Method for preparing neopentyl glycol
By filling different proportions of catalysts with a mixture of copper-based catalysts under high temperature and high pressure conditions, the problems of catalyst strength reduction and component elution are solved, the yield and process stability of neopentyl glycol are improved, and the length of catalysts is achieved Time running and high yield.
Patent Information
- Application Number
- CN202480002176.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-02-08
- Filing Date
- 2024-02-13
- Publication Date
- 2024-11-26
AI Technical Summary
When preparing neopentyl glycol under high temperature and high pressure conditions, the reduction in the strength of the catalyst and the elution of components lead to a decrease in process stability and yield, and a method is needed to improve the stability of the catalyst and prevent the elution of the catalyst components.
Using a mixture of the first hydrogenation catalyst and the second hydrogenation catalyst containing copper, the hydrogenation reactor is filled with different proportions of catalysts to meet a specific specific surface area and density range and hydrogenation is carried out under high temperature and high pressure conditions. The reaction prevents the elution of the catalyst components.
It improves the yield and process stability of neopentyl glycol, extends the life of the catalyst, reduces the elution of silica, and enhances the stability and activity of the catalyst.
Smart Images

Figure CN119032074A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for preparing neopentyl glycol.
[0002] This application claims priority to and the benefits of Korean Patent Applications No. 10-2023-0018881 and No. 10-2024-0019690 filed on February 13, 2023 and February 8, 2024, respectively, in the Korean Intellectual Property Office, the entire contents of which are incorporated into this specification by reference. Background Art
[0003] Neopentyl glycol (NPG) is a white crystalline material with a melting point above 130°C. It is used as an important intermediate for various synthetic resins and is also widely used in industry as a raw material for various plastic powder coatings, synthetic lubricants, plasticizers, surfactants, fiber processing agents, etc.
[0004] Such NPG is usually prepared by the aldol condensation reaction of isobutyraldehyde with formaldehyde to prepare hydroxypivalaldehyde (HPA), and then reacting the HPA with hydrogen in the presence of a catalyst. In this case, in order to obtain a high yield, the reaction is carried out under high temperature (above 160° C.) and high pressure (above 35 bar) conditions in the presence of a copper-based catalyst.
[0005] Since the reaction is carried out under such high temperature and high pressure conditions, the problem of reduced strength of the catalyst may occur. When the strength of the catalyst is reduced, the reactivity of the catalyst is reduced, which may cause problems in terms of process stability.
[0006] In addition, since the reaction is carried out under high temperature and high pressure conditions, the silica component as the catalyst carrier is eluted, so the silica component in the neopentyl glycol solution to be prepared may also be eluted. These problems may require additional processes to purify the silica component.
[0007] Therefore, efforts are being made to develop a catalyst having improved catalyst stability and excellent catalyst activity due to excellent catalyst strength even under high temperature and high pressure conditions. In addition, efforts are being made to develop a technology capable of preventing the elution of the catalyst component.
[0008] [Citation List] (Patent Document 1) Korean Patent Application Publication No. 10-2011-0038324 Summary of the invention
[0009] Technical issues
[0010] The present invention is directed to providing a method for preparing neopentyl glycol, which method reduces the elution amount of catalyst components while maintaining a high yield.
[0011] Technical Solution
[0012] An exemplary embodiment of the present invention provides a method for preparing neopentyl glycol, the method comprising: filling an inlet of a hydrogenation reactor with a first hydrogenation catalyst comprising copper; filling an outlet of the hydrogenation reactor with a second hydrogenation catalyst; introducing a raw material gas comprising hydroxypivaldehyde and hydrogen into the hydrogenation reactor filled with the first hydrogenation catalyst and the second hydrogenation catalyst; and performing a hydrogenation reaction while contacting the introduced raw material gas with the first hydrogenation catalyst and the second hydrogenation catalyst in sequence, wherein the first hydrogenation catalyst has 200 m 2 / g or more and a density of 500 g / L or more and less than 600 g / L, the first hydrogenation catalyst and the second hydrogenation catalyst are different from each other and satisfy the following Formula 1 and Formula 2.
[0013] [Formula 1]
[0014] x+y=100(%)
[0015] [Formula 2]
[0016] x>y
[0017] In equation 1 and equation 2,
[0018] x represents the filling ratio (%) of the first hydrogenation catalyst in the hydrogenation reactor,
[0019] y represents the filling ratio (%) of the second hydrogenation catalyst in the hydrogenation reactor.
[0020] An exemplary embodiment of the present invention provides a method for preparing neopentyl glycol, the method comprising: filling an inlet of a hydrogenation reactor with a first hydrogenation catalyst comprising copper; filling the hydrogenation reactor with a second hydrogenation catalyst and a third hydrogenation catalyst in sequence, so that an outlet of the hydrogenation reactor is filled with the third hydrogenation catalyst, and a position between a position filled with the first hydrogenation catalyst and a position filled with the third hydrogenation catalyst is filled with the second hydrogenation catalyst; introducing a raw material gas comprising hydroxypivaldehyde and hydrogen into the hydrogenation reactor filled with the first to third hydrogenation catalysts; and performing a hydrogenation reaction while contacting the introduced raw material gas with the first to third hydrogenation catalysts in sequence, wherein the first to third hydrogenation catalysts are different from each other and satisfy the following Formulas 3 and 4.
