SiC transistor with firm short-circuit characteristic and preparation method thereof

By designing the P-zone wrapped around the bottom corner of the trench in the trench gate SiC MOSFET and forming a JFET structure, the problem of short-circuit withstand time of the device and easy breakdown of the oxidation layer at the bottom of the trench is solved, and a higher short-circuit withstand is achieved Time and device reliability.

CN119028823APending Publication Date: 2024-11-26YANGZHOU YANGJIE ELECTRONIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411384451.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-30
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The short-circuit withstand time of SiC MOSFET devices is relatively short, which is prone to failure of short-circuit breakdown, resulting in unstable system, and the corner gate oxide layer at the bottom of the trench is prone to breakdown, affecting device reliability.

Method used

In the trench gate SiC MOSFET, a P-zone wraps the bottom corner of the trench, forms a JFET structure to suppress short-circuit current, and extends the short-circuit withstand time through the combination of P-zone, N-zone and Pwell zone, and improves the short-circuit characteristics and use of the device. reliability.

Benefits of technology

It effectively extends the short-circuit withstand time of SiC MOSFET, improves the short-circuit characteristics and reliability of the device, and avoids the early breakdown failure of the corner gate oxide layer at the bottom of the channel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028823A_ABST
    Figure CN119028823A_ABST
Patent Text Reader

Abstract

The invention discloses a SiC transistor with a firm short-circuit characteristic and a preparation method thereof. Relates to the technical field of semiconductors. Comprising the following steps: S100, forming a SiC Drift layer on the top surface of a SiC Sub layer through epitaxial deposition, and injecting into the SiC Drift layer to form a layer of P region; s200, carrying out epitaxial deposition on the top surface of the SiC Drift layer to form an N region, sequentially forming a Pwell region and an NP region in the N region, and activating and forming an injection region through high-temperature ion annealing; s300, etching the top surface of the NP region downwards to form a groove; s400, forming a gate oxide layer in the groove; s500, forming a Poly layer in the groove in a polycrystalline silicon deposition mode; s600, forming an isolation dielectric layer on the top surfaces of the gate oxide layer and the Poly layer; s700, carrying out Ni metal sputtering on the top surface of the NP region and then carrying out rapid thermal annealing to form a front ohmic contact alloy layer; and S800, forming a front electrode metal layer on the uppermost part of the device through Ti and AlCu metal sputtering. According to the invention, advanced breakdown failure of the corner gate oxide layer at the bottom of the channel is avoided, and the use reliability of the device is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a SiC transistor with strong short-circuit characteristics and a preparation method thereof. Background Art

[0002] After decades of development, semiconductor materials have evolved from the first generation of traditional Si materials to the second generation of GaAs and InP, and even to the currently popular third generation materials SiC and GaN, all of which are moving towards achieving higher power levels with smaller chip areas, and increasing power density. Among them, SiC wide bandgap materials are the most prominent, with many physical performance advantages, such as large bandgap width, high critical breakdown electric field, small intrinsic carrier concentration, fast saturation drift velocity, high melting point, and high thermal conductivity. Therefore, SiC-based power devices have great advantages in the field of high voltage and high power, and have begun to be used on a large scale, such as SiC diodes and SiC MOSFET devices.

[0003] Although SiC MOSFET power devices have gradually replaced Si IGBT devices in the field of high voltage and high power, SiC MOSFET devices with smaller chip area and thickness also have certain risks in use, which is insufficient compared to Si IGBT. In SiIGBT devices, the short-circuit withstand time can usually reach about 10us, while SiC MOSFET devices, due to their greater power density, have a short-circuit withstand time of only about 3us, which puts more stringent requirements on the design of system circuits. If the design is improper, it is easy to cause the device to short-circuit and breakdown and fail, damaging the entire system. Therefore, improving the short-circuit characteristics is also a crucial part of the long-term safe and stable use of SiC MOSFET devices. Summary of the invention

[0004] In the trench gate SiC MOSFET device, the present invention designs P regions on both sides of the bottom corner of the trench, completely wraps the bottom corner in the P region to achieve protection of the corner, and avoids breakdown failure of the gate oxide layer at the bottom corner of the trench. At the same time, the P region, the N region and the Pwell region above form a JFET structure. When the device is short-circuited, the short-circuit current needs to flow through the JFET region to reach the other electrode, and the JFET region suppresses the short-circuit current, thereby extending the short-circuit tolerance time of the device and improving the short-circuit characteristics.

