Simple preparation method of pre-patterned copper-clad ceramic circuit board

By introducing laser ablation equipment to finely remove the solder, the problems of customization of printed screen boards and spillover of solder in the prior art are solved, and the simple preparation of AMB copper-clad ceramic circuit board is realized, which reduces costs and increases the Preparation accuracy and consistency promote large-scale production of products.

CN119053042APending Publication Date: 2024-11-29JIANGSU AOLIWEI SENSING TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411182549.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

During the preparation process of existing AMB copper-clad ceramic circuit boards, printed screen boards need to be specially customized and the solder spills are irregular, which makes it difficult to promote on a large scale.

Method used

Introduce laser ablation equipment to finely remove the printed and pre-baked brazed brazing material, use the CCD camera of the laser ablation equipment to identify the Mark point for alignment, and perform laser ablation according to preset parameters to avoid overflow of brazing material , and prevent pollution through vacuuming air knives and water cooling system.

Benefits of technology

It reduces the customization demand for printed screen boards, improves the accuracy and consistency of brazing material removal, reduces costs, and realizes copper-clad ceramic circuit board products with no residues in solder and controllable size, with advantages of large-scale promotion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119053042A_ABST
    Figure CN119053042A_ABST
Patent Text Reader

Abstract

The invention discloses a simple preparation method of a pre-patterned copper-clad ceramic circuit board, and the method comprises the steps: S1), drilling and cleaning a ceramic chip, and cleaning a copper sheet; S2), printing a brazing material on the front surface of the ceramic chip through a general printing screen, and carrying out the pre-baking after the printing; s3) printing the brazing material on the reverse side of the ceramic chip by adopting a general printing screen, and pre-baking after printing; s4) removing the welding flux through laser ablation; s5) lamination; s6) performing high-temperature brazing; according to the method, by introducing laser ablation equipment, optimization of an existing preparation method is achieved, the customization requirement of a printing screen in an existing scheme is reduced, printed and pre-baked brazing filler metal is finely removed, and the poor appearance or poor function loss caused by irregular overflow of the brazing filler metal in the brazing filler metal printing process is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of semiconductor technology, and in particular to a simple preparation method for a pre-patterned copper-clad ceramic circuit board. Background Art

[0002] AMB copper-clad ceramic substrate materials are widely used in semiconductor module device packaging with high power and high heat dissipation requirements due to their high thermal conductivity and high insulation properties.

[0003] The preparation process of AMB copper-clad ceramic circuit boards mainly involves three kinds of raw materials, namely ceramic substrates, copper, and brazing materials. Among them, ceramics are mostly silicon nitride, aluminum nitride, and aluminum oxide. The thickness of ceramics is generally ≤2mm. Brazing materials are mostly silver-copper-titanium or copper-titanium alloy materials. The thickness of brazing materials is generally ≤0.05mm. Copper is mostly oxygen-free copper with a purity of more than 99.9%, and the thickness of copper strips is generally ≤2mm. At present, most of the companies that have the ability to mass-produce AMB copper-clad ceramic circuit boards are foreign-funded enterprises, and most domestic companies are in the sample stage. Reducing costs in the process of converting samples to mass production is an important issue in the industrialization of AMB copper-clad ceramic circuit board products.

[0004] In the prior art, patent document CN114466519B provides a pre-patterned copper-clad ceramic substrate and a preparation method thereof. By making a pattern on the printing screen in advance, the etching of the brazing material in this area after the brazing is completed can be avoided, thereby achieving the original intention of cost saving. However, in the actual preparation process, due to the inconsistency of the product patterns on the front and back sides, the printing screens on the front and back sides of the ceramic sheet need to be specially customized, and the precision requirements for the opening size of the printing screen are extremely high. After the brazing material is printed, it is limited by the irregular overflow characteristics of the brazing material. The brazing material will overflow to the edge of the pattern, and the size of the brazing material overflow area is not fixed, and the thickness is uneven. Overall, this solution has limitations, high process difficulty, and it is difficult to promote on a large scale. Summary of the invention

[0005] The purpose of the present invention is to overcome the defects of the prior art and provide a simple preparation method for a pre-patterned copper-clad ceramic circuit board. By introducing laser ablation equipment, the existing preparation method is optimized, the customization requirements of the printing screen in the existing scheme are reduced, and the printed and pre-baked solder is finely removed to avoid irregular overflow of the solder during the solder printing process, resulting in poor appearance or poor function.

