Multi-layer metal insulation substrate of power module and preparation method of multi-layer metal insulation substrate

By introducing multi-layer metal insulating substrate structure and heating and pressurization technology of high thermal conductivity insulating materials into the power module, the mutual inductance cancellation layer is solved, and the problems of complex substrate processing and large stray inductance in the existing technology are achieved, and more efficient Switching performance and easier preparation process.

CN119050103AActive Publication Date: 2024-11-29FUDAN UNIVERSITY
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411138836.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-29
Estimated Expiration
2044-08-19

AI Technical Summary

Technical Problem

The metal insulating substrates in the main circuit of the existing power module have complex processing technology, high energy consumption and short life, and the large stray inductors lead to high switching energy loss, which limits the high frequency development of power modules.

Method used

Using a multi-layer metal insulating substrate structure, the layers are superimposed and fixed by setting up functional layers, base layers and offset layers, and using high thermal conductivity insulation materials and heating and pressurization technology, introducing mutual inductance cancellation to reduce stray inductance.

Benefits of technology

It significantly reduces the switching energy loss of the power module, improves switching performance, simplifies the preparation process, improves design flexibility and heat dissipation effect, and the process is more energy-saving and environmentally friendly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure HDA0005000168680000011
    Figure HDA0005000168680000011
  • Figure HDA0005000168680000021
    Figure HDA0005000168680000021
Patent Text Reader

Abstract

The invention relates to a multi-layer metal insulation substrate of a power module and a preparation method thereof, the multi-layer metal insulation substrate comprises a functional layer, the functional layer comprises a lower bridge arm metal layer and an upper bridge arm metal layer which are respectively arranged on the left and the right, a base layer is arranged below the functional layer, and an offset layer is arranged between the base layer and the functional layer. The counteracting layer comprises a first counteracting current-conducting plate, a counteracting insulating layer and a second counteracting current-conducting plate which are transversely fixed from top to bottom in sequence; the left side of the first counteracting current-conducting plate is electrically connected with the left side of the second counteracting current-conducting plate; the basic insulating plate, the offset insulating plate and the insulating sheets are all made of a high-thermal-conductivity insulating material; according to the invention, the switching energy loss of the power module can be effectively reduced, the switching performance of the power module is further remarkably improved, the technical development is promoted in the high-frequency direction of the power module, and meanwhile, the number of layers of the substrate can be increased according to needs, so that the vertical space is fully utilized, and the interconnection density is improved; and the substrate can be partitioned according to requirements so as to improve the heat dissipation effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of power modules, and in particular to a multilayer metal insulating substrate of a power module and a preparation method thereof. Background Art

[0002] A power module is an electronic component that converts electrical energy into different power forms. Its main function is to convert DC power in equipment such as motor drivers, UPS power supplies, frequency converters, and green energy into AC power, or to convert high-voltage, high-current DC power into low-voltage, low-current power. Power modules have the advantages of high efficiency, high stability, low cost, and low noise, providing strong support for power electronics, industrial automation, and green energy. The power module consists of two parts: the main circuit and the drive circuit. The main circuit usually consists of components such as chips, substrates, and heat sinks, and is used to control and adjust power parameters such as current and voltage. The drive circuit is used to provide control and protection signals, control the main circuit power switch, and make it output the required current and voltage to ensure safe operation of the circuit.

