Wafer processing method
By forming a convex ring structure on the edge of the second surface of the wafer and applying a viscous material to a specific area of the protective film, the problem of difficulty in perfect fit in the traditional film method is solved, tight fit and simplified removal steps are achieved, and crystallization is improved Mechanical strength and yield of the circle.
Patent Information
- Application Number
- CN202411131785.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-26
AI Technical Summary
During wafer processing, the convex ring structure makes it difficult for traditional film stickers to fit perfectly, resulting in bubbles, increasing the risk of breakage or fragmentation when tearing the film, and affecting the yield rate.
The convex ring structure is formed on the edge of the second surface of the wafer, and the adhesive material is applied to the second area of the protective film. The protective film is gradually applied by releasing it along the radial region of the protective film to ensure a tight fit and reduce the Air bubbles are formed and the convex ring structure and protective film are uniformly removed in subsequent steps.
It significantly enhances the mechanical strength of the wafer, reduces the risk of crushing, ensures reliable coating of the protective film, simplifies processing steps, reduces production costs and damage risks, and improves the yield rate.
Smart Images

Figure CN119028808A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a wafer processing method. Background Art
[0002] In the field of semiconductor manufacturing, with the continuous advancement of technology, wafers are becoming thinner and thinner to meet the design requirements of high performance and low power consumption. However, this trend also brings a significant problem: during the transfer, handling and processing of wafers, the fragility of wafers increases significantly, and they are prone to breakage or damage. In order to meet this challenge, the industry generally adopts the Taiko process, which is to add a convex ring structure (also called a ring) on the edge of the wafer to improve the strength of the wafer.
[0003] In addition, during wafer processing, especially when it comes to single-sided plating and other processes, how to prevent the non-plated surface (i.e. the back of the wafer where the convex ring structure is located) from being plated and causing interlayer separation (peeling) of the wafer has become a key issue. For this reason, the industry usually applies a protective film on the back of the wafer. This protective film can not only prevent the non-plated surface from being corroded by the chemical plating solution, but also reduce the risk of mechanical damage to a certain extent.
[0004] However, due to the presence of the convex ring structure, traditional film lamination methods often have difficulty achieving perfect lamination inside the convex ring, resulting in the generation of bubbles. These bubbles can become potential hidden dangers in subsequent process steps. Especially during the film tearing process, due to the lack of sufficient adhesion at the bubble, the tearing force may not be evenly distributed on the entire back of the wafer. This will cause the wafer to be subjected to uneven stress at the bubble, thereby increasing the risk of breakage or fragmentation, seriously affecting the wafer yield. Summary of the invention
[0005] The technical problem solved by the present invention is how to improve the yield rate of wafers.
[0006] To solve the above technical problems, an embodiment of the present invention provides a wafer processing method, which includes: providing a wafer, wherein the wafer has a first surface and a second surface relative to each other; grinding the second surface to form a convex ring structure on the edge of the second surface; applying a protective film on the second surface, wherein the protective film is adsorbed on the second surface and is adhesively connected to the convex ring structure; performing at least one processing step on the first surface; and removing the protective film.
[0007] Optionally, the side of the protective film facing the second surface includes a first area and a second area, the second area is closer to the edge of the protective film than the first area, the second area corresponds to the convex ring structure, and the second area is coated with an adhesive material.
[0008] Optionally, the size of the second area is adjustable.
[0009] Optionally, the adhesive material is selected from: acrylic, polyurethane and epoxy resin.
[0010] Optionally, removing the protective film includes: cutting off the convex ring structure and a portion of the protective film attached to the convex ring structure; and removing a remaining portion of the protective film.
[0011] The cutting off of the convex ring structure and the portion of the protective film attached to the convex ring structure is achieved by a ring cutting process.
[0012] Optionally, the protective film is seamlessly bonded to the second surface.
[0013] Optionally, the material of the protective film is selected from: propylene oxide, polyethylene, polypropylene, polyester and silicone; and / or the protective film is a UV film.
[0014] Optionally, laminating the protective film on the second surface includes: adsorbing the protective film on an adsorption plate; moving the adsorption plate above the second surface; and releasing the protective film in radial regions along the protective film so that the protective film is gradually laminating on the second surface.
