Strong-adhesion electromagnetic shielding sealing rubber material as well as preparation method and application thereof
By using tackifiers such as polyisobutylene and MQ silicone resin in electromagnetic shielding sealing rubber, combined with conductive metal powder and cerium oxide, the construction of electromagnetic shielding sealing rubber when bonding at low surface energy interfaces in the prior art is solved. The problem of difficulty and degradation of adhesive force achieves efficient electromagnetic shielding performance and adhesion, ensuring the durability and reliability of electromagnetic shielding protection.
Patent Information
- Application Number
- CN202411287101.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-09-13
AI Technical Summary
When the existing electromagnetic shielding sealing rubber is bonded with low surface energy interfaces, there are problems such as difficulty in construction, poor bonding, non-shear resistance, and decreasing adhesion over time, which affects the protection effect of electromagnetic shielding.
Polyisobutylene and MQ silicone resin are used as tackifiers, combined with conductive metal powder, cerium oxide, gas-phase white carbon black and other components, to build a multi-dimensional conductive network system to improve viscosity and shear resistance, and enhance the adhesion of silicone rubber and anti-aging properties.
It realizes efficient electromagnetic shielding performance and adhesion, ensures the durability and reliability of electromagnetic shielding protection, and is suitable for the adhesion of different types of substrates, especially low-surface energy substrates such as polyethylene, polypropylene and glass.
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of electromagnetic shielding materials, and in particular to a strong-adhesion electromagnetic shielding sealing rubber material and a preparation method and application thereof. Background Art
[0002] With the continuous upgrading of electronic equipment and military equipment, a large amount of electromagnetic radiation has been generated, which has potential hazards to the normal operation of electronic equipment and human health, and also puts forward higher requirements on the electromagnetic protection capabilities of modern electronic information systems. As a new type of electromagnetic shielding material, electromagnetic shielding rubber is widely used in sealing scenarios of wireless communications, electronic equipment, and military equipment due to its excellent conductivity, processing performance and flexibility, providing good sealing and electromagnetic protection.
[0003] At present, room temperature vulcanized silicone rubber is often used in the industry to prepare electromagnetic shielding sealing materials, which are used to plug or repair gaps in electronic equipment or places. When electromagnetic shielding sealing rubber is used for plugging or repairing, it needs to be in close contact with the substrate to prevent electromagnetic waves from leaking from the gap. This requires that the electromagnetic shielding sealing rubber has good mutual adhesion and self-adhesion. However, silicone rubber has low surface energy and poor adhesion. When bonding with low surface energy interfaces such as polyethylene, polypropylene, and glass, there are a series of problems such as difficult construction, poor adhesion, no shear resistance, and decreased adhesion over time, which seriously affect the construction and greatly reduce the actual electromagnetic shielding protection effect.
[0004] Therefore, designing and optimizing the formula to improve the viscosity of the sealing rubber so that it can have both excellent electromagnetic protection effect and adhesion performance is of great significance to improving the electromagnetic protection reliability and ease of use of the electromagnetic shielding sealing rubber. Summary of the invention
[0005] In view of the deficiencies in the above-mentioned background technology, the present invention provides a strong adhesion electromagnetic shielding sealing rubber material and its preparation method and application. In the present invention, polyisobutylene and MQ silicone resin are both viscous liquid thickeners with high viscosity and strong penetration, and are widely used in pressure-sensitive adhesives, hot melt adhesives, mouse sticky boards and other fields. When applied to adhesives and sealants, it can effectively improve their viscosity, can be used to bond different types of substrates, and effectively improve the shear resistance of adhesives, making them less likely to break or deform, which is very important in some occasions. For example, when pasting hard materials such as glass and metal, strong shear resistance is required to maintain the bonding effect.
[0006] To achieve the above objectives, the first objective of the present invention is to provide a strong adhesion electromagnetic shielding sealing rubber material, comprising the following components by weight: 100 parts of 107 silicone rubber, 200-600 parts of conductive metal powder, 2-10 parts of conductive reinforcing agent, 2-10 parts of cerium oxide, 20-50 parts of tackifier, 5-15 parts of fumed silica, 4-8 parts of curing agent, and 3-6 parts of silane coupling agent; The tackifier is MQ silicone resin and / or polyisobutylene.
[0007] Preferably, the viscosity of the 107 silicone rubber is 750-100000 mPa﹒s.
[0008] Preferably, the conductive metal powder is one or more of silver-coated copper powder, silver-coated aluminum powder, silver-coated nickel powder, and silver-coated glass beads.
