Combined machining system and method combining flat-top laser and normal-temperature plasma

Through the composite processing system combining flat top laser with room temperature plasma, the problems of low surface pretreatment efficiency and poor activation effect of CFRP are solved, and efficient and uniform surface modification and adhesion enhancement are achieved, which is suitable for industrial application of composite materials.

CN119035780APending Publication Date: 2024-11-29SCI & TECH INNOVATION RES CENT OF UNIT 32178 OF THE CHINESE PEOPLES LIBERATION ARMY +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410942147.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The existing CFRP surface pretreatment methods have problems such as low efficiency, poor activation effect, large thermal effect, damage to the surface structure and limited processing accuracy. It is especially difficult to achieve uniform removal and efficient modification in the heterogeneous material treatment of fibers and resins. sex.

Method used

A composite processing system that combines flat top laser with room temperature plasma is used to micro-nano treatment through ultraviolet picosecond laser to form a surface microstructure, and a plasma machine is used to activate chemical bonds to improve surface roughness and adhesion, combining automated control and smoke. Gas purification device to achieve efficient surface treatment.

Benefits of technology

It improves the efficiency and quality of CFRP surface treatment, enhances the surface activation effect, reduces fiber damage, achieves more uniform surface modification and higher adhesion, and is suitable for industrial applications of composite materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119035780A_ABST
    Figure CN119035780A_ABST
Patent Text Reader

Abstract

The invention provides a combined machining system and method combining flat-top laser and normal-temperature plasma. The processing system is composed of an auxiliary displacement platform, a purple picosecond laser, an energy meter, a first test total reflection mirror, a second test total reflection mirror, a light beam quality analyzer, a beam expander, a light beam shaper, a light beam adjusting device, an auxiliary displacement platform and a plasma machine. The invention further provides a method for carrying out multi-system laser processing by adopting the system. According to the processing system and the processing method provided by the invention, the problems of poor effect, fiber damage, relatively low efficiency and poor activation effect when a single Gaussian laser or a single plasma is used for treating the surface of the composite material can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of composite material processing, and specifically relates to a composite processing system and method combining flat-top laser and room-temperature plasma, which is a composite surface treatment method for carbon fiber composite materials using high-energy processing and high-activation plasma combination. Background Art

[0002] Carbon fiber composite material (CFRP, Carbon Fiber Reinforced Polymer / Plastic) is a composite material with resin as the matrix and carbon fiber as the reinforcement. Compared with traditional metal materials, carbon fiber reinforced resin-based composite materials have a series of excellent properties such as high specific strength, high specific modulus, corrosion resistance, fatigue resistance, and easy conductivity. It is widely used as a lightweight material in aerospace, automobile, wind power, construction, sporting goods, civil engineering and other fields.

[0003] CFRP has many advantages, but it also has disadvantages such as low compressive strength and low low temperature resistance. In most application areas, CFRP needs to be combined with composite materials or metals to build a complete structure. The traditional mechanical connection (such as riveting and bolting) between CFRP and other material joints will not only reduce the static strength of the joint but also increase the load on the material. Therefore, adhesive bonding as a new means can disperse the force to the entire connection surface, thereby reducing stress concentration, which is beneficial to improve the durability and bearing capacity of the connection. Secondly, adhesive bonding can form a uniform distribution on the connection surface, improve the accuracy of the connection surface and reduce corrosion on the connection surface, thereby improving the quality of the connection. The simple adhesive operation can disperse the force to the entire connection surface, thereby reducing stress concentration, which is beneficial to improve the durability and bearing capacity of the connection.

[0004] The surface of CFRP is covered with a layer of highly crystalline polymer resin, which is usually hydrophobic, so it is difficult for adhesives to adhere and form a strong bond. Therefore, before painting or bonding, the CFRP surface needs to be pretreated to remove various surface dirt and increase surface energy, making it more conducive to adhesion, thereby improving quality and reliability. At present, chemical treatment, mechanical grinding and other methods are generally used to treat the surface of CFRP and metal to remove residual impurities on the surface, increase activation energy, and increase surface roughness, but these methods have the disadvantages of large pollution, low efficiency, and uneven surface treatment. Laser connection technology is a connection technology that has developed very rapidly in recent years. Due to its small heat input, high precision, simple operation, and high efficiency, it can enhance the roughness and fine surface activity of the CFRP surface. It is very suitable for processing the surface of composite materials, filling the shortcomings of traditional processing technology, and has a very broad application prospect.

[0005] When using picosecond lasers to microprocess CFRP, the laser pulse duration is much shorter than the electron-lattice energy coupling and heat conduction time scale of the material lattice (10 -11 -10 -12 seconds). During this time, the material lattice motion and thermal diffusion can be ignored. The material will undergo an instantaneous non-thermal optical phase change process. The laser energy has not yet completely propagated and diffused to the surrounding area, and the plasma has been formed and ejected from the surface, thereby effectively reducing the impact of thermal effects on the surface structure and improving the processing quality. However, due to the heterogeneity of the fiber and polymer distribution of the CFRP composite material itself, the energy absorption and processing effect of ultra-high density laser pulses in different areas may be different. Under Gaussian conditions, the carbon fibers may be exposed in the edge area of ​​the polymer due to the polymer removal reaction, and it is easy to cause great damage to the fibers. In addition, too long a pretreatment time will also reduce the processing efficiency and easily damage the surface activation effect.