[0015] Optionally, the adsorption plate is provided with a plurality of pores, and the arrangement and shape of the plurality of pores satisfy at least one of the following: the plurality of pores are arranged in an array; the plurality of pores are evenly distributed on the adsorption plate; the plurality of pores have the same size.
[0016] Optionally, adsorbing the protective film on the adsorption plate includes: adsorbing the protective film on the adsorption plate by extracting air from at least a portion of the plurality of pores.
[0017] Optionally, releasing the protective film in regions along the radial direction of the protective film comprises: stopping the extraction of air from the pores one by one or row by row along the radial direction to release the protective film in regions.
[0018] Compared with the prior art, the technical solution of the embodiment of the present invention has the following beneficial effects:
[0019] By adopting the technical solution of the present application, a convex ring structure is formed in the edge area of the second surface of the wafer, which significantly enhances the mechanical strength of the wafer. This makes the wafer more stable during subsequent transfer, handling and processing, and reduces the risk of breakage due to external forces. The convex ring structure provides additional support for the wafer, making the wafer more resilient when facing various process challenges. Furthermore, the adhesive material is only applied to the area where the protective film and the convex ring structure are in contact. On the one hand, it can ensure that the protective film is reliably attached to the second surface to avoid the protective film accidentally falling off from the second surface when the wafer is moved during subsequent processing steps. On the other hand, since most of the second surface (i.e., the area within the convex ring structure) is simply vacuum adsorbed to the protective film, the risk of damage to the wafer during the subsequent film tearing process is also reduced.
[0020] Furthermore, the protective film is attached by releasing the protective film in different regions along the radial direction of the protective film, which can effectively avoid the generation of bubbles. This method ensures that each region (especially at the convex ring structure) can be closely attached by gradually attaching each region of the protective film to the second surface of the wafer, thereby reducing the possibility of bubble formation.
[0021] Furthermore, after the subsequent process is completed on the first side of the wafer, the method removes the convex ring structure and the protective film through a unified step, that is, only one process is required to remove the convex ring structure and the protective film at the same time. This processing method simplifies the processing steps and reduces production costs and time costs. At the same time, since the convex ring structure and the protective film are removed in the same step, the risk of wafer damage caused by multiple processing is also reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 is a flow chart of a wafer processing method according to an embodiment of the present invention;
[0023] Figure 2 yes Figure 1 A flowchart of an implementation of step S15;
[0024] Figure 3 Yes Execution Figure 1 Schematic diagram of the device obtained in step S12;
[0025] Figure 4 yes Figure 3 Cross-sectional view along AA direction;
[0026] Figure 5 is a schematic diagram of a protective film according to an embodiment of the present invention;
[0027] Figure 6 is a schematic diagram of an adsorption plate according to an embodiment of the present invention;
[0028] Figure 7 yes Figure 6 Schematic diagram of the adsorption plate releasing the protective film;
[0029] Figure 8 Yes Execution Figure 1 The schematic diagram of the device obtained in step S13;
[0030] Fig. 9 Yes Execution Figure 2 The device schematic diagram obtained in step S151;
[0031] Fig.10 Yes Execution Figure 2 Schematic diagram of the device obtained in step S152. DETAILED DESCRIPTION
[0032] As mentioned in the background technology, in the prior art, the wafer becomes thinner and becomes fragile during processing. Although the strength is improved by adding a convex ring structure through the Taiko process, the convex ring structure makes it difficult for the traditional film bonding method to perfectly bond on the back of the wafer, resulting in bubbles and increasing the risk of wafer breakage or fragmentation when the film is torn off. In addition, in the prior art, a viscous material is usually coated on the entire surface of the protective film used to bond the wafer, which makes it easy for the viscous material to remain on the surface of the wafer during the subsequent removal of the protective film, or the viscous force is too large to damage the wafer, seriously affecting the wafer yield.
[0033] To solve the above technical problems, an embodiment of the present invention provides a wafer processing method, which includes: providing a wafer, wherein the wafer has a first surface and a second surface relative to each other; grinding the second surface to form a convex ring structure on the edge of the second surface; applying a protective film on the second surface, wherein the protective film is adsorbed on the second surface and is adhesively connected to the convex ring structure; performing at least one processing step on the first surface; and removing the protective film.