[0021] [Formula 3]
[0022] x+y+z=100(%)
[0023] [Formula 4]
[0024] x>y+z
[0025] In equation 3 and equation 4,
[0026] x represents the filling ratio (%) of the first hydrogenation catalyst in the hydrogenation reactor,
[0027] y represents the filling ratio (%) of the second hydrogenation catalyst in the hydrogenation reactor,
[0028] z represents the filling ratio (%) of the third hydrogenation catalyst in the hydrogenation reactor.
[0029] Beneficial Effects
[0030] According to the method for preparing neopentyl glycol of the present invention, the stability of the process for preparing neopentyl glycol can be enhanced by preventing the elution of the catalyst component even in a high temperature and high pressure reaction. That is, since the process can be carried out for a long time, the productivity can be improved.
[0031] The method for preparing neopentyl glycol according to the present invention can improve the yield of neopentyl glycol. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 is a view showing a conventional method for preparing neopentyl glycol.
[0033] Figure 2 and Figure 3 is a view showing a method for preparing neopentyl glycol according to the present invention.
[0034] [Explanation of Reference Numerals]
[0035] 1: Reaction raw material supply pipe
[0036] 2: Reactor
[0037] 3: Area filled with the first hydrogenation catalyst
[0038] 4: Area filled with the second hydrogenation catalyst
[0039] 4': Area filled with the second hydrogenation catalyst and the third hydrogenation catalyst
[0040] 5: Reaction product outlet pipe
[0041] 6: Reaction product circulation pipe DETAILED DESCRIPTION
[0042] Hereinafter, the present invention will be described in detail so that those skilled in the art to which the present invention pertains can easily implement the present invention. However, the present invention can be implemented in various different forms and is not limited to the configurations described in this specification.
[0043] In the present specification, when a part “comprises” one component, unless otherwise specifically described, this does not mean excluding another component but means that another component may be further included.
[0044] In this specification, "p to q" means "p or more and q or less".
[0045] In this specification, "specific surface area" is measured by the BET method, specifically, calculated from the amount of nitrogen adsorbed at liquid nitrogen temperature (77K) using BELSORP-mino II manufactured by BEL Japan, Inc. That is, in the present invention, the BET specific surface area may refer to a specific surface area measured by the measurement method.
[0046] In this specification, the value of "density" is determined by measuring the weight of the catalyst introduced into a 1 L measuring cylinder commonly used in the art.
[0047] In the present specification, as the "diameter", a value obtained by measuring the diameters of 20 catalyst samples using a vernier caliper commonly used in the art and then averaging the values is used.
[0048] In this specification, "nth hydrogenation catalyst" is an expression for classifying hydrogenation catalysts according to the position of filling, and the hydrogenation catalyst first filled based on the inlet of the reactor is defined as the first hydrogenation catalyst. When the reactor is vertically oriented, the inlet of the reactor can be represented as the top of the reactor, the outlet of the reactor can be represented as the bottom of the reactor, and regardless of the orientation of the reactor, the area between the inlet (or top) of the reactor and the outlet (or bottom) of the reactor can be represented as the middle of the reactor.
[0049] Furthermore, in describing the present invention, detailed descriptions of related known technologies that may unnecessarily obscure the gist of the present invention will be omitted.
[0050] An exemplary embodiment of the present invention provides a method for preparing neopentyl glycol, the method comprising: filling an inlet of a hydrogenation reactor with a first hydrogenation catalyst comprising copper; filling an outlet of the hydrogenation reactor with a second hydrogenation catalyst; introducing a raw material gas comprising hydroxypivaldehyde and hydrogen into the hydrogenation reactor filled with the first hydrogenation catalyst and the second hydrogenation catalyst; and performing a hydrogenation reaction while contacting the introduced raw material gas with the first hydrogenation catalyst and the second hydrogenation catalyst in sequence, wherein the first hydrogenation catalyst and the second hydrogenation catalyst are different from each other, and the first hydrogenation catalyst has 200 m 2 / g or more and a density of 500g / L or more and less than 600g / L, and satisfying the above formulas 1 and 2.
[0051] The method for preparing neopentyl glycol according to the present invention is characterized in that a mixture of two or more hydrogenation catalysts is used, and these hydrogenation catalysts show different core properties for operating conditions according to the position of the reactor. In addition, the first hydrogenation catalyst must contain copper, characterized in that the inside of the hydrogenation reactor is filled with a first hydrogenation catalyst having a larger proportion than the second hydrogenation catalyst. Therefore, even in high temperature and high pressure reactions, the stability of the process for preparing neopentyl glycol can be enhanced by preventing the elution of the catalyst component. In other words, since the process can be carried out for a long time, productivity can be improved. In addition, owing to using a catalyst suitable for the position of the reactor, the method for preparing neopentyl glycol according to the present invention has a high neopentyl glycol yield.
[0052] That is, the first hydrogenation catalyst according to the present invention is a copper-based catalyst.
[0053] In an exemplary embodiment of the present invention, the first hydrogenation catalyst may have 200 m 2 / g or more, preferably 300m 2 / g or more specific surface area.
[0054] In an exemplary embodiment of the present invention, the first hydrogenation catalyst may have 1,000 m 2 / g or less specific surface area.
[0055] In an exemplary embodiment of the present invention, the first hydrogenation catalyst may have 200 m 2 / g or more and 1,000m 2 / g or less, preferably 300m 2 / g or more and 1,000m 2 / g or less specific surface area.
