Machine barrel for drying high polymer material and expansion dryer

By designing multiple independent heating jacket blocks and anti-corrosion layers in the expansion dryer, the stress corrosion and uneven heating problems caused by chloride ion corrosion are solved, and the convenience of replacement and the extension of service life are achieved.

CN119022588AActive Publication Date: 2024-11-26CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202310592325.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-24
Publication Date
2024-11-26
Estimated Expiration
2043-05-24

AI Technical Summary

Technical Problem

The heating jacket of the expansion dryer works for a long time in the chloride-containing corrosive medium, resulting in stress corrosion and cracking, affecting service life, and in the prior art, the heating is uneven and the replacement cost is high.

Method used

Design a barrel for drying polymer materials, adopting multiple independent heating jacket blocks, each jacket block is equipped with a high-temperature steam air inlet and air outlet, and cobalt-based and tungsten-nickel cobalt carbide on the surface of the cylinder Anti-corrosion layer to increase the resistance to chlorine corrosion.

Benefits of technology

The uniformity of heating and convenience of replacement are achieved, the replacement cost is reduced, and the service life of the cylinder is extended through the anti-corrosion layer, cracking is prevented, and the normal operation of the expansion dryer is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119022588A_ABST
    Figure CN119022588A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of expansion drying machines, and provides a machine barrel for drying a high polymer material and an expansion drying machine, the machine barrel comprises a barrel body and a heating jacket block, at least three grooves are formed in the outer surface of the barrel body around the axis of the barrel body at equal arc distances, and the length direction of the grooves is the same as the length direction of the barrel body; the number of the heating jacket blocks is the same as that of the grooves, each heating jacket block is installed in the corresponding groove, a high-temperature steam inlet and a high-temperature steam outlet are formed in each heating jacket block, a first anti-corrosion layer is arranged on the inner surface of the barrel, and a second anti-corrosion layer is arranged on the outer surface of the barrel. And a second anti-corrosion layer is arranged on the outer surface of the cylinder body. A plurality of independent heating jacket blocks are arranged, so that the heating uniformity is ensured, the disassembly is convenient, and the replacement cost is reduced; and by arranging the first anti-corrosion layer and the second anti-corrosion layer, the chlorine corrosion resistance of the barrel is improved, it can be effectively guaranteed that the barrel cannot crack, and therefore the service life of the expansion drying machine is guaranteed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the technical field of expansion dryers, and more specifically, relates to a barrel for drying polymer materials and an expansion dryer. Background Art

[0002] The expansion dryer is one of the key units for post-processing of synthetic rubber. The screw of the expansion dryer is driven by the main motor through a hydraulic coupling and a gearbox, and rotates at a speed of 120 to 350 revolutions per minute. The material from the extrusion dehydrator is continuously added to the hopper and squeezed into the barrel by the continuous spiral blade. In the first compression stage, the material is pushed forward while the extrusion force it is subjected to is getting greater and greater. The four rows of shear screws installed around the machine body increase the friction force on the material and provide friction heat, so that the rubber is gradually heated. A part of the water is squeezed out of the material and discharged from the machine body through the dehydration screen plate. As the material moves forward and the steam jacket of the expansion dryer is continuously heated, the material reaches the required temperature (150 to 190°C) and the required pressure (3 to 10MPa) before it reaches the die plate. When the overheated water and the material in the high temperature and high pressure state are squeezed out of the die head, the pressure suddenly drops to normal pressure, and flash evaporation occurs. At this time, the over-mature water in the rubber immediately vaporizes and escapes from the material, thereby achieving the purpose of drying.

[0003] The barrel of the expansion dryer works in a corrosive medium containing chloride ions for a long time. The presence of chloride ions destroys the protective film on the surface of austenitic stainless steel, causing stress corrosion on the barrel and cracking of the barrel, which seriously affects the normal operation and life of the expansion dryer and also has a serious impact on the normal operation of the entire device.