[0003] The substrate structure in the main circuit of the power module currently on the market is usually a three-layer structure, which is a metal conductive layer used to fix the chip and play a role in power transmission, an insulating layer fixed at the bottom of the metal conductive layer, and a metal heat dissipation layer fixed at the bottom of the insulating layer; the processing technology of the metal insulating substrate of the existing power module is relatively complicated. Take the most mainstream DBC substrate as an example: it is formed by eutectic sintering of the ceramic layer and the copper layer by high temperature (1065℃) heating, and finally, according to the wiring requirements, the circuit is formed by etching; but bubbles will inevitably be generated on the bonding surface and will continue to form during subsequent use. It becomes larger, so the process is complicated, the energy consumption is high and the life is short; and because the current in the commutation circuit only flows through the metal conductive layer connected to the chip, there is only a single direction and the path is also long, which will increase the amount of stray inductance on the path when flowing through the metal conductive layer, so the total amount of stray inductance of the power module increases, and then the loss of switching energy remains high, which ultimately reduces the switching performance, and thus seriously restricts the high-frequency development of the power module. Therefore, reducing parasitic inductance to reduce switching losses has become a key point that urgently needs to be broken through in the field of power module technology. Summary of the invention

[0004] In view of the current status of the above-mentioned prior art, the technical problem to be solved by the present invention is to provide a multilayer metal insulating substrate of a power module and a preparation method thereof that can significantly improve the switching performance to promote the technological development in the high-frequency direction of the power module, and at the same time utilize the excellent bonding ability of high thermal conductivity insulating materials and adopt heating and pressurizing methods to stack and fix the functional layer, the offset layer and the base layer together to realize the preparation of the multilayer substrate more easily, and the preparation process is more energy-saving and environmentally friendly.

[0005] The technical solution adopted by the present invention to solve the above technical problems is: a multi-layer metal insulation substrate of a power module, including a functional layer, the functional layer includes a lower bridge arm metal layer and an upper bridge arm metal layer respectively arranged on the left and right, the upper bridge arm metal layer includes a first functional conductive plate arranged horizontally and a DC positive terminal fixed on the right side of the first functional conductive plate, and the lower bridge arm metal layer includes a second functional conductive plate arranged horizontally and an AC terminal fixed on the left side of the top of the second functional conductive plate, characterized in that:

[0006] A base layer is also provided below the functional layer, and the base layer includes a laterally arranged base insulating plate and a base metal plate laterally fixed to the bottom of the base insulating plate, and the bottoms of the first functional conductive plate and the second functional conductive plate are both fixed to the top of the base insulating plate.

[0007] A compensation layer is also provided between the base layer and the functional layer, and the compensation layer includes a first compensation conductive plate, a compensation insulating layer, and a second compensation conductive plate which are fixed laterally in sequence from top to bottom, and the bottom of the second compensation conductive plate is fixed on the top of the base insulating plate, and the first compensation conductive plate, the compensation insulating layer, and the second compensation conductive plate are respectively provided with a first accommodating cavity, a second accommodating cavity, and a third accommodating cavity which cooperate with each other, and the first functional conductive plate and the second functional conductive plate are both arranged in the first accommodating cavity, the second accommodating cavity, and the third accommodating cavity; the left side of the first compensation conductive plate is electrically connected to the left side of the second compensation conductive plate.

[0008] Preferably, a first positioning groove located below the DC positive terminal is opened on the right inner wall of the first accommodating cavity, and correspondingly, a second positioning groove located below the first positioning groove is opened on the right inner wall of the second accommodating cavity, and the compensation layer also includes a DC negative terminal fixed on the right side of the top of the second compensation conductive plate and arranged inside the second positioning groove, and an insulating sheet fixed between the DC positive terminal and the DC negative terminal and located inside the first positioning groove.

[0009] Preferably, a first groove is formed on the left edge of the first functional conductive plate, and correspondingly, a second groove cooperating with the first groove is formed on the right edge of the second functional conductive plate.

[0010] Preferably, the offset layer further comprises a plurality of overlapping wires arranged sequentially from front to back, and two ends of each overlapping wire are respectively electrically connected to the left edge of the first offset conductive plate and the left edge of the second offset conductive plate.

[0011] Preferably, the basic insulating board, the offset insulating board and the insulating sheet are all made of a high thermal conductivity insulating material.