[0056] In an exemplary embodiment of the present invention, the first hydrogenation catalyst may have a density of 500 g / L or more and less than 600 g / L, preferably 550 g / L or more and less than 600 g / L.
[0057] Generally, as the specific surface area of the hydrogenation catalyst increases, the hydrogenation reaction activity tends to increase. However, when the specific surface area of the hydrogenation catalyst increases, the density generally tends to decrease, which may cause the elution amount of silicon dioxide (Si) and the stability of the catalyst to increase and decrease, respectively. The first hydrogenation catalyst has high activity at low temperatures by satisfying the specific surface area range, and at the same time satisfies the above-mentioned density range, so the elution of silicon dioxide can be prevented and the stability of the catalyst can be enhanced.
[0058] That is, the first hydrogenation catalyst is a catalyst having characteristics of exhibiting high activity at low temperatures while having an appropriate level of catalyst stability.
[0059] In an exemplary embodiment of the present invention, the first hydrogenation catalyst may be a catalyst having an extruded or spherical morphology.
[0060] In an exemplary embodiment of the present invention, the first hydrogenation catalyst may have a diameter of 1 mm to 6 mm, preferably 2 mm to 5 mm. When the diameter is satisfied, the yield of neopentyl glycol may be increased.
[0061] In an exemplary embodiment of the present invention, the second hydrogenation catalyst comprises a copper component and may have a 30 m 2 / g or more and less than 200m 2 / g specific surface area and a density of 600 g / L or more. That is, the second hydrogenation catalyst may be a copper-based catalyst. However, the second hydrogenation catalyst has a different specific surface area and density range from the first hydrogenation catalyst.
[0062] In an exemplary embodiment of the present invention, the second hydrogenation catalyst may have 30 m 2 / g or more and less than 200m 2 / g, preferably 80m 2 / g or more and less than 160m 2 / g specific surface area.
[0063] In an exemplary embodiment of the present invention, the second hydrogenation catalyst may have a density of 600 g / L or more, preferably 650 g / L or more.
[0064] In an exemplary embodiment of the present invention, the second hydrogenation catalyst may have a density of 800 g / L or less.
[0065] In an exemplary embodiment of the present invention, the second hydrogenation catalyst may have a density of 600 g / L or more and 800 g / L or less, preferably 650 g / L or more and 800 g / L or less.
[0066] The second hydrogenation catalyst can minimize the decrease in catalyst activity by satisfying the specific surface area range, and can reduce the elution amount of silicon dioxide (Si) by satisfying the density range, thereby increasing the stability of the catalyst. That is, since the second hydrogenation catalyst has high activity at low temperatures and satisfies the specific surface area range while satisfying the above-mentioned density range, the elution of silicon dioxide can be prevented and the stability of the catalyst can be enhanced.
[0067] That is, the second hydrogenation catalyst is a catalyst having a characteristic of being highly stable at high temperature and high pH while having an appropriate level of catalyst activity.
[0068] In an exemplary embodiment of the present invention, the second hydrogenation catalyst may be a catalyst having an extruded or spherical morphology.
[0069] In an exemplary embodiment of the present invention, the second hydrogenation catalyst may have a diameter of 2 mm to 8 mm, preferably 3 mm to 6 mm. When the diameter is satisfied, the yield of neopentyl glycol may be increased.
[0070] In an exemplary embodiment of the present invention, the method may further include filling the hydrogenation reactor with a hydrogenation catalyst different from the first hydrogenation catalyst and the second hydrogenation catalyst, so that a position between a position filled with the first hydrogenation catalyst and a position filled with the second hydrogenation catalyst in the hydrogenation reactor is filled with the hydrogenation catalyst.
[0071] An exemplary embodiment of the present invention provides a method for preparing neopentyl glycol, the method comprising: filling an inlet of a hydrogenation reactor with a first hydrogenation catalyst comprising copper; filling the hydrogenation reactor with a second hydrogenation catalyst and a third hydrogenation catalyst in sequence, so that an outlet of the hydrogenation reactor is filled with the third hydrogenation catalyst, and a position between a position filled with the first hydrogenation catalyst and a position filled with the third hydrogenation catalyst is filled with the second hydrogenation catalyst; introducing a raw material gas comprising hydroxypivaldehyde and hydrogen into the hydrogenation reactor filled with the first to third hydrogenation catalysts; and performing a hydrogenation reaction while contacting the introduced raw material gas with the first to third hydrogenation catalysts in sequence, wherein the first to third hydrogenation catalysts are different from each other and satisfy the following Formulas 3 and 4.
[0072] [Formula 3]
[0073] x+y+z=100(%)
[0074] [Formula 4]
[0075] x>y+z
[0076] In equation 3 and equation 4,
[0077] x represents the filling ratio (%) of the first hydrogenation catalyst in the hydrogenation reactor,
[0078] y represents the filling ratio (%) of the second hydrogenation catalyst in the hydrogenation reactor,
[0079] z represents the filling ratio (%) of the third hydrogenation catalyst in the hydrogenation reactor.