[0009] Preferably, the conductive reinforcing agent is one or more of silver powder, conductive carbon black, carbon nanotubes, and graphene.
[0010] Preferably, the particle size of the silver powder is 1-20 μm; the particle size of the cerium oxide is 10-50 μm.
[0011] Preferably, the curing agent is one or more of methyltrimethoxysilane, methyltriethoxysilane, tetramethoxysilane, dibutyltin dilaurate, and dibutyltin diacetate.
[0012] Preferably, the silane coupling agent is one or more of KH-550, KH-560, KH-570, and KH-792.
[0013] The second object of the present invention is to provide a method for preparing a strong adhesion electromagnetic shielding sealing rubber material, comprising the following steps: The 107 silicone rubber, conductive metal powder, conductive reinforcing agent, cerium oxide, tackifier and fumed silica are added into a kneader, and mixed under vacuum at 110-130° C. for 1-2 hours to remove internal moisture as a first-stage glue; after the first-stage glue is cooled to ≤50° C., it is added into a double planetary mixer, stirred, and a curing agent is added, and the mixture is vacuum stirred for 30-60 minutes, and then taken out for packaging.
[0014] The third object of the present invention is to provide a rubber material for use in electromagnetic shielding.
[0015] Compared with the prior art, the present invention has the following beneficial effects: The present invention provides a strong adhesion electromagnetic shielding sealing rubber material and its preparation method and application. By adding conductive metal powder as a primary conductive filler and a conductive reinforcing agent as a secondary conductive filler, a multi-dimensional conductive network system is constructed to achieve synergistic enhancement of conductivity; cerium oxide is used as an antioxidant to reduce the decrease in the binding force on the filler caused by rubber aging, thereby extending the service life; the tackifier has good compatibility with silicone rubber, weakens the intermolecular force of silicone rubber, improves the flexibility of silicone rubber and provides excellent adhesion, and the end group of the silane coupling agent contains amino groups, epoxy groups, etc., which improve the wettability with the bonding substrate, and the synergistic effect of the two gives silicone rubber strong adhesion; fumed silica reinforces silicone rubber to improve the strength and shear resistance of silicone rubber. The strong adhesion electromagnetic shielding sealing rubber material prepared by the present invention has both high shielding performance and high adhesion. The strong adhesion electromagnetic shielding sealing rubber material prepared by the preparation method provided by the present invention is easy to construct and has a wide range of applicability. It can be used to bond low surface energy substrates such as polyethylene, polypropylene, and glass, and other high surface energy substrates, and can adhere to the vertical interface without falling off. The strong adhesion electromagnetic shielding sealing rubber material prepared by the preparation method is resistant to shearing and has long-lasting adhesion, thereby ensuring the durability and reliability of electromagnetic shielding protection. DETAILED DESCRIPTION
[0016] In order to enable those skilled in the art to better understand and implement the technical solution of the present invention, the present invention is further described below in conjunction with specific embodiments, but the embodiments are not intended to limit the present invention.
[0017] The polyisobutylene and MQ silicone resin provided by the present invention are both viscous liquid tackifiers with high viscosity and strong penetration, and are widely used in the fields of pressure-sensitive adhesives, hot melt adhesives, mouse traps, etc. When applied to adhesives and sealants, they can effectively improve their viscosity, can be used to bond different types of substrates, and effectively improve the shear resistance of the adhesive, making it less likely to break or deform, which is very important in some occasions. For example, when bonding hard materials such as glass and metal, strong shear resistance is required to maintain the bonding effect.
[0018] The first aspect of the present invention provides a strong adhesion electromagnetic shielding sealing rubber material, comprising the following components by weight: 100 parts of 107 silicone rubber, 200-600 parts of conductive metal powder, 2-10 parts of conductive reinforcing agent, 2-10 parts of cerium oxide, 20-50 parts of tackifier, 5-15 parts of fumed silica, 4-8 parts of curing agent, and 3-6 parts of silane coupling agent; The tackifier is MQ silicone resin and / or polyisobutylene.
[0019] The viscosity of the 107 silicone rubber is 750-100000 mPa﹒s.
[0020] The conductive metal powder is one or more of silver-coated copper powder, silver-coated aluminum powder, silver-coated nickel powder, and silver-coated glass microbeads.
[0021] The conductive reinforcing agent is one or more of silver powder, conductive carbon black, carbon nanotubes, and graphene.
[0022] The particle size of the silver powder is 1-20 μm; the particle size of the cerium oxide is 10-50 μm.
[0023] The curing agent is one or more of methyltrimethoxysilane, methyltriethoxysilane, tetramethoxysilane, dibutyltin dilaurate, and dibutyltin diacetate.
