Double-color product injection mold convenient to demold and using method
Through the design of the top-free mold release mechanism and sliding separation assembly, the smooth mold release of the two-color product injection mold is achieved, solving the problem of restricted mold release in the prior art, reducing manufacturing costs and improving product quality.
Patent Information
- Application Number
- CN202411382421.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing two-color product injection molds are limited during the mold release process, making it difficult to use complex product structures, resulting in increased manufacturing costs and poor product quality. Traditional thimbles or thimble rods are prone to breaking or bending, affecting yield.
Adopting a top-free mold release mechanism, combined with the design of sliding separation components and pushing components, through structures such as electric telescopic rods and guide columns, the smooth separation and automatic ejection of the upper molded kernel and the molded injection molded parts can be achieved, avoiding the traces of the thrust needle and adapting to Complex product structure.
It improves the demolding efficiency and quality of the mold, reduces manufacturing costs, ensures uniform thrust and smooth demolding, and solves the problem of restricted demolding.
Smart Images

Figure CN119036779A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of injection molds, in particular to a two-color product injection mold that is easy to demould and a use method thereof. Background Art
[0002] Two-color injection molding technology is a process that uses two different colors of plastic materials. Through a specially designed mold, the two materials are injected and combined together in the same injection cycle to achieve the diversity and beauty of the product appearance. This technology is innovative and versatile in product design and is widely used in electronic products, automotive parts, daily necessities and other fields. In order to ensure the effect of two-color injection molding, the mold usually contains complex runners, partitions and scissor structures to accurately control the feeding time and position of the two materials to achieve precise segmentation and gradient effects.
[0003] In the prior art, there is a two-color product injection mold that is easy to demould, such as the publication number CN111633911B, which includes: an upper mold plate, a lower mold plate, an upper mold core is provided on the upper mold core, a lower mold core is provided on the lower mold core, an upper cavity is provided on the upper mold core, and a lower cavity is provided on the lower mold core. The upper cavity and the lower cavity correspond to each other and can form a cavity. The lower mold core is provided with a guide cavity, which is connected to the lower cavity, and a first pressure block is provided in the guide cavity. The lower mold plate is provided with a slide, which is located on the right side of the first pressure block, and the slide is connected to the guide cavity. A slider is provided in the slide, and the slider contacts the first pressure block. A casting hole is provided on the upper mold plate, and the casting hole is connected to the upper cavity. The purpose of the above document is to provide a two-color product injection mold that is easy to demould quickly and has high product molding quality.
[0004] However, in actual use, the injection mold is demolded by using a traditional ejector pin or ejector rod structure. The ejector pin or ejector rod needs to be precisely installed on the mold to ensure that the force is evenly applied during the demolding process to avoid deformation or damage of the plastic part. This requires the mold to have high processing accuracy, which increases the manufacturing cost of the mold. Once the traditional ejector pin demolding is unevenly applied, the ejector pin is likely to break or bend, and the plastic part may be deformed, affecting the yield rate of the injection mold for two-color products.
[0005] Therefore, the present invention proposes a two-color product injection mold that is easy to demold and a method of use to solve the problems of limited demolding of existing injection molds and difficulty in using complex product structures. It can reduce manufacturing costs, improve product quality, ensure uniform thrust, and smooth demolding. Summary of the invention
[0006] The object of the present invention is to provide a two-color product injection mold that is easy to demould and a method of using it, so as to solve the problems raised in the above background technology.
[0007] To achieve the above-mentioned purpose, the present invention provides the following technical scheme: a two-color product injection mold for easy demoulding, comprising a bottom plate, lower support seats are fixedly installed on both sides of the bottom plate, the upper end of the lower support seat is fixedly connected with a fixed mold seat, the upper surface of the fixed mold seat is movably connected with an ejection template, electric telescopic rods are fixedly installed on both sides of the bottom plate, the upper ends of the electric telescopic rods are respectively fixedly connected to the lower surfaces of both sides of the ejection template, an upper mold seat is movably installed on the upper surface of the ejection template, an upper top mold is fixedly installed at the lower end of the upper mold seat, the lower surface of the upper top mold is movably engaged with the upper surface of the ejection template, an upper mold core 1 and an upper mold core 2 are slidably installed on the upper surface of the ejection template, an outer side of the upper mold core 1 and the upper mold core 2 is provided with a topless demoulding mechanism, the topless demoulding mechanism comprises a sliding separation component and a push component, the push component comprises a lower movable mold core, and the upper mold core 1 and the upper mold core 2 cooperate to form a complete injection runner groove after the mold is closed.
