Photocuring wafer grinding protective adhesive tape, preparation method thereof and wafer thinning method
By adjusting the ratio of modified acrylic resin to hardeners and photoinitiators, combining delay catalysts and organic nano-colored powders, a photocurable wafer grinding protective tape is formed, and contamination caused by insufficient peeling force or excessive weight in the prior art is solved. and damage problems achieve effective protection and efficient thinning of wafers.
Patent Information
- Application Number
- CN202411523972.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-30
- Publication Date
- 2024-11-26
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
During the manufacturing process of semiconductor devices, the existing wafer abrasive protective tape is insufficient during peeling, resulting in contamination, or the peeling force is too large to damage the wafer structure, affecting the chip quality.
The photocurable wafer grinding protective tape is used to adjust the ratio of the modified acrylic resin to the hardener and photoinitiator, and combine the retardant catalyst and organic nano-colored powder to form an adhesive layer to control the peeling force and improve the protection effect.
It realizes effective protection of wafers during wafer grinding and thinning, avoids contamination and damage, ensures subsequent chip production efficiency, and does not have residual glue after peeling.
Smart Images

Figure CN119019947A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of semiconductor wafer processing, and in particular relates to a light-curing wafer grinding protection tape and a preparation method thereof, and a wafer thinning method. Background Art
[0002] With the development of science and technology, in the field of semiconductor device manufacturing, the size of semiconductor devices continues to decrease, and the size of electronic chips also continues to decrease. For this reason, in the process of semiconductor device manufacturing, after many semiconductor devices are formed on the functional surface of the wafer, a wafer back grinding process is performed, and a flattening process is used to grind the back of the wafer corresponding to the functional surface to remove part of the thickness of the wafer to reduce the thickness of the chip formed subsequently. In the process of grinding the back of the wafer, a layer of protective tape will first be covered on the functional surface of the wafer to protect the wafer from contamination by impurities or water during the grinding process to ensure the quality of the chip. However, after the grinding is completed, the protective tape needs to be peeled off from the functional surface of the wafer. When the peeling force is large, it is easy to damage the structure on the functional surface of the wafer and affect the normal operation of the chip; when the peeling force is small, glue penetration is easy to occur during the grinding process, resulting in chip contamination.
[0003] Therefore, how to provide a photocurable wafer grinding protection tape, and control the peeling force between the wafer grinding protection tape and the wafer by adjusting the ratio between the modified acrylic resin, the hardener and the photoinitiator, thereby improving the protection effect of the wafer during the grinding and thinning process, is a technical problem that technical personnel in this field urgently need to solve. Summary of the invention
[0004] The object of the present invention is to provide a photocurable wafer grinding protective tape and a preparation method thereof, and a wafer thinning method, so as to solve at least one of the above-mentioned technical problems.
[0005] To achieve the above-mentioned purpose, the first aspect of the present invention provides a photocurable wafer grinding protective tape, which comprises an adhesive layer and a substrate layer, wherein the substrate layer is made of thermoplastic polyurethane; the adhesive layer comprises the following components by mass percentage: 61% to 63% of modified acrylic resin, 1.5% to 3.5% of hardener, 1.0% to 2.5% of photoinitiator, 3.1% of delayed catalyst, 0.3% of organic nano-color powder, and 30% to 32% of solvent.
[0006] In the first aspect, the mass ratio of the modified acrylic resin to the hardener is 100:3 to 100:5, and the mass ratio of the modified acrylic resin to the photoinitiator is 100:2 to 100:4.
[0007] In the first aspect, the hardener comprises an aliphatic polyisocyanate.
[0008] In the first aspect, the photoinitiator is a free radical type photoinitiator.
[0009] In a first aspect, the delayed catalyst comprises acetylacetone.
[0010] In the first aspect, the model of the organic nano-color powder includes 7080K.
[0011] In the first aspect, the solvent comprises ethyl acetate.
