Preparation method of electrochemical sensing glove for detecting chemical toxic agent marker
Through the screen printing electrode technology of Cu-BTC and Au@Cu-BTC electrode modification materials, the problem of low selectivity and sensitivity of chemical warfare hydrolysate detection in existing electrochemical detection technology is solved, and EMPA and IMPA are realized It is fast and accurate detection of TDG, suitable for field applications in the field.
Patent Information
- Application Number
- CN202411286450.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-09-13
Smart Images

Figure CN119044270A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of detection of chemical agent markers, and in particular to a method for preparing an electrochemical sensing glove for detecting chemical agent markers. Background Art
[0002] Chemical warfare agents (CWAs) are characterized by high toxicity, rapid onset, and the potential to cause systemic poisoning. The threat posed by CWAs to international peace and security has raised serious concerns due to their rapid action, strong toxicity, and widespread destructive potential. Typical chemical warfare agents are divided into two categories: nerve agents, including sarin (GB), soman (GD), VX, and mustard gas (HD). For example, HD nerve gas can be hydrolyzed in an aqueous environment to form ethyl methyl phosphate (EMPA) and isopropyl methyl phosphate (IMPA). Mustard gas (HD) can generate thiodiglycol (TDG) as a toxic blistering agent. Compounds such as EMPA, IMPA, or TDG are considered environmental markers that can be used to track whether chemical warfare agents have been used intentionally or accidentally.
[0003] It is crucial to develop a simple, rapid and accurate method to detect trace levels of chemical warfare agents in the environment. In the past few decades, a variety of methods for chemical warfare agent detection have been established, such as gas chromatography-mass spectrometry (GC-MS), liquid chromatography-mass spectrometry (LC-MS), mass spectrometry imaging and surface-enhanced Raman spectroscopy. However, expensive instruments or professional personnel limit their application. Therefore, it is urgent to develop cost-effective, user-friendly and practical field detection methods to identify chemical warfare agents in realistic environments for military and civilian use.
[0004] Electrochemical detection is used to determine the electrochemical activity and reaction characteristics of substances on the electrode surface, and the detection of substances is achieved by observing changes in current, voltage or impedance. Electrochemical technology has attracted much attention due to its advantages such as high sensitivity, good selectivity, simple operation and low cost. Electrochemical detection can achieve real-time detection on site. The hydrolysis products of CWAs have high chemical stability and are difficult to participate in electrochemical redox reactions. Therefore, they usually show limited electrochemical activity, which often leads to low selectivity, low sensitivity and reproducibility. The application of modified electrodes solves this problem. However, electrode modification still has challenges such as high material cost, complex preparation process and insufficient stability. Therefore, people have been studying catalytic materials that can provide good sensing performance and sensitivity of electrochemical sensors. Summary of the invention
[0005] To solve the above problems, the present invention synthesized Cu-BTC and Au@Cu-BTC electrode modification materials with high sensitivity and selective response to the hydrolysis products of CWAs (EMPA, IMPA and TDG), and constructed a screen-printed electrode (SPE) electrochemical sensing glove with the above materials as the core to achieve rapid and sensitive detection of CWAs markers. Compared with traditional technologies, this detection method is simpler and faster, with low detection sensitivity, and can achieve field detection.
[0006] To achieve the above object, the present invention adopts the following technical solution:
[0007] Step 1: Preparation of Cu-BTC and Au@Cu-BTC electrode modification materials
[0008] (1) Preparation of Cu-BTC
[0009] Weigh copper nitrate trihydrate (Cu(NO3)2·3H2O) and dissolve it in ethanol solution, then add acetic acid and trimethylamine in turn and stir evenly. Then, add trimesic acid (H3BTC) to the solution, stir evenly, and transfer to a polytetrafluoroethylene-lined autoclave. After continuous heating and heat preservation for a period of time, cool naturally to room temperature, centrifuge, and wash with ethanol several times.
[0010] (2) Preparation of gold nanoparticles (AuNPs)
[0011] In order to obtain AuNPs aqueous solution, a mixed aqueous solution of tetrachloroauric acid (HAuCl4) and sodium citrate is treated with low-temperature plasma driven by alternating current. The plasma jet is placed above the solution. The plasma jet uses a needle-ring electrode structure as a high-voltage electrode. A copper strip is wrapped around the surface of the quartz tube as a ground electrode. After a period of plasma treatment, the color of the solution gradually changes from light yellow to pink, and Au nanoparticles are obtained.