[0004] In actual work, the integrated heating jacket on the cylinder has cracked many times. Although the cracks were repaired by melting welding, the problem was still not fundamentally solved. Therefore, the cause of the cracking of the heating jacket in the expansion dryer was analyzed. After analyzing the corrosion products on the crack surface, a large amount of chloride ions were detected, indicating that the large amount of chloride ions contained in the process water is related to the cracking of the heating jacket. The heating jacket has been working in a corrosive medium containing chloride ions for a long time, and the presence of chloride ions destroys a protective film on the surface of austenitic stainless steel, thereby causing stress corrosion to the heating jacket.

[0005] Meanwhile, the existing integrated heating jacket on the cylinder generally has only one steam inlet and one steam outlet, so heating takes a lot of time, and the heating temperature distribution is uneven, and once the heating jacket needs to be replaced, the replacement cost is high. Summary of the invention

[0006] The purpose of the embodiments of the present application is to provide a barrel for drying polymer materials, so as to solve the technical problems in the prior art that chloride ion corrosion seriously affects the service life of the barrel and the replacement cost of the heating jacket is high.

[0007] To achieve the above-mentioned purpose, the technical solution adopted in the present application is: to provide a barrel for drying polymer materials, including a barrel and a heating jacket block, the outer surface of the barrel is provided with at least three grooves at equal arc distances around its axis, the length direction of the grooves is the same as the length direction of the barrel, the number of the heating jacket blocks is the same as the number of the grooves, one heating jacket block is installed in each of the grooves, each of the heating jacket blocks is provided with a high-temperature steam inlet and a high-temperature steam outlet, the inner surface of the barrel is provided with a first anti-corrosion layer, and the outer surface of the barrel is provided with a second anti-corrosion layer.

[0008] In one embodiment, the first anti-corrosion layer is a cobalt-based coating.

[0009] In one embodiment, the second anti-corrosion layer is a tungsten carbide and nickel-cobalt coating.

[0010] In one embodiment, the surface treatment roughness Sa of the cobalt-based coating reaches level 2.5; the thickness of the cobalt-based coating is greater than 1 mm; and the hardness HV of the cobalt-based coating is greater than 850.

[0011] In one embodiment, the surface treatment roughness Sa of the tungsten carbide and nickel-cobalt coatings reaches level 2.5; the thickness of the tungsten carbide and nickel-cobalt coatings is 0.1-0.3 mm; and the hardness HV of the tungsten carbide and nickel-cobalt coatings is greater than 800.

[0012] In one embodiment, four heating jacket blocks are arranged at equal arc distances.

[0013] In one embodiment, the length of the cylinder is 1.2m-1.31m, the inner diameter of the cylinder is 0.295m-0.330m, and the outer diameter of the cylinder is 0.400m-0.420m.

[0014] In one embodiment, flanges are provided at both ends of the cylinder, and the flanges are connected to the cylinder by solution treatment.

[0015] In one embodiment, the cylinder is made of UNS N08020 alloy material.

[0016] Another object of the present application is to provide an expansion dryer, comprising the barrel for drying polymer materials as described above.

[0017] The beneficial effects of the barrel for drying polymer materials and the expansion dryer provided in the present application are: a plurality of independent heating jacket blocks are provided, which can ensure heating uniformity and facilitate disassembly, thereby reducing replacement costs; and each heating jacket block is provided with a high-temperature steam inlet and a high-temperature steam outlet, which can effectively reduce the pressure stress at the outlet and prevent cracking; by providing a first anti-corrosion layer and a second anti-corrosion layer, the chlorine corrosion resistance of the barrel is increased, which can effectively ensure that the barrel will not crack, thereby ensuring the service life of the expansion dryer. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0019] Figure 1 A schematic diagram of the cross-sectional structure of a barrel axis for drying polymer materials provided in an embodiment of the present application;

[0020] Figure 2 This is a schematic diagram of the radial cross-sectional structure of a barrel for drying polymer materials provided in an embodiment of the present application.