[0008] Preferably, the sliding separation assembly includes a guide column and a connecting wedge block, the guide column is fixedly mounted on the upper surface of the fixed mold base, and the outer surface of the guide column is movably plugged into the inner wall of the ejection mold base, the connecting wedge block is fixedly mounted on the outer surfaces of both sides of the fixed mold base, the connecting wedge blocks are arranged in four, every two of the connecting wedge blocks form a group, and each group of the connecting wedge blocks is mirror-distributed about the horizontal center axis of the fixed mold base, the upper end outer surface of the connecting wedge block is an integrally formed inclined surface, and the upper outer surface of the connecting wedge block is movably connected with a connecting slider.
[0009] Preferably, the outer surfaces on both sides of the connecting slider are slidably connected to limiting side plates, the limiting side plates are fixedly mounted on the upper surface of the ejection template, and a limiting groove is provided on the inner wall of the connecting slider, and the inner wall of the limiting groove is movably connected to the outer surface of the connecting block.
[0010] Preferably, a mounting groove is provided on the inner wall of the upper end of the ejection template, and a mounting assembly is provided in the inner cavity of the mounting groove. The mounting assembly includes a lower injection molding mold, and the lower injection molding mold is fixedly installed on the bottom surface of the inner cavity of the mounting groove. A receiving groove is provided on the inner wall of the upper end of the lower injection molding mold, and a reserved hole is provided on the bottom surface of the inner cavity of the receiving groove, and the inner surface of the reserved hole is penetrated and connected with a limiting push rod.
[0011] Preferably, three groups of the limit push rods are provided, and the outer surfaces of the three groups of the limit push rods are slidably connected to the inner walls of the ejection template and the lower injection molding mold, and a fixed sleeve is provided on the outer side of the limit push rod, and the fixed sleeve is fixedly installed on the upper surface of the base plate.
[0012] Preferably, a cross movable groove is opened on the inner wall of the fixed sleeve, and a cross slider is fixedly installed on the outer surface of the lower end of the limiting push rod. The cross slider is a "+"-shaped block structure. The outer surface of the cross slider is adapted to slide with the inner wall of the cross movable groove, and a reset component is provided on the outer surface of the lower end of the cross slider.
[0013] Preferably, the reset assembly includes a telescopic sleeve rod and a spring, the upper ends of the telescopic sleeve rod and the spring are respectively fixedly connected to the lower surface of the cross slider, the outer surfaces of the lower ends of the telescopic sleeve rod and the spring are fixedly connected to the bottom surface of the inner cavity of the fixed sleeve, and the spring sliding sleeve is arranged on the outside of the telescopic sleeve rod.
[0014] Preferably, a mold closing groove is arranged above the injection runner groove, an injection hole is opened in the center of the mold closing groove, and the injection runner groove and the injection hole are communicated between the upper mold core 1 and the upper mold core 2 after the mold is closed.
[0015] Preferably, a docking hole is provided on the lower surface of the upper ejector mold, and a docking block is movably embedded on the inner surface of the docking hole. The docking block is fixedly installed on the upper surface of the ejection template. The docking block has a triangular pyramidal structure as a whole. Four docking blocks are provided and correspond one to one with the docking holes. Two of the docking blocks form a group and are respectively arranged on the outside of upper mold core one and upper mold core two.
[0016] A method for using a two-color product injection mold that is easy to demould comprises the following steps:
[0017] Step 1: The electric telescopic rod drives the ejector template and the fixed mold base to the initial merged position, the upper mold core 1 and the upper mold core 2 are closed to form a complete cavity, and an injection runner groove is formed between the lower movable mold core;
[0018] Step 2: The upper mold base drives the upper top mold to move downward and close the mold with the ejector mold plate, and injects the injection plastic into the injection runner groove through the injection hole;
[0019] Step 3: After waiting for a period of time, a complete molded plastic part is formed between the injection runner grooves, and the electric telescopic rod is controlled to extend so that the ejection template is ejected upward;
[0020] Step 4: The ejection template drives the upper mold core 1 and the upper mold core 2 bracket to separate laterally under the action of the sliding separation component, and the lower movable mold core is ejected upward synchronously;
[0021] Step 5: Remove the ejector-molded plastic parts.