[0012] A method for preparing a multilayer metal insulating substrate of a power module, characterized by comprising the following steps:

[0013] S1. Making a base layer: taking a piece of metal sheet with a complete shape as a base metal plate, and pasting a base insulating plate on the top of the base metal plate;

[0014] S2. Making functional layer:

[0015] S2.1. Select a metal sheet of appropriate size as the first functional conductive plate according to the number of upper bridge arm chips; then weld the DC positive terminal to the top right side of the first functional conductive plate;

[0016] S2.2. Select a metal sheet of appropriate size as the second functional conductive plate according to the number of lower bridge arm chips; and then fix the AC terminal to the left side of the top of the second functional conductive plate;

[0017] S3. Make an offset layer:

[0018] S3.1. First, a first accommodating cavity, a second accommodating cavity and a third accommodating cavity are respectively processed on the first offset conductive plate, the offset insulating plate and the second offset conductive plate;

[0019] S3.2, stacking the first offset conductive plate, the offset insulating plate and the second offset conductive plate in sequence and sticking them to each other on the top of the basic insulating plate;

[0020] S3.3, finally, welding the two ends of each lap wire to the left edge of the first offset conductive plate and the left edge of the second offset conductive plate respectively to electrically connect the two;

[0021] S4, integrating the base layer, the functional layer and the offset layer by step-by-step hot pressing or hot pressing at the same time;

[0022] S4.1. If a step-by-step hot pressing method is adopted, the first offset conductive plate, the offset insulating plate and the second offset conductive plate are first heated and pressurized so that the offset insulating plate is cured by the characteristics of its own material, and then the first offset conductive plate, the offset insulating plate and the second offset conductive plate are fixed together; then the second offset conductive plate is fixed on the top of the basic insulating plate to achieve insulation between layers; finally, the first functional conductive plate and the second functional conductive plate are placed in the first accommodating cavity, the second accommodating cavity and the third accommodating cavity and are both pasted on the top of the basic insulating plate and heated and pressurized so that the basic insulating plate is cured by the characteristics of its own material, and then the first functional conductive plate and the second functional conductive plate are fixed on the basic insulating plate.

[0023] S4.2. If the method of hot pressing is adopted, first place the first functional conductive plate and the second functional conductive plate in the first accommodating cavity, the second accommodating cavity and the third accommodating cavity and stick them on the top of the basic insulating plate; then heat and pressurize the first offset conductive plate, the offset insulating plate, the second offset conductive plate, the first functional conductive plate and the second functional conductive plate at the same time, and then use the curing characteristics of the offset insulating plate and the basic insulating plate's own materials to fix the first offset conductive plate, the offset insulating plate, the second offset conductive plate, the first functional conductive plate and the second functional conductive plate on the basic insulating plate at one time.

[0024] Preferably, the step S2.1 further comprises opening a first groove on the left edge of the first functional conductive plate to accommodate the right part of the bonding wire unit cooperating with each upper bridge arm chip.

[0025] Preferably, the step S2.2 further comprises opening a second groove cooperating with the first groove on the right edge of the second functional conductive plate to accommodate the left part of the bonding wire unit cooperating with each lower bridge arm chip.

[0026] Preferably, the step S3.3 further comprises welding two ends of each bridging wire to the left edge of the first offset conductive plate and the left edge of the second offset conductive plate respectively to electrically connect the two.

[0027] Compared with the prior art, the advantages of the present invention are: the present invention introduces mutual inductance cancellation effect around the chip by setting a cancellation layer, and then reduces the stray inductance of the power module through the mutual inductance cancellation effect, thereby effectively reducing the switching energy loss of the power module, and then significantly improving the switching performance of the power module to promote the technical development in the high-frequency direction of the power module; on the basis of ensuring the mutual inductance cancellation structure, the number of substrate layers can be increased as needed to fully utilize the vertical space and improve the interconnection density, and it has good design flexibility; the substrate can be partitioned and arranged and surrounded by the chip as needed, thereby increasing the thickness of the copper layer under the chip to improve the heat dissipation effect; in addition, the excellent bonding ability of high thermal conductivity insulating materials is reasonably utilized and the functional layer, the compensation layer and the base layer are stacked and fixed together by heating and pressurizing to realize the preparation of a multi-layer substrate in a relatively simple manner. The temperature and pressure required for the preparation process are relatively mild, with less material waste, and more energy-saving and environmentally friendly. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is the exploded structural diagram of the right front side of the present invention;