[0080] The method for preparing neopentyl glycol according to the present invention may further include a third hydrogenation catalyst, characterized in that, considering the operating conditions and core performance, the reactor is also filled with the third hydrogenation catalyst. Even in this case, the reactor is filled with the first hydrogenation catalyst at the largest ratio, and the filling ratio of the first hydrogenation catalyst is higher than the total filling ratio of the second hydrogenation catalyst and the third hydrogenation catalyst.
[0081] Therefore, even in a high temperature and high pressure reaction, the stability of the process for preparing neopentyl glycol can be enhanced by preventing the elution of the catalyst component. That is, since the process can be carried out for a long time, the productivity can be improved, and the yield of the neopentyl glycol to be prepared is high.
[0082] When the first to third hydrogenation catalysts are used, the above description may be applied to the description of the first hydrogenation catalyst and the second hydrogenation catalyst.
[0083] In an exemplary embodiment of the present invention, the third hydrogenation catalyst comprises a copper component and may have a 30 m 2 / g or more and less than 200m 2 / g specific surface area and a density of 600 g / L or more. That is, the third hydrogenation catalyst may be a copper-based catalyst. However, the third hydrogenation catalyst has a different specific surface area and density range from the first hydrogenation catalyst.
[0084] In an exemplary embodiment of the present invention, the third hydrogenation catalyst may have 30 m 2 / g or more and less than 200m 2 / g, preferably 80m 2 / g or more and less than 160m 2 / g specific surface area.
[0085] In an exemplary embodiment of the present invention, the third hydrogenation catalyst may have a density of 600 g / L or more, preferably 650 g / L or more.
[0086] In an exemplary embodiment of the present invention, the third hydrogenation catalyst may have a density of 800 g / L or less.
[0087] In an exemplary embodiment of the present invention, the third hydrogenation catalyst may have a density of 600 g / L or more and 800 g / L or less, preferably 650 g / L or more and 800 g / L or less.
[0088] The third hydrogenation catalyst can minimize the decrease in catalyst activity by satisfying the specific surface area range, and can reduce the elution amount of silicon dioxide (Si) by satisfying the density range, thereby increasing the stability of the catalyst. That is, the third hydrogenation catalyst has high activity at low temperatures by satisfying the specific surface area range, while satisfying the above-mentioned density range, so that the elution of silicon dioxide can be prevented and the stability of the catalyst can be enhanced.
[0089] That is, like the second hydrogenation catalyst, the third hydrogenation catalyst is also a catalyst having characteristics of being highly stable at high temperature and high pH while having an appropriate level of catalyst activity.
[0090] In an exemplary embodiment of the present invention, the third hydrogenation catalyst may be a catalyst having an extruded or spherical morphology.
[0091] Herein, the fact that the catalyst has a spherical morphology means that the catalyst is prepared by coating a spherical support with an active ingredient, unlike an extruded catalyst formed using an extruder.
[0092] In an exemplary embodiment of the present invention, the third hydrogenation catalyst may have a diameter of 2 mm to 8 mm, preferably 3 mm to 6 mm. When the diameter is satisfied, the yield of neopentyl glycol may be increased.
[0093] In an exemplary embodiment of the present invention, specific surface areas of the first to third hydrogenation catalysts may satisfy Formula 5 below.
[0094] [Formula 5]
[0095] S a >S b >S c
[0096] In formula 5,
[0097] S a is the specific surface area of the first hydrogenation catalyst (unit: m 2 / g),
[0098] S b is the specific surface area of the second hydrogenation catalyst (unit: m 2 / g),
[0099] S c is the specific surface area of the third hydrogenation catalyst (unit: m 2 / g).
[0100] That is, the specific surface area of the catalyst filled at the inlet of the reactor is the largest, the specific surface area of the catalyst filled at the outlet of the reactor is the smallest, and the specific surface area of the catalyst filled at a position between the inlet and the outlet is of an intermediate size.
[0101] In an exemplary embodiment of the present invention, the densities of the first to third hydrogenation catalysts may satisfy Formula 6 below.
[0102] [Formula 6]
[0103] d c >d b >d a
[0104] In formula 6,
[0105] d a is the density of the first hydrogenation catalyst (unit: g / L),
[0106] d b is the density of the second hydrogenation catalyst (unit: g / L),
[0107] d c is the density of the third hydrogenation catalyst (unit: g / L).
[0108] That is, the density of the catalyst filled at the inlet of the reactor is the smallest, the density of the catalyst filled at the outlet of the reactor is the largest, and the density of the catalyst filled at a position between the inlet and the outlet has an intermediate value.
[0109] The method for preparing neopentyl glycol according to the present invention is characterized in that, in the process of developing a catalyst having improved catalyst stability and excellent catalyst activity due to excellent catalyst strength even under high temperature and high pressure conditions, the method and conditions for preparing the catalyst are optimized and applied. That is, in order to adjust the specific surface area to below a predetermined level and to improve the stability of the catalyst (or reduce the elution amount of silica) within a range that minimizes the decrease in the activity of the catalyst, the yield of neopentyl glycol can be increased by applying a catalyst whose density has been adjusted to above a predetermined level to the method for preparing neopentyl glycol.
[0110] That is, when the relationship between the specific surface area and density of the first to third hydrogenation catalysts satisfies the above-mentioned Formula 5 and / or Formula 6, the activity and stability of the hydrogenation catalyst can be optimized, so that the case of using it to prepare neopentyl glycol has an excellent yield of neopentyl glycol.