[0022] Compared with the prior art, the present invention has the following beneficial effects:
[0023] The present invention proposes a two-color product injection mold that is easy to demold and a method of using the same. The mold demolding efficiency and demolding quality of the mold are improved by adopting a topless demolding mechanism, and the design of a sliding separation component and a push component is combined. The topless demolding mechanism can smoothly separate the upper mold core 1, the upper mold core 2 and the formed injection molded part through the guiding and connecting action of the sliding separation component when the mold is opened, and realize the automatic ejection of the lower movable mold core. In this way, the molded injection molded part is ejected, and ejector marks are avoided. It is adaptable to complex product structures, reduces manufacturing costs, and improves product quality. It ensures uniform thrust and smooth demolding, and solves the problems of limited demolding of existing injection molds and difficulty in using complex product structures. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a schematic diagram of the structure of the mold closing state of the present invention;
[0025] Figure 2 This is a schematic diagram of the structure of the mold opening state of the present invention;
[0026] Figure 3 It is a schematic structural diagram of the upper mold core 1 and the upper mold core 2 in the separated state of the present invention;
[0027] Figure 4 It is a schematic diagram of the test cross-section structure of the present invention;
[0028] Figure 5 For the present invention Figure 4 A schematic diagram of the enlarged structure at point A;
[0029] Figure 6 It is a schematic diagram of the separated cross-sectional structure of the upper mold core 1 and the upper mold core 2 of the present invention;
[0030] Figure 7 It is a schematic diagram of a half-section structure of the upper mold core 1 and the upper mold core 2 of the present invention;
[0031] Figure 8 For the present invention Figure 7 A schematic diagram of the enlarged structure at B;
[0032] Fig. 9 It is a schematic diagram of the state structure of the lower movable mold core ejecting the receiving groove of the present invention;
[0033] Fig.10 It is a schematic diagram of the structure of the upper mold core 1 and the upper mold core 2 in the mold closing state of the present invention;
[0034] Fig.11 It is a schematic diagram of the structure of the upper mold core 1 and the upper mold core 2 in the mold closing state when viewed from above;
[0035] Fig.12 It is a schematic diagram of the three-dimensional structure of the lower injection molding mold of the present invention;
[0036] Fig.13It is a structural schematic diagram of the push assembly of the present invention;
[0037] Fig.14 For the present invention Fig.13 A schematic diagram of the enlarged structure at C;
[0038] Fig.15 It is a flow chart of the present invention.
[0039] In the figure: 1, bottom plate; 2, lower support seat; 3, fixed die seat; 4, ejector die plate; 5, upper die seat; 6, upper ejector die; 21, electric telescopic rod; 31, guide column; 8, upper die core 1;
[0040] 9. Upper mold core 2; 60. Docking hole; 61. Docking block; 32. Connecting wedge; 10. Connecting slider; 101. Limiting groove; 102. Limiting side plate; 40. Mounting groove; 41. Lower injection molding mold; 410. Receiving groove; 4100. Reserved hole; 7. Lower movable mold core; 71. Fixed sleeve; 710. Cross movable groove; 72. Limiting push rod; 721. Cross slider;
[0041] 73, telescopic sleeve rod; 731, spring; 70, injection runner groove; 11, injection hole; 12, mold forming groove. DETAILED DESCRIPTION
[0042] In order to make the purpose and technical solution of the present invention clearly and completely described, and the advantages more clearly understood, the embodiments of the present invention are further described in detail with reference to the accompanying drawings. It should be understood that the specific embodiments described herein are part of the embodiments of the present invention, rather than all of the embodiments, and are only used to explain the embodiments of the present invention, and are not used to limit the embodiments of the present invention. All other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0043] Embodiment 1