[0012] (3) Preparation of Au@Cu-BTC
[0013] Cu-BTC and polyvinyl pyrrolidone (PVP) were dissolved in an ethanol solution, and then the prepared AuNPs were added during stirring. The mixture was vigorously stirred at room temperature. The sample was then centrifuged and washed to obtain Au@Cu-BTC.
[0014] Step 2: Preparation of SPE based on Cu-BTC and Au@Cu-BTC
[0015] (1) The screen-printed electrode was immersed in a sulfuric acid solution and subjected to cyclic voltammetry scanning, and then washed with ultrapure water and dried to obtain an activated screen-printed electrode.
[0016] (2) Adding Cu-BTC and Au@Cu-BTC suspensions to the surface of the above electrodes and drying them at room temperature to obtain Cu-BTC / SPE and Au@Cu-BTC / SPE electrodes.
[0017] Step 3: Preparation of SPE electrochemical sensing gloves
[0018] The Cu-BTC / SPE and Au@Cu-BTC / SPE electrodes obtained in step 2 were combined with protective gloves to prepare sensing gloves. Cu-BTC / SPE was loaded on the index finger to form IF / Cu-BTC / SPE, which was used for EMPA detection; Cu-BTC / SPE was loaded on the middle finger to form MF / Cu-BTC / SPE, which was used for IMPA detection; Au@Cu-BTC / SPE was loaded on the ring finger to form RF / Au@Cu-BTC / SPE, which was used for TDG detection.
[0019] Step 4: SPE electrochemical sensing gloves performance test
[0020] (1) Phosphate buffered saline (PBS) and different concentrations of EMPA, IMPA and TDG solutions were added dropwise onto the surface of the screen-printed electrode prepared in step 2.
[0021] (2) Cyclic voltammetry is used to activate and stabilize the electrode.
[0022] (3) The screen-printed electrode to which PBS buffer was added was subjected to differential pulse voltammetry (DPV) measurement, and its response current was recorded as I0.
[0023] (4) The DPV current change of the screen-printed electrode with different concentrations of EMPA was measured and the current response was recorded. Finally, the standard curve was drawn with the current change as the ordinate and the EMPA concentration as the abscissa, and the scanning voltage was -0.6 to 0.6 V, and the detection limit (LOD) was calculated.
[0024] (5) The DPV current change of the screen-printed electrode with different concentrations of IMPA was measured and the current response was recorded. Finally, a standard curve was drawn with the current change as the ordinate and the IMPA concentration as the abscissa, and the detection limit (LOD) was calculated.
[0025] (6) The DPV current change of the screen-printed electrode with different concentrations of TDG was measured and the current response was recorded. Finally, a standard curve was drawn with the current change as the ordinate and the TDG concentration as the abscissa, and the detection limit (LOD) was calculated.
[0026] As a further scheme of the present invention: the optional range of the volume of the ethanol solution in step 1 is 100-120 mL, the preferred range of the mass of copper nitrate trihydrate is 1.0 g-4.35 g, the preferred volume of acetic acid is 6-10 mL, the preferred range of the volume of trimethylamine is 5.0-10 mL, and the preferred range of the mass of trimesic acid is 2.10-4.50 g.
[0027] As a further solution of the present invention: the stirring time in step 1 is preferably 0.5 h,
[0028] As a further solution of the present invention: in step 1, the heating temperature is preferably 100° C., and the insulation time is preferably in the range of 12 to 24 hours.
[0029] As a further solution of the present invention: in step 1, the mixing ratio of HAuCl4 and sodium citrate is 1:5-1:10, the plasma jet is placed 1-3 cm above the solution, the inner diameter of the high-voltage electrode hollow stainless steel tube is 1.5 mm, the wall thickness is 0.1 mm, and the length is 150 mm. The copper strip is 10 mm wide and 180 μm thick, and the plasma treatment time is 30-90 s.
