Preparation process of heat-resistant multi-layer barrier composite bottle

Through the preparation process of heat-resistant multi-layer barrier composite bottles, using technologies such as molten polyolefin powder and quartz glass fiber composite nail sheets, the problem of insufficient sealing performance and structural strength of carbon fiber composite pressure vessels under high temperature and high pressure conditions is solved, and the problem of insufficient sealing performance and structural strength of carbon fiber composite pressure vessels under high temperature and high pressure conditions is achieved. High density and high strength composite bottle body.

CN119036721AActive Publication Date: 2024-11-29HANGZHOU HENGFENG PLASTIC PROD CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202411349635.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-25
Publication Date
2024-11-29
Estimated Expiration
2044-09-25

AI Technical Summary

Technical Problem

The existing carbon fiber composite pressure vessels have insufficient sealing performance and structural strength under high temperature and high pressure conditions, making it difficult to meet the strict requirements in the aerospace field.

Method used

A heat-resistant multi-layer barrier composite bottle preparation process is adopted, combining low-viscosity epoxy resin and five-machine Ferrite particles form a dense and high-strength structure.

Benefits of technology

It achieves good sealing performance and structural strength under high pressure, improves the lateral strength and impact resistance of the bottle body, and reduces the risk of deformation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure HDA0005061976520000011
    Figure HDA0005061976520000011
Patent Text Reader

Abstract

The invention relates to the technical field of heat-resistant multi-layer barrier composite bottle preparation processes, and discloses a heat-resistant multi-layer barrier composite bottle preparation process, which comprises the following steps: step 1, selecting polyolefin powder with high melt index and good fluidity, filling a rotational molding mold with the polyolefin powder, heating the mold to a temperature above the melting point of the polyolefin powder, and carrying out melt molding; and two mutually perpendicular rotating shafts of the mold are controlled to revolve and rotate, so that the molten powder is uniformly distributed on the inner wall of the mold to form a hollow inner barrel structure, and the powder is naturally cooled and demolded after being formed. The shell is high in compactness, good sealing performance can be kept under high pressure, the structural strength is high, the side edge strength of the shell is improved through the supporting performance of the shell pieces after the bottle body is pressed and expanded, and the phenomenon that the shell pieces are prone to deformation after being impacted is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of a preparation process for a heat-resistant multi-layer barrier composite bottle, in particular to a preparation process for a heat-resistant multi-layer barrier composite bottle. Background Art

[0002] Existing solid attitude control power systems are used for orbit transfer, terminal velocity correction, and attitude control of aircraft. They mainly include cooling systems, single / dual component liquid systems, and solid attitude control power systems. The solid attitude control system uses solid fuel as energy. When it is needed, the high-energy solid fuel is ignited by an electric igniter to generate high-temperature and high-pressure gas as energy for attitude control. Once the attitude needs to be corrected, the high-temperature combustion gas can be controlled by the solenoid valve to be on and off, and discharged from the nozzle to generate the required thrust;

[0003] At present, the main applications of carbon fiber composite pressure vessels are: medical respirator systems, including household and medical oxygen respirators, self-contained positive pressure air respirators for fire fighting, and compressed oxygen recirculating respirators for rescue; aerospace field, including aircraft escape slide inflators, ejection seats, and shells; new energy vehicle field, including steel liner carbon fiber hoop-wound steel composite gas cylinders (CNG-2), aluminum liner carbon fiber fully wrapped composite gas cylinders (CNG-3), plastic liner fully wrapped composite gas cylinders (CNG-4) and other compressed natural gas storage cylinders, high-pressure hydrogen storage pressure vessels, etc. Summary of the invention

[0004] The technical problem to be solved by the present invention is: in order to overcome the above problems, a process for preparing a heat-resistant multi-layer barrier composite bottle is provided, which solves the above problems.