[0024] The silane coupling agent is one or more of KH-550, KH-560, KH-570 and KH-792.
[0025] A second aspect of the present invention provides a method for preparing a strong adhesion electromagnetic shielding sealing rubber material, comprising the following steps: The 107 silicone rubber, conductive metal powder, conductive reinforcing agent, cerium oxide, tackifier and fumed silica are added into a kneader, and mixed under vacuum at 110-130° C. for 1-2 hours to remove internal moisture as a first-stage glue; after the first-stage glue is cooled to ≤50° C., it is added into a double planetary mixer, stirred, and a curing agent is added, and the mixture is vacuum stirred for 30-60 minutes, and then taken out for packaging.
[0026] In one embodiment, a method for preparing a strong adhesion electromagnetic shielding sealing rubber material comprises the following steps: Add the 107 silicone rubber, conductive metal powder, conductive reinforcing agent, cerium oxide, tackifier, and fumed silica into a kneader, vacuum and stir at 120°C for 1-2 hours, and remove the internal moisture to form a first-stage glue. After the first-stage glue is cooled to below 50°C, add it into a double planetary mixer, stir it, add the curing agent, vacuum and stir for 30-60 minutes, and take it out for packaging.
[0027] A third aspect of the present invention provides an application of a rubber material in electromagnetic shielding.
[0028] It should be noted that the experimental methods used in the present invention are all conventional methods unless otherwise specified; the reagents and materials used are all commercially available unless otherwise specified.
[0029] The following embodiment provides a method for preparing a strong adhesion electromagnetic shielding sealing rubber material, which is specifically as follows: According to the formula in Table 1, after weighing the materials according to the mass ratio, add the materials into the kneader, seal the kneader and start running, set the kneader temperature to 120°C, evacuate, stir and mix for 2 hours, then turn off the heating, and wait for the materials to cool to below 50°C. This process ensures that the vacuum pump continues to operate. Transfer a section of glue to a double planetary mixer, add a curing agent and a silane coupling agent, seal, evacuate and stir and mix. After continuing to mix for 30 minutes, take out the materials and package them to obtain an embodiment.
[0030] Table 1 Electromagnetic shielding sealing rubber material formula (weight ratio) project Example 1 Example 2 Example 3 Example 4 Comparative Example 1 Comparative Example 2 107 silicone rubber, viscosity 750 mPa﹒ s. 80 70 0 0 0 0 107 silicone rubber, viscosity 30000 mPa﹒ s. 0 0 100 100 100 100 107 silicone rubber, viscosity 100000 mPa﹒ s. 20 30 0 0 0 0 Silver-coated aluminum powder, particle size 20μm 300 0 450 0 0 0 Silver coated glass beads, particle size 40μm 0 350 0 0 350 0 Silver-coated copper powder, particle size 40μm 0 0 0 400 0 400 Silver powder 10 0 5 0 0 0 Carbon Nanotubes 0 5 0 3 5 3 Cerium Oxide 3 4 5 4 4 4 MQ Silicone Resin 30 30 0 0 0 0 Polyisobutylene 0 0 40 40 0 0 Curing agent 4 4 6 6 4 6 Silane coupling agent KH-550 2 2 3 3 2 3 Silane coupling agent KH-792 1 1 2 2 1 2 The adhesives of Examples 1 to 4 were subjected to performance tests.
[0031] Test the bonding performance of polypropylene according to GB / T7124-2008 "Determination of tensile shear strength of adhesives (rigid material to rigid material)" Test the surface drying time of the rubber compound according to the provisions of GB / T13477.5-2002.
[0032] The shear displacement capacity is tested according to GB / T 22083-2008 "Classification and requirements of building adhesives".
[0033] The electromagnetic shielding performance of the rubber compound is tested according to MIL-G-83528.