[0111] An exemplary embodiment of the present invention provides a method for preparing neopentyl glycol, the method comprising conducting a hydrogenation reaction by introducing a hydroxypivalaldehyde (HPA) solution and hydrogen into a hydrogenation reactor, wherein the hydrogenation reactor is filled with a hydrogenation catalyst satisfying the characteristics of the first to third hydrogenation catalysts described above.
[0112] That is, in an exemplary embodiment of the present invention, the hydrogenation reactor may be filled with the above-mentioned first to third hydrogenation catalysts.
[0113] More specifically, in an exemplary embodiment of the present invention, the hydrogenation reactor may be filled with the above-mentioned first hydrogenation catalyst and the second hydrogenation catalyst, or the hydrogenation reactor may be filled with all of the above-mentioned first to third hydrogenation catalysts.
[0114] In an exemplary embodiment of the present invention, the inlet and outlet of the hydrogenation reactor may be filled with alumina balls. The alumina balls may have a diameter of 2 mm to 6 mm and may be used to uniformly disperse the reactants.
[0115] In an exemplary embodiment of the present invention, the method for preparing neopentyl glycol may be a method known in the art except for including the catalyst for preparing neopentyl glycol according to the present invention.
[0116] For example, the hydrogenation reactor may be a fixed bed reactor (FBR) filled with a catalyst for preparing neopentyl glycol, in which case there is no need to separate the catalyst and the reaction product, and since the reaction temperature and reaction pressure can be lowered compared to the prior art, the hydrogenation reactor is stably operated and economical, and since the catalyst is easy to replace and the reactor size can be reduced, there is an effect of significantly reducing investment costs.
[0117] Figure 1 The conventional method for preparing neopentyl glycol is shown, and the case where the reactor is filled with a first hydrogenation catalyst is shown. Specifically, a reaction raw material supply pipe 1 for supplying raw material gas including hydroxypivaldehyde and hydrogen is connected to a reactor 2, and the reactor 2 is filled with a first hydrogenation catalyst. A region 3 filled with the first hydrogenation catalyst in the reactor 2 is as shown in FIG. Figure 1 In this case, the reactor 2 may be a fixed bed reactor (FBR) as described above. The raw gas supplied from the reaction raw material supply pipe 1 is hydrogenated while contacting with the first hydrogenation catalyst filled in the reactor 2, and as a result, neopentyl glycol can be obtained. The neopentyl glycol thus obtained can be transported from the reactor 2 through the reaction product outlet pipe 5. In this case, a portion of the neopentyl glycol can be transferred to the reaction raw material supply pipe 1 through the reaction product circulation pipe 6 and reused for the reaction in the reactor 2.
[0118] Figure 2 The method for preparing neopentyl glycol according to the present invention is shown, and the case where the reactor is filled with a first hydrogenation catalyst and a second hydrogenation catalyst is shown. Figure 1 compared to, Figure 2The difference is that the interior of the reactor 2 is filled with the first hydrogenation catalyst and the second hydrogenation catalyst. Specifically, the inlet of the reactor 2 is filled with x% of the first hydrogenation catalyst, and the outlet of the reactor 2 is filled with y% of the second hydrogenation catalyst. The region 3 filled with the first hydrogenation catalyst and the region 4 filled with the second hydrogenation catalyst in the reactor 2 are as shown in FIG. Figure 2 In addition, the inlet of the reactor 2 here refers to the position where the raw material gas is supplied. More specifically, the inlet of the reactor 2 refers to the position of the portion where the reactor 2 is connected to the reaction raw material supply pipe 1.
[0119] The outlet of the reactor 2 refers to the position of the part where the produced neopentyl glycol is discharged from the reactor. More specifically, the outlet of the reactor 2 refers to the position of the part where the reactor 2 is connected to the reaction product outlet pipe 5.
[0120] In this case, the filling ratio of the first hydrogenation catalyst is higher than the filling ratio of the second hydrogenation catalyst. Figure 2 As shown in , the conditions x+y=100 and x>y are satisfied. Figure 1 The description can be applied to Figure 2 .
[0121] Figure 3 Another method for preparing neopentyl glycol according to the present invention is shown, and a case where the reactor is filled with the first to third hydrogenation catalysts is shown. In this case, the filling ratio of the first hydrogenation catalyst is higher than the sum of the filling ratio of the second hydrogenation catalyst and the filling ratio of the third hydrogenation catalyst. That is, Figure 3 As shown in , the conditions x+y+z=100 and x>y+z are satisfied. Figure 1 and Figure 2 The description can be applied to Figure 3 In this case, in the reactor 2, the region 3 filled with the first hydrogenation catalyst and the region 4′ filled with the second hydrogenation catalyst and the third hydrogenation catalyst are as follows: Figure 3 as shown in .
[0122] In an exemplary embodiment of the present invention, the hydroxypivaldehyde solution may include 50% to 80% by weight of hydroxypivaldehyde, 1% to 5% by weight of neopentyl glycol, 15% to 35% by weight of alcohol, and 1% to 10% by weight of water, in which case, because the heat of reaction can be minimized without reducing reactivity, the effect of suppressing the generation of by-products is achieved. In addition, the hydroxypivaldehyde solution may further include a high boiling point material. That is, in an exemplary embodiment of the present invention, the hydroxypivaldehyde solution may further include a high boiling point material of 1% to 6% by weight.