[0006] Plasma machines have advantages such as excellent activation effect and strong timeliness, but they also have the following problems: ① The treatment temperature is difficult to control. The temperature generated by plasma treatment is high and difficult to measure directly, and it is difficult to ensure that the surface is in the temperature range of activation rather than damage. ② Excessive temperature can easily lead to damage to the surface structure of CFRP. ③ The surface morphology is difficult to control precisely. When the power of the plasma modification effect is too high, it is easy to become a random modification, and it is difficult to form a regular nanoscale surface structure, making it difficult to clearly improve the surface performance. ④ The treatment range is limited. The depth and width of plasma modification are difficult to exceed several millimeters, and it is impossible to achieve consistent modification inside the composite material or in large areas. ⑤ Secondary damage is easy to occur. Long-term exposure to high temperature and plasma may cause secondary damage such as thermal disintegration and decarburization of pre-impregnation.

[0007] The different physical properties of fiber, heat, light, etc. between fiber and resin make it difficult to remove the resin uniformly at the microscopic scale, although the surface treatment effect is excellent when the treatment process acts on both fiber and matrix at the same time, resulting in processing damage, limited processing accuracy, etc. With the gradual improvement of industrialization, various industries have more stringent requirements for processing.

[0008] Therefore, developing a technology that can overcome the shortcomings of existing CFRP surface pretreatment methods has become an urgent problem to be solved. Summary of the invention

[0009] In order to solve the above problems, the purpose of the present invention is to provide a composite processing system combining flat-top laser and room-temperature plasma. The system uses laser thermal coupling to enhance the micro-nano processing of composite materials, which can solve the problems of poor effect, low efficiency and poor activation effect when a single pulse width laser is used to treat the surface of composite materials, as well as poor etching and poor effect when a single plasma is used to treat the surface of composite materials.

[0010] Another object of the present invention is to provide a composite processing method combining flat-top laser and room temperature plasma.

[0011] In order to achieve the above-mentioned purpose, the present invention provides a composite processing system combining flat-top laser and room-temperature plasma, which consists of a master control platform, an ultraviolet picosecond laser, an energy meter, a first test total reflection mirror, a beam expander, a beam shaper, a second test total reflection mirror, a beam quality analyzer, a first total reflection mirror, a second total reflection mirror, a beam adjustment device, a flue gas purification device, an auxiliary displacement platform, an automatic zoom three-dimensional surface profiler, a plasma machine controller, a plasma injection head, and an XYZ three-axis automated mobile platform;

[0012] The energy meter has a first detection head;

[0013] The beam quality analyzer is provided with a second detection head;

[0014] The master control platform is wirelessly connected to the ultraviolet picosecond laser and the beam adjustment device;

[0015] The first test total reflection mirror is detachably arranged on the laser light path emitted by the ultraviolet picosecond laser, and the mirror surface of the first test total reflection mirror is inclined at 45° toward the ultraviolet picosecond laser; the first detection head of the energy meter is arranged on the light path of the laser emitted by the ultraviolet picosecond laser reflected by the first test total reflection mirror, so that the first detection head receives the energy signal of the laser emitted by the ultraviolet picosecond laser;

[0016] The beam expander, the beam shaper, the second test total reflector, and the first total reflector are sequentially arranged behind the first test total reflector on the laser light path emitted by the ultraviolet picosecond laser; wherein the second test total reflector is detachably arranged, and the mirror surface of the second test total reflector is inclined at 45° toward the ultraviolet picosecond laser;

[0017] The second detection head of the beam quality analyzer is arranged on the optical path of the laser emitted by the ultraviolet picosecond laser optical path and reflected by the second testing total reflection mirror, so that the second detection head receives the energy signal of the laser emitted by the ultraviolet picosecond laser optical path;

[0018] The mirror surface of the first total reflection mirror is inclined at 45° toward the ultraviolet picosecond laser;

[0019] The second total reflection mirror is arranged on the reflection light path of the first total reflection mirror, and the mirror surface of the second total reflection mirror is opposite to and parallel to the mirror surface of the first total reflection mirror;

[0020] A beam adjustment device and an auxiliary displacement platform are arranged on the reflection light path of the second total reflection mirror;

[0021] The light beam adjustment device comprises a scanning galvanometer and a field mirror located on the reflection light path of the second total reflection mirror;

[0022] The auxiliary displacement platform is used to fix the target material, and the target material is irradiated by the laser after passing through the field lens;

[0023] The auxiliary displacement platform is used to fix the target material on one side of which a fume purification device is arranged;

[0024] The plasma machine is composed of a plasma generator host, a flexible conduit, a jet plasma spray gun, and an XYZ three-axis automated mobile platform; the plasma generator host is connected to the jet plasma spray gun through the flexible conduit, the jet plasma spray gun is arranged on a bracket located above the XYZ three-axis automated mobile platform, and the jet port of the jet plasma spray gun points to the XYZ three-axis automated mobile platform; the XYZ three-axis automated mobile platform is used to fix the target material;

[0025] The automatic zoom three-dimensional surface measuring instrument is used for scanning the surface topography of a target material, and the target material is transferred to the automatic zoom three-dimensional surface measuring instrument during scanning.

[0026] As described above, the output power of the ultraviolet picosecond laser is 5-30W, the frequency of the ultraviolet laser emitted by the ultraviolet picosecond laser is 200-1000kHz, and the spot diameter is 20-50μm.

[0027] As described above, the plasma machine controller has a plasma machine power of 0 to 800 W, a scanning speed of 0.01 to 1 m / s, and a frequency of 20 kHz.

