Method for mass transfer of electronic components with adjustable spacing
Through pyrolysis or photolysis technology, the arrangement spacing of electronic components is adjusted row by row by row, which solves the problem of fixed spacing of electronic components in the prior art, and improves its application flexibility and density matching capabilities on display panels.
Patent Information
- Application Number
- CN202410547488.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-29
- Filing Date
- 2024-05-06
- Publication Date
- 2024-11-29
AI Technical Summary
The existing huge transfer of electronic components cannot adjust the spacing between electronic components, limiting their application scope.
By using a substrate and a light source with pyrolysis or photolysis characteristics, the electronic components are stripped and bonded row by row, and their arrangement spacing on the target substrate is adjusted to form an electronic components matrix with different row spacing and column spacing.
It realizes flexible adjustment of the spacing of electronic components, improving the application flexibility and density matching capabilities of electronic components on display panels.
Smart Images

Figure CN119050208A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for mass transferring electronic components, and in particular to a method for mass transferring electronic components with adjustable spacing. Background Art
[0002] Light-emitting diodes have the advantages of active light emission, high brightness, and energy saving. Therefore, they have been widely used in technical fields such as lighting, display, and projector, and micro-LED display has gradually become a new generation of display technology. However, a high-density (FHD) display has 1920 rows x 1080 columns, about 2 million pixels, and each pixel is further divided into three sub-pixels (Sub pixel) of red, green, and blue. Therefore, a high-density light-emitting diode display (FHD LED Display) has a total of about 6 million LED dies. To cut and paste these 6 million dies on the substrate of the display panel, the key technology lies in how to accurately transfer a certain amount of micro-LEDs to the substrate of the display panel and fix them together.
[0003] Figures 1A to 1D The top view of FIG. 1 shows a conventional method for mass transferring electronic components, the steps of which include: providing a Figure 1A The temporary substrate 10 shown in the figure has a first upper surface 10A and a first lower surface 10B opposite to each other, and a plurality of electronic components 12 are formed on the first upper surface 10A, and the plurality of electronic components 12 are arranged at intervals to form an electronic component matrix (not shown), and the row spacing and column spacing of the electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0, wherein the temporary substrate 10 is a pyrolytic adhesive film or a photolytic adhesive film; providing a Figure 1B The target substrate 20 shown in the figure has a second upper surface 20A and a second lower surface 20B opposite to each other, and then the temporary substrate 10 is placed above the target substrate 20 so that the first upper surface 10A of the temporary substrate 10 faces the second upper surface 20A of the target substrate 20; then, a light with a first wavelength (not shown) is provided above the temporary substrate 10, and the light with the first wavelength is irradiated along the temporary substrate 20 to make it pyrolyzed or photolyzed to lose viscosity, and the plurality of electronic components 12 are made as Figure 1C As shown in FIG. 1 , all of the electronic components 12 are peeled off and bonded to the second upper surface 20A of the target substrate 20. Although the conventional method of mass transferring electronic components can be used to quickly transfer a plurality of electronic components 12 from the first upper surface 10A of the temporary substrate to the second upper surface 20A of the target substrate 20, Figure 1DAs shown, the electronic component matrix (not shown) formed by the plurality of electronic components 12 located on the second upper surface 20A still has row and column spacings of X1 and Y1, and the spacing between the electronic components cannot be adjusted as needed, which greatly limits its application.
[0004] In view of this, a method for mass transferring electronic components with adjustable spacing is eagerly anticipated by the industry. Summary of the invention
[0005] The present invention discloses a method for mass transfer of electronic components with adjustable spacing, characterized in that it includes the following steps: providing a first substrate, the first substrate having a first upper surface and a first lower surface opposite to each other, wherein the first upper surface of the first substrate has a plurality of electronic components, and the plurality of electronic components are arranged along a first axis direction and a second axis direction respectively, forming a first electronic component matrix formed by arranging M rows of electronic components by N columns of electronic components, wherein the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 are respectively, and X1 and Y1>0; a second substrate is provided, and the second substrate is arranged below the first substrate, the second substrate has a second upper surface and a second lower surface relative to each other, and the first upper surface of the first substrate faces the second upper surface of the second substrate; and the plurality of electronic components located on the first substrate are fully or partially transferred to the second substrate, and a second electronic component matrix is formed on the second upper surface of the second substrate, and the row spacing and column spacing of the second electronic component matrix are respectively X2 and Y2, X2 and Y2>0, and X1≠X2, Y1≠Y2.
[0006] The aforementioned method for mass transfer of electronic components with adjustable spacing, wherein the step of forming the second electronic component matrix includes: providing a first light with a first wavelength above the first substrate, and irradiating the first light with the first wavelength to the first substrate where the electronic components in the Jth row and the Kth column of the first electronic component matrix are located to cause them to be thermally decomposed or photolyzed to lose viscosity, and selectively peeling off and bonding the electronic components in the Jth row and the Kth column to the second upper surface of the second substrate, and then displacing the first substrate relative to the second substrate along the first axis direction by a distance of (X2-X1) , so that the first light with a first wavelength irradiates the first substrate where the electronic components in the (J+1)th row and the Kth column of the first electronic component matrix are located, so that they are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the (J+1)th row and the Kth column are selectively peeled off and bonded to the second upper surface of the second substrate, wherein J, K, and X2 are all natural numbers, and 1≤J≤(M-1), 1≤K≤(N-1); and when all or part of the multiple electronic components in the Kth column of the first electronic component matrix are selectively peeled off and bonded to the second upper surface of the second substrate, firstly The first substrate is realigned to the second substrate, and the first substrate is displaced by a distance (Y2-Y1) relative to the second substrate along the second axis direction, and the first light having the first wavelength is irradiated on the first substrate where the electronic components in the Jth row and the (K+1)th column of the first electronic component matrix are located, so that the electronic components are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the Jth row and the (K+1)th column are selectively peeled off and bonded to the second upper surface of the second substrate, and the first substrate is displaced by a distance (X2-X1) relative to the second substrate along the first axis direction, and the electronic components in the Jth row and the (K+1)th column are selectively peeled off and bonded to the second upper surface of the second substrate, and the first substrate is displaced by a distance (X2-X1) relative to the second substrate along the first axis direction, and the electronic components in the Jth row and the (K+1)th column of the first electronic component matrix are selectively peeled off and bonded to the second upper surface of the second substrate, and the electronic components in the Jth row and the (K+1)th column ... The first light with a first wavelength irradiates the first substrate where the electronic components in the (J+1)th row and (K+1)th column of the first electronic component matrix are located, causing them to be thermally decomposed or photolyzed and lose their viscosity, and causes the electronic components in the (J+1)th row and (K+1)th column to be selectively peeled off and bonded to the second upper surface of the second substrate, where Y2 is a natural number; wherein, when all or part of the multiple electronic components located on the first substrate are selectively peeled off and bonded to the second upper surface of the second substrate, the second electronic component matrix can be formed on the second upper surface of the second substrate.
[0007] The aforementioned method for mass transfer of electronic components with adjustable spacing, wherein the step of forming the second electronic component matrix includes: providing a first light with a first wavelength above the first substrate, and irradiating the first light with the first wavelength to the first substrate where the electronic components in the Jth row and the Kth column of the first electronic component matrix are located to cause them to be thermally decomposed or photolyzed to lose viscosity, and selectively peeling off and bonding the electronic components in the Jth row and the Kth column to the second upper surface of the second substrate, and then displacing the first substrate relative to the second substrate along the second axis direction by a distance (Y2-Y1) , so that the first light with a first wavelength irradiates the first substrate where the electronic components in the Jth row and the (K+1)th column of the first electronic component matrix are located, so that they are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the Jth row and the (K+1)th column are selectively peeled off and bonded to the second upper surface of the second substrate, wherein J, K, and Y2 are all natural numbers, and 1≤J≤(M-1), 1≤K≤(N-1); and when all or part of the multiple electronic components in the Jth row of the first electronic component matrix are selectively peeled off and bonded to the second upper surface of the second substrate, firstly The first substrate is realigned to the second substrate, and the first substrate is displaced by a distance (X2-X1) relative to the second substrate along the first axis direction, and the first light having the first wavelength is irradiated on the first substrate where the electronic components in the (J+1)th row and the Kth column of the first electronic component matrix are located, so that the electronic components are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the (J+1)th row and the Kth column are selectively peeled off and bonded to the second upper surface of the second substrate, and the first substrate is displaced by a distance (Y2-Y1) relative to the second substrate along the second axis direction, and the first substrate is displaced by a distance (Y2-Y1) relative to the second substrate, and the first light having the first wavelength is irradiated on the first substrate where the electronic components in the (J+1)th row and the Kth column of the first electronic component matrix are located, so that the electronic components in the (J+1)th row and the Kth column are selectively peeled off and bonded to the second upper surface of the second substrate, and the first substrate is displaced by a distance (Y2-Y1) relative to the second substrate along the second axis direction, and the first substrate is displaced by a distance (Y2-Y1) relative to the second substrate, and the first light having the first wavelength is irradiated on the first substrate where the electronic components in the (J+1)th row and the Kth column of the first electronic component matrix are located, The first light with a first wavelength irradiates the first substrate where the electronic components in the (J+1)th row and (K+1)th column of the first electronic component matrix are located, causing them to be thermally decomposed or photolyzed and lose their viscosity, and causes the electronic components in the (J+1)th row and (K+1)th column to be selectively peeled off and bonded to the second upper surface of the second substrate, where X2 is a natural number; wherein, when all or part of the multiple electronic components located on the first substrate are selectively peeled off and bonded to the second upper surface of the second substrate, the second electronic component matrix can be formed on the second upper surface of the second substrate.
[0008] In the aforementioned method for mass transferring electronic components with adjustable spacing, the first substrate is a pyrolytic adhesive film, and the first light with a first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0009] In the aforementioned method for mass transferring electronic components with adjustable spacing, the first substrate is a photosensitive adhesive film, and the first light with a first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0010] In the aforementioned method for mass transferring electronic components with adjustable spacing, the plurality of electronic components are selected from one or more groups consisting of light emitting diodes, laser diodes and semiconductor components.
[0011] In the aforementioned method for mass transferring electronic components with adjustable spacing, the light emitted by the plurality of light emitting diodes is red light, green light, blue light, yellow light, white light, infrared light or ultraviolet light.
[0012] In the aforementioned method for mass transfer of electronic components with adjustable spacing, the wavelengths of the plurality of laser diodes are between 390 nanometers and 1700 nanometers.
[0013] The aforementioned method for mass transferring electronic components with adjustable spacing, wherein the plurality of semiconductor components are selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits and analog integrated circuits.
[0014] The present invention discloses another method for mass transfer of electronic components with adjustable spacing, characterized in that it includes the following steps: providing a first substrate, the first substrate having a first upper surface and a first lower surface opposite to each other, wherein the first upper surface of the first substrate has a plurality of electronic components, and the plurality of electronic components are arranged along a first axis direction and a second axis direction respectively, forming a first electronic component matrix formed by arranging M rows of electronic components by N columns of electronic components, wherein the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are The row and column distances of the second electronic component matrix are X1 and Y2 or X2 and Y1, respectively, and X1 and Y1>0; a second substrate is provided, and the second substrate is arranged below the first substrate, the second substrate has a second upper surface and a second lower surface opposite to each other, and the first upper surface of the first substrate faces the second upper surface of the second substrate; and the plurality of electronic components located on the first substrate are transferred in whole or in part to the second substrate, and a second electronic component matrix is formed on the second substrate, and the row and column distances of the second electronic component matrix are X1 and Y2 or X2 and Y1, respectively, wherein X2 and Y2>0, and X1≠X2, Y1≠Y2.
[0015] Another method for mass transfer of electronic components with adjustable spacing, wherein the row spacing and column spacing of the second electronic component matrix are X1 and Y2 respectively, and the steps for forming the second electronic component matrix include: providing a first light with a first wavelength above the first substrate, and irradiating the first light with the first wavelength on the first substrate where the multiple electronic components in the Kth column of the first electronic component matrix are located, so that the first substrate is thermally decomposed or photolyzed to lose viscosity, and the multiple electronic components in the Kth column are all peeled off and bonded to the second upper surface of the second substrate; and making the first substrate relative to the second substrate along the second axis The method further comprises: displacing the plurality of electronic components in the (K+1)th column of the first electronic component matrix by a distance of (Y2-Y1) in the direction, and then irradiating the first substrate where the plurality of electronic components in the (K+1)th column of the first electronic component matrix are located with the first light having the first wavelength, so that the plurality of electronic components in the (K+1)th column are thermally decomposed or photolyzed to lose their viscosity, and causing all or part of the plurality of electronic components in the (K+1)th column to be peeled off and bonded to the second upper surface of the second substrate, K is a natural number, and 1≤K≤(N-1); wherein, when all or part of the plurality of electronic components located on the first substrate are selectively peeled off and bonded to the second upper surface of the second substrate, the second electronic component matrix can be formed on the second substrate.
[0016] Another method for mass transferring electronic components with adjustable spacing as mentioned above further includes the following steps: providing a third substrate and disposing the third substrate below the second substrate, the third substrate having a third upper surface and a third lower surface relative to each other, and the second upper surface of the second substrate faces the third upper surface of the third substrate; and transferring all or part of the multiple electronic components located on the second substrate to the third substrate, and forming a third electronic component matrix on the third substrate, and the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively.
[0017] Another method for mass transfer of electronic components with adjustable spacing, wherein the step of forming the third electronic component matrix includes: providing a second light with a second wavelength above the second substrate, and irradiating the second light with the second wavelength on the second substrate where the multiple electronic components in the Jth row of the second electronic component matrix are located, so that the second substrate is thermally decomposed or photolyzed to lose its viscosity, and the multiple electronic components in the Jth row are completely or partially peeled off and bonded to the third upper surface of the third substrate; and displacing the second substrate relative to the third substrate along the first axis direction by (X2-X1) distance, and then irradiate the second substrate where the multiple electronic components in the (J+1)th row of the second electronic component matrix are located with the second light having a second wavelength, so that the second substrate is thermally decomposed or photolyzed to lose its viscosity, and the multiple electronic components in the (J+1)th row are completely or partially peeled off and bonded to the third upper surface of the third substrate, J is a natural number, and 1≤J≤(M-1); wherein, when the multiple electronic components located on the second substrate are completely or partially selectively peeled off and bonded to the third upper surface of the third substrate, the third electronic component matrix can be formed on the third substrate.
[0018] Another method for mass transfer of electronic components with adjustable spacing, wherein the row spacing and column spacing of the second electronic component matrix are X2 and Y1 respectively, and the steps for forming the second electronic component matrix include: providing a first light with a first wavelength above the first substrate, and irradiating the first light with the first wavelength on the first substrate where the multiple electronic components of the Jth row of the first electronic component matrix are located, so that the first light irradiates the first substrate with the first wavelength so that the multiple electronic components of the Jth row are thermally decomposed or photolyzed to lose viscosity, and the multiple electronic components of the Jth row are completely or partially peeled off and bonded to the second upper surface of the second substrate; and making the first substrate relative to the second substrate along the first The first substrate where the multiple electronic components in the (J+1)th row of the first electronic component matrix are located is irradiated with the first light having the first wavelength, so that the multiple electronic components in the (J+1)th row are thermally decomposed or photolyzed to lose their viscosity, and the multiple electronic components in the (J+1)th row are completely or partially peeled off and bonded to the second upper surface of the second substrate, J is a natural number, and 1≤J≤(M-1); wherein, when the multiple electronic components located on the first substrate are completely or partially selectively peeled off and bonded to the second upper surface of the second substrate, the second electronic component matrix can be formed on the second substrate.
