Preparation method of HJT solar cell

By adopting polished surface and multi-layer film layer structure in HJT solar cells and combining screen printing technology, the problems of large composite and poor passivation effect of the back fleece making process are solved, the battery performance and light utilization rate are improved, and the film layer contact is optimized .

CN119050203AInactive Publication Date: 2024-11-29HUAINAN YIHENG TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411170788.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The back fleece making process of the existing HJT solar cells has problems with large composite and poor passivation effect, and there are problems with the contact interface of the conventional film layer, which affects the battery performance.

Method used

Using N/P type silicon wafers as substrate, wet cleaning and oxide film growth form a polishing surface, deposit amorphous silicon and microcrystalline silicon film layers, combine high-work function and low-work function TCO film layers, and use a wire mesh The printing process completes the preparation of metal electrodes, and optimizes film contact and process matching.

Benefits of technology

The passivation effect and light utilization rate on the back of the battery are improved, the open circuit voltage and filling factor of the battery are enhanced, the recombination rate is reduced, and the film contact problem is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119050203A_ABST
    Figure CN119050203A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of an HJT solar cell, which belongs to the technical field of solar cells, and comprises the following steps: S1, preparing a textured surface on the front surface and a polished surface on the back surface by using an N / P type silicon wafer substrate; s2, an amorphous silicon film layer is deposited on the outer layer of the suede in the S1, then a microcrystalline silicon film layer is deposited, and the total thickness is 15-30 nanometers; s2, an amorphous silicon film layer is deposited on the outer layer of the polished surface in the step S1, then a microcrystalline silicon film layer is deposited, and the total thickness is 20-40 nanometers; s3, depositing a high work function TCO film layer on the outer layer of the microcrystalline silicon film layer; s4, depositing a low work function TCO film layer on the high work function TCO film layer; according to the battery back polishing structure, the effects that the recombination rate of the battery back is reduced and the passivation effect is obviously improved can be realized, so that the open-circuit voltage and the filling factor of the battery are obviously improved; and meanwhile, light reflection is enhanced through back polishing, so that light reflected back to the interior of the cell is absorbed again, and the light utilization rate is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of solar cells, and more specifically, to a method for preparing a HJT solar cell. Background Art

[0002] HJT cells have good photoelectric conversion efficiency, high bifaciality, low attenuation, no HID and other good characteristics, but their double-sided structure makes subsequent process development more difficult. The front side of the HJT cell is the light-receiving side where sunlight is mainly directly irradiated, while the back side is mainly reflected; therefore, there are obvious differences in the front and back processes.

[0003] The current heterojunction texturing and cleaning process is mainly double-sided texturing, that is, the texturing surfaces on the front and back sides are consistent. Due to the differences between the front and back sides of the heterojunction, the existing back-side texturing process has major problems: after back-side texturing, the back surface of the battery is highly composite and the passivation effect is poor; the work function of the conventional single-layer TCO film layer is poor in interface contact with the amorphous film layer and microcrystalline film layer of CVD and the silver paste of the silk-screen process, and the light transmittance of the conventional target film layer is slightly worse than that of the high-work-function composite film layer.

[0004] To this end, a method for preparing a HJT solar cell is proposed. Summary of the invention

[0005] In view of the problems existing in the prior art, the object of the present invention is to provide a method for preparing a HJT solar cell, which can improve the passivation effect.

[0006] To solve the above problems, the present invention adopts the following technical solutions.

[0007] A method for preparing a HJT solar cell comprises the following steps:

[0008] S1, using an N / P type silicon wafer substrate, preparing the front side as a velvet surface and the back side as a polished surface;

[0009] S2, depositing an amorphous silicon film layer on the outer layer of the velvet surface described in S1, and then depositing a microcrystalline silicon film layer, with a total thickness of 15 to 30 nanometers;

[0010] Depositing an amorphous silicon film layer on the outer layer of the polished surface described in S1, and then depositing a microcrystalline silicon film layer, with a total thickness of 20 to 40 nanometers;

[0011] S3, depositing a high work function TCO film layer on the outer layer of the microcrystalline silicon film layer;

[0012] S4, depositing a low work function TCO film layer on the high work function TCO film layer;

[0013] S5. After coating, the double-sided metal electrode is prepared using a screen printing process.