[0021] Among them, the reference numerals in the figure are:

[0022] 1. Cylinder; 11. First anti-corrosion layer; 12. Second anti-corrosion layer; 2. Heating jacket block; 21. High-temperature steam inlet; 22. High-temperature steam outlet; 3. Flange. DETAILED DESCRIPTION

[0023] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0024] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.

[0025] It should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0026] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0027] Please also read Figure 1 and Figure 2 , a barrel for drying polymer materials provided in an embodiment of the present application is now described in detail. In this embodiment, the barrel comprises a barrel body 1 and a heating jacket block 2 having an inner cavity, the outer surface of the barrel body 1 is provided with at least three grooves at equal arc distances around its axis, the length direction of the grooves is the same as the length direction of the barrel body 1, the number of the heating jacket blocks 2 is the same as the number of the grooves, a heating jacket block 2 is installed in each groove, and the heating jacket block 2 is detachably installed, which is convenient for subsequent replacement; the length direction of the plurality of heating jacket blocks 2 is the same as the length direction of the barrel body 1 and is evenly distributed around the barrel body 1, so as to ensure the uniformity of heating.

[0028] Each heating jacket block 2 is provided with a high-temperature steam inlet 21 and a high-temperature steam outlet 22. Therefore, each heating jacket block 2 is an independent individual. When cracks appear in one of the heating jacket blocks 2, only the heating jacket block 2 with cracks needs to be replaced, thereby reducing the replacement cost. Each heating jacket block 2 is provided with a high-temperature steam inlet 21 and a high-temperature steam outlet 22. Compared with the prior art in which the cylinder 1 adopts an integrated heating jacket, the pressure stress at the high-temperature steam outlet 22 can be effectively reduced to prevent cracking. In this embodiment, the inner surface of the cylinder 1 is provided with a first anti-corrosion layer 11, and the outer surface of the cylinder 1 is provided with a second anti-corrosion layer 12. By providing the first anti-corrosion layer 11 and the second anti-corrosion layer 12, the chlorine corrosion resistance of the cylinder 1 is increased, and the cylinder 1 can be effectively guaranteed not to crack, and chloride ions can be prevented from corroding the heating jacket block 2, thereby ensuring the service life of the expansion dryer.

[0029] Preferably, the first anti-corrosion layer 11 is a cobalt-based coating, which has excellent wear resistance, heat resistance and chloride ion corrosion resistance, thereby ensuring that the cylinder 1 does not crack.

[0030] Preferably, the second anti-corrosion layer 12 is a tungsten carbide and nickel-cobalt coating, which has excellent properties such as high melting point, high hardness, high wear resistance, and high corrosion resistance, and can directly contact the heating jacket block 2 without being damaged.

[0031] Specifically, the surface treatment roughness Sa of the cobalt-based coating reaches level 2.5; the thickness of the cobalt-based coating is greater than 1 mm; and the hardness HV of the cobalt-based coating is greater than 850.

[0032] Specifically, the surface treatment roughness Sa of the tungsten carbide and nickel-cobalt coatings reaches level 2.5; the thickness of the tungsten carbide and nickel-cobalt coatings is 0.1-0.3 mm, preferably 0.25 or 0.3 mm; the hardness HV of the tungsten carbide and nickel-cobalt coatings is greater than 800.

[0033] In this embodiment, four heating jacket blocks 2 are arranged at equal arc distances. In other embodiments, the number of heating jacket blocks 2 is five, six or seven, and the specific number is selected according to actual needs.

[0034] In this embodiment, the length of the barrel 1 is 1.2m-1.31m, the inner diameter of the barrel 1 is 0.295m-0.330m, and the outer diameter of the barrel 1 is 0.400m-0.420m. By providing a plurality of heating jacket blocks 2, the size of the barrel 1 in the prior art can be improved, such as increasing the inner diameter and the length of the barrel 1, so that the feed volume is increased, and the outer diameter is reduced, which can increase the heating speed.

[0035] In this embodiment, flanges 3 are provided at both ends of the cylinder 1, and the flanges 3 are connected to the cylinder 1 by solid solution treatment. This is to eliminate welding stress and unify the organizational structure of the welding point.