[0019] Another method for mass transferring electronic components with adjustable spacing as mentioned above further includes the following steps: providing a third substrate and disposing the third substrate below the second substrate, the third substrate having a third upper surface and a third lower surface relative to each other, and the second upper surface of the second substrate faces the third upper surface of the third substrate; and transferring all or part of the multiple electronic components located on the second substrate to the third substrate, and forming a third electronic component matrix on the third substrate, and the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively.
[0020] Another method for mass transfer of electronic components with adjustable spacing, wherein the step of forming the third electronic component matrix includes: providing a second light with a second wavelength above the second substrate, and irradiating the second light with the second wavelength on the second substrate where the multiple electronic components in the Kth column of the second electronic component matrix are located, so that the second substrate is thermally decomposed or photolyzed to lose its viscosity, and the multiple electronic components in the Jth row are completely or partially peeled off and bonded to the third upper surface of the third substrate; and displacing the second substrate relative to the third substrate along the second axis direction (Y2-Y1) distance, and then irradiate the second substrate where the multiple electronic components in the (K+1)th column of the second electronic component matrix are located with the second light having a second wavelength, so that the second substrate is thermally decomposed or photolyzed to lose its viscosity, and the multiple electronic components in the (K+1)th column are completely or partially peeled off and bonded to the third upper surface of the third substrate, K is a natural number, and 1≤K≤(N-1); wherein, when the multiple electronic components located on the second substrate are completely or partially selectively peeled off and bonded to the third upper surface of the third substrate, the third electronic component matrix can be formed on the third substrate.
[0021] In the aforementioned method for mass transferring electronic components with adjustable spacing, the first substrate is a pyrolytic adhesive film, and the first light with a first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0022] In the aforementioned method for mass transferring electronic components with adjustable spacing, the first substrate is a photoresist film, and the first light with a first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0023] In the aforementioned method for mass transferring electronic components with adjustable spacing, the second substrate is a pyrolytic adhesive film, and the second light with a second wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0024] In the aforementioned method for mass transferring electronic components with adjustable spacing, the second substrate is a photosensitive adhesive film, and the second light with a second wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0025] In the aforementioned method for mass transferring electronic components with adjustable pitch, the plurality of electronic components are selected from one or more groups consisting of light emitting diodes, laser diodes and semiconductor components.
[0026] In the aforementioned method for mass transferring electronic components with adjustable spacing, the light emitted by the plurality of light emitting diodes is red light, green light, blue light, yellow light, white light, infrared light or ultraviolet light.
[0027] In the aforementioned method for mass transferring electronic components with adjustable spacing, the wavelengths of the plurality of laser diodes are between 390 nanometers and 1700 nanometers.
[0028] In the aforementioned method for mass transferring electronic components with adjustable pitch, the plurality of semiconductor components are selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
[0029] The present invention discloses another method for mass transfer of electronic components with adjustable spacing, characterized in that it includes the following steps: providing a first substrate, the first substrate having a first upper surface and a first lower surface relative to each other, wherein the first upper surface of the first substrate has a plurality of electronic components, and the plurality of electronic components are arranged along a first axis direction and a second axis direction respectively to form a first electronic component matrix formed by arranging M rows of electronic components by N columns of electronic components, wherein the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing of the first electronic component matrix is , column spacings are X1 and Y1 respectively, and X1 and Y1>0; providing a second substrate, and disposing the second substrate below the first substrate, the second substrate having a second upper surface and a second lower surface opposite to each other, and the first upper surface of the first substrate faces the second upper surface of the second substrate; and transferring the plurality of electronic components located on the first substrate to the second substrate, and forming a second electronic component matrix on the second upper surface of the second substrate, which is formed by arranging P rows of electronic components by Q columns of electronic components, wherein P and Q are natural numbers greater than 1, and P≠M and / or Q≠N.
[0030] In the aforementioned method for mass transferring electronic components with adjustable spacing, the column spacing of the second electronic component matrix is Y2, Y2>0 and Y1≠Y2.
[0031] Another aforementioned method for mass transfer of electronic components with adjustable spacing, wherein the step of forming the second electronic component matrix includes: using the multiple electronic components located in the R1th column of the first substrate as a first baseline of the first substrate along the first axis direction, using the multiple electronic components located in the R2th column of the second substrate as a second baseline of the second substrate along the first axis direction, and aligning the first baseline with the second baseline; and providing a first light with a first wavelength above the first substrate, so that the first light with the first wavelength irradiates the first substrate where the or multiple electronic components located in the N1th column of the first electronic component matrix are located, so that they are The electronic components are selectively peeled off from the N1th column of the first substrate by thermal decomposition or photolysis, and bonded to the second upper surface of the second substrate so that they are located in the N2th column of the second electronic component matrix, wherein R1, R2, N1, and N2 are natural numbers, N1≤N, N2≤Q, and 1≤R1≤N1, 1≤R2≤N2; wherein, when the electronic components are located in the N1th column of the first electronic component matrix of the first substrate and are transferred to the N2th column of the second electronic component matrix of the second substrate, their relative movement distance along the second axis direction is [(N2-R2)*Y2-(N1-R1)*Y1].
[0032] Another method for transferring a large amount of electronic components with adjustable spacing as mentioned above further includes the following steps: providing a third substrate and disposing the third substrate below the second substrate, the third substrate having a third upper surface and a third lower surface relative to each other, and the second upper surface of the second substrate faces the third upper surface of the third substrate; and transferring the second electronic component matrix located on the second substrate to the third substrate, and forming a third electronic component matrix on the third substrate formed by arranging U rows of electronic components by V columns of electronic components, and the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively, wherein U and V are natural numbers greater than 1.
[0033] Another aforementioned method for mass transfer of electronic components with adjustable spacing, wherein the step of forming the third electronic component matrix includes: using the multiple electronic components located in the S1th row of the second substrate as a third baseline of the second substrate along the second axis direction, using the multiple electronic components located in the S2th row of the third substrate as a fourth baseline of the third substrate along the second axis direction, and aligning the third baseline with the fourth baseline; and providing a second light with a second wavelength above the second substrate, so that the second light with the second wavelength irradiates the second substrate where the or multiple electronic components located in the M1th row of the second electronic component matrix are located, so that they are The electronic components located in the M1th row of the second substrate are selectively peeled off by thermal or photolysis to lose viscosity and bonded to the third upper surface of the third substrate so that they are located in the M2th column of the third electronic component matrix, wherein S1, S2, M1, and M2 are natural numbers, M1≤M, M2≤U, and 1≤S1≤M1, 1≤S2≤M2; wherein, when the electronic components located in the M1th row of the second electronic component matrix of the second substrate are transferred to the M2th row of the third electronic component matrix of the third substrate, their relative movement distance along the first axis direction is [(M2-S2)*X2-(M1-S1)*X1].
[0034] In the aforementioned method for mass transferring electronic components with adjustable spacing, the row spacing of the second electronic component matrix is X2, X2>0 and X1≠X2.
[0035] Another aforementioned method for mass transfer of electronic components with adjustable spacing, wherein the step of forming the second electronic component matrix includes: using the multiple electronic components located in the S1th row of the first substrate as a first baseline of the first substrate along the second axis direction, using the multiple electronic components located in the S2th row of the second substrate as a second baseline of the second substrate along the second axis direction, and aligning the first baseline with the second baseline; and providing a first light with a first wavelength above the first substrate, so that the first light with the first wavelength irradiates the first substrate where the or multiple electronic components located in the M1th row of the first electronic component matrix are located, so that they are The electronic components located in the M1th row of the first substrate are selectively peeled off by thermal or photolysis to lose viscosity and bonded to the second upper surface of the second substrate so that they are located in the M2th column of the second electronic component matrix, wherein S1, S2, M1, and M2 are natural numbers, M1≤M, M2≤P, and 1≤S1≤M1, 1≤S2≤M2; wherein, when the electronic components located in the M1th row of the first electronic component matrix of the first substrate are transferred to the M2th row of the second electronic component matrix of the second substrate, their relative movement distance along the first axis direction is [(M2-S2)*X2-(M1-S1)*X1].
[0036] Another method for transferring a large amount of electronic components with adjustable spacing as mentioned above further includes the following steps: providing a third substrate and disposing the third substrate below the second substrate, the third substrate having a third upper surface and a third lower surface relative to each other, and the second upper surface of the second substrate faces the third upper surface of the third substrate; and transferring the second electronic component matrix located on the second substrate to the third substrate, and forming a third electronic component matrix on the third substrate formed by arranging U rows of electronic components by V columns of electronic components, and the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively, wherein U and V are natural numbers greater than 1.
[0037] Another aforementioned method for mass transfer of electronic components with adjustable spacing, wherein the step of forming the third electronic component matrix includes: using the multiple electronic components located in the R1th column of the second substrate as a third baseline of the second substrate along the first axis direction, using the multiple electronic components located in the R2th column of the third substrate as a fourth baseline of the third substrate along the first axis direction, and aligning the third baseline with the fourth baseline; and providing a second light with a second wavelength above the second substrate, so that the second light with the second wavelength irradiates the second substrate where the or multiple electronic components located in the N1th column of the second electronic component matrix are located, so that they are The electronic components are selectively peeled off by thermal or photolysis and bonded to the third upper surface of the third substrate so that they are located in the N2th column of the third electronic component matrix, wherein R1, R2, N1, and N2 are natural numbers, N1≤N, N2≤V, and 1≤R1≤N1, 1≤R2≤N2; wherein, when the electronic components are located in the N1th column of the second electronic component matrix of the second substrate and are transferred to the N2th column of the third electronic component matrix of the third substrate, their relative movement distance along the second axis direction is [(N2-R2)*Y2-(N1-R1)*Y1].
[0038] In the aforementioned method for mass transferring electronic components with adjustable spacing, the first substrate is a pyrolytic adhesive film, and the first light with the first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0039] In the aforementioned method for mass transferring electronic components with adjustable spacing, the first substrate is a photosensitive adhesive film, and the first light with a first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0040] In the aforementioned method for mass transferring electronic components with adjustable spacing, the second substrate is a pyrolytic adhesive film, and the second light with a second wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0041] In the aforementioned method for mass transferring electronic components with adjustable spacing, the second substrate is a photosensitive adhesive film, and the second light with a second wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
[0042] In the aforementioned method for mass transferring electronic components with adjustable pitch, the plurality of electronic components are selected from one or more groups consisting of light emitting diodes, laser diodes and semiconductor components.
[0043] In the aforementioned method for mass transferring electronic components with adjustable spacing, the light emitted by the plurality of light emitting diodes is red light, green light, blue light, yellow light, white light, infrared light or ultraviolet light.
[0044] In the aforementioned method for mass transferring electronic components with adjustable spacing, the wavelengths of the plurality of laser diodes are between 390 nanometers and 1700 nanometers.
[0045] In the aforementioned method for mass transferring electronic components with adjustable pitch, the plurality of semiconductor components are selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figures 1A to 1D The top view shows a conventional method for mass transferring electronic components.
[0047] Figures 2A to 2H The top view is a method for mass transferring electronic components with adjustable spacing according to an embodiment of the present invention.
[0048] Figures 3A to 3E The top view is a method for mass transferring electronic components with adjustable spacing according to the second embodiment of the present invention.
[0049] Figures 4A to 4I The top view is a method for mass transferring electronic components with adjustable spacing according to the third embodiment of the present invention.
[0050] Figures 5A to 5H The top view is a method for mass transferring electronic components with adjustable spacing according to the fourth embodiment of the present invention.
[0051] Figures 6A to 6E The top view is a method for mass transferring electronic components with adjustable spacing according to the fifth embodiment of the present invention.
[0052] Figures 7A to 7E The top view is a method for mass transferring electronic components with adjustable spacing according to the sixth embodiment of the present invention.
[0053] Among them, the simple description of the symbols in the accompanying drawings is as follows:
[0054] 10 Temporary substrate
[0055] 10A First upper surface
[0056] 10B First lower surface
[0057] 12 Electronic components
[0058] 20 Target substrate
[0059] 20A Second upper surface
[0060] 20B Second lower surface
[0061] 100 First substrate
[0062] 100A First upper surface
[0063] 100B First lower surface
[0064] 110, 110' First Baseline
[0065] 1211~121J, 121M, 1221~122J, 122M, 12K1~12KJ, 12KM, 12N1~12NJ, 12NM, 12(N1)1~12(N1)J, 12(N1)M, 121(M1)~12N(M1), 121(M1)~12K(M1), 12N(M1) electronic components
[0068] 2211~221(j), 221(M2)~22k(M2), 22Q(M2), 221P~22kP, 2221~222(j), 222P,
[0069] 22(N2)1~22(N2)j、22(N2)P、22Q1~22Q(J)、22QP electronic components
[0070] 3211~321(M2), 321U~32(N2)U, 3221~322(M2), 322U, 32k1~32k(M2), 32kU, 32V1~32V(M2), 3211~321J, 321U, 33221~322j, 322U, 2(N2)1~32(N2)j, 32(N2)U, 32Vj, 32VU Electronic components
[0073] 200 Second substrate
[0074] 200A Second upper surface
[0075] 200B Second lower surface
[0076] 210, 210' Second baseline
[0077] 300 Third substrate
[0078] 300A Third upper surface
[0079] 300B Third lower surface
[0080] 210, 210' Second baseline
[0081] 250, 250' Third Baseline
[0082] 350, 350' Fourth Baseline DETAILED DESCRIPTION
[0083] In order to make the description of the disclosed content of the present invention more detailed and complete, the following is an illustrative description of the implementation and specific embodiments of the present invention; however, this is not the only form of implementing or using the specific embodiments of the present invention. The various embodiments disclosed below can be combined or replaced with each other under beneficial circumstances, and other embodiments can be added to one embodiment without further recording or explanation.
[0084] In the following description, many specific details will be described in detail to enable the reader to fully understand the following embodiments. However, embodiments of the present invention can be practiced without these specific details. In other cases, well-known structures and devices are only schematically depicted in the figures to simplify the drawings.
[0085] Example
[0086] Embodiment 1
[0087] The following will refer to Figures 2A to 2H The top view illustrates in detail a method for mass transferring electronic components with adjustable spacing disclosed in the first embodiment.
[0088] First, see Figure 2A .like Figure 2A As shown, a first substrate 100 is provided, the first substrate 100 has a first upper surface 100A and a first lower surface 100B opposite to each other, wherein the first upper surface 100A of the first substrate 100 has a plurality of electronic components 1211-12NM, and the plurality of electronic components 1211-12NM are arranged along the first axis direction and the second axis direction respectively, forming a first electronic component matrix (not shown) formed by M rows of electronic components multiplied by N columns of electronic components, wherein the first substrate 100 is a pyrolytic adhesive film or a photolytic adhesive film, the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0. In the first embodiment, the first axis direction is the X axis direction and the second axis direction is the Y axis direction as an example, but in other embodiments according to the present invention, the first axis direction can also be selected as the Y axis direction and the second axis direction as the X axis direction as needed.