[0034] Table 2 Performance of Examples and Comparative Examples project Example 1 Example 2 Example 3 Example 4 Comparative Example 1 Comparative Example 2 Surface drying time, min 26min 28min 32min 30min 25min 28min Bond strength, MPa, polypropylene 0.68 0.67 0.75 0.72 0.26 0.23 Displacement Capacity ±50 √ √ √ √ × × +100 / -50 √ √ √ √ × × Volume resistivity, mΩ·cm 3.6 2.2 1.6 2.5 1.7 1.2 Shielding effectiveness, 10MHz 65 68 74 72 69 75 Shielding Effectiveness, 10GHz 85 88 112 108 90 112 Shielding Effectiveness, 18GHz 95 98 115 112 106 114 As can be seen from Table 2, compared with Comparative Example 1-2, the surface drying time and conductive properties of Example 1-4 are not much different, but because the tackifier has a similar modulus to the silicone rubber and good compatibility, it can be evenly dispersed in the silicone rubber, penetrate into the silicone rubber molecular chains to weaken the interaction between the silicone rubber molecular chains, improve the flexibility of the silicone rubber, and entangle with the silicone rubber molecular chains. The dispersion of fumed silica in the matrix forms segregation, most of which reinforces the silicone rubber matrix and improves the strength of the silicone rubber. A small amount exists in the tackifier, which retains the flexibility of the tackifier, and significantly improves the shear resistance and bonding performance of the silicone rubber. It can be used for bonding in low surface energy interface electromagnetic shielding occasions such as polyethylene, polypropylene, and glass. It has strong shear resistance and can solve a series of problems such as the difficulty of bonding construction of electromagnetic shielding sealing rubber, poor bonding, non-shear resistance, and decreased bonding force over time. However, in Comparative Example 1-2, no tackifier was added to toughen and thicken the silicone rubber, resulting in lower rubber bonding strength; the fumed silica over-reinforced the silicone rubber, which, on the one hand, easily formed stress concentration inside the silicone rubber, and on the other hand, caused interface damage between the silicone rubber and the bonding substrate, resulting in bonding failure.
[0035] The above is only the best implementation mode of the present invention, but the protection scope of the patent of the present invention is not limited to this. All technicians familiar with this technical field can also make various corresponding changes and modifications to the present invention. Under the premise of not violating the principles of the invention, they should all fall within the protection scope of the claims attached to the present invention.
Claims
1. A strong adhesion electromagnetic shielding sealing rubber material, characterized in that: The composition comprises the following components by weight: 100 parts of 107 silicone rubber, 200-600 parts of conductive metal powder, 2-10 parts of conductive reinforcing agent, 2-10 parts of cerium oxide, 20-50 parts of tackifier, 5-15 parts of fumed silica, 4-8 parts of curing agent, and 3-6 parts of silane coupling agent; The tackifier is MQ silicone resin and / or polyisobutylene.
2. The strong adhesion electromagnetic shielding sealing rubber material according to claim 1, characterized in that: The viscosity of the 107 silicone rubber is 750-100000 mPa﹒s.
3. The strong adhesion electromagnetic shielding sealing rubber material according to claim 1, characterized in that: The conductive metal powder is one or more of silver-coated copper powder, silver-coated aluminum powder, silver-coated nickel powder, and silver-coated glass microbeads.
4. The strong adhesion electromagnetic shielding sealing rubber material according to claim 1, characterized in that: The conductive reinforcing agent is one or more of silver powder, conductive carbon black, carbon nanotubes, and graphene.
5. The strong adhesion electromagnetic shielding sealing rubber material according to claim 1, characterized in that: The particle size of the silver powder is 1-20 μm; the particle size of the cerium oxide is 10-50 μm.
6. The strong adhesion electromagnetic shielding sealing rubber material according to claim 1, characterized in that: The curing agent is one or more of methyltrimethoxysilane, methyltriethoxysilane, tetramethoxysilane, dibutyltin dilaurate, and dibutyltin diacetate.
7. The strong adhesion electromagnetic shielding sealing rubber material according to claim 1, characterized in that: The silane coupling agent is one or more of KH-550, KH-560, KH-570 and KH-792.
8. A method for preparing the strong adhesion electromagnetic shielding sealing rubber material according to any one of claims 1 to 7, characterized in that: The following steps are involved: Add the 107 silicone rubber, conductive metal powder, conductive reinforcing agent, cerium oxide, tackifier, and fumed silica into a kneader, and mix them under vacuum at 110-130° C. for 1-2 hours to remove the internal moisture to form a first-stage glue; After a section of glue is cooled to ≤50℃, add it to a double planetary mixer, stir it, add curing agent, vacuum and stir for 30~60 minutes, and then take it out and package it.
9. Use of the rubber material according to any one of claims 1 to 7 in electromagnetic shielding.
Citation Information
Patent Citations
Single-component room-temperature vulcanization conductive silica gel and preparation method thereof
CN105907361A
Organosilicon electromagnetic shielding pressure-sensitive adhesive and preparation method thereof
CN110713816A
Cable accessory insulation reinforcing sealant as well as preparation method and application thereof
CN116814214A
Liquid silicone elastomer composition for radiation-shielding material, method of producing liquid silicone elastomer composition for radiation-shielding material, and molded article of radiation-shielding silicone rubber