[0030] As a further solution of the present invention: the mixing ratio of Cu-BTC and polyvinyl pyrrolidone in step 1 is 1:10, dissolved in 50-100 mL of ethanol solution, 0.1-1 g of AuNPs is added, and the mixture is vigorously stirred for 1-2 h.
[0031] As a further solution of the present invention: in step 1, the centrifugal speed is 8000-10000 rpm, and the time is 5-10 minutes.
[0032] As a further solution of the present invention: the mass fraction of the sulfuric acid solution in step 2 is 1% to 5%, and the cyclic voltammetry scanning voltage is -1V to 1V.
[0033] As a further solution of the present invention: in step 2, 1 to 100 μL of 5 mg / mL Cu-BTC and Au@Cu-BTC suspension is added.
[0034] As a further solution of the present invention: the pH value of the phosphate buffered saline solution in step 3 is 6, and the concentrations of EMPA, IMPA and TDG solutions are 1 ng / mL to 100 μg / mL.
[0035] As a further solution of the present invention: in step 3, the scanning voltage range of the cyclic voltammetry is -1V to 1V, the scanning speed is 20mV / s to 50mV / s, and the number of scanning circles is 5 to 10 circles.
[0036] As a further solution of the present invention: in step 3, the scanning voltage of the differential pulse voltammetry is -0.6 to 0.6 V, and the scanning rate is 0.005 V s -1 , pulse amplitude is 0.05V, sampling width is 0.05s, pulse period is 0.5s, sensitivity is 1.0×10 -3 AV -1 .
[0037] The beneficial effects of the present invention are:
[0038] 1. The Cu-BTC layered metal organic framework material constructed by the present invention has the characteristics of large specific surface area, strong surface reactivity, strong electron transfer ability, easy functionalization and composite, etc., which can effectively improve and enhance the performance of electrochemical sensors and effectively improve their electronic properties and conductivity. The Cu-BTC material can be 2+ and organic ligands to adjust its physical and chemical properties, making it multifunctional. Cu has excellent conductivity, which is conducive to the transmission of electrical signals. 2+ Cu-BTC has a strong affinity for P=O and is used for electrochemical sensing of organophosphorus compounds, which improves the sensitivity of electrochemical detection and enables rapid and reliable detection of EMPA and IMPA.
[0039] 2. Combining AuNPs and Cu-BTC MOF materials to modify the surface of the screen-printed electrode can not only improve the conductivity of the electrode surface, enhance electron transfer, and effectively amplify the detection signal, but Au can also form an Au-S bond with the S element in TDG to achieve electrochemical detection of TDG.
[0040] 3. Combining the modified screen-printed electrodes with protective gloves can realize the integration of protection and detection, and realize the rapid, convenient, sensitive and low-cost detection of nerve agent hydrolysis products EMPA and IMPA and mustard gas hydrolysis product TDG in a complex environment containing chemical agents. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] Figure 1 Schematic diagram of electrochemical sensing gloves based on Cu-BTC / SPE and Au@Cu-BTC / SPE
[0042] Figure 2 Schematic diagram of the preparation process of electrochemical detection system based on Cu-BTC / SPE and Au@Cu-BTC / SPE
[0043] Figure 3 (A) SEM images of Cu-BTC, (B) Au@Cu-BTC, (C) TEM images of AuNPs
[0044] Figure 4 (A) DPV response curve of the electrochemical sensor based on IF / Cu-BTC / SPE for detection of EMPA solutions with different concentrations, (B) fitting curve between DPV current response and EMPA concentration.
[0045] Figure 5 (A) DPV response curve of the electrochemical sensor based on MF / Cu-BTC / SPE for the detection of IMPA solutions with different concentrations, (B) fitting curve between DPV current response and IMPA concentration.
[0046] Figure 6 (A) DPV response curve of the electrochemical sensor based on RF / Au@Cu-BTC / SPE for TDG solutions with different concentrations, (B) fitting curve between DPV current response and TDG concentration.