[0012] The second aspect of the present invention provides a method for preparing a photocurable wafer grinding protective tape as described in the first aspect, characterized in that the preparation method comprises: adding the components of the bonding layer into a mixing barrel according to their respective mass percentages, and stirring them evenly by a planetary mixer to obtain a first slurry, wherein the mass percentages of the components specifically include: 61% to 63% of modified acrylic resin, 1.9% to 3.1% of hardener, 1.2% to 2.5% of photoinitiator, 3% to 3.1% of delayed catalyst, 0.3% of organic nano-color powder, and 30% to 32% of solvent; transferring the first slurry to the vacuum degassing barrel, performing vacuum degassing, and obtaining a second slurry; coating the second slurry on a release film, baking and drying, and obtaining a bonding layer; laminating a substrate layer on the bonding layer, removing the release film, and obtaining a photocurable wafer grinding protective tape.
[0013] In the second aspect, the working parameters of the planetary mixer include: stirring time of 5 to 15 minutes, stirring speed of 1200r / min; the vacuum degassing is positive pressure degassing, and the working parameters of the positive pressure degassing include: degassing time of 10 to 30 minutes, degassing pressure of 0.5MPa; the coating method is slit coating; the baking temperature is 60 to 90°C.
[0014] The third aspect of the present invention provides a wafer thinning method, which includes: obtaining a wafer body; setting a plurality of raised electrodes on the front side of the wafer body to form a wafer functional surface; laminating a layer of photocurable wafer grinding protection tape as described in the first aspect on the wafer functional surface, and performing grinding to obtain a ground wafer; placing the ground wafer under ultraviolet light, and performing photocuring to obtain a photocured wafer; and peeling off the wafer grinding protection tape from the photocured wafer to obtain a thinned wafer.
[0015] Beneficial effects: The invention provides a photocurable wafer grinding protection tape, which is used for protecting a wafer from being polluted and damaged during wafer grinding and thinning. The tape comprises a bonding layer and a substrate layer, wherein the substrate layer is made of thermoplastic polyurethane so as to cut the wafer. The bonding layer comprises the following components by mass percentage: 61% to 63% of a modified acrylic resin, 1.5% to 3.5% of a hardener, 1.0% to 2.5% of a photoinitiator, 3.1% of a delayed catalyst, 0.3% of an organic nano-color powder, and 30% to 32% of a solvent. The modified acrylic resin contains a plurality of functional groups, so that the initial adhesion of the modified acrylic resin is too high. By adding the hardener, the active functional groups in the molecule are reduced, the adhesion of the bonding layer is reduced, and the film-forming property and hardness of the bonding layer are also improved through a cross-linking reaction. By adding the photoinitiator, the photoinitiator reacts with the remaining active functional groups under ultraviolet light, so as to further reduce the adhesion of the bonding layer and improve the hardness of the bonding layer, thereby improving the protective effect on the wafer during the wafer grinding and thinning process. The present invention improves the film-forming property and hardness of the bonding layer and reduces the adhesion to the wafer by adjusting the ratio between the modified acrylic resin, the hardener and the photoinitiator, and combining the delayed catalyst, the organic nano-color powder and the solvent, thereby controlling the peeling force between the wafer grinding protection tape and the wafer and improving the protective effect of the wafer grinding protection tape on the wafer during the grinding and thinning process. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiments of this specification or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0017] Figure 1 A flow chart of a method for preparing a light-curing wafer grinding protection tape provided by the present invention; Figure 2 The present invention provides a flow chart of a wafer thinning method. DETAILED DESCRIPTION
[0018] The present invention will be described in detail below in conjunction with specific implementations and examples, and the advantages and various effects of the present invention will be more clearly presented. It should be understood by those skilled in the art that these specific implementations and examples are used to illustrate the present invention, rather than to limit the present invention.
[0019] Throughout the specification, unless otherwise specifically stated, the terms used herein should be understood as meanings commonly used in the art. Therefore, unless otherwise defined, all technical and scientific terms used herein have the same meanings as those generally understood by those skilled in the art to which the present invention belongs. In the event of a conflict, the present specification takes precedence.
[0020] Unless otherwise specified, various raw materials, reagents, instruments and equipment used in the present invention can be purchased from the market or obtained by existing methods.