[0005] The present invention solves the technical problem by adopting the following technical solutions:

[0006] A process for preparing a heat-resistant multi-layer barrier composite bottle comprises the following steps:

[0007] Step 1: Select polyolefin powder with high melt index and good fluidity and load it into the rotational molding mold, heat the mold to above the melting point of the polyolefin powder, control the two mutually perpendicular rotating axes of the mold to revolve and rotate, so that the powder is evenly distributed on the inner wall of the mold to form a hollow inner barrel structure after melting, and naturally cool and demold after molding;

[0008] Step 2: clamp the outer wall of the hollow inner barrel structure after step 1 by a split jacket mold, and then heat the mold surface to a temperature higher than the melting point of the polyolefin powder and form a hexagonal protrusion on the inner wall of the mold under constant pressure. Figure 1 The reinforced hot-rolled structure shown;

[0009] Step 3, applying glue to the hexagonal hot-rolled mouth in step 2 and embedding a hexagonal quartz glass fiber composite armor plate therein, wherein the thickness of the quartz glass fiber composite armor plate is consistent with the depth of the hexagonal hot-rolled mouth, and the side is a clearance fit, so as to obtain a reinforced inner liner bottle body;

[0010] Step 4, injecting pressurized air for constant pressure into the reinforced inner liner bottle body completed in step 3, and then winding it with carbon fiber;

[0011] Step 5: Apply fiber-reinforced resin to the outside of the bottle after the carbon fiber winding is completed, and rotate the fixture to ensure that the resin flows evenly;

[0012] Step 6: After the reinforcing resin is applied, the surface reinforcing resin is photocured by microwave lighting equipment;

[0013] Step 7: Repeat steps 5 and 6 until the outermost layer of reinforcing resin is completely cured.

[0014] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, during the carbon fiber winding process, the carbon fiber dry filaments are wound on multiple coarse yarn winding frames, guided by a fixed pulley, and fully impregnated in liquid epoxy resin to form a one-centimeter ribbon-shaped fiber bundle. Under computer control, the fiber bundle is repeatedly wound around the outer periphery of the inner liner through the axial reciprocating motion of the laying box and the rotation drive device of the inner liner.

[0015] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, the viscosity of the reinforcing resin on the outside is lower than that of the reinforcing resin on the inside, which makes it easier to discharge bubbles during repeated winding, thereby obtaining a dense winding structure.

[0016] In an embodiment of a process for preparing a heat-resistant multilayer barrier composite bottle, the temperature of the carbon fiber after being fully impregnated in liquid epoxy resin shall not be lower than 140 degrees Celsius before being wound around the outside of the reinforced inner liner bottle body.

[0017] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, 1 wt% of low-viscosity EVA-g-MA is added to the end material of the reinforced inner liner bottle body by hot melting to increase the viscosity and torque of the gas injection ports at both ends of the reinforced inner liner bottle body, thereby facilitating the installation of the metal filling port and improving the sealing of the material.

[0018] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, the viscosity of the epoxy resin is 4000-8000 cP at 25 degrees Celsius, and the particle size of the solid particles therein is less than 10-30 microns.

[0019] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, the equivalent of the epoxy resin to the curing agent is 1:1, and the pentaferrite particles that can absorb microwaves are evenly dispersed.

[0020] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, the temperature during curing of the epoxy resin should be controlled to be 20 degrees Celsius below the softening point of the polyolefin powder.

[0021] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, a clay film having a thickness of not less than one nanometer is coated on the inside and outside of a carbon fiber impregnated epoxy resin matrix, thereby effectively improving the density and sealing effect of the composite bottle.

[0022] The advantages and positive effects of the present invention are: high density, good sealing performance can be maintained under high pressure, and high structural strength. The support of the armor plate after the bottle body is compressed and expanded improves its side strength and reduces the phenomenon of easy deformation under impact. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0024] Figure 1 It is a structural schematic diagram of the present invention. DETAILED DESCRIPTION

[0025] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, which only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.