[0028] As mentioned above, the master control platform is a computer or a tablet computer.

[0029] The present invention also provides a composite processing method using the above system, characterized in that it comprises the following steps:

[0030] 1) Ultrasonic cleaning is performed on the surface of the target material, and then the target material to be processed is fixed on the auxiliary displacement platform;

[0031] 2) adjusting the working position of the ultraviolet picosecond laser, turning on the laser indicator light of the ultraviolet picosecond laser, so that the laser emitted by the ultraviolet picosecond laser irradiates the first test total reflection mirror and is reflected to the first detection head, and the laser signal is collected by the energy meter to measure the laser power;

[0032] 3) disassembling the first test total reflector, allowing the laser emitted by the ultraviolet picosecond laser to be expanded through a beam expander, and the Gaussian spot after the expansion is vertically incident into the beam shaper;

[0033] 4) The Gaussian spot incident on the beam shaper is converted into a flat-top laser through the beam shaper, and then passes through the second test total reflection mirror and is incident on the second detection head. The laser signal is collected by the beam quality analyzer to determine whether the spot is converted from Gaussian laser to flat-top laser and the beam quality test;

[0034] 5) disassembling the second test total reflection mirror, so that the laser light emitted by the ultraviolet picosecond laser is reflected by the first total reflection mirror to the second reflection mirror, and finally vertically incident into the beam adjustment device;

[0035] 6) The laser passes through the scanning galvanometer and field mirror in the beam adjustment device, and the output indicator light is irradiated on the surface of the target material. The beam adjustment device is controlled and adjusted through the master control platform, and the optical path is accurately focused so that the brightness of the light spot acting on the target material is maximized; then observe whether the beam and the beam adjustment device have polarization or light leakage. After ensuring that there is no polarization or light leakage, turn off the ultraviolet picosecond laser to complete the laser preparation;

[0036] 7) Run the plasma machine, check whether the plasma machine jet and the XYZ three-axis automated moving platform are operating normally, ensure that the action time and displacement distance are normal, then turn off the plasma machine and complete the preparation of the plasma machine;

[0037] 8) Turn on the switch of the UV picosecond laser, wait for the UV picosecond laser to be preheated, and then start the plasma machine to preheat;

[0038] 9) Set the parameters of the ultraviolet picosecond laser as follows: laser output wavelength 355nm, pulse width 10ps, repetition rate 200-2000kHz, output power 1-30W; spot diameter 20-50μm.

[0039] 10) The picosecond laser output by the ultraviolet picosecond laser passes through the first total reflection mirror and the second total reflection mirror, and is incident on the beam adjustment device. The laser passes through the beam adjustment device including the scanning galvanometer and the field mirror to complete the adjustment of the laser;

[0040] 11) The adjusted laser beam is irradiated on the surface of the target material for processing and marking; at the same time, the smoke and fog generated during the processing and marking process are absorbed by the smoke purification system, the beam adjustment device is adjusted by the master control platform, and the position of the target material is adjusted by the auxiliary displacement platform; the depth, roughness and surface morphology of the target material surface are observed and data is collected by using an automatic zoom three-dimensional surface measuring instrument, and input into the master control platform for analysis;

[0041] 12) Further feedback adjustment is performed according to the analysis results of the master control platform: Steps 7) to 10) are repeated to achieve the best treatment effect and the highest treatment efficiency on the target surface;

[0042] 13) Then, the target material after the surface etching after the laser action is completed is moved to the XYZ three-axis automated moving platform;

[0043] 14) Operate the plasma machine controller, set the corresponding scanning area and parameters, the plasma machine power is 0-800W, and the scanning speed is 0.5m / s.

[0044] The present invention has the following characteristics:

[0045] The present invention realizes more efficient surface treatment. An ultraviolet picosecond laser with a wavelength of 355nm is combined with a room-temperature plasma. The output adopts a flat-top laser to irradiate the surface of the composite material, so that the material on the surface of the composite material melts or vaporizes. Then, the surface is treated with plasma to achieve an efficient treatment effect.

[0046] The present invention achieves high surface performance. The ultraviolet picosecond laser first removes the resin on the composite material, and melts, vaporizes and solidifies the material through the picosecond laser high-energy laser pulse to form a surface microstructure to make the material surface rough. Subsequently, the material surface is further roughened by a plasma machine to further improve the surface quality and performance.

[0047] The plasma generated by the plasma machine in the present invention has an activation effect on the surface of the composite material, which can activate the chemical bonds on the surface of the material, increase the surface roughness, thereby increasing the surface energy, enhancing the adhesion and wettability of the material, and making it more suitable for applications such as surface coating and bonding. This treatment method has higher efficiency than the traditional single laser surface cleaning method, thereby improving the surface quality and performance.

[0048] The beneficial effects of the present invention are:

[0049] The present invention provides a composite processing system and processing method combining flat-top laser and room-temperature plasma. The system can produce micro-nano morphology through laser and render with plasma to increase activity, thereby solving the problems of poor surface treatment effect, large fiber damage, low efficiency and poor activation effect of composite materials with single Gaussian laser or single plasma. BRIEF DESCRIPTION OF THE DRAWINGS

[0050] Figure 1 This is a schematic structural diagram of a composite processing system combining flat-top laser and room-temperature plasma provided by the present invention.