[0014] Furthermore, in S1, firstly, an N / P type silicon wafer is used as a substrate, and double-sided polishing is completed through a wet cleaning step;

[0015] Then, a tubular diffusion furnace is used to grow the oxide film; as a mask protection layer, it can protect the underlying silicon wafer from being corroded by the cleaning and texturing solution;

[0016] Then the front oxide film is removed through etching equipment;

[0017] Then, the texturing process is carried out through the cleaning texturing equipment. Because there is a mask protection layer on the back, it will not be corroded. Therefore, this step can only produce a single-sided textured silicon wafer, and an oxide film cleaning step is added after the texturing step to complete the cleaning of the oxide protective film on the back;

[0018] Finally, a clean silicon wafer surface structure is formed with a pyramid velvet surface on the front and a polished surface on the back.

[0019] Furthermore, in S2, an amorphous silicon film layer is first deposited on the velvet surface by a PECVD process, and then a microcrystalline silicon film layer is deposited, with a total thickness of 15 to 30 nanometers.

[0020] The back polished surface is first deposited with an amorphous silicon film layer, and then with a microcrystalline silicon film layer, with a total thickness of 20 to 40 nanometers;

[0021] Among them, the doping elements of the microcrystalline silicon film layer can be adjusted accordingly according to the properties of the silicon wafer; the amorphous silicon and microcrystalline silicon film layers can also be made into film layers with suitable properties such as oxidation and carbonization.

[0022] Furthermore, in S3, the prepared microcrystalline silicon thin film is used as a battery substrate, and a TCO high work function thin film and a low work function thin film are prepared on the battery substrate.

[0023] Furthermore, in S1, a tubular diffusion furnace is used to grow the oxide film; the oxide film serves as a mask protection layer to protect the underlying silicon wafer from being corroded by the cleaning and texturing solution.

[0024] N / P type silicon wafer is used as substrate, and then a tubular diffusion furnace is used to complete the oxide film growth; the oxide film is used as a mask protection layer to protect the lower silicon wafer from being corroded by the cleaning and texturing solution, and then a wet cleaning step is performed to complete double-sided polishing; a tubular diffusion furnace is used to complete the oxide film growth, and the oxide film is used as a mask protection layer to protect the lower silicon wafer from being corroded by the cleaning and texturing solution, and the front oxide film is removed by etching equipment; the texturing process is performed by the cleaning and texturing equipment, and at this time, the back side will not be corroded due to the presence of a mask protection layer, so this step can only produce a single-sided velvet silicon wafer, and an oxide film cleaning step is added after the texturing step to complete the cleaning of the oxide protection film on the back side, and finally a clean silicon wafer surface structure with a pyramid velvet surface on the front side and a polished surface on the back side is formed.

[0025] Through the PECVD process, an amorphous silicon film layer is first deposited on the velvet surface, and then a microcrystalline silicon film layer is deposited, with a total thickness of 15 to 30 nanometers. An amorphous silicon film layer is first deposited on the polished back surface, and then a microcrystalline silicon film layer is deposited, with a total thickness of 20 to 40 nanometers.

[0026] Among them, the doping elements of the microcrystalline silicon film layer can be adjusted accordingly according to the properties of the silicon wafer; amorphous silicon and microcrystalline silicon film layers can also be made into suitable oxidation, carbonization and other properties of the film layer

[0027] The TCO high work function film and low work function film are prepared on the substrate using PVD or RPD equipment; firstly, the high work function film layer is deposited to make the high work function film layer contact with the microcrystalline film and the microcrystalline silicon film, and then the low work function film layer is deposited to make contact with the silver paste external electrode, thereby finally achieving the effect of improving the technical difficulty of process matching between the TCO film layer and the microcrystalline silicon film and the upper and lower electrodes, and optimizing the contact problem between the film layers at the same time.

[0028] Compared with the prior art, the present invention has the following beneficial effects:

[0029] (1) After the back of the battery is polished, the recombination rate on the back of the battery decreases and the passivation effect is significantly increased, resulting in a significant increase in the open circuit voltage and fill factor of the battery; at the same time, the back polishing enhances the reflection of light, causing the light reflected back into the battery to be reabsorbed, thereby improving the utilization rate of light.