[0044] See also Figure 1 - Fig.15The present invention provides a technical solution: a two-color product injection mold that is easy to demould, comprising a bottom plate 1, lower support seats 2 are fixedly installed on both sides of the bottom plate 1, the upper end of the lower support seat 2 is fixedly connected to a fixed mold seat 3, and the upper surface of the fixed mold seat 3 is movably connected to an ejection template 4, electric telescopic rods 21 are fixedly installed on both sides of the bottom plate 1, and the upper ends of the electric telescopic rods 21 are respectively fixedly connected to the lower surfaces of both sides of the ejection template 4, an upper mold seat 5 is movably installed on the upper surface of the ejection template 4, and an upper top mold 6 is fixedly installed at the lower end of the upper mold seat 5, and the lower surface of the upper top mold 6 is movably connected to the upper surface of the ejection template 4, and an upper mold core 1 8 and an upper mold core 2 9 are slidably installed on the upper surface of the ejection template 4, and a topless demoulding mechanism is arranged on the outer sides of the upper mold core 1 8 and the upper mold core 2 9, and the topless demoulding mechanism includes The sliding separation component and the pushing component, the pushing component includes a lower movable mold core 7, an upper mold core 1 8 and an upper mold core 2 9, which cooperate to form a complete injection runner groove 70 after the mold is closed; by adopting a topless demoulding mechanism, combined with the design of the sliding separation component and the pushing component, the demoulding efficiency and demoulding quality of the mold are improved. The topless demoulding mechanism can, when the mold is opened, through the guiding and connecting effect of the sliding separation component, make the upper mold core 1 8, the upper mold core 2 9 and the formed injection molded part smoothly separate, and realize the automatic ejection of the lower movable mold core 7. In this way, the molded injection molded plastic parts are ejected, avoiding ejector marks, adapting to complex product structures, reducing manufacturing costs, and improving product quality. It ensures uniform thrust and smooth demoulding, and solves the problems of limited demoulding of existing injection molds and difficulty in using complex product structures.
[0045] Embodiment 2
[0046] On the basis of the first embodiment, in order to realize ejector-free demoulding and avoid the deformation of the rubber part during demoulding: the sliding separation component includes a guide column 31 and a connecting wedge 32, the guide column 31 is fixedly mounted on the upper surface of the fixed mold base 3, and the outer surface of the guide column 31 is movably plugged with the inner wall of the ejection template 4, the connecting wedge 32 is fixedly mounted on the outer surfaces of both sides of the fixed mold base 3, four connecting wedges 32 are provided, and every two connecting wedges 32 form a group, and each group of connecting wedges 32 is mirror-distributed about the horizontal central axis of the fixed mold base 3, the upper end outer surface of the connecting wedge 32 is an integrally formed inclined surface, and the upper outer surface of the connecting wedge 32 is movably connected with a connecting slider 10; the outer surfaces of both sides of the connecting slider 10 are slidably connected to the limiting side plates 102, and the limiting side plates 102 are fixedly mounted on the upper surface of the ejection template 4, and the inner wall of the connecting slider 10 is provided with a limiting groove 101, and the inner wall of the limiting groove 101 is movably connected with the outer surface of the connecting wedge 32;
[0047] When the mold is closed, the upper mold base 5 moves downward and synchronously drives the upper ejector mold 6 to merge tightly with the ejection template 4. At this time, the upper mold core 1 8 and the upper mold core 2 9 are in a tightly merged state, and the injection molding material is injected into the injection runner groove 70 formed between the lower movable mold core 7 and the mold closing molding groove 12 through the injection hole 11. After cooling for a period of time, the injection molding part is formed. Subsequently, the upper ejector mold 6 is controlled to separate from the ejection template 4. At this time, the electric telescopic rod 21 is controlled to be extended and retracted, and the piston rod at the output end of the electric telescopic rod 21 drives the ejection template 4 to move upward longitudinally as a whole. According to the inclined surface cooperation between the limiting groove 101 and the guide column 31, in the process of the ejection template 4 moving upward, the upper mold core 1 8 and the upper mold core 2 9 are respectively separated to the corresponding sides by the pulling force of the connecting slider 10. In this way, the mold closing molding groove 12 is laterally separated from the molded injection molding part, thereby ensuring the automatic ejection of the molded injection molding part, replacing the traditional structure of pushing the demoulding by the ejector pin or ejector rod, and avoiding the ejector pin marks of the injection molding part.