[0029] Figure 2 It is a preparation flow chart of the present invention. DETAILED DESCRIPTION

[0030] Unless otherwise defined, the technical terms or scientific terms used in the present invention should be understood by people with ordinary skills in the field to which the present invention belongs. The words "first", "second" and similar words used in the present invention do not indicate any order, quantity or importance, but are only used to distinguish different components. "Include" or "comprise" and similar words mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Connect" or "connected" and similar words are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0031] In order to keep the following description of the embodiments of the present invention clear and concise, detailed descriptions of well-known functions and well-known components are omitted.

[0032] like Figure 1 As shown, a multilayer metal insulating substrate of a power module includes a functional layer, the functional layer includes a lower bridge arm metal layer 2 and an upper bridge arm metal layer 1 respectively arranged on the left and right, the upper bridge arm metal layer 1 includes a first functional conductive plate 101 arranged horizontally and a DC positive terminal 103 fixed on the right side of the first functional conductive plate 101, the lower bridge arm metal layer 2 includes a second functional conductive plate 201 arranged horizontally and an AC terminal 203 fixed on the left side of the top of the second functional conductive plate 201; a base layer is also provided below the functional layer, the base layer includes a base insulating plate 4 arranged horizontally and a base metal plate 5 fixed horizontally at the bottom of the base insulating plate 4, the bottom of the first functional conductive plate 101 and the second functional conductive plate 201 are connected to each other. All parts are fixed on the top of the basic insulating plate 4; a compensation layer is also provided between the basic layer and the functional layer, and the compensation layer includes a first compensation conductive plate 6, a compensation insulating plate 7 and a second compensation conductive plate 8 which are fixed laterally from top to bottom, and the bottom of the second compensation conductive plate 8 is fixed on the top of the basic insulating plate 4, and the first compensation conductive plate 6, the compensation insulating plate 7 and the second compensation conductive plate 8 are respectively provided with a first accommodating cavity 61, a second accommodating cavity 71 and a third accommodating cavity 81 which cooperate with each other, and the first functional conductive plate 101 and the second functional conductive plate 201 are both arranged in the first accommodating cavity 61, the second accommodating cavity 71 and the third accommodating cavity 81; the left side of the first compensation conductive plate 6 is electrically connected to the left side of the second compensation conductive plate 8.

[0033] A first positioning groove 62 located below the DC positive terminal 103 is opened on the right inner wall of the first accommodating cavity 61. Correspondingly, a second positioning groove 72 located below the first positioning groove 62 is opened on the right inner wall of the second accommodating cavity 71. The compensation layer also includes a DC negative terminal 25 fixed on the right side of the top of the second compensation conductive plate 8 and arranged inside the second positioning groove 72, and an insulating sheet 24 fixed between the DC positive terminal 103 and the DC negative terminal 25 and located inside the first positioning groove 62.

[0034] A first groove 1011 is formed on the left edge of the first functional conductive plate 101 , and correspondingly, a second groove 2011 cooperating with the first groove 1011 is formed on the right edge of the second functional conductive plate 201 .

[0035] The compensation layer also includes a plurality of jumper wires 9 arranged sequentially from front to back, and two ends of each jumper wire 9 are electrically connected to the left edge of the first compensation conductive plate 6 and the left edge of the second compensation conductive plate 8 respectively.

[0036] The basic insulating plate 4 , the offset insulating plate 7 and the insulating sheet 24 are all made of a highly thermally conductive insulating material.

