Sewing method of high-density silk wool worsted fabric and clothes
By using 60S filament thread and silk piping process, combined with sewing machine pressure testing and dry ironing, the wrinkles and unevenness of high-dense filament worsted fabrics during sewing, achieving the smooth and beautiful effect of the clothes.
Patent Information
- Application Number
- CN202411211485.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-11-29
AI Technical Summary
High-dense wool worsted fabrics are prone to wrinkles and unevenness during sewing, and are difficult to deal with during ironing. The prior art has not effectively solved these problems.
The 60S filament thread is used for sewing, and the clothing is ensured to be smooth and beautiful by adjusting the pressure test of the sewing machine and using the silk piping process, combined with flat car sewing and dry ironing.
It effectively reduces wrinkles and unevenness at the stitching, improves the beauty and lightness of the clothes, reduces the difficulty of operation, and ensures good sewing effect of high-dense silk-wooled fabrics.
Smart Images

Figure CN119033180A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of clothing processing, in particular to a sewing method for high-density silk-wool worsted fabrics and clothing. Background Art
[0002] High-density silk-wool worsted fabrics are made of high-quality wool and mulberry silk. Through a special physical spinning process, they are very dense, thus achieving a high windproof and moisture-permeable effect. The wool fiber is pre-stretched and then spun, weaved, and the fabric shrinks greatly during the finishing process, thus producing a very high-density fabric. The fabric is wide and full, with a special feel, and is a very novel jacket windbreaker fabric. The warp density of the fabric usually reaches 390-470 strands / 10CM, and the weft density is 330-440 strands / 10CM. The fabric contains 80%-90% wool and 20%-10% silk. Worsted fabrics refer to fabrics made by spinning and weaving wool tops after combing. Combing is a process of combing wool.
[0003] Due to the extremely high density of the fabric, not only is it easy to produce wrinkles and unevenness at the seams, but it is also difficult to perform the pulling-back technique during ironing, so it is necessary to improve the sewing difficulty by adjusting the process details. For example, for this special fabric, it is necessary to specify the use of smooth long filament thread to reduce the resistance of the sewing machine needle when passing through the fabric. When sewing this kind of high-density fabric according to the conventional sewing machine pressure value, unevenness and wrinkles will occur at the seams, so for high-density fabrics, it is necessary to re-do the pressure test between the presser foot and the sewing panel. Patent CN109619739A discloses a plate making and sewing process for cashmere fabrics, and patent CN112522865B provides a control method for sewing equipment, but fails to solve the above problems. Summary of the invention
[0004] In view of the defects in the prior art, the object of the present invention is to provide a method for sewing high-density silk-wool worsted fabrics and clothing.
[0005] The sewing method of high-density silk-wool worsted fabric comprises the following steps:
[0006] Step S1, selecting high-density silk wool worsted fabric and selecting a rolling strip;
[0007] Step S2, cutting samples of clothing, cutting rolling strips, and selecting lining and pocket fabric;
[0008] Step S3, testing the presser foot pressure of the sewing machine;
[0009] Step S4, selecting the stitch lengths of the upper thread, the blind stitch thread and the overlock thread, and sewing the garment pieces with a flat sewing machine;
[0010] Step S5, rolling and polishing the inside of the sewn clothing;
[0011] Step S6, finishing the garments by ironing, inspecting the quality of the garments and verifying the size of the garments.
[0012] Preferably, in step S1, the composition of the high-density silk-wool worsted fabric is 80%-90% wool and 20%-10% silk, and the warp density of the fabric is 390-470 strands / 10CM, and the weft density is 330-440 strands / 10CM;
[0013] The composition of the tapered strip is 100% silk, and the tapered strip uses 12MM or 16MM double crepe (silk fabric with crepes on both sides) tapered strip.
[0014] Preferably, in step S2, the roll is cut into a 12MM (12 momme) double crepe roll with a slope of 15°-75° (the angle of the long side of the roll relative to the horizontal line) and a width of 3CM;
[0015] The pocket cloth is made of 40S (yarn count) organic cotton.