[0005] The technical solution of the present invention is: A method for preparing a SiC transistor with strong short-circuit characteristics comprises the following steps: S100, forming a SiC Drift layer on the top surface of the SiC Sub layer by epitaxial deposition, and implanting a P region into the SiC Drift layer; S200, epitaxially depositing an N region on the top surface of the SiC Drift layer, and sequentially forming a Pwell region and an NP region in the N region, and activating the implanted region by high temperature ion annealing; S300, etching downwards to form a groove on the top surface of the NP region; S400, forming a gate oxide layer in the trench; S500, forming a Poly layer inside the trench by depositing polysilicon; S600, forming an isolation dielectric layer on top of the gate oxide layer and the Poly layer; S700, forming a front ohmic contact alloy layer on the top surface of the NP region by Ni metal sputtering followed by rapid thermal annealing; S800, forming a front electrode metal layer on the top of the device by sputtering Ti and AlCu metals.

[0006] Specifically, in step S100, the doping concentration of the SiC Sub layer is 5E18-2E19cm -2 , the doping concentration of SiC Drift layer is 1E15-5E16cm -2 .

[0007] Specifically, the doping concentration of the P region in step S100 is 5E17-1E19cm -2 The depth from the bottom surface to the top surface of the SiC Drift layer is 0.4um-1um.

[0008] Specifically, the doping concentration of the N region in step S200 is 5E16-5E17cm -2 , thickness is 0.6um-2um.

[0009] Specifically, the doping concentration of the Pwell region in step S200 is 1E17-3E18cm -2 , thickness is 0.4um -1.8um.

[0010] Specifically, the doping concentration of the NP region in step S200 is 1E18-1E19 cm -2 , the bottom depth is 0.2um-1.5um.

[0011] Specifically, in step S300 , the depth of the bottom of the trench is 0 um-0.3 um less than the depth of the bottom surface of the P region.

[0012] Specifically, the thickness of the gate oxide layer in step S400 is 30 nm-80 nm.

[0013] Specifically, in step S800 , the thickness of the Ti metal is 0.1 um-0.6 um, and the thickness of the AlCu metal is 2 um-5 um.

[0014] A SiC transistor with strong short-circuit characteristics, comprising a SiC Sub layer, a SiC Drift layer, an N region, an isolation dielectric layer and a front electrode metal layer arranged in sequence from bottom to top; The SiC Drift layer is provided with a P region extending downward from the top surface; The N region is provided with: A Pwell region extending downward from the top surface of the N region and having a spacing from the bottom surface of the N region; An NP region extending downward from the top surface of the Pwell region; A gate oxide layer, having a U-shaped cross section, extending downward from the top surface of the NP region to the P region; A Poly layer, filled in the gate oxide layer, wherein the top surface of the Poly layer is flush with the top surface of the gate oxide layer; The bottom surface of the isolation dielectric layer is respectively connected to the NP region, the gate oxide layer and the Poly layer, and the side portion is provided with a front ohmic contact alloy layer connected to the NP region.

[0015] Beneficial effects of the present invention: 1. Improve the short-circuit characteristics of the device: The present invention is directed to a trench gate SiC MOSFET, and a JFET structure (P region, N region and Pwell region in the structure) is formed inside the device. When the device is short-circuited, the short-circuit current needs to flow through the JFET region to reach the other electrode, and the JFET region suppresses the short-circuit current, thereby extending the short-circuit withstand time of the device and improving the short-circuit characteristics of the SiC MOSFET.

[0016] 2. Protect the gate oxide layer of the device and improve the reliability of use: Although the size of the trench gate SiC MOSFET can be extremely small, the electric field concentration of the gate oxide layer at the bottom corner of the trench can easily cause premature breakdown failure here, damaging the device, which has always been a major problem of the trench gate SiC MOSFET device. The present invention aims at this problem, by designing P regions on both sides of the bottom corner of the trench of the trench gate SiC MOSFET, the bottom corner is completely wrapped in the P region to achieve protection of the corner, avoid premature breakdown failure of the gate oxide layer at the bottom corner of the trench, and improve the reliability of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 Schematic diagram of the structure of the trench gate SiC MOSFET of the present invention; Figure 2 is a structural schematic diagram of step S100 of the present invention; Figure 3 is a structural schematic diagram of step S200 of the present invention; Figure 4is a schematic structural diagram of step S300 of the present invention; Figure 5 is a structural schematic diagram of step S400 of the present invention; Figure 6 is a schematic structural diagram of step S500 of the present invention; Figure 7 is a schematic structural diagram of step S700 of the present invention; Figure 8 is a structural schematic diagram of step S800 of the present invention; Fig. 9 is a structural schematic diagram of step S900 of the present invention; Fig.10 is a structural schematic diagram of step S1000 of the present invention; Fig.11 is a structural schematic diagram of step S1100 of the present invention; Fig.12 is a schematic diagram of the structure of step S1200 of the present invention; In the figure, 1 is SiC Sub layer, 2 is SiCDrift layer, 3 is P region, 4 is N region, 5 is Pwell region, 6 is NP region, 7 is gate oxide layer, 8 is Poly layer, 9 is isolation dielectric layer, 10 is front ohmic contact alloy layer, and 11 is front electrode metal layer. DETAILED DESCRIPTION

[0018] The present invention is described in detail below in conjunction with specific practical cases. Examples of the embodiments are shown in the accompanying drawings, and the schematic implementation methods of the present invention and their descriptions are only used to explain the present invention and are not intended to limit the present invention.

