Construction method for tunnel lining small side wall construction joint
By laying chisel belts on the surface of the construction joints of the small side wall of the tunnel, the problems of difficulty in chiseling and low quality in tunnel construction are solved, and efficient and convenient construction joint treatment is achieved, reducing costs and improving construction quality.
Patent Information
- Application Number
- CN202411066487.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-29
AI Technical Summary
In tunnel construction, due to the limited construction space, the existing chiseling treatment methods rely on manual operations, resulting in low construction efficiency, high cost and difficult to guarantee quality.
By laying a chisel belt on the surface of the construction joint of the small side wall, the chisel belt includes several pyramid-shaped convex teeth for forming chisel grooves, which are used to fit the end face of the small side wall, instead of manual chiseling treatment, to be used to concrete After initial solidification, remove the chisel belt and complete the construction joint after the concrete is completely solidified.
It realizes efficient and convenient processing of construction joints, reduces the labor intensity and cost of construction workers, and improves construction quality. The chiseled belts are reusable and are suitable for different concrete materials.
Smart Images

Figure CN119041938A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of tunnel construction, and in particular to a method for constructing a small side wall construction joint of a tunnel lining. Background Art
[0002] During the tunnel construction process, due to construction technology and construction organization reasons, the tunnel structure cannot be cast completely in one piece, so it needs to be cast in sections. There must be a bonding surface between the first and later poured concrete, namely the construction joint. In order to ensure the connection strength and waterproofness between adjacent concretes, most people choose to roughen the bonding surface of the first poured concrete during the concrete pouring process.
[0003] Roughening treatment refers to chiseling out a series of indentations on the joint surface of the first poured concrete to remove dust, mortar, oil stains, etc. on the concrete surface and increase the contact area between the first and later poured concretes. However, in the existing roughening construction process, due to the limited construction space in the tunnel, manual chiseling using electric picks, pneumatic picks and other equipment is required, which not only has high labor costs and low construction efficiency, but also the quality of the roughening depends on manual technology, and the quality of the roughening is difficult to guarantee.
[0004] Therefore, an efficient and high-quality construction joint treatment method is urgently needed to solve the above problems.
[0005] The information disclosed in this background technology section is only used to deepen the understanding of the background technology of the present disclosure, and should not be regarded as acknowledging or suggesting in any form that the information constitutes the prior art known to those skilled in the art. Summary of the invention
[0006] In view of at least one of the above technical problems, the present disclosure provides a method for constructing small side wall construction joints of tunnel lining, which solves the problem of difficult roughening treatment and low roughening quality of small side wall construction joints by laying roughening tape on the surface of the small side wall construction joints.
[0007] According to one aspect of the present disclosure, a method for constructing a small side wall construction joint of a tunnel lining is provided, comprising: S1: Tie up the steel skeleton of the tunnel invert and small side wall; S2: Install the end formwork and side formwork of the tunnel invert and small side wall and reinforce them; S3: pouring concrete into the enclosed area of the end formwork and the side formwork of the tunnel invert, and finishing the concrete surface after vibrating and compacting; S4: pour concrete into the enclosed area of the end formwork and the side formwork of the small side wall, vibrate and compact it, and then add slurry to finish the concrete surface; S5: laying a roughening tape at the top end surface of the small side wall corresponding to the construction joint, and compacting the roughening tape to make it fit tightly with the top end surface of the small side wall; the roughening tape is used to fit the end surface of the small side wall and is arranged with a plurality of convex teeth in an array for forming roughening grooves; S6: After the concrete of the small side wall has initially set, the roughening tape is removed, and after the concrete has completely set, the construction joint is completed.
[0008] In some embodiments of the present disclosure, in step S2, the end formwork and side formwork of the tunnel invert and small side wall are steel structure formworks; the end formworks of the tunnel invert and small side wall are arranged at both ends of the tunnel invert and small side wall; the side formworks of the tunnel invert and small side wall are arranged on one side of the tunnel invert and small side wall close to the center of the tunnel.
[0009] In some embodiments of the present disclosure, in the step S4, the height of the slurry is 1.5 to 2 cm.
[0010] In some embodiments of the present disclosure, in the step S5, before the chiseled tape is laid, a release agent is applied to the end surface of the chiseled tape to be bonded.
[0011] In some embodiments of the present disclosure, in step S5, the top end surface of the small side wall is horizontal, the area of the roughening belt is not less than 75% of the surface area of the top end surface of the small side wall, and the height of the convex teeth of the roughening belt is not less than 8 mm.
[0012] In some embodiments of the present disclosure, in step S5, the protruding teeth are pyramidal in shape.
[0013] In some embodiments of the present disclosure, in the step S5, the height of the protruding teeth of the chiseling belt for fine stone concrete is greater than the height of the protruding teeth of the chiseling belt for medium-coarse stone concrete.
[0014] One or more technical solutions provided in the embodiments of the present application have at least any of the following technical effects or advantages: 1. A roughening tape is laid on the surface of the construction joint of the small side wall to replace manual roughening. After the initial setting of the concrete of the small side wall, the roughening tape is removed, and the roughening surface corresponding to the construction joint can be formed. The operation is simple and convenient, and is not affected by the skills of the construction workers. It greatly facilitates the roughening treatment of the construction joint, reduces the labor intensity of the construction workers, and has good construction quality and high construction efficiency.