[0123] Furthermore, in an exemplary embodiment of the present invention, the hydrogenation reaction may be performed at a reaction temperature of 100°C to 250°C, preferably 100°C to 200°C, and more preferably 100°C to 180°C.
[0124] In addition, in an exemplary embodiment of the present invention, the hydrogenation reaction may be performed at a reaction pressure of 35 bar or more. The reaction pressure refers to a measured pressure.
[0125] When the catalyst for preparing neopentyl glycol according to an exemplary embodiment of the present invention is applied to the preparation of neopentyl glycol, it is possible to prevent the problem that the catalyst component (eg, silica component) in the neopentyl glycol solution to be prepared is eluted.
[0126] Therefore, when the catalyst for preparing neopentyl glycol according to an exemplary embodiment of the present invention is applied to the preparation of neopentyl glycol, a purification process due to elution of the catalyst component (such as the silica component) is not required, and the catalyst life is extended, thereby obtaining an effect of being able to reduce the preparation cost.
[0127] Hereinafter, the present invention will be described in detail with reference to the embodiments for specifically describing the present invention. However, embodiments according to the present invention may be modified in various forms, and should not be interpreted as limiting the scope of the present invention to the embodiments described in detail below. Embodiments of the present invention are provided to more fully illustrate the present invention to those of ordinary skill in the art.
[0128] <Experimental Example 1> Performance measurement of hydrogenation catalyst
[0129] The performance of the hydrogenation catalysts was measured using hydrogenation catalysts A to C, which are CuO / SiO2-based hydrogenation catalysts, and a reaction feedstock consisting of 65 wt% HPA, 2 wt% NPG, 25 wt% 2-ethylhexanol (2-EH), 5 wt% H2O, and 3 wt% of a high boiling point material.
[0130] First, in order to measure the activity of the catalyst, 2.5 ml of catalyst A to catalyst C were added to 100 g of the reaction raw material, and then the H2 consumption was measured while performing a hydrogenation reaction at 160° C. and 35 bar for 1 hour (hr). When the H2 consumption is large, it means that the activity of the catalyst is high.
[0131] In addition, in order to measure the amount of Si eluted from the catalyst support, after a small amount of each catalyst A to catalyst C is added to the excess reaction raw material, a hydrogenation reaction is carried out at 180°C for 6 hours, which is a more severe condition than normal reaction conditions, and then the content of Si eluted in the reaction product is measured. The Si content is measured by ICP-OES analysis. More specifically, the content of Si eluted into the reaction product after the hydrogenation reaction is calculated as a relative ratio compared to the content of Si contained in the initial catalyst. The high content of Si eluted means that the stability of the catalyst is relatively low.
[0132] In addition, the specific surface area, density, and diameter of each of the hydrogenation catalysts A to C were measured using the BET method, a 1 L measuring cylinder, and a vernier caliper.
[0133] The properties of the hydrogenation catalysts A to C measured by the above-mentioned method are shown in Table 1 below.
[0134] [Table 1]
[0135]
[0136] In the following examples and comparative examples, catalysts A to C whose performances were measured in Experimental Example 1 above were used as hydrogenation catalysts. More specifically, catalysts A and B are catalysts having an extruded morphology, and catalyst C corresponds to a catalyst having a spherical morphology. For reference, for catalyst A, a commercially available catalyst called Octolyst 2009 product manufactured by Evonik Industries was used, and for catalyst D, a NiSAT360 product manufactured by Clariant was used.
[0137] In addition, Catalyst B was prepared by synthesizing a catalyst intermediate using a copper precursor and a silica sol aqueous solution, and then pulverizing the catalyst intermediate into fine powder. Thereafter, a known binder was mixed with Catalyst B to extrude the catalyst, and then the extruded catalyst was dried at a temperature of 100° C. or less. Thereafter, Catalyst B was prepared by firing at a temperature of 250° C. to 450° C.
[0138] In addition, Catalyst C was prepared by preparing a coating powder using a copper precursor and a silica sol aqueous solution, coating a support with the coating powder using an alcohol aqueous solution, and then drying and firing the coated support. Here, the coprecipitation, drying, and firing steps were performed in the same manner as the conditions for Catalyst C.
[0139] Furthermore, the catalyst activity and elution amount were calculated using the following equations.
[0140] *Catalyst activity (%) = H2 consumption of target catalyst (L) / H2 consumption of reference catalyst (L) * 100 (%)
[0141] * Si elution amount (%) = Si content eluted into the reaction product after reaction (parts by weight) / total amount of Si contained in the initial catalyst (parts by weight) × 100 (%)
[0142] Catalyst A was defined as the reference catalyst in the catalyst activity.
[0143] 1) Embodiment
[0144] A fixed bed reactor with a reactor diameter of 35.5 mm was used, and the top of the reactor was filled with 3 mm and 5 mm alumina balls, respectively, at a height of 100 mm to allow for uniform distribution of the reactants.
[0145] Subsequently, starting from the bottom, the reactor was filled in order to a height of 350 mm and 200 mm respectively with hydrogenation catalyst A and hydrogenation catalyst B. The bottom of the reactor was filled to 200 mm with 3 mm alumina balls.
[0146] While supplying 2-EH at a flow rate of 1.7 g / min and H2 at a flow rate of 100 ml / min to the reactor filled with the catalyst, the catalyst was first activated by gradually increasing the temperature of the reactor from 120°C to 200°C.