[0037] like Figure 2 As shown, a method for preparing a multi-layer metal insulating substrate of a power module comprises the following steps:

[0038] S1. Making a base layer: Take a piece of metal sheet with a complete shape as a base metal plate 5 (close to the outside of the module and away from the chip), and stick a base insulating plate 4 made of a high thermal conductivity insulating material on the top of the base metal plate 5;

[0039] S2. Making functional layer:

[0040] S2.1. Select a metal sheet of appropriate size as the first functional conductive plate 101 according to the number of upper bridge arm chips. The thickness of the first functional conductive plate 101 can be relatively thick so that the heat generated by the chip can be fully diffused. Open a first groove 1011 on the left edge of the first functional conductive plate 101 to accommodate the right part of the bonding wire unit 23 that cooperates with each upper bridge arm chip, and then weld the DC positive terminal 103 to the top right side of the first functional conductive plate 101.

[0041] S2.2. Select a metal sheet of appropriate size as the second functional conductive plate 201 according to the number of lower bridge arm chips. The thickness of the second functional conductive plate 201 can be relatively thick so that the heat generated by the chip can be fully diffused. A second groove 2011 that cooperates with the first groove 1011 is opened on the right edge of the second functional conductive plate 201 to accommodate the left part of the bonding wire unit 23 that cooperates with each lower bridge arm chip, and then the AC terminal 203 is fixed to the left side of the top of the second functional conductive plate 201.

[0042] S3. Make an offset layer:

[0043] S3.1, firstly, a first accommodating cavity 61, a second accommodating cavity 71 and a third accommodating cavity 81 are respectively processed on the first offset conductive plate 6, the offset insulating plate 7 and the second offset conductive plate 8;

[0044] S3.2, stack the first offset conductive plate 6, the offset insulating plate 7 and the second offset conductive plate 8 in sequence and stick them to each other on the top of the basic insulating plate 4;

[0045] S3.3, finally, the two ends of each bridging wire 9 are respectively welded to the left edge of the first offset conductive plate 6 and the left edge of the second offset conductive plate 8 to electrically connect the two;

[0046] S4. The base layer, functional layer and offset layer are integrated by step-by-step hot pressing or hot pressing at the same time. The integrated structure can undertake more complex and diverse electrical interconnection functions and improve the flexibility of module design.

[0047] S4.1. If a step-by-step hot pressing method is adopted, the first offset conductive plate 6, the offset insulating plate 7 and the second offset conductive plate 8 are first heated and pressurized so that the offset insulating plate 7 is cured by the characteristics of its own material, and then the first offset conductive plate 6, the offset insulating plate 7 and the second offset conductive plate 8 are fixed together; then the second offset conductive plate 8 is fixed on the top of the basic insulating plate 4 to achieve insulation between layers; finally, the first functional conductive plate 101 and the second functional conductive plate 201 are placed in the first accommodating cavity 61, the second accommodating cavity 71 and the third accommodating cavity 81 and are both pasted on the top of the basic insulating plate 4 and heated and pressurized so that the basic insulating plate 4 is cured by the characteristics of its own material, and then the first functional conductive plate 101 and the second functional conductive plate 201 are fixed on the basic insulating plate 4.

[0048] S4.2. If the hot pressing method is adopted, first place the first functional conductive plate 101 and the second functional conductive plate 201 in the first accommodating cavity 61, the second accommodating cavity 71 and the third accommodating cavity 81 and stick them on the top of the basic insulating plate 4; then heat and pressurize the first offset conductive plate 6, the offset insulating plate 7, the second offset conductive plate 8, the first functional conductive plate 101 and the second functional conductive plate 201 at the same time, and then use the curing characteristics of the offset insulating plate 7 and the basic insulating plate 4's own materials to fix the first offset conductive plate 6, the offset insulating plate 7, the second offset conductive plate 8, the first functional conductive plate 101 and the second functional conductive plate 201 on the basic insulating plate 4 at one time.