[0015] 2. The construction loss of the chiseling belt is small and it can be reused more than 50 times, which greatly reduces the construction cost. The chiseling belt includes chiseling belts with different tooth heights. For concrete with different material ratios, chiseling belts with corresponding tooth heights are selected to ensure the forming effect and quality of the chiseled surface.
[0016] 3. The convex teeth of the chiseling belt are pyramidal. The chiseling seam effect can be improved through the special structural limitation of the convex teeth of the chiseling belt. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 This is a schematic diagram of the cross-section of a small side wall of a tunnel lining in one embodiment of the present application.
[0018] Figure 2 This is a schematic plan view of the construction joint of the small side wall of the tunnel lining in one embodiment of the present application.
[0019] Figure 3 This is a schematic diagram of the structure of a large-toothed chiseling belt in one embodiment of the present application.
[0020] Figure 4 This is a schematic diagram of the structure of a small-toothed chiseling belt in one embodiment of the present application.
[0021] Figure 5 This is a flow chart of the roughening-free construction joint construction of the small side wall of the tunnel lining in one embodiment of the present application.
[0022] In the above figures, 1 is the tunnel invert, 2 is the small side wall, 3 is the main reinforcement, 4 is the tunnel invert side formwork, 5 is the small side wall side formwork, 6 is the roughening belt, 7 is the large-toothed roughening belt, and 8 is the small-toothed roughening belt. DETAILED DESCRIPTION
[0023] In order to better understand the technical solution of the present application, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0024] In the description of this application, it should be understood that the terms "upper", "lower", "front", "back", "left", "right", "top", "bottom", "inside", "outside", "vertical", "horizontal", "clockwise", "counterclockwise", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing this application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as a limitation on this application. The "connection" and "coupling" involved in this application, unless otherwise specified, include direct and indirect connections (couplings).
[0025] Unless otherwise specified, the components, structures, and mechanisms involved in the following embodiments are conventional commercially available products.
[0026] The embodiment of the present application provides a method for constructing a small side wall construction joint of a tunnel lining, thereby solving the problem that it is difficult to roughen the existing small side wall construction joints manually and the roughening quality is not high. By laying a roughening belt on the surface of the small side wall construction joint, the roughening treatment of the construction joint is completed efficiently and with high quality.
[0027] This example discloses a method for constructing a small side wall construction joint in a tunnel lining. Figures 1 to 5 , including the following steps: S1: See Figure 1 , tie up the steel skeleton of the tunnel invert 1 and the small side wall 2, and set up two layers of inner and outer main reinforcement 3. The main reinforcement 3 is Φ20 steel bar. The tunnel invert and the small side wall steel skeleton are integrated. The bending part of the steel skeleton is arc-shaped and cannot be a right-angle structure.
[0028] S2: See Figure 1 After the steel skeleton is installed, the tunnel invert 1 and the small side wall 2 are supported by formwork; the tunnel invert is set at the bottom of the small side wall and cast as a whole, and end formworks are installed at both ends of the tunnel invert and the small side wall. The end formworks are steel structure formworks. Bolts are used to fix the end formworks with the tunnel side wall and the bottom, and sealing strips are set at the connection between the end formwork and the tunnel to prevent concrete leakage; side formworks are respectively installed on the side of the tunnel invert and the small side wall close to the tunnel center. The side formworks include a tunnel invert side formwork 4 and a small side wall side formwork 5. The side formworks are also steel structure formworks, and bolts are used to fix the side formworks with the end formworks, and sealing strips are set at the corresponding connection between the side formworks and the end formworks; release agents are provided on the inner surfaces of the end formworks and the side formworks to prevent the formworks from adhering to the concrete and damaging the concrete structure.
[0029] S3: After the tunnel invert 1 and the small side wall 2 are supported, the tunnel invert and the small side wall are cast by a concrete tanker; C30 concrete is cast into the enclosed area of the end formwork and the side formwork of the tunnel invert, and a chute is provided on the concrete tanker to allow the concrete to be smoothly poured into the tunnel invert. During the casting process, an insert vibrator is inserted into the concrete for vibration to make the concrete dense. After the concrete is cast and vibrated densely, the concrete is finished, and the concrete surface is smoothed with a trowel to remove bubbles and uneven parts on the concrete surface.
[0030] S4: After the concrete finishing of the tunnel invert is completed, the small side wall is poured. The C30 concrete is poured into the enclosed area of the end formwork and the side formwork of the small side wall using a concrete tank truck and a chute. The concrete is vibrated and compacted with an inserted vibrator, and the vibrator is used to raise the slurry. The slurry raising depth is 1.5 to 2 cm to prevent concrete shrinkage cracks and ensure the smoothness of the concrete surface. Finally, the concrete surface is finished.