[0019] In the description of the present invention, it should be understood that the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention. In the description of the present invention, unless otherwise specified, "plurality" means two or more.

[0020] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0021] A SiC transistor with robust short-circuit characteristics comprises the following steps: S100, forming a SiC Drift layer 2 on the top surface of the SiC Sub layer 1 by epitaxial deposition; The SiC Sub layer 1 in step S100 is heavily doped, with a doping concentration of 5E18-2E19cm -2 , SiC Drift layer 2 is lightly doped, with a doping concentration of 1E15-5E16cm -2 .

[0022] S200, forming a P region 3 on the top surface of the SiC Drift layer 2 by Al ion implantation; The P region 3 in step S200 is heavily doped, with a doping concentration of 5E17-1E19cm -2 The depth between the bottom surface and the top surface of the SiC Drift layer 2 is 0.4um-1um.

[0023] S300, forming an N region 4 on the top surface of the SiC Drift layer 2 by epitaxial deposition; The N region 4 in step S300 is lightly doped, with a doping concentration of 5E16-5E17cm -2 , thickness is 0.6um-2um.

[0024] S400, forming a Pwell region 5 on the top surface of the N region 4 by Al ion implantation; The Pwell region 5 in step S400 is lightly doped, with a doping concentration of 1E17-3E18cm -2 , thickness is 0.4um -1.8um.

[0025] S500, forming a NP region 6 on the top surface of the Pwell region 5 by N ion implantation; The NP region 6 in step S500 is heavily doped, with a doping concentration of 1E18-1E19 cm -2 , the bottom depth is 0.2um-1.5um.

[0026] S600, activating and forming the implanted regions of the P region 3, the Pwell region 5 and the NP region 6 by high temperature ion annealing; The high temperature ion annealing condition in step S600 is a temperature of 1600° C.-1900° C.

[0027] S700, forming a trench on the top surface of the NP region 6 by etching downward, and the bottom surface of the trench coincides with the bottom surface of the P region 3; The depth of the bottom of the trench in step S700 is 0um-0.3um less than the bottom depth of the P region 3 , and the P region 3 must wrap around the bottom corners on both sides of the trench.

[0028] S800, forming a gate oxide layer 7 on the inner wall of the trench by introducing oxygen to perform dry oxygen oxidation; The thickness of the gate oxide layer 7 in step S800 is 30 nm-80 nm.

[0029] S900, forming a Poly layer 8 inside the trench by depositing polysilicon; S1000, forming an isolation dielectric layer 9 on the top surfaces of the NP region 6 and the Poly layer 8 by oxide deposition; S1100, forming a front ohmic contact alloy layer 10 on the top surface of the NP region 6 by Ni metal sputtering followed by rapid thermal annealing; The Ni metal thickness in step S1100 is 0.3um-1um.

[0030] S1200, forming a front electrode metal layer 11 on the top of the device by sputtering Ti and AlCu metals; The thickness of the Ti metal in step S1200 is 0.1um-0.6um, and the thickness of the AlCu metal is 2um-5um.

[0031] A SiC transistor with strong short-circuit characteristics, comprising a SiC Sub layer (1), a SiC Drift layer (2), an N region (4), an isolation dielectric layer (9), and a front electrode metal layer (11) arranged in sequence from bottom to top; The SiC Drift layer (2) is provided with a P region (3) extending downward from the top surface; The N region (4) is provided with: A Pwell region (5) extending downward from the top surface of the N region (4) and having a spacing from the bottom surface of the N region (4); An NP region (6) extending downward from the top surface of the Pwell region (5); The gate oxide layer (7) has a U-shaped cross-section and extends downward from the top surface of the NP region (6) to the inside of the P region (3); the P region 3 wraps around the bottom corners on both sides of the gate oxide layer 7; A Poly layer (8) filled in the gate oxide layer (7), wherein the top surface of the Poly layer (8) is flush with the top surface of the gate oxide layer (7); The bottom surface of the isolation dielectric layer (9) is respectively connected to the NP region (6), the gate oxide layer (7) and the Poly layer (8), and a front ohmic contact alloy layer (10) connected to the NP region (6) is provided on the side.

[0032] The bottom surface of the N region (4) is connected to the P region (3) and the SiC Drift layer (2) respectively.

[0033] The bottom surface of the front electrode metal layer (11) is respectively connected to the front ohmic contact alloy layer (10) and the isolation dielectric layer (9).