[0026] The embodiments of the present invention are further described in detail below with reference to the accompanying drawings:

[0027] like Figure 1 As shown, the preparation process of a heat-resistant multi-layer barrier composite bottle according to the present invention comprises the following steps:

[0028] Step 1: Select polyolefin powder with high melt index and good fluidity and load it into the rotational molding mold, heat the mold to above the melting point of the polyolefin powder, control the two mutually perpendicular rotating axes of the mold to revolve and rotate, so that the powder is evenly distributed on the inner wall of the mold to form a hollow inner barrel structure after melting, and naturally cool and demold after molding;

[0029] Step 2: clamp the outer wall of the hollow inner barrel structure after step 1 by a split jacket mold, and then heat the mold surface to a temperature higher than the melting point of the polyolefin powder and form a hexagonal protrusion on the inner wall of the mold under constant pressure. Figure 1 The reinforced hot-rolled structure shown;

[0030] Step 3, applying glue to the hexagonal hot-rolled mouth in step 2 and embedding a hexagonal quartz glass fiber composite armor plate therein, wherein the thickness of the quartz glass fiber composite armor plate is consistent with the depth of the hexagonal hot-rolled mouth, and the side is a clearance fit, so as to obtain a reinforced inner liner bottle body;

[0031] Step 4, injecting pressurized air for constant pressure into the reinforced inner liner bottle body completed in step 3, and then winding it with carbon fiber;

[0032] Step 5: Apply fiber-reinforced resin to the outside of the bottle after the carbon fiber winding is completed, and rotate the fixture to ensure that the resin flows evenly;

[0033] Step 6: After the reinforcing resin is applied, the surface reinforcing resin is photocured by microwave lighting equipment;

[0034] Step 7: Repeat steps 5 and 6 until the outermost layer of reinforcing resin is completely cured.

[0035] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, during the carbon fiber winding process, the carbon fiber dry filaments are wound on multiple coarse yarn winding frames, guided by a fixed pulley, and fully impregnated in liquid epoxy resin to form a one-centimeter ribbon-shaped fiber bundle. Under computer control, the fiber bundle is repeatedly wound around the outer periphery of the inner liner through the axial reciprocating motion of the laying box and the rotation drive device of the inner liner.

[0036] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, the viscosity of the reinforcing resin on the outside is lower than that of the reinforcing resin on the inside, which makes it easier to discharge bubbles during repeated winding, thereby obtaining a dense winding structure.

[0037] In an embodiment of a process for preparing a heat-resistant multilayer barrier composite bottle, the temperature of the carbon fiber after being fully impregnated in liquid epoxy resin shall not be lower than 140 degrees Celsius before being wound around the outside of the reinforced inner liner bottle body.

[0038] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, 1 wt% of low-viscosity EVA-g-MA is added to the end material of the reinforced inner liner bottle body by hot melting to increase the viscosity and torque of the gas injection ports at both ends of the reinforced inner liner bottle body, thereby facilitating the installation of the metal filling port and improving the sealing of the material.

[0039] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, the viscosity of the epoxy resin is 4000-8000 cP at 25 degrees Celsius, and the particle size of the solid particles therein is less than 10-30 microns.

[0040] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, the equivalent of the epoxy resin to the curing agent is 1:1, and the pentaferrite particles that can absorb microwaves are evenly dispersed.

[0041] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, the temperature during curing of the epoxy resin should be controlled to be 20 degrees Celsius below the softening point of the polyolefin powder.

[0042] In an embodiment of a process for preparing a heat-resistant multi-layer barrier composite bottle, a clay film having a thickness of not less than one nanometer is coated on the inside and outside of a carbon fiber impregnated epoxy resin matrix, thereby effectively improving the density and sealing effect of the composite bottle.

[0043] It should be emphasized that the embodiments described in the present invention are illustrative rather than restrictive, and therefore the present invention is not limited to the embodiments described in the specific implementation manners. Any other implementation manners derived by those skilled in the art based on the technical solutions of the present invention also fall within the scope of protection of the present invention.