[0048] Embodiment 3
[0049] On the basis of the second embodiment, in order to achieve uniform force and smooth demolding at the bottom of the injection molded plastic part formed in the inner cavity of the injection runner groove 70: a mounting groove 40 is provided on the inner wall of the upper end of the ejection template 4, and the inner cavity of the mounting groove 40 is provided with a mounting assembly, and the mounting assembly includes a lower injection molding mold 41, and the lower injection molding mold 41 is fixedly installed on the bottom surface of the inner cavity of the mounting groove 40, and a receiving groove 410 is provided on the inner wall of the upper end of the lower injection molding mold 41, and a reserved hole 4100 is provided on the bottom surface of the inner cavity of the receiving groove 410, and the inner surface of the reserved hole 4100 is penetrated and connected with a limit push rod 72; the limit push rod 72 Three groups are provided, and the outer surfaces of the three groups of limit push rods 72 are slidably connected with the inner walls of the ejection template 4 and the lower injection molding mold 41. A fixed sleeve 71 is provided on the outer side of the limit push rod 72, and the fixed sleeve 71 is fixedly installed on the upper surface of the bottom plate 1; a cross movable groove 710 is provided on the inner wall of the fixed sleeve 71, and a cross slider 721 is fixedly installed on the outer surface of the lower end of the limit push rod 72. The cross slider 721 is a "+"-shaped block structure, and the outer surface of the cross slider 721 is adapted to slide with the inner wall of the cross movable groove 710, and a reset component is provided on the outer surface of the lower end of the cross slider 721;
[0050] When the upper mold core 1 8 and the upper mold core 2 9 are combined, a complete mold closing groove 12 is formed, and an injection runner groove 70 is formed between the mold closing groove 12 and the lower movable mold core 7 for injecting plastic material, and the injection hole 11 penetrates the inside of the injection runner groove 70, and the lower injection molding mold 41 is installed through the installation groove 40 opened on the upper surface of the ejection template 4. When the ejection template 4 is pushed upward to separate the upper mold core 1 8 from the upper mold core 2 9, the lower movable mold core 7 and the fixed sleeve 71 move upward synchronously with the lower injection molding mold 41, and at this time, the cross slider 721 slides in the inner cavity of the cross movable groove 710 to ensure the smooth ejection of the lower movable mold core 7, and when the ejection template 4 moves upward, the telescopic sleeve rod 73 and the spring 731 are stretched and deformed.
[0051] Embodiment 4
[0052] On the basis of the third embodiment, in order to realize the smooth reset of the lower movable mold core 7: the reset component includes a telescopic sleeve rod 73 and a spring 731, the upper ends of the telescopic sleeve rod 73 and the spring 731 are respectively fixedly connected to the lower surface of the cross slider 721, the lower end outer surfaces of the telescopic sleeve rod 73 and the spring 731 are fixedly connected to the inner cavity bottom surface of the fixed sleeve 71, and the spring 731 is slidably sleeved on the outside of the telescopic sleeve rod 73; a mold closing groove 12 is provided above the injection runner groove 70, and an injection hole 11 is opened at the center of the mold closing groove 12, and the upper mold core 1 8 and the upper mold core 2 9 are connected between the injection runner groove 70 and the injection hole 11 after the mold is closed;
[0053] After the molded injection molded part is taken out, the electric telescopic rod 21 is retracted to make the ejection template 4 return to its original position and no longer exert an ejection force on the injection molded part. Then the limit push rod 72 slides on the inner wall of the cross movable groove 710. Due to the sliding cooperation between the limit push rod 72 and the inner wall of the cross movable groove 710, and the reverse elastic force between the telescopic sleeve rod 73 and the spring 731, the reset component starts to work. Specifically, the telescopic sleeve rod 73 slides in the spring 731 and is compressed, while releasing the stored elastic potential energy, pushing the limit push rod 72 and the entire movable mold part to move to the initial position. In the process of the limit push rod 72 sliding along the inner wall of the cross movable groove 710, energy is automatically released to push the movable mold part to reset to the initial position, preparing for the next injection molding cycle, thereby improving the automation degree and operation efficiency of the mold.
[0054] Embodiment 5
[0055] On the basis of the fourth embodiment, in order to achieve the stability of the mold closing between the upper top mold 6 and the ejection mold plate 4: a docking hole 60 is opened on the lower surface of the upper top mold 6, and a docking block 61 is movably embedded on the inner surface of the docking hole 60. The docking block 61 is fixedly installed on the upper surface of the ejection mold plate 4. The docking block 61 has a triangular pyramid structure as a whole. Four docking blocks 61 are provided and correspond to the docking holes 60 one by one. Two docking blocks 61 are set as a group and are respectively arranged on the outer sides of the upper mold core 1 8 and the upper mold core 2 9;
[0056] When the upper mold base 5 drives the upper top mold 6 to move synchronously to achieve mold closing, the docking hole 60 and the docking block 61 are adapted to fit together. The docking hole 60 and the docking block 61 here can achieve precise alignment of the mold closing to prevent the mold closing from shifting. By respectively arranging the docking blocks 61 on the outside of the upper mold core 1 8 and the upper mold core 2 9, they can also play a blocking role for the upper mold core 1 8 and the upper mold core 2 9 of the open mold.