[0016] Preferably, in step S3, the method for testing the presser foot pressure of the sewing machine comprises the following steps:
[0017] Step N1, placing two test fabrics on a pressure plate of a sewing machine;
[0018] Step N2, placing a piece of A4 paper between the two test fabrics;
[0019] Step N3, pulling off the A4 paper with a set pulling force;
[0020] Step N4, the pressure level is displayed on the sewing machine.
[0021] Preferably, in step S4, the needle distance of the upper thread is 3CM, 11-12 needles, that is, 11-12 stitches are set within a length of 3CM, and the material is 50S or 60S long filament thread;
[0022] The stitch length of the blind stitch (the distance between stitches in the blind stitch process) is 3CM, 12-13 stitches, and the material is 50S or 60S long silk thread;
[0023] The material of the overlock thread is 50S or 60S long filament thread.
[0024] Preferably, in step S5, the internal piping structure adopts an open seam piping or a reverse seam piping. The open seam piping irons the seam between two pieces of fabric into an open seam, and wraps the raw edges of the seam with cloth strips on both sides of the seam. The reverse seam piping irons the seam between two pieces of fabric into a guide side, and wraps the raw edges of the seam with cloth strips.
[0025] Preferably, in step S6, the garment is ironed by dry ironing without steam spraying.
[0026] Preferably, the cutting width D of the piping strip and the width B of the piping strip after sewing satisfy B*(N+1)=D, wherein N is the number of piping polishing layers.
[0027] Compared with the prior art, the present invention has the following beneficial effects:
[0028] 1. This application uses 60S long filament sewing thread, and adjusts the sewing force according to the specified method to solve the wrinkles and unevenness generated at the seam. 60S long filament thread can be used for high-density silk and wool worsted fabrics to reduce the resistance of the sewing machine needle when passing through the fabric.
[0029] 2. The present application uses the silk piping process to make the clothes more beautiful and light, because the silk fabric is relatively smooth and easy to stretch and twist during operation. The present application irons a very thin woven lining on the silk rolling strip to reduce the difficulty of operation. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Other features, objects and advantages of the present invention will become more apparent from the detailed description of non-limiting embodiments made with reference to the following drawings:
[0031] Figure 1 To sew the reverse side of the garment using the silk piping method;
[0032] Figure 2 It is a schematic diagram of the silk piping structure;
[0033] Figure 3 This is a schematic diagram of the pressure test of a sewing machine;
[0034] Figure 4 Schematic diagram of the rolling bar structure;
[0035] As shown in the figure:
[0036] DETAILED DESCRIPTION
[0037] The present invention is described in detail below in conjunction with specific embodiments. The following embodiments will help those skilled in the art to further understand the present invention, but are not intended to limit the present invention in any form. It should be noted that, for those of ordinary skill in the art, several changes and improvements can also be made without departing from the concept of the present invention. These all belong to the protection scope of the present invention.
[0038] Example 1
[0039] like Figure 1-4 As shown, this embodiment includes the following steps:
[0040] Step 1. Choose high-density silk-wool worsted fabric: High-density silk-wool worsted fabric is made of high-quality wool and mulberry silk. It is made very dense through a special physical spinning process, thus achieving a high windproof and moisture-permeable effect. The wool fiber is pre-stretched and then spun, weaved, and the fabric shrinks greatly during the finishing process, thus producing a very high-density fabric. The fabric is wide and full, with a special feel. It is a very novel jacket windbreaker fabric. The warp density of the fabric is 390-470 strands / 10CM, and the weft density is 330-440 strands / 10CM. The fabric contains 80%-90% wool and 20%-10% silk. Worsted fabric refers to the fabric made by spinning and weaving the wool tops after combing. Combing is a process of combing wool.
[0041] Step 2: Cut the sample of the garment and the roll strips. Cut the roll strips into 12MM double crepe roll strips with a slope of 15°-75° and a width of 3CM. The lining material is WT230, which is the name of a lining material provided by NITTOBO. This lining has a larger particle size and is smoother when used on fabrics with wool components. The pocket cloth is made of 40S organic cotton.