Claims

1. A process for preparing a heat-resistant multi-layer barrier composite bottle, characterized in that: The steps include: Step 1: Select polyolefin powder with high melt index and good fluidity and load it into the rotational molding mold, heat the mold to above the melting point of the polyolefin powder, control the two mutually perpendicular rotating axes of the mold to revolve and rotate, so that the powder is evenly distributed on the inner wall of the mold to form a hollow inner barrel structure after melting, and naturally cool and demold after molding; Step 2: clamp the outer wall of the hollow inner barrel structure after step 1 by a split jacketed mold, and then heat the mold surface to a temperature higher than the melting point of the polyolefin powder and form a reinforced hot-rolled structure as shown in FIG1 under constant pressure through the hexagonal protrusions on the inner wall of the mold; Step 3, applying glue to the hexagonal hot-rolled mouth in step 2 and embedding a hexagonal quartz glass fiber composite armor plate therein, wherein the thickness of the quartz glass fiber composite armor plate is consistent with the depth of the hexagonal hot-rolled mouth, and the side is a clearance fit, so as to obtain a reinforced inner liner bottle body; Step 4, injecting pressurized air for constant pressure into the reinforced inner liner bottle body completed in step 3, and then winding it with carbon fiber; Step 5: Apply fiber-reinforced resin to the outside of the bottle after the carbon fiber winding is completed, and rotate the fixture to ensure that the resin flows evenly; Step 6: After the reinforcing resin is applied, the surface reinforcing resin is photocured by microwave lighting equipment; Step 7: Repeat steps 5 and 6 until the outermost layer of reinforcing resin is completely cured.

2. The process for preparing a heat-resistant multi-layer barrier composite bottle according to claim 1, characterized in that: During the carbon fiber winding process, the carbon fiber dry filaments are wound on multiple coarse yarn winding frames, guided by a fixed pulley, and fully impregnated in liquid epoxy resin. Then, they are gathered into a one-centimeter ribbon-shaped fiber bundle. Under computer control, the axial reciprocating motion of the laying box and the rotation drive device of the inner liner are used to repeatedly wrap the fiber bundle around the outer periphery of the inner liner.

3. The process for preparing a heat-resistant multi-layer barrier composite bottle according to claim 2, characterized in that: The viscosity of the reinforcing resin on the outside is lower than that of the reinforcing resin on the inside, which makes it easier to discharge bubbles during repeated winding, thereby obtaining a dense winding structure.

4. The process for preparing a heat-resistant multi-layer barrier composite bottle according to claim 3, characterized in that: After the carbon fiber is fully impregnated in the liquid epoxy resin, the temperature must not be lower than 140 degrees Celsius before it is wound around the outside of the reinforced inner liner bottle.

5. The process for preparing a heat-resistant multi-layer barrier composite bottle according to claim 4, characterized in that: 1 wt% of low-viscosity EVA-g-MA is added to the end material of the enhanced inner liner bottle body by hot melting to increase the viscosity and torque of the gas injection ports at both ends of the enhanced inner liner bottle body, thereby facilitating the installation of the metal filling port and improving the sealing of the material.

6. The process for preparing a heat-resistant multi-layer barrier composite bottle according to claim 5, characterized in that: The viscosity of the epoxy resin is 4000-8000 cP at 25 degrees Celsius, and the particle size of the solid particles therein is less than 10-30 microns.

7. The process for preparing a heat-resistant multi-layer barrier composite bottle according to claim 6, characterized in that: The equivalent of the epoxy resin and the curing agent is 1:1, and the pentaferrite particles capable of absorbing microwaves are evenly dispersed.

8. The process for preparing a heat-resistant multi-layer barrier composite bottle according to claim 7, characterized in that: When curing epoxy resin, the temperature should be controlled at 20 degrees Celsius below the softening point of polyolefin powder.

9. The process for preparing a heat-resistant multi-layer barrier composite bottle according to claim 8, characterized in that: A clay film with a thickness of not less than one nanometer is applied on the inside and outside of the carbon fiber impregnated epoxy resin matrix, which effectively improves the density and sealing effect of the composite bottle.

Citation Information

Patent Citations

  • Glass fiber all-winding aluminum liner composite cylinder and manufacturing process thereof

    CN103112181A

  • Novel bulletproof structure and manufacturing process

    CN112659583A

  • Puncture-proof fabric with porous buffer structure and preparation method of puncture-proof fabric

    CN114858002A

  • Preparation method of lining-free cryogenic high-pressure hydrogen storage cylinder

    CN115143386A

  • Preparation method of IV-type gas cylinder with thermoplastic polyimide composite material winding layer

    CN115625913A