[0034] By adopting the technical solution of the present application, a convex ring structure is formed in the edge area of the second surface of the wafer, which significantly enhances the mechanical strength of the wafer. This makes the wafer more stable during subsequent transfer, handling and processing, and reduces the risk of breakage due to external forces. The convex ring structure provides additional support for the wafer, making the wafer more resilient when facing various process challenges. Furthermore, the adhesive material is only applied to the area where the protective film and the convex ring structure are in contact. On the one hand, it can ensure that the protective film is reliably attached to the second surface to avoid the protective film accidentally falling off from the second surface when the wafer is moved during subsequent processing steps. On the other hand, since most of the second surface (i.e., the area within the convex ring structure) is simply vacuum adsorbed to the protective film, the risk of damage to the wafer during the subsequent film tearing process is also reduced.
[0035] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0036] Figure 1 It is a flow chart of a wafer processing method according to an embodiment of the present invention.
[0037] refer to Figure 1 , the wafer processing method comprises:
[0038] Step S11, providing a wafer, wherein the wafer has a first surface and a second surface opposite to each other;
[0039] Step S12, grinding the second surface to form a convex ring structure at the edge of the second surface;
[0040] Step S13, applying a protective film on the second surface, wherein the protective film is adsorbed on the second surface and is adhesively connected to the convex ring structure;
[0041] Step S14, performing at least one processing step on the first surface;
[0042] Step S15, removing the protective film.
[0043] Specifically, a wafer is a basic component in the field of semiconductor manufacturing. It is a specially processed circular thin sheet, usually made of silicon (Si) or other semiconductor materials. By performing different processes on the wafer, semiconductor devices with different functions and sizes can be produced.
[0044] Combination Figure 3 and Figure 4 , the wafer 1 has a first surface 11 and a second surface 12 relative to each other, and these two surfaces will be subjected to different treatments and processing in the subsequent manufacturing process. Among them, the first surface 11 can be used as the front side of the wafer 1, and various functional layers or functional devices are usually formed on the first surface 11 by processes such as photolithography, etching, ion implantation, and metallization. The second surface 12 can be used as the back side of the wafer 1. Usually, no complex circuit processing will be performed on the second surface 12, but a series of specific treatments will be performed to meet the requirements of packaging, heat dissipation or mechanical support. For example, in the manufacturing process of the wafer 1, the second surface 12 can be further processed by the back thinning process to reduce the thickness of the entire wafer 1, which not only helps to improve the heat dissipation efficiency of the chip supported subsequently, but also meets the requirements of specific packaging forms (such as thin packaging). After the second surface 12 is thinned, it can also be further subjected to surface roughening treatment (Backside Roughening) to increase the adhesion between the chip and the substrate during packaging and prevent the chip from falling off during the packaging process.
[0045] In addition, in order to enhance the mechanical strength of the wafer and prevent breakage during subsequent processing or transportation, the second surface 12 may also be coated with a protective coating (such as a polymer coating or a metal coating), thereby not only providing additional mechanical support but also preventing chemical corrosion and physical damage to a certain extent.
[0046] For another example, in some special applications, such as the manufacture of power semiconductor devices, the second surface 12 can also be metallized to form a heat sink or directly used as an electrode. Such metallization treatment generally involves depositing a layer of metal material with high thermal conductivity (such as copper, aluminum or their alloys) on the second surface 12 of the wafer 1, and forming the required pattern and thickness through specific process steps (such as electroplating, sputtering, etc.).
[0047] Combination Figure 3 and Figure 4 After step S12 is completed, a convex ring structure 121 is formed on the edge of the second surface 12 to enhance the overall structural strength and toughness of the wafer 1, thereby avoiding accidents such as curling, warping, or even breakage during subsequent handling and transfer, which would affect the wafer yield.