[0051] Figure 2 Surface morphology of a CFRP target material after being processed by an ultraviolet picosecond laser in the composite processing system combining flat-top laser and room-temperature plasma provided by the present invention; wherein (A) has a laser power of 6 W; (B) has a laser power of 8 W; (C) has a laser power of 10 W; and (D) has a laser power of 12 W.

[0052] Figure 3 This is the original morphology of the CFRP target material surface that has not been processed.

[0053] Figure 4A Schematic diagram of CFRP three-dimensional morphology, depth measurement and surface roughness (Ra, Sa) using plasma, where the plasma power is 800W, the scanning speed is 0.5m / s, and the number of scans is 10.

[0054] Figure 4B for Figure 4A Depth measurement graph in .

[0055] Figure 5A Schematic diagram of the three-dimensional morphology, depth measurement and surface roughness (Ra, Sa) of CFRP treated with ultraviolet picosecond laser, where the laser power is 6W, the scanning speed is 1m / s, and the number of scans is 2.

[0056] Figure 5B for Figure 5A Depth measurement graph in .

[0057] Fig. 6A A surface morphology image of the CFRP surface treated by a composite processing method of plasma activation followed by ultraviolet flat-top picosecond laser etching in the composite processing system combining flat-top laser and room temperature plasma provided by the present invention, wherein the parameters are laser power 10W, scanning speed 1m / s, number of scans 2, and margin spacing 0.11mm: plasma power 800W, scanning speed 0.5m / s, and number of scans 10.

[0058] Figure 6B for Fig. 6A Depth measurement graph in .

[0059] Reference numerals:

[0060] 1: The system consists of a master control platform; 2: UV picosecond laser; 3: energy meter; 31: first detector head; 4: first test total reflection mirror; 5: beam expander; 6: beam shaper; 7: second test total reflection mirror; 8: beam quality analyzer; 81: second detector head; 9: first total reflection mirror; 10: second total reflection mirror; 11: beam adjustment device; 111: scanning galvanometer; 112: field mirror; 12: flue gas purification device; 13: auxiliary displacement platform; 131: target material; 14: automatic zoom three-dimensional surface morphometer; 15: plasma machine controller; 16: plasma jet head; 17: XYZ three-axis automated moving platform; 18: flexible catheter. DETAILED DESCRIPTION

[0061] The embodiments of the present invention will be described in detail and comprehensively below so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present invention.

[0062] equipment:

[0063] 1. The master control platform is a computer and is equipped with the Jinchengzi board produced by Beijing Jinchengzi Technology Co., Ltd. and the corresponding control software that comes with the board.

[0064] 2. The UV picosecond laser was purchased from Beijing Shenglei Technology Co., Ltd. with the product number: leonis-355-30.

[0065] 3. The energy meter was purchased from Ophir, product number: 30A-BB-18.

[0066] 4. The beam quality analyzer was purchased from BEAMAGE-M2 / Beamage-4M, product number: Gentec-eoGXjg2022-20564

[0067] 5. The scanning galvanometer in the beam adjustment device was purchased from Anshan Precision Optical Scanning Technology Co., Ltd., product number: RAY-MOTION; the field mirror was purchased from Nanjing Wavelength Optoelectronics Technology Co., Ltd., product model: NJSL-427SL-355-110-160Q-D12.

[0068] 6. The flue gas purification device is a small desktop purifier purchased from Shenzhen Jiuyefeng Technology Co., Ltd.

[0069] 7. The auxiliary displacement platform was purchased from Beijing Fuliqintian Optoelectronics Technology Co., Ltd.

[0070] 8. The automatic zoom three-dimensional surface measuring instrument was purchased from Alicona, Austria, product number: InfiniteFocus G5.

[0071] 9. The plasma surface treatment machine was purchased from Taifengrui (Tianjin) Electronic Equipment Manufacturing Co., Ltd., product model: TFR02-PL-3500Z.

[0072] 10. The beam shaper was purchased from Adloptica, product number: Focal-πShaper_NVU-Q-5.

[0073] The present invention provides a composite processing system combining flat-top laser and room temperature plasma, such as Figure 1As shown, the system consists of a master control platform 1, an ultraviolet picosecond laser 2, an energy meter 3, a first test total reflector 4, a beam expander 5, a beam shaper 6, a second test total reflector 7, a beam quality analyzer 8, a first total reflector 9, a second total reflector 10, a beam adjustment device 11, a flue gas purification device 12, an auxiliary displacement platform 13, an automatic zoom three-dimensional surface profiler 14, a plasma machine controller 15, a plasma injection head 16, and an XYZ three-axis automated mobile platform 17.

[0074] The energy meter 3 has a first detection head 31;

[0075] The beam quality analyzer 8 has a second detection head 81;

[0076] The master control platform 1 is wirelessly connected to the ultraviolet picosecond laser 2 and the beam adjustment device 11; Figure 1 A short dashed line indicates a wireless connection;

[0077] The first test total reflection mirror 4 is detachably arranged on the optical path of the laser emitted by the ultraviolet picosecond laser 2, and the mirror surface of the first test total reflection mirror 4 is inclined at 45° toward the ultraviolet picosecond laser 2; the first detection head 31 of the energy meter 3 is arranged on the optical path of the laser emitted by the ultraviolet picosecond laser 2 reflected by the first test total reflection mirror 4, so that the first detection head 31 receives the energy signal of the laser emitted by the ultraviolet picosecond laser 2;