[0089] The aforementioned multiple electronic components 1211-12NM of the first embodiment are, for example, but not limited to, selected from one or more groups consisting of light emitting diodes, laser diodes, and semiconductor components. Among them, the aforementioned multiple light emitting diodes are, for example, but not limited to, emitting red light, green light, blue light, yellow light, white light, infrared light, or ultraviolet light; the wavelengths of the aforementioned multiple laser diodes are, for example, but not limited to, between 390 nanometers and 1700 nanometers; the aforementioned multiple semiconductor components are, for example, but not limited to, selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
[0090] Secondly, please refer to Figure 2B A second substrate 200 is provided and disposed below the first substrate 100 . The second substrate 200 has a second upper surface 200A and a second lower surface 200B opposite to each other, and the first upper surface 100A of the first substrate 100 faces the second upper surface 200A of the second substrate 200 .
[0091] Secondly, please refer to Figures 2B to 2D A first light with a first wavelength is provided above the first substrate 100. The first light with the first wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12000 nanometers. The first light with the first wavelength is irradiated on the first substrate 100 where the electronic components 12KJ in the Jth row and the Kth column of the first electronic component matrix are located, so that the electronic components 12KJ in the Jth row and the Kth column are thermally decomposed or photolyzed to lose viscosity. The electronic components 12KJ in the Jth row and the Kth column are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200. Then, the first substrate 100 is moved relative to the first substrate 100. The second substrate 200 is displaced a distance of (X2-X1) along the first axis direction, so that the first light with the first wavelength irradiates the first substrate 100 where the electronic component 12(K+1)J in the (J+1)th row and Kth column of the first electronic component matrix is located, so that it is thermally decomposed or photolyzed to lose its viscosity, and the electronic component in the (J+1)th row and Kth column is selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, wherein J, K, and X2 are all natural numbers, X1≠X2, and 1≤J≤(M-1), 1≤K≤(N-1). In the first embodiment, all of the electronic components 12K1 to 12KM in the Kth column are selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as an example for explanation. However, according to other embodiments of the present invention, part of the electronic components 12K1 to 12KM in the Kth column may be selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as needed.
[0092] like Figure 2BAs shown, when J=1 and K=1, the first light with the first wavelength is irradiated along the first axis direction (X-axis direction) to the first substrate 100 where the electronic components 1211 in the 1st row and 1st column of the first electronic component matrix are located, so that they are thermally decomposed or photolyzed to lose their viscosity, and the electronic components 1211 in the 1st row and 1st column are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200.
[0093] Then, if Figure 2C-2D As shown, the first substrate 100 is displaced relative to the second substrate 200 by a distance (X2-X1) along the first axis direction (X axis direction), and the first light with the first wavelength is irradiated along the first axis direction (X axis direction) on the first substrate 100 where the electronic components in the second row and the first column of the first electronic component matrix are located, so that they are thermally decomposed or photolyzed to lose viscosity, and the electronic components 1212 in the second row and the first column are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200. Similarly, the other electronic components 1213 to 121M in the first column can also be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 using the same method as described above.
[0094] Then, please refer to Figures 2E to 2GAfter the plurality of electronic components 12K1-12KM in the Kth column of the first electronic component matrix are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, the first substrate 100 is first realigned with the second substrate 200, and then the first substrate 100 is displaced by a distance (Y2-Y1) relative to the second substrate 200 along the second axis direction (Y axis direction), Y2>0, and Y1≠Y2, and then the first light with the first wavelength is irradiated on the first substrate 100 where the electronic component 12(K+1)J in the Jth row and the (K+1)th column of the first electronic component matrix is located. The first light with the first wavelength is, for example but not limited to, light with a wavelength between 100 nanometers and 12000 nanometers, so that the electronic component 12(K+1)K in the Jth row and the (K+1)th column is thermally decomposed or photolyzed to lose its viscosity, and the electronic component 12(K+1)K in the Jth row and the (K+1)th column is selectively peeled off and bonded to the second upper surface 200A of the second substrate 200. Then, the first substrate 100 is displaced relative to the second substrate 200 by a distance (X2-X1) along the first axis direction (X axis direction), and the first light having the first wavelength is irradiated on the first substrate 100 where the electronic component 12(K+1)(J+1) in the (J+1)th row and (K+1)th column of the first electronic component matrix is located, so that the electronic component 12(K+1)(J+1) in the (J+1)th row and (K+1)th column is pyrolyzed or photolyzed to lose its viscosity, and the electronic component 12(K+1)(J+1) in the (J+1)th row and (K+1)th column is selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, wherein Y2 is a natural number. After the plurality of electronic components 1211-12NM located on the first substrate 100 are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, a second electronic component matrix (not shown) can be formed on the second upper surface 200A of the second substrate 200. In the first embodiment of the present invention, all of the electronic components 1211-121M located in the first electronic component matrix (not marked) of the first substrate 100 are selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200. However, according to other embodiments of the present invention, part of the electronic components 1211-121M located in the first electronic component matrix (not marked) of the first substrate 100 may be selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as needed.
[0095] like Figure 2EAs shown, when K = 1, after the electronic components 1213 to 121M in the first column are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, the first substrate 100 is first realigned with the second substrate 200. Next, the first substrate 100 is displaced by a distance (Y2 - Y1) in the second axis direction (Y-axis direction) relative to the second substrate 200, and then the first light having the first wavelength is irradiated onto the first substrate 100 where the electronic component 1221 in the second column and the first row of the first electronic component matrix is located, so that it is pyrolyzed or photolyzed to lose its adhesiveness, and the electronic component 1221 in the second column and the first row is selectively peeled off and bonded to the second upper surface 200A of the second substrate 200. Then, as Figure 2F shown, the first substrate 100 is displaced by a distance (X2 - X1) in the first axis direction (X-axis direction) relative to the second substrate 200, and the first light having the first wavelength is irradiated onto the first substrate 100 where the electronic component 1222 in the second column and the second row of the first electronic component matrix is located, so that it is pyrolyzed or photolyzed to lose its adhesiveness, and the electronic component 1222 in the second column and the second row is selectively peeled off and bonded to the second upper surface 200A of the second substrate 200. Similarly, as Figure 2G shown, the other electronic components 1223 to 122M in the 3rd to Mth rows can also be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 by the same method as described above.
[0096] As Figure 2H shown, after the multiple electronic components 1211 to 12NM on the first substrate 100 are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 by the above method, a second electronic component matrix (not labeled) can be formed on the second upper surface 200A of the second substrate 200, and the row pitch and column pitch of the second electronic component matrix are X2 and Y2 respectively. Among them, when X2 > X1, that is, the row pitch X2 of the second electronic component matrix is greater than the row pitch X1 of the first electronic component matrix; when X2 < X1, that is, the row pitch X2 of the second electronic component matrix is less than the row pitch X1 of the first electronic component matrix. In addition, when Y2 > Y1, that is, the column pitch Y2 of the second electronic component matrix is greater than the column pitch Y1 of the first electronic component matrix; when Y2 < Y1, that is, the column pitch Y2 of the second electronic component matrix is less than the column pitch Y1 of the first electronic component matrix.
[0097] Embodiment 2
[0098] Hereinafter, another method for transferring a large number of electronic components with adjustable pitch disclosed in this Embodiment 2 will be described in detail with reference to Figures 3A to 3E the top view.
[0099] First, see Figure 3A .like Figure 3A As shown, a first substrate 100 is provided, the first substrate having a first upper surface 100A and a first lower surface 100B opposite to each other, wherein the first upper surface 100A of the first substrate 100 has a plurality of electronic components 1211-12NM, and the plurality of electronic components 1211-12NM are arranged along the first axis direction and the second axis direction respectively, forming a first electronic component matrix (not shown) formed by M rows of electronic components multiplied by N columns of electronic components, wherein the first substrate 100 is a pyrolytic adhesive film or a photolytic adhesive film, the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0. In the first embodiment, the first axis direction is the X axis direction and the second axis direction is the Y axis direction as an example, but in other embodiments according to the present invention, the first axis direction can also be selected as the Y axis direction and the second axis direction as the X axis direction as needed.
[0100] The aforementioned multiple electronic components 1211-12NM of the second embodiment are, for example, but not limited to, selected from one or more groups consisting of light emitting diodes, laser diodes, and semiconductor components. Among them, the aforementioned multiple light emitting diodes are, for example, but not limited to, emitting red light, green light, blue light, yellow light, white light, infrared light, or ultraviolet light; the wavelengths of the aforementioned multiple laser diodes are, for example, but not limited to, between 390 nanometers and 1700 nanometers; the aforementioned multiple semiconductor components are, for example, but not limited to, selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
[0101] Secondly, please refer to Figure 3B A second substrate 200 is provided and disposed below the first substrate 100 . The second substrate 200 has a second upper surface 200A and a second lower surface 200B opposite to each other, and the first upper surface 100A of the first substrate 100 faces the second upper surface 200A of the second substrate 200 .
[0102] Secondly, please refer to Figures 3B to 3EA first light with a first wavelength is provided above the first substrate 100, and the first light with the first wavelength is used to irradiate the first substrate 100 where the electronic component 12KJ in the Jth row and the Kth column of the first electronic component matrix is located. The first light with the first wavelength is, for example but not limited to, light with a wavelength between 100 nanometers and 12000 nanometers, so that the electronic component 12KJ in the Jth row and the Kth column is thermally decomposed or photolyzed to lose its viscosity, and the electronic component 12KJ in the Jth row and the Kth column is selectively peeled off and bonded to the second upper surface 200A of the second substrate 200. Then, as Figure 3C As shown, the first substrate 100 is first displaced relative to the second substrate 200 along the second axis direction (Y axis direction) by a distance of (Y2-Y1), Y2>0 and Y1≠Y2, and then the first light with the first wavelength is irradiated on the first substrate 100 where the electronic component 12(K+1)J in the Jth row and the (K+1)th column of the first electronic component matrix is located, so that it is thermally decomposed or photolyzed to lose its viscosity, and the electronic component 12(K+1)J in the Jth row and the (K+1)th column is selectively peeled off and bonded to the second upper surface of the second substrate 200, wherein J, K, and Y2 are all natural numbers, and 1≤J≤(M-1), 1≤K≤(N-1). In the second embodiment, all the electronic components 121J~12NJ in the Jth row are selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as an example for explanation. However, according to other embodiments of the present invention, part of the electronic components 121J~12NJ in the Jth row can also be selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as needed.
[0103] like Figure 3B As shown, when J=1 and K=1, a first light with a first wavelength is provided above the first substrate 100, and the first light with the first wavelength is irradiated on the first substrate 100 where the electronic components 1211 in the first column and the first row of the first electronic component matrix are located. The first light with the first wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12000 nanometers, so that the electronic components 1211 in the first column and the first row are thermally decomposed or photolyzed to lose their viscosity, and the electronic components 1211 in the first column and the first row are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200. Then, as Figure 3CAs shown, the first substrate 100 is first displaced relative to the second substrate 200 along the second axis direction (Y axis direction) by a distance (Y2-Y1), and then the first light with the first wavelength is irradiated on the first substrate 100 where the electronic components 1221 in the second column and the first row of the first electronic component matrix are located, so that they are thermally decomposed or photolyzed to lose their viscosity, and the electronic components 1221 in the second column and the first row are selectively peeled off and bonded to the second upper surface of the second substrate 200. Similarly, the other electronic components 1231-12N1 in the first row can also be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 using the same method as described above.
[0104] Then, please refer to Figures 3D to 3E After the aforementioned plurality of electronic components 121J-12NJ in the Jth row of the aforementioned first electronic component matrix are selectively peeled off and bonded to the second upper surface 200A of the aforementioned second substrate 200, the aforementioned first substrate 100 is first realigned with the aforementioned second substrate 200, and then the aforementioned first substrate 100 is displaced by a distance (X2-X1) along the aforementioned first axis direction (X axis direction) relative to the aforementioned second substrate 200, X2>0 and X1≠X2, and then the aforementioned first light with the first wavelength is irradiated on the first substrate 100 where the electronic component 12K(J+1) in the (J+1)th row and the Kth column of the aforementioned first electronic component matrix is located, so that it is pyrolyzed or photolyzed to lose its viscosity, and the electronic component 12K(J+1) in the (J+1)th row and the Kth column is selectively peeled off and bonded to the second upper surface 200A of the aforementioned second substrate 200. Then, the first substrate is displaced by a distance (Y2-Y1) relative to the second substrate along the second axis direction, and the first light with the first wavelength is irradiated on the first substrate 100 where the electronic component 12(K+1)(J+1) in the (J+1)th row and (K+1)th column of the first electronic component matrix is located, so that it is thermally decomposed or photolyzed to lose its viscosity, and the electronic component 12(K+1)(J+1) in the (J+1)th row and (K+1)th column is selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, wherein X2 is a natural number; wherein, when all or part of the plurality of electronic components located on the first substrate are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, the second electronic component matrix (not shown) can be formed on the second upper surface 200A of the second substrate 200.
[0105] like Figure 3DAs shown, when J = 1 and K = 1, and after the multiple electronic components 1211 - 12N1 in the first row of the first electronic component matrix are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, first realign the first substrate 100 with respect to the second substrate 200, then displace the first substrate 100 relative to the second substrate 200 by a distance (X2 - X1) along the first axis direction (X-axis direction). Then, irradiate the first substrate 100 where the electronic component 1212 in the second row and the first column of the first electronic component matrix is located with the first light having the first wavelength to pyrolyze or photolyze it and make it lose its adhesiveness, and selectively peel off and bond the electronic component 1212 in the second row and the first column to the second upper surface 200A of the second substrate 200. Then, as Figure 3E shown, first displace the first substrate 100 relative to the second substrate 200 by a distance (Y2 - Y1) along the second axis direction (Y-axis direction), then irradiate the first substrate 100 where the electronic component 1222 in the second row and the second column of the first electronic component matrix is located with the first light having the first wavelength to pyrolyze or photolyze it and make it lose its adhesiveness, and selectively peel off and bond the electronic component 1222 in the second row and the second column to the second upper surface 200A of the second substrate 200. Similarly, the other electronic components 1232 - 12N2 in the second row can also be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 by using the same method as described above.
[0106] As Figure 3E shown, when the multiple electronic components 1211 - 12NM on the first substrate 100 are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 by using the above method, a second electronic component matrix (not labeled) can be formed on the second upper surface 200A of the second substrate 200, and the row pitch and column pitch of the second electronic component matrix are X2 and Y2 respectively. Among them, when X2 > X1, that is, the row pitch X2 of the second electronic component matrix is greater than the row pitch X1 of the first electronic component matrix; when X2 < X1, that is, the row pitch X2 of the second electronic component matrix is less than the row pitch X1 of the first electronic component matrix. Among them, when Y2 > Y1, that is, the column pitch Y2 of the second electronic component matrix is greater than the column pitch Y1 of the first electronic component matrix; when Y2 < Y1, that is, the column pitch Y2 of the second electronic component matrix is less than the column pitch Y1 of the first electronic component matrix.