[0034] The present invention is Figure 1 In the trench gate SiC MOSFET device shown, by designing P region 3 on both sides of the bottom corner of the trench, the bottom corner is completely wrapped in P region 3 to achieve protection of the corner, avoiding breakdown failure of the gate oxide layer at the bottom corner of the channel. At the same time, the P region 3, the N region 4 and the Pwell region 5 above form a JFET structure represented by the dotted box in the figure. When the device is short-circuited, the short-circuit current ID represented by the arrow in the figure needs to flow through the JFET region to reach the other electrode, and the JFET region suppresses the short-circuit current ID, thereby extending the short-circuit withstand time of the device and improving the short-circuit characteristics.

Claims

1. A method for preparing a SiC transistor with strong short-circuit characteristics, characterized in that: The steps include: S100, forming a SiC Drift layer (2) on the top surface of the SiC Sub layer (1) by epitaxial deposition, and implanting a P region (3) into the SiC Drift layer (2); S200, epitaxially depositing an N region (4) on the top surface of the SiC Drift layer (2), and sequentially forming a Pwell region (5) and an NP region (6) in the N region (4), and activating the implanted region by high temperature ion annealing; S300, etching downwards to form a groove on the top surface of the NP region (6); S400, forming a gate oxide layer (7) in the trench; S500, forming a Poly layer (8) inside the trench by depositing polysilicon; S600, forming an isolation dielectric layer (9) on top surfaces of the gate oxide layer (7) and the Poly layer (8); S700, forming a front ohmic contact alloy layer (10) on the top surface of the NP region (6) by Ni metal sputtering followed by rapid thermal annealing; S800, forming a front electrode metal layer (11) on the top of the device by sputtering Ti and AlCu metals.

2. The method for preparing a SiC transistor with strong short-circuit characteristics according to claim 1, characterized in that: In step S100, the doping concentration of the SiC Sub layer (1) is 5E18-2E19cm -2 , the doping concentration of SiC Drift layer (2) is 1E15-5E16cm -2 .

3. The method for preparing a SiC transistor with strong short-circuit characteristics according to claim 1, characterized in that: In step S100, the doping concentration of the P region (3) is 5E17-1E19cm -2 The depth between the bottom surface and the top surface of the SiC Drift layer (2) is 0.4um-1um.

4. The method for preparing a SiC transistor with a strong short-circuit characteristic according to claim 1, characterized in that: In step S200, the doping concentration of N region (4) is 5E16-5E17cm -2 , thickness is 0.6um-2um.

5. The method for preparing a SiC transistor with strong short-circuit characteristics according to claim 1, characterized in that: In step S200, the doping concentration of the Pwell region (5) is 1E17-3E18cm -2 , thickness is 0.4um -1.8um.

6. The method for preparing a SiC transistor with strong short-circuit characteristics according to claim 1, characterized in that: In step S200, the doping concentration of the NP region (6) is 1E18-1E19 cm -2 , the bottom depth is 0.2um-1.5um.

7. The method for preparing a SiC transistor with strong short-circuit characteristics according to claim 1, characterized in that: In step S300, the depth of the bottom of the trench is 0um-0.3um less than the depth of the bottom surface of the P region (3).

8. The method for preparing a SiC transistor with strong short-circuit characteristics according to claim 1, characterized in that: The thickness of the gate oxide layer (7) in step S400 is 30nm-80nm.

9. The method for preparing a SiC transistor with strong short-circuit characteristics according to claim 1, characterized in that: In step S800 , the thickness of the Ti metal is 0.1um-0.6um, and the thickness of the AlCu metal is 2um-5um.

10. A SiC transistor with a strong short-circuit characteristic, prepared by the method for preparing a SiC transistor with a strong short-circuit characteristic according to any one of claims 1 to 9, characterized in that: It comprises a SiC Sub layer (1), a SiC Drift layer (2), an N region (4), an isolation dielectric layer (9) and a front electrode metal layer (11) which are arranged in sequence from bottom to top; The SiC Drift layer (2) is provided with a P region (3) extending downward from the top surface; The N region (4) is provided with: A Pwell region (5) extending downward from the top surface of the N region (4) and having a spacing from the bottom surface of the N region (4); An NP region (6) extending downward from the top surface of the Pwell region (5); A gate oxide layer (7) having a U-shaped cross-section and extending downward from the top surface of the NP region (6) to the inside of the P region (3); A Poly layer (8) filled in the gate oxide layer (7), wherein the top surface of the Poly layer (8) is flush with the top surface of the gate oxide layer (7); The bottom surface of the isolation dielectric layer (9) is respectively connected to the NP region (6), the gate oxide layer (7) and the Poly layer (8), and a front ohmic contact alloy layer (10) connected to the NP region (6) is provided on the side.