[0048] In some embodiments, the grinding process used for the second surface 12 may be, for example, Taiko Grinding. Taiko Grinding is a key process in semiconductor manufacturing and can be used to produce and process ultra-thin wafers. Through Taiko Grinding, the second surface 12 of the wafer 1 forms a circle of raised edges, that is, a convex ring structure 121. Thus, through the convex ring structure 121, the edge strength of the wafer 1 can be effectively enhanced to prevent the ultra-thin wafer 1 from being easily broken during processing and transportation. Furthermore, the convex ring structure 121 can support the edge of the wafer 1 to prevent the wafer 1 from warping due to uneven internal stress after thinning. In addition, in the subsequent processing flow, the convex ring structure 121 can also be used as a reference for positioning and fixing the wafer 1 to improve production efficiency and yield.
[0049] In a typical application scenario, the grinding process for the second surface 12 of the wafer 1 may include the following steps:
[0050] First, before formally performing Taiko grinding, the second surface 12 of the wafer 1 may be pre-thinned to a certain extent to reduce the difficulty and time of subsequent grinding.
[0051] Then, select appropriate grinding equipment and grinding media (such as grinding wheels, grinding fluid, etc.) to ensure grinding accuracy and efficiency.
[0052] Furthermore, the wafer 1 is fixed on a grinding device, and the second surface 12 is ground by controlling the parameters of the grinding device (such as pressure, rotation speed, grinding time, etc.). During the grinding process, the grinding medium will gradually remove part of the material of the wafer 1 close to the second surface 12, and at the edge of the wafer 1, due to the special design of the grinding device or the control of the grinding parameters, a circle of raised edges, namely the convex ring structure 121, will be formed.
[0053] Further, combined with Figures 3 to 5 , a protective film 2 is applied to the second surface 12 to prevent the second surface 12 from being damaged by corrosive chemicals, high temperature treatment or mechanical stress when a series of fine processing steps (such as photolithography, etching, ion implantation and chemical plating) are performed on the first surface 11 of the wafer 1. In addition, the protective film 2 can also avoid the risk of cross contamination between different process steps during the processing of the wafer 1. For example, impurities or residues on the second surface 12 may be transferred to the first surface 11 during the processing of the first surface 11, affecting product quality.
[0054] Furthermore, the side of the protective film 2 facing the second surface 12 includes a first area 21 and a second area 22, the second area 22 is closer to the edge of the protective film 2 than the first area 21, the second area 22 corresponds to the convex ring structure 121, and the second area 22 is coated with an adhesive material. In other words, on the second surface 12, the convex ring structure 121 and the protective film 2 are adhesively connected, and the area other than the convex ring structure (i.e., the flat area) and the protective film 2 are vacuum adsorbed.
[0055] In a specific embodiment, when the protective film 2 is attached to the second surface 12, the protective film 2 must not only be tightly adsorbed on the flat area of the second surface 12, but also needs to achieve a stable adhesive connection with the convex ring structure 121 to avoid accidental detachment of the protective film in subsequent processes. At the same time, the adhesive material is only coated on the second area 22, and the first area 21 is only attached to the flat area on the second surface 12 by vacuum adsorption. In this way, the risk of the wafer being torn and damaged when the protective film 2 is removed can be reduced. Experiments show that if the protective film 2 is fully coated with glue and the viscosity is too strong, the surface of the wafer 1 may be damaged when the protective film 2 is torn off, especially when the wafer 1 is very thin or has been processed many times to become fragile. The degree of damage and the probability of damage are greatly increased. Therefore, this embodiment only coats the adhesive material on the second area 22 of the protective film 2, which can reduce the direct force on the surface of the wafer 1 when the protective film 2 is torn off while maintaining sufficient connection strength, thereby reducing the risk of damage.
[0056] In some embodiments, the size of the second area 22 is adjustable. For example, the size of the second area 22 can be adjusted according to the size of the wafer 1. For a wafer 1 with a smaller diameter, the width of the second area 22 coated with the adhesive material along the radial direction of the wafer may be narrower; while for a wafer with a larger diameter, in order to ensure sufficient protection and a stable connection, the second area 22 coated with the adhesive material may need to be widened accordingly.
[0057] In some embodiments, the area of the second region 22 may also be smaller than the surface area of the convex ring structure 121. Thus, when the protective film 2 is attached to the second surface 12, the viscous material coated on the second region 22 is prevented from being squeezed and flowing to the area (i.e., the flat area) other than the convex ring structure 121, thereby wasting the material of the wafer 1 and reducing production efficiency.