[0049] Packaging steps:

[0050] A plurality of upper bridge arm chips 102 are fixed on the top of the first functional conductive plate 101 in the upper bridge arm metal layer 1, and the gate region or source region of each upper bridge arm chip 102 is electrically connected to a plurality of first control terminals 104; similarly, a plurality of lower bridge arm chips 202 are fixed on the top of the second functional conductive plate 201 in the lower bridge arm metal layer 2, and the gate region or source region of each lower bridge arm chip 202 is electrically connected to a plurality of second control terminals 204.

[0051] A first metal conductive block 14 is fixed to the top source region of each upper bridge arm chip 102 and the top source region of each lower bridge arm chip 202, and a laterally distributed third insulating plate 11 is arranged above the upper bridge arm metal layer 1 and the lower bridge arm metal layer 2, and a lower bridge arm conductive plate 12 and an upper bridge arm conductive plate 13 are fixed to the bottom of the third insulating plate 11, which are arranged on the left and right sides respectively.

[0052] The ends of the first metal conductive blocks 14 located on each upper bridge arm chip 102 are fixed to the bottom of the upper bridge arm conductive plate 13 so that the top source region of each upper bridge arm chip 102 is electrically connected to the upper bridge arm conductive plate 13 through a first metal conductive block 14; the ends of the first metal conductive blocks 14 located on each lower bridge arm chip 202 are fixed to the bottom of the lower bridge arm conductive plate 12 so that the top source region of each lower bridge arm chip 202 is electrically connected to the lower bridge arm conductive plate 12 through a first metal conductive block 14.

[0053] Several second metal conductive blocks 15 are also fixed on the top of the second functional conductive plate 201 and the first offset conductive plate 6. The end of each second metal conductive block 15 located on the second functional conductive plate 201 is fixed to the bottom of the upper bridge arm conductive plate 13 to electrically connect the second functional conductive plate 201 with the upper bridge arm conductive plate 13. The end of each second metal conductive block 15 located on the first offset conductive plate 6 is fixed to the bottom of the lower bridge arm conductive plate 12 to electrically connect the first offset conductive plate 6 with the lower bridge arm conductive plate 12.

[0054] If a radiator is to be installed on the top, a metal connecting plate 10 needs to be fixed laterally on the top of the third insulating plate 11, or the metal connecting plate 10 can be directly replaced with a radiator to achieve heat dissipation without a bottom plate, which reduces the number of layers and improves the heat dissipation capacity.

[0055] Working principle:

[0056] The current of the commutation loop is input from the DC positive terminal 103 to the first functional conductive plate 101 and flows into each upper bridge arm chip 102. The current output from the top source region of each upper bridge arm chip 102 is conducted to the upper bridge arm conductive plate 13 via a first metal conductive block 14, and then conducted to the second functional conductive plate 201 via each second metal conductive block 15 fixed on the second functional conductive plate 201; then, the current output from the top source region of each lower bridge arm chip 202 is also conducted to the lower bridge arm conductive plate 12 via a first metal conductive block 14, and then conducted to the first offset conductive plate 6 via each second metal conductive block 15 fixed on the top of the first offset conductive plate 6, and then conducted to the second offset conductive plate 8 via each jumper 9, and finally conducted to the lower bridge arm conductive plate 12 via the DC negative terminal 103. Terminal 25 is output outward; in the above process, the area where mutual inductance cancellation occurs is between the first canceling conductive plate 6 and the second canceling conductive plate 8, because the current conducted to the second canceling conductive plate 8 is concentrated on its upper surface and the direction is from left to right, while the current conducted to the first canceling conductive plate 6 is concentrated on its lower surface and the direction is from right to left. In this way, based on the principle of proximity effect, the magnetic fields generated by the currents of the above two commutation circuits are in opposite directions, and then mutual inductance cancellation occurs, thereby reducing the total loop inductance, thereby reducing parasitic parameters, reducing losses, and improving switching performance; if single-sided heat dissipation is adopted, the heat sink can be installed at the bottom of the base metal plate 5; if double-sided heat dissipation is adopted, a heat sink needs to be installed on the top of the second metal heat dissipation plate 10.

