same time, the alkalinity is enhanced and the temperature is increased. This treatment method can effectively kill bacteria and ensure the safety of the treated sludge during the disposal process.
[0028] The advantages are: through the treatment of the above chemical reagents, the sludge can be effectively stabilized, and at the same time achieve the purpose of solidification and sterilization, and can also improve storage and transportation conditions, avoid secondary pollution, and the stabilized sludge meets the requirements of recycling and reuse, such as being used in cement clinker, building materials, garden soil and soil conditioner, realizing the resource utilization of sludge.
[0029] In step 10, the biological leaching technology process: keep the water temperature of the A and B reaction tanks between 30-35°C and the pH value between 6-9, and put a combination of Thiobacillus ferrooxidans, Thiobacillus thiooxidans and Aspergillus niger in a ratio of 3:1:2 into the reaction tank to interact with the copper ions in the sludge. At the same time, introduce 50% oxygen into the bottom of the A and B reaction tanks, and start the agitator to stir for 2-4 hours.
[0030] Step 11 Final treatment: Add 20% sodium hydroxide, 10% hydrochloric acid, 10% potassium hydroxide or 5% sulfuric acid to the treated wastewater to neutralize the wastewater discharged from reaction tanks A and B. When the pH value of the neutralization treatment is between 7 and 8, it is discharged into a comprehensive wastewater pool or a municipal sewage network. For high ammonia nitrogen copper sulfate wastewater, ammonia nitrogen solidification, copper ion collection and sulfate separation can be used.
[0031] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is defined by the appended claims and their equivalents.
Claims
1. A method for treating wastewater containing copper nitrate and copper sulfate in the high-purity copper industry, characterized in that: The following steps are involved: Step 1: Pretreatment: Filter the copper nitrate and copper sulfate wastewater separately, and collect the filtrate into the A and B reaction tanks respectively; Step 2: Add flocculant: Add flocculant to the reaction tank of copper nitrate and copper sulfate; Step 3: Optimize the pH value of the reaction tank: Use an online monitoring instrument to monitor the pH value of the reaction tank during the reaction process and adjust the pH value in real time; Step 4: Decomposition of complexes: Add hydrogen peroxide to reaction tank A to decomposition the complexed copper and convert it into Cu2+, with the supernatant as the effluent; Step 5: Conversion: The copper nitrate and copper sulfate wastewater from reaction tanks A and B are treated by diffusion dialysis technology respectively; Step 6: Advanced treatment: Use activated carbon adsorption and reverse osmosis separation technology to further remove residual copper ions; Step 7: Sludge stabilization treatment: Stabilization treatment is performed on the sludge produced by deep treatment; Step 8: Sludge washing: The sludge is washed 8 times with circulating water; Step 9: Sludge composting: Based on sludge stabilization, the sludge is converted into organic fertilizer through composting technology; Step 10: Heavy metal recovery: Bioleaching technology uses microorganisms or their metabolites to interact with metals in sludge to leach valuable metals; Step 11: Final treatment: neutralize the treated wastewater and then discharge it into the integrated wastewater pool; Step 12: Recycling: The recovered copper is electrolyzed to produce a 98% pure copper product.
2. The method for treating wastewater containing copper nitrate and copper sulfate in a high-purity copper industry according to claim 1, wherein: The pretreatment in step 1 is as follows: the copper nitrate and copper sulfate wastewater are filtered separately to obtain copper nitrate filtrate and copper sulfate filtrate, the copper nitrate filtrate is collected into reaction tank A, and the copper sulfate filtrate is collected into reaction tank B.
3. The method for treating wastewater containing copper nitrate and copper sulfate in a high-purity copper industry according to claim 1, wherein: In the step 2, flocculants are added: 15% polyaluminium chloride is added to reaction tank A, and 20% polyacrylamide is added to reaction tank B.