[0042] Step three, test the pressure of the presser foot of the sewing machine: place two test fabrics 1 on the pressure plate of the sewing machine; place an A4 paper 2 between the two test fabrics 1; pull off the A4 paper 2 with a set tension; the pressure size is displayed on the sewing machine pressure display 3, and the parameters of the pressure display 3 can be used as the processing parameters of the subsequent sewing machine for high-density silk and wool worsted fabrics. If the fabric changes, it can be set in the same way. The pressure regulator 201 of the sewing machine is a tool for adjusting the pressure between the presser foot and the sewing panel. The force of pulling off the white paper between the two layers of fabric is different when this value is different. When the value displayed on the pressure regulator 201 is larger, the downward pressure is smaller, and the pulling force of pulling off the white paper is smaller. Pulling off the A4 paper is a method based on the actual test of the sewing flatness between the fabrics. This embodiment quantifies this force, and the tension displayed by the dynamometer 5 when pulling the A4 paper is 11N, achieving the best sewing force.
[0043] Step 4. Use a flatbed sewing machine to sew garment pieces: select the stitch length and material of the upper thread, blind stitch thread and overlock thread. The stitch length of the upper thread is 3CM, 11-12 stitches, and the material is 50S or 60S long silk thread; the stitch length of the blind stitch thread is 3CM, 12-13 stitches, and the material is 50S or 60S long silk thread; the material of the overlock thread is 50S or 60S long silk thread.
[0044] Step 5: Roll the inside of the sewn garment to make it smoother. Figure 2 As shown, a 3CM wide oblique cloth strip rotated 45° with respect to the horizontal line is used to wrap the damaged edge of the fabric due to cutting.
[0045] The internal piping structure adopts an open seam piping 4 or a reverse seam piping. The open seam piping 4 irons the seam between two pieces of fabric into an open seam, and wraps the raw edges of the seam with cloth strips on both sides of the seam; the reverse seam piping irons the seam between two pieces of fabric into a guide side, and wraps the raw edges of the seam with cloth strips.
[0046] Step 6: Finish the garments by ironing, inspecting their quality and verifying their sizes. Dry ironing is used for garment ironing, and steam cannot be sprayed.
[0047] The cutting width D of the piping strip and the width B of the piping strip after sewing satisfy B*(N+1)=D, where N is the number of piping polishing layers. In one embodiment, D is 3CM, N is 4 layers, and B is 0.6CM.
[0048] Example 2
[0049] Example 2 is a preferred example of Example 1.
[0050] like Figure 1-4 As shown, this embodiment includes:
[0051] Step 1: Make special adjustments to the sewing machine presser foot strength;
[0052] Place two test fabrics 1 on the pressure plate of the sewing machine, and place an A4 paper 2 between the two test fabrics 1. Pull the paper 2 off with a certain pulling force. The pressure displayed on the sewing machine at this time will be used as the value of the corresponding fabric for subsequent processing.
[0053] Step 2: Use 60S long filament thread and flat car process to make the seams;
[0054] The preferred sewing thread is 60S filament thread, and the self-cut silk roll can be selected in various slopes and widths. The preferred width selected in this embodiment is 3CM and the slope is 45°. The calculation method of the width of the silk roll is: 0.6CM*(4+1)=3CM, 0.6CM represents the finished width of the roll, and multiplying by "4+1" means that the roll is finished with 4 layers. Since the width of the silk bias-cut fabric will become narrower after stretching, the width should be doubled.
[0055] The optimal choice for sewing thread density is: the surface thread stitch length is 3CM, 11-12 needles, and the blind stitch stitch length is 3CM, 12-13 needles.
[0056] Step 3: Use silk double crepe piping on the raw edges of the garment seams;
[0057] Silk double crepe piping can be used for other tight fabrics or stretch fabrics. If the clothing fabric is a stretch fabric, the piping can be adjusted to silk stretch double crepe, and the double crepe silk strands are changed to horizontal silk (the horizontal silk is perpendicular to the edge of the cloth). Because the horizontal silk of stretch double crepe has greater elasticity, it is suitable for piping stretch fabrics.