[0057] Embodiment 6
[0058] Based on the fifth embodiment, a method for using a two-color product injection mold that is easy to demould comprises the following steps:
[0059] Step 1: The electric telescopic rod 21 drives the ejector mold plate 4 and the fixed mold base 3 to the initial merged position, the upper mold core 1 8 and the upper mold core 2 9 are closed to form a complete cavity, and an injection flow channel groove 70 is formed between the lower movable mold core 7;
[0060] Step 2: The upper mold base 5 drives the upper ejector mold 6 to move downward to close the mold with the ejector mold plate 4, and injects the injection plastic into the injection runner groove 70 through the injection hole 11;
[0061] Step 3: After waiting for a period of time, a complete molded plastic part is formed between the injection runner grooves 70, and the electric telescopic rod 21 is controlled to extend so that the ejection template 4 is ejected upward;
[0062] Step 4: The ejection template 4 drives the upper mold core 1 8 and the upper mold core 2 9 bracket to separate laterally under the action of the sliding separation component, and the lower movable mold core 7 is ejected upward synchronously;
[0063] Step 5: Remove the ejector-molded plastic parts.
[0064] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A two-color product injection mold that is easy to demould, comprising a bottom plate (1), characterized in that: Lower support seats (2) are fixedly mounted on both sides of the base plate (1), the upper end of the lower support seat (2) is fixedly connected to a fixed die seat (3), the upper surface of the fixed die seat (3) is movably connected to an ejection die plate (4), electric telescopic rods (21) are fixedly mounted on both sides of the base plate (1), the upper ends of the electric telescopic rods (21) are respectively fixedly connected to the lower surfaces of both sides of the ejection die plate (4), an upper die seat (5) is movably mounted on the upper surface of the ejection die plate (4), and an upper ejection die seat (5) is fixedly mounted at the lower end of the upper die seat (5). (6), the lower surface of the upper top mold (6) is movably engaged with the upper surface of the ejection mold plate (4), the upper surface of the ejection mold plate (4) is slidably mounted with an upper mold core 1 (8) and an upper mold core 2 (9), the outer sides of the upper mold core 1 (8) and the upper mold core 2 (9) are provided with a topless demoulding mechanism, the topless demoulding mechanism includes a sliding separation component and a push component, the push component includes a lower movable mold core (7), the upper mold core 1 (8) and the upper mold core 2 (9) cooperate to form a complete injection runner groove (70) after the mold is closed.
2. The two-color product injection mold that is easy to demould according to claim 1, characterized in that: The sliding separation component comprises a guide column (31) and a connecting wedge (32), wherein the guide column (31) is fixedly mounted on the upper surface of the fixed mold base (3), and the outer surface of the guide column (31) is movably plugged into the inner wall of the ejection mold plate (4), and the connecting wedge (32) is fixedly mounted on the outer surfaces of both sides of the fixed mold base (3). The connecting wedge (32) is arranged in four pieces, and each two connecting wedges (32) form a group. Each group of connecting wedges (32) is mirror-distributed about the horizontal central axis of the fixed mold base (3). The upper end outer surface of the connecting wedge (32) is an integrally formed inclined surface, and the upper side outer surface of the connecting wedge (32) is movably connected with a connecting slider (10).
3. The two-color product injection mold that is easy to demould according to claim 2, characterized in that: The outer surfaces of both sides of the connecting slider (10) are slidably connected to the limiting side plates (102), and the limiting side plates (102) are fixedly mounted on the upper surface of the ejection template (4). The inner wall of the connecting slider (10) is provided with a limiting groove (101), and the inner wall of the limiting groove (101) is movably connected to the outer surface of the connecting block (32).
4. The two-color product injection mold that is easy to demould according to claim 3 is characterized by: An installation groove (40) is provided on the inner wall of the upper end of the ejection template (4), and an installation component is provided in the inner cavity of the installation groove (40). The installation component includes a lower injection molding die (41), and the lower injection molding die (41) is fixedly installed on the bottom surface of the inner cavity of the installation groove (40). A receiving groove (410) is provided on the inner wall of the upper end of the lower injection molding die (41), and a reserved hole (4100) is provided on the bottom surface of the inner cavity of the receiving groove (410), and the inner surface of the reserved hole (4100) is penetrated and connected with a limiting push rod (72).