4. The method for treating wastewater containing copper nitrate and copper sulfate in a high-purity copper industry according to claim 1, wherein: In the step three, the pH value of the reaction tank is optimized: when the pH of reaction tank A is less than 6, 20% sodium hydroxide is added for adjustment; when the pH of reaction tank A is greater than 9, 10% hydrochloric acid is added for adjustment; when the pH of reaction tank B is less than 6, 10% potassium hydroxide is added for adjustment; when the pH of reaction tank A is greater than 9, 5% sulfuric acid is added for adjustment.
5. The method for treating wastewater containing copper nitrate and copper sulfate in a high-purity copper industry according to claim 1, wherein: The network breaking conditions in step 4 are: S1.
1. Control the solution pH between 6-9; S1.
2. While using hydrogen peroxide, add 80 mg and 40 mg of polyacrylamide.
6. The method for treating wastewater containing copper nitrate and copper sulfate in a high-purity copper industry according to claim 1, wherein: The conversion process in step 5 is as follows: S2.1, pretreatment step: using diffusion dialysis equipment to filter the copper nitrate and copper sulfate waste liquid; S2.2 Operation process: Use sulfur dioxide as a reducing agent for the copper nitrate and copper sulfate filtrates to reduce copper sulfate to copper. Control the pH value of the copper nitrate and copper sulfate filtrates in reaction tanks A and B between 6-9. Set the ambient temperature to 20-30°C, let it stand for 2 hours, and the inlet water acidity is 5g / L. S2.
3. Re-separation: Diffusion dialysis equipment is installed at the outlet to separate copper and sulfuric acid.
7. The method for treating wastewater containing copper nitrate and copper sulfate in high-purity copper industry according to claim 1, characterized in that: In step six, the deep treatment is as follows: activated carbon with a ratio of 3 is put into reaction tank A to adsorb residual copper ions, and reverse osmosis separation technology is used to further remove the copper ions adsorbed by the activated carbon. In reaction tank B, the copper sulfate wastewater is passed through a reactor equipped with ion exchange resin at a flow rate of 10 meters per second.
8. The method for treating wastewater containing copper nitrate and copper sulfate in high-purity copper industry according to claim 1, characterized in that: In step 7, sludge stabilization treatment: When the pH of the A and B reaction tanks is greater than 9, the sludge produced by the deep treatment is subjected to stabilization treatment, using a combination of calcium oxide and magnesium salt in a ratio of 5:1, and uniformly mixed with the sludge, and then added to the A and B reaction tanks: Calcium oxide reacts with water: CaO+H2O→Ca(OH)2+heatCaO+H2O→Ca(OH)2+heat Calcium hydroxide reacts with carbon dioxide: Ca(OH)2+CO2→CaCO3+H2O+heatCa(OH)2+CO2→CaCO3+H2O+heat.
9. The method for treating wastewater containing copper nitrate and copper sulfate in high-purity copper industry according to claim 1, characterized in that: The biological leaching technology process in step 10 is as follows: when the water temperature of the A and B reaction tanks is maintained between 30-35°C and the pH value is between 6-9, a combination of Thiobacillus ferrooxidans, Thiobacillus thiooxidans, and Aspergillus niger in a ratio of 3:1:2 is added to the reaction tank to interact with the copper ions in the sludge, and 50% oxygen is introduced into the bottom of the A and B reaction tanks at the same time, and the stirring paddle is turned on for stirring for 2-4 hours.
10. The method for treating wastewater containing copper nitrate and copper sulfate in high-purity copper industry according to claim 1, characterized in that: The final treatment of step 11 is as follows: 20% sodium hydroxide, 10% hydrochloric acid, 10% potassium hydroxide or 5% sulfuric acid are added to the treated wastewater to neutralize the wastewater discharged from the A and B reaction tanks. When the pH value of the neutralization treatment is between 7 and 8, it is discharged into the integrated sewage pool or the municipal sewage network.
Citation Information
Patent Citations
Treatment method for electroless copper plating wastewater
CN110451688A
Treatment method of copper-containing wastewater
CN116606018A
The invention discloses a copper-containing wastewater treatment and copper recovery system
CN208898671U
Method for treating waste water and recovering copper, and chemical agent used therefor
JP2003251369A