[0058] The best choice for rolling strips: 12MM double crepe with a 45° slope and 3CM width. Rolling strips of other angles and widths are also applicable, with the best angle range of 15°-75°.
[0059] Step 4: During the finishing and ironing stage of the garment, use a dry iron and do not spray steam.
[0060] In the description of the present application, it should be understood that the terms "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0061] The above describes the specific embodiments of the present invention. It should be understood that the present invention is not limited to the above specific embodiments, and those skilled in the art can make various changes or modifications within the scope of the claims, which does not affect the essence of the present invention. In the absence of conflict, the embodiments of the present application and the features in the embodiments can be combined with each other arbitrarily.
Claims
1. A method for sewing high-density silk-wool worsted fabrics, characterized in that: The following steps are involved: Step S1, selecting high-density silk wool worsted fabric and selecting a rolling strip; Step S2, cutting samples of clothing, cutting rolling strips, and selecting lining and pocket fabric; Step S3, testing the presser foot pressure of the sewing machine and determining the parameters of the sewing machine pressure display (3); Step S4, selecting the stitch length and material of the upper thread, the blind stitch thread and the overlock thread, and sewing the garment pieces with a flat sewing machine; Step S5, rolling and polishing the inside of the sewn clothing; Step S6, finishing the garments by ironing, inspecting the quality of the garments and verifying the size of the garments.
2. The method for sewing high-density silk-wool worsted fabric according to claim 1, characterized in that: In step S1, the warp density of the high-density silk-wool worsted fabric is 390-470 strands / 10CM, and the weft density is 330-440 strands / 10CM, and the high-density silk-wool worsted fabric contains 80%-90% wool and 20%-10% silk; The composition of the tape is 100% silk, and the tape uses 12MM or 16MM double crepe tape.
3. The method for sewing high-density silk-wool worsted fabric according to claim 1, characterized in that: In step S2, the rolling strip is cut into a 12MM double crepe rolling strip with a slope of 15°-75° and a width of 3CM; The pocket cloth is made of 40S organic cotton.
4. The method for sewing high-density silk-wool worsted fabric according to claim 1, characterized in that: In step S3, the method for testing the presser foot pressure of the sewing machine includes the following steps: Step N1, placing two test fabrics (1) on a pressure plate of a sewing machine; Step N2, placing a piece of A4 paper (2) between the two test fabrics (1); Step N3, pulling off the A4 paper (2) with a set pulling force using a force gauge (5); Step N4, the pressure value is displayed on the pressure display (3) of the sewing machine, and the pressure value of the pressure display (3) at this time is set as the pressure parameter of the sewing machine.
5. The method for sewing high-density silk-wool worsted fabric according to claim 1, characterized in that: In step S4, the needle length of the upper thread is 3CM, 11-12 needles, and the material is 50S or 60S long silk thread; The stitch length parameter of the blind stitch is to set 11-12 stitches within a length of 3CM, and the material is 50S or 60S long silk thread; The material of the overlock thread is 50S or 60S long filament thread.
6. The method for sewing high-density silk-wool worsted fabric according to claim 1, characterized in that: In step S5, the internal piping structure adopts open seam piping (4) or reverse seam piping.
7. The method for sewing high-density silk-wool worsted fabric according to claim 1, characterized in that: In step S6, the garment is ironed using dry ironing.
8. The method for sewing high-density silk-wool worsted fabric according to claim 3, characterized in that: The cutting width D of the piping strip and the width B of the piping strip after sewing satisfy B*(N+1)=D, wherein N is the number of piping polishing layers.
9. A garment, characterized in that: The high-density silk-wool worsted fabric is made by the sewing method of any one of claims 1 to 8.
Citation Information
Cited By
Liquid phase treatment method and device for welt for heat-proof sewing of high-density fabric