[0058] In some embodiments, the material of the protective film 2 can be selected from: propylene oxide, polyethylene, polypropylene, polyester and silicone. As a result, the protective film 2 made of the above materials can have a certain elasticity and deformation ability, and can fit tightly to the complex shape of the second surface 12 of the wafer 1. Whether it is a flat area or a raised convex ring structure 121, the protective film 2 can achieve good fitting through its elastic deformation, thereby avoiding gaps or peeling during the movement or processing of the wafer 1. In addition, the above materials show good chemical stability under common processing conditions for the wafer 1, and will not react with the surface of the wafer 1 or the processing liquid, thereby protecting the wafer 1 from chemical corrosion or contamination. In addition, the protective film 2 made of the above materials can be easily and cleanly removed after completing the task, without leaving any residue or substances that affect the subsequent processing of the wafer 1. This helps to maintain the cleanliness of the surface of the wafer 1 and provides a good foundation for subsequent steps such as packaging and testing.
[0059] In some embodiments, the protective film 2 may also be a UV film (Ultraviolet Film), which can facilitate procurement and processing and reduce the production cost of the wafer 1.
[0060] In some embodiments, the adhesive material can be selected from materials such as acrylic acid, polyurethane, and epoxy resin. The above materials can form a strong chemical or physical bonding force with the bonded surface (i.e., the second region 22 of the protective film 2 and the surface of the convex ring structure 121), ensuring the firmness and durability of the bonding. In addition, the above materials also have certain weather resistance and chemical corrosion resistance, and can maintain stable performance under different environmental conditions. As a result, the yield rate of the wafer 1 can be further improved.
[0061] In some embodiments, step S13, i.e., a way to implement the step of attaching the protective film 2 to the second surface 12, may be: adsorbing the protective film 2 on the adsorption plate 3; moving the adsorption plate 3 to the top of the second surface 12; and releasing the protective film 2 in radial regions of the protective film 2, so that the protective film 2 is gradually attached to the second surface 12. Thus, it is possible to ensure that the protective film 2 can be evenly, bubble-free, and accurately attached to the second surface 12, thereby improving the protection effect and production efficiency of the wafer 1.
[0062] Specifically, adsorbing the protective film 2 onto the adsorption plate 3 is a preparatory stage of the laminating process. By adsorbing the surface of the protective film 2 not coated with the adhesive material by the adsorption plate 3, stable control of the protective film 2 can be achieved. The adsorption plate 3 usually has an adsorption material or structure compatible with the surface of the protective film 2, which can ensure that the protective film 2 will not fall off or wrinkle during the movement.
[0063] Furthermore, after the protective film 2 is stably adsorbed on the adsorption plate 3 , the entire adsorption plate 3 and the protective film 2 are moved above the second surface 12 of the wafer 1 , and the second area 22 is aligned with the convex ring structure 121 .
[0064] Furthermore, by releasing the protective film 2 in different regions along the radial direction of the protective film 2, it is ensured that the protective film 2 can be gradually and evenly attached to the second surface 12 of the wafer 1. When releasing each region, the partial protective film 2 in the region is separated from the adsorption plate 3 and attached to the second surface 12 by controlling the adsorption force of the adsorption plate 3 or applying external pressure. In this way, the gap and bubbles between the protective film 2 and the second surface 12 can be gradually reduced, and finally complete attachment can be achieved.
[0065] In some embodiments, the release of the protective film 2 in different regions along the radial direction of the protective film 2 may be, for example, first releasing one end of the protective film 2 and then gradually releasing it to the other end along the radial direction, or, for example, first releasing the central region of the protective film and then gradually releasing it to the edge.
[0066] In some embodiments, the process of attaching the protective film 2 to the second surface 12 can be performed in a vacuum environment. As a result, as the protective film 2 is released, the protective film 2 is gradually vacuum-absorbed on the second surface 12, which can effectively avoid the generation of bubbles during the film attaching process, which is conducive to further improving the yield rate of the wafer 1.