[0047] In the figure, 1. protective gloves; 2. screen printed (SPE) electrode; 6. adapter; 3. counter electrode (3); 4. working electrode; 5. reference electrode; 41. Cu-BTC material; 42. Au@Cu-BTC material; 7. wire; 8. protective layer. DETAILED DESCRIPTION
[0048] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0049] The present invention adopts an electrochemical sensing glove based on Cu-BTC / SPE and Au@Cu-BTC / SPE, such as Figure 1 As shown, it includes a protective glove (1), a screen-printed (SPE) electrode (2) and an adapter (6). The SPE electrode is composed of a counter electrode (3), a working electrode (4) and a reference electrode (5), and the working electrode (4) is modified by two metal organic framework materials, Cu-BTC material (41) and Au@Cu-BTC material (42). The adapter (6) leads out three wires (7) at equal distances and is respectively connected to the three electrodes of the SPE, and a protective layer (8) is attached to the lead wires (7).
[0050] Figure 2The schematic diagram of the electrochemical detection system based on Cu-BTC / SPE and Au@Cu-BTC / SPE is shown in Figure 1. First, the Cu-BTC material was prepared by solvothermal synthesis, and then the tetrachloroauric acid was reduced by plasma technology to obtain gold nanoparticles. Finally, the gold nanoparticles were mixed with Cu-BTC to form Au@Cu-BTC material. Then, the working electrode (WE) fixed on the index and middle fingers of the glove was modified with 10.0μL Cu-BTC (5mg / mL) uniform solution. The index finger was named IF / Cu-BTC and applied to EMPA detection. The middle finger was called MF / Cu-BTC in IMPA. 10.0μL Au@Cu-BTC uniform solution (5mg / mL) was dropped on the ring finger WE to detect TDG, which was RF / Au@Cu-BTC. The electrochemical signals of hydrolysis products of different concentrations were measured by DPV to achieve fast and convenient detection.
[0051] The implementation steps are as follows:
[0052] 1. Preparation of Cu-BTC and Au@Cu-BTC electrode modified materials
[0053] (1) 4.35 g of zinc nitrate trihydrate, 6.2 mL of acetic acid and 5.0 mL of trimethylamine were added to 12 mL of ethanol in sequence. After stirring for 1 h, 2.10 g of trimesic acid was added to the solution. The mixture was stirred for 2 h to form a uniform solution, which was then transferred to a polytetrafluoroethylene-lined autoclave. The mixture was heated at 120 °C for 24 h, cooled naturally to room temperature, centrifuged and washed with ethanol for 3 to 5 times. Figure 3 (A) is a SEM characterization image of Cu-BTC. The Cu-BTC material has nano-scale particle size, a relatively smooth surface, and a layered porous structure. The layered porous structure is more conducive to the transmission of electrical signals, increases the peak current response, and improves the sensitivity of detection. This shows that the Cu-BTC material was successfully prepared.
[0054] (2) A mixed aqueous solution of tetrachloroauric acid (1.214 mM) and sodium citrate (34 mM) was treated with a low-temperature plasma driven by alternating current. The plasma jet was placed 1 cm above the solution. The plasma jet used a typical needle-ring electrode structure: a hollow stainless steel tube (inner diameter 1.5 mm, wall thickness 0.1 mm, length 150 mm) as a high-voltage electrode. A copper strip with a width of 10 mm and a thickness of 180 μm was wrapped around the surface of the quartz tube as a ground electrode. After 30 seconds, the color of the solution gradually changed from light yellow to pink, and AuNPs were obtained. Figure 3 (B) is the TEM image of AuNPs, which are evenly distributed without clustering, which is conducive to their uniform dispersion in Cu-BTC.
[0055] (3) 1 g Cu-BTC and 5 g PVP were dissolved in an ethanol solution and ultrasonicated for 30 min. Then, the prepared AuNPs (0.1 g) were added during the stirring process. The mixture was vigorously stirred at room temperature for 2 h. The sample was then centrifuged at 8000 rpm for 5 min and washed with ethanol three times. Finally, it was dried at 60 °C for 12 h to obtain Au@Cu-BTC. Figure 3 (C) is the SEM image of Au@Cu-BTC material. Due to the use of PVP, Cu-BTC presents a cohesive layered structure, and uniformly dispersed spherical AuNPs are observed, indicating that the Au@Cu-BTC material is successfully prepared.
[0056] 2. Preparation of SPE based on Cu-BTC and Au@Cu-BTC
[0057] (1) The screen-printed electrode is immersed in a 1% to 5% sulfuric acid solution and subjected to cyclic voltammetry scanning at a scanning voltage of -1 V to 1 V. It is then washed with ultrapure water and dried to obtain an activated screen-printed electrode.