5. The two-color product injection mold that is easy to demould according to claim 4, characterized in that: The limiting push rods (72) are provided in three groups, and the outer surfaces of the three groups of limiting push rods (72) are slidably connected to the inner walls of the ejection mold plate (4) and the lower injection molding mold (41); a fixing sleeve (71) is provided on the outer side of the limiting push rods (72), and the fixing sleeve (71) is fixedly mounted on the upper surface of the base plate (1).
6. The two-color product injection mold that is easy to demould according to claim 5, characterized in that: A cross movable groove (710) is provided on the inner wall of the fixed sleeve (71), a cross slider (721) is fixedly mounted on the outer surface of the lower end of the limit push rod (72), the cross slider (721) is a "+"-shaped block structure, the outer surface of the cross slider (721) is adapted to slide with the inner wall of the cross movable groove (710), and a reset component is provided on the outer surface of the lower end of the cross slider (721).
7. The two-color product injection mold that is easy to demould according to claim 6, characterized in that: The reset assembly comprises a telescopic sleeve rod (73) and a spring (731); the upper ends of the telescopic sleeve rod (73) and the spring (731) are respectively fixedly connected to the lower surface of the cross slide block (721); the lower end outer surfaces of the telescopic sleeve rod (73) and the spring (731) are fixedly connected to the bottom surface of the inner cavity of the fixed sleeve (71); and the spring (731) is slidably sleeved on the outside of the telescopic sleeve rod (73).
8. The two-color product injection mold that is easy to demould according to claim 1, characterized in that: A mold closing groove (12) is arranged above the injection molding flow channel groove (70), an injection molding hole (11) is opened at the center of the mold closing groove (12), and the injection molding flow channel groove (70) and the injection molding hole (11) are communicated between the upper mold core 1 (8) and the upper mold core 2 (9) after the mold is closed.
9. The two-color product injection mold that is easy to demould according to claim 8, characterized in that: The lower surface of the upper ejector mold (6) is provided with a docking hole (60), and the inner surface of the docking hole (60) is movably embedded with a docking block (61). The docking block (61) is fixedly mounted on the upper surface of the ejector mold plate (4). The docking block (61) is in a triangular pyramid structure as a whole. Four docking blocks (61) are provided and correspond to the docking holes (60) one by one. Two docking blocks (61) form a group and are respectively arranged on the outer sides of the upper mold core 1 (8) and the upper mold core 2 (9).
10. A method for using a two-color product injection mold that is easy to demould, which is based on the two-color product injection mold that is easy to demould according to any one of claims 1 to 9, and is characterized in that: The method for using the two-color product injection mold that is easy to demould comprises the following steps: Step 1: The electric telescopic rod (21) drives the ejection template (4) and the fixed mold base (3) to be in the initial merging position, the upper mold core 1 (8) and the upper mold core 2 (9) are closed to form a complete cavity, and an injection flow channel groove (70) is formed between the lower movable mold core (7); Step 2: The upper mold base (5) drives the upper ejector mold (6) to move downward to close the mold with the ejector mold plate (4), and injects the injection molding rubber into the injection runner groove (70) through the injection hole (11); Step 3: After waiting for a period of time, a complete molded plastic part is formed between the injection runner grooves (70), and the electric telescopic rod (21) is controlled to extend so that the ejection template (4) is ejected upward; Step 4: The ejection template (4) drives the upper mold core 1 (8) and the upper mold core 2 (9) bracket to separate laterally under the action of the sliding separation component, and the lower movable mold core (7) is ejected upward synchronously; Step 5: Remove the ejector-molded plastic parts.
Citation Information
Patent Citations
Side forming die mechanism
CN212733822U
Injection mold with automatic demolding mechanism
CN213198658U
Lateral core-pulling limiting mold opening mold structure
CN215203255U
Side core-pulling mechanism and injection mold
CN215791468U
Thick-wall headlamp lens injection mold structure
CN221677880U
Cited By
Injection mold facilitating demolding of injection product
CN120816681A
Rubber drainage tank forming device and forming method
CN121515372A
A rubber drainage channel molding device and molding method
CN121515372B