[0067] In some embodiments, reference Figure 6, the adsorption plate is provided with a plurality of pores 31, and the arrangement and shape of the plurality of pores 31 satisfy at least one of the following: the plurality of pores 31 are arranged in an array; the plurality of pores 31 are evenly distributed on the adsorption plate 3; the plurality of pores 31 have the same size. In this scenario, the protective film 2 can be adsorbed to the adsorption plate 3 by exhausting air from at least a portion of the plurality of pores 31.
[0068] Further, the release process of the protective film 2 can be as follows Figure 7 As shown, the air is sucked out from the air holes 31 one by one or in rows along the radial direction to release the protective film 2 in different regions.
[0069] Further, refer to Figure 8 After the protective film 2 is completely released and attached to the second surface 12, the protective film is seamlessly attached to the second surface 12. In other words, the tortuous shape of the protective film 2 is consistent with the surface morphology of the second surface 12. Thus, the protective film 2 is seamlessly attached to the second surface 12 of the wafer 1, which can avoid the generation of tiny bubbles or wrinkles between the protective film 2 and the second surface 12, resulting in the performance degradation or even damage of the subsequently manufactured device.
[0070] Furthermore, after the protective film 2 is completely attached to the second surface 12, at least one processing step is performed on the first surface 11. The processing step may be, for example, photolithography, etching, ion implantation, metallization, etc., for preparing a semiconductor device with a desired function, such as a MOS device, on the first surface 11.
[0071] In some embodiments, reference Figure 2 , the implementation of step S15 may include, for example:
[0072] Step S151, cutting off the convex ring structure and the portion of the protective film that is attached to the convex ring structure;
[0073] Step S152, removing the remaining portion of the protective film.
[0074] Further, the structure of the device after step S151 is completed can refer to Fig. 9 shown.
[0075] In some embodiments, the portion of the wafer 1 forming the convex ring structure can be removed by a ring cutting process. The ring cutting process usually uses high-precision cutting equipment, such as a laser cutter, a diamond wire saw or a water jet, to cut along the edge of the convex ring structure 121 on the wafer 1 close to the flat area. By precisely controlling the depth and width of the cutting, it is ensured that only the convex ring structure 121 is removed without damaging the flat area of the wafer 1.
[0076] Furthermore, since the second region 22 of the protective film 2 bonded to the convex ring structure 121 is also removed when the convex ring structure 121 is cut off, the protective film 2 can be removed without an additional debonding step, which is conducive to simplifying the process and improving production efficiency.
[0077] Furthermore, since there is no adhesive material between the first area 21 of the protective film 2 and the wafer 1, the first area 21 of the protective film 2 is simply adsorbed on the wafer 1 by vacuum adsorption. Therefore, when the second area 22 is removed together with the convex ring structure 121, the first area 21 of the protective film 2 can also be easily removed from the wafer 1. No complicated tearing operation is required, which reduces the risk of damage to the wafer 1 and improves the yield of the wafer 1.
[0078] The structure of the wafer 1 after step S152 is completed can be referred to Fig.10 .
[0079] From the above, by adopting the technical solution of the present application, the mechanical strength of the wafer 1 is significantly enhanced by forming a convex ring structure 121 in the edge area of the second surface 12 of the wafer 1. This makes the wafer 1 more stable during subsequent transfer, handling and processing, and reduces the risk of breakage due to external forces. The convex ring structure 121 provides additional support for the wafer 1, making the wafer 1 more resilient when facing various process challenges. Furthermore, the adhesive material is only applied to the area where the protective film 2 and the convex ring structure 121 are in contact. On the one hand, it can ensure that the protective film 2 is reliably attached to the second surface 12 to avoid the protective film 2 accidentally falling off from the second surface 12 when the wafer 1 is moved during subsequent processing steps. On the other hand, since most of the area of the second surface 12 (i.e., the area located in the convex ring structure) is simply vacuum adsorbed with the protective film 2, the risk of damage to the wafer 1 during the subsequent film tearing process is also reduced.
[0080] Furthermore, the protective film 2 is attached by releasing the protective film 2 in different regions along the radial direction of the protective film 2, which can effectively avoid the generation of bubbles. This method ensures that each region (especially at the convex ring structure 121) can be closely attached by gradually attaching each region of the protective film 2 to the second surface 12 of the wafer 1, thereby reducing the possibility of bubble formation.