[0006] The object of the present invention is achieved by: a simple method for preparing a pre-patterned copper-clad ceramic circuit board, comprising the following steps: S1) Ceramic sheet drilling and cleaning, copper sheet cleaning: Ceramic sheets are drilled using laser technology. After drilling, the ceramic sheets need to be cleaned to remove residues and contaminants generated during the processing; copper sheets are cleaned to remove oil and impurities on the surface; S2) The brazing material on the front side of the ceramic sheet is printed using a universal printing screen and pre-baked after printing; S3) The brazing material on the reverse side of the ceramic sheet is printed using a universal printing screen and pre-baked after printing; S4) Laser ablation to remove solder: By introducing laser ablation equipment, the printed and pre-baked solder is finely removed to achieve pre-patterning of the solder; S5) Lamination: Placing copper foil layers on both sides of a ceramic substrate coated with metal solder to form a copper-solder-ceramic-solder-copper structure for lamination assembly; S6) High temperature brazing: clamp the treated copper foil and ceramic substrate together, and then put them into a vacuum brazing furnace for vacuum welding; S7) Copper line etching: After the test is passed, etching and surface treatment are carried out. The copper on the ceramic surface is chemically etched according to the design requirements to generate the designed patterns and lines.

[0007] Furthermore, the step 4) specifically includes: during the laser ablation process to remove the solder, the ceramic sheet that has been pre-baked with the solder is placed on the workbench, the vacuum suction is turned on to fix the product, the CCD camera of the laser ablation equipment is used to identify the mark point on the ceramic sheet to achieve alignment, and then the laser ablation equipment performs laser ablation at a specific position according to the preset solder removal pattern and preset parameters of the ceramic sheet; during the entire laser ablation process, a vacuum air knife and a water cooling system are configured to ensure that the vaporized substances generated during the solder ablation process will not contaminate the surface of the ceramic sheet, and after the solder ablation is completed, the vacuum suction is turned off.

[0008] Furthermore, the laser power range of the laser ablation equipment in step 4) is 10W-1000W; the laser pulse frequency range is 50KHz-2000KHz; the laser pulse width is 10fs-10ms; and the laser scanning speed is 10-2000mm / s.

[0009] Furthermore, the vacuum suction pressure ranges from -0.08MPa to 0Mpa.

[0010] Furthermore, the temperature of the water cooling system is set to 0-20°C.

[0011] The present invention adopts the above technical scheme, and compared with the prior art, the beneficial effects are as follows: 1) by introducing laser ablation equipment, the existing preparation method is optimized, the customization requirements of the printing screen in the existing scheme are reduced, and a conventional full-surface screen printing screen can be selected, the screen size requirements are low, the cost is low, and it is easy to promote on a large scale; 2) by introducing laser ablation equipment, the existing preparation method is optimized, the high-precision screen printing screen requirements in the existing scheme are avoided, the accuracy of the pre-pattern can ignore the influence of the irregular overflow of the solder after printing, and it is controlled by the laser ablation equipment, and the size accuracy is higher; 3) by introducing laser ablation equipment, the existing preparation method is optimized, and the solder step etching size in the process of etching the solder by the existing chemical solution is simple and controllable by laser ablation, which is not affected by the matching of the solder etching solution and the solder composition, and is more convenient to control the size consistency in the solder etching step process; 4) the copper-clad ceramic circuit board product prepared by this method has no solder residue and controllable size, and has cost advantages and large-scale promotion advantages. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 Flowchart of the present invention. DETAILED DESCRIPTION