[0057] The present invention introduces mutual inductance cancellation effect around the chip by arranging a cancellation layer, and then reduces the stray inductance of the power module through the mutual inductance cancellation effect, thereby effectively reducing the switching energy loss of the power module, and then significantly improving the switching performance of the power module to promote the technical development in the high-frequency direction of the power module; on the basis of ensuring the mutual inductance cancellation structure, the number of substrate layers can be increased as needed to fully utilize the vertical space and improve the interconnection density, and it has good design flexibility; the substrate can be partitioned and arranged around the chip as needed, thereby increasing the thickness of the copper layer under the chip to improve the heat dissipation effect; in addition, the excellent bonding ability of high thermal conductivity insulating materials is reasonably utilized and the functional layer, the compensation layer and the base layer are stacked and fixed together by heating and pressurizing to realize the preparation of a multi-layer substrate in a relatively simple manner. The temperature and pressure required for the preparation process are relatively mild, with less material waste, and more energy-saving and environmentally friendly.

[0058] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A multilayer metal insulating substrate of a power module, comprising a functional layer, the functional layer comprising a lower bridge arm metal layer and an upper bridge arm metal layer respectively arranged on the left and right sides, the upper bridge arm metal layer comprising a first functional conductive plate arranged horizontally and a DC positive terminal fixed on the right side of the first functional conductive plate, the lower bridge arm metal layer comprising a second functional conductive plate arranged horizontally and an AC terminal fixed on the left side of the top of the second functional conductive plate, characterized in that: A base layer is also provided below the functional layer, the base layer comprising a transversely arranged base insulating plate and a base metal plate transversely fixed to the bottom of the base insulating plate, the bottoms of the first functional conductive plate and the second functional conductive plate are both fixed to the top of the base insulating plate; A compensation layer is also provided between the base layer and the functional layer, and the compensation layer includes a first compensation conductive plate, a compensation insulating layer, and a second compensation conductive plate which are fixed laterally in sequence from top to bottom, and the bottom of the second compensation conductive plate is fixed on the top of the base insulating plate, and the first compensation conductive plate, the compensation insulating layer, and the second compensation conductive plate are respectively provided with a first accommodating cavity, a second accommodating cavity, and a third accommodating cavity which cooperate with each other, and the first functional conductive plate and the second functional conductive plate are both arranged in the first accommodating cavity, the second accommodating cavity, and the third accommodating cavity; the left side of the first compensation conductive plate is electrically connected to the left side of the second compensation conductive plate.

2. The multi-layer metal insulation substrate of a power module according to claim 1, characterized in that: A first positioning groove is provided on the right inner wall of the first accommodating cavity and is located below the DC positive terminal. Correspondingly, a second positioning groove is provided on the right inner wall of the second accommodating cavity and is located below the first positioning groove. The compensation layer also includes a DC negative terminal fixed on the right side of the top of the second compensation conductive plate and arranged inside the second positioning groove, and an insulating sheet fixed between the DC positive terminal and the DC negative terminal and located inside the first positioning groove.

3. The multi-layer metal insulation substrate of a power module according to claim 1, characterized in that: A first groove is formed on the left edge of the first functional conductive plate, and correspondingly, a second groove matching with the first groove is formed on the right edge of the second functional conductive plate.

4. The multi-layer metal insulation substrate of a power module according to claim 1, characterized in that: The offset layer also includes a plurality of overlapping wires arranged sequentially from front to back, and two ends of each overlapping wire are electrically connected to the left edge of the first offset conductive plate and the left edge of the second offset conductive plate respectively.