[0078] The beam expander 5, the beam shaper 6, the second test total reflection mirror 7, and the first total reflection mirror 9 are sequentially arranged behind the first test total reflection mirror 4 on the laser light path emitted by the ultraviolet picosecond laser 2; wherein the second test total reflection mirror 7 is detachably arranged, and the mirror surface of the second test total reflection mirror 7 is inclined at 45° toward the ultraviolet picosecond laser 2;

[0079] The second detection head 81 of the beam quality analyzer 8 is arranged on the optical path of the laser emitted by the optical path of the ultraviolet picosecond laser 2 and reflected by the second testing total reflection mirror 7, so that the second detection head 81 receives the energy signal of the laser emitted by the optical path of the ultraviolet picosecond laser 2;

[0080] The mirror surface of the first total reflection mirror 9 is inclined at 45° toward the ultraviolet picosecond laser 2;

[0081] The second total reflection mirror 10 is disposed on the reflection light path of the first total reflection mirror 9, and the mirror surface of the second total reflection mirror 10 is opposite to and parallel to the mirror surface of the first total reflection mirror 9;

[0082] A beam adjustment device 11 and an auxiliary displacement platform 13 are arranged on the reflection light path of the second total reflection mirror 10;

[0083] The beam adjustment device 11 includes a scanning galvanometer 111 and a field lens 112 located on the reflection light path of the second total reflection mirror 10;

[0084] The auxiliary displacement platform 13 is used to fix the target material 131, and the target material 131 is irradiated by the laser after passing through the field lens 112;

[0085] The auxiliary displacement platform 13 is used to fix the target material 131 on one side of which a flue gas purification device 12 is arranged;

[0086] The plasma machine is composed of a plasma generator host 15, a flexible conduit 18, a jet plasma spray gun 16, and an XYZ three-axis automated mobile platform 17; the plasma generator host 15 is connected to the jet plasma spray gun 16 through the flexible conduit 18, the jet plasma spray gun 16 is arranged above the XYZ three-axis automated mobile platform 17, and the jet port of the jet plasma spray gun 16 points to the XYZ three-axis automated mobile platform 17; the XYZ three-axis automated mobile platform 17 is used to fix the target material 131;

[0087] The automatic zoom three-dimensional surface measuring instrument 14 is used to scan the surface morphology of the target material 131; when the target material 131 fixed on the auxiliary displacement platform 13 or the XYZ three-axis automated moving platform 17 is moved to the automatic zoom three-dimensional surface measuring instrument 14 for scanning, it is determined whether the processing effect of the target material 131 meets the expectations. Figure 1 The dotted line in the figure indicates that the scanning object of the automatic zoom three-dimensional surface measuring instrument 14 is the target material 131, and the direction of the arrow indicates that the target material 131 is transferred to the automatic zoom three-dimensional surface measuring instrument 14 after laser irradiation to scan the three-dimensional morphology to see whether it meets the requirements. If it meets the requirements, it is transferred to the XYZ three-axis automated moving platform 17 for plasma injection.

[0088] Among them, the output power of the ultraviolet picosecond laser is 5-30W, the frequency of the ultraviolet laser emitted by the ultraviolet picosecond laser is 200-1000kHz, and the spot diameter is 20-50μm.

[0089] Among them, the plasma machine controller, plasma machine power 0 ~ 800W, scanning speed 0.01 ~ 1m / s, frequency is 20kHz.

[0090] Among them, the master control platform is a computer or tablet computer.

[0091] When a single UV picosecond laser is used to treat the surface of CFRP, the heating and melting process of CFRP is short during the treatment process, which is mainly affected by photophysical and photochemical effects. The photophysical effect: UV picosecond laser can generate high-intensity electromagnetic fields and localized plasmas through nonlinear optical effects, thereby achieving efficient removal of impurities, pollutants and resins on the surface of CFRP. Photochemical reaction: Under the irradiation of ultraviolet light, the chemical bonds on the surface of CFRP will break or reorganize, thereby achieving surface modification and modification. Therefore, in the process of UV picosecond laser treatment of CFRP, the etching is rapid and obvious, but the high energy of Gaussian laser is concentrated in a small area, which leads to the pursuit of high surface free energy. When the power is high, it is easy to cause greater damage. For example, fiber damage.

[0092] When the laser power is low (laser power 6W, repetition frequency 1000kHz, scanning number 2, spot diameter 30μm), the resin etching is not obvious, and the laser activation effect is also small. Figure 2 As shown in (A). When the laser power is further increased (laser power 8W, repetition frequency 1000kHz, scanning number 2, spot diameter 30μm), only part of the resin can be removed, exposing part of the carbon fiber, and the resin or contaminants on the surface of the resin-based composite material cannot be completely treated. The surface resin cannot be completely removed, and the fiber is not damaged. Figure 2 As shown in (B), when the laser power is gradually increased, after multiple scans (laser power 10W, repetition frequency 1000kHz, scanning number 8, spot diameter 19μm), a large amount of resin is removed and the surface is smooth and flat, as shown in Figure 2 As shown in (C), the laser power was further increased (laser power 13W, repetition frequency 1000kHz, scanning number 2, spot diameter 30μm), resulting in a large number of fiber damage, such as Figure 2 As shown in (D).

[0093] The measurement results of the original CFRP surface by a three-dimensional surface topography instrument show that the arithmetic average roughness (Ra) of the CFRP surface is 0.079μm, while the three-dimensional surface roughness (Sa) is 0.185μm. Figure 3 As shown, the surface roughness is low and cannot meet the bonding requirements.