[0058] (2) Add 10 μL of 5 mg / mL Cu-BTC and Au@Cu-BTC suspensions to the surface of the above electrodes and dry them at room temperature to obtain Cu-BTC / SPE and Au@Cu-BTC / SPE electrodes.
[0059] Step 3: Preparation of SPE electrochemical sensing gloves
[0060] The Cu-BTC / SPE and Au@Cu-BTC / SPE electrodes in step 2 were combined with protective gloves, including: the index finger was IF / Cu-BTC / SPE and was used for EMPA detection, the middle finger was MF / Cu-BTC / SPE and was used for IMPA, and the ring finger was RF / Au@Cu-BTC / SPE and was used for TDG detection.
[0061] Step 4: SPE electrochemical sensing gloves performance test
[0062] (1) A phosphate buffered saline (PBS) solution with a pH value of 6 and EMPA, IMPA and TDG solutions with a concentration of 1 ng / mL to 100 μg / mL were added dropwise onto the surface of the screen-printed electrode prepared in step 2.
[0063] (2) Cyclic voltammetry is used to activate and stabilize the electrode, with a scanning voltage range of -1V to 1V, a scanning speed of 20mV / s to 50mV / s, and a scanning number of 5 to 10 circles.
[0064] (3) The screen-printed electrode with PBS buffer added was subjected to differential pulse voltammetry (DPV) measurement, and its response current was recorded as I0. The scanning voltage was -0.6 to 0.6 V, and the scanning rate was 0.005 V s -1 , pulse amplitude is 0.05V, sampling width is 0.05s, pulse period is 0.5s, sensitivity is 1.0×10 -3 AV -1 .
[0065] (4) Measure the DPV current change of the screen-printed electrode with different concentrations of EMPA added, and record the current response. Figure 4 Finally, the standard curve was drawn with the current change as the ordinate and the EMPA concentration as the abscissa, the scanning voltage was -0.6 to 0.6 V, and the detection limit (LOD) was calculated as shown in Figure 4 (B) shown.
[0066] (5) Measure the DPV current change of the screen-printed electrode with different concentrations of IMPA added, and record the current response, such as Figure 5 Finally, the standard curve was drawn with the current change as the ordinate and the IMPA concentration as the abscissa, and the detection limit (LOD) was calculated, as shown in Figure 5 (B) shown.
[0067] (6) Measure the DPV current change of the screen-printed electrode with different concentrations of TDG added, and record the current response, such as Figure 6 Finally, the standard curve was drawn with the current change as the ordinate and the TDG concentration as the abscissa, and the detection limit (LOD) was calculated, as shown in Figure 6 (B) shown.
[0068] 4. Detection of EMPA in actual water samples
[0069] Three water samples with different concentrations were selected, namely 1 ng / mL (sample 1), 10 ng / mL (sample 2), and 100 ng / mL (sample 3). 60 μL of water sample was added dropwise to IF / Cu-BTC / SPE. Differential pulse voltammetry (DPV) on the electrochemical workstation was used to detect EMPA solutions of different concentrations, and the corresponding response current was recorded: According to the working curve Y=35.23logC+276.7 obtained in step 3, the concentration of EMPA in each water sample was calculated. The test results are shown in Table 1.
[0070] Table 1 Detection of EMPA in real samples using IF / Cu-BTC sensor (n=3).
[0071]
[0072]
[0073] 5. Detection of IMPA in actual water samples
[0074] Three water samples with different concentrations were selected, namely 1 ng / mL (sample 1), 10 ng / mL (sample 2), and 100 ng / mL (sample 3). 60 μL of water sample was taken and dripped on MF / Cu-BTC / SPE. Differential pulse voltammetry (DPV) on the electrochemical workstation was used to detect IMPA solutions of different concentrations and the corresponding response current was recorded: According to the working curve Y=59.27logC+514.39 obtained in step 3, the concentration of IMPA in each water sample was calculated. The test results are shown in Table 2.
[0075] Table 2 MF / Cu-BTC sensor detects IMPA in actual samples (n=3).