[0107] Embodiment 3
[0108] The following will refer to Figures 4A to 4I the top view to detail a method for massively transferring electronic components with adjustable pitch disclosed in this Embodiment 3.
[0109] First, see Figure 4A .like Figure 4A As shown, a first substrate 100 is provided, the first substrate 100 has a first upper surface 100A and a first lower surface 100B opposite to each other, wherein the first upper surface 100A of the first substrate 100 has a plurality of electronic components 1211-12NM, and the plurality of electronic components 1211-12NM are arranged along the first axis direction and the second axis direction respectively, forming a first electronic component matrix (not shown) formed by M rows of electronic components multiplied by N columns of electronic components, wherein the first substrate 100 is a pyrolytic adhesive film or a photolytic adhesive film, the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0. In the first embodiment, the first axis direction is the X axis direction and the second axis direction is the Y axis direction as an example, but in other embodiments according to the present invention, the first axis direction can also be selected as the Y axis direction and the second axis direction as the X axis direction as needed.
[0110] The aforementioned multiple electronic components 1211-12NM of the third embodiment are, for example, but not limited to, selected from one or more groups consisting of light emitting diodes, laser diodes, and semiconductor components. Among them, the aforementioned multiple light emitting diodes are, for example, but not limited to, emitting red light, green light, blue light, yellow light, white light, infrared light, or ultraviolet light; the wavelengths of the aforementioned multiple laser diodes are, for example, but not limited to, between 390 nanometers and 1700 nanometers; the aforementioned multiple semiconductor components are, for example, but not limited to, selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
[0111] Secondly, please refer to Figure 4B A second substrate 200 is provided and disposed below the first substrate 100. The second substrate 200 has a second upper surface 200A and a second lower surface 200B opposite to each other, and the first upper surface 100A of the first substrate 100 faces the second upper surface 200A of the second substrate 200. The second substrate 200 is a thermal adhesive film or a photo-adhesive film.
[0112] Secondly, please refer to Figures 4B to 4DA first light with a first wavelength is provided above the first substrate 100. The first light with the first wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12,000 nanometers. The first light with the first wavelength is irradiated on the first substrate 100 where the plurality of electronic components 12K1 to 12KM in the Kth column of the first electronic component matrix are located, so that the plurality of electronic components 12K1 to 12KM in the Kth column are thermally decomposed or photolyzed to lose viscosity, and all of the plurality of electronic components in the Kth column are peeled off and bonded to the second upper surface 200A of the second substrate 200. The third embodiment is described by taking the selective peeling off and bonding of all of the electronic components 12K1 to 12KM in the Kth column to the second upper surface 200A of the second substrate 200 as an example. However, according to other embodiments of the present invention, part of the electronic components 12K1 to 12KM in the Kth column may be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as needed. Then, the first substrate 100 is displaced relative to the second substrate 200 along the second axis direction (Y axis direction) by a distance of (Y2-Y1), Y2>0 and Y1≠Y2, and then the first light with the first wavelength is irradiated on the first substrate 100 where the plurality of electronic components 12(K+1)1~12(K+1)M in the (K+1)th column of the first electronic component matrix are located. The first light with the first wavelength is, for example but not limited to, light with a wavelength between 100 nanometers and 12000 nanometers, so that the plurality of electronic components 12(K+1)1~12(K+1)M in the (K+1)th column are thermally decomposed or photolyzed to lose viscosity, and all or part of the plurality of electronic components 12(K+1)1~12(K+1)M in the (K+1)th column are peeled off and bonded to the second upper surface 200A of the second substrate 200, K is a natural number, and 1≤K≤(N-1), Y2>0, and Y1≠Y2. In the third embodiment, all of the electronic components 12(K+1)1~12(K+1)M in the (K+1)th column are selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as an example for explanation. However, according to other embodiments of the present invention, part of the electronic components 12(K+1)1~12(K+1)M in the (K+1)th column can be selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as needed.
[0113] like Figure 4BAs shown, when K=1, a first light with a first wavelength is provided above the aforementioned first substrate 100. The aforementioned first light with a first wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12000 nanometers, and the aforementioned first light with a first wavelength is irradiated on the first substrate 100 where the aforementioned multiple electronic components 1211~121M in the first column of the aforementioned first electronic component matrix are located, so that they are thermally decomposed or photolyzed to lose viscosity, and the aforementioned multiple electronic components 1211~121M in the first column are all peeled off and bonded to the second upper surface 200A of the aforementioned second substrate 200. This third embodiment uses the example that all the electronic components 1211~121M in the first column are selectively peeled off and bonded to the second upper surface 200A of the aforementioned second substrate 200. However, according to other embodiments of the present invention, part of the electronic components 1211~121M in the first column can also be selectively peeled off and bonded to the second upper surface 200A of the aforementioned second substrate 200 as needed. Then, as Figure 4C As shown, the first substrate 100 is displaced a distance (Y2-Y1) along the second axis direction (Y axis direction) relative to the second substrate 200, and then the first light with the first wavelength is irradiated on the first substrate 100 where the plurality of electronic components 1221-122M in the second column of the first electronic component matrix are located. The first light with the first wavelength is, for example but not limited to, light with a wavelength between 100 nanometers and 12000 nanometers, so that the plurality of electronic components 1221-122M in the second column are thermally decomposed or photolyzed to lose viscosity, and all the plurality of electronic components 1221-122M in the second column are peeled off and bonded to the second upper surface 200A of the second substrate 200, Y2>0, and Y1≠Y2. In the third embodiment, all the electronic components 1221-122M in the second row are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as an example. However, according to other embodiments of the present invention, part of the electronic components 1221-122M in the second row can also be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as needed. Similarly, Figure 4D As shown, the other electronic components 1231 - 12NM in the 3rd to Nth columns can also be selectively peeled off in whole or in part and bonded to the second upper surface 200A of the second substrate 200 by the same method as described above.
[0114] like Figure 4EAs shown, after all of the plurality of electronic components 1211 to 12NM located on the foregoing first substrate 100 are selectively peeled off and bonded to the second upper surface 200A of the foregoing second substrate 200 by using the above method, a second electronic component matrix (not labeled) can be formed on the second upper surface 200A of the foregoing second substrate 200, and the row pitch and column pitch between the foregoing second electronic component matrices are X1 and Y2, respectively. Among them, when Y2 > Y1, that is, the column pitch of the second electronic component matrix is greater than the column pitch of the first electronic component matrix; when Y2 < Y1, that is, the column pitch of the second electronic component matrix is less than the column pitch of the first electronic component matrix.
[0115] As Figures 4F to 4I shown, in the third embodiment, all or part of the plurality of electronic components 1211 to 12NM located on the foregoing second substrate 200 can be further transferred to the foregoing third substrate 300, and a third electronic component matrix (not labeled) can be formed on the foregoing third substrate 300, and the row pitch and column pitch of the foregoing third electronic component matrix are X2 and Y2, respectively, and X1 ≠ X2, Y1 ≠ Y2.
[0116] As Figures 4F to 4IAs shown, a third substrate 300 is provided and disposed below the second substrate 200. The third substrate 300 has a third upper surface 300A and a third lower surface 300B opposite to each other, and the second upper surface 200A of the second substrate 200 faces the third upper surface 300A of the third substrate 300. Then, a second light with a second wavelength is provided above the second substrate 200, and the second light with the second wavelength is irradiated on the second substrate 200 where the plurality of electronic components in the Jth row of the second electronic component matrix are located. The second light with the second wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12000 nanometers, so that the second substrate 200 is thermally decomposed or photolyzed to lose its viscosity, and the plurality of electronic components 121J to 12NJ in the Jth row are all peeled off and bonded to the third upper surface 300A of the third substrate 300. Next, the second substrate 200 is displaced relative to the third substrate 300 along the first axis direction by a distance of (X2-X1), wherein X2>0 and X1≠X2, and then the second light having the second wavelength is irradiated on the second substrate 200 where the plurality of electronic components 121(J+1) to 12N(J+1) in the (J+1)th row of the second electronic component matrix are located, so that the second substrate 200 is thermally decomposed or photolyzed to lose its viscosity, and the plurality of electronic components 121(J+1) to 12N(J+1) in the (J+1)th row are completely or partially peeled off and bonded to the third upper surface 300A of the third substrate 300, where J is a natural number and 1≤J≤(M-1). When all of the aforementioned multiple electronic components 1211~12NM located on the aforementioned second substrate 200 are selectively peeled off and bonded to the third upper surface 300A of the aforementioned third substrate 300, a third electronic component matrix (not marked) can be formed on the aforementioned third substrate 300, and the row spacing and column spacing of the aforementioned third electronic component matrix (not marked) are X2 and Y2 respectively. In the third embodiment, the aforementioned multiple electronic components 121J~12NJ in the Jth row and the aforementioned multiple electronic components 121(J+1)~12N(J+1) in the (J+1)th row are all selectively stripped and bonded to the third upper surface 300A of the aforementioned third substrate 300 as an example for explanation. However, according to other embodiments of the present invention, the aforementioned multiple electronic components 121J~12NJ in the Jth row and the aforementioned multiple electronic components 121(J+1)~12N(J+1) in the (J+1)th row can also be partially selectively stripped and bonded to the third upper surface 300A of the aforementioned third substrate 300 as needed.
[0117] like Figure 4FAs shown, when J = 1, a second light of a second wavelength is provided above the second substrate, and the second light of the second wavelength is irradiated onto the second substrate 200 where the multiple electronic components in the first row of the second electronic component matrix are located. The second light of the second wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12,000 nanometers. The second substrate 200 is pyrolyzed or photolyzed to lose its adhesiveness, and all or part of the multiple electronic components 1211 - 12N1 in the first row are peeled off and bonded to the third upper surface 300A of the third substrate 300.
[0118] Next, as Figure 4G shown, the second substrate 200 is displaced by a distance (X2 - X1) in the first axis direction relative to the third substrate 300, and then the second light of the second wavelength is irradiated onto the second substrate 200 where the multiple electronic components 1212 - 12N2 in the second row of the second electronic component matrix are located. The second substrate 200 is pyrolyzed or photolyzed to lose its adhesiveness, and all or part of the multiple electronic components 1212 - 12N2 in the second row are peeled off and bonded to the third upper surface 300A of the third substrate 300.
[0119] Then, as Figure 4H shown, the second substrate 200 is displaced again by a distance (X2 - X1) in the first axis direction relative to the third substrate 300, and then the second light of the second wavelength is irradiated onto the second substrate 200 where the multiple electronic components 1213 - 12N3 in the third row of the second electronic component matrix are located. The second substrate 200 is pyrolyzed or photolyzed to lose its adhesiveness, and all or part of the multiple electronic components 1213 - 12N3 in the third row are peeled off and bonded to the third upper surface 300A of the third substrate 300. Similarly, the other electronic components 1214 - 12NM in the fourth row to the Mth row can also be selectively peeled off and bonded to the third upper surface 300A of the third substrate 300 using the same method described above.
[0120] As Fig. 4I shown, after all of the multiple electronic components 1211 - 12NM located on the second substrate 200 are selectively peeled off and bonded to the third upper surface 300A of the third substrate 300, a third electronic component matrix (not labeled) can be formed on the third substrate 300, and the row pitch and column pitch of the third electronic component matrix are X2 and Y2 respectively. Among them, when X2 > X1, that is, the row pitch of the third electronic component matrix is greater than the row pitch of the second electronic component matrix; when X2 < X1, that is, the row pitch of the third electronic component matrix is less than the row pitch of the second electronic component matrix.
[0121] In the third embodiment, all of the aforementioned multiple electronic components 1211-12NM in the second electronic component matrix of the second substrate 200 are selectively stripped and bonded to the third upper surface 300A of the aforementioned third substrate 300 as an example for explanation. However, according to other embodiments of the present invention, part of the aforementioned multiple electronic components 1211-12NM in the second electronic component matrix of the second substrate 200 can also be selectively stripped and bonded to the third upper surface 300A of the aforementioned third substrate 300 as needed.
[0122] Embodiment 4
[0123] The following will refer to Figures 5A to 5H The top view illustrates in detail a method for mass transferring electronic components with adjustable spacing disclosed in the fourth embodiment.
[0124] First, see Figure 5A .like Figure 5A As shown, a first substrate 100 is provided, the first substrate 100 has a first upper surface 100A and a first lower surface 100B opposite to each other, wherein the first upper surface 100A of the first substrate 100 has a plurality of electronic components 1211-12NM, and the plurality of electronic components 1211-12NM are arranged along the first axis direction and the second axis direction respectively, forming a first electronic component matrix (not shown) formed by M rows of electronic components multiplied by N columns of electronic components, wherein the first substrate 100 is a pyrolytic adhesive film or a photolytic adhesive film, the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0. In the first embodiment, the first axis direction is the X axis direction and the second axis direction is the Y axis direction as an example, but in other embodiments according to the present invention, the first axis direction can also be selected as the Y axis direction and the second axis direction as the X axis direction as needed.
[0125] The aforementioned multiple electronic components 1211-12NM of the fourth embodiment are, for example, but not limited to, selected from one or more groups consisting of light emitting diodes, laser diodes, and semiconductor components. Among them, the aforementioned multiple light emitting diodes are, for example, but not limited to, emitting red light, green light, blue light, yellow light, white light, infrared light, or ultraviolet light; the wavelengths of the aforementioned multiple laser diodes are, for example, but not limited to, between 390 nanometers and 1700 nanometers; the aforementioned multiple semiconductor components are, for example, but not limited to, selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
[0126] Secondly, please refer to Figure 5BA second substrate 200 is provided and disposed below the first substrate 100. The second substrate 200 has a second upper surface 200A and a second lower surface 200B opposite to each other, and the first upper surface 100A of the first substrate 100 faces the second upper surface 200A of the second substrate 200. The second substrate 200 is a thermal adhesive film or a photo-adhesive film.
[0127] Secondly, please refer to Figures 5B to 5D A first light with a first wavelength is provided above the first substrate 100. The first light with the first wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12000 nanometers. The first light with the first wavelength is irradiated on the first substrate 100 where the plurality of electronic components 121J-12NJ in the Jth row of the first electronic component matrix are located, so that the plurality of electronic components 121J-12NJ in the Jth row are thermally decomposed or photolyzed to lose viscosity, and the plurality of electronic components 121J-12NJ in the Jth row are all peeled off and bonded to the second upper surface 200A of the second substrate 200. The fourth embodiment is described by exemplifying that the plurality of electronic components 121J-12NJ in the Jth row are all selectively peeled off and bonded to the second upper surface 200A of the second substrate 200. However, according to other embodiments of the present invention, a portion of the plurality of electronic components 121J-12NJ in the Jth row may be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as needed. Next, the first substrate 100 is displaced relative to the second substrate 200 along the first axis direction by a distance (X2-X1), X2>0 and X1≠X2. Then, the first light having the first wavelength is irradiated on the first substrate 200 where the plurality of electronic components 121(J+1) to 12N(J+1) in the (J+1)th row of the first electronic component matrix are located, so that the plurality of electronic components 121(J+1) to 12N(J+1) in the (J+1)th row are thermally decomposed or photolyzed to lose viscosity, and all the plurality of electronic components 121(J+1) to 12N(J+1) in the (J+1)th row are peeled off and bonded to the second upper surface 200A of the second substrate 200, where J is a natural number and 1≤J≤(M-1). In the fourth embodiment, all of the aforementioned multiple electronic components 121(J+1)~12N(J+1) in the (J+1)th row are selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as an example for explanation. However, according to other embodiments of the present invention, part of the aforementioned multiple electronic components 121(J+1)~12N(J+1) in the (J+1)th row can also be selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as needed.