[0021] The present invention provides a photocurable wafer grinding protection tape, which comprises an adhesive layer and a substrate layer, wherein the substrate layer is made of thermoplastic polyurethane; the adhesive layer comprises the following components by mass percentage: 61% to 63% of modified acrylic resin, 1.5% to 3.5% of hardener, 1.0% to 2.5% of photoinitiator, 3.1% of delayed catalyst, 0.3% of organic nano-color powder, and 30% to 32% of solvent.
[0022] Specifically, the present invention provides a photocurable wafer grinding protection tape, which is used to protect wafers from being contaminated and damaged during wafer grinding and thinning. The tape comprises an adhesive layer and a substrate layer, wherein the substrate layer is made of thermoplastic polyurethane so as to cut the wafer; the adhesive layer comprises the following components by mass percentage: 61% to 63% of modified acrylic resin, 1.5% to 3.5% of hardener, 1.0% to 2.5% of photoinitiator, 3.1% of delayed catalyst, 0.3% of organic nano-color powder, and 30% to 32% of solvent. The modified acrylic resin contains multiple functional groups, so that the initial adhesion of the modified acrylic resin is too high. By adding the hardener, the active functional groups in the molecule are reduced, the adhesion of the adhesive layer is reduced, and the film-forming property and hardness of the adhesive layer are also improved through a cross-linking reaction; by adding the photoinitiator, the photoinitiator reacts with the remaining active functional groups under ultraviolet light, further reducing the adhesion of the adhesive layer and improving the hardness of the adhesive layer, thereby improving the protective effect on the wafer during wafer grinding and thinning. The present invention improves the film-forming property and hardness of the bonding layer and reduces the adhesion to the wafer by adjusting the ratio between the modified acrylic resin, the hardener and the photoinitiator, and combining the delayed catalyst, the organic nano-color powder and the solvent, thereby controlling the peeling force between the wafer grinding protection tape and the wafer and improving the protective effect of the wafer grinding protection tape on the wafer during the grinding and thinning process.
[0023] In some possible embodiments, the mass ratio of the modified acrylic resin to the hardener is 100:3 to 100:5, and the mass ratio of the modified acrylic resin to the photoinitiator is 100:2 to 100:4.
[0024] This is because the modified acrylic resin, as the base resin of the bonding layer, provides the bonding performance of the bonding layer. Taking the modified acrylic resin as the benchmark, when the amount of hardener added is too large, the cross-linking reaction between the modified acrylic resin and the hardener is complete, and the adhesion of the bonding layer is significantly reduced, but the hardness of the bonding layer will also increase significantly, resulting in loose bonding with the wafer, bubbles, and easy water seepage after immersion in water. In the subsequent wafer grinding and thinning process, the wafer structure is easily damaged, thereby affecting the chip production efficiency; when the amount of hardener added is too small, there are still a large number of active functional groups in the modified acrylic resin. When the amount of photoinitiator added is too small, the reaction is also incomplete, and there are still a large number of active functional groups in the bonding layer, resulting in the presence of colloids on the wafer after stripping; when the amount of photoinitiator added is too large, the active functional groups of the bonding layer are almost completely reacted, and the bonding force and hardness of the bonding layer are moderate, which can be used to protect the wafer during the wafer grinding and thinning process, but the production cost will be increased. Therefore, in the present application, the adhesion and hardness of the bonding layer are adjusted by controlling the ratio of the hardener and the photoinitiator to be suitable for the protection of the wafer during the wafer grinding and thinning process. In a specific embodiment, the model of the modified acrylic resin can be HSN10-0, SD-612 or CF-679.
[0025] In some possible embodiments, the hardener includes aliphatic polyisocyanate.
[0026] Those skilled in the art can understand that the hardener includes aliphatic polyisocyanate, which can undergo a cross-linking reaction with a modified acrylic resin to form a network structure to reduce the adhesion of the bonding layer and improve the film-forming property of the bonding layer. The model of the aliphatic polyisocyanate can be N3300.
[0027] In some possible embodiments, the photoinitiator is a free radical photoinitiator.
[0028] This is because the free radical photoinitiator will break down into free radicals under the irradiation of ultraviolet light, and quickly undergo photo-crosslinking and curing reaction with the modified acrylic resin, thereby reducing the adhesion of the bonding layer. The model of the free radical photoinitiator can be 907.