[0030] (2) The present invention can effectively reduce the back recombination of the battery, improve the battery passivation effect, and improve the film contact problem by polishing the back side and stacking a high work function TCO film layer and a work function TCO film layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 This is a schematic diagram of Example 1 of the present invention. DETAILED DESCRIPTION

[0032] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention; it is obvious that the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments, and all other embodiments obtained by ordinary technicians in this field based on the embodiments of the present invention without making creative work are within the scope of protection of the present invention.

[0033] Embodiment 1:

[0034] See also Figure 1 , a method for preparing a HJT solar cell, comprising the following steps:

[0035] S1, using an N / P type silicon wafer substrate, preparing the front side as a velvet surface and the back side as a polished surface;

[0036] S2, depositing an amorphous silicon film layer first on the outer layer of the velvet surface described in S1, and then depositing a microcrystalline silicon film layer, and depositing an amorphous silicon film layer first on the outer layer of the polished surface described in S1, and then depositing a microcrystalline silicon film layer;

[0037] S3, depositing a high work function TCO film layer on the outer layer of the microcrystalline silicon film layer;

[0038] S4, depositing a low work function TCO film layer on the high work function TCO film layer;

[0039] S5. After coating, the double-sided metal electrode is prepared using a screen printing process.

[0040] In S1, firstly, an N / P type silicon wafer is used as a substrate, and double-sided polishing is completed through a wet cleaning step;

[0041] Then a tubular diffusion furnace is used to complete the oxide film growth;

[0042] Then the front oxide film is removed through etching equipment;

[0043] Then the texturing equipment is cleaned and the texturing process is carried out, and an oxide film cleaning step is added after the texturing step to complete the cleaning of the oxide protective film on the back;

[0044] Finally, a clean silicon wafer surface structure is formed with a pyramid velvet surface on the front and a polished surface on the back.

[0045] In S2, an amorphous silicon film layer is first deposited on the textured surface, and then a microcrystalline silicon film layer is deposited; and an amorphous silicon film layer is first deposited on the polished surface, and then a microcrystalline silicon film layer is deposited.

[0046] In S3, the prepared microcrystalline silicon thin film is used as a battery substrate, and a TCO high work function thin film and a low work function thin film are prepared on the battery substrate.

[0047] In S1, a tubular diffusion furnace is used to grow an oxide film; the oxide film serves as a mask protection layer to protect the underlying silicon wafer from being corroded by a cleaning and texturing solution.

[0048] N / P type silicon wafer is used as substrate, and then a tubular diffusion furnace is used to complete the oxide film growth; the oxide film is used as a mask protection layer to protect the lower silicon wafer from being corroded by the cleaning and texturing liquid, and then a wet cleaning step is performed to complete double-sided polishing. After the back surface is polished, the back surface of the battery is reduced, and at the same time, the reflection of light is enhanced, resulting in the light reflected back into the battery being reabsorbed, thereby improving the utilization rate of light; a tubular diffusion furnace is used to complete the oxide film growth, and the oxide film is used as a mask protection layer to protect the lower silicon wafer from being corroded by the cleaning and texturing liquid, and the front oxide film is removed by etching equipment; the texturing process is performed by the cleaning and texturing equipment, and at this time, due to the presence of a mask protection layer on the back side, it will not be corroded, so this step can only produce a single-sided velvet silicon wafer, and an oxide film cleaning step is added after the texturing step to complete the cleaning of the back oxide protection film, and finally a clean silicon wafer surface structure with a pyramid velvet surface on the front side and a polished surface on the back side is formed.

[0049] Amorphous silicon and microcrystalline silicon films are deposited on the front and back sides in sequence through the PECVD process

[0050] PVD or RPD equipment is used to prepare TCO high work function film and low work function film on the substrate; first, the high work function film layer is deposited to make the high work function film layer contact with the microcrystalline film and the amorphous silicon film, and then the low work function film layer is deposited to make contact with the silver paste external electrode, thereby finally achieving the effect of improving the technical difficulty of process matching between the TCO film layer and the microcrystalline silicon film and the upper and lower electrodes, and optimizing the contact problem between the film layers.