[0128] like Figure 5BAs shown, when J=1, a first light with a first wavelength is provided above the first substrate 100. The first light with the first wavelength is, for example but not limited to, light with a wavelength between 100 nanometers and 12000 nanometers, and the first light with the first wavelength is irradiated on the first substrate 100 where the plurality of electronic components 1211-12N1 in the first row of the first electronic component matrix are located, so that the plurality of electronic components 1211-12N1 in the first row are thermally decomposed or photolyzed to lose viscosity, and the plurality of electronic components 1211-12N1 in the first row are all peeled off and bonded to the second upper surface 200A of the second substrate 200. The fourth embodiment of the present invention uses the plurality of electronic components 1211-12N1 in the first row to be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as an example for explanation. However, according to other embodiments of the present invention, part of the plurality of electronic components 1211-12N1 in the first row may be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as needed. Secondly, as Figure 5C As shown, the first substrate 100 is first displaced relative to the second substrate 200 along the first axis direction by a distance (X2-X1), X2>0 and X1≠X2. Then, the first light with the first wavelength is irradiated on the first substrate 200 where the plurality of electronic components 1212~12N2 in the second row of the first electronic component matrix are located, so that the plurality of electronic components 1212~12N2 in the second row are thermally decomposed or photolyzed to lose their viscosity, and all of the plurality of electronic components 1212~12N2 in the second row are peeled off and bonded to the second upper surface 200A of the second substrate 200. This fourth embodiment uses the example of all of the plurality of electronic components 1212~12N2 in the second row being selectively peeled off and bonded to the second upper surface 200A of the second substrate 200, but according to other embodiments of the present invention, part of the plurality of electronic components 1212~12N2 in the second row may also be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as needed. Similarly, Figure 5D As shown, the other electronic components 1213 - 12NM in the 3rd to Mth rows can also be selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 using the same method as described above.
[0129] like Figure 5EAs shown, after all of the plurality of electronic components 1211 to 12NM located on the first substrate 100 are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 using the above method, a second electronic component matrix (not labeled) can be formed on the second upper surface 200A of the second substrate 200, and the row pitch and column pitch between the second electronic component matrices are X2 and Y1, respectively. Among them, when X2 > X1, that is, the row pitch X2 of the second electronic component matrix is greater than the row pitch X1 of the first electronic component matrix; when X2 < X1, that is, the row pitch X2 of the second electronic component matrix is less than the row pitch X1 of the first electronic component matrix.
[0130] As Figures 5F to 5H shown, in the fourth embodiment, all or part of the plurality of electronic components 1211 to 12NM located on the second substrate 200 can be further transferred to the third substrate 300, and a third electronic component matrix (not labeled) is formed on the third substrate 300, and the row pitch and column pitch of the third electronic component matrix (not labeled) are X2 and Y2, respectively.
[0131] As Figures 5F to 5HAs shown, a third substrate 300 is provided and disposed below the second substrate 200. The third substrate 300 has a third upper surface 300A and a third lower surface 300B opposite to each other, and the second upper surface 200A of the second substrate 200 faces the third upper surface 300A of the third substrate 300. Then, a second light with a second wavelength is provided above the second substrate 200. The second light with a second wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12000 nanometers, and the second light with the second wavelength is irradiated on the second substrate 200 where the plurality of electronic components 12K1-12KM in the Kth column of the second electronic component matrix are located, K is a natural number, and 1≤K≤(N-1), so that the second substrate 200 is thermally decomposed or photolyzed to lose its viscosity, and the plurality of electronic components 12K1-12KM in the Kth column are all or partially peeled off and bonded to the third upper surface of the third substrate. In the fourth embodiment, all of the aforementioned multiple electronic components 12K1~12KM in the Kth column are selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as an example for explanation. However, according to other embodiments of the present invention, part of the aforementioned multiple electronic components 12K1~12KM in the Kth column can also be selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200 as needed. Then, the second substrate 200 is displaced relative to the third substrate 300 along the second axis direction by a distance (Y2-Y1), wherein Y2>0 and Y1≠Y2, and then the second light with the second wavelength is irradiated on the second substrate 200 where the plurality of electronic components 12(K+1)1~12(K+1)M in the (K+1)th column of the second electronic component matrix are located, so that the second substrate 200 is thermally decomposed or photolyzed to lose its viscosity, and the plurality of electronic components 12(K+1)1~12(K+1)M in the (K+1)th column are fully or partially peeled off and bonded to the third upper surface 300A of the third substrate 300. When all or part of the aforementioned multiple electronic components 1211~12NM located on the aforementioned second substrate 200 are selectively peeled off and bonded to the third upper surface 300A of the aforementioned third substrate 300, a third electronic component matrix (not marked) can be formed on the aforementioned third substrate 300, and the row spacing and column spacing of the aforementioned third electronic component matrix (not marked) are X2 and Y2 respectively.
[0132] like Fig. 5FAs shown, when K=1, a second light with a second wavelength is provided above the second substrate 200. The second light with a second wavelength is, for example but not limited to, a light with a wavelength between 100 nanometers and 12000 nanometers, and the second light with the second wavelength is irradiated on the second substrate 200 where the plurality of electronic components 1211-121M in the first column of the second electronic component matrix are located, so that the second substrate 200 is thermally decomposed or photolyzed to lose viscosity, and the plurality of electronic components 1211-121M in the first column are all peeled off and bonded to the third upper surface of the third substrate. In the fourth embodiment, the plurality of electronic components 1211-121M in the first column are all selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as an example. However, according to other embodiments of the present invention, the plurality of electronic components 1211-121M in the first column may also be partially selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as needed.
[0133] Then, if Figure 5G As shown, the second substrate 200 is displaced relative to the third substrate 300 along the second axis direction by a distance (Y2-Y1), wherein Y2>0 and Y1≠Y2, and then the second light having the second wavelength is irradiated on the second substrate 200 where the plurality of electronic components 1221-122M in the second column of the second electronic component matrix are located, so that the second substrate 200 is thermally decomposed or photolyzed to lose its viscosity, and the plurality of electronic components 1221-122M in the second column are all peeled off and bonded to the third upper surface 300A of the third substrate 300. In the fourth embodiment, the plurality of electronic components 1221-122M in the second column are all selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as an example. However, according to other embodiments of the present invention, the plurality of electronic components 1221-122M in the second column may also be partially selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 as needed. Similarly, the other electronic components 1231 - 12NM in the 3rd to Nth columns can also be selectively peeled off in whole or in part and bonded to the third upper surface 300A of the third substrate 300 by the same method as described above.
[0134] like Figure 5HAs shown, after all of the plurality of electronic components 1211-12NM located on the second substrate 200 are selectively peeled off and bonded to the third upper surface 300A of the third substrate 300, a third electronic component matrix (not labeled) can be formed on the third substrate 300, and the row pitch and column pitch of the third electronic component matrix (not labeled) are X2 and Y2, respectively. Among them, when Y2>Y1, that is, the column pitch of the third electronic component matrix is greater than the column pitch of the second electronic component matrix; when Y2<Y1, that is, the column pitch of the third electronic component matrix is less than the column pitch of the second electronic component matrix.
[0135] In the fourth embodiment, it is exemplified that all of the plurality of electronic components 1211-12NM of the second electronic component matrix located on the second substrate 200 are selectively peeled off and bonded to the third upper surface 300A of the third substrate 300. However, in other embodiments of the present invention, it is also possible to selectively peel off and bond a part of the plurality of electronic components 1211-12NM of the second electronic component matrix located on the second substrate 200 to the third upper surface 300A of the third substrate 300 as needed.
[0136] Embodiment Five
[0137] Hereinafter, reference will be made to Figures 6A to 6E to describe in detail a method for transferring a large number of electronic components with adjustable pitch disclosed in this fifth embodiment.
[0138] First, please refer to Fig. 6A . As Fig. 6A shown, a first substrate 100 is provided. The first substrate 100 has opposite first upper surface 100A and first lower surface 100B. Among them, the first upper surface 100A of the first substrate 100 has a plurality of electronic components 1211-12NM, and the plurality of electronic components 1211-12NM are respectively arranged along the first axis direction and the second axis direction to form a first electronic component matrix (not labeled) formed by arranging M rows of electronic components multiplied by N columns of electronic components. Among them, the first substrate 100 is a thermal de-bonding film or a photo de-bonding film. The first axis direction and the second axis direction are substantially perpendicular to each other. M and N are natural numbers greater than 1, and the row pitch and column pitch of the first electronic component matrix are X1 and Y1, respectively, and X1, Y1>0. In the first embodiment, it is exemplified that the first axis direction is the X-axis direction and the second axis direction is the Y-axis direction. However, in other embodiments of the present invention, it is also possible to select the first axis direction as the Y-axis direction and the second axis direction as the X-axis direction as needed.
[0139] The aforementioned multiple electronic components 1211-12NM of the fifth embodiment are, for example, but not limited to, selected from one or more groups consisting of light emitting diodes, laser diodes, and semiconductor components. Among them, the aforementioned multiple light emitting diodes are, for example, but not limited to, emitting red light, green light, blue light, yellow light, white light, infrared light, or ultraviolet light; the wavelengths of the aforementioned multiple laser diodes are, for example, but not limited to, between 390 nanometers and 1700 nanometers; the aforementioned multiple semiconductor components are, for example, but not limited to, selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
[0140] Secondly, please refer to Figures 6B to 6C .like Figures 6B to 6C As shown, a second substrate 200 is provided and disposed below the first substrate 100. The second substrate 200 has a second upper surface 200A and a second lower surface 200B relative to each other, and the first upper surface 100A of the first substrate 100 faces the second upper surface 200A of the second substrate 200, wherein the second substrate 200 is a thermal adhesive film or a photolytic adhesive film.
[0141] Secondly, the plurality of electronic components located in the R1th row of the first substrate are used as a first baseline 110 of the first substrate 100 along the first axis direction, and the plurality of electronic components located in the R2th row of the second substrate 200 are used as a second baseline 210 of the second substrate 200 along the first axis direction, and the first baseline 110 is aligned with the second baseline 210. Then, a first light with a first wavelength is provided above the first substrate 100, and the first light with a first wavelength is a wavelength such as but not limited to light between 100 nanometers and 12000 nanometers, so that the first light with the first wavelength irradiates the first substrate 100 where the electronic component 12 (N1) J located in the N1th row of the first electronic component matrix or the plurality of electronic components 12 (N1) 1 to 12 (N1) M are located, so that the electronic component 12 (N1) J located in the N1th row of the first substrate or the plurality of electronic components 12 (N1) 1 to 12 (N1) M are pyrolyzed or photolyzed to lose viscosity, and the electronic component 12 (N1) J located in the N1th row of the first substrate or the plurality of electronic components 1 2(N1)1~12(N1)M are selectively stripped and bonded to the second upper surface 200A of the second substrate 200, so that they become the electronic components 22(N2)(j) in the N2th column of the second electronic component matrix located on the second upper surface 200A of the second substrate 200 or the aforementioned plurality of electronic components 22(N2)1~22(N2)P, wherein R1, R2, N1, N2, J, j are natural numbers, N1≤N, N2≤Q, 1≤R1≤N1, 1≤R2≤N2, 1≤J≤M, 1≤j≤P, and P is a natural number greater than 1, P≠M. Figure 6CAs shown, when all or part of the aforementioned multiple electronic components 1211~12NM located on the aforementioned first substrate 100 are transferred to the aforementioned second substrate 200, a second electronic component matrix (not marked) formed by P rows of electronic components multiplied by Q columns of electronic components can be formed on the second upper surface 200 of the aforementioned second substrate 200, wherein P and Q are natural numbers greater than 1, P≠M and / or Q≠N, and wherein the column spacing of the aforementioned second electronic component matrix is Y2, Y2>0 and Y1≠Y2.
[0142] Among them, the distance ΔY1 between the electronic component 12 (N1) J located in the N1th column of the aforementioned first substrate 100 or the aforementioned multiple electronic components 12 (N1) 1~12 (N1) M and the first baseline 110 of the first substrate 100 is = (N1-R1)*Y1; the distance ΔY2 between the electronic component 22 (N2) J located in the N2th column of the aforementioned second substrate 200 or the aforementioned multiple electronic components 22 (N2) 1~12 (N2)P and the second baseline 210 of the second substrate 200 is = (N1-R2)*Y2. Therefore, when the electronic component 12 (N1) J located in the N1th column of the first electronic component matrix of the aforementioned first substrate 100 or the aforementioned multiple electronic components 12 (N1) 1 to 12 (N1) M are transferred to the aforementioned second substrate 200 and become the electronic component 22 (N2) J in the N2th column of the aforementioned second electronic component matrix or the aforementioned multiple electronic components 22 (N2) 1 to 12 (N2) P, the relative movement distance ΔY along the aforementioned second axis direction (Y-axis direction) is [(N2-R2)*Y2-(N1-R1)*Y1].
[0143] like Figures 6B to 6CAs shown, when R1=1 and R2=2, the plurality of electronic components in the first column of the first substrate serve as a first baseline 110 of the first substrate 100 along the first axis direction, and the plurality of electronic components in the second column of the second substrate 200 serve as a second baseline 210 of the second substrate 200 along the first axis direction, and the first baseline 110 is aligned with the second baseline 210. Then, a first light with a first wavelength is provided above the first substrate 100. The first light with the first wavelength is a light with a wavelength, for example but not limited to, between 100 nanometers and 12000 nanometers, so that the first light with the first wavelength irradiates the first substrate 100 where the electronic component 12 (N1) J located in the N1th column of the first electronic component matrix or the plurality of electronic components 12 (N1) 1 to 12 (N1) M are located, so that the electronic component 12 (N1) J located in the N1th column of the first substrate or the plurality of electronic components 12 (N1) 1 to 12 (N1) M are thermally decomposed or photolyzed to lose viscosity, and the electronic component 12 (N1) J located in the N1th column of the first substrate or the plurality of electronic components 12 (N1) 1 to 12 (N1) M are selectively peeled off and bonded to the second upper surface 200A of the second substrate 200 to become the electronic component 22 (N2) J located in the N2th column of the second electronic component matrix or the plurality of electronic components 22 (N2) 1 to 12 (N2) P, wherein N1 and N2 are natural numbers, N1≤N, N2≤Q.
[0144] like Figure 6C As shown, the distance between the electronic component 12 (N1) J located in the N1th column of the first substrate 100 or the plurality of electronic components 12 (N1) 1 to 12 (N1) M and the first baseline 110 of the first substrate 100 is ΔY1 = (N1-1)*Y1; the distance between the electronic component 22 (N2) J located in the N2th column of the second substrate 200 or the plurality of electronic components 22 (N2) 1 to 22 (N2) P and the second baseline 110 of the second substrate 200 is ΔY2 = (N2-2)*Y2. Therefore, when the electronic component 12 (N1) J located in the N1th column of the first electronic component matrix of the aforementioned first substrate 100 or the aforementioned multiple electronic components 12 (N1) 1 to 12 (N1) M are transferred to the aforementioned second substrate 200 and become the electronic component 22 (N2) J in the N2th column of the aforementioned second electronic component matrix or the aforementioned multiple electronic components 22 (N2) 1 to 12 (N2) P, the relative movement distance ΔY along the aforementioned second axis direction is ΔY = ΔY2 - ΔY1, that is, ΔY is [(N2-2)*Y2-(N1-1)*Y1].