[0076]
[0077] 5. Detection of TDG in actual water samples
[0078] Three water samples with different concentrations were selected, namely 1 ng / mL (sample 1), 10 ng / mL (sample 2), and 100 ng / mL (sample 3). 60 μL of water sample was added to RF / Au@Cu-BTC / SPE. Differential pulse voltammetry (DPV) on the electrochemical workstation was used to detect TDG solutions of different concentrations, and the corresponding response current was recorded: According to the working curve Y=199.27logC+1861.21 obtained in step 3, the concentration of TDG in each water sample was calculated. The test results are shown in Table 3.
[0079] Table 3 RF / Au@Cu-BTC / SPE sensor detects TDG in actual samples (n=3)
[0080]
Claims
1. An electrochemical sensing glove based on Cu-BTC and Au@Cu-BTC materials, comprising a protective glove (1), a screen printed (SPE) electrode (2) and an adapter (6). The SPE electrode is composed of a counter electrode (3), a working electrode (4) and a reference electrode (5), wherein the working electrode (4) is characterized in that: The adapter (6) is modified by two metal organic framework materials, namely, Cu-BTC material (41) and Au@Cu-BTC material (42). The adapter (6) leads out three wires (7) at equal distances, which are respectively connected to three electrodes of the SPE, and a protective layer (8) is attached to the lead wires (7).
2. A method for preparing an electrochemical sensing glove based on Cu-BTC and Au@Cu-BTC materials, using the electrochemical sensing glove based on Cu-BTC and Au@Cu-BTC materials according to claim 1, characterized in that The method comprises the following steps: Step 1: Preparation of Cu-BTC and Au@Cu-BTC electrode modification materials (1) Preparation of Cu-BTC Weigh copper nitrate trihydrate (Cu(NO3)2·3H2O) and dissolve it in ethanol solution, then add acetic acid (CH3COOH) and trimethylamine (C3H9N, TMA) in turn and stir evenly. Then, add trimesic acid (H3BTC) to the solution, stir evenly, and transfer it to a polytetrafluoroethylene-lined autoclave. After continuous heating and heat preservation for a period of time, cool it naturally to room temperature, centrifuge it, and wash it with ethanol several times. (2) Preparation of gold nanoparticles (AuNPs) In order to obtain AuNPs aqueous solution, a mixed aqueous solution of tetrachloroauric acid (HAuCl4) and sodium citrate was treated with low-temperature plasma driven by alternating current. The plasma jet was placed above the solution, and the plasma jet used a needle-ring electrode structure as a high-voltage electrode, and a copper strip was wrapped around the surface of the quartz tube as a ground electrode. After a period of plasma treatment, the color of the solution gradually changed from light yellow to pink, and Au nanoparticles were obtained. (3) Preparation of Au@Cu-BTC Cu-BTC and polyvinyl pyrrolidone (PVP) were dissolved in an ethanol solution, and then the prepared AuNPs were added during stirring. The mixture was vigorously stirred at room temperature, and then the sample was centrifuged and washed to obtain Au@Cu-BTC. Step 2: Preparation of SPE based on Cu-BTC and Au@Cu-BTC (1) The SPE was immersed in a sulfuric acid solution, subjected to cyclic voltammetry scanning, and then washed with ultrapure water and dried to obtain an activated screen-printed electrode. (2) Adding Cu-BTC and Au@Cu-BTC suspensions to the surface of the above electrodes and drying them at room temperature to obtain Cu-BTC / SPE and Au@Cu-BTC / SPE electrodes. Step 3: Preparation of SPE electrochemical sensing gloves The Cu-BTC / SPE and Au@Cu-BTC / SPE electrodes obtained in step 2 were combined with protective gloves, and Cu-BTC / SPE was loaded on the index finger to form IF / Cu-BTC / SPE, which was used for EMPA detection; / Cu-BTC / SPE was loaded on the middle finger to form MF / Cu-BTC / SPE, which was used for IMPA detection; Au@Cu-BTC / SPE was loaded on the ring finger to form RF / Au@Cu-BTC / SPE, which was used for TDG detection. Step 4: SPE electrochemical sensing gloves performance test (1) Phosphate buffered saline (PBS) and different concentrations of EMPA, IMPA and TDG solutions were added dropwise onto the surface of the screen-printed electrode prepared in step 2. (2) Cyclic voltammetry is used to activate and stabilize the electrode. (3) The screen-printed electrode to which PBS buffer was added was subjected to differential pulse voltammetry (DPV) measurement, and its response current was recorded, which was denoted as I0. (4) The DPV current change of the screen-printed electrode with different concentrations of EMPA was measured and the current response was recorded. Finally, the standard curve was drawn with the current change as the ordinate and the EMPA concentration as the abscissa, and the scanning voltage was -0.6 to 0.6 V, and the detection limit (LOD) was calculated. (5) The DPV current change of the screen-printed electrode with different concentrations of IMPA was measured and the current response was recorded. Finally, a standard curve was drawn with the current change as the ordinate and the IMPA concentration as the abscissa, and the detection limit (LOD) was calculated. (6) The DPV current change of the screen-printed electrode with different concentrations of TDG was measured and the current response was recorded. Finally, a standard curve was drawn with the current change as the ordinate and the TDG concentration as the abscissa, and the detection limit (LOD) was calculated.