5. The multi-layer metal insulation substrate of a power module according to claim 2, characterized in that: The basic insulating plate, the offset insulating plate and the insulating sheet are all made of a high thermal conductivity insulating material.

6. A method for preparing a multilayer metal insulating substrate of a power module, characterized in that: The following steps are involved: S1. Making a base layer: taking a piece of metal sheet with a complete shape as a base metal plate, and pasting a base insulating plate on the top of the base metal plate; S2. Making functional layer: S2.

1. Select a metal sheet of appropriate size as the first functional conductive plate according to the number of upper bridge arm chips; and then weld the DC positive terminal to the top right side of the first functional conductive plate; S2.

2. Select a metal sheet of appropriate size as the second functional conductive plate according to the number of lower bridge arm chips; and then fix the AC terminal to the left side of the top of the second functional conductive plate; S3. Make an offset layer: S3.

1. First, a first accommodating cavity, a second accommodating cavity and a third accommodating cavity are respectively processed on the first offset conductive plate, the offset insulating plate and the second offset conductive plate; S3.2, stacking the first offset conductive plate, the offset insulating plate and the second offset conductive plate in sequence and sticking them to each other on the top of the basic insulating plate; S3.3, finally, welding the two ends of each lap wire to the left edge of the first offset conductive plate and the left edge of the second offset conductive plate respectively to electrically connect the two; S4, integrating the base layer, the functional layer and the offset layer by step-by-step hot pressing or hot pressing at the same time; S4.

1. If a step-by-step hot pressing method is adopted, the first offset conductive plate, the offset insulating plate and the second offset conductive plate are first heated and pressurized so that the offset insulating plate is cured by the characteristics of its own material, and then the first offset conductive plate, the offset insulating plate and the second offset conductive plate are fixed together; then the second offset conductive plate is fixed on the top of the basic insulating plate to achieve insulation between layers; finally, the first functional conductive plate and the second functional conductive plate are placed in the first accommodating cavity, the second accommodating cavity and the third accommodating cavity and are both pasted on the top of the basic insulating plate and heated and pressurized so that the basic insulating plate is cured by the characteristics of its own material, and then the first functional conductive plate and the second functional conductive plate are fixed on the basic insulating plate. S4.

2. If the method of hot pressing is adopted, first place the first functional conductive plate and the second functional conductive plate in the first accommodating cavity, the second accommodating cavity and the third accommodating cavity and stick them on the top of the basic insulating plate; then heat and pressurize the first offset conductive plate, the offset insulating plate, the second offset conductive plate, the first functional conductive plate and the second functional conductive plate at the same time, and then use the curing characteristics of the offset insulating plate and the basic insulating plate's own materials to fix the first offset conductive plate, the offset insulating plate, the second offset conductive plate, the first functional conductive plate and the second functional conductive plate on the basic insulating plate at one time.

7. The method for preparing a multi-layer metal insulating substrate of a power module according to claim 6, characterized in that: The step S2.1 further includes opening a first groove on the left edge of the first functional conductive plate to accommodate the right portion of the bonding wire unit that cooperates with each upper bridge arm chip.

8. The method for preparing a multi-layer metal insulating substrate of a power module according to claim 6, characterized in that: The step S2.2 also includes opening a second groove cooperating with the first groove on the right edge of the second functional conductive plate to accommodate the left part of the bonding wire unit cooperating with each lower bridge arm chip.

9. The method for preparing a multi-layer metal insulating substrate of a power module according to claim 6, characterized in that: The step S3.3 also includes welding two ends of each bridging wire to the left edge of the first offset conductive plate and the left edge of the second offset conductive plate to electrically connect the two.

Citation Information

Patent Citations

  • SiC double-sided cooling module with low parasitic inductance and high heat dissipation performance

    CN116314170A

  • Method for producing power semiconductor module

    CN1163481A

  • HIGH CURRENT, LOW SWITCHING LOSS SiC POWER MODULE

    WO2015175820A1