[0145] The fifth embodiment of the present invention can further transfer the second matrix located on the aforementioned second substrate 200 to a third substrate 300, and form a third electronic component matrix (not shown) formed by U rows of electronic components multiplied by V columns of electronic components on the aforementioned third substrate 300, and the row spacing and column spacing of the aforementioned third electronic component matrix are X2 and Y2 respectively, wherein U and V are natural numbers greater than 1, X2, Y2>0, and X1≠X2, Y1≠Y2.
[0146] like Figure 6D~4F As shown, the fifth embodiment may further provide a third substrate 300, and the third substrate 300 is disposed below the second substrate 200, the third substrate 300 having a third upper surface 300A and a third lower surface 300B relative to each other, and the second upper surface 200A of the second substrate 200 faces the third upper surface 300A of the third substrate 300, and the second electronic component matrix located on the second substrate 200 is transferred to the third substrate 300, and a third electronic component matrix (not shown) formed by U rows of electronic components multiplied by V columns of electronic components is formed on the third upper surface 300A of the third substrate 300, and the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively, wherein U and V are natural numbers greater than 1.
[0147] The aforementioned multiple electronic components 221 (S1)~22Q (S1) located in the S1th row of the aforementioned second substrate 200 are used as a third baseline 250 of the aforementioned second substrate 200 along the aforementioned second axis direction, and the aforementioned multiple electronic components 221 (S2)~22V (S2) located in the S2th row of the aforementioned third substrate 300 are used as a fourth baseline 350 of the aforementioned third substrate 300 along the aforementioned second axis direction, and the aforementioned third baseline 250 is aligned with the aforementioned fourth baseline 350. Then, a second light with a second wavelength is provided above the second substrate, wherein the second light with a second wavelength is a light with a wavelength between 100 nanometers and 12000 nanometers, and the second light with the second wavelength is irradiated on the electronic component 22K (M1) located in the M1th row of the second electronic component matrix or the second substrate 200 where the plurality of electronic components 221 (M1) to 22Q (M1) are located, so that the electronic component 22K (M1) located in the M1th row of the second substrate is thermally decomposed or photo-decomposed to lose its viscosity and the electronic component 22K (M1) located in the M1th row of the second substrate is decomposed. M1) or the aforementioned multiple electronic components 221 (M1) ~ 22Q (M1) are selectively peeled off and bonded to the third upper surface 300A of the aforementioned third substrate 300, and become the electronic component 32k (M2) of the M2th row of the aforementioned third electronic component matrix or the aforementioned multiple electronic components 321 (M2) ~ 32V (M2), wherein S1, S2, M1, M2, K, k are natural numbers, M1≤M, M2≤U, 1≤S1≤M1, 1≤S2≤M2, and 1≤K≤Q, 1≤k≤V.
[0148] The distance ΔX1 between the electronic component 22K (M1) located in the M1th row of the second substrate 200 or the aforementioned multiple electronic components 221 (M1) to 22Q (M1) and the third baseline 250 of the second substrate 200 is equal to (M1-S1)*X1; the distance ΔX2 between the electronic component 32k (M2) located in the M2th row of the third substrate 300 or the aforementioned multiple electronic components 321 (M2) to 32V (M2) and the fourth baseline 350 of the third substrate 300 is equal to (M1-S2)*X2. Therefore, when the electronic component 22K (M1) or the plurality of electronic components 221 (M1) to 22Q (M1) located in the M1th row of the second substrate 200 is transferred to the third substrate 300 and becomes the electronic component 32k (M2) or the plurality of electronic components 321 (M2) to 32V (M2) in the M2th column of the third electronic component matrix, the relative movement distance ΔX along the first axis direction (X axis direction) is [(M2-S2)*X2-(M1-S1)*X1]
[0149] like Fig.6DAs shown, when S1=1 and S2=2, the plurality of electronic components 2211~22Q1 located in the first row of the second substrate 200 are used as a third baseline 250 of the second substrate 200 along the second axis direction, and the plurality of electronic components 2212~22V2 located in the second row of the third substrate 300 are used as a fourth baseline 350 of the third substrate 300 along the second axis direction, and the third baseline 250 is aligned with the fourth baseline 350. Then, a second light with a second wavelength is provided above the second substrate, wherein the second light with the second wavelength is a light with a wavelength between 100 nanometers and 12000 nanometers, and the second light with the second wavelength is irradiated on the second substrate 200 where the electronic component 22K (M1) located in the M1th row of the second electronic component matrix or the plurality of electronic components 221 (M1) to 22Q (M1) are located, so that the electronic component 22K (M1) located in the M1th row of the second substrate or the plurality of electronic components 221 (M1) to 22Q (M1) are thermally decomposed or photolyzed to lose viscosity, and the electronic component 22K (M1) located in the M1th row of the second substrate or the plurality of electronic components 221 (M1) to 22Q (M1) are selectively peeled off and bonded to the third upper surface 300A of the third substrate 300, and become the electronic component 32k (M2) located in the M2th row of the third electronic component matrix or the plurality of electronic components 321 (M2) to 32V (M2). Among them, M1, M2, K, k are natural numbers, M1≤M, M2≤U, and 1≤K≤Q, 1≤k≤V.
[0150] like Fig. 6E As shown, the distance ΔX1 between the electronic component 22K (M1) located in the M1th row of the second substrate 200 or the aforementioned multiple electronic components 221 (M1) ~ 22Q (M1) and the third baseline 250 of the second substrate 200 is = (M1-1)*X1; the distance ΔX2 between the electronic component 32k (M2) located in the M2th row of the third substrate 300 or the aforementioned multiple electronic components 321 (M2) ~ 32V (M2) and the fourth baseline 350 of the third substrate 300 is = (M1-2)*X2. Therefore, when the electronic component 22K (M1) located in the M1th row of the aforementioned second substrate 200 or the aforementioned multiple electronic components 221 (M1) to 22Q (M1) are transferred to the aforementioned third substrate 300 and become the electronic component 32k (M2) in the M2th column of the aforementioned third electronic component matrix or the aforementioned multiple electronic components 321 (M2) to 32V (M2), the relative movement distance ΔX along the aforementioned first axis direction (X-axis direction) is equal to ΔX2-ΔX1, that is, ΔX=[(M2-2)*X2-(M1-1)*X1].
[0151] like Fig. 6EAs shown, when the plurality of electronic components 2211-12QP located on the second substrate 200 are selectively peeled off and bonded to the third upper surface 300A of the third substrate 300, a third electronic component matrix (not marked) can be formed on the third substrate 300, and the row spacing and column spacing of the third electronic component matrix (not marked) are X2 and Y2 respectively.
[0152] Embodiment 6
[0153] The following will refer to Figures 7A to 7E A method for mass transferring electronic components with adjustable spacing disclosed in the sixth embodiment is described in detail.
[0154] First, see Fig. 7A .like Fig. 7A As shown, a first substrate 100 is provided, the first substrate 100 has a first upper surface 100A and a first lower surface 100B opposite to each other, wherein the first upper surface 100A of the first substrate 100 has a plurality of electronic components 1211-12NM, and the plurality of electronic components 1211-12NM are arranged along the first axis direction and the second axis direction respectively, forming a first electronic component matrix (not shown) formed by M rows of electronic components multiplied by N columns of electronic components, wherein the first substrate 100 is a pyrolytic adhesive film or a photolytic adhesive film, the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0. In the first embodiment, the first axis direction is the X axis direction and the second axis direction is the Y axis direction as an example, but in other embodiments according to the present invention, the first axis direction can also be selected as the Y axis direction and the second axis direction as the X axis direction as needed.
[0155] The aforementioned multiple electronic components 1211-12NM of the sixth embodiment are, for example, but not limited to, selected from one or more groups consisting of light emitting diodes, laser diodes, and semiconductor components. Among them, the aforementioned multiple light emitting diodes are, for example, but not limited to, emitting red light, green light, blue light, yellow light, white light, infrared light, or ultraviolet light; the aforementioned multiple laser diodes have wavelengths, for example, but not limited to, between 390 nanometers and 1700 nanometers; the aforementioned multiple semiconductor components are, for example, but not limited to, selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
[0156] Secondly, please refer to Figures 7B to 7C .like Figures 7B to 7CAs shown, a second substrate 200 is provided and disposed below the first substrate 100. The second substrate 200 has a second upper surface 200A and a second lower surface 200B relative to each other, and the first upper surface 100A of the first substrate 100 faces the second upper surface 200A of the second substrate 200, wherein the second substrate 200 is a thermal adhesive film or a photolytic adhesive film.
[0157] Secondly, the plurality of electronic components located in the S1th row of the first substrate 100 are used as a first baseline 110' of the first substrate 100 along the second axis (Y axis), and the plurality of electronic components located in the S2th row of the second substrate 200 are used as a second baseline 210' of the second substrate 200 along the second axis (Y axis), and the first baseline 110' is aligned with the second baseline 210'. Then, a first light with a first wavelength is provided above the first substrate 100, and the first light with a first wavelength is a wavelength such as but not limited to light between 100 nanometers and 12000 nanometers, so that the first light with the first wavelength irradiates the first substrate 100 where the electronic component 12K (M1) located in the M1th row of the first electronic component matrix or the plurality of electronic components 121 (M1) to 12N (M1) are located, so that the electronic components are thermally decomposed or photodecomposed to lose viscosity and the electronic components located in the M1th row of the first substrate 100 are decomposed. The sub-component 12K (M1) or the aforementioned multiple electronic components 121 (M1) to 12N (M1) are selectively stripped and bonded to the second upper surface 200A of the aforementioned second substrate 200, so that they become the electronic component 22k (M2) or the aforementioned multiple electronic components 221 (M2) to 22Q (M2) located in the M2th column of the second electronic component matrix of the aforementioned second substrate 200, wherein S1, S2, M1, and M2 are natural numbers, M1≤M, M2≤P, and 1≤S1≤M1, 1≤S2≤M2. Figure 7C As shown, when all or part of the aforementioned multiple electronic components 1211~12NM located on the aforementioned first substrate 100 are transferred to the aforementioned second substrate 200, a second electronic component matrix (not marked) formed by P rows of electronic components multiplied by Q columns of electronic components can be formed on the second upper surface 200 of the aforementioned second substrate 200, wherein P and Q are natural numbers greater than 1, P≠M and / or Q≠N, and wherein the row spacing of the aforementioned second electronic component matrix is X2, X2>0 and X1≠X2.
[0158] Among them, the distance ΔX1 between the electronic component 12K (M1) located in the M1th row of the aforementioned first substrate 100 or the aforementioned multiple electronic components 121 (M1) ~ 12N (M1) and the first baseline 110' of the first substrate 100 is = (M1-S1)*X1; the distance ΔX2 between the electronic component 22k (M2) located in the M2th row of the aforementioned second substrate 200 or the aforementioned multiple electronic components 221 (M2) ~ 22Q (M2) and the second baseline 210' of the second substrate 200 is = (M2-S2)*X2. Therefore, when the electronic component 12K (M1) located in the M1th row of the first electronic component matrix of the aforementioned first substrate 100 or the aforementioned multiple electronic components 121 (M1) to 12N (M1) are transferred to the aforementioned second substrate 200 and become the electronic component 22k (M2) located in the M2th column of the second electronic component matrix of the aforementioned second substrate 200 or the aforementioned multiple electronic components 221 (M2) to 22Q (M2), the relative movement distance ΔX along the aforementioned first axis (X-axis) direction is ΔX2–ΔX1, that is, ΔX2=[(M2-S2)*X2-(M1-S1)*X1].
[0159] like Figure 7B As shown, when S1=1 and S2=2, the plurality of electronic components 1211~12N1 located in the first row of the first substrate 100 are used as a first baseline 110' of the first substrate 100 along the second axis (Y axis) direction, and the plurality of electronic components 2212~22V2 located in the second row of the second substrate 200 are used as a second baseline 210' of the second substrate 200 along the second axis (Y axis) direction, and the first baseline 110 is aligned with the second baseline 210. Then, a first light with a first wavelength is provided above the first substrate 100. The first light with a first wavelength is a light with a wavelength, for example but not limited to, between 100 nanometers and 12000 nanometers. The first light with the first wavelength irradiates the first substrate 100 where the electronic component 12K (M1) or the plurality of electronic components 121 (M1) to 12N (M1) located in the M1th row of the first electronic component matrix is located, so that the electronic component 12K (M1) or the plurality of electronic components 121 (M1) to 12N (M1) are thermally decomposed or photodecomposed to lose viscosity and the first substrate 100 located in the first electronic component matrix is thermally decomposed or photodecomposed to lose viscosity and the first substrate 10 ... The electronic component 12K (M1) in the M1th row of the substrate 100 or the aforementioned multiple electronic components 121 (M1) to 12N (M1) are selectively peeled off and bonded to the second upper surface 200A of the aforementioned second substrate 200, so that they become the electronic component 22k (M2) in the M2th column of the second electronic component matrix of the aforementioned second substrate 200 or the aforementioned multiple electronic components 221 (M2) to 22Q (M2), wherein M1 and M2 are natural numbers, M1≤M, M2≤P.
[0160] like Figure 7CAs shown, when all or part of the aforementioned multiple electronic components 1211~12NM located on the aforementioned first substrate 100 are transferred to the aforementioned second substrate 200, a second electronic component matrix (not marked) formed by P rows of electronic components multiplied by Q columns of electronic components can be formed on the second upper surface 200 of the aforementioned second substrate 200, wherein P and Q are natural numbers greater than 1, P≠M and / or Q≠N, and wherein the row spacing of the aforementioned second electronic component matrix is X2, X2>0 and X1≠X2.
[0161] Among them, the distance ΔX1 between the electronic component 12K (M1) located in the M1th row of the aforementioned first substrate 100 or the aforementioned multiple electronic components 121 (M1) ~ 12N (M1) and the first baseline 110' of the first substrate 100 is = (M1-1)*X1; the distance ΔX2 between the electronic component 22k (M2) located in the M2th row of the aforementioned second substrate 200 or the aforementioned multiple electronic components 221 (M2) ~ 22Q (M2) and the second baseline 210' of the second substrate 200 is = (M2-2)*X2. Therefore, when the electronic component 12K (M1) located in the M1th row of the first electronic component matrix of the aforementioned first substrate 100 or the aforementioned multiple electronic components 121 (M1) to 12N (M1) are transferred to the aforementioned second substrate 200 and become the electronic component 22k (M2) located in the M2th column of the second electronic component matrix of the aforementioned second substrate 200 or the aforementioned multiple electronic components 221 (M2) to 22Q (M2), the relative movement distance ΔX along the aforementioned first axis (X-axis) direction is equal to ΔX2-ΔX1, that is, ΔX=[(M2-2)*X2-(M1-1)*X1].