3. The method for preparing an electrochemical sensing glove based on Cu-BTC and Au@Cu-BTC materials according to claim 2, characterized in that: In step 1, the volume of the ethanol solution can be selected in the range of 100 to 120 mL, the mass of copper nitrate trihydrate is preferably in the range of 1.0 g to 4.35 g, the preferred volume of acetic acid is 6 to 10 mL, the preferred volume of trimethylamine is 5.0 to 10 mL, and the preferred mass of trimesic acid (H3BTC) is 2.10 to 4.50 g. The stirring time is preferably 0.5 h, the heating temperature is preferably 100 ° C, and the insulation time is preferably in the range of 12 to 24 h. The mixing ratio of HAuCl4 and sodium citrate is 1:5 to 1:10, the plasma jet is placed 1 to 3 cm above the solution, the inner diameter of the high-voltage electrode hollow stainless steel tube is 1.5 mm, the wall thickness is 0.1 mm, and the length is 150 mm. The copper strip is 10 mm wide and 180 μm thick, and the plasma treatment time is 30 to 90 s. The mixing ratio of Cu-BTC and polyvinyl pyrrolidone is 1:10, dissolved in 50-100 mL of ethanol solution, and 0.1-1 g of AuNPs is added. The mixture is vigorously stirred for 1-2 hours. The centrifugal speed is 8000-10000 rpm, and the time is 5-10 minutes.
4. The method for preparing an electrochemical sensing glove based on Cu-BTC and Au@Cu-BTC materials according to claim 2, characterized in that: The mass fraction of the sulfuric acid solution in step 2 is 1% to 5%, and the cyclic voltammetry scanning voltage is -1 V to 1 V. The preferred volume range of the Cu-BTC and Au@Cu-BTC suspensions is 1 to 100 μL, and the preferred concentration is 5 mg / mL.
5. The method for preparing an electrochemical sensing glove based on Cu-BTC and Au@Cu-BTC materials according to claim 2, characterized in that: The pH value of the phosphate buffer solution in step 3 is 6, and the concentrations of EMPA, IMPA and TDG solutions are 1 ng / mL to 100 μg / mL. The scanning voltage range of cyclic voltammetry is -1V to 1V, the scanning speed is 20mV / s to 50mV / s, and the number of scanning circles is 5 to 10 circles. The scanning voltage of differential pulse voltammetry is -0.6 to 0.6V, and the scanning rate is 0.005V s -1 , pulse amplitude is 0.05V, sampling width is 0.05s, pulse period is 0.5s, sensitivity is 1.0×10 -3 AV -1 .
Citation Information
Patent Citations
Electrochemical sensor on basis of hierarchical porous Cu-BTC materials and application of electrochemical sensor to detecting glyphosate in pesticides
CN107271522A
Method for detecting nereistoxin insecticide based on neurotoxin promoting electron transfer effect
CN110632158A
Electrochemical SERS (Surface Enhanced Raman Scattering) dual-mode sensor based on wearable flexible glove and preparation and application thereof
CN116559144A
Devices and methods to detect and quantify trace gases
US9329154B1
Cited By
A dual-functional electrochemical and surface-enhanced raman spectroscopy sensing element with metal-organic framework
TWI939135B