[0036] In this embodiment, the cylinder 1 is made of UNS N08020 alloy material, so that the cylinder 1 can be used in a chloride ion environment with a temperature lower than 540° C., ensuring the normal use of the cylinder 1.

[0037] This embodiment also provides an expansion dryer, including the barrel for drying polymer materials as described above. The expansion dryer also includes conventional structures such as a main motor, a coupling, a reduction gearbox, and a screw, which will not be described in detail here.

[0038] In a specific implementation of this embodiment, the inner diameter of the barrel is 0.320m, the outer diameter is 0.400m, the length of the barrel is 1.302m, and four heating jacket blocks are provided; the advantages and disadvantages of the barrel of this size are compared with the barrel of the prior art using an integrated heating jacket, and the comparison results are shown in Table 1:

[0039]

[0040] In another specific implementation of this embodiment, the inner diameter of the barrel is 0.330m, the outer diameter is 0.395m, the length of the barrel is 1.310m, and four heating jacket blocks are provided; the advantages and disadvantages of the barrel of this size are compared with the barrel of the prior art using an integrated heating jacket, and the comparison results are shown in Table 2:

[0041]

[0042] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present application should be included in the protection scope of the present application.

Claims

1. A barrel for drying polymer materials, It is characterized in that The invention comprises a cylinder (1) and a heating jacket block (2), wherein the outer surface of the cylinder (1) is provided with at least three grooves at equal arc distances around its axis, the length direction of the grooves is the same as the length direction of the cylinder (1), the number of the heating jacket blocks (2) is the same as the number of the grooves, one heating jacket block (2) is installed in each of the grooves, each of the heating jacket blocks (2) is provided with a high-temperature steam inlet (21) and a high-temperature steam outlet (22), the inner surface of the cylinder (1) is provided with a first anti-corrosion layer (11), and the outer surface of the cylinder (1) is provided with a second anti-corrosion layer (12).

2. The barrel for drying polymer materials according to claim 1, Features: The first anti-corrosion layer (11) is a cobalt-based coating.

3. The barrel for drying polymer materials according to claim 1, Features: The second anti-corrosion layer (12) is a tungsten carbide and nickel-cobalt coating.

4. The barrel for drying polymer materials as claimed in claim 2, Features: The surface treatment roughness Sa of the cobalt-based coating reaches level 2.5; the thickness of the cobalt-based coating is greater than 1 mm; and the hardness HV of the cobalt-based coating is greater than 850.

5. The barrel for drying polymer materials as claimed in claim 3, Features: The surface treatment roughness Sa of the tungsten carbide and nickel-cobalt coatings reaches level 2.5; the thickness of the tungsten carbide and nickel-cobalt coatings is 0.1-0.3 mm; the hardness HV of the tungsten carbide and nickel-cobalt coatings is greater than 800.

6. The barrel for drying polymer materials according to any one of claims 1 to 5, Features: Four heating jacket blocks (2) are arranged at equal arc distances.

7. The barrel for drying polymer materials according to any one of claims 1 to 5, Features: The length of the cylinder (1) is 1.2m-1.31m, the inner diameter of the cylinder (1) is 0.295m-0.330m, and the outer diameter of the cylinder (1) is 0.400m-0.420m.

8. The barrel for drying polymer materials according to any one of claims 1 to 5, Features: Flanges (3) are provided at both ends of the cylinder (1), and the flanges (3) are connected to the cylinder (1) by solution treatment.

9. The barrel for drying polymer materials according to any one of claims 1 to 5, Features: The cylinder (1) is made of UNS N08020 alloy material.

10. An expansion dryer, It is characterized in that It comprises a barrel for drying polymer materials as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Jacket and heat preservation device thereof

    CN116066653A

  • A novel cooling jacket subassembly for freeze dryer

    CN206056128U

  • Water delivery pipe fitting with cavity intermediate layer

    CN206487944U

  • Temperature control device of plastic extruding machine

    CN209832553U

  • Manufacture of barrel with jacket

    JP1994322412A