[0029] In some possible embodiments, the delay catalyst includes acetylacetone.
[0030] Those skilled in the art will appreciate that adding acetylacetone to the bonding layer can slow down the photocuring reaction between the photoinitiator and the modified acrylic resin, thereby improving the film-forming property of the bonding layer so that it can be closely bonded to the wafer later.
[0031] In some possible embodiments, the model of the organic nano-color powder includes 7080K.
[0032] In some possible embodiments, the solvent includes ethyl acetate.
[0033] By selecting ethyl acetate as the solvent, the raw materials in the bonding layer can be completely dissolved, thereby increasing the subsequent cross-linking reaction rate and improving the film-forming property of the bonding layer.
[0034] Based on a general inventive concept, see Figure 1 The second aspect of the present invention provides a method for preparing the light-curing wafer grinding protection tape as described in the first aspect, the preparation method comprising: S1. Add the components of the bonding layer into a mixing barrel according to their respective mass percentages, and mix them evenly with a planetary mixer to obtain a first slurry, wherein the mass percentages of the components specifically include: 61% to 63% of modified acrylic resin, 1.9% to 3.1% of hardener, 1.2% to 2.5% of photoinitiator, 3% to 3.1% of delayed catalyst, 0.3% of organic nano-color powder, and 30% to 32% of solvent; S2, transferring the first slurry to the vacuum degassing barrel, performing vacuum degassing to obtain a second slurry; S3, coating the second slurry on the release film, baking and drying, to obtain a bonding layer; S4, laminating a substrate layer on the adhesive layer, removing the release film, and obtaining a light-curing wafer grinding protective tape.
[0035] In combination with the second aspect of the present application, the working parameters of the planetary mixer include: stirring time of 5 to 15 minutes, stirring speed of 1200r / min; the vacuum degassing is positive pressure degassing, and the working parameters of the positive pressure degassing include: degassing time of 10 to 30 minutes, degassing pressure of 0.5MPa; the coating method is slit coating; the baking temperature is 60 to 90°C.
[0036] Specifically, the present application provides a method for preparing a photocurable wafer grinding protective tape, which comprises the following steps: first, preparing an adhesive layer, adding each component of the raw materials in the adhesive layer into a mixing barrel according to their respective mass percentages, and mixing them evenly using a planetary mixer to obtain a first slurry; then transferring the slurry to a vacuum degassing barrel for positive pressure degassing to remove bubbles generated during the mixing process to obtain a second slurry, so as to improve the film-forming property of the adhesive layer; then, coating the second slurry on a release film using a slit-type coating method, and baking and drying the slurry to remove small molecule solvents to obtain an adhesive layer with adhesion and film-forming property; finally, laminating a substrate layer on the upper layer of the adhesive layer, and removing the release film to obtain a photocurable wafer grinding protective tape, and transferring the photocurable wafer grinding protective tape to the functional surface of the wafer to protect the wafer from damage during the grinding and thinning process, and the wafer can also be cut using the photocurable wafer grinding protective tape to obtain a number of chips.
[0037] Based on a general inventive concept, the third aspect of the present invention provides a wafer thinning method, the wafer thinning method comprising: Obtaining a wafer body; A plurality of protruding electrodes are arranged on the front surface of the wafer body to form a wafer functional surface; Laying a layer of the light-curable wafer grinding protection tape as described in the first aspect on the functional surface of the wafer, and performing grinding to obtain a ground wafer; Placing the ground wafer under ultraviolet light for photocuring to obtain a photocured wafer; The wafer grinding protection tape is peeled off from the photocured wafer to obtain a thinned wafer.
[0038] The present application will be further described below in conjunction with specific embodiments. It should be understood that these embodiments are intended only to illustrate the present application and are not intended to limit the scope of the present application. The experimental methods for which specific conditions are not specified in the following examples are usually measured according to national standards. If there is no corresponding national standard, then the conditions recommended by the manufacturer are followed.