[0162] The sixth embodiment of the present invention can further transfer the second matrix located on the aforementioned second substrate 200 to a third substrate 300, and form a third electronic component matrix (not shown) on the aforementioned third substrate 300, which is formed by arranging U rows of electronic components by V columns of electronic components, and the row spacing and column spacing of the aforementioned third electronic component matrix are X2 and Y2 respectively, wherein U and V are natural numbers greater than 1, X2, Y2>0, and X1≠X2, Y1≠Y2.
[0163] like Figures 7D to 7EAs shown, the fifth embodiment may further provide a third substrate 300, and the third substrate 300 is disposed below the second substrate 200, the third substrate 300 having a third upper surface 300A and a third lower surface 300B relative to each other, and the second upper surface 200A of the second substrate 200 faces the third upper surface 300A of the third substrate 300, and the second electronic component matrix located on the second substrate 200 is transferred to the third substrate 300, and a third electronic component matrix (not shown) formed by U rows of electronic components multiplied by V columns of electronic components is formed on the third upper surface 300A of the third substrate 300, and the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively, wherein U and V are natural numbers greater than 1.
[0164] like Figures 7D to 7E As shown, the plurality of electronic components located in the R1th row of the second substrate are used as a third baseline 250' of the second substrate 200 along the first axis (X axis), and the plurality of electronic components located in the R2th row of the third substrate 300 are used as a fourth baseline 350' of the third substrate 300 along the first axis (X axis), and the third baseline 250' is aligned with the fourth baseline 350'. Then, a second light with a second wavelength is provided above the second substrate 200. The second light with a second wavelength is a wavelength such as but not limited to light between 100 nanometers and 12000 nanometers, so that the second light with a second wavelength irradiates the second substrate 200 where the electronic component 22 (N1) J located in the M1th row of the second electronic component matrix or the plurality of electronic components 22 (N1) 1 to 22 (N1) P are located, so that the electronic components are thermally decomposed or photodecomposed to lose viscosity, and the second light located in the N1th row of the second substrate is irradiated with the second light. The electronic component 22 (N1) J or the aforementioned multiple electronic components 22 (N1) 1 to 22 (N1) P are selectively stripped and bonded to the third upper surface 300A of the aforementioned third substrate 300, so that it is the electronic component 32 (N2) j or the aforementioned multiple electronic components 32 (N2) 1 to 32 (N2) U located in the N2th column of the third electronic component matrix of the third substrate 300, wherein R1, R2, N1, and N2 are natural numbers, N1≤P, N2≤U, and 1≤R1≤N1, 1≤R2≤N2.
[0165] Among them, the distance ΔY1 between the electronic component 22 (N1) J located in the N1th row of the aforementioned second substrate 200 or the aforementioned multiple electronic components 22 (N1) 1~22 (N1) P and the aforementioned third baseline 250' is (N1-R1)*Y1; the distance ΔY2 between the electronic component 32 (N2) j located in the N2th row of the aforementioned third substrate 300 or the aforementioned multiple electronic components 32 (N2) 1~32 (N2) U and the aforementioned fourth baseline 350' is (N2-R2)*Y2. Therefore, when the electronic component 22 (N1) J located in the N1th row of the second electronic component matrix of the aforementioned second substrate or the aforementioned multiple electronic components 22 (N1) 1 to 22 (N1) P are transferred to the electronic component 32 (N2) j located in the N2th row of the third electronic component matrix of the aforementioned third substrate 300 or the aforementioned multiple electronic components 32 (N2) 1 to 32 (N2) U, their relative movement distance ΔY along the aforementioned second axis (Y axis) direction is equal to ΔY2-ΔY1, that is, ΔY=[(N2-R2)*Y2-(N1-R1)*Y1].
[0166] like Fig.7D As shown, when R1=1 and R2=2, the plurality of electronic components 2211~221P located in the first column of the second substrate are used as a third baseline 250' of the second substrate 200 along the first axis (X-axis) direction, and the plurality of electronic components 3221~322U located in the second row of the third substrate 300 are used as a fourth baseline 350' of the third substrate 300 along the first axis (X-axis) direction, and the third baseline 250' is aligned with the fourth baseline 350'. Then, a second light with a second wavelength is provided above the second substrate 200. The second light with a second wavelength is a light with a wavelength, for example but not limited to, between 100 nanometers and 12000 nanometers. The second light with a second wavelength irradiates the second substrate 200 where the electronic component 22 (N1) J located in the M1th row of the second electronic component matrix or the plurality of electronic components 22 (N1) 1 to 22 (N1) P are located, so that the electronic component 22 (N1) 1 to 22 (N1) P are thermally decomposed or photo-decomposed to lose viscosity and the second substrate 200 is The electronic component 22 (N1) J in the N1th row of the substrate or the aforementioned multiple electronic components 22 (N1) 1 to 22 (N1) P are selectively stripped and bonded to the third upper surface 300A of the aforementioned third substrate 300, so that they are located in the N2th column of the third electronic component matrix of the third substrate 300. The electronic component 32 (N2) j or the aforementioned multiple electronic components 32 (N2) 1 to 32 (N2) U, wherein R1, R2, N1, and N2 are natural numbers, N1≤P, N2≤U.
[0167] Among them, the distance ΔY1 between the electronic component 22 (N1) J located in the N1th row of the aforementioned second substrate 200 or the aforementioned multiple electronic components 22 (N1) 1~22 (N1) P and the aforementioned third baseline 250' is (N1-1)*Y1; the distance ΔY2 between the electronic component 32 (N2) j located in the N2th row of the aforementioned third substrate 300 or the aforementioned multiple electronic components 32 (N2) 1~32 (N2) U and the aforementioned fourth baseline 350' is (N2-2)*Y2. Therefore, when the electronic component 22 (N1) J located in the N1th row of the second electronic component matrix of the aforementioned second substrate 200 or the aforementioned multiple electronic components 22 (N1) 1 to 22 (N1) P are transferred to the electronic component 32 (N2) j located in the N2th row of the third electronic component matrix of the aforementioned third substrate 300 or the aforementioned multiple electronic components 32 (N2) 1 to 32 (N2) U, their relative movement distance ΔY along the aforementioned second axis (Y axis) direction is equal to ΔY2-ΔY1, that is, ΔY=[(N2-2)*Y2-(N1-1)*Y1].
[0168] like Fig. 7E As shown, when the plurality of electronic components 2211-12QP located on the second substrate 200 are selectively peeled off and bonded to the third upper surface 300A of the third substrate 300, a third electronic component matrix (not marked) can be formed on the third substrate 300, and the row spacing and column spacing of the third electronic component matrix (not marked) are X2 and Y2 respectively.
[0169] Although the present invention has been disclosed as above by way of embodiments, it is not intended to limit the present invention. Anyone skilled in the art may make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be determined by the definition of the appended claims.
Claims
1. A method for mass transfer of electronic components with adjustable spacing, Features The following steps are involved: A first substrate is provided, the first substrate having a first upper surface and a first lower surface opposite to each other, wherein the first upper surface of the first substrate has a plurality of electronic components, and the plurality of electronic components are arranged along a first axis direction and a second axis direction respectively, forming a first electronic component matrix formed by arranging M rows of electronic components by N columns of electronic components, wherein the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0; a second substrate is provided, and the second substrate is disposed below the first substrate, the second substrate having a second upper surface and a second lower surface opposite to each other, and the first upper surface of the first substrate faces the second upper surface of the second substrate; as well as The plurality of electronic components on the first substrate are transferred in whole or in part to the second substrate, and a second electronic component matrix is formed on the second upper surface of the second substrate, wherein the row spacing and column spacing of the second electronic component matrix are X2 and Y2 respectively, X2 and Y2>0, and X1≠X2 and Y1≠Y2.
2. The method for mass transferring electronic components with adjustable spacing as claimed in claim 1, wherein the step of forming the second electronic component matrix is: include: Providing a first light with a first wavelength above the first substrate, and irradiating the first substrate with the first light with the first wavelength where the electronic components in the Jth row and the Kth column of the first electronic component matrix are located so that the electronic components are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the Jth row and the Kth column are selectively peeled off and bonded to the second upper surface of the second substrate, and then displacing the first substrate by a distance of (X2-X1) relative to the second substrate along the first axis direction, and irradiating the first substrate with the first light with the first wavelength where the electronic components in the (J+1)th row and the Kth column of the first electronic component matrix are located so that the electronic components are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the (J+1)th row and the Kth column are selectively peeled off and bonded to the second upper surface of the second substrate, wherein J, K, and X2 are all natural numbers, and 1≤J≤(M-1), 1≤K≤(N-1); and After all or part of the multiple electronic components in the Kth column of the first electronic component matrix are selectively peeled off and bonded to the second upper surface of the second substrate, the first substrate is firstly realigned with the second substrate, and then the first substrate is displaced by a distance (Y2-Y1) relative to the second substrate along the second axis direction, and then the first light with the first wavelength is irradiated to the first substrate where the electronic components in the Jth row and the (K+1)th column of the first electronic component matrix are located, so that the electronic components are thermally decomposed or photodecomposed to lose viscosity, and the electronic components in the Jth row and the (K+1)th column of the first electronic component matrix ... The sub-components are selectively peeled off and bonded to the second upper surface of the second substrate, and then the first substrate is displaced by a distance (X2-X1) relative to the second substrate along the first axis direction, and the first light with the first wavelength is irradiated on the first substrate where the electronic components in the (J+1)th row and (K+1)th column of the first electronic component matrix are located, so that they are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the (J+1)th row and (K+1)th column are selectively peeled off and bonded to the second upper surface of the second substrate, wherein Y2 is a natural number; When all or part of the plurality of electronic components on the first substrate are selectively peeled off and bonded to the second upper surface of the second substrate, the second electronic component matrix can be formed on the second upper surface of the second substrate.
3. The method for mass transferring electronic components with adjustable spacing as claimed in claim 1, wherein the step of forming the second electronic component matrix is: include: Providing a first light with a first wavelength above the first substrate, and irradiating the first substrate with the first light with the first wavelength where the electronic components in the Jth row and the Kth column of the first electronic component matrix are located, so that the electronic components are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the Jth row and the Kth column are selectively peeled off and bonded to the second upper surface of the second substrate, and then displacing the first substrate by a distance (Y2-Y1) relative to the second substrate along the second axis direction, so that the first light with the first wavelength irradiates the first substrate where the electronic components in the Jth row and the (K+1)th column of the first electronic component matrix are located, so that the electronic components are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the Jth row and the (K+1)th column are selectively peeled off and bonded to the second upper surface of the second substrate, wherein J, K, and Y2 are all natural numbers, and 1≤J≤(M-1), 1≤K≤(N-1); and After all or part of the multiple electronic components in the Jth row of the first electronic component matrix are selectively peeled off and bonded to the second upper surface of the second substrate, the first substrate is first realigned with the second substrate, and then the first substrate is displaced by a distance (X2-X1) relative to the second substrate along the first axis direction, and then the first light with the first wavelength is irradiated to the first substrate where the electronic components in the (J+1)th row and the Kth column of the first electronic component matrix are located, so that the electronic components are thermally decomposed or photodecomposed to lose their viscosity, and the electronic components in the (J+1)th row and the Kth column of the first electronic component matrix are The sub-components are selectively peeled off and bonded to the second upper surface of the second substrate, and then the first substrate is displaced by a distance (Y2-Y1) relative to the second substrate along the second axis direction, and the first light with the first wavelength is irradiated on the first substrate where the electronic components in the (J+1)th row and (K+1)th column of the first electronic component matrix are located, so that they are thermally decomposed or photolyzed to lose viscosity, and the electronic components in the (J+1)th row and (K+1)th column are selectively peeled off and bonded to the second upper surface of the second substrate, wherein X2 is a natural number; When all or part of the plurality of electronic components on the first substrate are selectively peeled off and bonded to the second upper surface of the second substrate, the second electronic component matrix can be formed on the second upper surface of the second substrate.
4. The method for mass transfer of electronic components with adjustable pitch as claimed in claim 2 or 3, wherein the first substrate is a pyrolytic adhesive film, and the first light with the first wavelength is a light with a wavelength between 100 nanometers and 12000 nanometers.
5. The method for mass transferring electronic components with adjustable pitch as claimed in claim 2 or 3, wherein the first substrate is a photoresist film, and the first light with the first wavelength is a light with a wavelength between 100 nanometers and 12000 nanometers. 6 . The method for mass transferring electronic components with adjustable pitch as claimed in claim 1 , wherein the plurality of electronic components are selected from one or more groups consisting of light emitting diodes, laser diodes and semiconductor components. 7 . The method for mass transferring electronic components with adjustable pitch as claimed in claim 6 , wherein the light emitted by the plurality of light emitting diodes is red light, green light, blue light, yellow light, white light, infrared light or ultraviolet light. 8 . The method for mass transferring electronic components with adjustable pitch as claimed in claim 6 , wherein the wavelengths of the plurality of laser diodes are between 390 nanometers and 1700 nanometers.
9. The method for mass transferring electronic components with adjustable pitch as claimed in claim 6, wherein the plurality of semiconductor components are selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits and analog integrated circuits.
10. A method for mass transfer of electronic components with adjustable spacing, Features The following steps are involved: A first substrate is provided, the first substrate having a first upper surface and a first lower surface opposite to each other, wherein the first upper surface of the first substrate has a plurality of electronic components, and the plurality of electronic components are arranged along a first axis direction and a second axis direction respectively, forming a first electronic component matrix formed by arranging M rows of electronic components by N columns of electronic components, wherein the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0; a second substrate is provided, and the second substrate is disposed below the first substrate, the second substrate having a second upper surface and a second lower surface opposite to each other, and the first upper surface of the first substrate faces the second upper surface of the second substrate; as well as The plurality of electronic components located on the first substrate are transferred in whole or in part to the second substrate. A substrate is provided, and a second electronic component matrix is formed on the second substrate, and the row spacing and column spacing of the second electronic component matrix are respectively X1, Y2 or X2, Y1, wherein X2, Y2>0, and X1≠X2, Y1≠Y2.
11. The method for mass transfer of electronic components with adjustable spacing as claimed in claim 10, wherein the row spacing and column spacing of the second electronic component matrix are X1 and Y2 respectively, and the step of forming the second electronic component matrix is: include: Providing a first light with a first wavelength above the first substrate, and irradiating the first light with the first wavelength on the first substrate where the plurality of electronic components in the Kth column of the first electronic component matrix are located, so as to thermally decompose or photodecompose the first substrate to lose viscosity, and all the plurality of electronic components in the Kth column are peeled off and bonded to the second upper surface of the second substrate; as well as The first substrate is displaced relative to the second substrate along the second axis direction by a distance of (Y2-Y1), and then the first light with a first wavelength is irradiated on the first substrate where the multiple electronic components in the (K+1)th column of the first electronic component matrix are located, so that the first substrate is thermally decomposed or photolyzed to lose its viscosity, and the multiple electronic components in the (K+1)th column are completely or partially peeled off and bonded to the second upper surface of the second substrate, K is a natural number, and 1≤K≤(N-1); wherein, when the multiple electronic components located on the first substrate are completely or partially selectively peeled off and bonded to the second upper surface of the second substrate, the second electronic component matrix can be formed on the second substrate.