[0147] Once the catalyst activation was completed, the hydrogenation reaction was started while supplying a reaction raw material consisting of 65 wt% HPA, 2 wt% NPG, 25 wt% 2-EH, 5 wt% H2O, and 3 wt% of a high boiling point material at a constant flow rate of 3.4 g / min. In this case, while the inlet temperature of the catalyst layer in the reactor was maintained at 130° C., the hydrogenation reaction product was recycled to the inlet of the reactor at a flow rate of 17 g / min to control the temperature of the catalyst layer caused by the heat of the hydrogenation reaction to not exceed 180° C.
[0148] While continuous operation was performed for 72 hours, the composition of the reaction product was confirmed by GC analysis to calculate the HPA conversion rate and the NPG yield, and the total amount of Si eluted from the reaction product was confirmed by ICP-OES analysis. For GC analysis, an HP-1 column (L: 30 m, ID: 0.32 mm, film: 1.05 m) was used, and the organic material was analyzed using a gas chromatography analysis device (device name: Agilent 7890) under the temperature conditions of an oven of 70° C. / 3 minutes-10° C. / minute-280° C. / 35 minutes, in this case, the organic material analysis was measured at a temperature of 280° C. using FID as a detector.
[0149] ICP-OES analysis was performed under the same conditions as in Experimental Example 1.
[0150] The results are shown in Table 2 below.
[0151] 2) Example 2 and Example 3 and Comparative Example 1 and Comparative Example 2
[0152] The hydrogenation reactions of Examples 2 and 3 and Comparative Examples 1 and 2 were performed in the same manner as in Example 1, except that the catalysts shown in Table 1 above were filled at the top, middle, and bottom of the catalyst layer to the heights shown in Table 2 below, and then the HPA conversion rate and NPG yield were calculated, and the total amount of Si eluted was confirmed.
[0153] The results are shown in Table 2 below.
[0154] 3) Comparative Examples 3 to 5
[0155] The hydrogenation reactions of Comparative Examples 3 to 5 were performed in the same manner as in Example 1, except that the catalysts shown in Table 1 above were filled at the top, middle, and bottom of the catalyst layer to the heights shown in Table 2 below, and then the HPA conversion rate and NPG yield were calculated, and the elution amount of Si was confirmed. The results are shown in Table 2 below.
[0156] [Table 2]
[0157]
[0158]
[0159] In the above Table 2, Example 1 and Example 2 indicate that the reactor is filled with two types of catalysts corresponding to Catalyst A and Catalyst B and Catalyst A and Catalyst C, respectively, Example 3 indicates that the reactor is filled with three types of catalysts from Catalyst A to Catalyst C, and Comparative Example 1 and Comparative Example 2 indicate that the reactor is filled with one type of catalyst corresponding to Catalyst A and Catalyst B, respectively. The numbers in brackets indicate the filling height of the filled catalyst. In addition, the conversion rate, yield and elution amount were calculated using the following equations.
[0160] *HPA conversion rate (%) = moles of HPA reacted / moles of HPA supplied × 100 (%)
[0161] *NPG yield = moles of NPG produced / moles of HPA supplied × 100 (%)
[0162] * Si elution amount (%) = Si content eluted into the reaction product after reaction (parts by weight) / total amount of Si contained in the initial catalyst (parts by weight) × 100 (%)
[0163] As can be seen from the results in Table 2 above, when a single catalyst is used in the process of filling the reactor with a hydrogenation catalyst as in Comparative Examples 1 and 2, or when the first hydrogenation catalyst containing copper filled on the top as in Comparative Example 3 has a catalyst content of less than 200 m 2 / g of specific surface area and a density of 600 g / L or above, the elution amount of Si is relatively high or the NPG yield is reduced, while when a mixture of two or more types of hydrogenation catalysts is used for filling as in Examples 1 to 3, the NPG yield is as high as 99% and the elution amount of Si is also reduced.
[0164] Specifically, as in Comparative Example 1, when the specific surface area is 200 m 2 When Catalyst A having the conditions of 200 g / L or more and a density of 500 g / L or more and less than 600 g / L was used as the first hydrogenation catalyst containing copper introduced into the top, although the HPA conversion rate and the NPG yield were good, the elution amount of Si was 0.3%, which resulted in a shortened catalyst life due to a decrease in catalyst strength, and as in Comparative Example 2, when the specific surface area of 200 m2 was not satisfied, the elution amount of Si was 0.3%. 2 When Catalyst B having a density of 500 g / L or more and a density of 500 g / L or more and less than 600 g / L is used as the first hydrogenation catalyst containing copper introduced into the top portion, although the elution amount of Si is good, both the HPA conversion rate and the NPG yield are reduced to less than 99%. Specifically, when the HPA conversion rate is less than 99%, there is a problem that unreacted materials accumulate in the reaction product circulation pipe 6, resulting in a significant increase in the amount of catalyst required. As in Comparative Example 3, Catalyst B is used at the top portion, while Catalyst B having a specific surface area of 30 m2 is used at the bottom portion. 2 / g or more and less than 200m 2 / g and a density of 600 g / L or more catalyst C, but as in Comparative Example 2, there was no improvement in the HPA conversion and NPG yield.