[0081] Furthermore, after the subsequent process is completed on the first side 11 of the wafer 1, the method removes the convex ring structure 121 and the protective film 2 through a unified step, that is, only one process is required to remove the convex ring structure and the protective film at the same time. This processing method simplifies the processing steps and reduces production costs and time costs. At the same time, since the convex ring structure 121 and the protective film 2 are removed in the same step, the risk of damage to the wafer 1 caused by multiple processing is also reduced.
[0082] It should be understood that the term "and / or" herein is merely an association relationship describing associated objects, indicating that three relationships may exist, for example, A and / or B, which may represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " herein indicates that the associated objects before and after are in an "or" relationship. As used herein, unless otherwise expressly stated, the term "or" covers all possible combinations unless it is not feasible. For example, if a component is stated to include A or B, then unless otherwise expressly stated or not feasible, the component may include A, or B, or A and B. As a second example, if a component is stated to include A, B, or C, then unless otherwise expressly stated or not feasible, the component may include A, or B, or C, or A and B, or A and C, or B and C, or A and B and C. The "multiple" appearing in the embodiments of the present application refers to two or more.
[0083] The relational terms appearing in the embodiments of the present application, such as first, second, etc., are only used to distinguish an entity or operation from another entity or operation, and do not require or imply any actual relationship or order between these entities or operations. In addition, the words "include", "have" and "comprise" and other similar forms are intended to be equivalent in meaning, and are open-ended, and one or more items behind any of these words are not meant to be an exhaustive list of such one or more items, or mean to be limited to one or more items listed. In the accompanying drawings and the specification, exemplary embodiments have been disclosed. However, many changes and modifications can be made to these embodiments. Therefore, although specific terms have been adopted, they are only used in a general and descriptive sense, not for the purpose of limitation.
[0084] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
[0085] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A wafer processing method, characterized in that: include: Providing a wafer having a first side and a second side opposite to each other; grinding the second surface to form a convex ring structure at an edge of the second surface; A protective film is attached to the second surface, wherein the protective film is adsorbed on the second surface and is adhesively connected to the convex ring structure; Perform at least one processing step on the first surface; The protective film is removed.
2. The method according to claim 1, characterized in that: The side of the protective film facing the second surface includes a first area and a second area, the second area is closer to the edge of the protective film than the first area, the second area corresponds to the convex ring structure, and the second area is coated with an adhesive material.
3. The method according to claim 2, characterized in that The size of the second area is adjustable.
4. The method according to claim 2, characterized in that: The adhesive material is selected from the group consisting of acrylic acid, polyurethane and epoxy resin.
5. The method according to claim 1, characterized in that The removing of the protective film comprises: Cutting off the convex ring structure and the portion of the protective film that is attached to the convex ring structure; The remaining portion of the protective film is removed.
6. The method according to claim 5, characterized in that The cutting off of the convex ring structure and the portion of the protective film attached to the convex ring structure is achieved by a ring cutting process.
7. The method according to claim 1, characterized in that The protective film is seamlessly attached to the second surface.
8. The method according to claim 1, characterized in that The material of the protective film is selected from: propylene oxide, polyethylene, polypropylene, polyester and silica gel; and / or the protective film is a UV film.
9. The method according to claim 1, characterized in that: The step of applying a protective film on the second surface comprises: Adsorbing the protective film onto an adsorption plate; Moving the adsorption plate to above the second surface; The protective film is released in sections along the radial direction of the protective film, so that the protective film is gradually attached to the second surface.
10. The method according to claim 9, characterized in that The adsorption plate is provided with a plurality of pores, and the arrangement and shape of the plurality of pores satisfy at least one of the following: Multiple air holes are arranged in an array; The plurality of pores are evenly distributed on the adsorption plate; The multiple air holes have the same size.
11. The method according to claim 10, characterized in that The step of adsorbing the protective film on the adsorption plate comprises: The protective film is adsorbed onto the adsorption plate by exhausting air from at least a portion of the plurality of air holes.
12. The method according to claim 10, characterized in that The step of releasing the protective film in different regions along the radial direction of the protective film comprises: The air extraction from the air holes is stopped one by one or row by row along the radial direction to release the protective film in different regions.