12. The method for mass transferring electronic components with adjustable spacing as claimed in claim 11, further comprising the following steps: Providing a third substrate and disposing the third substrate below the second substrate, the third substrate having a third upper surface and a third lower surface opposite to each other, and the second upper surface of the second substrate faces the third upper surface of the third substrate; and The plurality of electronic components on the second substrate are transferred in whole or in part to the third substrate, and a third electronic component matrix is formed on the third substrate, wherein the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively.
13. The method for mass transferring electronic components with adjustable spacing as claimed in claim 12, wherein the step of forming the third electronic component matrix is: include: A second light with a second wavelength is provided above the second substrate, and the second light with the second wavelength is used to irradiate the second substrate where the plurality of electronic components in the Jth row of the second electronic component matrix are located, so that the second substrate is thermally decomposed or photodecomposed to lose viscosity, and the Jth row of the second electronic component matrix is formed. All or part of the plurality of electronic components in a row are peeled off and bonded to the third upper surface of the third substrate; and The second substrate is displaced relative to the third substrate along the first axis by a distance of (X2-X1), and then the second light having the second wavelength is irradiated on the second substrate where the plurality of electronic components in the (J+1)th row of the second electronic component matrix are located, so that the second substrate is thermally decomposed or photolyzed to lose its viscosity, and the plurality of electronic components in the (J+1)th row are completely or partially peeled off and bonded to the third upper surface of the third substrate, where J is a natural number and 1≤J≤(M-1); When all or part of the plurality of electronic components on the second substrate are selectively peeled off and bonded to the third upper surface of the third substrate, the third electronic component matrix can be formed on the third substrate.
14. The method for mass transfer of electronic components with adjustable spacing as claimed in claim 10, wherein the row spacing and column spacing of the second electronic component matrix are X2 and Y1 respectively, and the step of forming the second electronic component matrix is: include: Providing a first light with a first wavelength above the first substrate, and irradiating the first light with the first wavelength on the first substrate where the plurality of electronic components in the Jth row of the first electronic component matrix are located, so as to thermally decompose or photodecompose the first substrate to lose viscosity, and so that all or part of the plurality of electronic components in the Jth row are peeled off and bonded to the second upper surface of the second substrate; as well as The first substrate is displaced relative to the second substrate by a distance of (X2-X1) along the first axis direction, and then the first light with a first wavelength is irradiated on the first substrate where the multiple electronic components in the (J+1)th row of the first electronic component matrix are located, so that the first substrate is thermally decomposed or photolyzed to lose its viscosity, and the multiple electronic components in the (J+1)th row are completely or partially peeled off and bonded to the second upper surface of the second substrate, J is a natural number, and 1≤J≤(M-1); wherein, when the multiple electronic components located on the first substrate are completely or partially selectively peeled off and bonded to the second upper surface of the second substrate, the second electronic component matrix can be formed on the second substrate.
15. The method for mass transferring electronic components with adjustable spacing as claimed in claim 14, further comprising the following steps: Providing a third substrate and disposing the third substrate below the second substrate, the third substrate having a third upper surface and a third lower surface opposite to each other, and the second upper surface of the second substrate faces the third upper surface of the third substrate; and The plurality of electronic components on the second substrate are transferred in whole or in part to the third substrate, and a third electronic component matrix is formed on the third substrate, wherein the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively.
16. The method for mass transferring electronic components with adjustable spacing as claimed in claim 15, wherein the step of forming the third electronic component matrix is: include: A second light with a second wavelength is provided above the second substrate, and the second light with the second wavelength is used to irradiate the second substrate where the plurality of electronic components in the Kth column of the second electronic component matrix are located, so that the second substrate is thermally decomposed or photodecomposed to lose viscosity, and the Jth column of the second electronic component matrix is formed. All or part of the plurality of electronic components in a row are peeled off and bonded to the third upper surface of the third substrate; and The second substrate is displaced relative to the third substrate along the second axis direction by a distance of (Y2-Y1), and then the second light having the second wavelength is irradiated on the second substrate where the plurality of electronic components in the (K+1)th column of the second electronic component matrix are located, so that the second substrate is thermally decomposed or photolyzed to lose viscosity, and the plurality of electronic components in the (K+1)th column are completely or partially peeled off and bonded to the third upper surface of the third substrate, where K is a natural number and 1≤ K≤(N-1); When all or part of the plurality of electronic components on the second substrate are selectively peeled off and bonded to the third upper surface of the third substrate, the third electronic component matrix can be formed on the third substrate. 17 . The method for mass transferring electronic components with adjustable pitch as claimed in claim 11 or 14 , wherein the first substrate is a pyrolytic adhesive film, and the first light with the first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
18. The method for mass transfer of electronic components with adjustable pitch as claimed in claim 11 or 14, wherein the first substrate is a photoresist film, and the first light with the first wavelength is a light with a wavelength between 100 nanometers and 12000 nanometers.
19. The method for mass transferring electronic components with adjustable pitch as claimed in claim 13 or 16, wherein the second substrate is a pyrolytic adhesive film, and the second light with the second wavelength is a light with a wavelength between 100 nanometers and 12000 nanometers.
20. The method for mass transfer of electronic components with adjustable pitch as claimed in claim 13 or 16, wherein the second substrate is a photoresist film, and the second light with a second wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
21. The method for mass transferring electronic components with adjustable pitch as claimed in claim 10, wherein the plurality of electronic components are selected from one or more of the group consisting of light emitting diodes, laser diodes and semiconductor components.
22. The method for mass transferring electronic components with adjustable pitch as claimed in claim 21, wherein the light emitted by the plurality of light emitting diodes is red light, green light, blue light, yellow light, white light, infrared light or ultraviolet light.
23. The method for mass transferring electronic components with adjustable pitch as claimed in claim 21, wherein the wavelengths of the plurality of laser diodes are between 390 nanometers and 1700 nanometers.
24. The method for mass transferring electronic components with adjustable pitch as claimed in claim 21, wherein the plurality of semiconductor components are selected from one or more of the group consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
25. A method for mass transfer of electronic components with adjustable spacing, Features The following steps are involved: A first substrate is provided, the first substrate having a first upper surface and a first lower surface opposite to each other, wherein the first upper surface of the first substrate has a plurality of electronic components, and the plurality of electronic components are arranged along a first axis direction and a second axis direction respectively, forming a first electronic component matrix formed by arranging M rows of electronic components by N columns of electronic components, wherein the first axis direction and the second axis direction are substantially perpendicular to each other, M and N are natural numbers greater than 1, and the row spacing and column spacing of the first electronic component matrix are X1 and Y1 respectively, and X1 and Y1>0; a second substrate is provided, and the second substrate is disposed below the first substrate, the second substrate having a second upper surface and a second lower surface opposite to each other, and the first upper surface of the first substrate faces the second upper surface of the second substrate; as well as The plurality of electronic components located on the first substrate are transferred to the second substrate, and a second electronic component matrix formed by arranging P rows of electronic components by Q columns of electronic components is formed on the second upper surface of the second substrate, where P and Q are natural numbers greater than 1. P≠M and / or Q≠N. 26 . The method for mass transferring electronic components with adjustable pitch as claimed in claim 24 , wherein the column pitch of the second electronic component matrix is Y2 , Y2>0 and Y1≠Y2.
27. The method for mass transferring electronic components with adjustable spacing as claimed in claim 26, wherein the step of forming the second electronic component matrix is: include: Using the plurality of electronic components located in the R1th column of the first substrate as a first baseline of the first substrate along the first axis direction, using the plurality of electronic components located in the R2th column of the second substrate as a second baseline of the second substrate along the first axis direction, and aligning the first baseline with the second baseline; as well as A first light with a first wavelength is provided above the first substrate, so that the first light with the first wavelength irradiates the first substrate where the electronic components or the plurality of electronic components located in the N1th column of the first electronic component matrix are located, so that the electronic components or the plurality of electronic components located in the N1th column of the first substrate are thermally decomposed or photolyzed to lose viscosity, and the electronic components or the plurality of electronic components located in the N1th column of the first substrate are selectively peeled off and bonded to the second upper surface of the second substrate so that the electronic components or the plurality of electronic components located in the N2th column of the second electronic component matrix are located, wherein R1, R2, N1, and N2 are natural numbers, N1≤N, N2≤Q, and 1≤R1≤ N1, 1≤R2≤N2; Among them, when the one or more electronic components located in the N1th column of the first electronic component matrix of the first substrate are transferred to the N2th column of the second electronic component matrix of the second substrate, the relative movement distance along the second axis direction is [(N2-R2)*Y2-(N1-R1)*Y1].
28. The method for mass transferring electronic components with adjustable spacing as claimed in claim 27, further comprising the following steps: Providing a third substrate and disposing the third substrate below the second substrate, the third substrate having a third upper surface and a third lower surface opposite to each other, and the second upper surface of the second substrate faces the third upper surface of the third substrate; and The second electronic component matrix located on the second substrate is transferred to the third substrate, and a third electronic component matrix formed by U rows of electronic components multiplied by V columns of electronic components is formed on the third substrate, and the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively, where U and V are natural numbers greater than 1.
29. The method for mass transferring electronic components with adjustable spacing as claimed in claim 28, wherein the step of forming the third electronic component matrix is: include: Using the plurality of electronic components located in the S1th row of the second substrate as a third baseline of the second substrate along the second axis direction, using the plurality of electronic components located in the S2th row of the third substrate as a fourth baseline of the third substrate along the second axis direction, and aligning the third baseline with the fourth baseline; as well as A second light with a second wavelength is provided above the second substrate, so that the second light with the second wavelength irradiates the second substrate where the electronic components or the plurality of electronic components located in the M1th row of the second electronic component matrix are located, so that the electronic components or the plurality of electronic components located in the M1th row of the second substrate are thermally decomposed or photolyzed to lose viscosity and the electronic components or the plurality of electronic components located in the M1th row of the second substrate are selectively peeled off and bonded to the third upper surface of the third substrate so that the electronic components or the plurality of electronic components located in the M2th row of the third electronic component matrix are located, wherein S1, S2, M1, and M2 are natural numbers, M1≤M, M2≤U, and 1≤S1≤M1, 1≤S2≤M2; Among them, when the one or more electronic components located in the M1th row of the second electronic component matrix of the second substrate are transferred to the M2th row of the third electronic component matrix of the third substrate, their relative movement distance along the first axis direction is [(M2-S2)*X2-(M1-S1)*X1]. 30 . The method for mass transferring electronic components with adjustable pitch as claimed in claim 23 , wherein a row pitch of the second electronic component matrix is X2, X2>0 and X1≠X2.
31. The method for mass transferring electronic components with adjustable spacing as claimed in claim 30, wherein the step of forming the second electronic component matrix is: include: Using the plurality of electronic components located in the S1th row of the first substrate as a first baseline of the first substrate along the second axis direction, using the plurality of electronic components located in the S2th row of the second substrate as a second baseline of the second substrate along the second axis direction, and aligning the first baseline with the second baseline; as well as Providing a first light with a first wavelength above the first substrate, so that the first light with the first wavelength irradiates the first substrate where the electronic components or the plurality of electronic components located in the M1th row of the first electronic component matrix are located, so that the electronic components or the plurality of electronic components located in the M1th row of the first substrate are thermally decomposed or photolyzed to lose viscosity and the electronic components or the plurality of electronic components located in the M1th row of the first substrate are selectively peeled off and bonded to the second upper surface of the second substrate so that the electronic components or the plurality of electronic components located in the M2th row of the second electronic component matrix, wherein S1, S2, M1, and M2 are natural numbers, M1≤M, M2≤P, and 1≤S1≤M1, 1≤S2≤M2; Among them, when the one or more electronic components located in the M1th row of the first electronic component matrix of the first substrate are transferred to the M2th row of the second electronic component matrix of the second substrate, the relative movement distance along the first axis direction is [(M2-S2)*X2-(M1-S1)*X1].
32. The method for mass transferring electronic components with adjustable spacing as claimed in claim 31, further comprising the following steps: Providing a third substrate and disposing the third substrate below the second substrate, the third substrate having a third upper surface and a third lower surface opposite to each other, and the second upper surface of the second substrate faces the third upper surface of the third substrate; and The second electronic component matrix located on the second substrate is transferred to the third substrate, and a third electronic component matrix formed by U rows of electronic components multiplied by V columns of electronic components is formed on the third substrate, and the row spacing and column spacing of the third electronic component matrix are X2 and Y2 respectively, where U and V are natural numbers greater than 1.
33. The method for mass transferring electronic components with adjustable spacing as claimed in claim 32, wherein the step of forming the third electronic component matrix is: include: Using the plurality of electronic components located in the R1th column of the second substrate as a third baseline of the second substrate along the first axis direction, using the plurality of electronic components located in the R2th column of the third substrate as a fourth baseline of the third substrate along the first axis direction, and aligning the third baseline with the fourth baseline; as well as A second light with a second wavelength is provided above the second substrate, so that the second light with the second wavelength irradiates the second substrate where the electronic components or the plurality of electronic components located in the N1th column of the second electronic component matrix are located, so that the electronic components or the plurality of electronic components located in the N1th column of the second substrate are thermally decomposed or photolyzed to lose viscosity, and the electronic components or the plurality of electronic components located in the N1th column of the second substrate are selectively peeled off and bonded to the third upper surface of the third substrate so that the electronic components or the plurality of electronic components located in the N2th column of the third electronic component matrix are located, wherein R1, R2, N1, and N2 are natural numbers, N1≤N, N2≤V, and 1≤R1≤ N1, 1≤R2≤N2; Among them, when the one or more electronic components located in the N1th column of the second electronic component matrix of the second substrate are transferred to the N2th column of the third electronic component matrix of the third substrate, the relative movement distance along the second axis direction is [(N2-R2)*Y2-(N1-R1)*Y1].
34. The method for mass transfer of electronic components with adjustable pitch as claimed in claim 27 or 31, wherein the first substrate is a pyrolytic adhesive film, and the first light with the first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
35. The method for mass transfer of electronic components with adjustable pitch as claimed in claim 27 or 31, wherein the first substrate is a photoresist film, and the first light with the first wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
36. The method for mass transferring electronic components with adjustable pitch as claimed in claim 29 or 33, wherein the second substrate is a pyrolytic adhesive film, and the second light with a second wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
37. The method for mass transfer of electronic components with adjustable pitch as claimed in claim 29 or 33, wherein the second substrate is a photoresist film, and the second light with a second wavelength is a light with a wavelength between 100 nanometers and 12,000 nanometers.
38. The method for mass transferring electronic components with adjustable pitch as claimed in claim 25, wherein the plurality of electronic components are selected from one or more groups consisting of light emitting diodes, laser diodes and semiconductor components.
39. The method for mass transferring electronic components with adjustable pitch as claimed in claim 38, wherein the light emitted by the plurality of light emitting diodes is red light, green light, blue light, yellow light, white light, infrared light or ultraviolet light.
40. The method for mass transferring electronic components with adjustable pitch as claimed in claim 38, wherein the wavelengths of the plurality of laser diodes are between 390 nanometers and 1700 nanometers.
41. The method for mass transferring electronic components with adjustable pitch as claimed in claim 38, wherein the plurality of semiconductor components are selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits and analog integrated circuits.