[0039] The components of the bonding layer raw materials in the wafer grinding protection tapes in Comparative Examples 1-6 and Examples 1-9 are shown in Table 1 according to mass percentage: Table 1 Mass percentage of each component of bonding layer raw materials The wafer grinding protection tapes provided in Examples 1-9 and Comparative Examples 1-6 were subjected to peeling force test, water seepage test, film sticking test, grinding test and residual adhesive test before and after UV curing. The specific test process is as follows: 1. Peel force test of wafer grinding protective tape before and after UV curing: Test reference standard: ASTM D3330-04, tested using a universal tensile machine.
[0040] 2. Water seepage test: After the wafer grinding protection tape is attached to the wafer, soak it in water for 36 hours and observe whether there is water seepage under a microscope. The number of wafers tested: 25.
[0041] 3. Film test: Use a semi-automatic wafer film mounter to mount the film, and observe the bonding effect (whether there are bubbles) under a microscope. The number of films mounted: 25 pieces.
[0042] 4. Grinding test: After the wafer grinding protection tape is attached to the wafer, grinding is carried out, and TTV (total thickness change) is measured after grinding; the test equipment is a Lintec grinder, and the grinding is performed first in rough grinding and then in fine grinding. The initial thickness of the wafer is 750μm, and it is thinned to 150μm; the number of grinding wafers: 25 pieces.
[0043] 5. Residual adhesive test: After the wafer grinding protection tape is attached to the wafer, it is ground by a grinder and then the film is peeled off to observe whether there is any residual adhesive on the wafer; number of test pieces: 25 pieces.
[0044] The test results are shown in Table 2 below: Table 2 Test results From the above table, we can see that: (1) In Comparative Example 1, the mass ratio of modified acrylic resin to hardener is 100:2, and no photoinitiator is added. Under this ratio, after the modified acrylic resin reacts with polyisocyanate, the modified acrylic resin has more residual active functional groups, resulting in a relatively high peel strength of the adhesive layer, and the insufficient degree of crosslinking leads to a relatively low strength of the adhesive layer, resulting in a large amount of residual adhesive when the film is torn off; (2) In Comparative Example 2, the mass ratio of modified acrylic resin to hardener was 100:6, and no photoinitiator was added. Under this ratio, after the modified acrylic resin reacted with polyisocyanate, the remaining active functional groups of the acrylic resin were relatively small, resulting in low peel strength of the adhesive layer, and the degree of crosslinking was too high, resulting in high strength of the adhesive layer, bubbles when applying the film, and water seepage after soaking in water; (3) In Comparative Example 3, the added mass ratio of modified acrylic resin: hardener is 100:4. Under this ratio, after the modified acrylic resin reacts with polyisocyanate, the amount of remaining active functional groups of the modified acrylic resin is within a controllable range, the peel strength of the adhesive layer is moderate, the film lamination effect is good, there are no bubbles, and no water seepage, but residual glue appears due to the lack of photoinitiator; (4) In Comparative Example 4, the mass ratio of modified acrylic resin: photoinitiator is 100:1, and the mass ratio of modified acrylic resin: hardener is controlled to be 100:4. Under this ratio, the proportion of photoinitiator is too small, resulting in a large number of residual active functional groups in the modified acrylic resin after photocrosslinking and curing, a high peel strength of the adhesive layer after photocuring, and residual adhesive when the film is torn off; (5) The test results of Comparative Example 5 and Comparative Example 6 are almost the same, but the amount of photoinitiator in Comparative Example 5 is too much, which means that the excess photoinitiator does not participate in the reaction and has little effect on the performance of the wafer grinding protection tape, but it will increase the cost. From the perspective of production cost, the amount of photoinitiator added should be controlled; (6) In Examples 1-9, the addition ratio of modified acrylic resin: hardener is between 100:3 and 100:5, and the addition ratio of modified acrylic resin: photoinitiator is between 100:2 and 100:4. After the modified acrylic resin reacts with polyisocyanate, the amount of remaining active functional groups in the modified acrylic resin is within a controllable range, the peel strength of the adhesive layer is moderate, the film-sticking effect is good, there are no bubbles, no water seepage, and after light curing, the test results are good.
[0045] To sum up, the photocurable wafer grinding protection tape provided by the present invention has an ultra-thin grinding function. During the wafer grinding and thinning process, it can provide support for the wafer to prevent the wafer from bending and sagging. After ultraviolet light curing, the wafer grinding protection tape can be easily peeled off from the functional surface of the wafer without residual adhesive. It not only achieves the effect of wafer thinning, but also provides protection for the wafer, thereby improving the subsequent chip production efficiency.