[0013] like Figure 1 A simple method for preparing a pre-patterned copper-clad ceramic circuit board is shown, comprising the following steps: S1) Ceramic sheet drilling and cleaning, copper sheet cleaning: Ceramic sheets are drilled using laser technology. After drilling, the ceramic sheets need to be cleaned to remove residues and contaminants generated during the processing; copper sheets are cleaned to remove oil and impurities on the surface; S2) The brazing material on the front side of the ceramic sheet is printed using a universal printing screen and pre-baked after printing; S3) The brazing material on the reverse side of the ceramic sheet is printed using a universal printing screen and pre-baked after printing; In step 2) and step 3), the stencil is universal and does not need to be specially customized, which is low-cost; S4) Laser ablation to remove solder: By introducing laser ablation equipment, the printed and pre-baked solder is finely removed to achieve pre-patterning of the solder; during the laser ablation to remove solder, the pre-baked ceramic sheet is placed on the workbench, the vacuum suction is turned on to fix the product, and the CCD camera of the laser ablation equipment is used to identify the mark point on the ceramic sheet to achieve alignment, and then the laser ablation equipment performs laser ablation at a specific position according to the preset solder removal pattern and preset parameters of the ceramic sheet; during the entire laser ablation process, a vacuum air knife and a water cooling system are configured to ensure that the vaporized substances generated during the solder ablation process will not contaminate the surface of the ceramic sheet, and the vacuum suction is turned off after the solder ablation is completed; The laser power range of the laser ablation equipment is 10W-1000W; the laser pulse frequency range is 50KHz-2000KHz; the laser pulse width is 10fs-10ms; the laser scanning speed is 10-2000mm / s; the laser scanning interval is 0.01-0.2mm; the laser scanning times is 10-2000mm / s; the vacuum pressure range is -0.08MPa-0Mpa. The water cooling system temperature is set to 0-20℃; S5) Lamination: Placing copper foil layers on both sides of a ceramic substrate coated with metal solder to form a copper-solder-ceramic-solder-copper structure for lamination assembly; S6) High temperature brazing: clamp the treated copper foil and ceramic substrate together, and then put them into a vacuum brazing furnace for vacuum welding; S7) Copper line etching: After the test is passed, etching and surface treatment are carried out. The copper on the ceramic surface is chemically etched according to the design requirements to generate the designed patterns and lines.

[0014] The present invention provides a simple preparation method for a pre-patterned copper-clad ceramic circuit board. By introducing a laser ablation device, the printed and pre-baked solder is finely removed to avoid the poor appearance or poor function caused by the irregular overflow of the solder during the solder printing process.

[0015] The present invention is not limited to the above-mentioned embodiments. On the basis of the technical solution disclosed in the present invention, technicians in this field can make some substitutions and deformations to some technical features therein according to the disclosed technical content without creative labor, and these substitutions and deformations are all within the protection scope of the present invention.

Claims

1. A simple method for preparing a pre-patterned copper-clad ceramic circuit board, characterized in that: The following steps are involved: S1) Ceramic sheet drilling and cleaning, copper sheet cleaning: Ceramic sheets are drilled using laser technology. After drilling, the ceramic sheets need to be cleaned to remove residues and contaminants generated during the processing; copper sheets are cleaned to remove oil and impurities on the surface; S2) The brazing material on the front side of the ceramic sheet is printed using a universal printing screen and pre-baked after printing; S3) The brazing material on the reverse side of the ceramic sheet is printed using a universal printing screen and pre-baked after printing; S4) Laser ablation to remove solder: By introducing laser ablation equipment, the printed and pre-baked solder is finely removed to achieve pre-patterning of the solder; S5) Lamination: Placing copper foil layers on both sides of a ceramic substrate coated with metal solder to form a copper-solder-ceramic-solder-copper structure for lamination assembly; S6) High temperature brazing: clamp the treated copper foil and ceramic substrate together, and then put them into a vacuum brazing furnace for vacuum welding; S7) Copper line etching: After the test is passed, etching and surface treatment are carried out. The copper on the ceramic surface is chemically etched according to the design requirements to generate the designed patterns and lines.

2. A simple method for preparing a pre-patterned copper-clad ceramic circuit board according to claim 1, characterized in that: The step 4) specifically includes: during the process of laser ablation to remove the solder, placing the ceramic sheet that has been pre-baked with the solder on a workbench, turning on the vacuum suction to fix the product, using the CCD camera of the laser ablation equipment to identify the mark point on the ceramic sheet to achieve alignment, and then the laser ablation equipment performs laser ablation at a specific position according to the preset solder removal pattern and preset parameters of the ceramic sheet; during the entire laser ablation process, a vacuum air knife and a water cooling system are configured to ensure that the vaporized substances generated during the solder ablation process will not contaminate the surface of the ceramic sheet, and after the solder ablation is completed, the vacuum suction is turned off.

3. The simple preparation method of a pre-patterned copper-clad ceramic circuit board according to claim 1, characterized in that: The laser power range of the laser ablation equipment in step 4) is 10W-1000W; the laser pulse frequency range is 50KHz-2000KHz; the laser pulse width is 10fs-10ms; and the laser scanning speed is 10-2000mm / s.

4. The simple preparation method of a pre-patterned copper-clad ceramic circuit board according to claim 2, characterized in that: The vacuum suction pressure ranges from -0.08MPa to 0Mpa.

5. The simple preparation method of a pre-patterned copper-clad ceramic circuit board according to claim 2, characterized in that: The water cooling system temperature is set at 0-20°C.

Citation Information

Cited By

  • High-temperature heat pipe recovery device and method

    CN120243594A