[0094] Atmospheric pressure plasma jet is to apply high voltage to the gas introduced to ionize it, including excited electrons and atoms, molecules, and free radicals, which flow along the nozzle under the pressure of the gas to form a jet for surface modification. This gas ionization produces a large number of active particles, which collide with the polymer surface to cause a series of physical changes and chemical reactions, such as etching, cleaning, surface activation or cross-linking, etc., which can produce high-energy polar groups on the surface of the substrate and significantly improve the wettability and adhesion of the substrate. However, due to the atmospheric pressure plasma used, the temperature is relatively low, so the surface activity can be significantly improved when treating the CFRP surface. However, in terms of improving the surface roughness, three-dimensional morphology observation and roughness measurement using a laser confocal microscope found that no obvious changes were found in the surface morphology, such as Figure 4A Schematic diagram of the three-dimensional morphology of the CFRP surface after plasma treatment. Figure 4B The depth measurement curve is shown in Table 1. The surface roughness parameter analysis is shown in Table 1.

[0095] Table 1 Arithmetic mean roughness of CFRP surface

[0096]

[0097]

[0098] Note: Rp refers to the maximum peak height of the surface. Rv represents the minimum valley depth of the surface. Rz is the total vertical distance between peaks and valleys on the surface. Rc refers to the horizontal distance between the highest peak and the lowest valley within the measuring length. Rt represents the average vertical distance between peaks and valleys on the surface, which is the sum of all peak and valley heights divided by the measuring length. Ra is the average value of surface roughness, which represents the average of the absolute values ​​of all peak and valley heights within the measuring length. Rq is the root mean square value of surface roughness, which represents the average of the square roots of all peak and valley heights within the measuring length. Rsk is used to describe the distribution symmetry of surface peaks and valleys. Rku is used to describe the distribution shape of surface peaks and valleys. The above parameters are commonly used in engineering and manufacturing fields to evaluate surface quality, adaptability and processing performance.

[0099] Table 2 Three-dimensional surface roughness of CFRP surface

[0100]

[0101] As can be seen from Table 1, the arithmetic mean roughness (Ra) of the CFRP surface is 0.205, and as shown in Table 2, the three-dimensional surface roughness (Sa) of the CFRP surface is 1.237 μm. The improvement of the surface roughness is small, and thus the mechanical bonding or interlocking ability is weak.

[0102] For CFRP, the three-dimensional morphology of CFRP was scanned after Gaussian laser treatment (laser power 8W, repetition frequency 1000kHz, cross scanning mode, and interval distance 0.03mm). Figure 5A The figure shows the three-dimensional morphology of CFRP after step 13). Figure 5B Shown Figure 5A Table 3 shows the arithmetic mean roughness of CFRP, and Table 4 shows the three-dimensional surface roughness of CFRP.

[0103] Table 3 Arithmetic mean roughness of CFRP surface

[0104]

[0105] Table 4 Three-dimensional surface roughness of CFRP surface

[0106]

[0107]

[0108] from Figure 5A and Figure 5B As can be seen from Tables 3 and 4, after laser treatment, the arithmetic average roughness (Ra) of CFRP reaches 5.795 μm, and the three-dimensional surface roughness (Sa) reaches 7.904 μm.

[0109] Example 1

[0110] 1) Ultrasonic cleaning is performed on the surface of the target material, and then the target material to be processed is fixed on the auxiliary displacement platform;

[0111] 2) adjusting the working position of the ultraviolet picosecond laser, turning on the laser indicator light of the ultraviolet picosecond laser, so that the laser emitted by the ultraviolet picosecond laser irradiates the first test total reflection mirror and is reflected to the first detection head, and the laser signal is collected by the energy meter to measure the laser power;

[0112] 3) The first test total reflector is disassembled, so that the laser emitted by the ultraviolet picosecond laser is normally expanded by the beam expander, and the light spot after the expansion is incident into the beam shaper;

[0113] 4) The Gaussian spot incident on the beam shaper is converted into a flat-top laser by the beam shaper, and then passes through the second test total reflection mirror and is incident on the second detection head. The laser signal is collected by the beam quality analyzer to determine whether the spot is converted from Gaussian laser to flat-top laser and the beam quality;

[0114] 5) disassembling the second test total reflection mirror, so that the laser light emitted by the ultraviolet picosecond laser is normally reflected by the first total reflection mirror to the second reflection mirror, and finally vertically incident into the beam adjustment device;

[0115] 6) The light beam passes through the scanning galvanometer and field mirror in the beam adjustment device, and the output indicator light is irradiated on the surface of the target material. The beam adjustment device is controlled and adjusted through the master control platform, and the optical path is accurately focused so that the brightness of the light spot acting on the target material is maximized; then observe whether the light beam and the beam adjustment device have polarization or light leakage. After ensuring that there is no polarization or light leakage, turn off the ultraviolet picosecond laser and complete the laser preparation;

[0116] 7) Run the plasma machine, check whether the plasma machine jet and the XYZ three-axis automated moving platform are operating normally, ensure that the action time and displacement distance are normal, then turn off the plasma machine and complete the preparation of the plasma machine;

[0117] 8) Turn on the switch of the UV picosecond laser and the beam modulator, wait for the laser to finish running, and start the plasma machine to preheat;

[0118] 9) The parameters of the ultraviolet picosecond laser are set as follows: laser output wavelength 355nm, pulse width 10ps, repetition rate 200-2000kHz, output power 1-30W; spot diameter 20-50μm, scanning mode U-shaped filling, margin spacing 0.5-0.2mm.