[0046] Finally, it should be noted that the terms "comprises," "includes," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that includes a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements that are inherent to such process, method, article, or apparatus.
[0047] Although the preferred embodiments of the present invention have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.
[0048] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A light-curing wafer grinding protective tape, characterized in that: The wafer grinding protection tape comprises an adhesive layer and a substrate layer, wherein the substrate layer is made of thermoplastic polyurethane; the adhesive layer comprises the following components by mass percentage: 61% to 63% of modified acrylic resin, 1.5% to 3.5% of hardener, 1.0% to 2.5% of photoinitiator, 3.1% of delayed catalyst, 0.3% of organic nano-color powder, and 30% to 32% of solvent.
2. The light-curing wafer grinding protection tape according to claim 1, characterized in that: The mass ratio of the modified acrylic resin to the hardener is 100:3 to 100:5, and the mass ratio of the modified acrylic resin to the photoinitiator is 100:2 to 100:
4.
3. The light-curing wafer grinding protection tape according to claim 2, characterized in that: The hardener includes an aliphatic polyisocyanate.
4. The light-curing wafer grinding protection tape according to claim 3, characterized in that: The photoinitiator is a free radical photoinitiator.
5. The light-curing wafer grinding protection tape according to claim 4, characterized in that: The delayed catalyst includes acetylacetone.
6. The light-curing wafer grinding protection tape according to claim 5, characterized in that: The models of the organic nano-color powder include 7080K.
7. The light-curing wafer grinding protection tape according to claim 6, characterized in that: The solvent includes ethyl acetate.
8. A method for preparing the light-curing wafer grinding protection tape according to any one of claims 1 to 7, characterized in that: The preparation method comprises: Add the components of the bonding layer into a mixing barrel according to their respective mass percentages, and mix them evenly with a planetary mixer to obtain a first slurry, wherein the mass percentages of the components specifically include: 61% to 63% of modified acrylic resin, 1.9% to 3.1% of hardener, 1.2% to 2.5% of photoinitiator, 3% to 3.1% of delayed catalyst, 0.3% of organic nano-color powder, and 30% to 32% of solvent; Transferring the first slurry to the vacuum degassing barrel and performing vacuum degassing to obtain a second slurry; The second slurry is coated on the release film, and baked and dried to obtain a bonding layer; A base material layer is laminated on the adhesive layer, and the release film is removed to obtain a light-curing wafer grinding protective tape.
9. The method for preparing the light-curing wafer grinding protection tape according to claim 8, characterized in that: The working parameters of the planetary mixer include: stirring time of 5 to 15 minutes, stirring speed of 1200 r / min; The vacuum degassing is positive pressure degassing, and the working parameters of the positive pressure degassing include: degassing time is 10 to 30 minutes, and degassing pressure is 0.5 MPa; The coating method is slot coating; The baking temperature is 60-90°C.
10. A wafer thinning method, characterized in that: The wafer thinning method comprises: Obtaining a wafer body; A plurality of protruding electrodes are arranged on the front surface of the wafer body to form a wafer functional surface; Laying a layer of the light-curable wafer grinding protection tape as described in any one of claims 1 to 7 on the functional surface of the wafer, and performing grinding to obtain a ground wafer; Placing the ground wafer under ultraviolet light for photocuring to obtain a photocured wafer; The wafer grinding protection tape is peeled off from the photocured wafer to obtain a thinned wafer.
Citation Information
Patent Citations
Adhesive tape for protecting surfaces of semiconductor wafers and method for processing semiconductor wafer
CN108028190A
Protective adhesive tape for wafer grinding and preparation method thereof
CN111925739A
Adhesive and UV adhesive tape
CN115181515A
Ultraviolet debonding protective film for wafer cutting as well as preparation method and application of ultraviolet debonding protective film
CN117186790A
Adhesive tape
CN117659884A
Cited By
Adhesive tape for semiconductor wafer thinning and preparation process thereof
CN121045980A