[0031] S5: See Figure 1 , Figure 2After the concrete pouring of the tunnel invert 1 and the small side wall 2 is completed, a chiseling strip 6 is laid at the top surface of the corresponding construction joint of the small side wall 2. In order to ensure the connection strength between the first and the second poured concrete, the chiseling area of the construction joint is not less than 75% of the surface area of the construction joint, and the chiseling depth is not less than 8 mm. The range of the construction joint of the small side wall that needs to be chiseled is within the range of the double-layer main reinforcement 3 of the small side wall, and no reinforcement is required within the chiseling range; the chiseling strip 6 is cut on-site according to the preset laying area, and a release agent is applied to the end surface of the chiseling strip corresponding to the fitting, and it is laid along the axial direction of the tunnel, and the chiseling strip is compacted to make it fit tightly with the top surface of the small side wall; the entire chiseling strip is integrally formed, and the operation is convenient. Compared with the manual chiseling operation between the double-layer main reinforcement using a pneumatic pick, the construction efficiency of the chiseling strip is greatly improved, and the chiseling quality is higher.
[0032] See also Figure 3 , Figure 4 The roughening belt 6 is a rubber material, which includes a large-toothed roughening belt 7 and a small-toothed roughening belt 8. The roughening belt is used to fit the end face of the small side wall. The array is arranged with a number of convex teeth for forming roughening grooves. The convex teeth are pyramidal, and the cross-section of the convex teeth is an inverted right triangle. The convex tooth height and surface area of the large-toothed roughening belt 7 are greater than the convex tooth height and surface area of the small-toothed roughening belt 8. The large-toothed roughening belt 7 is used for fine stone concrete, and the small-toothed roughening belt 8 is used for medium-coarse stone concrete. For concrete with different material ratios, a roughening belt with a corresponding tooth height is selected, and the construction is flexible to ensure the roughening surface molding effect and quality; the roughening belt has low construction loss, and each roughening belt can be reused more than 50 times, which greatly reduces the construction cost.
[0033] S6: After the initial setting of the concrete of the small side wall 2, the roughening belt 6 is removed in time. When removing the roughening belt 6, it is removed from the right angle of the convex teeth to the triangular inclined surface to avoid damaging the concrete roughening structure. At this time, a pit corresponding to the roughening belt 6 is formed on the concrete surface of the small side wall 2. After the concrete is completely solidified, the concrete surface achieves the roughening effect of the construction joint.
[0034] Although some preferred embodiments of the present application have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present application.
[0035] Obviously, those skilled in the art can make various changes and modifications to the present application without departing from the spirit and scope of the inventive concept. Thus, if these modifications and variations of the present application fall within the scope of the claims of the present application and their equivalents, the present application is also intended to include these modifications and variations.
Claims
1. A method for constructing a small side wall construction joint of a tunnel lining, characterized in that: include: S1: Tie up the steel skeleton of the tunnel invert and small side wall; S2: Install the end formwork and side formwork of the tunnel invert and small side wall and reinforce them; S3: pouring concrete into the enclosed area of the end formwork and the side formwork of the tunnel invert, and finishing the concrete surface after vibrating and compacting; S4: pour concrete into the enclosed area of the end formwork and the side formwork of the small side wall, vibrate and compact it, and then add slurry to finish the concrete surface; S5: laying a roughening tape at the top end surface of the small side wall corresponding to the construction joint, and compacting the roughening tape to make it fit tightly with the top end surface of the small side wall; the roughening tape is used to fit the end surface of the small side wall and is arranged with a plurality of convex teeth in an array for forming roughening grooves; S6: After the concrete of the small side wall has initially set, the roughening tape is removed, and after the concrete has completely set, the construction joint is completed.
2. The method for constructing a tunnel lining small side wall construction joint according to claim 1, characterized in that: In step S2, the end formwork and side formwork of the tunnel invert and small side wall are steel structure formworks; the end formworks of the tunnel invert and small side wall are arranged at both ends of the tunnel invert and small side wall; the side formworks of the tunnel invert and small side wall are arranged on one side of the tunnel invert and small side wall close to the center of the tunnel.
3. The method for constructing a tunnel lining small side wall construction joint according to claim 1, wherein: In the step S4, the height of the slurry is 1.5 to 2 cm.
4. The method for constructing a tunnel lining small side wall construction joint according to claim 1, characterized in that: In the step S5, before the chiseled tape is laid, a release agent is applied to the end surface of the chiseled tape to be bonded.
5. The method for constructing a tunnel lining small side wall construction joint according to claim 1, characterized in that: In step S5, the top end surface of the small side wall is horizontal, the area of the roughening belt is not less than 75% of the surface area of the top end surface of the small side wall, and the height of the convex teeth of the roughening belt is not less than 8 mm.
6. The method for constructing a small side wall construction joint of a tunnel lining according to claim 1, characterized in that: In the step S5, the protruding teeth are pyramid-shaped.
7. The method for constructing a small side wall construction joint of a tunnel lining according to claim 1, characterized in that: In the step S5, the height of the protruding teeth of the chiseling belt for fine stone concrete is greater than the height of the protruding teeth of the chiseling belt for medium-coarse stone concrete.