[0119] 10) The picosecond laser output by the ultraviolet picosecond laser passes through the first total reflection mirror and the second total reflection mirror, and is incident on the beam adjustment device. The laser passes through the beam adjustment device including the scanning galvanometer and the field mirror to complete the adjustment of the laser;

[0120] 11) The adjusted combined laser beam is irradiated on the target surface for processing and marking; at the same time, the smoke and fog generated during the processing and marking process are absorbed by the smoke purification system, the beam adjustment device is adjusted by the master control platform, and the position of the target is adjusted by the auxiliary displacement platform; the depth, roughness and surface morphology of the target surface are observed and data is collected and analyzed by the automatic zoom three-dimensional surface measuring instrument;

[0121] 12) Further feedback adjustment is performed based on the analysis results of the master control platform: Steps 9) to 11) are repeated to achieve the best treatment effect and the highest treatment efficiency on the target surface.

[0122] 13) The target material after surface etching after the laser action is completed is then moved to the XYZ three-axis automated moving platform.

[0123] 14) Operate the plasma machine controller, set the corresponding scanning area and parameters, plasma machine power 0 ~ 800W, scanning speed 0.1 ~ 1m / s.

[0124] 15) Further feedback adjustment is performed based on the analysis results: step 14) is repeated to achieve the best treatment effect and the highest treatment efficiency on the target surface.

[0125] 16) Laser power 10W, scanning speed 1m / s, number of scans 2, margin distance 0.11mm: plasma power 800W, scanning speed 0.5m / s, number of scans 10.

[0126] The processed CFRP target is scanned, where Fig. 6A is a schematic diagram of the three-dimensional morphology of CFRP. Figure 6B Shown Fig. 6A Table 5 shows the arithmetic mean roughness of CFRP, and Table 6 shows the three-dimensional surface roughness of CFRP.

[0127] Table 5 Arithmetic mean roughness of CFRP surface

[0128]

[0129]

[0130] Table 6 Three-dimensional surface roughness of CFRP surface

[0131]

[0132] like Figure 5B As shown in the figure, it can be seen that the single action area of ​​​​the Gaussian is about 10 to 20μm. Figure 6B As shown in the figure, the path width and the action area of ​​the CFRP after the flat-top laser deformation by the beam shaper are larger and more uniform. Subsequently, through further activation of the plasma, the action area is further expanded to 150-200 μm. The grooves of this structure can better and more absorb glue and improve the shear strength. Compared with Tables 1 and 2, which are only rendered by plasma, Tables 5 and 6 show that the surface roughness has been effectively improved.

[0133] The treated samples were bonded and a composite material-composite material tensile shear strength test was conducted according to GB / T 33334-2016. After composite processing, the average tensile shear strength of the original CFRP without surface treatment increased from 4.3MPa to 12.3MPa, an increase of 280%.

[0134] As can be seen from the above embodiments, the present invention provides a composite processing system and method combining flat-top laser and room temperature plasma, wherein the ultraviolet picosecond laser processing uses extremely short laser pulses (picosecond level) to efficiently transfer energy to the surface of carbon fiber reinforced polymer (CFRP). This treatment mainly affects the surface layer of the material through a non-thermal mechanism. The high energy of the light beam causes the chemical bonds in the resin to break rapidly and vaporize locally without significantly increasing the overall temperature of the material, thereby minimizing thermal damage. By precisely controlling the laser parameters, specific micro-nano structures can be formed on the surface of the CFRP to increase the surface roughness. Picosecond lasers provide enhanced surface activation effects by physically changing the surface structure of the material, such as adding micro-nano structures, and are suitable for high-performance applications that require precise control. Plasma provides rapid and uniform surface activation through chemical modification, but has less effect on surface roughness and is more suitable for large-scale production environments.

[0135] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0136] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A composite processing system combining flat-top laser and room temperature plasma, characterized in that: The system consists of a master control platform, an ultraviolet picosecond laser, an energy meter, a first test total reflector, a beam expander, a beam shaper, a second test total reflector, a beam quality analyzer, a first total reflector, a second total reflector, a beam adjustment device, a flue gas purification device, an auxiliary displacement platform, and a plasma machine; The energy meter has a first detection head; The beam quality analyzer is provided with a second detection head; The master control platform is wirelessly connected to the ultraviolet picosecond laser and the beam adjustment device; The first test total reflection mirror is detachably arranged on the laser light path emitted by the ultraviolet picosecond laser, and the mirror surface of the first test total reflection mirror is inclined at 45° toward the ultraviolet picosecond laser; the first detection head of the energy meter is arranged on the light path of the laser emitted by the ultraviolet picosecond laser reflected by the first test total reflection mirror, so that the first detection head receives the energy signal of the laser emitted by the ultraviolet picosecond laser; The beam expander, the beam shaper, the second test total reflector, and the first total reflector are sequentially arranged behind the first test total reflector on the laser light path emitted by the ultraviolet picosecond laser; wherein the second test total reflector is detachably arranged, and the mirror surface of the second test total reflector is inclined at 45° toward the ultraviolet picosecond laser; The second detection head of the beam quality analyzer is arranged on the optical path of the laser emitted by the ultraviolet picosecond laser optical path and reflected by the second testing total reflection mirror, so that the second detection head receives the energy signal of the laser emitted by the ultraviolet picosecond laser optical path; The mirror surface of the first total reflection mirror is inclined at 45° toward the ultraviolet picosecond laser; The second total reflection mirror is arranged on the reflection light path of the first total reflection mirror, and the mirror surface of the second total reflection mirror is opposite to and parallel to the mirror surface of the first total reflection mirror; A beam adjustment device and an auxiliary displacement platform are arranged on the reflection light path of the second total reflection mirror; The light beam adjustment device comprises a scanning galvanometer and a field mirror located on the reflection light path of the second total reflection mirror; The auxiliary displacement platform is used to fix the target material, and the target material is irradiated by the laser after passing through the field lens; The auxiliary displacement platform is used to fix the target material on one side of which a fume purification device is arranged; The plasma machine is composed of a plasma generator host, a flexible conduit, a jet-type plasma spray gun, and an XYZ three-axis automated mobile platform; the plasma generator host is connected to the jet-type plasma spray gun through the flexible conduit, the jet-type plasma spray gun is arranged on a bracket located above the XYZ three-axis automated mobile platform, and the jet port of the jet-type plasma spray gun points to the XYZ three-axis automated mobile platform; the XYZ three-axis automated mobile platform is used to fix the target material; The automatic zoom three-dimensional surface measuring instrument is used to scan the surface morphology of a target material.