[0051] Usage: Take N / P type silicon wafer as substrate, and then use tubular diffusion furnace to complete oxide film growth; use oxide film as mask protection layer to protect lower silicon wafer from being corroded by cleaning and texturing solution, and then complete double-sided polishing through wet cleaning step; remove front oxide film through etching equipment; use tubular diffusion furnace to complete oxide film growth, use oxide film as mask protection layer to protect lower silicon wafer from being corroded by cleaning and texturing solution, and perform texturing process through cleaning and texturing equipment. At this time, due to the existence of mask protection layer on the back side, it will not be corroded, so this step can only produce single-sided velvet silicon wafer, and add oxide film cleaning step after texturing step to complete the cleaning of oxide protection film on the back side, and finally form a clean silicon wafer surface structure with pyramid velvet surface on the front side and polished surface on the back side.

[0052] Through the PECVD process, an amorphous silicon film layer is first deposited on the velvet surface, and then a microcrystalline silicon film layer is deposited, with a total thickness of 15 to 30 nanometers. An amorphous silicon film layer is first deposited on the polished back surface, and then a microcrystalline silicon film layer is deposited, with a total thickness of 20 to 40 nanometers.

[0053] Among them, the doping elements of the microcrystalline silicon film layer can be adjusted accordingly according to the properties of the silicon wafer; amorphous silicon and microcrystalline silicon film layers can also be made into suitable oxidation, carbonization and other properties of the film layer

[0054] Prepare TCO high work function film and low work function film on substrate using PVD or RPD equipment;

[0055] First, a high work function film layer is deposited to make it contact with the microcrystalline film and the amorphous silicon film, and then a low work function film layer is deposited to make it contact with the silver paste external electrode, thereby ultimately achieving the effect of improving the technical difficulty of process matching between the TCO film layer and the microcrystalline silicon film and the upper and lower electrodes, while optimizing the contact problem between the film layers.

[0056] The above is only a preferred specific implementation of the present invention; however, the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical solution and its improved conception within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A method for preparing a HJT solar cell, Features: The following steps are involved: S1, using an N / P type silicon wafer substrate, preparing the front side as a velvet surface and the back side as a polished surface; S2, depositing an amorphous silicon film layer first on the outer layer of the velvet surface described in S1, and then depositing a microcrystalline silicon film layer, and depositing an amorphous silicon film layer first on the outer layer of the polished surface described in S1, and then depositing a microcrystalline silicon film layer; S3, depositing a high work function TCO film layer on the outer layer of the microcrystalline silicon film layer; S4, depositing a low work function TCO film layer on the high work function TCO film layer; S5. After coating, the double-sided metal electrode is prepared using a screen printing process.

2. The method for preparing a HJT solar cell according to claim 1, Features: In S1, firstly, an N / P type silicon wafer is used as a substrate, and double-sided polishing is completed through a wet cleaning step; Then a tubular diffusion furnace is used to complete the oxide film growth; Then the front oxide film is removed through etching equipment; Then the texturing equipment is cleaned and the texturing process is carried out, and an oxide film cleaning step is added after the texturing step to complete the cleaning of the oxide protective film on the back; Finally, a clean silicon wafer surface structure is formed with a pyramid velvet surface on the front and a polished surface on the back.

3. The method for preparing a HJT solar cell according to claim 2, Features: In S2, an amorphous silicon film layer is first deposited on the textured surface, and then a microcrystalline silicon film layer is deposited; and an amorphous silicon film layer is first deposited on the polished surface, and then a microcrystalline silicon film layer is deposited.

4. The method for preparing a HJT solar cell according to claim 3, Features: In S3, the prepared microcrystalline silicon thin film is used as a battery substrate, and a TCO high work function thin film and a low work function thin film are prepared on the battery substrate.

5. The method for preparing a HJT solar cell according to claim 4, Features: In S1, a tubular diffusion furnace is used to grow an oxide film; the oxide film serves as a mask protection layer to protect the underlying silicon wafer from being corroded by a cleaning and texturing solution.