[0165] Comparative Example 4 corresponds to the case where [Formula 2] is not satisfied: 2 / g or more and a density of 500g / L or more and less than 600g / L of catalyst A filled to a height of 150mm from the top, with a specific surface area of 30m 2 / g or more and less than 200m 2 / g and a density of 600g / L or more catalyst B filled in the middle to a height of 300mm, with a specific surface area of 30m 2 / g or more and less than 200m 2 / g and a catalyst C with a density of more than 600 g / L was filled at the bottom to a height of 100 mm. Although the elution amount of Si was maintained at a good level, the HPA conversion rate and NPG yield were both below 99%, and there was no improvement in the HPA conversion rate and NPG yield.
[0166] Furthermore, in the case of Comparative Example 5, the HPA hydrogenation reaction was performed by introducing a Ni-based catalyst instead of a copper-based catalyst to the top of the catalyst layer, but when the continuous reaction was performed for 72 hours, the catalyst activity continued to decrease, making it impossible to measure the stable catalyst activity. In other words, the reaction stability of the Ni-based catalyst was too low to measure the catalyst activity for the HPA hydrogenation reaction, and thus it was found that the catalyst was not suitable as a catalyst for the preparation of NPG.
[0167] That is, it was confirmed that when the method for producing neopentyl glycol according to the present invention is applied, by reducing the elution amount of the Si component as a catalyst carrier while maintaining a high reaction yield, the decrease in catalyst strength can be suppressed and the life of the catalyst can be extended.
Claims
1. A method for preparing neopentyl glycol, the method comprising: filling an inlet of a hydrogenation reactor with a first hydrogenation catalyst comprising copper; filling the outlet of the hydrogenation reactor with a second hydrogenation catalyst; introducing a raw material gas containing hydroxypivaldehyde and hydrogen into the hydrogenation reactor filled with the first hydrogenation catalyst and the second hydrogenation catalyst; and The hydrogenation reaction is carried out while the introduced raw material gas is contacted with the first hydrogenation catalyst and the second hydrogenation catalyst in sequence, Wherein, the first hydrogenation catalyst has 200m 2 / g or more and a density of 500g / L or more and less than 600g / L, The first hydrogenation catalyst and the second hydrogenation catalyst are different from each other and satisfy the following Formula 1 and Formula 2: [Formula 1] x+y=100(%) [Formula 2] x>y In equation 1 and equation 2, x represents the filling ratio (%) of the first hydrogenation catalyst in the hydrogenation reactor, y represents the filling ratio (%) of the second hydrogenation catalyst in the hydrogenation reactor.
2. The method according to claim 1, wherein: The first hydrogenation catalyst has a diameter of 1 mm to 6 mm.
3. The method according to claim 1, wherein: The second hydrogenation catalyst comprises a copper component, The second hydrogenation catalyst has 30m 2 / g or more and less than 200m 2 / g specific surface area and a density of more than 600g / L.
4. The method according to claim 1, wherein: The second hydrogenation catalyst has a diameter of 2 mm to 8 mm.
5. A method for preparing neopentyl glycol, the method comprising: filling an inlet of a hydrogenation reactor with a first hydrogenation catalyst comprising copper; sequentially filling the hydrogenation reactor with a second hydrogenation catalyst and a third hydrogenation catalyst, so that the outlet of the hydrogenation reactor is filled with the third hydrogenation catalyst, and a position between a position filled with the first hydrogenation catalyst and a position filled with the third hydrogenation catalyst is filled with the second hydrogenation catalyst; introducing a raw material gas containing hydroxypivaldehyde and hydrogen into the hydrogenation reactor filled with the first to third hydrogenation catalysts; and The hydrogenation reaction is carried out while the introduced raw material gas is contacted with the first to third hydrogenation catalysts in sequence, The first to third hydrogenation catalysts are different from each other and satisfy the following Formula 3 and Formula 4: [Formula 3] x+y+z=100(%) [Formula 4] x>y+z In equation 3 and equation 4, x represents the filling ratio (%) of the first hydrogenation catalyst in the hydrogenation reactor, y represents the filling ratio (%) of the second hydrogenation catalyst in the hydrogenation reactor, z represents the filling ratio (%) of the third hydrogenation catalyst in the hydrogenation reactor.
6. The method according to claim 5, wherein: The third hydrogenation catalyst comprises a copper component, and The third hydrogenation catalyst has 30m 2 / g or more and less than 200m 2 / g specific surface area and a density of more than 600g / L.
7. The method according to claim 5, wherein: The third hydrogenation catalyst has a diameter of 2 mm to 8 mm.
8. The method according to claim 5, wherein: The specific surface areas of the first to third hydrogenation catalysts satisfy the following formula 5: [Formula 5] S a >S b >S c In formula 5, S a is the specific surface area of the first hydrogenation catalyst (unit: m 2 / g), S b is the specific surface area of the second hydrogenation catalyst (unit: m 2 / g), S c is the specific surface area of the third hydrogenation catalyst (unit: m 2 / g).
9. The method according to claim 5, wherein: The densities of the first to third hydrogenation catalysts satisfy the following formula 6: [Formula 6] d c >d b >d a In formula 6, d a is the density of the first hydrogenation catalyst (unit: g / L), d b is the density of the second hydrogenation catalyst (unit: g / L), d c is the density of the third hydrogenation catalyst (unit: g / L).
Citation Information
Patent Citations
Method for the hydrogenation of aldehydes and apparatus using the same