2. The composite processing system combining flat-top laser and room temperature plasma as claimed in claim 1, characterized in that: The output power of the ultraviolet picosecond laser is 5-30W, the frequency of the ultraviolet laser emitted by the ultraviolet picosecond laser is 200-1000kHz, and the spot diameter is 20-50μm.

3. The composite processing system combining flat-top laser and room temperature plasma as claimed in claim 1, characterized in that: The plasma machine controller has a plasma machine power of 0 to 800 W, a scanning speed of 0.01 to 1 m / s, and a frequency of 20 kHz.

4. The composite processing system combining flat-top laser and room temperature plasma as claimed in claim 1, characterized in that: The master control platform is a computer or a tablet computer.

5. A composite processing method using the system according to any one of claims 1 to 4, characterized in that: The steps include: 1) Ultrasonic cleaning is performed on the surface of the target material, and then the target material to be processed is fixed on the auxiliary displacement platform; 2) adjusting the working position of the ultraviolet picosecond laser, turning on the laser indicator light of the ultraviolet picosecond laser, so that the laser emitted by the ultraviolet picosecond laser irradiates the first test total reflection mirror and is reflected to the first detection head, and the laser signal is collected by the energy meter to measure the laser power; 3) disassembling the first test total reflector, allowing the laser emitted by the ultraviolet picosecond laser to be expanded through a beam expander, and the Gaussian spot after the expansion is vertically incident into the beam shaper; 4) The Gaussian spot incident on the beam shaper is converted into a flat-top laser through the beam shaper, and then passes through the second test total reflection mirror and is incident on the second detection head. The laser signal is collected by the beam quality analyzer to determine whether the spot is converted from Gaussian laser to flat-top laser and the beam quality; 5) disassembling the second test total reflection mirror, so that the laser light emitted by the ultraviolet picosecond laser is reflected by the first total reflection mirror to the second reflection mirror, and finally vertically incident into the beam adjustment device; 6) The laser passes through the scanning galvanometer and field mirror in the beam adjustment device, and the output indicator light is irradiated on the surface of the target material. The beam adjustment device is controlled and adjusted through the master control platform, and the optical path is accurately focused so that the brightness of the light spot acting on the target material is maximized; then observe whether the beam and the beam adjustment device have polarization or light leakage. After ensuring that there is no polarization or light leakage, turn off the ultraviolet picosecond laser to complete the laser preparation; 7) Run the plasma machine, check whether the plasma machine jet and the XYZ three-axis automated moving platform are operating normally, ensure that the action time and displacement distance are normal, then turn off the plasma machine and complete the preparation of the plasma machine; 8) Turn on the switch of the UV picosecond laser, wait for the UV picosecond laser to be preheated, and start the plasma machine to preheat; 9) Setting the parameters of the ultraviolet picosecond laser as follows: laser output wavelength 355nm, pulse width 10ps, repetition rate 200-2000kHz, output power 1-30W; spot diameter 20-50μm; 10) The picosecond laser output by the ultraviolet picosecond laser passes through the first total reflection mirror and the second total reflection mirror, and is incident on the beam adjustment device. The laser passes through the beam adjustment device including the scanning galvanometer and the field mirror to complete the adjustment of the laser; 11) The adjusted laser beam is irradiated on the surface of the target material for processing and marking; at the same time, the smoke and fog generated during the processing and marking process are absorbed by the smoke purification system, the beam adjustment device is adjusted by the master control platform, and the position of the target material is adjusted by the auxiliary displacement platform; the depth, roughness and surface morphology of the target material surface are observed and data is collected by using an automatic zoom three-dimensional surface measuring instrument, and input into the master control platform for analysis; 12) Further feedback adjustment is performed according to the analysis results of the master control platform, and steps 7) to 10) are repeated to achieve the best treatment effect and the highest treatment efficiency on the target surface; 13) Then, the target material after the surface etching after the laser action is completed is moved to the XYZ three-axis automated moving platform on the plasma machine; 14) Operate the plasma generator host, set the corresponding scanning area and parameters, the plasma machine power is 0~800W, and the scanning speed is 0.5m / s.

Citation Information

Cited By

  • Double-pulse system and method for improving depth resolution of laser ionization mass spectrum

    CN119827609A